Method for producing powder solid composite, and powder solid composite
By blending non-volatile liquid oily components and powdered waxes into powdered cosmetics and treating them at specific temperatures, the problems of reduced impact resistance and user experience were solved, achieving high impact resistance and excellent user experience.
Patent Information
- Application Number
- CN202080085945.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-12-25
- Filing Date
- 2020-12-14
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-12-14
AI Technical Summary
In existing powdered cosmetics, increasing the amount of gloss-enhancing materials or increasing the particle size can reduce impact resistance, and molten wax may hinder solvent evaporation, leading to reduced usability.
A powdered solid composite was prepared by using a non-volatile liquid oily component as a base agent, mixing it with powdered wax, evaporating the solvent at a temperature where the wax does not melt, and then heating the base agent at the melting temperature of the wax.
It improves the impact resistance and usability of powder solids compounds, such as moisturizing, glossy, soft and pearlescent feel, while avoiding the hindrance of solvent evaporation.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure HDA0003687606240000011
Abstract
Description
Technical Field
[0001] The present invention relates to a method for producing a powder solid composite and a powder solid composite. Background Art
[0002] Powdered cosmetics such as foundation and eye shadow are mixed with oily components to give a feeling of use such as moisturizing and glossiness. In addition, conventional powdered cosmetics are mixed with wax to give impact resistance (for example, see Patent Document 1). In addition, conventional powdered cosmetics are mixed with ingredients such as glossing materials to give additional properties such as pearlescent feeling during use (for example, see Patent Document 2).
[0003] Prior art literature
[0004] Patent Literature
[0005] Patent Document 1: Japanese Patent Application Publication No. 2005-220053
[0006] Patent Document 2: Japanese Patent Application Publication No. 2002-275033 Summary of the invention
[0007] Problems to be solved by the invention
[0008] Conventional powdered cosmetics have a reduced impact resistance if the amount of ingredients such as glossing materials is increased or the particle size of the ingredients is increased, thus limiting the ability to add additional properties such as pearlescent effects. In addition, although the reduction in impact resistance can be suppressed to some extent by melting wax during the production of powdered cosmetics, the film of the melted wax may hinder the volatilization of the solvent, and the usability of the resulting powdered cosmetic may be reduced.
[0009] An object of the present invention is to provide a method for producing a powdered solid composite material capable of improving additional properties without deteriorating the feeling of use.
[0010] Means for solving problems
[0011] A method for producing a powdered solid composite according to one embodiment of the present invention comprises a base into which a non-volatile liquid oil component is mixed, the method comprising the following steps: a step of mixing a powdered wax into the base, a step of dispersing the base in a solvent, a step of volatilizing the solvent at a first temperature at which the wax does not melt, and a step of heating the base at a second temperature at which the wax melts, wherein the mixing amount of the non-volatile liquid oil component is greater than 15% by mass and less than 40% by mass relative to the base.
[0012] Effects of the Invention
[0013] According to one aspect of the present invention, a method for producing a powdered solid composite material capable of improving additional properties without deteriorating the feeling of use can be provided. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 This is a flow chart of a method for producing a powdered solid composite according to an embodiment of the present invention.
[0015] Figure 2 This is a process diagram of a method for producing a powder solid composite (mixing method) according to the present embodiment.
[0016] Figure 3 It is a process diagram of the method for producing the powder solid composite (molding method) according to the present embodiment. DETAILED DESCRIPTION
[0017] Regarding the embodiments of the present invention, Figure 1 It should be noted that the same reference numerals are used for the common parts in the drawings and the description thereof may be omitted.
[0018] <Method for producing powdered solid composite>
[0019] Figure 1 It is a flow chart of a method for producing a powdered solid composite according to an embodiment of the present invention. Figure 2 , Figure 3 It is a process diagram of the method for producing the powder solid composite material according to the present embodiment.
[0020] The method for producing a powder solid compound according to the present embodiment is a method for producing a powder solid compound containing a base into which a non-volatile liquid oily component is mixed. In this specification, a powder solid compound refers to a solid object made by molding a compound containing a powder or a powder. In addition, the base contains a powder or a powder as a main component. Furthermore, the liquid oily component refers to a liquid oil component or grease. In addition, non-volatility refers to a situation where the kinematic viscosity is 5 cSt (centistokes) or more.
[0021] The method for producing a powdered solid composite according to the present embodiment includes the step of mixing a powdered wax with a base mixed with a non-volatile liquid oil component (see Figure 1 Specifically, powder B, wax W, non-volatile liquid oil component L, glossy powder G, and non-volatile silicone oil O are added to the Henschel mixer 10 and kneaded (refer to Figure 2 ).
[0022] The structure of the Henschel mixer 10 is arbitrary, and for example, it includes a mixing tank 11, a main body 12 with a built-in motor, a rotating shaft 13, and a blade 14 (see Figure 2). It should be noted that the scheme of mixing the powder B, wax W, etc. is not limited to this.
