Multi-frequency reconfigurable absorber based on water-graphene-VO2 stack

By using temperature-controlled Vanadium dioxide and graphene Fermi level tuning in the water-graphene-VO2 stacked absorber, the multi-band absorption and reconstructible wave bands are achieved, and the existing technology is solved The problem of difficulty in tuning and reconstruction of multi-band wave absorbers has achieved efficient multi-band absorption and flexible frequency adjustment.

CN114759358BActive Publication Date: 2024-11-22XIDIAN UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210360049.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-06
Publication Date
2024-11-22
Estimated Expiration
2042-04-06

AI Technical Summary

Technical Problem

The prior art is difficult to realize the tunable and reconfigurable of the absorber in a multi-band range, especially the tuning and reconstruction functions in a small range of the absorption bands above four bands and the absorption bands, which limits its application range.

Method used

Using a multi-frequency reconstructible absorber based on water-graphene-VO2 stack, the dielectric and metal states of vanadium dioxide are converted through external temperature control, combined with the Fermi level tuning of graphene, and the full dielectric material structure is used. The absorber is designed including a water-based polytetrafluoroethylene layer, a graphene layer, a silicon layer and a metal layer to achieve multi-band absorption and reconstructible absorption bands.

Benefits of technology

Absorption of multiple bands in the 0-3 THz frequency band, and the number of absorption bands is adjusted at different temperatures to reach an absorption rate of more than 99%. The structure is simple and easy to process, and is suitable for applications in multi-band and multi-absorbing bands.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114759358B_ABST
    Figure CN114759358B_ABST
Patent Text Reader

Abstract

The present invention proposes a multi-frequency reconfigurable perfect absorber based on water-graphene-VO2 stacking, which mainly solves the problem that it is difficult for existing terahertz absorbers to achieve perfect absorption, small-range tunable absorption bands and reconfigurable absorption bands while absorbing waves in multiple bands. It includes a water-based polytetrafluoroethylene layer, a water layer, a graphene layer, two silicon layers, a vanadium dioxide layer and a metal layer, wherein the water-based polytetrafluoroethylene layer is a hollow cube, and the interior of its cavity is completely filled with a water layer, forming an integral structure in which the water-based polytetrafluoroethylene layer, the graphene layer, the first silicon layer, the vanadium dioxide layer, the second silicon layer and the metal layer are arranged in order from top to bottom, and each layer is tightly and seamlessly fitted to each other. The present invention improves the absorption effect through the water layer, so that the absorption rate of multiple bands reaches more than 99%, and the temperature-varying characteristics of the vanadium dioxide layer are used to realize the reconfigurable absorption frequency. The absorption frequency and absorption rate intensity of multiple bands are tuned by controlling the size of the graphene Fermi level, which can be used for the absorption of terahertz electromagnetic waves.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of metamaterial devices, and in particular relates to a reconfigurable multi-frequency absorber which can be used for absorbing terahertz electromagnetic waves. Background Art

[0002] Terahertz waves have broad application prospects in broadband communications, spectrum analysis, detection and sensing, etc. Terahertz metamaterial absorbers are devices that can convert electromagnetic wave energy incident on their surface into other energy losses at the working frequency band. People have used metamaterial technology to prepare various terahertz wave absorbers, which can achieve single-band, multi-band, broadband and ultra-broadband absorption.

[0003] In the terahertz band, multi-band tunable metamaterial absorbers are more attractive and are the main development direction at present. In particular, in the field of frequency-selective terahertz thermal imaging, terahertz absorbers that can dynamically and continuously adjust the absorption bandwidth are usually required. Multi-band metamaterial tunable absorbers absorb at multiple specific frequency points or multiple specific frequency ranges, and can dynamically and continuously adjust the absorption bandwidth.

