Construction and application of a pressure difference model for blast furnace block belt
By constructing a blast furnace block zone pressure difference model, the problem of furnace condition fluctuations caused by changes in sinter varieties during blast furnace smelting was solved, precise adjustment of blast furnace parameters and fuel optimization were achieved, and smelting production efficiency was improved.
Patent Information
- Application Number
- CN202210600765.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-05-30
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-05-30
AI Technical Summary
Changes in sinter varieties during the blast furnace smelting process lead to fluctuations in furnace conditions. The lack of data model support makes it difficult for operators to accurately control blast furnace parameters, making it difficult to maintain optimal fuel consumption and smelting intensity.
Construct a pressure difference model for the blast furnace block zone, establish a pressure difference simulation binary equation based on the change of void content after the material type is changed, simulate the influence of parameters such as top pressure, air volume, distribution matrix, etc., and make quantitative adjustments to find the best production capacity and fuel Compare.
It achieves precise adjustment of blast furnace parameters, reduces the impact of material changes on furnace conditions, and improves smelting production efficiency and fuel utilization.
Smart Images

Figure BDA0003669873210000021 
Figure BDA0003669873210000022 
Figure BDA0003669873210000023
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of ironmaking, and in particular relates to the construction and application of a blast furnace block belt pressure difference model. Background Art
[0002] As a closed high-temperature and high-pressure container, the smelting process of the blast furnace is a typical black box problem. However, with the gradual progress of ironmaking technology in the past decade. Blast furnace visualization and various mathematical models have become research hotspots, enabling better simulation capabilities for the conditions inside the furnace. However, at the blast furnace operation level, blast furnace operators often still rely on operating methods formed by experience. Their operating methods lack "quantitative" operations based on data models. They are still based on experience. Therefore, the blast furnace smelting method that combines mathematical models with operating experience is the key to whether the mathematical model can be applied to the actual smelting production of the blast furnace and improve the smelting production efficiency.
[0003] In blast furnace smelting production, the change of sintered ore varieties is a common and thorny problem for blast furnaces. Due to the differences in sintered ore particle size composition and low-temperature reduction performance, the adjustment of furnace conditions after the sintering variety of the blast furnace is usually based on the operator's experience. However, due to the lack of model support and quantitative calculation, the operator can only rely on experience to maintain the smelting intensity and fuel consumption after the material change to the greatest extent. It is difficult to accurately control blast furnace parameters such as top pressure, wind pressure, pressure difference, wind speed, coke ratio, and coal ratio in the optimal state. Taking a steel plant blast furnace as an example, due to the large gap in sintering, the blast furnace materials are frequently adjusted. This causes great fluctuations in furnace conditions. Summary of the invention
[0004] In order to overcome the deficiencies of the prior art, the purpose of the present invention is to provide a construction and application of a blast furnace block belt pressure difference model, and establish a pressure difference simulation binary equation through the change of porosity after the material type is changed. Then using this model, it is possible to accurately simulate the influence of top pressure, air volume, platform width of the distribution matrix, central coke ratio, batch weight, coke ratio into the furnace, pellet ratio, change of sintering particle size composition, and low-temperature reduction pulverization rate on the blast furnace pressure difference. Then, through simulation, the matching relationship between top pressure and air volume is continuously corrected, and the batch weight, coal ratio, upper charging system, and other parameters are quantitatively adjusted to find the best production capacity and fuel ratio under the conditions of the material type.