[0023] The components of the powder are not particularly limited, and examples thereof include talc, kaolin, mica, sericite, muscovite, phlogopite, synthetic mica, red mica, biotite, vermiculite, magnesium carbonate, calcium carbonate, aluminum silicate, barium silicate, calcium silicate, magnesium silicate, strontium silicate, metal tungstate, magnesium, silicon dioxide, zeolite, barium sulfate, calcined calcium sulfate (gypsum), calcium phosphate, fluoroapatite, hydroxyapatite, ceramic powder, silicone powder, magnesium myristate (magnesium myristate), zinc myristate, calcium palmitate, aluminum stearate, chlorophenol ether, boron nitride, etc. The components of these powders may be used alone or in combination of two or more.
[0024] In the method for manufacturing a powder-solid composite involved in this embodiment, although the mixing amount of the powder is arbitrary, it is preferably greater than 10 mass % and less than 70 mass % relative to 100 mass % of the powder-solid composite, more preferably greater than 15 mass % and less than 65 mass %, and further preferably greater than 20 mass % and less than 60 mass %.
[0025] The wax W in the Henschel mixer 10 is kneaded in a pulverized state. The pulverized wax is an example of a powdered wax in the method for producing a powdered solid composite of the present invention. The wax is not particularly limited, but is preferably a wax having a melting point of 55°C to 90°C, more preferably a wax having a melting point of 60°C to 85°C, and further preferably a wax having a melting point of 65°C to 80°C.
[0026] The components of the wax are not particularly limited, and examples thereof include beeswax, candelilla wax, cotton wax, carnauba wax, bayberry wax, insect wax, spermaceti wax, montan wax, bran wax (rice bran wax), kapok wax, lacquer wax, acetylated lanolin, liquid lanolin, sugarcane wax, lanolin fatty acid isopropyl ester, hexyl laurate, reduced lanolin, jojoba ester (hydrogenated jojoba oil), hard lanolin, shellac wax, yellow wax, microcrystalline wax, paraffin, POE lanolin alcohol ether, POE lanolin alcohol acetate, POE cholesterol ether, lanolin fatty acid polyethylene glycol, fatty acid glyceride, hardened castor oil, POE hydrogenated lanolin alcohol ether, sucrose fatty acid ester (sucrose triacetate tetrastearate), etc. The components of these waxes can be used alone or in combination of two or more.
[0027] The blending amount of the wax is arbitrary, but can be set to 0.5 mass % to 10 mass % relative to the base, preferably 1 mass % to 6.5 mass %, more preferably 1.5 mass % to 6 mass %, further preferably 2 mass % to 5.5 mass %.
[0028] The components of the nonvolatile liquid oil component are not particularly limited, and examples thereof include liquid paraffin, ozokerite, squalene, batylene, ceresin, petrolatum, tri(2-ethylhexanoin)glyceryl, isopropyl myristate, cetyl octanoate, octyldodecyl myristate, isopropyl palmitate, butyl stearate, hexyl laurate, myristyl myristate, decyl oleate, hexyldecyl dimethyl octanoate, lactic acid, Cetyl alcohol esters, myristyl lactate, acetylated lanolin, isocetyl stearate, isocetyl isostearate, 12-hydroxystearate cholesterol ester, ethylene glycol di(2-ethylhexanoate), dipentaerythritol fatty acid esters, n-alkyl glycol monoisostearate, neopentyl glycol dicaprate, diisostearyl malate, glyceryl di(2-heptyl undecanoate), trimethylolpropane tri(2-ethylhexanoate), trimethylolpropane triisostearate, tetra(2-ethylhexanoate pentane)erythritol ester, glyceryl tri(2-ethylhexanoate), trimethylolpropane triisostearate, cetyl alcohol 2-ethylhexanoate, 2-ethylhexyl palmitate, glyceryl trimyristate, glyceryl tri(2-heptyl undecanoate), castor oil fatty acid methyl ester, oleyl oleate, acetylglycerol, 2-heptyl undecyl palmitate, diisobutyl adipate, 2-Octyldodecyl N-lauroyl-L-glutamate, Di-(2-heptylundecyl) adipate, Ethyl laurate, Di(2-ethylhexyl) sebacate, 2-hexyldecyl myristate, 2-hexyldecyl palmitate, 2-hexyldecyl adipate, Diisopropyl sebacate, 2-ethylhexyl succinate, Ethyl acetate, Butyl acetate, Amyl acetate, Triethyl citrate, Cromiton (C 13 H 17 NO), etc. These liquid oil components may be used alone or in combination of two or more.
[0029] The amount of the nonvolatile liquid oil component blended is arbitrary, but is preferably 15% by mass to 40% by mass, more preferably 20% by mass to 38% by mass, and even more preferably 25% by mass to 35% by mass, relative to the base.
[0030] The glossy powder can be mixed arbitrarily. In this embodiment, the glossy powder G in the Henschel mixer 10 is kneaded in a pulverized state together with the powder B and the wax W. The pulverized glossy powder G is an example of the glossy powder in the method for producing a powder-solid composite of the present invention.
[0031] The average particle size of the glossy powder is arbitrary, but is preferably 30 μm or more, more preferably 35 μm or more, and further preferably 40 μm or more. The average particle size is a particle size corresponding to 50% of the cumulative distribution based on volume measured by laser diffraction / scattering method.