[0004] Nanjing University of Science and Technology disclosed in its patent document with application number 202011492297.X a beam controller with dual functions of bandpass filtering and absorption in the terahertz frequency band. It uses two different types of tunable materials to design a one-dimensional photonic crystal tunable terahertz device. When VO2 is in the metal phase, it can realize the electromagnetic wave absorption function of a single frequency point. When VO2 is in the insulating phase, the terahertz wave with a frequency in the defect state will enter the one-dimensional photonic crystal to propagate, realizing the bandpass filtering function, and tuning the working frequency by adjusting the chemical potential of graphene to achieve the purpose of dual tuning of the absorbing function and the working frequency. Due to the limitations of the selected material, this absorber can only be used for single-band absorption and can only be tuned within a small range of absorption bands. It is not suitable for the current wider application scenarios with multi-band absorption, tunable in a small range of multiple absorption bands, and reconfigurable multi-absorption bands.

[0005] Nanjing University of Aeronautics and Astronautics disclosed a multi-band THz absorber based on a superstructure in its patent document with application number 202011620376.4. It designed a hollow snowflake-shaped micro-unit structure layer, which can obtain multiple absorption peaks in the 0.2-3.0THz frequency band. However, this micro-unit structure can only produce a specific number of absorption peaks, and the absorption rate cannot reach the absorption rate, which cannot meet the current needs for multi-band absorption, tunable multi-absorbing bands within a small range, and reconfigurable multi-absorbing bands.

[0006] In summary, although existing research can achieve the functions of single-band absorption, multi-band absorption and tunable single absorption band within a small range, it is difficult to achieve simultaneous absorption in multiple bands, tunable absorption band within a small range and reconfigurable absorption band due to its material and structural limitations. In particular, it is impossible to achieve absorption in more than four bands, tunable absorption band within a small range and reconfigurable absorption band, which greatly limits its application range. Summary of the invention

[0007] The purpose of the present invention is to address the problems existing in the prior art and propose a multi-frequency reconfigurable absorber based on water-graphene-VO2 stacking, so as to further realize the reconfiguration of the absorption band on the basis of realizing multiple band absorption in the frequency band range of 0-3THz, and to facilitate processing.

[0008] The technical ideas for achieving the purpose of the present invention are: to achieve reconfigurable absorption band by converting the dielectric and metal states of the vanadium dioxide resonance unit through external temperature control; to tune the absorption frequency by controlling the Fermi level of graphene; and to avoid the existence of micro-unit structure by adopting all-dielectric materials, which is easier to process.

[0009] According to the above ideas, the multi-frequency reconfigurable absorber based on water-graphene-VO2 stack of the present invention includes a water-based polytetrafluoroethylene layer, a graphene layer, a silicon layer and a metal layer, and is characterized by:

[0010] The silicon layer is provided as two layers, namely, a first silicon layer and a second silicon layer, so as to increase the thickness of the medium and realize multi-band absorption;

[0011] The water-based polytetrafluoroethylene layer is a hollow cube, the interior of which is completely filled with a water layer to enhance the absorption loss of incident electromagnetic waves and achieve an absorption rate of more than 99%;

[0012] The layers are arranged from top to bottom in the order of a water-based polytetrafluoroethylene layer, a graphene layer, a first silicon layer, a vanadium dioxide layer, a second silicon layer, and a metal layer, and the layers are tightly and seamlessly attached to each other to form an integrated structure.

[0013] Preferably, the water-based polytetrafluoroethylene layer adopts a hollow cube with a width range of 0.001μm to 0.7μm on both sides, a bottom thickness range of 0.001μm to 0.1μm, a top thickness range of 0.001μm to 0.3μm, and an overall thickness range of 7.4μm to 10.4μm to completely encapsulate the water layer.

[0014] Preferably, the graphene layer is a thin cube patch with a thickness d of 0.1 μm to 10 μm, the relaxation time of which is set to 0.1 ps, and the Fermi level μ c The variation in the range of 0.1eV to 1eV is selected to achieve tuning of multiple bands of absorbing frequencies in a small range.

