Method for selecting adhesive and power generation cell

By selecting and adhering the thermoplastic resin adhesive with flow control in the power generation battery, the problem of the adhesive softening the inflow fluid flow path under high temperature and high humidity environment is solved, and the power generation performance is improved.

CN115117345BActive Publication Date: 2024-11-08HONDA MOTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210172443.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-03-19
Filing Date
2022-02-24
Publication Date
2024-11-08
Estimated Expiration
2042-02-24

AI Technical Summary

Technical Problem

In power generation batteries, the adhesive of thermoplastic resin is easily softened and flows into the fluid flow path when exposed to a high temperature and high humidity environment, resulting in an increase in the pressure loss of the fluid, which in turn affects the power generation performance.

Method used

Through the laminated body formation process, load application process, exposure process and measurement process, a thermoplastic resin adhesive with a flow amount of less than a predetermined amount is selected, and it is adhered to one side of the resin frame member to prevent the adhesive from flowing into the fluid flow road.

Benefits of technology

It effectively suppresses the adhesive flow into the fluid flow path when the power generation battery is running, reduces the pressure loss of the fluid and improves the power generation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115117345B_ABST
    Figure CN115117345B_ABST
Patent Text Reader

Abstract

The present invention provides a method for selecting an adhesive and a power generation cell. The method for selecting an adhesive (40a) of a thermoplastic resin arranged in a manner exposed in a fluid flow path (78) of a power generation cell (10) includes a load application step, an exposure step, a measurement step, and a selection step. In the load application step, a compressive load in a stacking direction is applied to a stack (86) formed by sandwiching an adhesive (84a) between a first resin film (80) and a second resin film (82). In the exposure step, the stack (86) is exposed to an environment heated to a specified temperature and humidified to a specified humidity. In the measurement step, the flow rate M of the adhesive (84a) during the exposure step is measured. In the selection step, an adhesive (84a) having a flow rate (M) of less than a specified amount (M1) is selected as an adhesive (40a) for the power generation cell (10). Accordingly, it is possible to suppress the reduction in power generation performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for selecting a binder and a power generation cell. Background Art

[0002] For example, Japanese Patent Publication No. 2017-111962 discloses an adhesive layer for bonding the inner periphery of a resin frame member to the outer periphery of an electrolyte membrane in an MEA with a resin frame. The adhesive layer is an adhesive (hot melt adhesive) of a thermoplastic resin. Summary of the invention

[0003] In addition, the power generation cell has a fluid flow path, which is used to flow a fluid as a reaction gas or a cooling medium for power generation. The reaction gas is an oxidant gas or a fuel gas. In such a power generation cell, the adhesive of the thermoplastic resin is sometimes exposed to the fluid flow path. In this case, when the power generation cell is running, the adhesive is exposed to a high temperature and high humidity environment and softens. As a result, the adhesive sometimes flows into the fluid flow path. When the adhesive flows into the fluid flow path, the pressure loss of the fluid flowing in the fluid flow path increases, so the power generation performance may decrease.

[0004] The purpose of the present invention is to solve the above-mentioned technical problems.

[0005] A technical solution of the present invention is a method for selecting an adhesive, wherein the adhesive is a thermoplastic resin and is arranged in a manner exposed to a fluid flow path of a power generation cell, the selection method comprising a stack formation process, a load application process, an exposure process, a measurement process and a selection process, wherein, in the stack formation process, a stack is formed by sandwiching an adhesive between a first resin film and a second resin film; in the load application process, a compressive load in a stacking direction is applied to the stack; in the exposure process, the stack is exposed to an environment heated to a specified temperature and humidified to a specified humidity; in the measurement process, the flow rate of the adhesive during the exposure process is measured; and in the selection process, the adhesive having a flow rate below a specified amount is selected as the adhesive for the power generation cell.

[0006] Another technical solution of the present invention is a power generation cell, which has an MEA with a resin frame and metal separators arranged on both sides of the MEA with a resin frame, wherein the MEA with a resin frame has an MEA and a resin frame member arranged on the outer periphery of the MEA in a manner protruding outward from the outer periphery of the MEA, the MEA includes an electrolyte membrane and electrodes arranged on both sides of the electrolyte membrane, and the separator has a fluid flow path and a sealing flange (seal bead) portion, wherein the fluid flow path is used to allow a fluid such as a reaction gas or a cooling medium for power generation to flow therein; the sealing flange portion surrounds the fluid flow path to prevent leakage of the fluid, the sealing flange portion is integrally formed with the partition in a manner of protruding toward the resin frame member, an adhesive layer as an adhesive of a thermoplastic resin is adhered to one surface of the resin frame member, the inner peripheral portion of the adhesive layer joins the outer peripheral portion of the electrolyte membrane to the inner peripheral portion of the resin frame member, and the outer peripheral portion of the adhesive layer joins the top of the sealing flange portion to the outer peripheral portion of the resin frame member, and the adhesive is an adhesive selected by the above-mentioned adhesive selection method.

[0007] According to the present invention, a compressive load in the stacking direction is applied to a laminated body formed by sandwiching an adhesive between a first resin film and a second resin film. In addition, the flow rate of the adhesive when the laminated body is exposed to an environment heated to a specified temperature and humidified to a specified humidity is measured. Thus, the flow rate of the adhesive in an environment close to the environment when the power generation cell is operating can be simply known. Moreover, an adhesive whose measured flow rate is less than a specified amount is selected as an adhesive for the power generation cell. Therefore, it is possible to simply select an adhesive that is not easy to soften and flow into the fluid flow path when the power generation cell is operating.

[0008] In the power generation cell, the adhesive layer as the adhesive selected by the above method is adhered to one side of the resin frame member. Therefore, even when the top of the sealing flange portion is in contact with the adhesive layer, the adhesive is not easy to flow into the fluid flow path when the power generation cell is in operation. Thus, the pressure loss of the fluid flowing in the fluid flow path caused by the adhesive can be suppressed, thereby suppressing the decline in power generation performance.

[0009] The above-mentioned objects, features, and advantages will be easily understood from the following description of the embodiments described with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 This is a partially omitted exploded perspective view of a fuel cell stack having an adhesive selected by the adhesive selection method according to one embodiment of the present invention.

[0011] Figure 2 It is along Figure 1A partially omitted longitudinal sectional view of II-II.

[0012] Figure 3 This is a plan view of the joined separators as viewed from the first separator toward the second separator.

[0013] Figure 4 It is along Figure 1 A partially omitted cross-sectional view of IV-IV.

[0014] Figure 5 It is along Figure 1 A partially omitted sectional view of VV.

[0015] Figure 6 This is a plan view of the joined separators viewed from the second separator toward the first separator.

[0016] Figure 7 It is along Figure 6 A partially omitted longitudinal sectional view of VII-VII.