[0032] It should be noted that the upper limit of the average particle size of the glossy powder is not particularly limited, but from the viewpoint of maintaining the impact resistance of the powder-solid composite, the average particle size of the glossy powder is preferably 200 μm or less, more preferably 150 μm or less, and further preferably 100 μm or less.
[0033] The components of the glossy powder are not particularly limited, and examples thereof include titanium oxide-coated mica, titanium oxide-coated synthetic mica, titanium oxide-coated silica, titanium oxide-coated talc, zinc oxide-coated silica, titanium oxide-coated colored mica, red iron-coated mica titanium, red iron oxide / black iron oxide-coated mica titanium, carmine-coated mica titanium, Prussian blue-coated mica titanium, etc. These glossy powder components may be used alone or in combination of two or more.
[0034] The blending amount of the glossy powder is arbitrary, but is preferably 10% by mass to 60% by mass, more preferably 15% by mass to 55% by mass, and further preferably 20% by mass to 50% by mass, relative to the base.
[0035] The non-volatile silicone oil can be mixed arbitrarily. Here, the non-volatile silicone oil refers to silicone oil with a kinematic viscosity of 5 cSt (centistokes) or more. The components of the non-volatile silicone oil are not particularly limited, and examples thereof include dimethyl polysiloxane (dimethyl silicone oil), methylphenyl polysiloxane, methyl hydrogen polysiloxane, etc. These silicone oil components can be used alone or in combination of two or more.
[0036] In the method for producing a powder solid composite according to the present embodiment, the mixing amount of the non-volatile silicone oil is arbitrary, and is preferably 10% to 30% by mass, more preferably 13% to 28% by mass, and further preferably 15% to 25% by mass, relative to the base.
[0037] The method for producing a powdered solid composite according to the present embodiment includes the step of dispersing a base in a solvent (see Figure 1 Here, dispersing the base in the solvent means preparing the powder solid composite in a wet process. Specifically, the solvent S is further added to the Henschel mixer 10 and stirred (refer to Figure 2 ).
[0038] The components of the solvent are not particularly limited, and examples thereof include water, ethanol, propanol, isopropanol, isobutanol, tert-butanol, etc. These solvent components may be used alone or in combination of two or more.
[0039] The amount of the solvent mixed is arbitrary, and is preferably 3 mass % to 50 mass % relative to 100 mass % of the base (the total amount obtained by mixing wax, glossy powder, etc. into the base), more preferably 5 mass % to 40 mass %, and further preferably 10 mass % to 30 mass %.
[0040] In the method for producing a powdered solid composite of the present embodiment, colorants, antioxidants, preservatives, and the like other than the above-mentioned components may be blended within a range that does not impair the effects of the present invention.
[0041] Examples of colorants include red iron oxide, yellow iron oxide, black iron oxide, inorganic white pigments (e.g., zinc oxide, etc.); inorganic red pigments (e.g., iron titanate, etc.); inorganic purple pigments (e.g., manganese violet, cobalt violet, etc.); inorganic green pigments (e.g., chromium oxide, chromium hydroxide, cobalt titanate, etc.); inorganic blue pigments (e.g., ultramarine, Prussian blue, etc.); metal powder pigments (e.g., aluminum powder, copper powder, etc.); organic pigments such as zirconium, barium or aluminum lakes (e.g., Red 201, Red 202, Red 204, Red 205, Organic pigments such as Red 220, Red 226, Red 228, Red 405, Orange 203, Orange 204, Yellow 205, Yellow 401, Blue 404, Red 3, Red 104, Red 106, Red 227, Red 230, Red 401, Red 505, Orange 205, Yellow 4, Yellow 5, Yellow 202, Yellow 203, Green 3, Blue 1, etc.); natural pigments (e.g., chlorophyll, β- or carotene, etc.). It should be noted that the mixing amount of the colorant is arbitrary.
[0042] Examples of the antioxidant include ascorbic acid, α-tocopherol, dibutylhydroxytoluene, and butylhydroxyanisole.
[0043] The amount of the antioxidant compounded is arbitrary, but is preferably 0.005% by mass to 0.2% by mass, more preferably 0.05% by mass to 0.1% by mass, and even more preferably 0.015% by mass to 0.05% by mass, relative to the base.
[0044] Examples of the preservative include parabens, phenoxyethanol, ethylhexyl glycerol, benzoic acid, salicylic acid, phenol, sorbic acid, p-chloro-m-cresol, hexachlorophene, benzalkonium chloride, chlorhexidine hydrochloride, and trichlorocarbamide.
[0045] The amount of the preservative compounded is arbitrary, but is preferably 0.05% by mass to 0.5% by mass, more preferably 0.1% by mass to 0.4% by mass, and even more preferably 0.15% by mass to 0.3% by mass, based on the base.
[0046] The powder B, wax W, glossy powder G, nonvolatile liquid oil component L, nonvolatile silicone oil O, and solvent S in the Henschel mixer 10 are stirred to form a paste-like slurry P (see Figure 2 Then, the slurry P in the Henschel mixer 10 is poured into the molding die 20 (see Figure 2 At this time, it is preferred that the slurry P is filled into the molding die 20 while being filtered.