[0005] To achieve the above object, the present invention is implemented through the following technical solutions:
[0006] A blast furnace block belt pressure difference model is constructed, comprising the following steps:
[0007] 1) The blast furnace block belt is divided into a central coke area and a coke-ore mixed area, and equations are established for the regional cross-sectional area and porosity of the two areas respectively; a pressure difference model is established based on the pressure balance principle;
[0008] 2) Obtain the cross-sectional area model of the central coke area, and calculate the radius and cross-sectional area of the central coke circular area through the material surface volume fitting results and the ore and coke volumes, the material distribution matrix angle, and the central coke ratio;
[0009] 3) Calculate the average cross-sectional area of the coke-ore mixed area in the lump zone based on the calculated cross-sectional area of the central coke circular area, the furnace body angle, and the height of the lump zone;
[0010] 4) Obtain the material column resistance coefficient model of the two regions of the block belt. The resistance coefficient of the central coke area is calculated by the coke porosity, and the resistance coefficient of the coke-ore mixed area is calculated by the natural stacking porosity after the mixture of pellets and sintered ore, the ratio of the ore layer and the coke layer thickness, and the sintering low-temperature reduction pulverization rate;
[0011] 5) According to the equations established in steps 1) and 4) and the calculated parameters, the pressure difference of the blast furnace block belt is simulated and calculated.
[0012] The pressure difference model described in step 1):
[0013]
[0014] In formula (1): △P: is the pressure difference of the block belt, the unit is Pa;
[0015] V 腹 : is the amount of gas in the furnace, in m 3 / min;
[0016] S1: The lower cross-sectional area of the coke-ore mixed area in the blocky zone, in m 2 ;
[0017] S2: The cross-sectional area of the central coke area, in m 2 ;
[0018] K1: The material column resistance coefficient in the area after the coke-ore mixture, dimensionless unit;
[0019] Kc: The material column resistance coefficient in the central focal area, dimensionless unit;
[0020] M: relative molecular mass of air 29g / mol;
[0021] ρ: Density of gas at normal pressure, about 1.29-1.3, unit is kg / m 3 ;
[0022] H: Height of blocky zone, in m;
[0023] R: is a constant of 8.313, with the unit of J / (mol·k);
[0024] T 顶: is the blast furnace top temperature, unit is K;
[0025] Pt: blast furnace top pressure, unit is Pa.
[0026] Step 2) The circular cross-sectional area of the central coke region S2 = πL 2 , the relationship between the radius L of the circular cross-sectional area of the central coke area and the distribution parameters:
[0027]
[0028]
[0029] In formula (2): L is the radius of the central coke area, in meters;
[0030] R 喉 is the blast furnace throat radius, in m;
[0031] V 矿 is the ore batch weight, in t;
[0032] α1: calculation process quantity, dimensionless unit;
[0033] H1 is the thickness of the ore layer, which is obtained by fitting the material surface height to the coke volume and ore volume in the material line equation, and the unit is m;
[0034] In formula (3), A is the outer pile angle of coke at the point where the central coke tilting angle falls, in degrees;
[0035] B is the inner pile angle of the ore at the point where the minimum tilt angle of the ore distribution falls, in degrees.
[0036] Step 3) Relationship between the average cross-sectional area of the coke ore mixed area in the blocky zone and the furnace body angle, furnace throat diameter and the cross-sectional area of the central coke area:
[0037]
[0038] In formula (4): β is the blast furnace shaft angle, unit is °;
[0039] R 喉 is the blast furnace throat radius, in m;
[0040] H: Height of blocky zone, in m;
[0041] S1: The lower cross-sectional area of the coke-ore mixed area in the blocky zone, in m 2 ;
[0042] S2: The cross-sectional area of the central coke area, in m 2 .
[0043] Step 4) Relationship between the resistance coefficient of the coke-ore mixing zone and the blast furnace charge parameters:
[0044]
[0045] In formula (5):
[0046] K1: The material column resistance coefficient in the area after the coke-ore mixture, dimensionless unit;
[0047] K c : is the material column resistance coefficient in the central focal area, dimensionless unit;
[0048] E: is the ratio of the thickness of the ore layer to the thickness of the coke layer in the coke mixing area, dimensionless unit;
[0049] N: is the interlayer effect coefficient, which is the airflow resistance effect between the coke layer and the ore layer, dimensionless unit, and the value range is 1.15~1.32;
[0050] ∈ o To consider the porosity of the ore layer under compression after low-temperature reduction, the dimension is %;
[0051] d po is the average particle size of the ore layer, in m;
[0052] is the average shape coefficient of the ore layer, with the unit of % and the value range of 0.65-0.75;
[0053]
[0054] In formula (6):
[0055] ∈ o1 : It is the porosity of the natural state of the sintered and pelletized ore after mixing, the unit is %;
[0056] is the charge compression rate, in %, with a value of 0.85% to 0.88%;
[0057] RDI -0.5 : It is the percentage of the sintered ore low-temperature reduction pulverization index -0.5mm, in %.