[0017] Figure 8 It is along Figure 6 A partially omitted cross-sectional view of VIII-VIII.

[0018] Fig. 9 It is used for Figure 1 A flow chart of a method for selecting a binder for a power generation cell.

[0019] Fig.10 It is an explanatory diagram of the step of forming a laminate.

[0020] Fig.11A This is a diagram for explaining the load application process and the exposure process. Fig. 11B This is a diagram for explaining the measurement process.

[0021] Fig.12 It is a graph showing the relationship between the flow rate of the adhesive and the pressure loss.

[0022] Fig.13 Yes Description Figure 1 Flow chart of a method for manufacturing a fuel cell stack.

[0023] Fig.14A This is a diagram for explaining the bonding process. Fig. 14B This is a diagram illustrating the processing steps.

[0024] Fig.15 This is a diagram for explaining the joining process.

[0025] Fig.16 This is a diagram for explaining the lamination process. DETAILED DESCRIPTION

[0026] like Figure 1As shown, the power generation cell 10 is a unit cell of a fuel cell stack 12. The fuel cell stack 12 includes a plurality of power generation cells 10. The plurality of power generation cells 10 are stacked in the direction of arrow A. The fuel cell stack 12 is mounted on a fuel cell electric vehicle (not shown) as a vehicle-mounted fuel cell stack, for example.

[0027] The power generation cell 10 has a horizontally long rectangular shape and includes a resin framed MEA 14 (a resin framed electrolyte membrane-electrode assembly), a first separator 16 , and a second separator 18 . The resin framed MEA 14 is disposed between the first separator 16 and the second separator 18 .

[0028] The first partition plate 16 and the second partition plate 18 are respectively formed by stamping a cross section of a metal thin plate into a corrugated shape. The metal thin plate is, for example, a steel plate, a stainless steel plate, an aluminum plate, or a plated steel plate. The metal thin plate may also be a stainless steel plate with a surface treatment for corrosion prevention or an aluminum plate with a surface treatment for corrosion prevention. The first partition plate 16 and the second partition plate 18 are joined to each other by a plurality of joining lines (not shown) realized by laser welding or the like to form a joined partition plate 20.

[0029] exist Figure 1 and Figure 2 In the embodiment, the MEA 14 with a resin frame includes an MEA 22 (electrolyte membrane-electrode assembly) and a resin frame member 24. The resin frame member 24 is attached to an outer peripheral portion 22o of the MEA 22 so as to protrude outward from the outer peripheral portion 22o.

[0030] like Figure 2 As shown, MEA22 has an electrolyte membrane 26, a first electrode 28 and a second electrode 30. The first electrode 28 is arranged on one surface 26a of the electrolyte membrane 26. The second electrode 30 is arranged on the other surface 26b of the electrolyte membrane 26. The electrolyte membrane 26 is, for example, a solid polymer electrolyte membrane (cation exchange membrane). The solid polymer electrolyte membrane is, for example, a film of perfluorosulfonic acid containing water. The electrolyte membrane 26 is sandwiched by the first electrode 28 and the second electrode 30. The electrolyte membrane 26 can also be a fluorine electrolyte or an HC (hydrocarbon) electrolyte.

[0031] The first electrode 28 includes a first electrode catalyst layer 32 and a first gas diffusion layer 34. The first electrode catalyst layer 32 is bonded to one surface 26a of the electrolyte membrane 26. The first gas diffusion layer 34 is stacked on the first electrode catalyst layer 32. The second electrode 30 includes a second electrode catalyst layer 36 and a second gas diffusion layer 38. The second electrode catalyst layer 36 is bonded to the other surface 26b of the electrolyte membrane 26. The second gas diffusion layer 38 is stacked on the second electrode catalyst layer 36.

[0032] The first electrode catalyst layer 32 includes, for example, porous carbon particles with a platinum alloy supported on the surface. The porous carbon particles are uniformly coated on the surface of the first gas diffusion layer 34 together with an ion conductive polymer binder. The second electrode catalyst layer 36 includes, for example, porous carbon particles with a platinum alloy supported on the surface. The porous carbon particles are uniformly coated on the surface of the second gas diffusion layer 38 together with an ion conductive polymer binder. The first gas diffusion layer 34 and the second gas diffusion layer 38 include carbon paper or carbon cloth, etc.

[0033] The resin frame member 24 has electrical insulation properties. Examples of the constituent material of the resin frame member 24 include PPS (polyphenylene sulfide), PPA (polyphthalamide), PEN (polyethylene naphthalate), PES (polyethersulfone), LCP (liquid crystal polymer), PVDF (polyvinylidene fluoride), silicone resin, fluororesin, m-PPE (modified polyphenylene ether resin), PET (polyethylene terephthalate), PBT (polybutylene terephthalate), or modified polyolefin.

[0034] The resin frame member 24 is a member in the shape of a quadrilateral ring (see Figure 1 ). The inner peripheral portion 24i of the resin frame member 24 is arranged between the outer peripheral portion 28o of the first electrode 28 and the outer peripheral portion 30o of the second electrode 30. Specifically, the inner peripheral portion 24i of the resin frame member 24 is clamped by the outer peripheral portion 26o of the electrolyte membrane 26 and the outer peripheral portion 30o of the second electrode 30. One surface 24a of the resin frame member 24 faces the outer peripheral portion 26o of the electrolyte membrane 26. The other surface 24b of the resin frame member 24 faces the outer peripheral portion 30o of the second electrode 30. In addition, the inner peripheral portion 24i of the resin frame member 24 can also be clamped by the outer peripheral portion 26o of the electrolyte membrane 26 and the outer peripheral portion 28o of the first electrode 28.

[0035] An adhesive layer 40 of an adhesive 40a (hot melt adhesive) as a thermoplastic resin is adhered to one surface 24a (one side) of the resin frame member 24. The outer peripheral portion 26o of the electrolyte membrane 26 is in contact with the adhesive layer 40. In other words, the inner peripheral portion 40i of the adhesive layer 40 joins the outer peripheral portion 26o of the electrolyte membrane 26 to the inner peripheral portion 24i of the resin frame member 24. The adhesive 40a can be liquid or solid. Specifically, the resin material used as the adhesive 40a can include, for example, silicone resins, fluororesins, epoxy resins, etc.

[0036] like Figure 1As shown, one end edge portion in the long side direction of each power generation cell 10 has an oxidant gas supply through hole 42a, a cooling medium supply through hole 44a, and a fuel gas discharge through hole 46b. One end edge portion in the long side direction of each power generation cell 10 is an end edge portion in the direction of arrow B1 of each power generation cell 10. The oxidant gas supply through hole 42a, the cooling medium supply through hole 44a, and the fuel gas discharge through hole 46b are arranged along the short side direction of each power generation cell 10. The short side direction of each power generation cell 10 is along the arrow C direction.

