A high temperature gas-cooled reactor metal monitoring method, system and storage medium
By systematically inspecting and maintaining non-nuclear-grade metal parts of high-temperature gas-cooled reactors, the problem of lack of applicable methods in the existing technology is solved, and effective supervision and maintenance of metal parts of high-temperature gas-cooled reactors is achieved, and safety and reliability.
Patent Information
- Application Number
- CN202210583254.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-05-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2042-05-26
AI Technical Summary
The prior art lacks non-nuclear-grade metal supervision methods suitable for high-temperature gas-cooled reactors, and cannot effectively monitor and maintain metal components in high-temperature gas-cooled reactors, resulting in risk of safe operation.
A high-temperature air-cooled relay metal supervision method is proposed, including specific inspection and maintenance steps for steam turbine generators, fixed pressure vessels, soda pipes and heat exchanger heat transfer pipes, and a variety of detection methods such as surface detection and hardness are adopted. For measurement, non-destructive testing, etc., targeted supervision and treatment and regular inspection plans are formulated based on the test results.
Effective supervision and maintenance of non-nuclear-grade metal components of high-temperature gas-cooled reactors is achieved, the safety and reliability of equipment are improved, and the basis for metal supervision is provided for high-temperature gas-cooled reactors.
Smart Images

Figure CN114999689B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of in-service inspection of nuclear power plants, and in particular to a metal monitoring method, system and storage medium for a high-temperature gas-cooled reactor. Background Art
[0002] Metal supervision and inspection is an indispensable and important technical support to ensure the safe operation of nuclear power plants. Most of the nuclear power plants that have been put into operation and are under construction in my country are pressurized water reactor nuclear power plants. For metal supervision and inspection of pressurized water reactor nuclear power plants, a certain targeted metal supervision and inspection plan has been formed. There is no experience and specific standards for metal supervision of high-temperature gas-cooled reactors for reference, and the operating parameters of high-temperature gas-cooled reactors are also different from those of pressurized water reactor nuclear power plants. The secondary circuit steam parameters are close to the steam parameters of thermal power plants. This leads to the supervision method of non-nuclear metals in high-temperature gas-cooled reactors being different from the metal supervision method in pressurized water reactor nuclear power plants, and in actual operation, it is impossible to find a supervision method for non-nuclear metals suitable for high-temperature gas-cooled reactors in the industry.
[0003] Therefore, the inventor believes that it is necessary to propose a metal monitoring method suitable for high temperature gas-cooled reactors. Summary of the invention
[0004] The present invention aims to solve one of the technical problems in the related art at least to a certain extent.
[0005] To achieve the above object, the present invention proposes a high temperature gas-cooled reactor metal monitoring method, comprising the following steps:
[0006] S1. Define the scope of non-nuclear grade metal parts of high temperature gas-cooled reactors. The scope of non-nuclear grade metal parts includes steam turbine generator parts, fixed pressure vessel parts, steam-water pipeline parts and heat exchanger heat transfer tube parts;
[0007] S2. The high-temperature gas-cooled reactor steam turbine generator components are further divided into steam turbine components and generator components, and targeted inspections are conducted on metal parts at different positions in the steam turbine components and generator components, and targeted supervision and processing is conducted based on the inspection results of metal parts at various positions;
[0008] S3. Inspect metal parts at different locations in the fixed pressure vessel components of the high-temperature gas-cooled reactor, and assess the safety level of the inspected metal parts based on the inspection results. Based on the safety level assessment, formulate a targeted regular inspection plan again;
[0009] S4. Detect metals at different positions in the steam-water pipeline components of the high-temperature gas-cooled reactor, and repair or replace metal parts at different positions in the steam-water pipeline components according to the detection results;
[0010] S5. Inspect the heat transfer tube components of the high temperature gas-cooled reactor heat exchanger. Heat transfer tubes with historical defects must be inspected. Other heat transfer tubes are divided into units and sampled according to the units. Heat exchanger heat transfer tube components are replaced and repaired according to the inspection results.
[0011] S6. A supervision record report of non-nuclear grade metal components of a high-temperature gas-cooled reactor is formed based on the test results of S2 to S5, and a metal supervision result evaluation of non-nuclear grade metal components of a high-temperature gas-cooled reactor is generated based on the report results.
[0012] The present invention proposes a set of metal supervision methods suitable for high temperature gas-cooled reactors, gives the key points of metal supervision work in steam turbine generators, fixed pressure vessel steam-water pipelines and condenser heat transfer tubes of high temperature gas-cooled reactors, and provides a basis for carrying out metal supervision work in high temperature gas-cooled reactors.
[0013] Optionally, in S2, the detection method includes one or more combinations of surface detection, hardness measurement, metallographic structure inspection, non-destructive testing, ultrasonic testing, and overspeed testing.
[0014] Furthermore, in S3, the detection method includes annual inspection and periodic inspection.
[0015] Further, in S4, the detection method includes one or more combinations of appearance quality inspection, ultrasonic testing, penetration testing, magnetic particle testing, wall thickness measurement, X-ray testing, hardness testing, metallographic structure testing, and surface testing.
[0016] Further, in S5, the detection method includes one or more combinations of eddy current detection, helium leak detection, visual detection and acoustic emission detection.
[0017] Furthermore, in S2, the detection and supervision method for steam turbine components includes:
[0018] In each dismantling and overhaul after the unit is put into operation, in combination with the characteristics of the high-temperature gas-cooled reactor steam turbine generator, it is necessary to conduct surface inspections on the rotor shaft journal, the variable section R at the root of the high- and medium-pressure rotor speed regulating stage impeller, the front steam seal groove, the impeller, the small angle of the rim, the impeller balance hole, the blades, the blade tie bars, the tie bar holes, the shroud area, the nozzle, the partition, and the partition sleeve to ensure that there are no cracks, serious scratches, and collision marks;
[0019] During the first dismantling and overhaul after the unit is put into operation, the hardness test and metallographic structure inspection of the main shaft of the high-pressure rotor and the medium-pressure rotor are carried out. The hardness test parts are the main shaft end face and the speed regulating stage wheel plane, and the side fixed point position is recorded; the metallographic structure inspection part is the side plane of the speed regulating stage impeller. After the metallographic structure inspection, the inspection point needs to be cleaned several times;
[0020] After the unit is put into operation, non-destructive testing is carried out on the low-pressure rotor blades and blade roots, high-pressure rotor main shaft, medium-pressure rotor main shaft and blade roots during each dismantling and maintenance. The rotor body is subjected to surface testing depending on the equipment condition; ultrasonic testing is carried out on the axial keyway of the last-stage impeller of each level of pressure rotor.
[0021] Furthermore, according to the equipment condition, combined with each unit dismantling and maintenance or nuclear power plant overhaul, macro inspection and non-destructive testing are carried out on the thrust bearings and bearings of each level of the turbine components.
[0022] Furthermore, the supervisory measures taken on steam turbine components based on the test results include:
[0023] Shallow surface defects should be ground off;
[0024] No cracks are allowed in the bearing penetration test, and those that fail the ultrasonic test should be repaired or replaced;
[0025] When cracks occur on the blades, they should be replaced or the cracked blades and the corresponding blades should be cut off, and dynamic balancing tests should be carried out if necessary;
[0026] When the blades are severely eroded, they should be repaired or replaced;
[0027] When cracks occur at the variable section R and the steam seal groove at the root of the high- and medium-pressure rotor speed regulating stage impeller, the cracks should be turned. After turning, surface inspection should be carried out to ensure that the cracks are completely eliminated. After the cracks are eliminated, about 1mm should be turned again to eliminate the fatigue hardened layer. Then the journal strength should be checked and the fatigue life of the rotor should be estimated.
[0028] Furthermore, for the inspection method of generator components: after the unit is put into operation, the rotor shaft, guard ring, and air-cooled fan blades are subjected to surface inspection each time the unit is dismantled and inspected, mainly to check whether there are cracks, severe scratches, and collision marks on the surface. When there are doubts about the surface inspection, non-destructive testing is carried out, and magnetic particle testing is performed on the rotor.
[0029] Furthermore, for the guard rings made of Mn18Cr18 series materials, intergranular crack inspection shall be carried out when the unit is dismantled for the third time for overhaul. After the metallographic structure inspection, the inspection points shall be cleaned several times. For the guard rings with intergranular cracks, a more detailed inspection shall be carried out, and the defect elimination plan or replacement shall be determined according to the defect situation.
[0030] Furthermore, the detection method for steam turbine components and generator components includes:
[0031] During the first dismantling and overhaul after 10 years of operation, non-destructive testing of the rotor shaft is performed depending on the equipment condition;
[0032] For units that have been in operation for 20 years, non-destructive testing of the rotor shaft should be carried out every time they are dismantled for inspection;
[0033] And the turbine rotor needs to be inspected during the inspection of the rotor main shaft.
