A ladle air-permeable brick and ladle for enhancing molten pool stirring
By using a rotating slit structure in the ladle breathable brick to form a swirl gas, the problem of enhanced breathability in the prior art has been solved, and the more efficient melt pool stirring and removal effect is achieved, which improves the liquid steel Cleanliness and uniformity.
Patent Information
- Application Number
- CN202210313023.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-03-28
AI Technical Summary
When the existing slit-type ladle breathable bricks improve the agitation effect of the molten pool, the enhanced breathability will lead to a decrease in corrosion resistance, and the different arrangement positions will lead to differences in metallurgical effects, making it difficult to evenly control the temperature and composition of the molten steel.
A ladle breathable brick is designed to enhance the stirring of the molten pool, and a rotating slit structure with a circular table-shaped body connected to the gas partition chamber is designed to form a cyclone gas, improve the gas flow and contact area, and improve the stirring capacity.
Under the same conditions, the stirring capacity is increased by more than 20%, and the desulfurization rate and inclusion removal rate are increased by more than 5%, which significantly improves the cleanliness and uniformity of the steel.
Smart Images

Figure CN114635015B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of ladle bottom blowing in steelmaking process, and particularly relates to a ladle air-permeable brick and a ladle for enhancing molten pool stirring. Background Art
[0002] Ladle bottom blowing technology is a commonly used technology in the current steelmaking process. Inert gases such as argon are blown into the molten steel through the air-permeable bricks installed at the bottom of the ladle. The buoyancy of the inert gas bubbles is used to stir the molten pool, thereby enhancing the fluidity of the molten steel and making the temperature and composition of the molten steel uniform. At the same time, the bubbles can provide a matrix for the non-metallic inclusions in the steel to adhere to, so that they float up into the slag along with the bubbles, thereby removing the non-metallic inclusions in the steel and accurately controlling the composition of the molten steel.
[0003] Ladle air bricks are key functional components of ladle bottom blowing technology and are crucial to the metallurgical effect of ladle bottom blowing technology. Among them, slit-type ladle air bricks are widely used due to their advantages such as a large adjustable range of gas supply and good anti-erosion performance. At present, the most commonly used is the straight-through slit air brick. The center line of each slit of this type of slit air brick is parallel to the central axis of the air brick. Since the flow of gas in the slit air brick is laminar, the air flow formed by the gas after passing through the slit is also parallel to each other. As the capacity of the ladle gradually increases, it is necessary to increase the number of slits to enhance the air permeability of the air brick, but the increase in the number of slits will weaken the anti-erosion ability of the air brick, thereby reducing the life of the air brick. At the same time, the metallurgical effect achieved by the ladle bottom blowing technology varies greatly depending on the location of the air brick. Therefore, in order to improve the permeability of the ladle air brick and achieve better metallurgical effects, it is particularly important to optimize the structure and layout of the air brick. Summary of the invention
[0004] In order to solve the above technical problems, the present invention provides a ladle air brick and a ladle for enhancing molten pool stirring. The present invention can effectively remove non-metallic inclusions in molten steel, improve the cleanliness of molten steel, and at the same time play a role in uniformizing the temperature and composition of molten steel.
[0005] The technical solution adopted by the present invention is as follows:
[0006] A ladle air-permeable brick for enhancing molten pool stirring comprises a truncated cone-shaped main body, a gas distribution chamber is provided inside the large end of the truncated cone-shaped main body, an air inlet pipe is connected to the large end of the truncated cone-shaped main body, the air inlet pipe is communicated with the gas distribution chamber, a plurality of slits are arranged in the truncated cone-shaped main body, one end of the slit is communicated with the gas distribution chamber, the other end of the slit extends to the end face of the small end of the truncated cone-shaped main body, and the plurality of slits are rotationally symmetrical about the central axis of the truncated cone-shaped main body; the gas in the gas distribution chamber can form a vortex at the small end of the truncated cone-shaped main body after passing through the slits.
[0007] Preferably, the ports of the slit at the small end and the large end of the truncated cone-shaped body are arranged along the radial direction of the truncated cone-shaped body; for each slit, the ports at both ends of the slit have an angle of 3° to 15° along the end surface of the truncated cone-shaped body; the ports at both ends of the slit have the same shape and size, and the distances between the ports at both ends of the slit and the central axis of the truncated cone-shaped body are the same.