[0037] In the oxidant gas supply passage 42a, the oxidant gas (e.g., oxygen-containing gas) as one of the reaction gases flows in the direction of arrow A2. In the cooling medium supply passage 44a, the cooling medium (e.g., pure water, ethylene glycol, oil, etc.) flows in the direction of arrow A2. In the fuel gas discharge passage 46b, the fuel gas (e.g., hydrogen-containing gas) as the other reaction gas flows in the direction of arrow A1.

[0038] The other end edge portion in the long side direction of each power generation cell 10 has a fuel gas supply through hole 46a, a cooling medium discharge through hole 44b, and an oxidant gas discharge through hole 42b. The other end edge portion in the long side direction of each power generation cell 10 is the end edge portion in the arrow B2 direction of each power generation cell 10. The fuel gas supply through hole 46a, the cooling medium discharge through hole 44b, and the oxidant gas discharge through hole 42b are arranged in the arrow C direction.

[0039] The fuel gas flows in the direction of arrow A2 through the fuel gas supply passage 46a. The coolant flows in the direction of arrow A1 through the coolant discharge passage 44b. The oxidant gas flows in the direction of arrow A1 through the oxidant gas discharge passage 42b.

[0040] The number, arrangement, shape, and size of the communication holes (oxidant gas supply communication holes 42 a and the like) are not limited to the present embodiment, and may be appropriately set according to required specifications.

[0041] like Figure 2 and Figure 3 As shown, the first separator 16 has a rectangular shape. The surface of the first separator 16 facing the MEA 14 with a resin frame (hereinafter referred to as "surface 16a") has an oxidant gas flow path 48 (reaction gas flow path) extending along the long side direction (arrow B direction) of the power generation cell 10. The oxidant gas flow path 48 connects the oxidant gas supply connecting hole 42a and the oxidant gas discharge connecting hole 42b. The oxidant gas flow path 48 supplies the oxidant gas to the first electrode 28.

[0042] The oxidant gas flow path 48 has a plurality of first flow path grooves 52. Each of the first flow path grooves 52 is located between a plurality of first flow path protrusions 50 extending in the direction of arrow B. That is, in the oxidant gas flow path 48, the first flow path protrusions 50 and the first flow path grooves 52 are alternately arranged in the flow path width direction (arrow C direction). The plurality of first flow path protrusions 50 and the plurality of first flow path grooves 52 are integrally formed with the first partition plate 16 by stamping. The first flow path protrusions 50 and the first flow path grooves 52 extend linearly in the direction of arrow B. However, the first flow path protrusions 50 and the first flow path grooves 52 may also extend in a wave-like shape in the direction of arrow B.

[0043] exist Figure 2 In the embodiment, the cross-sectional shape of the first flow path protrusion 50 is a trapezoid. That is, the cross-sectional shape of the first flow path protrusion 50 gradually tapers toward the top in the protruding direction of the first flow path protrusion 50. In addition, the cross-sectional shape of the first flow path protrusion 50 may also be a rectangle.

[0044] exist Figure 3 In the embodiment, a first sealing flange portion 54 is provided on the surface 16a of the first separator 16 for preventing leakage of a fluid as a reaction gas (oxidant gas or fuel gas) or a cooling medium. The first sealing flange portion 54 extends in a straight line when viewed in the separator thickness direction (arrow A direction). However, the first sealing flange portion 54 may also extend in a wave shape when viewed in the separator thickness direction (stacking direction).

[0045] like Figure 2 , Figure 4 and Figure 5 As shown in FIG. 1 , the first sealing flange portion 54 is integrally formed with the first separator 16 in a manner protruding toward the MEA 14 with a resin frame. The first sealing flange portion 54 is elastically deformed by a compressive load in the direction of arrow A. The cross-sectional shape of the first sealing flange portion 54 is a trapezoid. That is, the cross-sectional shape of the first sealing flange portion 54 gradually tapers toward the top end in the protruding direction of the first sealing flange portion 54. In addition, the cross-sectional shape of the first sealing flange portion 54 may also be a rectangle.

[0046] exist Figure 3 In the embodiment, the first sealing flange 54 includes a plurality of first communication hole flanges 56 and a first flow path flange 58. The plurality of first communication hole flanges 56 surround a plurality of communication holes (such as the oxidizing gas supply communication hole 42a). The first flow path flange 58 is located at the outer periphery of the first separator 16.

[0047] Hereinafter, the flange portion surrounding the oxidant gas supply communication hole 42a among the plurality of first communication hole flange portions 56 is referred to as the "first communication hole flange portion 56a", and the flange portion surrounding the oxidant gas discharge communication hole 42b is referred to as the "first communication hole flange portion 56b". In addition, the flange portion surrounding the fuel gas supply communication hole 46a among the plurality of first communication hole flange portions 56 is referred to as the "first communication hole flange portion 56c", and the flange portion surrounding the fuel gas discharge communication hole 46b is referred to as the "first communication hole flange portion 56d". Furthermore, the flange portion surrounding the cooling medium supply communication hole 44a among the plurality of first communication hole flange portions 56 is referred to as the "first communication hole flange portion 56e", and the flange portion surrounding the cooling medium discharge communication hole 44b is referred to as the "first communication hole flange portion 56f".

[0048] The first flow path flange portion 58 surrounds the oxidant gas flow path 48 and the plurality of first communication hole flange portions 56a to 56d. The first communication hole flange portions 56e and 56f are located outside the first flow path flange portion 58. The first flow path flange portion 58 surrounds the power generation region 23 of the MEA 22 (see Figure 2 and Figure 3 ).

[0049] like Figure 3 and Figure 4 As shown, the inner portion 57a ​​of the first connecting hole flange portion 56a located between the oxidant gas supply connecting hole 42a and the oxidant gas flow path 48 has a plurality of first introduction connecting holes 59a. The plurality of first introduction connecting holes 59a connect the oxidant gas supply connecting hole 42a and the oxidant gas flow path 48 to each other. A plurality of first introduction guides 61a are integrally formed on the surface 16a of the first separator 16. The plurality of first introduction guides 61a guide the oxidant gas flowing through each of the first introduction connecting holes 59a to the oxidant gas flow path 48. Each of the first introduction guides 61a protrudes from the surface 16a of the first separator 16 toward the resin frame member 24. The first introduction guide 61a extends from the first connecting hole flange portion 56a toward the oxidant gas flow path 48.

[0050] The first inlet end of the first introduction guide portion 61a near the first communication hole flange portion 56a is separated from the inner portion 57a ​​of the first communication hole flange portion 56a. That is, there is a slight gap 65a between the first inlet end of the first introduction guide portion 61a and the inner portion 57a ​​of the first communication hole flange portion 56a. The first inlet opening 63a facing the first introduction communication hole 59a is located at the first inlet end of the first introduction guide portion 61a.