[0034] Further, the inspection of the steam turbine rotor includes:
[0035] For steam turbine rotors with center holes, the center holes of the rotors shall be inspected and tested by endoscope, ultrasonic wave and eddy current, and the center holes of the rotors shall be inspected 10 years after the unit is put into operation;
[0036] If it is a solid rotor, the rotor is subjected to surface and ultrasonic testing, and the subsequent testing interval is 2 dismantling and maintenance cycles;
[0037] If abnormal operating conditions occur during the operation of the unit, the rotor should be subjected to hardness measurement and non-destructive testing depending on the damage;
[0038] For turbine components and generator components with rotors that have excessive defects, use fracture mechanics methods to conduct safety assessment and defect extension life estimation;
[0039] At the same time, corresponding safety operation supervision measures shall be formulated according to the nature and severity of the defects.
[0040] Further, the fixed pressure vessel components include a pressure vessel body, safety accessories and several instruments;
[0041] The annual inspection includes the inspection of the safety management of the pressure vessel body, the inspection of the pressure vessel body and its operating status, the inspection of the safety accessories body and its operating status, and the inspection of each instrument body and its operating status;
[0042] The main inspection items for regular inspection are macro inspection, wall thickness measurement, surface defect inspection, safety accessories and instrument inspection. Additional inspection items will be added when necessary, including buried defect detection, material analysis, sealing fastener inspection, strength verification, pressure resistance test and leakage test.
[0043] Furthermore, the safety accessory body and the objects to be detected for its operation status include a safety valve, a bursting disc device, and a safety interlock device; the instrument body and the objects to be detected for its operation status include a pressure gauge, a liquid level gauge, and a temperature measuring instrument.
[0044] Furthermore, during the periodic inspection, if the user unit or inspection agency has doubts about the safety status of the pressure vessel, a pressure test should be carried out. The test parameters of the pressure test are calculated based on the allowable use parameters determined by this periodic inspection.
[0045] Furthermore, the safety level is 1-5, and the regular inspection plan is formulated again according to the safety level assessment, including:
[0046] For safety status levels 1 and 2, inspections are generally conducted every 6 years;
[0047] For safety status level 3, inspection is generally conducted every 3 to 6 years;
[0048] For safety status level 4, monitored use, the inspection cycle is determined by the inspection agency, and the cumulative monitored use time shall not exceed 3 years. During the monitored use period, the user unit shall take effective monitoring measures, and the period of regular inspection shall be determined by the inspection agency;
[0049] If the safety status level is 5, the defects should be dealt with, otherwise it should not be used further.
[0050] Furthermore, in S4, the steam-water pipeline components are divided into high-pressure water pipelines and high-pressure water-steam pipelines, low-pressure water pipelines and low-pressure water-steam pipelines, high-pressure steam pipelines and low-pressure steam pipelines. During each overhaul of the unit, the pipelines, welds, elbows or bends need to be inspected, including:
[0051] For high-pressure water pipes and high-pressure steam pipes, no less than 10% of the pipe welds shall be sampled each time, and the next sampled parts shall be those not sampled in the previous sample, and 100% inspection shall be completed by 10 years. For small-diameter pipe seat fillet welds connected to high-pressure water pipes and high-pressure steam pipes, no less than 20% shall be inspected, and the next sampled parts shall be those not sampled in the previous sample, and 100% inspection shall be completed by 10 years.
[0052] For each low-pressure water pipeline and low-pressure steam pipeline, at least one weld shall be randomly inspected for ultrasonic or radiographic testing, and at least one fillet weld of the nozzle seat shall be randomly inspected for penetration or magnetic particle testing;
[0053] For each type of high-pressure steam pipeline straight pipe and weld, no less than 10% of the ratio shall be inspected each time, and the next spot inspection shall be the parts that have not been inspected in the previous inspection, and 100% inspection shall be completed by 10 years. For the pipes connected to the high-pressure steam pipeline and the corner welds of the small-diameter pipes, no less than 20% shall be inspected, and the spot inspection shall be completed by 10 years;
[0054] For each type of low-pressure steam pipeline welds, no less than 10% shall be sampled each time for wall thickness measurement and ultrasonic testing. The last spot check shall be on the parts that were not inspected last time. If excessive defects are found, the inspection ratio shall be expanded. No less than 10% of the corner welds of small-diameter pipe seats connected to the low-pressure steam pipeline shall be inspected. The last spot check shall be on the parts that were not inspected last time.
[0055] Furthermore, during each overhaul of the unit, 10% of the pipe fittings and valve casings and at least one valve casing for each pipeline shall be randomly inspected for appearance quality, hardness, metallographic structure, wall thickness, ovality and non-destructive testing. When defects exceeding the standard are found, the inspection ratio shall be expanded, and the parts inspected in the subsequent overhaul shall be those that were not inspected in the previous overhaul.
[0056] Further, in S5, the heat exchanger heat transfer tube component includes conventional island condenser and other heat exchanger heat transfer tubes;
[0057] When inspecting the conventional island condenser, the outer heat transfer tubes and tubes with historical defects must be inspected, and the inner heat transfer tubes are sampled in "rows". If no defects are found in the sampled heat transfer tubes, the heat transfer tubes will not be inspected again during the inspection cycle. The eddy current inspection ratio for each overhaul shall not be less than 20%;
[0058] When inspecting other heat exchangers, tubes with historical defects must be inspected, and other heat transfer tubes are sampled in rows. If no defects are found in the sampled heat transfer tubes, the heat transfer tubes will not be inspected again during the inspection cycle. The eddy current inspection ratio for each overhaul shall not be less than 20%.
[0059] A high temperature gas-cooled reactor metal monitoring system includes the following modules:
[0060] The first module defines the scope of non-nuclear metal parts of high-temperature gas-cooled reactors. The scope of non-nuclear metal parts includes steam turbine generator parts, fixed pressure vessel parts, steam-water pipeline parts, and heat exchanger heat transfer tube parts.
[0061] In the second module, the high-temperature gas-cooled reactor steam turbine generator components are further divided into steam turbine components and generator components, and targeted inspections are carried out on metal parts at different positions in the steam turbine components and generator components, and targeted supervision and processing are carried out according to the inspection results of metal parts at various positions;
[0062] The third module is to inspect metal parts at different locations in the fixed pressure vessel components of the high-temperature gas-cooled reactor, and assess the safety level of the inspected metal parts based on the inspection results. Based on the safety level assessment, a regular inspection plan is formulated again;
[0063] The fourth module is to detect the metal at different positions in the steam-water pipeline components of the high-temperature gas-cooled reactor, and repair or replace the metal parts at different positions in the steam-water pipeline components according to the detection results;
[0064] The fifth module is to inspect the heat transfer tube components of the high temperature gas-cooled reactor heat exchanger. The heat transfer tubes with historical defects must be inspected. Other heat transfer tubes are divided into units and sampled according to the units. The heat transfer tube components of the heat exchanger are replaced and repaired according to the inspection results.
[0065] The sixth module forms a supervision record report on non-nuclear grade metal components of high temperature gas-cooled reactors based on the test results of S2 to S5, and generates a metal supervision result evaluation on non-nuclear grade metal components of high temperature gas-cooled reactors based on the report results.
[0066] A storage medium stores instructions executable by the above-mentioned high-temperature gas-cooled reactor metal monitoring system, and the instructions are used to implement a high-temperature gas-cooled reactor metal monitoring method as described in any one of the above items when executed by a processor included in the above-mentioned system.
[0067] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0068] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the following description of the embodiments in conjunction with the accompanying drawings, in which:
[0069] Figure 1 The figure is a schematic diagram of the overall method flow of a high temperature gas-cooled reactor metal supervision method according to the present invention. DETAILED DESCRIPTION
[0070] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0071] The present invention provides a high temperature gas-cooled reactor metal monitoring method, which is characterized by comprising the following steps:
[0072] S1. Define the scope of non-nuclear grade metal parts of high temperature gas-cooled reactors. The scope of non-nuclear grade metal parts includes steam turbine generator parts, fixed pressure vessel parts, steam-water pipeline parts and heat exchanger heat transfer tube parts;
[0073] S2. The steam turbine generator components are divided into steam turbine components and generator components again, and targeted inspections are conducted on metal parts at different positions in the steam turbine components and generator components, and targeted supervision and processing is conducted based on the inspection results of the metal parts at various positions. The inspection methods include one or more combinations of surface inspection, hardness measurement, metallographic structure inspection, non-destructive testing, ultrasonic testing, and overspeed testing;
[0074] S3. Inspect metal parts at different locations in fixed pressure vessel components, and assess the safety level of the inspected metal parts based on the inspection results. According to the safety level assessment, a regular inspection plan is formulated again. The inspection methods include annual inspection and regular inspection;
[0075] S4. Detect metals at different positions in the steam and water pipeline components, and repair or replace metal parts at different positions in the steam and water pipeline components according to the detection results. The detection method includes one or more combinations of appearance quality inspection, ultrasonic testing, penetration testing, magnetic particle testing, wall thickness measurement, radiographic testing, hardness testing, metallographic structure testing, and surface testing;
[0076] S5. Inspect the heat transfer tube components of the heat exchanger. Heat transfer tubes with historical defects must be inspected. Other heat transfer tubes are divided into units and sampled according to the units. Heat transfer tube components of the heat exchanger are replaced and repaired according to the inspection results. The inspection methods include one or more combinations of eddy current inspection, helium leak detection, visual inspection and acoustic emission inspection;
[0077] S6. A supervision record report of non-nuclear grade metal components of a high-temperature gas-cooled reactor is formed based on the test results of S2 to S5, and a metal supervision result evaluation of non-nuclear grade metal components of a high-temperature gas-cooled reactor is generated based on the report results.