[0058] An application of a blast furnace block belt pressure difference model, based on which the pressure difference model of different raw material conditions is estimated to determine the optimal value of each operating parameter, including:
[0059] 1) When the △P is predicted to decrease after the material change, the coke batch weight is reduced by 0.2t to 0.4t to achieve the best fuel consumption;
[0060] 2) When △P is predicted to increase after material change, first reduce the top temperature, open the furnace top to pump water, reduce the top temperature to the lowest value within the acceptable range of the dust removal process, and reduce air volume loss; reduce the ore batch weight by 1 to 4 tons. After reducing the batch weight, recalculate △P using the pressure difference model. If the △P predicted value is still higher than before the material change by >5kPa after reducing the ore batch weight by 4t, continue to increase the central coke ratio by 5% to 10%. If the △P predicted value is still higher than before the material change by >5kPa after the central coke ratio increases by 10%, reduce the minimum tilting angle of the ore by 0.5° to 1.5°. At the same time, by increasing the corresponding relationship between the top pressure and the air volume, the blast kinetic energy is reduced to 75% to 85% of the original kinetic energy, but the blast kinetic energy is ≮90kJ / s, thereby minimizing air volume loss.
[0061] Compared with the prior art, the present invention has the following beneficial effects:
[0062] Through the changes of porosity, particle size composition and low-temperature reduction pulverization rate after the material type is changed, a mathematical model of pressure difference of the block belt that conforms to the actual situation inside the blast furnace is established.
[0063] This model can describe the precise effects of top pressure, air volume, minimum ore angle of the distribution matrix, central coke ratio, batch weight, coke ratio into the furnace, pellet ratio, changes in sintering particle size composition, and low-temperature reduction pulverization rate on the blast furnace pressure difference. This model is then used to correct the matching relationship between top pressure and air volume, as well as to quantify the adjustment methods for batch weight, coal ratio, and upper charging system, in order to find the best production capacity and fuel ratio under the conditions of this material type.
[0064] This model can be used in the fields of blast furnace visualization simulation, blast furnace parameter design, etc.
[0065] Based on the block belt pressure difference model and the influence of various parameters on the pressure difference, a set of smelting schemes for blast furnace parameter setting and selection after the porosity of the bulk material layer changes before and after the blast furnace material change is proposed. The parameters that were adjusted based on experience before the material change can be adjusted systematically, scientifically and quantifiably. In this way, the blast furnace parameters can be adjusted to the most reasonable level and the influence of material changes on the furnace conditions can be minimized. DETAILED DESCRIPTION
[0066] The present invention is described in detail below, but it should be noted that the implementation of the present invention is not limited to the following embodiments.