[0015] Preferably, the first silicon layer and the second silicon layer both have a thickness of h s It is a solid cube of 50μm to 300μm to achieve absorption of incident electromagnetic waves.

[0016] Preferably, the vanadium dioxide layer has a thickness of h v It is a solid cube with a diameter of 1.5μm to 3.5μm to achieve reconstruction of the absorbing frequency band, that is, when the temperature is below 68°C, it is in an insulating state, and the absorbing body can achieve eight absorbing bands with an absorption rate of more than 99%; when the temperature is above 68°C, it is in a metallic state, and the absorbing body can achieve four absorbing bands with an absorption rate of more than 99%.

[0017] Preferably, the metal layer is made of gold, silver or copper, and its thickness h is 2 μm to 5 μm.

[0018] Preferably, the thickness of the water layer is w It is 7μm~10μm.

[0019] Compared with the prior art, the present invention has the following advantages:

[0020] 1. Since the present invention divides the traditional single dielectric silicon layer into two parts, the thickness of each silicon dielectric can be flexibly controlled while more conveniently adjusting the number of multiple absorption bands at different temperatures;

[0021] 2. In the present invention, since the water-based polytetrafluoroethylene layer is set as a hollow cube and the interior of the cavity is completely filled with a water layer, the high dielectric constant and large broadband loss characteristics of water in the terahertz frequency band can be used to increase the absorption loss of the incident electromagnetic wave, thereby achieving absorption in multiple bands;

[0022] 3. The present invention reduces the Fermi level μ of the graphene layer to c By changing in the range of 0.1eV to 1eV, the absorption frequency and absorption rate of multiple bands can be tuned.

[0023] 4. In the present invention, since the vanadium dioxide layer is laminated between the first silicon layer and the second silicon layer, the temperature control property of vanadium dioxide itself can be utilized to make the absorber generate absorption peaks of different numbers and different absorption bands at different temperatures.

[0024] 5. Since the present invention adopts all-dielectric materials, it has a simple structure and is easy to process. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a schematic diagram of the overall structure of the present invention;

[0026] Figure 2 A 3×3 array diagram formed by periodic arrangement of the present invention;

[0027] Figure 3 The absorption curves of the present invention simulated in TE and TM modes at temperatures of 50°C and 70°C respectively;

[0028] Figure 4 It is the absorption diagram of the present invention corresponding to the TE and TM modes with the incident angle changed at 50°C.

[0029] Figure 5 It is the absorption diagram of the present invention corresponding to the TE and TM modes with the incident angle changed at 70°C.

[0030] Figure 6 The absorption curve of graphene Fermi level adjusted at 50°C.

[0031] Figure 7 The absorption curve of graphene Fermi level adjusted at 70℃.

[0032] Figure 8 The absorption curve of the present invention in the frequency range of 0-6THz is simulated at 50°C.

[0033] Fig. 9 To set the thickness of the two silicon layers to be 110 μm, the absorption curve of the present invention within the frequency range of 0-3 THz was simulated at 50° C. DETAILED DESCRIPTION

[0034] The embodiments and effects of the present invention are further described in detail below in conjunction with the accompanying drawings. This example includes but is not limited to the following embodiments.

[0035] Refer to Figure 1 , this example includes a water-based polytetrafluoroethylene layer, a water layer, a graphene layer, a silicon layer, a vanadium dioxide layer and a metal layer. Wherein:

[0036] The water-based polytetrafluoroethylene layer 1 is a hollow cube, the width of both sides of the water-based polytetrafluoroethylene layer 1 is in the range of 0.001 μm to 0.7 μm, the thickness of the bottom is in the range of 0.001 μm to 0.1 μm, the thickness of the top is in the range of 0.001 μm to 0.3 μm, and the overall thickness is in the range of 7.4 μm to 10.4 μm. The internal cavity is completely filled with water, forming a thickness of h w The water layer 2 is 7 μm to 10 μm.

