A dynamically amplified photochromic film

By combining dynamic amplification layer and strong light color change in the film, the Fabry-Perot interference cavity structure using the metal nanoparticle layer and the dielectric film stack filter layer is achieved, and the three-dimensional dynamic effect and color change of the pattern are solved. The shortcomings of pattern display and anti-counterfeiting applications in the prior art have improved the anti-counterfeiting function.

CN114815006BActive Publication Date: 2024-11-19HUIZHOU FORYOU OPTICAL TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110072097.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-01-19
Publication Date
2024-11-19
Estimated Expiration
2041-01-19

AI Technical Summary

Technical Problem

The prior art is difficult to realize the film with variable pattern color under the display of three-dimensional dynamic effects and strong visible light, and its application in the field of anti-counterfeiting is limited.

Method used

A combined structure of dynamic amplification layer and a strong light color change layer is adopted, where the dynamic amplification layer includes a microlens array layer and a substrate layer, and a strong light color change layer includes a dielectric film stack filter layer and a metal nanoparticle layer, and the metal nanoparticle layer is located in the medium On the filter layer of the membrane stack, a Fabry-Perot interference cavity is formed, and the local surface plasmon resonance effect is used to achieve the three-dimensional dynamic effect and color change of the pattern.

Benefits of technology

It realizes optical responses of two different colors under ambient light and under strong visible light irradiation, improves the anti-counterfeiting function of the pattern, increases the difficulty of counterfeiting, and has multiple anti-counterfeiting capabilities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114815006B_ABST
    Figure CN114815006B_ABST
Patent Text Reader

Abstract

The present invention discloses a dynamically amplified photochromic film, the film comprising a dynamic amplification layer and a strong light color-changing layer; the dynamic amplification layer comprises a microlens array layer and a substrate layer; the strong light color-changing layer comprises a dielectric film stack filter layer and a metal nanoparticle layer, the metal nanoparticle layer is arranged on the upper surface of the dielectric film stack filter layer; the metal nanoparticle layer of the strong light color-changing layer is connected to the substrate layer of the dynamic amplification layer; the strong light color-changing layer constitutes a Fabry-Perot interference cavity. The dynamically amplified photochromic film disclosed by the present invention can simultaneously realize the optical characteristics of pattern three-dimensional dynamic effect display and pattern color changeability under strong visible light irradiation, has technical originality, and has great application potential in the fields of dynamic display and anti-counterfeiting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a film in the field of anti-counterfeiting technology, in particular to a film which has a three-dimensional dynamic effect and can change color under strong light. Background Art

[0002] The colors in nature mainly come from the interaction between light and matter. For example, the most common dyes or pigments produce different colors by absorbing light of specific wavelengths. However, this color rendering is not only low in brightness and color gamut, but also low in resolution. The design of micro-nano structures of different materials can cause interference, diffraction, scattering and transmission between light and objects, thereby making the objects appear colored, which is called the structural color of the object. In recent years, the field of structural design color technology has continued to develop. One important branch is to realize the structural color of plasma through the micro-nano structure of special materials. By using the interaction between light and plasma nanostructures, bright structural colors in the visible light band can be achieved, and the color is easy to control, the chromaticity is high, and the spatial resolution reaches the optical diffraction limit.

[0003] When light interacts with metal nanostructures, the electric field of the incident light causes the free electrons in the metal nanostructure to redistribute and polarize, while enhancing the metal structure's absorption of light, which is called localized surface plasmon resonance. Localized surface plasmon resonance binds energy within a subwavelength spatial range. By adjusting the parameters of the metal nanostructure, the absorption of light can be modulated, ultimately changing the corresponding transmission / reflection spectrum. Therefore, structural color devices based on localized surface plasmons have attracted great attention from researchers in recent years due to their advantages such as ultra-high resolution, good stability, and high tolerance for large-angle observation. Since the localized surface plasmon resonance effect itself is sensitive to the external environment (such as the surrounding refractive index) or light, heat, chemical reactions, etc., unlike single-response structural color devices, plasma structural color devices can integrate two or more colors into one pixel unit, becoming color-adjustable structural color devices, showing great application potential in the fields of encryption, dynamic color display, and anti-counterfeiting. Summary of the invention

[0004] The object of the present invention is to overcome the deficiencies of the above-mentioned prior art and to provide a film which can simultaneously realize the display of three-dimensional dynamic effects of patterns and the changeable color of patterns under strong visible light irradiation.