[0051] like Figure 3 and Figure 5As shown, the inner portion 57b of the first connecting hole flange portion 56b located between the oxidant gas discharge connecting hole 42b and the oxidant gas flow path 48 has a plurality of first outlet connecting holes 59b. The plurality of first outlet connecting holes 59b connect the oxidant gas discharge connecting hole 42b and the oxidant gas flow path 48 to each other. A plurality of first outlet guide portions 61b are integrally formed on the surface 16a of the first partition 16. The plurality of first outlet guide portions 61b guide the oxidant gas (oxidant exhaust gas) flowing in the oxidant gas flow path 48 to each first outlet connecting hole 59b. Each first outlet guide portion 61b protrudes from the surface 16a of the first partition 16 toward the resin frame member 24. The first outlet guide portion 61b extends from the oxidant gas flow path 48 toward the inner portion 57b of the first connecting hole flange portion 56b.

[0052] The first outlet end of the first lead-out guide portion 61b near the first connecting hole flange portion 56b is separated from the inner portion 57b of the first connecting hole flange portion 56b. That is, there is a slight gap 65b between the first outlet end of the first lead-out guide portion 61b and the inner portion 57b of the first connecting hole flange portion 56b. The first outlet opening 63b facing the first lead-out connecting hole 59b is located at the first outlet end of the first lead-out guide portion 61b.

[0053] like Figure 2 , Figure 4 and Figure 5 As shown, the top 60 of the first sealing flange 54 (the first connecting hole flange 56 and the first flow path flange 58) is in contact with the adhesive layer 40. In other words, the top 60 of the first sealing flange 54 (the first connecting hole flange 56 and the first flow path flange 58) is bonded to the outer peripheral portion 24o of the resin frame member 24 through the outer peripheral portion 40o of the adhesive layer 40. In addition, a rubber sealing layer (not shown) may be provided between the top 60 and the adhesive layer 40. The thickness of the rubber sealing layer is thicker than the thickness of the adhesive layer 40.

[0054] The adhesive 40a is exposed in the oxidant gas flow path 48 (the first flow path groove 52a located at the end in the direction of arrow C among the plurality of first flow path grooves 52) (see Figure 2 ). In addition, the adhesive 40a is exposed to the oxidant gas supply through hole 42a, the oxidant gas discharge through hole 42b, the cooling medium supply through hole 44a, the cooling medium discharge through hole 44b, the fuel gas supply through hole 46a and the fuel gas discharge through hole 46b (refer to Figure 4 and Figure 5 ).

[0055] like Figure 2 and Figure 6As shown, the second separator 18 has a rectangular shape. The surface of the second separator 18 facing the MEA 14 with a resin frame (hereinafter referred to as "surface 18a") has a fuel gas flow path 62 (reaction gas flow path) extending along the long side direction (arrow B direction) of the power generation cell 10. The fuel gas flow path 62 connects the fuel gas supply connecting hole 46a and the fuel gas discharge connecting hole 46b. The fuel gas flow path 62 supplies fuel gas to the second electrode 30.

[0056] The fuel gas flow path 62 has a plurality of second flow path grooves 66. Each second flow path groove 66 is located between a plurality of second flow path protrusions 64 extending in the direction of arrow B. That is, in the fuel gas flow path 62, the second flow path protrusions 64 and the second flow path grooves 66 are alternately arranged in the flow path width direction (arrow C direction). The plurality of second flow path protrusions 64 and the plurality of second flow path grooves 66 are integrally formed with the second separator 18 by stamping. The second flow path protrusions 64 and the second flow path grooves 66 extend in a straight line in the direction of arrow B. However, the second flow path protrusions 64 and the second flow path grooves 66 may also extend in a wave-like shape in the direction of arrow B.

[0057] exist Figure 2 In the embodiment, the cross-sectional shape of the second flow path protrusion 64 is a trapezoid. That is, the cross-sectional shape of the second flow path protrusion 64 gradually tapers toward the top end in the protruding direction of the second flow path protrusion 64. In addition, the cross-sectional shape of the second flow path protrusion 64 may also be a rectangle.

[0058] exist Figure 6 In the embodiment, a second sealing flange portion 68 for preventing leakage of a fluid as a reaction gas (oxidant gas or fuel gas) or a cooling medium is provided on the surface 18a of the second separator 18. The second sealing flange portion 68 extends in a straight line when viewed from the separator thickness direction (arrow A direction). However, the second sealing flange portion 68 may also extend in a wave shape when viewed from the separator thickness direction (stacking direction).

[0059] like Figure 2 , Figure 7 and Figure 8 As shown in FIG. 1 , the second sealing flange portion 68 is integrally formed with the second separator 18 in a manner protruding toward the MEA 14 with a resin frame. The second sealing flange portion 68 is elastically deformed by a compressive load in the direction of arrow A. The cross-sectional shape of the second sealing flange portion 68 is a trapezoid. That is, the cross-sectional shape of the second sealing flange portion 68 gradually tapers toward the top end in the protruding direction of the second sealing flange portion 68. In addition, the cross-sectional shape of the second sealing flange portion 68 may also be a rectangle.

[0060] exist Figure 6In the embodiment, the second sealing flange portion 68 includes a plurality of second communication hole flange portions 70 and a second flow path flange portion 72. The plurality of second communication hole flange portions 70 individually surround a plurality of communication holes (such as the oxidant gas supply communication hole 42a). The second flow path flange portion 72 is located at the outer periphery of the second separator 18. The second sealing flange portion 68 overlaps with the first sealing flange portion 54 when viewed in the separator thickness direction (stack direction) (see FIG. 1 ). Figure 2 , Figure 4 , Figure 5 , Figure 7 and Figure 8 ).

[0061] Hereinafter, the flange portion surrounding the oxidant gas supply connecting hole 42a among the plurality of second connecting hole flange portions 70 is referred to as the "second connecting hole flange portion 70a", and the flange portion surrounding the oxidant gas discharge connecting hole 42b is referred to as the "second connecting hole flange portion 70b". In addition, the flange portion surrounding the fuel gas supply connecting hole 46a among the plurality of second connecting hole flange portions 70 is referred to as the "second connecting hole flange portion 70c", and the flange portion surrounding the fuel gas discharge connecting hole 46b is referred to as the "second connecting hole flange portion 70d". Furthermore, the flange portion surrounding the cooling medium supply connecting hole 44a among the plurality of second connecting hole flange portions 70 is referred to as the "second connecting hole flange portion 70e", and the flange portion surrounding the cooling medium discharge connecting hole 44b is referred to as the "second connecting hole flange portion 70f".

