A forging forming method and die for tube plates of unequal wall thickness
Through the four-step forming method and mold design, the problems of complex forming of parts with unequal wall thickness and low material utilization rate in the traditional process are solved, efficient forming of pipes with unequal wall thickness is achieved, and the mechanical properties and material utilization rate of the parts are improved. .
Patent Information
- Application Number
- CN202210270058.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-18
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-03-18
AI Technical Summary
The traditional forming process of parts with unequal wall thickness is complex and the material utilization rate is low, making it difficult to meet the high requirements of modern manufacturing industry for the overall mechanical properties and assembly accuracy of parts.
Using a four-step forming method and mold design, including hole expansion, primary thickening, secondary thickening and thinning, through the synergy of the forming punch, die, die backing plate and mandrel, pipes with different wall thicknesses are realized of forming.
It improves the material utilization rate and the mechanical properties of parts, simplifies the process flow, reduces the forming load, and improves the forming accuracy.
Smart Images

Figure CN114932189B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal plastic forming, in particular to a forging forming method and a die for a tube plate with unequal wall thickness. Background Art
[0002] With the rapid development of the manufacturing industry, products have increasingly higher requirements on the overall mechanical properties and assembly accuracy of parts and components. Energy conservation and environmental protection are also the focus of common concern in today's world. These are driving the emergence and development of new processes and technologies.
[0003] At present, parts with different wall thickness are used in many structural parts, such as clutch gear rings and hubs of cars, as well as electronic product structural parts and automotive structural parts. Traditional parts with different wall thickness are mostly processed by pre-cold forging and then fine-machining of local dimensions. This method has complex process, large consumption and low material utilization rate.
[0004] Therefore, how to change the low material utilization rate when forming tubes with unequal wall thicknesses in the prior art has become an urgent problem to be solved by those skilled in the art. Summary of the invention
[0005] The purpose of the present invention is to provide a forging forming method and a die for a tube plate with unequal wall thickness, so as to solve the problems existing in the above-mentioned prior art and improve the material utilization rate of the forming.
[0006] To achieve the above-mentioned purpose, the present invention provides the following scheme: The present invention provides a forging forming die for tube plates of unequal wall thickness, comprising a forming punch, a die, a die pad and a mandrel. The first step forming punch and the outer die are coaxially placed, the second step forming punch, the outer die and the die pad are coaxially placed, the third step forming punch, the outer die and the die pad are coaxially placed, and the fourth step forming punch and the outer die are coaxially placed. There is a gap between the first step punch and the die, there is a gap between the second step mandrel and the die, there is a gap between the third step mandrel and the die, and there is a gap between the fourth step punch and the die. The positioning devices in the above-mentioned molds are all limit blocks.
[0007] The forming of tubes with different wall thicknesses is completed through four steps, namely, expanding the hole first, thickening once, thickening twice, and thinning finally. This method can produce tubes with different wall thicknesses but the same inner diameter along the length direction.
[0008] Specifically, the present invention uses four steps to prepare unequal thickness wall pipes, including the following steps:
[0009] Step 1: Place one end of the original tube blank with equal wall thickness on the lower die of the mold, i.e., the concave die. The forming punch slowly descends to force the metal material to expand the hole on both sides. After the punch moves to the lower limit, it remains stationary with a constant load. After the hole expansion is completed, the top piece is demolded to obtain the expanded part.
[0010] Step 2: Place the part that has been expanded in the previous step on the die pad, and the punch slowly moves downward, forcing the metal material to slowly fill the open cavity formed by the die and the mandrel. The metal material on the upper end of the part flows inward and outward at the same time to thicken the part. The part is then ejected by the ejector device under the press to obtain a part that has completed the first thickening.
[0011] Step 3: Place the part that has completed the first thickening in the previous step on the die pad. The punch slowly moves down and cooperates with the die to make the metal material on the upper end of the part flow inward for secondary thickening. The part is then ejected by the ejector device under the press to obtain a part that has completed the second thickening.