[0067] Take a steel plant No. 2 3200m 3Take the blast furnace as an example. Due to the change of sintering ore type, the blast furnace is changing from 1# sintering type to 3# sintering type. Since the average particle size of 3# sintering is too small, the porosity of the sintering ore and pellets after mixing is changed from 0.401% to 0.397%, and the average particle size of the ore layer is reduced from 0.019m to 0.015m. The pressure difference model is used to calculate the pressure difference of the block belt, analyze the change of the pressure difference of the block belt of the blast furnace before and after the material change, and then decide how to adjust the blast furnace setting parameters to maintain the best operation effect of the blast furnace. This is to illustrate the application process of the model:
[0068] Step 1:
[0069] The radius L of the central coke area is calculated according to formula 2:
[0070]
[0071] And from formula (2) we get: Known R 喉 =4.5m,V 矿 =49.12m 3 , the minimum ore tilting angle is 29°, the center coke ratio is 25%, A is the outer stack angle of coke at the center coke tilting angle landing point, under the condition of the center coke angle being 13°, then A=73.12-1.97*13°=47.5°B is the inner stack angle of ore at the minimum tilting angle landing point of ore distribution, the minimum ore tilting angle is 29°According to the inner stack angle calculation formula B=23.6°, substituted into formula (3), α1=0.654, H1 is the ore layer thickness, H1=0.887m is obtained by fitting the material surface height to the coke volume and ore volume in the material line equation, substituted into formula (2), L=1.318m is calculated.
[0072] Table 1 shows the No. 2 blast furnace of a steel plant. The coke batch volume is 37.48m 3 The volume of the ore batch is 49.12m 3 , when the minimum ore tilting angle is 29° and the center coking angle is 13°, the center coke ratio is 20% to 25%, and the center coke area radius L is calculated as follows:
[0073] Table 1 Effect of different central coke ratios on the central coke radius L of 2 blast furnaces in a steel plant
[0074] Center focus ratio Mine layer height H1 Central focal radius L 0.2 0.862 1.159 0.21 0.868 1.200 0.22 0.874 1.239 0.23 0.878 1.264 0.24 0.883 1.294 0.25 0.887 1.318
[0075] Step 2:
[0076] Calculate S2 and S1. According to the radius L of the central coke area calculated in step 1, calculate S2 = πL 2 =3.14*1.318 2 =5.45m 2 ,
[0077] S1 is given by formula (4) Calculation, where H is the blast furnace type parameter = 10.7m, the furnace body angle is 81°, R 喉 =4.5mThe result is S1=115.04m 2
[0078] Step 3:
[0079] Calculate K1 and K c
[0080] Coke column resistance coefficient K c
[0081]
[0082] Among them, ∈ c It is the void fraction of coke under compression, with the dimension of %; it is equal to the void fraction of coke under natural stacking state * the compression ratio of charge
[0083] d pc : is the average particle size of coke, in m;
[0084] is the coke shape coefficient, with the unit of %; the value range is 0.7~0.75; the coke shape coefficient is about 0.72;
[0085] It is known that the void ratio of 2 blast furnace coke in the natural stacking state is 0.502% and the charge compression ratio is 85%, then ∈ c =0.427%; 2 The average particle size of blast furnace coke is, d pc =0.055m, Substituting into formula (7) we get K c =325.43;
[0086] The material column resistance coefficient K1 in the area after coke-ore mixing:
[0087]
[0088] Known: RDI -0.5 =0.04, d p0 =0.019, Substituting into formula (5), we can calculate K1=2156.38;
[0089] Step 4
[0090] Calculate the pressure difference △P of the block belt. According to formula (1), the above three steps are used to calculate K1 and K c , S1, S2 are substituted into formula (1) and the amount of gas V is known.腹 , furnace top temperature T 顶 , furnace top pressure Pt, and finally calculated that before the material type was changed, the pressure difference of the block belt was △P = 42.2kPa.
[0091] Step 5
[0092] Repeat steps 1 to 4 to calculate the pressure difference of the block belt after changing the sintering material to 3# sintered ore, which is △P2=52.3kPa;
[0093] The calculation results show that after the sintering material is changed from 1# sintering to 3# sintering, if the blast furnace operating parameters are not adjusted, the pressure difference of the block belt will increase by 10kPa. If the parameters are not adjusted, the smooth operation of the blast furnace will inevitably deteriorate significantly.
[0094] Through steps one to five, the prediction of the pressure difference of the blast furnace lump belt is completed. A complete lump belt pressure difference model is established to quantitatively calculate the specific impact of the adjustable parameters of the blast furnace including (central coke ratio, coke batch weight, ore batch weight, ore minimum tilting angle, furnace gas volume, top pressure, top temperature) on the lump belt pressure difference.