[0005] To achieve the above-mentioned purpose, the technical solution adopted by the present invention is: a dynamically amplified photochromic film, the film comprising a dynamic amplification layer and a strong light color-changing layer;

[0006] The dynamic amplification layer includes a microlens array layer and a substrate layer;

[0007] The strong light color changing layer comprises a dielectric film stack filter layer and a metal nanoparticle layer, wherein the metal nanoparticle layer is arranged on the upper surface of the dielectric film stack filter layer;

[0008] The metal nanoparticle layer of the strong light color changing layer is connected to the base material layer of the dynamic amplification layer;

[0009] The strong light color-changing layer forms a Fabry-Perot interference cavity.

[0010] The dynamically amplified photochromic film of the present invention has a basic structure of a metal nanoparticle layer placed on the surface of the dielectric film stack filter layer. Due to its localized surface plasma resonance effect that enhances scattered light, it exhibits two different color optical responses under ambient light and strong visible light, which is essentially different from the traditional photochromic phenomenon. With the development of micro-nano processing technology and the high requirements of anti-counterfeiting technology for cards and tickets, it is difficult for a single anti-counterfeiting technology to be applied and developed in its field. The plasma structural color composite structure, because of its resolution that breaks through the optical diffraction limit, is very suitable for combination with a microlens array as a pixel unit that composes a pattern. While having strong light color change, it gives the pattern a three-dimensional dynamic effect, realizes multiple anti-counterfeiting functions, and greatly increases the difficulty of counterfeiting.

[0011] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the dielectric film stack filter layer is (aH1bL1) n cH2, and n is an integer, 0≤a, b≤6, 0<c≤6.

[0012] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the dielectric film stack filter layer includes a high-refractive dielectric layer and a low-refractive dielectric layer, and the metal nanoparticle layer is located on the upper surface of the high-refractive dielectric layer; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the material of the high-refractive dielectric layer is a material with a refractive index greater than 1.65, and the material of the low-refractive dielectric layer is a material with a refractive index less than or equal to 1.65.

[0013] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the material of the high-refractive dielectric layer is at least one of lanthanum titanate, titanium pentoxide, niobium pentoxide, zinc sulfide, zinc oxide, zirconium oxide, titanium dioxide, carbon, indium oxide, indium tin oxide, tantalum pentoxide, cerium oxide, yttrium oxide, europium oxide, iron oxide, iron tetroxide, hafnium nitride, hafnium carbide, hafnium oxide, lanthanum oxide, magnesium oxide, neodymium oxide, praseodymium oxide, samarium oxide, antimony trioxide, silicon carbide, silicon nitride, silicon monoxide, selenium trioxide, tin oxide and tungsten trioxide; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the low-refractive dielectric layer is at least one of lanthanum titanate, titanium pentoxide, niobium pentoxide, zinc sulfide, zinc oxide, zirconium oxide, titanium dioxide, carbon, indium oxide, indium tin oxide, tantalum pentoxide, cerium oxide, yttrium oxide, europium oxide, iron oxide, iron tetroxide, hafnium nitride, hafnium carbide, hafnium oxide, lanthanum oxide, magnesium oxide, neodymium oxide, praseodymium oxide, samarium oxide, antimony trioxide, silicon carbide, silicon nitride, silicon monoxide, selenium trioxide, tin oxide and tungsten trioxide; The material is at least one of silica, alumina, magnesium fluoride, aluminum fluoride, cerium fluoride, lanthanum fluoride, neodymium fluoride, samarium fluoride, barium fluoride, calcium fluoride, lithium fluoride, polystyrene, polyethylene, polymethyl methacrylate, polyamide-imide, polyperfluoroethylene propylene, tetrafluoroethylene, chlorotrifluoroethylene, cellulose propionate, cellulose acetate, cellulose acetate butyrate, methylpentene polymer, homopolyformaldehyde, acrylic resin, cellulose nitrate, ethyl cellulose, polypropylene, polysulfone, polyether sulfone, mica, heterogeneous isomorphous polymer, polybutene, ionomer, acrylic copolymer, styrene butadiene, polyvinyl chloride, urea-formaldehyde, styrene acrylonitrile, and polycarbonate.