[0037] The graphene layer 3 has a thickness d of 0.1 μm to 10 μm, a relaxation time of 0.1 ps, and a Fermi level μ c The variation range is 0.1eV~1eV, which is used to produce plasma resonance effect and confine the incident electromagnetic waves.

[0038] The silicon layer is divided into two parts, namely, a first silicon layer 4 and a second silicon layer 6, wherein the thickness of the first silicon layer 4 is h s1 is 50 μm to 300 μm, and the thickness of the second silicon layer 6 is h s2 It is 50μm~300μm, the thickness of the two silicon layers is the same or different, and according to the relationship between the absorption peak interval and the medium thickness in the Fabry-Perot resonance Δf=c / (2ndcosξ), the overall thickness parameters of the two silicon layers determine the value of the absorption frequency point, and at the same time, within a fixed frequency range, it also determines the number of absorption frequency bands, where c is the speed of light, n is the refractive index of the medium, d is the thickness of the medium, and ξ is the incident angle of the electromagnetic wave.

[0039] The vanadium dioxide layer 5 is loaded between the first silicon layer 4 and the second silicon layer 6, and its thickness is h v The thickness of the vanadium dioxide layer is 1.5 μm to 3.5 μm, and the vanadium dioxide layer presents different states as the temperature changes, that is, it is in an insulating state when the temperature is lower than 68°C, and it is in a metallic state when the temperature is higher than 68°C.

[0040] The metal layer 7 is made of gold, silver or copper metal material, and has a thickness h of 2 μm to 5 μm.

[0041] The water-based polytetrafluoroethylene layer 1, graphene layer 3, first silicon layer 4, vanadium dioxide layer 5, second silicon layer 6 and metal layer 7 are all cubes with a side length p of 20 μm to 500 μm, forming a tightly seamless overall structure composed of the water-based polytetrafluoroethylene layer 1, graphene layer 3, first silicon layer 4, vanadium dioxide layer 5, second silicon layer 6 and metal layer 7 arranged in the order from top to bottom.

[0042] Example 1:

[0043] In this example, but not limited to, the width of the water-based polytetrafluoroethylene layer 1 on both sides is 0.7 μm, the bottom thickness is 0.1 μm, the top thickness is 0.3 μm, and the overall thickness is 7.4 μm. The thickness of the water layer 2 is 7 μm, the length and width of the water layer 2 are both 38 μm, the thickness of the graphene layer 3 is 0.1 μm, the thickness of the first silicon layer 4 and the second silicon layer 6 are both 55 μm, the thickness of the vanadium dioxide layer 5 is 3 μm, the thickness of the metal layer 7 is 2 μm, and the side lengths of the water-based polytetrafluoroethylene layer 1, the graphene layer 3, the first silicon layer 4, the vanadium dioxide layer 5, the second silicon layer 6 and the metal layer 7 are set to 40 μm. The dielectric constants of silicon, vanadium dioxide, graphene and metal in the terahertz frequency band are all given by the Drude model, the dielectric constant of water is given by the Debye model, and the electromagnetic wave is incident in the vertical direction. According to the above structural relationship, a multi-frequency reconfigurable absorber is formed.

[0044] Example 2: In this example, the thickness of the two silicon layers is set to 110 μm, and the other structural parameters are the same as those of Example 1. A multi-frequency reconfigurable absorber is constructed according to the above structural relationship.

[0045] Example 3:

[0046] In order to cover a larger absorbing space, the above-mentioned Example 1 or Example 2 can be arranged into an m×n matrix absorber, such as Figure 2 The length and width of the matrix absorber can be freely selected according to the actual application, and the number of absorbers of the present invention can be freely selected. Figure 2 A 3×3 matrix absorber was demonstrated.

[0047] The wave absorbing effect of the present invention is further illustrated by the following specific embodiments.