[0008] Preferably, the slit is a slit of a spatial curved surface formed by relative rotation of the large end face and the small end face of the truncated cone-shaped body by 3° to 15°. The original slit is a rectangular slit, the axis of which is parallel to the central axis of the truncated cone-shaped body, and the ports at both ends of the rectangular slit have the same shape and size.
[0009] Preferably, the number of the slits is 8 to 36.
[0010] Preferably, the cross-section of the slit is rectangular, the thickness of the slit cross-section is 0.10 mm to 0.18 mm, and the ratio of the width of the slit cross-section to the radius of the small end of the truncated cone body is (1 to 2):3, wherein the rectangular width directions of the slit on the small end of the truncated cone body and the large end of the truncated cone body point to the center of the working surface and the bottom surface, respectively.
[0011] Preferably, the air distribution chamber is a cylindrical chamber coaxial with the truncated cone-shaped main body.
[0012] The present invention further provides a ladle, comprising a ladle body, on which the ladle body is provided with the ladle air-permeable bricks for enhancing molten pool stirring as described above.
[0013] Preferably, the ladle is a 30-400t ladle.
[0014] Preferably, when the ladle has a capacity of 60t or less, a ladle air brick for enhancing molten pool stirring is used at the bottom of the ladle body. In the radial direction of the bottom surface of the ladle body, the ladle air brick for enhancing molten pool stirring is arranged between 0.3R and 0.8R, and the angle between the ladle air brick for enhancing molten pool stirring and the arc radius of the water outlet on the ladle body is greater than 90°, wherein R is the radius of the bottom surface of the ladle body.
[0015] Preferably, when the ladle has a capacity of 60 t or more, two of the ladle air bricks for enhancing molten pool stirring are used at the bottom of the ladle body, and the two ladle air bricks for enhancing molten pool stirring are respectively recorded as the first ladle air brick and the second ladle air brick, the angle between the first ladle air brick and the radius of the arc where the water outlet is located is 100°~130°, the angle between the first ladle air brick and the radius of the arc where the second ladle air brick is located is 100°~150°, and the distance between the first ladle air brick and the second ladle air brick to the center of the bottom surface of the ladle body is between 0.5R and 0.65R, wherein R is the radius of the bottom surface of the ladle body.
[0016] The present invention has the following beneficial effects:
[0017] The slits of the ladle air brick for enhancing the stirring of the molten pool provided by the present invention have a certain inclination angle, and each slit is rotationally symmetrical about the central axis of the truncated cone-shaped body. This arrangement can change the airflow direction of the air brick, and a swirl-type slit arrangement is used to form a gas swirl, so that bubbles are dispersed in the molten steel, and the contact area between the gas stream and the molten steel is expanded, thereby promoting the flow of the molten pool in the ladle. Under the conditions of the same number of slits, slit cross-sectional area and bottom blowing flow rate, the ability of the ladle air brick provided by the present invention to penetrate and stir the molten pool is compared with the straight-through slit ladle air brick, and the stirring capacity is improved by more than 20%, the desulfurization rate can be increased by more than 5%, and the inclusion removal rate is increased by more than 5%. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The accompanying drawings are provided to provide a further understanding of the present invention and constitute a part of the specification.
[0019] Figure 1 A three-dimensional schematic diagram of a ladle air-permeable brick for enhancing molten pool stirring provided by the present invention.
[0020] Figure 2 A schematic diagram of a ladle provided by the present invention.
[0021] In the figure: 1-truncated cone-shaped body, 2-central axis of the truncated cone-shaped body, 3-gas chamber, 4-bottom surface, 5-inlet pipe, 6-slit, 7-central axis of the slit, 8-working surface, 9-ladle body, 9-1-water inlet, 9-2-ladle air brick A, 9-3-ladle air brick B, 9-4-ladle air brick C. DETAILED DESCRIPTION
[0022] The ladle air bricks and their arrangement and use methods of the present invention are further described below with reference to examples, but the protection scope of the present invention is not limited to these examples.