[0014] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the metal nanoparticles in the metal nanoparticle layer are spaced apart from each other; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the gaps between the metal nanoparticles in the metal nanoparticle layer are 2nm~1mm.

[0015] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the material of the metal nanoparticles is selected from aluminum, silver, gold, copper, platinum, ruthenium, palladium, rhodium, cobalt, iron, nickel, lead, osmium, iridium and alloys thereof.

[0016] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the strong light color-changing layer also includes a reflective layer, and the reflective layer is arranged on the lower surface of the dielectric film stack filter layer; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the thickness of the reflective layer is greater than 20nm; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the reflective layer adopts a metal material, and the metal material is selected from aluminum, silver, gold, copper, platinum, tin, titanium, palladium, rhodium, niobium, chromium, chromium and their alloys.

[0017] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the strong light color-changing layer also includes a protective layer, and the protective layer covers the surface of the metal nanoparticles; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the material of the protective layer is at least one of polystyrene, polyethylene, polymethyl methacrylate, polyamide-imide, polyperfluoroethylene propylene, tetrafluoroethylene, trifluorochloroethylene, cellulose propionate, cellulose acetate, cellulose acetate butyrate, methylpentene polymer, homopolyformaldehyde, acrylic resin, cellulose nitrate, ethyl cellulose, polypropylene, polysulfone, polyethersulfone, mica, heterogeneous isomorphous polymer, polybutene, ion cross-linked polymer, acrylic copolymer, thermoplastic, styrene butadiene, polyvinyl chloride, urea-formaldehyde, styrene acrylonitrile, polycarbonate, silica, alumina, magnesium fluoride, aluminum fluoride, cerium fluoride, lanthanum fluoride, neodymium fluoride, samarium fluoride, barium fluoride, calcium fluoride and lithium fluoride.

[0018] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the dynamic amplification layer and the strong light color-changing layer are connected by a transparent adhesive layer.

[0019] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the substrate layer in the dynamic amplification layer is made of PET, quartz or glass.

[0020] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, each microlens unit of the dynamic amplification layer has at least one strong light color-changing unit in the corresponding area of ​​the strong light color-changing layer.

[0021] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the physical distance from the optical center of the microlens in the dynamic amplification layer to the metal nanoparticle layer in the strong light color-changing layer is consistent with the focal length of the microlens.

[0022] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the strong light color-changing units corresponding to adjacent microlens units in the dynamic amplification layer have the same or different metal nanoparticle parameters; as a more preferred embodiment of the dynamically amplified photochromic film of the present invention, the metal nanoparticle parameters include the material type of the particles, the size of the particles, the gaps between the particles and the morphology of the particles.

[0023] As a preferred embodiment of the dynamically amplified photochromic film of the present invention, the strong light color changing units corresponding to adjacent microlens units in the dynamic amplification layer have the same or different interference cavity thicknesses.

[0024] The dynamically amplified photochromic film device of the present invention is mainly divided into two parts, a dynamic amplification layer and a strong light color-changing layer, which respectively realize the three-dimensional dynamic effect display of the pattern in the plasma structure color device and the optical characteristics of color change under strong visible light irradiation. The dynamic amplification layer includes a microlens array layer and a substrate layer, wherein the substrate layer can use a PET material with certain flexibility or a hard material quartz or glass, which can meet different application requirements. The pattern editing and strong light color-changing functions in the plasma structure color film device are realized by the strong light color-changing layer, and the color of the film can be regulated by changing the size, gap and morphology parameters of the metal nanoparticles or adjusting the thickness of the interference cavity. Strong light color-changing units with different structural parameters can achieve different strong light color-changing color effects. Therefore, the dynamically amplified photochromic film in the present invention can simultaneously realize the three-dimensional dynamic effect display of the pattern and the optical characteristics of the color change of the pattern under strong visible light irradiation, which has technical originality and has great application potential in the fields of dynamic display and anti-counterfeiting. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 The figure is a schematic structural diagram of an embodiment of the dynamically amplified photochromic film of the present invention.

[0026] Figure 2 for Figure 1 Schematic diagram of the preparation process of the dynamically enlarged photochromic film shown.