[0047] The method for producing a powdered solid composite according to the present embodiment includes a step of volatilizing a solvent at a first temperature at which the wax is not melted (see Figure 1 Step S3). The first temperature is arbitrary, but is preferably a temperature lower than the melting point of the wax (a temperature at which the wax does not melt). In addition, volatilizing the solvent means gasifying the liquid solvent.
[0048] In this step, the slurry P filled in the molding die 20 is heated at a temperature lower than the melting point of the wax (about 50° C.) (see Figure 3 ). It should be noted that the method for heating the slurry P is arbitrary, for example, the forming mold 20 filled with the slurry P can be placed in a thermostatic bath with a degassing device for heating. In addition, the heating time of the slurry P is arbitrary, for example, about 3 minutes to 3 hours.
[0049] Thus, the solvent S in the slurry P is volatilized and removed and degassed from the slurry P as a volatile solvent V. On the other hand, the wax W in the slurry P remains in the slurry P in a powdery state without being melted.
[0050] The method for producing a powdered solid composite according to the present embodiment includes the step of heating the base at a second temperature at which the wax melts (see Figure 1 The second temperature is arbitrary, but is preferably a temperature above the melting point of the wax (temperature at which the wax melts). In addition, heating the base means applying heat to the base to dry it.
[0051] Specifically, the second temperature is preferably 55°C to 90°C, more preferably 60°C to 85°C, and even more preferably 65°C to 80°C.
[0052] In this step, the slurry P filled in the molding die 20 is dried at a temperature higher than the melting point of the wax (about 70° C.) (see Figure 3 ). It should be noted that the method of heating the base is arbitrary, for example, the molding die 20 filled with the slurry P is placed in the above-mentioned constant temperature bath, and the temperature in the constant temperature bath is increased to dry. In addition, the heating time of the base is arbitrary, for example, about 3 minutes to 3 hours.
[0053] Thus, the slurry P is dried in a state where the solvent S is removed, and the powdered wax W is melted in the slurry P. Then, when the dried base is cooled to room temperature, a solid material is obtained.
[0054] The method for producing a powder-solid composite according to the present embodiment is suitably used in the production of solid powder cosmetics such as foundation, eye shadow, blush, talcum powder, scented talcum powder, baby powder, concealer foundation, deodorant powder, and perfume powder.
[0055] In this embodiment, as described above, a powdered wax is mixed into a base mixed with a nonvolatile liquid oil component, and the solvent in which the base is dispersed is volatilized at a first temperature at which the wax does not melt, thereby maintaining the powdered state of the wax mixed into the base while the solvent is volatilized. Therefore, the wax mixed into the base does not hinder the volatilization of the solvent.
[0056] In addition, by heating the base after mixing the wax at the second temperature at which the wax melts, the powdered wax can be melted in a state where the solvent is removed. The powdered solid composite obtained by solidifying the melted wax at room temperature becomes a material with high impact resistance. Therefore, even if the base contains components such as glossy powder, it is possible to prevent the impact resistance of the powdered solid composite from being reduced.
[0057] In addition, by melting the powdered wax after the solvent is removed, the residual solvent in the powdered solid composite can be suppressed, and the use feeling (e.g., moist feeling, glossy feeling, soft feeling, powder removal, etc.) of the obtained powdered solid composite can be improved. In this way, according to this embodiment, the additional characteristics of the powdered solid composite can be improved without reducing the use feeling.
[0058] Furthermore, by setting the blending amount of the nonvolatile liquid oil component to 15% by mass or more and 40% by mass or less relative to the base, the feel of the obtained powder solid composite can be improved. Therefore, according to this embodiment, a powder solid composite with excellent feel can be obtained.
[0059] In addition, in this embodiment, as described above, by setting the first temperature to a temperature lower than the melting point of the wax, the first temperature for volatilizing the solvent can be set to a temperature at which the wax does not melt. Thus, the powdery state of the wax mixed in the base can be maintained when the solvent volatilizes, and the wax can be prevented from becoming an obstacle to the volatilization of the solvent.
[0060] In addition, in this embodiment, as described above, by setting the second temperature to a temperature higher than the melting point of the wax, the second temperature at which the base is heated can be set to a temperature at which the wax melts. Thus, the powdered wax can be melted in a state where the solvent has been removed, and the impact resistance of the obtained powdered solid composite can be prevented from being reduced, thereby improving the feel of the powdered solid composite during use.
[0061] In this embodiment, as described above, by setting the second temperature to 55° C. to 90° C., the temperature range of the second temperature for melting the wax does not overlap with the temperature range of the first temperature for volatilizing the solvent without melting the wax, so that the powdered wax can be melted after the solvent is removed.
[0062] In addition, in this embodiment, by setting the second temperature to 55° C. to 90° C., a wax having a melting point of 55° C. to 90° C. can be used as the wax. Waxes having a melting point of 55° C. to 90° C. are all solid at room temperature and easy to handle. In addition, by using a wax having a melting point of 55° C. to 90° C., a wide range of choices of wax types is provided.