[0095] Step 6: Adjust parameters according to the pressure difference trend: When the raw material type or quality changes significantly, adjust the blast furnace operating parameters according to the pressure difference calculation results to achieve the most reasonable parameter setting. The main solutions include:
[0096] 1) When the △P is predicted to decrease after the material change, the coke batch weight is reduced by 0.2-0.4t to achieve the best fuel consumption;
[0097] 2) When △P is predicted to increase after material change, first reduce the top temperature, open the furnace top to pump water, reduce the top temperature to the lowest value within the acceptable range of the dust removal process, and reduce air volume loss; reduce the ore batch weight by 1 to 4 tons. After reducing the batch weight, recalculate △P using the pressure difference model. If the △P predicted value is still higher than before the material change by >5kPa after reducing the ore batch weight by 4t, continue to increase the central coke ratio by 5% to 10%. If the △P predicted value is still higher than before the material change by >5kPa after the central coke ratio increases by 10%, reduce the minimum tilting angle of the ore by 0.5° to 1.5°. At the same time, by increasing the corresponding relationship between the top pressure and the air volume, the blast kinetic energy is reduced to 75% to 85% of the original kinetic energy, but the blast kinetic energy is ≮90kJ / s, thereby minimizing air volume loss.
[0098] In step 5 of the application example, after the material change, the pressure difference increased to 52kPa, and the increase reached 10kPa, and the blast furnace condition was at risk of serious deterioration. The top temperature was reduced to the lowest limit of 90°C, and the ore batch weight was reduced by 4t. The pressure difference was calculated to be 50kPa using the pressure difference model again. The increase was still too large. The central coke ratio was increased to 35%, and the pressure difference was calculated to be 48kPa using the pressure difference model again. The minimum tilt angle of the ore was reduced by 1°, and the blast kinetic energy was reduced to 85% of the original value, which minimized the air volume loss and ensured the normal condition of the blast furnace.
Claims
1. A method for constructing a blast furnace block belt pressure difference model, characterized in that: The following steps are involved: 1) The blast furnace block belt is divided into a central coke circular area and a coke-ore mixed area, and equations are established for the regional cross-sectional area and porosity of the two areas respectively; a pressure difference model is established based on the pressure balance principle; The pressure difference model described: In formula (1): △P: is the pressure difference of the block belt, the unit is Pa; V 腹 : is the amount of gas in the furnace, in m 3 / min; S1: The lower cross-sectional area of the coke-ore mixed area in the blocky zone, in m 2 ; S2: The cross-sectional area of the central coke circular area, in m 2 ; K1: is the material column resistance coefficient in the coke-ore mixing area, dimensionless unit; Kc: The material column resistance coefficient in the central coke circular area, dimensionless unit; M: relative molecular mass of air 29g / mol; ρ: Density of gas at normal pressure, 1.29-1.3, unit is kg / m 3 ; H: Height of blocky zone, in m; R: is a constant of 8.313, with the unit of J / (mol·K); T 顶 : is the blast furnace top temperature, unit is K; Pt: blast furnace top pressure, unit is Pa; 2) Obtain the cross-sectional area model of the central coke circular area, and calculate the radius and cross-sectional area of the central coke circular area through the material surface volume fitting results and the ore and coke volumes, the material distribution matrix angle, and the central coke ratio; 3) Calculate the average cross-sectional area of the coke-ore mixed area in the lump zone based on the calculated cross-sectional area of the central coke circular area, the furnace body angle, and the height of the lump zone; 4) Obtain the material column resistance coefficient model of the two regions of the block belt. The resistance coefficient of the central coke circular area is calculated by the coke porosity, and the resistance coefficient of the coke-ore mixed area is calculated by the natural stacking porosity after the mixture of pellets and sintered ore, the ratio of the ore layer and the coke layer thickness, and the sintering low-temperature reduction pulverization rate; 5) According to the equations established in steps 1)-4) and the calculated parameters, the pressure difference of the blast furnace block belt is simulated and calculated.