[0012] Step 4: Place the part that has completed secondary thickening in the concave mold cavity, and the punch slowly moves downward to thin it into tubes of different wall thicknesses with the same inner diameter and different outer diameters. The part is then ejected by the ejector device at the bottom of the press. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. It is obvious that the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0014] Figure 1 It is a schematic cross-sectional structure diagram of step 1 of the forging die for tube plates of unequal wall thickness of the present invention when it is working;
[0015] Figure 2 It is a schematic cross-sectional structure diagram of step 2 when the forging die for forming a tube plate of unequal wall thickness of the present invention is working;
[0016] Figure 3 It is a schematic cross-sectional structure diagram of step three of the forging die for tube plates of unequal wall thicknesses of the present invention when it is working;
[0017] Figure 4 It is a schematic cross-sectional structure diagram of step 4 of the forging die for tube plates of unequal wall thicknesses of the present invention when it is working;
[0018] Figure 5a It is a schematic diagram of a tube blank during the forming process of the forging forming method of the tube plate with unequal wall thickness of the present invention;
[0019] Figure 5bIt is a schematic diagram of the tube after the hole expansion is completed in the forming process of the forging forming method of the tube plate with unequal wall thickness of the present invention;
[0020] Figure 5c It is a schematic diagram of a tube after the first thickening is completed in the forming process of the forging forming method of a tube plate with unequal wall thickness according to the present invention;
[0021] Figure 5d It is a schematic diagram of a tube after the second thickening is completed in the forming process of the forging forming method of the tube plate with unequal wall thickness of the present invention;
[0022] Figure 5e It is a schematic diagram of the tube after thinning during the forming process of the forging forming method of the tube plate with unequal wall thickness of the present invention, and is also a schematic diagram of the target part.
[0023] Among them, 1, 3, 7, 11 are forming convex dies, 2, 4, 8, 12 are concave dies, 5, 9 are mandrels, 6, 10 are concave die pads. t0 is the wall thickness of the original tube blank, L0 is the length of the original tube blank, D0 is the outer diameter of the original tube blank, D4 is the outer diameter of the target part, D5 is the inner diameter of the target part, and L is the length of the target part. DETAILED DESCRIPTION
[0024] The technical scheme in the embodiment of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiment of the present invention. Obviously, the described embodiment is only a part of the embodiment of the present invention, not all of the embodiments. Based on the embodiment of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0025] The purpose of the present invention is to provide a forging forming die for tube plates with unequal wall thicknesses, so as to solve the problems existing in the above-mentioned prior art and improve the material utilization rate of formed parts.
[0026] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0027] Please refer to Figure 1 , 2, 3, 4, among which, Figure 1 The schematic diagram of the cross-section structure of the first process of the forging die for the tube plate with unequal wall thickness according to the present invention is shown in FIG. Figure 2 The schematic diagram of the cross-section structure of the second process of the forging die for the tube plate with unequal wall thickness according to the present invention is shown in FIG. Figure 3 It is a schematic diagram of the cross-section structure of the third process when the forging die of the tube plate with unequal wall thickness is used. Figure 4 It is a schematic cross-sectional structure diagram of the fourth process when the forging die for tube plates of unequal wall thicknesses of the present invention is in operation.
[0028] Please refer to Figure 5a , 5b, 5c, 5d, 5e, Figure 5a-5e This is a schematic diagram of the tube forming process when using the unequal wall thickness tube plate forging forming method of the present invention. Figure 5a This is a schematic diagram of a tube blank formed by the forging forming method of the tube plate with unequal wall thickness according to the present invention. Figure 5b This is a schematic diagram of a pipe after the hole is expanded when the forging method of the pipe plate with unequal wall thickness is used. Figure 5c FIG. 5 is a schematic diagram of a tube after the first thickening is completed when the unequal wall thickness tube plate forging forming method of the present invention is used, and FIG. 5d is a schematic diagram of a tube after the second thickening is completed when the unequal wall thickness tube plate forging forming method of the present invention is used, Figure 5e It is a schematic diagram of a tube after thinning when the forging forming method of the tube plate with unequal wall thickness is used.