[0027] Figure 3 for Figure 1 The dynamically enlarged SEM morphology of Au nanoparticles in the photochromic film is shown.

[0028] Figure 4 for Figure 1 The dynamically enlarged picture of the strong light (mobile phone light) color-changing effect of the strong light color-changing layer in the photochromic film is shown.

[0029] Figure 5 It is a schematic structural diagram of another embodiment of the dynamically amplified photochromic film of the present invention.

[0030] in, Figure 1 and Figure 2 In the figure, 000 is an imprint template, 101 is a substrate layer, 102 is a metal nanoparticle layer, 103 is a high-refractive medium layer, 104 is a low-refractive medium layer, and 105 is a reflective layer.

[0031] Figure 5 In the figure, 200 is a reflective layer, 201 is a low-refractive medium layer, 202 is a high-refractive medium layer, 203 is a metal nanoparticle layer, 204 is a protective layer, 205 is a transparent adhesive layer, 206 is a substrate layer, and 207 is a microlens array layer. DETAILED DESCRIPTION

[0032] In order to better illustrate the purpose, technical solutions and advantages of the present invention, the present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.

[0033] Example 1

[0034] A structural embodiment of the dynamically amplified photochromic film of the present invention is shown in the attached figure. Figure 1 As shown, the dynamically amplified photochromic film includes a dynamic amplification layer and a strong light color-changing layer, the dynamic amplification layer includes a microlens array layer 106 and a substrate layer 101, the strong light color-changing layer includes a dielectric film stack filter layer, a metal nanoparticle layer 102 and a reflective layer 105, the dielectric film stack filter layer includes a high-refractive dielectric layer 103 and a low-refractive dielectric layer 104, the metal nanoparticle layer 102 is located on the surface of the high-refractive dielectric layer 103, and the reflective layer 105 is arranged on the surface of the low-refractive dielectric layer 104, that is, the strong light color-changing layer includes the reflective layer 105, the low-refractive dielectric layer 104, the high-refractive dielectric layer 103 and the metal nanoparticle layer 102 in sequence, and the metal nanoparticle layer 102 of the strong light color-changing layer is connected to the substrate layer 101 of the dynamic amplification layer.

[0035] The preparation method of the dynamically amplified photochromic film described in this embodiment is as shown in the attached Figure 2 As shown, a pit with a certain depth is formed on the surface of the PET substrate layer 101 by the action of the imprint template 000. Different pit depths can be obtained by adjusting the steps of the imprint template mold. Then, a layer of Au nanoparticle layer 102 is evaporated. The SEM morphology of the Au nanoparticle layer is shown in FIG. Figure 3 As shown, the average particle size is about 68nm and the gap is about 12nm. Then, a ZrO2 high-refractive medium layer 103 is plated to fill the pits, and then a SiO2 low-refractive medium layer 104 of a certain thickness is plated, and then a 30nm thick Al reflective layer 105 is evaporated to form a strong light color-changing layer. The dynamic color-changing effect of one of the strong light color-changing layers is as follows Figure 4 As shown in FIG. 1 , the strong light color changing unit, which is purple under ambient light, turns green under mobile phone lighting conditions, and the color change before and after lighting can be further controlled by adjusting the structural parameters of the strong light color changing unit. Finally, a PMMA microlens array layer 106 is formed on the surface of the substrate layer. Under this process flow, the structure of the dynamically amplified photochromic film is shown in FIG. Figure 1 shown.

[0036] When the materials of the nanoparticle layer, the high-refractive medium layer, the low-refractive medium layer, etc. in this embodiment are selected from other materials described in the present invention, the obtained dynamically amplified photochromic film has similar effects, which will not be described in detail here.

[0037] In this embodiment, the nanoimprint method is used to manufacture a strong light color-changing unit with interference cavities of different dielectric thicknesses, corresponding to the pixel points magnified by the microlens array. The strong light color-changing unit is a plasma structural color component. Different structural colors can be obtained by adjusting different dielectric layer thicknesses, and the color can change under strong visible light irradiation. Combined with the microlens array, according to the moiré magnification principle, a dynamically magnified structural color pattern is formed at the same time.