[0062] The second flow path flange portion 72 surrounds the fuel gas flow path 62 and the plurality of second communication hole flange portions 70a to 70d. The second communication hole flange portions 70e and 70f are located outside the second flow path flange portion 72. The second flow path flange portion 72 surrounds the power generation area 23 (see Figure 2 and Figure 6 ).

[0063] like Figure 6 and Figure 7 As shown, the inner portion 67a of the second connecting hole flange portion 70c located between the fuel gas supply connecting hole 46a and the fuel gas flow path 62 has a plurality of second introduction connecting holes 69a. The plurality of second introduction connecting holes 69a connect the fuel gas supply connecting hole 46a and the fuel gas flow path 62 to each other. A plurality of second introduction guides 71a are integrally formed on the surface 18a of the second separator 18. The plurality of second introduction guides 71a guide the fuel gas flowing in each second introduction connecting hole 69a to the fuel gas flow path 62. Each second introduction connecting hole 69a protrudes from the surface 18a of the second separator 18 toward the resin frame member 24. The second introduction guide 71a extends from the second connecting hole flange portion 70c toward the fuel gas flow path 62.

[0064] The second inlet end of the second introduction guide portion 71a near the second communication hole flange portion 70c is separated from the inner portion 67a of the second communication hole flange portion 70c. That is, there is a slight gap 75a between the second inlet end of the second introduction guide portion 71a and the inner portion 67a of the second communication hole flange portion 70c. The second inlet opening 73a facing the second introduction communication hole 69a is located at the second inlet end of the second introduction guide portion 71a.

[0065] like Figure 6 and Figure 8 As shown, the inner portion 67b of the second connecting hole flange portion 70d located between the fuel gas discharge connecting hole 46b and the fuel gas flow path 62 has a plurality of second lead-out connecting holes 69b. The plurality of second lead-out connecting holes 69b connect the fuel gas discharge connecting hole 46b and the fuel gas flow path 62 to each other. A plurality of second lead-out guide portions 71b are integrally formed on the surface 18a of the second separator 18. The plurality of second lead-out guide portions 71b guide the fuel gas (fuel exhaust gas) flowing in the fuel gas flow path 62 to each second lead-out connecting hole 69b. Each second lead-out guide portion 71b protrudes from the surface 18a of the second separator 18 toward the resin frame member 24. The second lead-out guide portion 71b extends from the fuel gas flow path 62 toward the inner portion 67b of the second connecting hole flange portion 70d.

[0066] The second outlet end of the second lead-out guide portion 71b near the second connecting hole flange portion 70d is separated from the inner portion 67b of the second connecting hole flange portion 70d. That is, there is a slight gap 75b between the second outlet end of the second lead-out guide portion 71b and the inner portion 67b of the second connecting hole flange portion 70d. The second outlet opening portion 73b facing the second lead-out connecting hole 69b is located at the second outlet end of the second lead-out guide portion 71b.

[0067] like Figure 2 , Figure 7 and Figure 8 As shown, the top 74 of the second sealing flange portion 68 (the second connecting hole flange portion 70 and the second flow path flange portion 72) contacts the other surface 24b of the resin frame member 24. In addition, a rubber sealing layer (not shown) may be provided between the top 74 and the other surface 24b of the resin frame member 24.

[0068] like Figure 1 As shown, the cooling medium flow path 76 is located between the surface 16b of the first separator 16 and the surface 18b of the second separator 18, which are joined to each other. The cooling medium flow path 76 connects the cooling medium supply passage 44a with the cooling medium discharge passage 44b. The cooling medium flow path 76 is formed by overlapping the back shape of the first separator 16 formed with the oxidant gas flow path 48 and the back shape of the second separator 18 formed with the fuel gas flow path 62.

[0069] In the above-mentioned fuel cell stack 12, the fluid flow path 78 includes the oxidant gas supply passage 42a, the oxidant gas passage 48, the oxidant gas discharge passage 42b, the fuel gas supply passage 46a, the fuel gas passage 62, the fuel gas discharge passage 46b, the cooling medium supply passage 44a, the cooling medium passage 76, and the cooling medium discharge passage 44b. The fluid as the reaction gas (oxidant gas and fuel gas) or the cooling medium for power generation flows in the fluid flow path 78.

[0070] The power generation cell 10 configured in this manner operates as follows.

[0071] First, if Figure 1 As shown, the oxidant gas is supplied to the oxidant gas supply passage 42a, the fuel gas is supplied to the fuel gas supply passage 46a, and the cooling medium is supplied to the cooling medium supply passage 44a.

[0072] The oxidant gas is introduced from the oxidant gas supply passage 42 a into the oxidant gas flow path 48 of the first separator 16 . The oxidant gas then moves in the direction of arrow B along the oxidant gas flow path 48 and is supplied to the first electrode 28 of the MEA 22 .

[0073] Meanwhile, the fuel gas is introduced from the fuel gas supply passage 46a into the fuel gas flow path 62 of the second separator 18. The fuel gas then moves in the direction of arrow B along the fuel gas flow path 62 and is supplied to the second electrode 30 of the MEA 22.

[0074] Therefore, in each MEA 22 , the oxidant gas supplied to the first electrode 28 and the fuel gas supplied to the second electrode 30 are consumed by electrochemical reactions in the first electrode catalyst layer 32 and the second electrode catalyst layer 36 . As a result, electric power is generated.

[0075] Then, if Figure 1 As shown in FIG. 1 , the oxidant gas supplied to the first electrode 28 and consumed flows from the oxidant gas flow path 48 toward the oxidant gas discharge passage 42b. Then, the oxidant gas is discharged in the direction of arrow A1 along the oxidant gas discharge passage 42b. Similarly, the fuel gas supplied to the second electrode 30 and consumed flows from the fuel gas flow path 62 toward the fuel gas discharge passage 46b. Then, the fuel gas is discharged in the direction of arrow A1 along the fuel gas discharge passage 46b.

[0076] In addition, the cooling medium supplied to the cooling medium supply passage 44a is introduced into the cooling medium flow path 76 formed between the first separator 16 and the second separator 18. After being introduced into the cooling medium flow path 76, the cooling medium flows in the direction of arrow B. After cooling the MEA 22, the cooling medium is discharged from the cooling medium discharge passage 44b.