[0029] The present invention provides a forging forming method and mold for tube plates of unequal wall thickness, comprising forming punches 1, 3, 7, 11, dies 2, 4, 8, 12, die pads 6, 10, and mandrels 5, 9. The first step forming punch 1 and the outer die 2 are coaxially placed, the second step forming punch 3, the outer die 4 and the die pad 6 are coaxially placed, the third step forming punch 7, the outer die 8 and the die pad 10 are coaxially placed, and the fourth step forming punch 11 and the outer die 12 are coaxially placed. There is a gap between the first step punch 1 and the die 2, there is a gap between the second step mandrel 5 and the die 4, there is a gap between the third step mandrel 9 and the die 8, and there is a gap between the fourth step punch 11 and the die 12. The positioning devices in the above-mentioned molds are all limit blocks.
[0030] When using the forging forming die for tube plates of unequal wall thickness of the present invention, the first step is to place one end of the original tube blank of equal wall thickness on the lower die of the die, i.e., the die 2, and the forming punch 1 slowly descends to force the metal material to expand holes on both sides. After the punch 1 moves to the lower limit, it remains stationary with a constant load. After the expansion is completed, the ejector is demolded to obtain the expanded part. The second step is to place the part that has been expanded in the previous step on the die pad 6, and then the punch 3 slowly descends to force the metal material to slowly fill the open cavity formed by the die 4 and the mandrel 5. The metal material at the upper end of the part flows inward and outward at the same time to thicken, and then the part is ejected by the ejector device below the press to obtain a part that has completed the first thickening. The third step is to continue to place the part that has completed the first thickening in the previous step on the die pad 10, and the punch 7 slowly descends to make the metal material at the upper end of the part flow inward for secondary thickening, and then the part is ejected by the ejector device below the press to obtain a part that has completed the second thickening. In the fourth step, the part that has completed the secondary thickening is placed in the die 12, and the punch 11 slowly descends to thin it into tubes of different wall thicknesses with the same inner diameter and different outer diameters. The part is then ejected by the ejector device below the press to obtain the target part.
[0031] The present invention also provides a method for forging a tube plate with unequal wall thickness, using the above-mentioned forging die for the tube plate with unequal wall thickness, comprising the following steps:
[0032] Step 1: According to the characteristics of the target part, a tube blank with a wall thickness of t0 is produced by wire cutting. One end of the initial tube blank is placed in the die 2. A punch 1 with a conical boss is allowed to slowly descend to the lower limit, forcing the metal material to expand the hole on both sides. Then the ejector mechanism under the press ejects the part upward. The taper angle of the conical boss is α, which should be ensured to be 72°. When it exceeds 72°, with the extrusion of the mold, the possibility of the tube bending outward in the circumferential direction will increase, resulting in difficulty in subsequent forming; the arc radius of the male and female molds R = 77°. When it is less than 77°, folding is likely to occur during subsequent thickening, resulting in difficulty in forming; the gap between the upper ends of the male and female molds 1 and 2 should be maintained between 1.1T and 1.5T. If the gap is too small, the tube wall will be thinned due to friction, and if the gap is too large, the flow of the metal material cannot be constrained; the maximum diameter of the male mold is equal to the required diameter of the tube after hole expansion. In order to avoid the phenomenon of tube rupture, the hole expansion degree should not be too large at one time, and the hole expansion coefficient K should be ensured to be ≤1.5;
[0033] Step 2: Place the part formed in step 1 into the die, place the mandrel 5 and the die 4 coaxially, and then slowly move the punch 3 downward to force the internal metal material to flow inward and outward at the same time to thicken the inside and outside. Then the part is ejected by the ejector device below the press. At this time, the upper wall thickness of the part is 1.4t0, and the lower wall thickness is t0;
[0034] Step 3: Place the part formed in step 2 into the die, place the mandrel 9 and the die 8 coaxially, and slowly move the punch 7 downward to force the internal metal material to flow inward for internal thickening. Then the part is ejected by the ejector device below the press. At this time, the upper wall thickness of the part is 2t0, and the lower wall thickness is t0.