[0063] In this embodiment, as described above, by mixing the nonvolatile silicone oil into the nonvolatile liquid oil component, the feel of the obtained powder solid composite can be further improved. Therefore, according to this embodiment, a powder solid composite with a more excellent feel can be obtained.
[0064] As described above, the nonvolatile silicone oil is blended in an amount of 10% to 30% by mass relative to the base, thereby improving the feel of the obtained powder solid composite. Therefore, according to this embodiment, a powder solid composite with a better feel can be obtained.
[0065] In this embodiment, as described above, by using wax having a melting point of 55° C. to 90° C. as the powdered wax, the solvent can be volatilized at the first temperature without melting the wax, and the wax can be melted at the second temperature. Thus, the wax does not hinder the volatilization of the solvent, and the powdered wax can be melted in a state where the solvent is removed.
[0066] In this embodiment, as described above, by setting the blending amount of the wax to 0.5 mass % or more and 10 mass % or less relative to the base, the impact resistance of the obtained powder solid composite can be improved. In addition, by setting the blending amount of the wax to such a range, the feel of use of the obtained powder solid composite can be improved.
[0067] In this embodiment, as described above, since the impact resistance of the powder solid composite can be improved, even if the glossy powder is mixed in the base, the impact resistance of the powder solid composite can be prevented from being reduced. Therefore, in this embodiment, by mixing the glossy powder in the base, the pearlescent feeling can be improved without reducing the use feeling of the obtained powder solid composite.
[0068] In addition, by improving the impact resistance of the powder solid composite, even if the amount of the glossy powder mixed is increased, the impact resistance of the powder solid composite can be prevented from decreasing. Therefore, in this embodiment, by mixing the glossy powder in an amount of 10% by mass to 60% by mass relative to the base, the pearlescent feeling of the obtained powder solid composite can be further improved.
[0069] Furthermore, in this embodiment, as described above, since the impact resistance of the powder solid composite can be improved, even if the particle size of the glossy powder mixed in the base is increased, the impact resistance of the powder solid composite can be prevented from being reduced. Therefore, in this embodiment, by mixing the glossy powder having an average particle size of 30 μm or more, the pearlescent feeling can be improved with high precision without reducing the feel of the obtained powder solid composite.
[0070] <Powdered solid complex>
[0071] The powder solid composite according to the present embodiment contains a nonvolatile liquid oil component blended with nonvolatile silicone oil, a wax having a melting point of 55° C. to 90° C., and a glossy powder having an average particle size of 30 μm or more.
[0072] The content of the nonvolatile liquid oil component is 15% to 40% by mass, preferably 23% to 38% by mass, and more preferably 25% to 35% by mass, based on 100% by mass of the powder-solid composite.
[0073] The content of the nonvolatile silicone oil is arbitrary, and is preferably 10% to 30% by mass, more preferably 13% to 28% by mass, and further preferably 15% to 25% by mass, relative to 100% by mass of the powder solid composite.
[0074] The content of the wax having a melting point of 55° C. to 90° C. is 2% to 10% by mass, preferably 2.5% to 4.5% by mass, and 3% to 4% by mass, based on 100% by mass of the powder solid composite.
[0075] The melting point of the wax is preferably 60° C. to 85° C., and more preferably 65° C. to 80° C. The properties of the wax are not particularly limited, but are preferably in a powdery state.
[0076] The content of the glossy powder having an average particle size of 30 μm or more is 10% to 60% by mass, preferably 15% to 55% by mass, and more preferably 20% to 50% by mass, relative to 100% by mass of the powder-solid composite.
[0077] In addition, the average particle size of the glossy powder is preferably 30 μm or more, more preferably 35 μm or more, and further preferably 40 μm or more. It should be noted that the upper limit of the average particle size of the glossy powder is arbitrary, and from the viewpoint of maintaining the impact resistance of the powder-solid composite, the average particle size of the glossy powder is preferably 200 μm or less, more preferably 150 μm or less, and further preferably 100 μm or less.
[0078] The powder solid compound involved in the present embodiment is obtained by the above-mentioned method for producing the powder solid compound. That is, the powder solid compound involved in the present embodiment can be obtained by performing the following steps, namely, the step of mixing a powdered wax into a base mixed with a non-volatile liquid oil component, the step of dispersing the base in a solvent, the step of volatilizing the solvent at a first temperature at which the wax does not melt, and the step of heating the base at a second temperature at which the wax melts.
[0079] The powder-solid composite material of this embodiment can be suitably used in solid powder cosmetics such as foundation, eye shadow, blush, talcum powder, scented talcum powder, baby powder, concealer foundation, deodorant powder, and perfume powder.
[0080] The powder solid composite obtained in this way has high impact resistance and excellent feel in use. In addition, in this embodiment, as described above, by containing a non-volatile liquid oil component mixed with non-volatile silicone oil, a wax having a melting point of 55°C to 90°C, and a glossy powder having an average particle size of 30 μm or more in amounts within respective prescribed ranges, the feel of the powder solid composite can be maintained while improving the pearlescent feel.