[0023] Reference Figure 1The ladle air brick for enhancing molten pool stirring of the present invention comprises a truncated cone-shaped main body 1 and an air inlet pipe 5. The large end of the truncated cone-shaped main body 1 has an air distribution chamber 3 inside, and the air distribution chamber 3 is a cylindrical chamber coaxial with the truncated cone-shaped main body 1. The large end center of the truncated cone-shaped main body 1 is connected with an air inlet pipe 5, and the air inlet pipe 5 is connected with the air distribution chamber 3. A plurality of slits 6 are arranged in the truncated cone-shaped main body 1, and the plurality of slits 6 form a slit group. One end of the slit 6 is connected with the air distribution chamber 3, and the other end of the slit 6 extends to the end face of the small end of the truncated cone-shaped main body 1. The plurality of slits 6 are rotationally symmetrical about the central axis 2 of the truncated cone-shaped main body 1; a plurality of slits 6 are combined to form a cyclonic slit, and an inert gas such as argon will form a cyclonic gas after passing through the cyclonic slit, so that bubbles are highly dispersed in the molten steel, and the contact area between the gas stream and the molten steel is expanded, thereby promoting the flow of the molten pool in the ladle. The number of slits 6 is 8 to 36, and the specific number is determined according to the capacity of the ladle, with the upper limit for large ladle and the lower limit for small ladle. The cross section of the slit 6 is rectangular, the thickness is 0.10 mm to 0.18 mm, and the ratio of the width to the radius of the main body working surface 8 (i.e., the small end surface of the truncated cone-shaped main body 1) is (1 to 2):3. The rectangular width direction of each slit 6 on the working surface 8 and the bottom surface 4 points to the center of the working surface 8 and the bottom surface 4 respectively. The slit 6 is a slit of a spatial curved surface formed by the original slit after the large end surface and the small end surface of the truncated cone-shaped main body 1 are relatively rotated by 3° to 15°. The original slit is a rectangular slit, the axis of the rectangular slit is parallel to the central axis 2 of the truncated cone-shaped main body, and the ports at both ends of the rectangular slit have the same shape and size.
[0024] The ladle air brick for enhancing molten pool stirring of the present invention is suitable for 30-400t ladle and is arranged as follows:
[0025] 1 For ladles with a capacity of 60t or less, a ladle air brick A is used and arranged between 0.3R and 0.8R in the radial direction of the ladle body 9, where R is the radius of the bottom surface of the ladle, and the angle between the ladle air brick A and the radius of the arc where the water inlet is located is greater than 90°;
[0026] 2 For ladles with a capacity of more than 60t, two air bricks are used, namely ladle air brick B and ladle air brick C. The angle α between the ladle air brick B and the radius of the arc where the water inlet is located is 100°~130°, and the angle β between the ladle air brick B and the radius of the arc where the ladle air brick C is located is 100°~150°. In the radial direction of the ladle body 9, the distance from the ladle air brick B and the ladle air brick C to the center of the ladle bottom surface is between 0.5R~0.65R.
[0027] The ladle of the present invention can effectively reduce the consumption of materials such as argon gas by reasonably arranging the ladle air-permeable bricks of the present invention, reduce production costs, improve production efficiency, and have significant economic benefits.
[0028] Embodiment 1:
[0029] The ladle air brick for enhancing the stirring of the molten pool in this embodiment is applied to a 50t ladle. The slit 6 is a slit of a space curved surface formed by rotating the large end face and the small end face of the truncated cone-shaped body 1 by 4°. The number of the slits 6 is 16, and the thickness of the slit 6 is 0.14 mm and the width is 20 mm. A ladle air brick A is used and arranged at 0.45R (where R is the radius of the bottom surface of the ladle). The angle between the ladle air brick A and the radius of the arc where the water inlet is located is 150°.
[0030] Embodiment 2:
[0031] The ladle air brick for enhancing the stirring of the molten pool in this embodiment is applied to a 180t ladle. The slit 6 is a slit of a space curved surface formed by rotating the large end face and the small end face of the truncated cone-shaped main body 1 by 8°. The number of the slits 6 is 24, and the thickness of the slit 6 is 0.17 mm and the width is 30 mm. Two air bricks are used, namely, ladle air brick B and ladle air brick C. The angle α between the ladle air brick B and the radius of the arc where the water inlet is located is 110°, the angle β between the ladle air brick B and the radius of the arc where the ladle air brick C is located is 130°, and the distance between the ladle air brick B and the ladle air brick C and the center of the bottom surface of the ladle is 0.55R.
[0032] Embodiment 3:
[0033] The ladle air bricks for enhancing the stirring of the molten pool in this embodiment are applied to a 350t ladle. The slits 6 are original slits with rectangular cross-sections, and the large end face and the small end face of the truncated cone-shaped body 1 are relatively rotated by 14° to form a slit of a spatial curved surface. The number of the slits 6 is 32, and the thickness of the slits 6 is 0.20 mm and the width is 36 mm. Two air bricks are used, namely, ladle air brick B and ladle air brick C. The angle α between the ladle air brick B and the radius of the arc where the water inlet is located is 120°, and the angle β between the ladle air brick B and the radius of the arc where the ladle air brick C is located is 140°. The distance between the ladle air brick B and the ladle air brick C and the center of the bottom surface of the ladle is 0.60R.