[0078] The following is a detailed description of the metal monitoring method for the steam turbine part in S2. The metal monitoring items of the steam turbine generator set need to refer to the maintenance manual and be formulated in conjunction with the overhaul plan for the steam turbine generator set in the preventive maintenance plan.
[0079] Corresponding to the above step S1, the scope of steam turbine generator components is defined, and the steam turbine generator components involving metal supervision include:
[0080] a) Steam turbine main shaft, high, medium and low pressure cylinder bodies, impellers, blades, blade roots, partitions, shrouds, bearings, etc.;
[0081] b) Generator shaft, bearings, etc.;
[0082] c) High-pressure main steam valve and high-pressure main regulating valve;
[0083] d) High temperature fastening bolts with size greater than or equal to M32.
[0084] Corresponding to the above step S2, the detection and supervision method for steam turbine components first includes:
[0085] In each dismantling and overhaul after the unit is put into operation, in combination with the characteristics of the high-temperature gas-cooled reactor steam turbine generator, it is necessary to conduct surface inspections on the rotor shaft journal, the variable section R at the root of the high- and medium-pressure rotor speed regulating stage impeller, the front steam seal groove, the impeller, the small angle of the rim, the impeller balance hole, the blades, the blade tie bars, the tie bar holes, the shroud, the nozzle, the partition, the partition sleeve and other parts to ensure that there are no cracks, no serious scratches, and no collision marks. Other parts need to be surface inspected when problems are suspected in the macro inspection;
[0086] During the first dismantling and overhaul after the unit is put into operation, the hardness and metallographic structure of the main shaft of the high-pressure rotor and the medium-pressure rotor are measured. The hardness measurement sites are the main shaft end face and the speed regulating stage wheel plane, and the side fixed point position is recorded; the metallographic structure inspection site is the speed regulating stage impeller side plane. After the metallographic structure inspection, the inspection point needs to be cleaned several times. After each dismantling and overhaul, the hardness measurement is carried out in the vicinity of the first inspection point on the side plane of the 1st-stage speed regulating port wheel; if the hardness has no obvious change compared with the first measurement, the metallographic structure inspection may not be carried out;
[0087] After the unit is put into operation, non-destructive testing is carried out on the low-pressure rotor blades and blade roots, high-pressure rotor main shaft, medium-pressure rotor main shaft and blade roots during each dismantling and maintenance. The rotor body can be surface tested depending on the equipment condition; ultrasonic testing is carried out on the axial keyway of the last-stage impeller of each level of pressure rotor.
[0088] During the first dismantling and overhaul after 10 years of operation, the rotor shaft is nondestructively tested according to the equipment condition; the center hole of the turbine rotor with a center hole is inspected and tested by endoscope, ultrasonic, eddy current and other methods; if it is a solid rotor, the rotor is subjected to surface and ultrasonic testing. Thereafter, the inspection interval is 2 dismantling and overhaul cycles. For units that have been in operation for 20 years, the rotor shaft of the turbine component should be nondestructively tested every time it is dismantled and overhauled.
[0089] For rotors with excessive defects, fracture mechanics methods are used to conduct safety assessments and estimate defect expansion life; at the same time, corresponding safe operation supervision measures are formulated based on the nature and severity of the defects.
[0090] At the same time, it is also necessary to note that when abnormal conditions occur during the operation of the unit, such as severe overspeed, overtemperature, etc., the rotor should be subjected to hardness measurement and non-destructive testing depending on the damage. According to the equipment condition, combined with each unit dismantling and overhaul or nuclear power plant overhaul, the thrust bearings and bearings of the turbine components at all levels should be macroscopically inspected and non-destructively tested.
[0091] In the subsequent metal supervision inspection of the generator components in S2, the above corresponding inspection of the rotor shaft and the rotor is also performed.
[0092] The supervisory measures taken on steam turbine components based on the test results include:
[0093] a) Shallow surface defects should be ground away;
[0094] b) Cracks are not allowed in the bearing penetration test, and those that fail the ultrasonic test should be repaired or replaced;
[0095] c) When cracks occur on blades, they should be replaced or the cracked blades and the corresponding blades should be cut off, and dynamic balancing tests should be carried out if necessary;
[0096] d) When the blades are severely eroded, they should be repaired or replaced;
[0097] e) After cracks appear at the variable section R and steam seal groove of the root of the speed regulating stage impeller of the high and medium pressure rotors, the cracks should be turned. After turning, surface inspection should be carried out to ensure that the cracks are completely eliminated. After the cracks are eliminated, about 1mm should be turned again to eliminate the fatigue hardened layer. Then the journal strength should be checked and the fatigue life of the rotor should be estimated.
[0098] The metal supervision method of the generator part in S2 is described in detail below.
[0099] The inspection and supervision methods for generator components include: surface inspection of the rotor shaft, guard ring, air-cooled fan blades and other components every time the unit is dismantled and overhauled after being put into operation. The main inspection is to check whether there are cracks, severe scratches, and collision marks on the surface. When there are doubts about the surface inspection, non-destructive testing is carried out, and magnetic particle testing is performed on the rotor. The rotor should be demagnetized after magnetic particle testing.
[0100] For rotors with excessive defects, fracture mechanics methods are used to conduct safety assessments and estimate defect expansion life. At the same time, corresponding safe operation supervision measures are formulated based on the nature and severity of the defects.
[0101] The first dismantling and overhaul after ten years of operation of the unit shall be carried out by non-destructive testing of the detectable parts of the rotor shaft and the guard ring according to the equipment condition. The period of inspection of the guard ring shall be the length of two dismantling and overhaul cycles. The rotor center hole shall be inspected 10 years after the unit is put into operation.
[0102] For the retaining rings made of Mn18Cr18 series materials, intergranular crack inspection shall be carried out when the unit is dismantled for the third time for overhaul. After the metallographic structure inspection, the inspection points shall be cleaned several times. For the retaining rings with intergranular cracks, a more detailed inspection shall be carried out, and the defect elimination plan or replacement shall be determined according to the defect situation.
[0103] When the unit is undergoing an overspeed test, the temperature of the rotor shaft in the steam turbine generator component should not be lower than the brittle transition temperature of the rotor material.
[0104] The following is a detailed description of the metal supervision method for fixed pressure vessel components in S3.
[0105] For step S1, the scope of the fixed pressure vessel is defined, including the pressure vessel body, safety accessories and instruments, where the pressure vessel body is defined within the following scope:
[0106] a) The slope surface of the first circumferential joint between the pressure vessel and the external pipeline or device by welding (bonding), the first threaded joint end face of the threaded connection, the first flange sealing surface of the flange connection, and the first sealing surface of the special connector or pipe fitting connection;
[0107] b) The pressure-bearing cover and its fasteners of the opening of the pressure vessel;
[0108] c) The connecting weld between non-pressure-bearing components and pressure-bearing components.
[0109] The main pressure-bearing components in the pressure vessel body, including cylinder joints (including reducers), spherical shell plates, shell plates of non-circular vessels, heads, flat covers, expansion joints, equipment flanges, tube sheets and heat exchange tubes of heat exchangers, studs of M36 or above (including M36), and pipe connections and pipe flanges with a nominal diameter greater than or equal to 250 mm;
[0110] Safety accessories for pressure vessels, including safety valves, bursting disc devices, fusible plugs, emergency shut-off devices, and safety interlock devices directly connected to the pressure vessels;
[0111] Instruments for pressure vessels include pressure, temperature, and liquid level measuring instruments directly connected to the pressure vessels.
[0112] Regarding the annual inspection and periodic inspection in step S3 above, the annual inspection is first described in detail.
[0113] The annual inspection includes the inspection of the safety management of the pressure vessel body, the inspection of the pressure vessel body and its operating status, the inspection of the safety accessories body and its operating status, and the inspection of each instrument body and its operating status. After the annual inspection is completed, an analysis of the safety status of the pressure vessel should be conducted, and the hidden dangers found during the annual inspection should be eliminated in a timely manner.