[0048] 1. Simulation conditions

[0049] The commercial simulation software CST Microwave Studio was used to perform data simulation on the present invention.

[0050] The object of simulation is this instance.

[0051] 2. Simulation content

[0052] Simulation 1, setting the frequency range to 0-3THz, for Example 1, setting the graphene Fermi level to 0.2eV at 50°C and setting the graphene Fermi level to 0.1eV at 70°C, the absorption curves of the TE and TM modes are simulated respectively. The results are as follows: Figure 3 Among them, the dark blue line represents the absorption curve of the absorber at 50°C and TE polarization, the triangle symbol represents the absorption curve of the absorber at 50°C and TM polarization, the light blue line represents the absorption curve of the absorber at 70°C and TE polarization, and the quadrilateral symbol represents the absorption curve of the absorber at 70°C and TM polarization.

[0053] from Figure 3 It can be seen that at 50°C, vanadium dioxide is in an insulating state, and the absorber has 8 absorption frequency points in the frequency band of 0-3THz, all of which are higher than 99%; at 70°C, vanadium dioxide is metallic, and the absorber has 4 absorption frequency points in the frequency band of 0-3THz, all of which are higher than 99%. This means that the present invention can realize the reconfiguration of the absorption frequency band under external temperature control conditions, and has polarization insensitivity to the incident electromagnetic wave.

[0054] Simulation 2, setting the frequency range to 0-3THz, and setting the graphene Fermi level to 0.2eV at 50°C for Example 1, simulate the absorption curves of adjusting the incident angle of electromagnetic waves in different TE and TM modes. The results are as follows: Figure 4 As shown, Figure 4 (a) is the absorption curve of Example 1 when adjusting the incident angle of electromagnetic wave at 50°C and TE polarization. Figure 4(b) is the absorption curve diagram of Example 1 when adjusting the incident angle of the electromagnetic wave at 50°C and TM polarization.

[0055] from Figure 4 It can be seen that the present invention can have an absorption rate of more than 90% for electromagnetic waves under TE polarization when the incident angle of the electromagnetic wave is between 0-50°, and an absorption rate of more than 80% for electromagnetic waves under TM polarization when the incident angle of the electromagnetic wave is between 0-70°.

[0056] Simulation 3, setting the simulation frequency range to 0-3THz, and setting the graphene Fermi level to 0.1eV at 70℃ for Example 1, simulate the absorption curves of adjusting the incident angle of electromagnetic waves in different TE and TM modes. The results are as follows: Figure 5 As shown, Figure 5 (a) is the absorption curve of Example 1 when adjusting the incident angle of electromagnetic wave at 70°C and TE polarization. Figure 5 (b) is the absorption curve diagram of Example 1 when adjusting the incident angle of electromagnetic waves at 70°C and TM polarization.

[0057] from Figure 5 It can be seen that the present invention can have an absorption rate of more than 80% for electromagnetic waves under TE polarization and TM polarization when the incident angle of the electromagnetic wave is between 0-60°.

[0058] Simulation 4, setting the frequency range to 0-3THz, simulates the absorption curve of graphene Fermi level at 50℃ in Example 1. The results are as follows: Figure 6 shown.

[0059] from Figure 6 It can be seen that adjusting the Fermi level of graphene will cause multiple absorption frequency points in this example to move, and the absorption rate of each absorption frequency point will also change, indicating that the present invention can achieve tuning of absorption frequencies and absorption rates in multiple bands by changing the Fermi level of graphene.

[0060] Simulation 5, setting the frequency range to 0-3THz, simulates the absorption curve of graphene Fermi level at 70℃ in Example 1. The results are as follows Figure 7 shown.

[0061] from Figure 7 It can be seen that adjusting the Fermi level of graphene will cause multiple absorption frequency points in this example to move, and the absorption rate of each absorption frequency point will also change, indicating that the present invention can achieve tuning of absorption frequencies and absorption rates in multiple bands by changing the Fermi level of graphene.