[0081] It should be noted that in the powder solid composite involved in the present embodiment, the powdered wax is not melted in the process of volatilizing the solvent at the first temperature, but the powdered wax is melted in the process of heating the base at the second temperature, and in the obtained powder solid composite, the solvent is removed and the powdery state of the wax disappears. Therefore, before the manufacture of the powder solid composite, the powdered wax is dispersed in the solvent together with the base, the non-volatile liquid oil component, and the glossy powder to obtain the powder solid composite, and it is currently technically difficult to clearly describe and determine the structure or characteristics of the powder solid composite involved in the present embodiment by analyzing the structure or characteristics of the obtained powder solid composite.
[0082] In addition, even if the structure or characteristics of the powdered solid composite material involved in the present embodiment can be analyzed by any method, the operation to determine the structure or characteristics of the powdered solid composite material involved in the present embodiment requires obviously excessive economic expenditure and time, given the nature of patent applications, the need for rapidity, etc. In other words, it is impossible / impractical to clearly record and directly determine the structure or characteristics of the powdered solid composite material involved in the present embodiment.
[0083] Example
[0084] The present invention will be further described below using examples. It should be noted that, in the following, "parts" and "%" are by mass unless otherwise specified. In addition, various tests and evaluations were performed according to the following methods.
[0085] <Test Subject>
[0086] Powder, wax, colorant, gloss powder, non-volatile liquid oil component, and non-volatile silicone oil were added to a Henschel mixer (SK-M, manufactured by Kyoritsu Riko Co., Ltd.) to mix the base (see Figure 1 Step S1, Figure 2 Then, a solvent was added to the Henschel mixer and stirred with a stirrer (manufactured by PRIMIX Co., Ltd., Robomix) to prepare a slurry (wet base) P (see Figure 1 Step S2, Figure 2 The slurry P in the Henschel mixer is poured into a plate-shaped molding die 20 (see Figure 2 The molding die 20 filled with the slurry P was mounted on a thermostatic bath (DF611 manufactured by Yamato Science Co., Ltd.) and heated at about 50° C. (a temperature lower than the melting point of the wax) for about 3 hours (refer to Figure 1 Step S3, Figure 3 Then, the temperature in the thermostatic bath is adjusted to about 70°C (a temperature above the melting point of the wax), and then heated for about 1 hour (drying) (refer to Figure 1 Step S4, Figure 3 The molding die 20 was taken out of the thermostatic chamber and placed in the chamber for about 1 hour. The obtained molding (solid) C was used as a test body (refer to Figure 3 ) It should be noted that the method for manufacturing the test body is not limited to the above conditions and can be appropriately changed according to the manufacturing equipment or manufacturing scale of a factory or the like.
[0087] <Impact Resistance>
[0088] The test piece was dropped from a height of 30 cm onto a metal plate, and the number of times until it broke was counted. For each test piece, an average of 5 or more times with a test number (N) of 3 was evaluated as good.
[0089]
[0090] Two professional panelists applied the test body around the eyes (eyelids) and evaluated the moist feeling according to the following criteria: When the evaluation was 2 or more, the moist feeling was evaluated as good.
[0091] 5: Feel very moisturized
[0092] 4: Feel moisturized
[0093] 3: Feel slightly moisturized
[0094] 2: Feel a little bit moisturized
[0095] 1: Not moisturized at all
[0096] <Gloss>
[0097] Two professional panelists applied the test body around the eyes (eyelids) and evaluated the glossiness according to the following criteria: When the evaluation was 2 or more, the glossiness was evaluated as good.
[0098] 5: Feels very shiny
[0099] 4: Feeling shiny
[0100] 3: Feels slightly glossy
[0101] 2: Feel a little bit glossy
[0102] 1: No glossiness at all
[0103] <Soft feeling>
[0104] Two professional panelists applied the test body around the eyes (eyelids) and evaluated the softness based on the following criteria: When the evaluation was 2 or more, the softness was evaluated as good.
[0105] 5: The answer feels very soft.
[0106] 4: Feel soft
[0107] 3: Slightly soft
[0108] 2: Feel a little soft
[0109] 1: No softness at all
[0110] <Pearle scenece>
[0111] Two professional judges applied the test body around the eyes (eyelids) and evaluated the pearly luster (gloss) according to the following criteria: When the evaluation was 2 or more, the pearly luster was evaluated as good.
[0112] 5: Feels very pearlescent
[0113] 4: Feeling pearly
[0114] 3: Feels slightly pearly
[0115] 2: Feel a little bit of pearly feeling
[0116] 1: There is no pearly feeling at all
[0117] <Powder extraction (powder extraction ease)>
[0118] Two professional panelists applied the test body around the eyes (eyelids) and evaluated the powdering property according to the following criteria: When the evaluation was 2 or more, the powdering property was evaluated as good.
[0119] 5: I feel that the powder-collecting property is very good
[0120] 4: Good powder-collecting property
[0121] 3: I feel that the powder extraction is slightly better
[0122] 2: The powdering property is only slightly better
[0123] 1: I can't feel the powder extraction is good at all
[0124] Examples and comparative examples are described below.