[0038] Example 2

[0039] A structural embodiment of the dynamically amplified photochromic film of the present invention. The structure of the dynamically amplified photochromic film of this embodiment is as shown in the attached figure. Figure 5 As shown, the dynamically amplified photochromic film includes a dynamic amplification layer and a strong light color-changing layer, the dynamic amplification layer includes a microlens array layer 207 and a substrate layer 206, the strong light color-changing layer includes a dielectric film stack filter layer, a metal nanoparticle layer 203, a reflective layer 200 and a protective layer 204, the dielectric film stack filter layer includes a high-refractive dielectric layer 202 and a low-refractive dielectric layer 201, the metal nanoparticle layer 203 is located on the surface of the high-refractive dielectric layer 202, the reflective layer 200 is arranged on the surface of the low-refractive dielectric layer 201, and the protective layer 204 covers the vegetarian The surface of the nanoparticle layer 203, i.e. the strong light color changing layer, comprises a reflective layer 200, a low refractive medium layer 201, a high refractive medium layer 202, a metal nanoparticle layer 203 and a protective layer 204 in sequence, and the dynamic amplification layer is connected to the strong light color changing layer through a transparent adhesive layer.

[0040] The preparation method of the dynamically amplified photochromic film described in this embodiment is as follows: using a winding coating device, first coating a layer of Al reflective layer 200 with a thickness of 30nm, then coating a SiO2 low-refractive medium layer 201 and a ZrO2 high-refractive medium layer 202 respectively, and after evaporating a layer of Au nanoparticle layer 203, the metal particles in the local area are remelted and agglomerated to grow, forming larger Au nanoparticles to obtain different structural colors. Then, a PMMA protective layer 204 is covered on the surface of the metal nanoparticle layer. Finally, the PMMA microlens array layer 207 with a PET substrate layer 206 and the strong light color-changing unit head are combined together through a transparent adhesive layer 205 to form a dynamically amplified photochromic film.

[0041] The dynamically amplified photochromic film described in this embodiment has similar effects to those of Example 1, and when the materials of the nanoparticle layer, high-refractive medium layer, low-refractive medium layer, reflective layer, protective layer, etc. described in this embodiment are selected from other materials described in the present invention, the resulting dynamically amplified photochromic film has similar effects, which will not be repeated here.

[0042] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the present invention.

Claims

1. A dynamically amplified photochromic film, characterized in that: The film comprises a dynamic amplification layer and a strong light color changing layer; The dynamic amplification layer includes a microlens array layer and a substrate layer; The strong light color changing layer comprises a dielectric film stack filter layer and a metal nanoparticle layer, wherein the metal nanoparticle layer is arranged on the upper surface of the dielectric film stack filter layer; The dielectric film stack filter layer includes a high-refractive dielectric layer and a low-refractive dielectric layer, and the metal nanoparticle layer is located on the upper surface of the high-refractive dielectric layer; The metal nanoparticle layer of the strong light color changing layer is connected to the base material layer of the dynamic amplification layer; The strong light color-changing layer constitutes a Fabry-Perot interference cavity; The gaps between the metal nanoparticles in the metal nanoparticle layer are 2 nm to 1 mm.

2. The dynamically amplified photochromic film according to claim 1, characterized in that: The dielectric film stack filter layer is (aH1bL1) n cH2, and n is an integer, 0≤a, b≤6, 0<c≤6.

3. The dynamically amplified photochromic film according to claim 1 or 2, characterized in that: The material of the high-refractive medium layer is a material with a refractive index greater than 1.65, and the material of the low-refractive medium layer is a material with a refractive index less than or equal to 1.

65.