[0077] In the power generation cell 10 as described above, when the power generation cell 10 is in operation, the adhesive 40a of the adhesive layer 40 adhered to one side of the resin frame member 24 is exposed to relatively high temperature and humidity. Therefore, the adhesive 40a softens. The softened adhesive 40a sometimes flows into the fluid flow path 78. Specifically, the softened adhesive 40a sometimes flows into the gap 65a and the gap 65b. The gap 65a is located between the inner part 57a of the first connecting hole flange part 56a and the first inlet end of the first introduction guide part 61a. The gap 65b is located between the inner part 57b of the first connecting hole flange part 56b and the first outlet end of the first outlet guide part 61b. As a result, the first introduction connecting hole 59a, the first inlet opening 63a, the first outlet connecting hole 59b and the first outlet opening 63b may be blocked by the adhesive 40a. In this case, since the pressure loss of the fluid flowing in the fluid flow path 78 increases, the power generation performance is reduced. In order to suppress such an increase in pressure loss in the fluid flow path 78 , it is necessary to appropriately select the binder 40 a that is unlikely to flow during operation of the power generation cell 10 .

[0078] Next, a description will be given of a method for selecting the binder 40a of the power generation cell 10. The binder 40a is exposed in the fluid flow path 78.

[0079] like Fig. 9 As shown, the method for selecting the adhesive 40a includes a laminate forming step, a load applying step, an exposing step, a measuring step, and a selecting step.

[0080] In the laminate forming process (step S1), Fig.10 As shown, a laminate 86 is formed by sandwiching an adhesive sheet 84 as an adhesive 84a between a first resin film 80 and a second resin film 82. The first resin film 80 and the second resin film 82 are, for example, the same resin material as the above-mentioned resin frame member 24. However, the constituent materials of the first resin film 80 and the second resin film 82 are not limited to the same resin material as the resin frame member 24, and can be appropriately set.

[0081] The first resin film 80 and the second resin film 82 have a rectangular (quadrilateral) shape. In addition, the shapes of the first resin film 80 and the second resin film 82 are not limited to quadrilaterals, and may be circular or polygonal (except for quadrilaterals). The plane size of the second resin film 82 is larger than the plane size of the first resin film 80.

[0082] The adhesive sheet 84 has the same plane size as the first resin film 80. The adhesive 84a may not be formed into a sheet in advance. That is, the adhesive 84a may be formed into a sheet by applying a liquid adhesive on one side of the first resin film 80. The adhesive 84a is a thermoplastic resin. As the resin material constituting the adhesive 84a, the same materials as the above-mentioned adhesive 40a can be listed.

[0083] Next, in the load application step ( Fig. 9 In step S2), as Fig.11A As shown, a compressive load in the stacking direction (thickness direction) is applied to the stacked body 86 obtained by the stacked body forming step. Specifically, in the load applying device, the first resin film 80 is pressed toward the second resin film 82 by the pressing member 202 while the second resin film 82 of the stacked body 86 is placed on the mounting table 200.

[0084] In addition, in the exposure process ( Fig. 9 In step S3), the laminate 86 is exposed to an environment heated to a predetermined temperature and humidified to a predetermined humidity. In addition, the exposure process and the load application process are performed simultaneously. That is, in this embodiment, a compressive load is applied to the laminate 86 in an environment heated to a predetermined temperature and humidified to a predetermined humidity. As a result, the adhesive 84a is softened and flows to the outside of the first resin film 80. In addition, the exposure process can also be performed after the load application process is performed.

[0085] In the exposure process, the prescribed temperature is set to, for example, a value corresponding to the temperature to which the adhesive 40a is subjected when the power generation cell 10 is in operation. Specifically, it is preferred that the prescribed temperature is set to, for example, 60°C or more and 120°C or less. However, the prescribed temperature may be set to a temperature higher than the temperature to which the adhesive 40a is subjected when the power generation cell 10 is in operation. The prescribed humidity is set to, for example, a value corresponding to the humidity to which the adhesive 40a is subjected when the power generation cell 10 is in operation. It is preferred that the prescribed humidity is set to, for example, 50% or more and 60% or less. However, the prescribed humidity may be set to a humidity higher than the humidity to which the adhesive 40a is subjected when the power generation cell 10 is in operation.

[0086] Next, in the measurement step ( Fig. 9 In step S4), as Fig. 11B As shown, the flow amount M of the adhesive 84a during the exposure process is measured. Specifically, in the measurement process, the overflow amount of the adhesive 84a overflowing from the periphery of the first resin film 80 (for example, the length overflowing from each side of the first resin film 80) is measured at multiple locations of the laminate 86, and the average value is used as the flow amount M of the adhesive 84a.

[0087] The flow amount M of the adhesive 84a can be appropriately specified. That is, in the measurement process, the maximum overflow length of the adhesive 84a overflowing from the outer periphery of the first resin film 80 can be measured as the flow amount M of the adhesive 84a. In addition, in the measurement process, the volume of the adhesive 84a overflowing from the outer periphery of the first resin film 80 can be measured as the flow amount M of the adhesive 84a. Moreover, in the measurement process, the area of ​​the adhesive 84a overflowing from the outer periphery of the first resin film 80 (the area of ​​the adhesive 84a overflowing from the outer periphery of the first resin film 80 when the stacked body 86 is observed from the stacking direction) can also be measured as the flow amount M of the adhesive 84a.

[0088] Then, in the selected process ( Fig. 9 In step S5), it is determined whether the flow amount M of the adhesive 84a measured in the measuring step is less than the predetermined amount M1. In this selection step, the adhesive 84a whose flow amount M is less than the predetermined amount M1 is selected as the adhesive 40a for the power generation cell 10. Fig.12 As shown, the predetermined amount M1 is set to a flow amount at which the pressure loss of the fluid caused by the adhesive 40 a flowing from the resin frame member 24 into the fluid flow path 78 during operation of the power generation cell 10 reaches the allowable upper limit value P1.

[0089] The permissible upper limit value P1 of the pressure loss is, for example, the upper limit value of the pressure loss that does not affect the power generation performance of the power generation cell 10 when the fluid (fuel gas, oxidant gas, and cooling medium) flows in the fluid flow path 78 at a specific flow rate. The above-mentioned specific flow rate is set so that the current density per unit area of ​​the MEA 22 reaches a specified value (for example, 2.5 A / cm 2 ) in a manner that allows the flow rate required for the operation of the power generation cell 10. The fact that the power generation performance of the power generation cell 10 is not affected also includes the fact that the impact on the power generation performance of the power generation cell 10 is so small that it can be ignored. When the selection process is completed, a series of action flows of the method for selecting the adhesive 40a are completed.

[0090] Next, a method for manufacturing the above-mentioned fuel cell stack 12 (power generation cell 10) will be described. Fig.13 As shown, the method for manufacturing the fuel cell stack 12 includes a bonding step, a processing step, a joining step, and a lamination step.

[0091] In the bonding process (step S10), Fig.14A As shown, an adhesive sheet 92 (hot melt adhesive) as the adhesive 40a is attached to one surface of the resin sheet 90. The resin sheet 90 is made of the same resin material as the resin frame member 24. The adhesive sheet 92 uses the adhesive 40a selected by the above-mentioned adhesive selection method.