[0114] When the annual inspection is carried out by the user unit, records shall be kept in accordance with the inspection items and requirements of this section, and an annual inspection report shall be issued. The annual inspection report shall be approved by the user unit's safety management person in charge or the authorized safety management personnel. The user unit shall conduct at least one annual inspection of the pressure vessels used each year, which may be carried out at the same time as the annual maintenance of the unit.
[0115] Among them, the safety management inspection mainly corresponds to the inspection of whether the safety management system of the pressure vessel is complete and effective, including:
[0116] a) Whether the design documents, completion drawings, product certificates, product quality certification documents, supervision and inspection certificates, and safety, modification, and maintenance information specified in the pressure vessel safety technical specifications are complete;
[0117] b) Whether the daily maintenance, operation records, and regular safety inspection records of pressure vessels meet the requirements;
[0118] c) Whether the annual inspection and periodic inspection reports of pressure vessels are complete, and whether the problems raised in the inspection and inspection reports have been resolved;
[0119] d) Whether the records of safety accessory inspection (verification), maintenance and replacement are complete and authentic;
[0120] e) Whether there are special emergency plans and drill records for pressure vessels;
[0121] f) Whether records of accidents and failures of pressure vessels are kept.
[0122] Among them, the inspection of the pressure vessel body and its operating conditions, the items and contents to be inspected include:
[0123] a) Whether the nameplate, paint color and marking of the pressure vessel comply with relevant regulations;
[0124] b) Check whether the pressure vessel body, interface (valves, pipes), welded joints, etc. have cracks, overheating, deformation, leakage, mechanical contact damage, etc.;
[0125] c) Whether there is corrosion, abnormal frost, condensation, etc. on the outer surface;
[0126] d) Whether the insulation layer is damaged, peeling, damp, or cold;
[0127] e) Check whether there is any leakage of liquid or air from the leak detection hole and signal hole, and whether the leak detection hole is unobstructed;
[0128] f) Whether there is abnormal vibration, noise or mutual friction between the pressure vessel and adjacent pipes or components;
[0129] g) Whether the support or bearing is damaged, whether the foundation is sunken, tilted or cracked, and whether the fasteners are complete and intact;
[0130] h) Whether the discharge (drainage, sewage) device is intact;
[0131] i) Whether there are overpressure, overtemperature, overload, etc. during operation;
[0132] j) If the tank has a grounding device, check whether the grounding device meets the requirements;
[0133] k) Monitor the pressure vessels in use and whether the monitoring measures are effectively implemented.
[0134] The objects to be inspected for the safety accessories and their operating conditions include safety valves, bursting disc devices, and safety interlock devices; the objects to be inspected for the instrument bodies and their operating conditions include pressure gauges, liquid level gauges, and thermometers. The specific inspection contents and requirements are as follows.
[0135] Safety valve inspection contents and requirements include:
[0136] a) Whether the selection is correct;
[0137] b) Whether it is used within the validity period of the calibration (safety valves are generally calibrated at least once a year);
[0138] c) Whether the device for preventing the free movement of the weight and the lever from running out of the lever-type safety valve is intact, whether the lead sealing device for the adjustment screw of the spring-type safety valve is intact, and whether the device for preventing the weight from flying off of the static weight safety valve is intact;
[0139] d) If a stop valve is installed between the safety valve and the discharge port, is the stop valve in the fully open position and is the lead seal intact?
[0140] e) Is there any leakage in the safety valve?
[0141] f) Check whether the vent pipe is unobstructed and the rain cap is intact.
[0142] Inspection contents and requirements of bursting disc device:
[0143] a) Whether the prescribed period of use has been exceeded;
[0144] b) Whether the installation direction of the bursting disc is correct and whether the bursting pressure and temperature on the product nameplate meet the operating requirements;
[0145] c) Whether the bursting disc device has leakage;
[0146] d) Whether there is a situation where the bursting disc does not explode under overpressure or does not explode under overpressure during use;
[0147] e) Whether the vent pipe connected to the bursting disc holder is unobstructed, whether there is water (or ice) in the vent pipe, and whether the waterproof cap and rainproof sheet are intact;
[0148] f) Whether the stop valve installed between the bursting disc and the pressure vessel is in the fully open state and whether the lead seal is intact;
[0149] g) When the bursting disc and the safety valve are used in series, if the bursting disc is installed on the inlet side of the safety valve, check whether the pressure gauge installed between the bursting disc and the safety valve has pressure display, and open the stop valve to check whether there is gas discharge;
[0150] h) The bursting disc and the safety valve are used in series. If the bursting disc is installed on the outlet side of the safety valve, check whether the pressure gauge installed between the bursting disc and the safety valve has any pressure display. If there is pressure display, the stop valve should be opened to check whether water can be drained and exhausted smoothly.
[0151] The following is a detailed description of the periodic detection in S3.
[0152] Periodic inspection refers to the compliance verification activities carried out by special equipment inspection agencies on the safety status of in-use pressure vessels according to this standard when the pressure vessels are shut down at a certain time period, with macro inspection, wall thickness measurement, surface defect inspection, safety accessories and instrument inspection as the main inspection items. Additional inspection items may be added when necessary, including buried defect detection, material analysis, sealing fastener inspection, strength verification, pressure resistance test and leakage test.
[0153] General requirements for periodic testing include:
[0154] (1) The general procedures of periodic inspection work include formulation of inspection plan, preparation before inspection, implementation of inspection, handling of defects and problems, summary of inspection results, issuance of inspection report, etc.;
[0155] (2) The inspection agency shall carry out periodic inspection of pressure vessels in accordance with the approved inspection scope, and the inspection and testing personnel shall obtain the corresponding special equipment inspection and testing personnel certificate;
[0156] (3) The user unit shall complete the periodic inspection of the pressure vessel before the expiration of the periodic inspection validity period;
[0157] (4) The safety status of pressure vessels in use is divided into levels 1 to 5. After the regular inspection is completed, the safety status of the pressure vessels shall be evaluated as required.
[0158] Before formally conducting regular inspections, the inspection personnel shall formulate an inspection plan based on the use, damage mode and failure mode of the pressure vessel in accordance with the requirements of technical standards. The inspection plan shall be reviewed and approved by the technical person in charge of the inspection agency. The design data, manufacturing data, pressure vessel installation completion data, modification or major repair data, use management data, inspection and inspection data and other materials shall be reviewed, and the site conditions shall be confirmed and cleaned up. The confirmation and cleaning of site conditions specifically include:
[0159] a) Clean or remove the auxiliary parts or other objects that may affect the inspection according to the inspection requirements;
[0160] b) The scaffolding, ladders and other facilities erected for inspection are safe and secure (safety guardrails are installed for scaffolding more than 2m above the ground);
[0161] c) The surfaces to be inspected, especially the corroded parts and the parts that may have crack defects, should be thoroughly cleaned to expose the metal body;
[0162] d) It is necessary to enter the pressure vessel for inspection, discharge and clean the internal medium, isolate all sources of liquid, gas or steam with blind plates, and set obvious isolation signs. It is prohibited to use closed valves instead of blind plates;
[0163] e) When entering the interior of a pressure vessel containing flammable, explosive, combustion-supporting, toxic or asphyxiating media for inspection, it is necessary to carry out replacement, neutralization, disinfection, cleaning, sampling and analysis, and the analysis results must meet the requirements of relevant specifications and standards; the interval between sampling and analysis must comply with the relevant regulations of the user unit; air replacement is strictly prohibited for pressure vessels containing flammable, explosive or combustion-supporting media;
[0164] f) After the manhole and inspection hole are opened, the flammable, explosive, toxic and harmful gases and liquids that may be retained must be removed, and the oxygen content of the gas in the internal space of the pressure vessel must be kept above 0.195; if necessary, ventilation, safety and rescue facilities must also be equipped;
[0165] g) For pressure vessels operating under high or low temperature conditions, the temperature shall be slowly lowered or raised according to the requirements of the operating procedures to reach a level suitable for inspection;
[0166] h) For pressure vessels that can rotate or have movable parts, the switches must be locked and fixed securely;
[0167] i) Cut off the power supply related to the pressure vessel and set up obvious safety warning signs; check that the voltage of lighting power shall not exceed 24V, and the cables introduced into the pressure vessel must be well insulated and reliably grounded;
[0168] j) When it is necessary to conduct X-ray testing on site, isolate the irradiation area, set up warning signs, and comply with relevant safety regulations.
[0169] In the following cases, the outer insulation layer of the pressure vessel shall be partially or completely removed as required:
[0170] a) The thermal insulation layer is damaged or ineffective:
[0171] b) There is a possibility of local corrosion or external surface cracking of the pressure vessel under the insulation layer;
[0172] c) It is impossible to conduct internal inspection of the pressure vessel and external inspection or internal inspection from the outer wall is required;
[0173] d) The inspector considers it necessary.