4. The dynamically amplified photochromic film according to claim 3, characterized in that: The material of the high-refractive dielectric layer is at least one of lanthanum titanate, titanium pentoxide, niobium pentoxide, zinc sulfide, zinc oxide, zirconium oxide, titanium dioxide, carbon, indium oxide, indium tin oxide, tantalum pentoxide, cerium oxide, yttrium oxide, europium oxide, iron oxide, iron tetroxide, hafnium nitride, hafnium carbide, hafnium oxide, lanthanum oxide, magnesium oxide, neodymium oxide, praseodymium oxide, samarium oxide, antimony trioxide, silicon carbide, silicon nitride, silicon monoxide, selenium trioxide, tin oxide and tungsten trioxide; the material of the low-refractive dielectric layer is at least one of silicon dioxide, aluminum oxide, magnesium fluoride, aluminum fluoride, cerium fluoride, At least one of lanthanum, neodymium fluoride, samarium fluoride, barium fluoride, calcium fluoride, lithium fluoride, polystyrene, polyethylene, polymethyl methacrylate, polyamide-imide, polyperfluoroethylene propylene, tetrafluoroethylene, chlorotrifluoroethylene, cellulose propionate, cellulose acetate, cellulose acetate butyrate, methylpentene polymer, homopolyformaldehyde, acrylic resin, cellulose nitrate, ethyl cellulose, polypropylene, polysulfone, polyethersulfone, mica, heterogeneous isomorphous polymer, polybutene, ionomer, acrylic copolymer, styrene butadiene, polyvinyl chloride, urea-formaldehyde, styrene acrylonitrile, and polycarbonate.

5. The dynamically amplified photochromic film according to claim 1, characterized in that: The metal nanoparticles in the metal nanoparticle layer are spaced apart from each other.

6. The dynamically amplified photochromic film according to claim 1 or 5, characterized in that: The material of the metal nanoparticles is selected from aluminum, silver, gold, copper, platinum, ruthenium, palladium, rhodium, cobalt, iron, nickel, lead, osmium, iridium and alloys thereof.

7. The dynamically amplified photochromic film according to claim 1, characterized in that: The strong light color-changing layer also includes a reflective layer, which is arranged on the lower surface of the dielectric film stack filter layer; the thickness of the reflective layer is greater than 20nm; the reflective layer is made of metal material, and the metal material is selected from aluminum, silver, gold, copper, platinum, tin, titanium, palladium, rhodium, niobium, chromium, chromium and its alloys.

8. The dynamically amplified photochromic film according to claim 1, characterized in that: The strong light color-changing layer also includes a protective layer, which covers the surface of the metal nanoparticles; the material of the protective layer is at least one of polystyrene, polyethylene, polymethyl methacrylate, polyamide-imide, polyperfluoroethylene, tetrafluoroethylene, trifluorochloroethylene, cellulose propionate, cellulose acetate, cellulose acetate butyrate, methylpentene polymer, homopolyformaldehyde, acrylic resin, cellulose nitrate, ethyl cellulose, polypropylene, polysulfone, polyethersulfone, mica, heterogeneous isomorphous polymer, polybutene, ion cross-linked polymer, acrylic copolymer, thermoplastic, styrene butadiene, polyvinyl chloride, urea-formaldehyde, styrene acrylonitrile, polycarbonate, silica, alumina, magnesium fluoride, aluminum fluoride, cerium fluoride, lanthanum fluoride, neodymium fluoride, samarium fluoride, barium fluoride, calcium fluoride and lithium fluoride.

9. The dynamically amplified photochromic film according to claim 1, characterized in that: The dynamic amplification layer and the strong light color changing layer are connected via a transparent adhesive layer.

10. The dynamically amplified photochromic film according to claim 1, characterized in that: The substrate layer in the dynamic amplification layer is made of PET, quartz or glass; The metal nanoparticle layer is an Au nanoparticle layer, which is generated by evaporating an Au nanoparticle layer on the upper surface of the high-refractive medium layer, and then using laser heating technology to remelt and agglomerate metal particles in a local area to form larger Au nanoparticles.

11. The dynamically amplified photochromic film according to claim 1, characterized in that: Each microlens unit of the dynamic amplification layer has at least one strong light color changing unit in the corresponding area of ​​the strong light color changing layer.

12. The dynamically amplified photochromic film according to claim 1, characterized in that: The physical distance from the optical center of the microlens in the dynamic amplification layer to the metal nanoparticle layer in the strong light color changing layer is consistent with the focal length of the microlens.

13. The dynamically amplified photochromic film according to claim 1, characterized in that: The strong light color changing units corresponding to adjacent microlens units in the dynamic amplification layer have the same or different metal nanoparticle parameters; the metal nanoparticle parameters include the material type of the particles, the size of the particles, the gaps between the particles and the morphology of the particles.

14. The dynamically amplified photochromic film according to claim 1, characterized in that: The strong light color changing units corresponding to adjacent microlens units in the dynamic amplification layer have the same or different interference cavity thicknesses.