[0035] Step 4: Place the part formed in step 3 into the die 12. The hydraulic cylinder drives the slider to slowly move the punch 11 downward, squeezing the metal material downward to reduce the thickness. The part is then ejected by the ejector device below the press. The inner diameter after thinning is the inner diameter of the target part. The punch 11 needs to be rounded. If the corners are not rounded, the metal tube will be subjected to a large axial force, and the contact part between the metal material and the punch is prone to instability and wrinkling.
[0036] The present invention realizes forming tubes of different wall thicknesses in four processes, effectively solves the problem of low material utilization, improves the material utilization rate and mechanical properties of target parts, and has the advantages of simple process, low forming load and high forming precision.
[0037] The present invention uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only used to help understand the method and core ideas of the present invention. At the same time, for those skilled in the art, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A method for forging a tube plate of unequal wall thickness, using a forging die for a tube plate of unequal wall thickness, Features: The mold comprises a first step forming punch (1), a first step die (2), a second step forming punch (3), a second step die (4), a second step mandrel (5), a second step die pad (6), a third step forming punch (7), a third step die (8), a third step mandrel (9), a third step die pad (10), a fourth step forming punch (11) and a fourth step die (12); Wherein, the first step forming convex die (1) and the first step forming concave die (2) are coaxially placed, and there is a gap between the first step forming convex die (1) and the first step forming concave die (2); The second-step forming convex die (3), the second-step concave die (4), the second-step mandrel (5) and the second-step concave die pad (6) are coaxially arranged, and a gap exists between the second-step concave die (4) and the second-step mandrel (5); The third-step forming convex die (7), the third-step concave die (8), the third-step mandrel (9) and the third-step concave die pad (10) are coaxially arranged, and there is a gap between the third-step concave die (8) and the third-step mandrel (9); The fourth step forming convex die (11) and the fourth step concave die (12) are coaxially placed, and there is a gap between the fourth step forming convex die (11) and the fourth step concave die (12); The forming method comprises the following steps: Step 1: placing one end of the original tube blank of equal wall thickness on the first step die (2), and then the first step forming punch (1) slowly descends to force the metal material to expand holes on both sides. After the first step forming punch (1) moves to the lower limit, it remains stationary with a constant load. After the hole expansion is completed, the top piece is demoulded to obtain a part with a completed hole expansion; Step 2: The part expanded in step 1 is placed on the second step die pad (6), and the second step forming punch (3) slowly moves downward, forcing the metal material to slowly fill the open cavity formed by the second step die (4) and the second step mandrel (5), and the metal material at the upper end of the part flows inward and outward at the same time to be thickened, and then the part is ejected by the ejector device below the press, thereby obtaining a part that has completed the first thickening; Step 3: The part that has completed the first thickening in step 2 is further placed on the third step die pad (10), and the third step forming punch (7) slowly moves downward to cooperate with the third step die (8) to make the metal material on the upper end of the part flow inward for secondary thickening, and then the part is ejected by the ejector device below the press to obtain a part that has completed the second thickening; Step 4: Place the part that has completed the secondary thickening in step 3 in the cavity of the fourth step die (12), and the fourth step forming punch (11) slowly descends to thin the part into tubes of different wall thicknesses with the same inner diameter and different outer diameters. The part is then ejected by the ejector device below the press to obtain the target part.
2. The forging method for tubes and plates of unequal wall thickness according to claim 1, Features: When expanding the hole in step 1, the hole expansion coefficient should ensure that K is less than or equal to 1.
5.
3. The forging method for tubes and plates of unequal wall thickness according to claim 1, Features: During the thickening step 2, the relationship between the thickness t after thickening and the thickness t0 before thickening should satisfy t / t0≤1.45.
Citation Information
Patent Citations
Extrusion forming process of thin-wall long pipe-shaped part blank with flange and mould
CN101829698A
Threaded steel pipe for piping
CN102563220A
Method for manufacturing different-thickness steel pipe, and different-thickness steel pipe
CN108712935A
Machining method of axle shaft sleeve of automobile drive axle
CN109047356A
Method for forming flange at any position of pipe in progressive thickeningmode
CN111346933A