[0174] The specific supervision inspection methods for each metal component during regular inspection are as follows.
[0175] (1) Macroscopic inspection. During the periodic macroscopic inspection, the macroscopic inspection mainly adopts visual method (when necessary, use endoscope, magnifying glass or other auxiliary instruments and measuring tools) to inspect the pressure vessel body structure, geometric dimensions, surface conditions (such as cracks, corrosion, leakage, deformation), as well as welds, thermal insulation layers, linings, etc.
[0176] (2) Wall thickness measurement. Ultrasonic thickness measurement is generally used. The measurement location should be representative and have sufficient measurement points. After the measurement, make a map and record, and make detailed marks for abnormal thickness measurement points. Generally, the following locations are selected:
[0177] a) Locations where the liquid level frequently fluctuates;
[0178] b) Parts susceptible to corrosion and erosion, such as material inlets, flow turns, and cross-section mutations;
[0179] c) Parts where the wall thickness is reduced during manufacturing and parts that are prone to deformation and wear during use;
[0180] d) Take-over location;
[0181] e) Suspicious areas found during macroscopic inspection.
[0182] When measuring the wall thickness, if delamination defects are found in the base material, additional measuring points should be added or ultrasonic testing should be used to find out the distribution of delamination and the inclination with the base material surface, and record them in a drawing.
[0183] (3) Surface defect detection. When conducting surface defect detection, magnetic particle detection and penetration detection methods should be adopted. Magnetic particle detection should be used as the surface detection method for pressure vessels made of ferromagnetic materials. The requirements for surface defect detection are as follows:
[0184] a) For low-temperature pressure vessels made of carbon steel and low-alloy steel, pressure vessels with environmental cracking tendency or mechanical damage phenomenon, pressure vessels with reheat crack tendency, Cr-Mo steel pressure vessels, low-alloy steel pressure vessels with standard tensile strength lower limit greater than 540MPa, pressure vessels designed according to fatigue analysis, and Category III pressure vessels with design pressure greater than or equal to 1.6MPa for the first periodic inspection, the inspection length shall not be less than 20% of the butt weld length;
[0185] b) Stress concentration areas, deformation areas, areas where cracks are found in macroscopic inspection, austenitic stainless steel cladding layers, dissimilar steel weld joints, T-joints, pipe angle joints, other suspected weld joints, repair welding areas, tooling marks, arc damage areas and areas prone to cracks should be inspected in particular; for materials that are sensitive to welding cracks, pay attention to inspecting possible delayed cracks;
[0186] c) When cracks are found during the inspection, the proportion or area of surface nondestructive inspection should be expanded to detect other possible defects;
[0187] d) If it is not possible to inspect the inner surface, other methods may be used on the outer surface to inspect the inner surface.
[0188] (4) Buried defect detection. When performing buried defect detection, the following requirements apply:
[0189] a) For buried defect detection, radiographic or ultrasonic testing methods shall be used. When any of the following situations occurs, the inspection personnel shall determine the non-destructive testing method and proportion to be used for spot checks based on the specific situation. If necessary, the acoustic emission testing method may be used to determine the activity of the defect:
[0190] 1) Parts that have been repaired during use;
[0191] 2) When cracks are found on the weld surface during inspection, it is considered necessary to conduct weld buried defect detection;
[0192] 3) The weld parts where the misalignment and edge angle exceed the requirements of product standards;
[0193] 4) The parts where welding joints leak during use and the extended parts at both ends;
[0194] 5) Welded joints and other stress concentration areas of pressure vessels subject to alternating loads;
[0195] 6) Parts required by the user or deemed necessary by the inspector.
[0196] b) If the buried defect detection has been carried out and there are no abnormalities during use, no further detection is required.
[0197] (5) Material analysis: Depending on the specific situation, chemical analysis, spectral analysis, hardness testing, metallographic analysis and other methods can be used. Material analysis is carried out in accordance with the following requirements:
[0198] a) If the material is unknown, it is generally necessary to find out the material type of the main pressure-bearing components; for Class III pressure vessels, the material must be found out;
[0199] b) For pressure vessels with a tendency of material degradation, hardness testing should be carried out and metallographic analysis should be carried out if necessary;
[0200] c) Pressure vessels with weld hardness requirements should be subject to hardness testing.
[0201] (6) Pressure vessels that cannot be inspected from the inside. Pressure vessels that cannot be inspected from the inside should be inspected from the outside using reliable inspection technology (such as endoscope, acoustic emission, ultrasonic testing, etc.).
[0202] (7) Strength verification: For pressure vessels with corrosion (and abrasion) depth exceeding the corrosion allowance, unknown nominal thickness, unreasonable structure (and serious defects have been found), or pressure vessels where the inspection personnel have doubts about the strength, strength verification shall be carried out. Strength verification shall be carried out by the inspection agency or entrusted to a capable pressure vessel design unit.
[0203] After a periodic inspection, each component needs to be assessed for safety level based on the inspection results. The safety level is 1-5. Pressure vessels are generally subject to the first periodic inspection within 3 years after commissioning. Based on the safety level assessment, a periodic inspection plan is formulated for each non-nuclear grade metal, including:
[0204] For safety status levels 1 and 2, inspections are generally conducted every 6 years;
[0205] For safety status level 3, inspection is generally conducted every 3 to 6 years;
[0206] For safety status level 4, monitored use, the inspection cycle is determined by the inspection agency, and the cumulative monitored use time shall not exceed 3 years. During the monitored use period, the user unit shall take effective monitoring measures, and the period of regular inspection shall be determined by the inspection agency;
[0207] If the safety status level is 5, the defects should be dealt with, otherwise it should not be used further.
[0208] When formulating the inspection plan, the company's preventive maintenance plan for pressure vessels should be combined, and the regular inspection cycle should be kept consistent with the maintenance cycle of manholes as much as possible.
[0209] The following is a detailed description of the metal supervision method for steam and water pipeline components.
[0210] For the scope definition of S1, the steam and water piping components include:
[0211] High-pressure water pipelines and high-pressure water vapor pipelines (main water supply pipelines with a working pressure of not less than 5.88MPa, etc.), and the pipe before the first valve connected to the pipeline;
[0212] Low-pressure water pipelines and low-pressure water vapor pipelines (condensate and cooling water pipelines with working pressure less than 5.88MPa and not less than 1.6MPa, deaerators and high-pressure and low-pressure heater drainage pipelines, etc.);
[0213] High-pressure steam pipelines (main steam pipelines with an operating temperature of not less than 450°C, start-up and shutdown pipelines, etc.), and the pipes before the first valve connected to the pipelines;
[0214] Low-pressure steam pipelines (turbine extraction steam, auxiliary steam, turbine shaft seal steam pipelines with an operating temperature less than 450°C and not less than 100°C, etc.).
[0215] In S4, the steam-water pipeline components are divided into high-pressure water pipelines and high-pressure water-steam pipelines, low-pressure water pipelines and low-pressure water-steam pipelines, high-pressure steam pipelines and low-pressure steam pipelines. During each overhaul of the unit, the pipelines, welds, elbows or bends need to be inspected, including:
[0216] For high-pressure water pipes and high-pressure steam pipes, no less than 10% of the pipe welds shall be sampled each time, and the next sampled parts shall be those not sampled in the previous sample, and 100% inspection shall be completed by 10 years. For small-diameter pipe seat fillet welds connected to high-pressure water pipes and high-pressure steam pipes, no less than 20% shall be inspected, and the next sampled parts shall be those not sampled in the previous sample, and 100% inspection shall be completed by 10 years.
[0217] For each low-pressure water pipeline and low-pressure steam pipeline, at least one weld shall be randomly inspected for ultrasonic or radiographic testing, and at least one fillet weld of the nozzle seat shall be randomly inspected for penetration or magnetic particle testing;
[0218] For each type of high-pressure steam pipeline straight pipe and weld, no less than 10% of the ratio shall be inspected each time, and the next spot inspection shall be the parts that have not been inspected in the previous inspection, and 100% inspection shall be completed by 10 years. For the pipes connected to the high-pressure steam pipeline and the corner welds of the small-diameter pipes, no less than 20% shall be inspected, and the spot inspection shall be completed by 10 years;
[0219] For each type of low-pressure steam pipeline welds, no less than 10% shall be sampled each time for wall thickness measurement and ultrasonic testing. The last spot check shall be on the parts that were not inspected last time. If excessive defects are found, the inspection ratio shall be expanded. No less than 10% of the corner welds of small-diameter pipe seats connected to the low-pressure steam pipeline shall be inspected. The last spot check shall be on the parts that were not inspected last time.