[0092] In the present embodiment, the bonding step is performed by a roll-to-roll method. That is, the resin sheet 90 is pulled out from a first roll (not shown), and the adhesive sheet 92 is pulled out from a second roll (not shown), and the adhesive sheet 92 is attached to one surface of the resin sheet 90 .

[0093] However, in the bonding step, a single adhesive sheet 92 may be attached to one surface of a single resin sheet 90. In addition, in the bonding step, a liquid adhesive 40a may be applied to one surface of the resin sheet 90.

[0094] Next, in the processing step ( Fig.13 In step S11), as Fig. 14B As shown, a central hole 94 is formed in the central part of the resin sheet 90. In addition, an oxidant gas supply connecting hole 42a, a fuel gas discharge connecting hole 46b and a cooling medium supply connecting hole 44a are formed at one end edge of the resin sheet 90. Moreover, a fuel gas supply connecting hole 46a, a cooling medium discharge connecting hole 44b and an oxidant gas discharge connecting hole 42b are formed at the other end edge of the resin sheet 90. Finally, the periphery is trimmed. Thus, a resin frame component 24 having an adhesive layer 40 as an adhesive 40a adhered to one side is formed. In the processing step, a stamping die can also be used to simultaneously form the central hole 94, the oxidant gas supply connecting hole 42a, the fuel gas discharge connecting hole 46b, the cooling medium supply connecting hole 44a, the fuel gas supply connecting hole 46a, the cooling medium discharge connecting hole 44b and the oxidant gas discharge connecting hole 42b on the resin sheet 90.

[0095] In the bonding process ( Fig.13 In step S12), as Fig.15 As shown, a resin frame member 24 provided with an adhesive layer 40, a first electrode 28, an electrolyte membrane 26, and a second electrode 30 are prepared. In addition, the first electrode 28 is previously bonded to one surface 26a of the electrolyte membrane 26. Then, the inner peripheral portion 24i of the resin frame member 24 (the inner peripheral portion 40i of the adhesive layer 40) is arranged between the outer peripheral portion 26o of the electrolyte membrane 26 and the outer peripheral portion 30o of the second electrode 30 and joined to each other. At this time, the first electrode 28, the electrolyte membrane 26, the resin frame member 24, and the second electrode 30 overlapped in the thickness direction are heated and joined by hot pressing with a load.

[0096] Thus, the other surface 26b of the electrolyte membrane 26 and the second electrode 30 are bonded to each other to form the MEA 22 (see Figure 1 and Figure 2 ). In addition, the inner peripheral portion 40i of the adhesive layer 40 joins the outer peripheral portion 26o of the electrolyte membrane 26 and the inner peripheral portion 24i of the resin frame member 24 to each other. Thus, the MEA 14 with a resin frame is formed.

[0097] After that, in the lamination process ( Fig.13 In step S13), a plurality of MEAs 14 with resin frames and a plurality of bonded separators 20 are prepared. Each bonded separator 20 is a component formed by bonding a first separator 16 and a second separator 18 to each other. Then, as Fig.16 As shown in FIG. 1 , the MEA 14 with a resin frame and the bonding separators 20 are positioned and alternately stacked to form a plurality of power generation cells 10 (fuel cell stack 12). At this time, the top 60 of the first sealing flange portion 54 of the first separator 16 is in contact with the outer peripheral portion 40o of the adhesive layer 40 (see FIG. 1 ). Figure 2 , Figure 4 , Figure 5 , Figure 7 and Figure 8 ). That is, the outer peripheral portion 40 o of the adhesive layer 40 joins the top portion 60 of the first sealing flange portion 54 and the outer peripheral portion 24 o of the resin frame member 24 to each other.

[0098] In the fuel cell stack 12, terminal plates, insulators, and end plates (not shown) are arranged at both ends in the stacking direction, and a compressive load is applied in the stacking direction. When the stacking process is completed, the series of operation flow of the method for manufacturing the power generation cell 10 (fuel cell stack 12) is completed.

[0099] This embodiment achieves the following effects.

[0100] In the power generation cell 10, the adhesive 40a of the thermoplastic resin is provided in a manner exposed to the fluid flow path 78. In the method for selecting the adhesive 40a, a compressive load in the stacking direction is applied to a laminated body 86 formed by sandwiching the adhesive 84a between the first resin film 80 and the second resin film 82. In addition, in the method for selecting the adhesive 40a, the flow amount M of the adhesive 84a when the laminated body 86 is exposed to an environment heated to a predetermined temperature and humidified to a predetermined humidity is measured. Thus, the flow amount of the adhesive 84a in an environment close to the environment when the power generation cell 10 is in operation can be easily known. And, the adhesive whose measured flow amount M is less than the predetermined amount M1 is selected as the adhesive 40a for the power generation cell 10. According to this, the adhesive 40a that is not easy to soften and flow into the fluid flow path 78 when the power generation cell 10 is in operation can be easily selected.

[0101] In the power generation cell 10, the adhesive layer 40, which is the adhesive 40a selected by the above method, is adhered to one surface 24a of the resin frame member 24. Therefore, even when the top 60 of the first sealing flange portion 54 is brought into contact with the adhesive layer 40, the adhesive 40a is unlikely to flow into the fluid flow path 78 during operation of the power generation cell 10. Thus, it is possible to suppress an increase in the pressure loss of the fluid flowing in the fluid flow path 78 due to the adhesive 40a, thereby suppressing a decrease in power generation performance.

[0102] The adhesive 40a used for the power generation cell 10 is adhered to one surface 24a of the resin frame member 24 and the top 60 of the first sealing flange portion 54 is joined to the resin frame member 24. The first sealing flange portion 54 surrounds the fluid flow path 78 through which the fluid of the reaction gas or cooling medium for power generation flows to prevent leakage of the fluid. The first sealing flange portion 54 is integrally formed with the first separator 16 in a manner protruding toward the resin frame member 24. The predetermined amount M1 is set to a flow amount that causes the pressure loss of the fluid caused by the adhesive 40a flowing from the resin frame member 24 into the fluid flow path 78 when the power generation cell 10 is operated to reach the allowable upper limit value P1.

[0103] According to such a method, in the power generation cell 10 using the binder 40 a selected by this method, it is possible to effectively suppress an increase in the pressure loss of the fluid in the fluid flow path 78 during the operation of the power generation cell 10 .

[0104] The planar size of the second resin film 82 is larger than the planar size of the first resin film 80. In the laminate forming step, the adhesive 84a is sandwiched between the first resin film 80 and the second resin film 82 in a state where the adhesive 84a is adhered to one surface of the first resin film 80. In the measuring step, the amount of the adhesive 84a overflowing from the outer periphery of the first resin film 80 is measured as the flow amount M.