[0062] Simulation 6, setting the simulation frequency range to 0-6THz, simulates the absorption curve of Example 1 when the graphene Fermi level is set to 0.2eV at 50℃. The results are as follows Figure 8 shown.

[0063] from Figure 8 It can be seen that the present invention has sixteen absorption peaks in the frequency range of 0-6 THz, indicating that the frequency range applicable to the present invention includes but is not limited to the frequency range of 0-3 THz.

[0064] Simulation 7, set the simulation frequency range to 0-3THz, and simulate the absorption curve of Example 2 at 50℃. The results are as follows Fig. 9 shown.

[0065] from Fig. 9 It can be seen that the present invention has fifteen absorption peaks in the 0-3THz frequency range, indicating that the present invention can theoretically achieve the absorption of a corresponding number of absorption peaks in the 0-3THz frequency range by flexibly adjusting the thickness parameters of the first silicon layer and the second silicon layer.

[0066] The above descriptions are only several preferred embodiments of the present invention and do not constitute a limitation to the present invention. A person skilled in the art may make several modifications and improvements without departing from the innovative concept of the present invention, but these changes shall all fall within the scope of protection of the present invention.

Claims

1. A multi-frequency reconfigurable absorber based on a water-graphene-VO2 stack, comprising a water-based polytetrafluoroethylene layer, a graphene layer, a silicon layer and a metal layer, characterized in that: The silicon layer is provided as two layers, namely a first silicon layer (4) and a second silicon layer (6), so as to increase the thickness of the medium and realize absorption of multiple frequency bands; The water-based polytetrafluoroethylene layer (1) is a hollow cube, the interior of which is completely filled with a water layer (2) to enhance the absorption loss of incident electromagnetic waves and achieve an absorption rate of more than 99%; The layers are arranged from top to bottom in the order of a water-based polytetrafluoroethylene layer (1), a graphene layer (3), a first silicon layer (4), a vanadium dioxide layer (5), a second silicon layer (6), and a metal layer (7), and the layers are tightly and seamlessly attached to each other to form an integrated structure.

2. The absorber according to claim 1, characterized in that: The water-based polytetrafluoroethylene layer (1) is a hollow cube with widths of both sides ranging from 0.001 μm to 0.7 μm, a bottom thickness ranging from 0.001 μm to 0.1 μm, a top thickness ranging from 0.001 μm to 0.3 μm, and an overall thickness ranging from 7.4 μm to 10.4 μm, so as to completely encapsulate the water layer (2).

3. The wave absorbing body according to claim 1, characterized in that: The graphene layer (3) is a thin cubic patch with a thickness d of 0.1 μm to 10 μm, and its relaxation time is set to 0.1 ps, and the Fermi level μ c The variation in the range of 0.1eV to 1eV is selected to achieve tuning of multiple bands of absorbing frequencies in a small range.

4. The absorber according to claim 1, characterized in that: The first silicon layer (4) and the second silicon layer (6) both have a thickness of h s It is a solid cube of 50μm to 300μm to achieve absorption of incident electromagnetic waves.

5. The absorber according to claim 1, characterized in that: The vanadium dioxide layer (5) has a thickness of h v It is a solid cube with a diameter of 1.5μm to 3.5μm to achieve reconstruction of the absorbing frequency band, that is, when the temperature is below 68°C, it is in an insulating state, and the absorber can achieve eight absorption bands with an absorption rate of more than 99%; when the temperature is above 68°C, it is in a metallic state, and the absorber can achieve four absorption bands with an absorption rate of more than 99%.

6. The absorber according to claim 1, characterized in that: The metal layer (7) is made of gold, silver or copper, and its thickness h is 2 μm to 5 μm.

7. The absorber according to claim 1, characterized in that: The thickness h of the water layer (2) w It is 7μm~10μm.