[0220] When inspecting high-pressure water pipes and high-pressure water vapor pipes, the appearance quality inspection shall be carried out on the pipes, welds and elbows / bends where the insulation layer has been removed. Any surface cracks, severe mechanical damage, heavy skin and other defects found shall be eliminated, and the actual wall thickness at the removed part shall not be less than the minimum required wall thickness of the cylinder pipe. The first inspection shall be carried out on the pipe section and the first elbow after the valve is adjusted in the main water supply pipe. The outer surface of the tees and valves on the pipeline shall be macroscopically inspected, and the suspicious parts shall be subjected to penetration or magnetic particle testing, and ultrasonic testing shall be carried out when necessary. The defects recorded on the pipeline welds shall be reviewed; the pipelines and welds with abnormal hardness shall be tracked and inspected. The wall thickness of the parts of the pipeline elbows (or the small-diameter pipes connected to them) that are prone to erosion and thinning shall be measured, and the neutral surface corrosion fatigue cracks in the parts of the pipeline elbows that are prone to water accumulation shall be detected.
[0221] When inspecting low-pressure water pipes and low-pressure steam pipes, measure the wall thickness of straight pipe sections and elbows that are easily eroded and thinned. Straight pipes and elbows whose wall thickness is less than the minimum required wall thickness of the pipeline should be replaced in a timely manner.
[0222] When inspecting high-pressure steam pipelines, the straight pipe section base material and welds, pipe fittings and valves, and pipes or small-diameter pipes connected to high-temperature steam pipelines are inspected separately in different areas, as follows.
[0223] (1) Metal detection supervision of the parent material and weld area of the straight pipe section;
[0224] Each time the unit is overhauled, the appearance quality, swelling and hardness of each type of high-temperature steam pipeline straight pipe and weld shall be inspected at a rate of not less than 10%. The weld shall be subjected to penetration (or magnetic powder) and ultrasonic testing, and the wall thickness of the straight pipe sections on both sides of the weld shall be measured. Portable Brinell hardness testers shall be used to review the parts with abnormal hardness. If they are still unqualified after the review, metallographic structure inspection shall be carried out. If excessive defects are found in the weld, the inspection ratio shall be expanded. The scope of random inspection in the next overhaul shall be the straight pipe sections and welds of the pipeline that were not inspected in the previous overhaul, and 100% inspection shall be completed in 10 years; for each overhaul of the unit, the following parts and items shall be focused on strengthening supervision and inspection:
[0225] a) Inspection of the appearance, wall thickness, hardness and metallographic structure of the straight pipe and weld of the supervised section, and 100% penetration or magnetic particle and ultrasonic testing of the weld. The hardness and metallographic inspection points should be at or near the previous inspection points.
[0226] b) Before installation or during the previous maintenance, the straight pipe sections and welds with abnormal hardness or metallographic structure shall be inspected for hardness and metallographic structure, as well as the expansion of the straight pipe sections and the penetration or magnetic particle and ultrasonic testing of the welds. The hardness and metallographic inspection points shall be at or near the previous inspection points.
[0227] c) Surface and ultrasonic testing should be carried out on areas where stress concentration exists (such as tee welds and welds connecting pipes and valves), welds at areas with large temperature differences and frequent temperature changes (such as superheat and reheat steam desuperheaters and start-up desuperheater pipeline welds), straight pipe sections and welds that have leaked before, welds with defects recorded during manufacturing or installation inspection or the last maintenance inspection (exceeding the standard and not handled), and welds affected by vibrating pipelines.
[0228] d) Straight pipes and welds where water accumulates should be subjected to ultrasonic testing.
[0229] e) Inspection of straight pipes and welds in areas with thinner pipe walls, appearance and wall thickness, and weld surface and ultrasonic testing.
[0230] (2) Metal detection supervision in pipe fittings and valve areas;
[0231] Each time the unit is overhauled, 10% of the pipe fittings and valve housings (at least one piece of each pipe type) are inspected for appearance quality, hardness, metallographic structure, wall thickness, ovality and non-destructive testing (the flaw detection of elbows includes surface penetration or magnetic particle testing on the outer arc side and ultrasonic testing on the inner wall surface between the neutral planes on both sides of the outer arc). When defects exceeding the standard are found, the inspection ratio should be increased. The parts inspected in the subsequent overhaul are those that were not inspected in the previous overhaul.
[0232] During each overhaul of the unit, the following parts and items are emphasized for supervision and inspection:
[0233] a) Carry out hardness and metallographic structure tests on the following pipe fittings. The hardness and metallographic structure test points should be at or near the previous test points: pipe fittings with abnormal hardness and metallographic structure, elbows and bends with large ovality and thin outer arc side wall thickness before installation, and elbows and bends near the turbine inlet.
[0234] b) Measure the ovality and wall thickness of elbows and bent pipes that have a large ovality and a thin outer arc wall thickness before installation or previous maintenance.
[0235] c) Valves, tees and other pipe fittings that have defects before installation and have been repaired for cracks during operation should be subjected to penetration (or magnetic particle) or ultrasonic testing after each overhaul. The welds of valves and tees (including stress concentration areas such as the shoulders of forged tees) should be subjected to penetration or magnetic particle testing, and the welds of tees should be subjected to ultrasonic testing.
[0236] (3) Metal detection supervision of pipes and small-diameter pipes connected to high-temperature steam pipes;
[0237] Including the inspection of the pipe socket weld and the butt weld, the inspection requirements for the pipe socket fillet welds of the pipes and small-diameter pipes connected to the high-temperature steam pipeline are as follows:
[0238] a) During each overhaul, the fillet welds of the pipes and small-diameter pipes connected to the high-temperature steam pipelines shall be subjected to penetration (or magnetic particle) and ultrasonic testing at a rate of not less than 20%, and the spot check shall be completed every 10 years;
[0239] b) During each overhaul, the following pipes and small-diameter pipes should be inspected in particular: pipes made of materials different from those of high-temperature steam pipes and small-diameter pipes, pipes that may have condensed water (pressure gauge pipes, drain pipes, the lower part of water spray coolers, long blind pipes or infrequently used connecting pipes), pipes in places where expansion is not smooth, and pipe holes and inner surfaces of connected mother pipes for cracks, pipes that have leaked during operation or have been found to have cracks during the previous overhaul;
[0240] The inspection requirements for pipelines, small-diameter pipes and butt welds connected to high-temperature steam pipelines are as follows:
[0241] a) For the welds in front of the primary gate of various pipelines and small-diameter pipes, at least 20% shall be randomly inspected by radiographic or ultrasonic testing during the first overhaul. For the welds of small-diameter pipes, radiographic testing is recommended. If excessive defects are found, the inspection ratio shall be increased;
[0242] b) During each overhaul, the following pipelines, small-diameter pipes and butt welds should be inspected: butt welds of pipelines and pipes in areas where expansion is not smooth, butt welds that have leaked, and wall thickness measurements of pipelines, straight sections or elbows that have leaked due to erosion and thinning;
[0243] c) Small-diameter pipes with a large difference in expansion coefficient from the high-temperature steam pipe material should be replaced;
[0244] d) Pipes or tubes that are prone to condensation and water accumulation and have poor expansion should be modified to prevent fatigue cracking and leakage during operation;
[0245] e) After 10 years of operation, the pipe sections, pipe fittings and valve casings in front of the primary door of the small-diameter pipe connected to the high-temperature steam pipeline should be completely replaced in conjunction with maintenance.
[0246] For each overhaul of the low-pressure steam pipeline unit, the following inspections are carried out on the low-temperature steam pipeline:
[0247] a) The pipes, welds, elbows and bent pipes whose insulation layers have been removed shall be macroscopically inspected. Any defects such as surface cracks, severe mechanical damage, and heavy skin shall be eliminated. The actual wall thickness of the removed area shall not be less than the minimum required wall thickness of the cylinder pipe.
[0248] b) For each overhaul of the unit, no less than 10% of the welds of each type of pipeline shall be sampled for wall thickness measurement and ultrasonic testing. The last spot check shall be the parts that were not inspected last time. If defects exceeding the standard are found, the inspection proportion shall be expanded.
[0249] c) For defects exceeding the standard found by ultrasonic testing of welds, repair welding should be carried out according to the original manufacturing or installation welding process after the defects are removed, and ultrasonic testing should be carried out on the repaired parts.
[0250] d) For each overhaul of the unit, no less than 10% of the corner welds of the pipe seats of small-diameter pipes (drain pipes, temperature measuring pipes, pressure gauge pipes, air pipes, safety valves, exhaust valves, nitrogen filling, sampling, pressure signal pipes, etc.) connected to the steam pipes shall be inspected. The inspection contents shall include appearance inspection, penetration or magnetic particle inspection; the latter spot check areas shall be those that were not inspected the previous time.
[0251] e) During each overhaul of the unit, the outer surface of the tees and valves of the steam pipes shall be macroscopically inspected, and suspicious areas shall be subjected to penetration or magnetic particle testing, and ultrasonic testing shall be performed when necessary.