[0125] [Example 1]
[0126] 2.5 parts of talc, 10 parts of synthetic phlogopite, 1 part of zinc oxide, 1 part of magnesium myristate, 4 parts of (vinyl dimethicone / methicone silsesquioxane crosspolymer), and 8 parts of boron nitride were mixed as powders, 2.5 parts of jojoba ester (Floratech, フローラエステル70HG) was mixed as wax, 1 part of red 226 / mica mixture was mixed as a colorant, 20 parts of synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 400, average particle size 37 μm, manufactured by Japan Koken Industry Co., Ltd.) and synthetic phlogopite / titanium oxide mixture (TW INCLEPEARL (registered trademark) 500, average particle size 90 μm) 20 parts as glossy powder, mixed with 2 parts of vaseline, 6 parts of diisostearyl malate, and 2 parts of triethylhexanoin as non-volatile liquid oil components, mixed with 20 parts of dimethyl silicone oil (manufactured by Shin-Etsu Chemical Co., Ltd., KF-96A-6cs) as non-volatile silicone oil, the whole as 100 parts of base, further mixed with 30 parts of 99% ethanol as a solvent, to prepare test bodies and conduct evaluation. The conditions and evaluation of the test bodies are shown in Table 1.
[0127] [Example 2]
[0128] The test body was prepared and evaluated in the same manner as in Example 1 except that the blending amount of synthetic phlogopite as powder was set to 30 parts, the blending amount of synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 400 manufactured by Japan Koken Industry Co., Ltd., average particle size 37 μm) as glossy powder was set to 10 parts, and the blending amount of synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 500 manufactured by Japan Koken Industry Co., Ltd., average particle size 90 μm) was set to 10 parts. The results are shown in Table 1.
[0129] [Example 3]
[0130] The test bodies were prepared and evaluated in the same manner as in Example 1 except that the blending amount of synthetic phlogopite as powder was set to 20 parts, the blending amount of synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 400 manufactured by Japan Koken Industry Co., Ltd., average particle size 37 μm) as glossy powder was set to 15 parts, and the blending amount of synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 500 manufactured by Japan Koken Industry Co., Ltd., average particle size 90 μm) was set to 15 parts. The results are shown in Table 1.
[0131] [Example 4]
[0132] As a powder, the synthetic phlogopite was not mixed, the mixing amount of the synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 400 manufactured by Japan Koken Industry Co., Ltd., with an average particle size of 37 μm) as a glossy powder was set to 25 parts, and the mixing amount of the synthetic phlogopite / titanium oxide mixture (TWINCLEPEARL (registered trademark) 500 manufactured by Japan Koken Industry Co., Ltd., with an average particle size of 90 μm) was set to 25 parts. Test bodies were prepared and evaluated in the same manner as in Example 1. The results are shown in Table 1.
[0133] [Example 5]
[0134] Test pieces were prepared and evaluated in the same manner as in Example 1 except that 2.5 parts of sucrose triacetate tetrastearate (Shugarwax (registered trademark) A-10E manufactured by Dai-ichi Kogyo Seiyaku Co., Ltd.) was blended as the wax instead of jojoba ester.
[0135] [Example 6]
[0136] Test pieces were prepared and evaluated in the same manner as in Example 1 except that 2.5 parts of a mixture of 92.5% paraffin wax and 7.5% microcrystalline wax (Parmic 160, manufactured by Nikko Rika Co., Ltd.) was blended as the wax instead of jojoba ester.
[0137] [Example 7]
[0138] Test pieces were prepared and evaluated in the same manner as in Example 1 except that 2.5 parts of a mixture of 80% polyethylene and 20% microcrystalline wax (PA Wax, manufactured by Nikko Rika Co., Ltd.) was blended as the wax instead of jojoba ester.
[0139] [Example 8]
[0140] The test pieces were prepared and evaluated in the same manner as in Example 1 except that the blending amount of synthetic phlogopite as a powder was 20 parts and the blending amount of dimethyl silicone oil as a nonvolatile silicone oil was 10 parts.
[0141] [Example 9]
[0142] A test piece was prepared and evaluated in the same manner as in Example 1 except that phlogopite was not mixed as a powder and the mixing amount of dimethyl silicone oil as a non-volatile silicone oil was changed to 30 parts. The results are shown in Table 1.
[0143] [Example 10]
[0144] The test pieces were prepared and evaluated in the same manner as in Example 1 except that the blending amount of synthetic phlogopite as a powder was 7.5 parts and the blending amount of jojoba ester as a wax was 5 parts.
[0145] [Example 11]
[0146] The test pieces were prepared and evaluated in the same manner as in Example 10 except that 5 parts of sucrose triacetate tetrastearate was blended as the wax instead of jojoba ester.
[0147] [Example 12]
[0148] The test pieces were prepared and evaluated in the same manner as in Example 10 except that 5 parts of a mixture of 92.5% paraffin wax and 7.5% microcrystalline wax was blended as the wax instead of jojoba ester.
[0149] [Example 13]
[0150] Test pieces were prepared and evaluated in the same manner as in Example 10 except that 5 parts of a mixture of 80% polyethylene and 20% microcrystalline wax (PA Wax, manufactured by Nikko Rika Co., Ltd.) was blended as wax instead of jojoba ester.