2. The method for constructing a blast furnace block belt pressure difference model according to claim 1, characterized in that: Step 2) The cross-sectional area of the central coke circular region S2 = πL 2 , the relationship between the radius L of the cross-sectional area of the central coke circular area and the distribution parameters: In formula (2): L is the radius of the central coke circular area, in m; R 喉 is the blast furnace throat radius, in m; V 矿 is the ore batch weight, in t; α1: calculation process quantity, dimensionless unit; H1 is the thickness of the ore layer, which is obtained by fitting the material surface height to the coke volume and ore volume in the material line equation, and the unit is m; In formula (3), A is the outer pile angle of coke at the point where the central coke tilting angle falls, in degrees; B is the inner pile angle of the ore at the point where the minimum tilt angle of the ore distribution falls, in degrees.
3. The method for constructing a blast furnace block belt pressure difference model according to claim 1, characterized in that: Step 3) Relationship between the average cross-sectional area of the coke-ore mixed area in the blocky zone and the furnace body angle, furnace throat diameter and the cross-sectional area of the central coke circular area: In formula (4): β is the blast furnace shaft angle, unit is °; R 喉 is the blast furnace throat radius, in m; H: Height of blocky zone, in m; S1: The lower cross-sectional area of the coke-ore mixed area in the blocky zone, in m 2 ; S2: The cross-sectional area of the central coke circular area, in m 2 .
4. The method for constructing a blast furnace block belt pressure difference model according to claim 1, characterized in that: Step 4) Relationship between the resistance coefficient of the coke-ore mixing area and the blast furnace charge parameters: In formula (5): K1: is the material column resistance coefficient in the coke-ore mixing area, dimensionless unit; K c : is the material column resistance coefficient of the central coke circular area, dimensionless unit; E: is the ratio of the thickness of the ore layer to the thickness of the coke layer in the coke-ore mixed area, dimensionless unit; N: is the interlayer effect coefficient, which is the airflow resistance effect between the coke layer and the ore layer, dimensionless unit, and the value range is 1.15~1.32; ∈ o To consider the porosity of the ore layer under compression after low-temperature reduction, the dimension is %; d po is the average particle size of the ore layer, in m; is the average shape coefficient of the ore layer, with the unit of % and the value range of 0.65-0.75; In formula (6): ∈ o1 : It is the porosity of the natural state of the sintered and pelletized ore after mixing, the unit is %; is the charge compression rate, in %, with a value of 0.85% to 0.88%; RDI -0.5 : It is the percentage of the sintered ore low-temperature reduction pulverization index -0.5mm, in %.
5. Application of the method for constructing a blast furnace block belt pressure difference model according to any one of claims 1 to 4, characterized in that: Based on the model, the pressure difference model of different raw material conditions is estimated to determine the optimal value of each operating parameter, including: 1) When the △P is predicted to decrease after the material change, the coke batch weight is reduced by 0.2t to 0.4t to achieve the best fuel consumption; 2) When the △P is predicted to increase after the material change, first reduce the top temperature, open the furnace top to pump water, reduce the top temperature to the lowest value within the acceptable range of the dust removal process, and reduce the air volume loss; reduce the ore batch weight by 1 to 4 tons. After reducing the batch weight, recalculate △P using the pressure difference model. When the ore batch weight is reduced by 4 tons, the predicted △P value is still higher than before the material change by >5kPa. Continue to increase the central coke ratio by 5% to 10%. When the central coke ratio increases by 10%, the predicted △P value is still higher than before the material change by >5kPa. Reduce the minimum tilting angle of the ore by 0.5° to 1.5°. At the same time, by increasing the corresponding relationship between the top pressure and the air volume, reduce the blast kinetic energy to 75% to 85% of the original kinetic energy, and the blast kinetic energy is ≮90kJ / s, thereby minimizing the air volume loss.