[0252] The following is a detailed description of the metal supervision method for heat exchanger heat transfer tube components.
[0253] According to the scope of S1, the heat exchanger heat transfer tube components are mainly targeted at non-nuclear grade nuclear island and conventional island heat exchangers for metal supervision inspection, including conventional island condensers and other heat exchanger heat transfer tubes, etc. Specifically:
[0254] a) Condenser: Carry out visual inspection on the inlet and outlet water chambers, return water chambers, tube sheets, and heat transfer tubes; and perform eddy current and helium leak tests on the heat transfer tubes.
[0255] b) Heat exchanger: Conduct eddy current, acoustic emission and helium leak detection tests on heat exchangers such as low-pressure heaters, high-pressure heaters and steam-water separator heat transfer tubes.
[0256] In S5, when inspecting the conventional island condenser, the outer heat transfer tubes and the tubes with historical defects must be inspected, and the inner heat transfer tubes are sampled in "rows". If no defects are found in the sampled heat transfer tubes, the heat transfer tubes will not be inspected again during the inspection cycle. The eddy current inspection ratio for each overhaul shall not be less than 20%;
[0257] When inspecting other heat exchangers, tubes with historical defects must be inspected, and other heat transfer tubes are sampled in rows. If no defects are found in the sampled heat transfer tubes, the heat transfer tubes will not be inspected again during the inspection cycle. The eddy current inspection ratio for each overhaul shall not be less than 20%.
[0258] After completing the metal supervision steps S2-S5, proceed to step S6. The generated record report needs to pay attention to the following: 1. A written inspection report must be formed for metal supervision inspections. Different inspection methods can adopt appropriate inspection report formats; 2. The integrity, reliability and authenticity of the one-way inspection report and the comprehensive project inspection report are reviewed. And when forming the result evaluation, the conclusions are divided into the following three categories: 1. The inspected parts are qualified and used normally; 2. The inspected parts have recordable defects, and the technical support department should repeat the defects in the three consecutive metal supervisions to track the changes in the defects; 3. The inspected parts have defects that exceed the standard, and they should be repaired, replaced or used after defect analysis and evaluation. And if the third situation occurs, it is necessary to report the defects exceeding the standard and the handling opinions to the superior supervisor in a timely manner.
[0259] The present invention also provides a high temperature gas-cooled reactor metal monitoring system, comprising the following modules:
[0260] The first module defines the scope of non-nuclear metal parts of high-temperature gas-cooled reactors. The scope of non-nuclear metal parts includes steam turbine generator parts, fixed pressure vessel parts, steam-water pipeline parts, and heat exchanger heat transfer tube parts.
[0261] In the second module, the high-temperature gas-cooled reactor steam turbine generator components are further divided into steam turbine components and generator components, and targeted inspections are carried out on metal parts at different positions in the steam turbine components and generator components, and targeted supervision and processing are carried out according to the inspection results of metal parts at various positions;
[0262] The third module is to inspect metal parts at different locations in the fixed pressure vessel components of the high-temperature gas-cooled reactor, and assess the safety level of the inspected metal parts based on the inspection results. Based on the safety level assessment, a regular inspection plan is formulated again;
[0263] The fourth module is to detect the metal at different positions in the steam-water pipeline components of the high-temperature gas-cooled reactor, and repair or replace the metal parts at different positions in the steam-water pipeline components according to the detection results;
[0264] The fifth module is to inspect the heat transfer tube components of the high temperature gas-cooled reactor heat exchanger. The heat transfer tubes with historical defects must be inspected. Other heat transfer tubes are divided into units and sampled according to the units. The heat transfer tube components of the heat exchanger are replaced and repaired according to the inspection results.
[0265] The sixth module forms a supervision record report on non-nuclear grade metal components of high temperature gas-cooled reactors based on the test results of S2 to S5, and generates a metal supervision result evaluation on non-nuclear grade metal components of high temperature gas-cooled reactors based on the report results.
[0266] The present invention also provides a storage medium, in which instructions executable by the above system are stored. When the instructions are executed by a processor included in the above system, they are used to implement a high-temperature gas-cooled reactor metal supervision method as described in any one of the above items.
[0267] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0268] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0269] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A high temperature gas-cooled reactor metal monitoring method, characterized in that: The following steps are involved: S1. Define the scope of non-nuclear grade metal parts of high temperature gas-cooled reactors. The scope of non-nuclear grade metal parts includes steam turbine generator parts, fixed pressure vessel parts, steam-water pipeline parts and heat exchanger heat transfer tube parts; S2. The high-temperature gas-cooled reactor steam turbine generator components are further divided into steam turbine components and generator components, and targeted inspections are conducted on metal parts at different positions in the steam turbine components and generator components, and targeted supervision and processing is conducted based on the inspection results of metal parts at various positions; S3. Inspect metal parts at different locations in the fixed pressure vessel components of the high-temperature gas-cooled reactor, and assess the safety level of the inspected metal parts based on the inspection results. Based on the safety level assessment, formulate a targeted regular inspection plan again; S4. Detect metals at different positions in the steam-water pipeline components of the high-temperature gas-cooled reactor, and repair or replace metal parts at different positions in the steam-water pipeline components according to the detection results; S5. Inspect the heat transfer tube components of the high temperature gas-cooled reactor heat exchanger. Heat transfer tubes with historical defects must be inspected. Other heat transfer tubes are divided into units and sampled according to the units. Heat exchanger heat transfer tube components are replaced and repaired according to the inspection results. S6. A supervision record report of non-nuclear grade metal components of a high-temperature gas-cooled reactor is formed based on the test results of S2 to S5, and a metal supervision result evaluation of non-nuclear grade metal components of a high-temperature gas-cooled reactor is generated based on the report results.
2. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 1, characterized in that: In S2, the detection method includes one or more combinations of surface detection, hardness measurement, metallographic structure inspection, non-destructive testing, ultrasonic testing, and overspeed testing.
3. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 1, characterized in that: In S3, the inspection methods include annual inspection and periodic inspection.
4. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 1, characterized in that: In S4, the inspection method includes one or more combinations of appearance quality inspection, ultrasonic inspection, penetration inspection, magnetic particle inspection, wall thickness measurement, X-ray inspection, hardness inspection, metallographic structure inspection, and surface inspection.
5. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 1, characterized in that: In S5, the detection method includes one or more combinations of eddy current detection, helium leak detection, visual detection, and acoustic emission detection.
6. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 2, characterized in that: In S2, the detection and supervision method for steam turbine components includes: In each dismantling and overhaul after the unit is put into operation, in combination with the characteristics of the high-temperature gas-cooled reactor steam turbine generator, it is necessary to conduct surface inspections on the rotor shaft journal, the variable section R at the root of the high- and medium-pressure rotor speed regulating stage impeller, the front steam seal groove, the impeller, the small angle of the rim, the impeller balance hole, the blades, the blade tie bars, the tie bar holes, the shroud area, the nozzle, the partition, and the partition sleeve to ensure that there are no cracks, serious scratches, and collision marks; During the first dismantling and overhaul after the unit is put into operation, the hardness test and metallographic structure inspection of the main shaft of the high-pressure rotor and the medium-pressure rotor are carried out. The hardness test parts are the main shaft end face and the speed regulating stage wheel plane, and the side fixed point position is recorded; the metallographic structure inspection part is the side plane of the speed regulating stage impeller. After the metallographic structure inspection, the inspection point needs to be cleaned several times; After the unit is put into operation, non-destructive testing is carried out on the low-pressure rotor blades and blade roots, high-pressure rotor main shaft, medium-pressure rotor main shaft and blade roots during each dismantling and maintenance. The rotor body is subjected to surface testing depending on the equipment condition; ultrasonic testing is carried out on the axial keyway of the last-stage impeller of each level of pressure rotor.
7. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 2, characterized in that: According to the equipment condition, combined with each unit dismantling and maintenance or nuclear power plant overhaul, macro inspection and non-destructive testing are carried out on the thrust bearings and bearings of each level of turbine components.
8. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 6, characterized in that: The supervisory measures taken on steam turbine components based on the test results include: Shallow surface defects should be ground off; No cracks are allowed in the bearing penetration test, and those that fail the ultrasonic test should be repaired or replaced; When cracks occur on the blades, they should be replaced or the cracked blades and the corresponding blades should be cut off, and dynamic balancing tests should be carried out if necessary; When the blades are severely eroded, they should be repaired or replaced; When cracks occur at the variable section R and the steam seal groove at the root of the high- and medium-pressure rotor speed regulating stage impeller, the cracks should be turned. After turning, surface inspection should be carried out to ensure that the cracks are completely eliminated. After the cracks are eliminated, about 1mm should be turned again to eliminate the fatigue hardened layer. Then the journal strength should be checked and the fatigue life of the rotor should be estimated.
9. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 2, characterized in that: In S2, the inspection method for generator components is as follows: after the unit is put into operation, the rotor shaft, guard ring, and air-cooled fan blades are subjected to surface inspection each time the unit is dismantled and overhauled, mainly to inspect whether there are cracks, severe scratches, and collision marks on the surface. If there is any doubt about the surface inspection, non-destructive testing is performed, and magnetic particle testing is performed on the rotor.
10. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 9, characterized in that: During the first dismantling and overhaul after ten years of operation, the guard ring is subjected to non-destructive testing. Thereafter, the guard ring is inspected at intervals equal to two dismantling and overhaul cycles.
11. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 10, characterized in that: For the retaining rings made of Mn18Cr18 series materials, intergranular crack inspection shall be carried out when the unit is dismantled for the third time for overhaul. After the metallographic structure inspection, the inspection points shall be cleaned several times. For the retaining rings with intergranular cracks, a more detailed inspection shall be carried out, and the defect elimination plan or replacement shall be determined according to the defect situation.
12. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 2, characterized in that: The inspection methods for steam turbine components and generator components include: During the first dismantling and overhaul after 10 years of operation, non-destructive testing of the rotor shaft is performed depending on the equipment condition; For units that have been in operation for 20 years, non-destructive testing of the rotor shaft should be carried out every time they are dismantled for inspection; And the turbine rotor needs to be inspected during the inspection of the rotor main shaft.
13. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 12, characterized in that: Inspection of steam turbine rotors includes: For steam turbine rotors with center holes, the center holes of the rotors shall be inspected and tested by endoscope, ultrasonic wave and eddy current, and the center holes of the rotors shall be inspected 10 years after the unit is put into operation; If it is a solid rotor, the rotor is subjected to surface and ultrasonic testing, and the subsequent testing interval is 2 dismantling and maintenance cycles; If abnormal operating conditions occur during the operation of the unit, the rotor should be subjected to hardness measurement and non-destructive testing depending on the damage; For turbine components and generator components with rotors that have excessive defects, use fracture mechanics methods to conduct safety assessment and defect extension life estimation; At the same time, corresponding safety operation supervision measures shall be formulated according to the nature and severity of the defects.
14. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 3, characterized in that: The components of a fixed pressure vessel include the pressure vessel body, safety accessories and several instruments; The annual inspection includes the inspection of the safety management of the pressure vessel body, the inspection of the pressure vessel body and its operating status, the inspection of the safety accessories body and its operating status, and the inspection of each instrument body and its operating status; The main inspection items for regular inspection are macro inspection, wall thickness measurement, surface defect inspection, safety accessories and instrument inspection. Additional inspection items will be added when necessary, including buried defect detection, material analysis, sealing fastener inspection, strength verification, pressure resistance test and leakage test.
15. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 14, characterized in that: The objects to be inspected for the safety accessory bodies and their operating conditions include safety valves, bursting disc devices, and safety interlock devices; the objects to be inspected for the instrument bodies and their operating conditions include pressure gauges, liquid level gauges, and temperature measuring instruments.
16. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 14, characterized in that: The leakage test includes an air tightness test and an ammonia, halogen and helium leak detection test.
17. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 14, characterized in that: During the periodic inspection, if the user unit or inspection agency has doubts about the safety status of the pressure vessel, a pressure test should be carried out. The test parameters of the pressure test shall be calculated based on the allowable use parameters determined by this periodic inspection.
18. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 3, characterized in that: The safety level is 1-5. According to the safety level assessment, a regular inspection plan is formulated again, including: For safety status levels 1 and 2, inspections are generally conducted every 6 years; For safety status level 3, inspection is generally conducted every 3 to 6 years; For safety status level 4, monitored use, the inspection cycle is determined by the inspection agency, and the cumulative monitored use time shall not exceed 3 years. During the monitored use period, the user unit shall take effective monitoring measures, and the period of regular inspection shall be determined by the inspection agency; If the safety status level is 5, the defects should be dealt with, otherwise it should not be used further.
19. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 4, characterized in that: In S4, the steam-water pipeline components are divided into high-pressure water pipelines and high-pressure water-steam pipelines, low-pressure water pipelines and low-pressure water-steam pipelines, high-pressure steam pipelines and low-pressure steam pipelines. During each overhaul of the unit, the pipelines, welds, elbows or bends need to be inspected, including: For high-pressure water pipes and high-pressure steam pipes, no less than 10% of the pipe welds shall be sampled each time, and the next sampled parts shall be those not sampled in the previous sample, and 100% inspection shall be completed by 10 years. For small-diameter pipe seat fillet welds connected to high-pressure water pipes and high-pressure steam pipes, no less than 20% shall be inspected, and the next sampled parts shall be those not sampled in the previous sample, and 100% inspection shall be completed by 10 years. For each low-pressure water pipeline and low-pressure steam pipeline, at least one weld shall be randomly inspected for ultrasonic or radiographic testing, and at least one fillet weld of the nozzle seat shall be randomly inspected for penetration or magnetic particle testing; For each type of high-pressure steam pipeline straight pipe and weld, no less than 10% of the ratio shall be inspected each time, and the next spot inspection shall be the parts that have not been inspected in the previous inspection, and 100% inspection shall be completed by 10 years. For the pipes connected to the high-pressure steam pipeline and the corner welds of the small-diameter pipes, no less than 20% shall be inspected, and the spot inspection shall be completed by 10 years; For each type of low-pressure steam pipeline welds, no less than 10% shall be sampled each time for wall thickness measurement and ultrasonic testing. The last spot check shall be on the parts that were not inspected last time. If excessive defects are found, the inspection ratio shall be expanded. No less than 10% of the corner welds of small-diameter pipe seats connected to the low-pressure steam pipeline shall be inspected. The last spot check shall be on the parts that were not inspected last time.
20. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 19, characterized in that: During each overhaul of the unit, 10% of the pipe fittings and valve housings and at least one valve housing for each pipeline shall be randomly inspected for appearance quality, hardness, metallographic structure, wall thickness, ovality and non-destructive testing. When excessive defects are found, the inspection ratio shall be expanded and the parts inspected in the subsequent overhaul shall be those that were not inspected in the previous overhaul.
21. A high temperature gas-cooled reactor metal monitoring method as claimed in claim 5, characterized in that: In S5, the heat exchanger heat transfer tube components include conventional island condenser and other heat exchanger heat transfer tubes; When inspecting the conventional island condenser, the outer heat transfer tubes and tubes with historical defects must be inspected, and the inner heat transfer tubes are sampled in "rows". If no defects are found in the sampled heat transfer tubes, the heat transfer tubes will not be inspected again during the inspection cycle. The eddy current inspection ratio for each overhaul shall not be less than 20%; When inspecting other heat exchangers, tubes with historical defects must be inspected, and other heat transfer tubes are sampled in "rows". If no defects are found in the sampled heat transfer tubes, the heat transfer tubes will not be inspected again during the inspection cycle. The eddy current inspection ratio for each overhaul shall not be less than 20%.
22. A high temperature gas-cooled reactor metal monitoring system, characterized in that: Includes the following modules: The first module defines the scope of non-nuclear metal parts of high-temperature gas-cooled reactors. The scope of non-nuclear metal parts includes steam turbine generator parts, fixed pressure vessel parts, steam-water pipeline parts, and heat exchanger heat transfer tube parts. In the second module, the high-temperature gas-cooled reactor steam turbine generator components are further divided into steam turbine components and generator components, and targeted inspections are carried out on metal parts at different positions in the steam turbine components and generator components, and targeted supervision and processing are carried out according to the inspection results of metal parts at various positions; The third module is to inspect metal parts at different locations in the fixed pressure vessel components of the high-temperature gas-cooled reactor, and assess the safety level of the inspected metal parts based on the inspection results. Based on the safety level assessment, a regular inspection plan is formulated again; The fourth module is to detect the metal at different positions in the steam-water pipeline components of the high-temperature gas-cooled reactor, and repair or replace the metal parts at different positions in the steam-water pipeline components according to the detection results; The fifth module is to inspect the heat transfer tube components of the high temperature gas-cooled reactor heat exchanger. The heat transfer tubes with historical defects must be inspected. Other heat transfer tubes are divided into units and sampled according to the units. The heat transfer tube components of the heat exchanger are replaced and repaired according to the inspection results. The sixth module forms a supervision record report on non-nuclear grade metal components of high temperature gas-cooled reactors based on the test results of S2 to S5, and generates a metal supervision result evaluation on non-nuclear grade metal components of high temperature gas-cooled reactors based on the report results.
23. A storage medium storing instructions executable by the system of claim 22, characterized in that: The instructions, when executed by a processor included in the system described in claim 22, are used to implement a high-temperature gas-cooled reactor metal supervision method as described in any one of claims 1-21.