[0151] [Comparative Example 1]
[0152] A test piece was prepared and evaluated in the same manner as in Example 1 except that the amount of synthetic phlogopite as a powder was 30 parts and no nonvolatile silicone oil was added (the total amount of nonvolatile liquid oil components was less than 15% by mass).
[0153] [Comparative Example 2]
[0154] The test pieces were prepared and evaluated in the same manner as in Example 1 except that no solvent was added, the base was prepared by dry method, and the heating was not performed at a temperature higher than the melting point of the wax (about 70° C.).
[0155] [Comparative Example 3]
[0156] A test piece was prepared and evaluated in the same manner as in Example 1 except that the amount of synthetic phlogopite as a powder was changed to 12.5 parts, no wax was added, and heating was not performed at a temperature not lower than the melting point of the wax (about 70° C.).
[0157]
[0158]
[0159] It can be seen from Tables 1 and 2 that 15% to 40% by mass of a non-volatile liquid oil component mixed with non-volatile silicone oil, 2% to 5% to 5% by mass of a powdered wax having a melting point of 55°C to 90°C, and 10% to 60% by mass of a glossy powder having an average particle size of 30 μm or more are wet mixed, the solvent is volatilized at about 50°C (a temperature at which the wax does not melt), and the base is heated at about 70°C (a temperature at which the wax melts) to obtain a powder solid composite, and the powder solid composite has good impact resistance, moisturizing feel, gloss, softness, pearly feel, and powder-collecting properties (Examples 1 to 13).
[0160] In contrast, as shown in Table 2, the powder-solid composite obtained by wet mixing with a total nonvolatile liquid oil component content of less than 15% by mass was inferior in moist feeling, gloss, soft feeling and powder-collecting property (Comparative Example 1).
[0161] In addition, as can be seen from Table 2, the powder solid composite which was dry mixed and not heated at a temperature higher than the melting point of the wax had poor impact resistance (Comparative Example 2).
[0162] In addition, as can be seen from Table 2, the impact resistance and powdering performance of the powder-solid composite without wax blending were poor (Comparative Example 3).
[0163] From these results, it can be judged that the method for producing a powder solid composite comprising the following steps: a step of mixing a powdered wax into a base, a step of dispersing the base in a solvent, a step of volatilizing the solvent at a first temperature at which the wax does not melt, and a step of heating the base at a second temperature at which the wax melts, can improve the additional properties without reducing the feel of use of the powder solid composite.
[0164] Although the embodiments of the present invention have been described above, the present invention is not limited to the specific embodiments, and various modifications and changes can be made within the scope of the invention described in the scope of protection.
[0165] This application claims priority based on Japanese Patent Application No. 2019-234724 filed on December 25, 2019, and all contents thereof are incorporated herein.
[0166] Description of the accompanying drawings
[0167] 10 Henschel mixer
[0168] 11 Mixing tank
[0169] 12 Main body (motor)
[0170] 13 Rotation axis
[0171] 14 Blade
[0172] 20 Forming mold
[0173] B powder
[0174] W Wax
[0175] L Non-volatile liquid oily component
[0176] S Solvent
[0177] O Non-volatile silicone oil
[0178] P Slurry
[0179] V Volatile Solvent
[0180] C Molded body (powder solid composite)
Claims
1. A method for producing a powder-solid composite, the powder-solid composite comprising a base mixed with a non-volatile liquid oil component, the method comprising the following steps: a step of mixing a powdered wax having a melting point of 55° C. to 90° C. into the base, The step of dispersing the base in a solvent, a step of volatilizing the solvent at a first temperature at which the wax does not melt, and After the step of volatilizing the solvent, the step of heating the base at a second temperature at which the wax melts, The amount of the nonvolatile liquid oil component blended is 15% by mass or more and 40% by mass or less relative to the base. 2 . The method for producing a powdered solid composite according to claim 1 , wherein the first temperature is a temperature lower than a melting point of the wax. 3 . The method for producing a powdered solid composite according to claim 1 , wherein the second temperature is a temperature equal to or higher than the melting point of the wax. 4 . The method for producing a powdered solid composite according to claim 1 , wherein the second temperature is 55° C. or higher and 90° C. or lower. 5 . The method for producing a powder-solid composite according to claim 1 , wherein the nonvolatile liquid oil component contains a nonvolatile silicone oil. 6 . The method for producing a powdered solid composite according to claim 5 , wherein the amount of the non-volatile silicone oil blended is 10% by mass or more and 30% by mass or less relative to the base. 7 . The method for producing a powdered solid composite according to claim 1 , wherein the amount of the wax blended is 0.5% by mass or more and 10% by mass or less relative to the base.
8. The method for producing a powder-solid composite according to claim 1 or 2, wherein a glossy powder is mixed into the base. 9 . The method for producing a powder-solid composite according to claim 8 , wherein the amount of the glossy powder blended is 10% by mass or more and 60% by mass or less relative to the base. 10 . The method for producing a powder-solid composite according to claim 8 , wherein the average particle size of the glossy powder is 30 μm or more.
11. A powdered solid composite obtained by the production method according to any one of claims 1 to 10.