[0105] According to such a method, the flow amount M of the adhesive 40 a can be easily measured.

[0106] In the power generation cell 10 , the fluid flow path 78 has a communication hole (eg, the fuel gas supply communication hole 46 a ) penetrating the first separator 16 in the thickness direction. The first sealing flange portion 54 surrounds the communication hole.

[0107] According to such a structure, it is possible to effectively prevent the adhesive 40 a from flowing into the communicating holes and increasing the pressure loss during the operation of the power generation cell 10 .

[0108] In the above-described embodiment, the adhesive layer 40 as the adhesive 40 a may be provided on the other surface 24 b of the resin frame member 24 .

[0109] In addition, the present invention is not limited to the above-mentioned embodiment, and various structures can be adopted without departing from the scope of the present invention.

[0110] The above implementation modes are summarized as follows.

[0111] The above embodiment discloses a method for selecting an adhesive (40a), wherein the adhesive (40a) is a thermoplastic resin and is arranged in a manner exposed in a fluid flow path (78) of a power generation cell (10), and the selection method includes a stack formation process, a load application process, an exposure process, a measurement process and a selection process, wherein, in the stack formation process, a stack (86) is formed by sandwiching an adhesive (84a) between a first resin film (80) and a second resin film (82); in the load application process, a compressive load is applied to the stack in a stacking direction; in the exposure process, the stack is exposed to an environment heated to a specified temperature and humidified to a specified humidity; in the measurement process, the flow rate (M) of the adhesive during the exposure process is measured; in the selection process, the adhesive having a flow rate below a specified rate (M1) is selected as the adhesive for the power generation cell.

[0112] In the above-mentioned method for selecting an adhesive, the power generation cell may include an MEA (22), a resin frame member (24) and a partition, wherein the resin frame member (24) is mounted on the outer peripheral portion (22o) of the MEA in a manner protruding outward from the outer peripheral portion; the partition is made of metal and is adjacent to the MEA, and the partition has a fluid flow path (78) and a sealing flange portion (54), wherein the fluid flow path (78) is used to allow a fluid as a reaction gas or a cooling medium for power generation to flow therein; and the sealing flange portion (54) surrounds the fluid The sealing flange is integrally formed with the partition in a manner protruding toward the resin frame member, the adhesive used for the power generation cell is adhered to one side (24a) of the resin frame member and the top (60) of the sealing flange is joined to the resin frame member, and the specified amount is set to a flow amount that causes the pressure loss of the fluid to reach an allowable upper limit value (P1), wherein the pressure loss of the fluid refers to the pressure loss caused by the adhesive flowing from the resin frame member into the fluid flow path when the power generation cell is operating.

[0113] In the above-mentioned method for selecting the adhesive, the planar size of the second resin film may be larger than the planar size of the first resin film, and in the laminate forming step, the adhesive is sandwiched between the first resin film and the second resin film while being adhered to one side of the first resin film, and in the measuring step, the amount of the adhesive overflowing from the periphery of the first resin film is measured as the flow amount.

[0114] The above embodiment discloses a power generation cell, which has an MEA (14) with a resin frame and a group of metal separators (16, 18) arranged on both sides of the MEA with the resin frame, wherein the MEA (14) with a resin frame has an MEA and a resin frame component installed on the outer periphery of the MEA in a manner protruding outward from the outer periphery of the MEA, the MEA includes an electrolyte membrane (26) and a group of electrodes (28, 30) arranged on both sides of the electrolyte membrane, and the group of separators respectively have a fluid flow path and a sealing flange portion, wherein the fluid flow path is used to allow a reaction gas used for power generation or a cooling gas to flow through the electrolyte membrane. The fluid of the medium flows therein; the sealing flange portion surrounds the fluid flow path to prevent leakage of the fluid, the sealing flange portion is integrally formed with the partition in a manner of protruding toward the resin frame member, an adhesive layer (40) as an adhesive of a thermoplastic resin is adhered to one surface of the resin frame member, the inner peripheral portion of the adhesive layer joins the outer peripheral portion (26o) of the electrolyte membrane to the inner peripheral portion of the resin frame member, and the outer peripheral portion of the adhesive layer joins the top of the sealing flange portion to the outer peripheral portion of the resin frame member, and the adhesive is an adhesive selected by the above-mentioned adhesive selection method.

[0115] In the above power generation cell, the fluid flow path may include a communication hole (42a, 42b, 44a, 44b, 46a, 46b) penetrating the separator in the thickness direction, and the sealing flange portion may extend to surround the communication hole.

Claims

1. A method for selecting an adhesive, wherein the adhesive is a thermoplastic resin and is disposed in a manner exposed to a fluid flow path of a power generation cell, It is characterized in that The method comprises a stacking body forming step, a load applying step, an exposing step, a measuring step and a selecting step, wherein: In the laminate forming step, a laminate is formed by sandwiching an adhesive between a first resin film and a second resin film; In the load applying step, a compressive load in a stacking direction is applied to the stacked body; In the exposing step, the laminate is exposed to an environment heated to a predetermined temperature and humidified to a predetermined humidity; In the measuring step, a flow amount of the adhesive that flows by performing the exposing step and the load applying step is measured; In the selecting step, the binder having the flow amount being equal to or less than a predetermined amount is selected as the binder to be used in the power generation cell.

2. The method for selecting an adhesive according to claim 1, characterized in that: The power generation cell comprises an MEA, a resin frame member and a separator, wherein: The resin frame member is mounted on the outer peripheral portion of the MEA in a manner protruding outward from the outer peripheral portion of the MEA; The separator is made of metal and is adjacent to the MEA. The partition plate has a fluid flow path and a sealing flange portion, wherein: The fluid flow path is used to allow a fluid serving as a reaction gas or a cooling medium for power generation to flow therein; The sealing flange portion surrounds the fluid flow path to prevent leakage of the fluid. The sealing flange portion is integrally formed with the partition plate in a manner protruding toward the resin frame member. The adhesive for the power generation cell is adhered to one side of the resin frame member and the top of the sealing flange portion is bonded to the resin frame member. The predetermined amount is set to a flow amount that causes a pressure loss of the fluid to reach an allowable upper limit value, wherein the pressure loss of the fluid is a pressure loss caused by the adhesive flowing from the resin frame member into the fluid flow path when the power generation cell is operated.

3. The method for selecting an adhesive according to claim 1, characterized in that: The second resin film has a larger plane size than the first resin film. In the laminate forming step, the adhesive is adhered to one surface of the first resin film and the adhesive is sandwiched between the first resin film and the second resin film. In the measuring step, the amount of the adhesive protruding from the outer periphery of the first resin film is measured as the flow amount.