[0034] The present invention provides a new type of ladle air brick, reasonably arranges the air bricks, and cooperates with a staged bottom blowing control system, thereby effectively reducing the consumption of materials such as argon and reducing production costs, improving production efficiency, and having significant economic benefits while ensuring the quality of molten steel.
Claims
1. A ladle air brick for enhancing molten pool stirring, characterized in that: The invention comprises a truncated cone-shaped body (1), wherein a gas distribution chamber (3) is provided inside the large end of the truncated cone-shaped body (1), an air inlet pipe (5) is connected to the large end of the truncated cone-shaped body (1), the air inlet pipe (5) is communicated with the gas distribution chamber (3), a plurality of slits (6) are arranged in the truncated cone-shaped body (1), one end of the slits (6) is communicated with the gas distribution chamber (3), the other end of the slits (6) extends to the end surface of the small end of the truncated cone-shaped body (1), and the plurality of slits (6) are rotationally symmetrical about the central axis (2) of the truncated cone-shaped body (1); the gas in the gas distribution chamber (3) can form a swirling flow at the small end of the truncated cone-shaped body (1) after passing through the slits (6); The ports of the slit (6) at the small end and the large end of the truncated cone-shaped body (1) are arranged along the radial direction of the truncated cone-shaped body (1); for each slit (6), the ports at both ends of the slit (6) have an angle of 4° to 14° along the end surface of the truncated cone-shaped body (1); the ports at both ends of the slit (6) have the same shape and size, and the distances between the ports at both ends of the slit (6) and the central axis (2) of the truncated cone-shaped body are the same; The slit (6) is a slit of a spatial curved surface formed by relatively rotating the large end face and the small end face of the truncated cone-shaped body (1) by 4° to 14°. The original slit is a rectangular slit, the axis of which is parallel to the central axis (2) of the truncated cone-shaped body, and the ports at both ends of the rectangular slit have the same shape and size. The cross section of the slit (6) is rectangular, and the rectangular width directions of the slit (6) on the small end of the truncated cone-shaped body (1) and the large end of the truncated cone-shaped body (1) point to the center of the working surface (8) and the bottom surface (4), respectively.
2. The ladle air brick for enhancing molten pool stirring according to claim 1, characterized in that: The number of the slits (6) is 8 to 36.
3. The ladle air brick for enhancing molten pool stirring according to claim 2, characterized in that: The cross-sectional thickness of the slit (6) is 0.10 mm to 0.18 mm, and the ratio of the cross-sectional width of the slit (6) to the radius of the small end of the truncated cone-shaped body (1) is (1 to 2):
3.
4. The ladle air brick for enhancing molten pool stirring according to claim 1, characterized in that: The gas separation chamber (3) is a cylindrical chamber coaxial with the truncated cone-shaped main body (1).
5. A ladle, characterized in that: It comprises a ladle body (9), on which the ladle body (9) is provided with the ladle air-permeable brick for enhancing molten pool stirring according to any one of claims 1 to 4.
6. A ladle according to claim 5, characterized in that: The ladle is a 30-400t ladle.
7. A ladle according to claim 6, characterized in that: When the ladle has a capacity of 60 t or less, the bottom of the ladle body (9) is provided with a ladle air brick for enhancing molten pool stirring. In the radial direction of the bottom surface of the ladle body (9), the ladle air brick for enhancing molten pool stirring is arranged between 0.3R and 0.8R. The angle between the ladle air brick for enhancing molten pool stirring and the arc radius of the water inlet on the ladle body (9) is greater than 90°, wherein R is the bottom surface radius of the ladle body (9).
8. A ladle according to claim 6, characterized in that: When the ladle has a capacity of 60 t or more, two ladle air bricks for enhancing molten pool stirring are used at the bottom of the ladle body (9), and the two ladle air bricks for enhancing molten pool stirring are respectively recorded as the first ladle air brick and the second ladle air brick. The angle between the first ladle air brick and the radius of the arc where the water inlet is located is 100°~130°, and the angle between the first ladle air brick and the radius of the arc where the second ladle air brick is located is 100°~150°. The distance between the first ladle air brick and the second ladle air brick to the center of the bottom surface of the ladle body (9) is between 0.5R~0.65R, wherein R is the radius of the bottom surface of the ladle body (9).