A high-hardness paperboard without cracking production process

Through the crushing, stirring and hot pressing treatment steps, the cracking problem caused by uneven stress in cardboard production is solved, and the production of high-hardness crack-free cardboard is achieved, and the performance and quality of cardboard is improved.

CN115125771BActive Publication Date: 2024-11-26ZHENGYE INT HLDG CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202210878965.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-25
Publication Date
2024-11-26
Estimated Expiration
2042-07-25

AI Technical Summary

Technical Problem

There is a phenomenon of tensile box folding and breaking during the production process of existing cardboard, resulting in uneven stress on the cardboard folding box, prone to cracking, and reducing the performance of the cardboard.

Method used

Adopt high-hardness cardboard crack-free production process, including crushing, stirring, embryo formation and hot pressing treatment steps, by crushing straw, mixing with water and materials, removing bubbles, hot pressing molding in a hot press box, adjusting pressure and temperature. Ensure uniform molding of the cardboard.

Benefits of technology

It improves the hardness and strength of the cardboard, avoids cracking, enhances the quality and toughness of the cardboard, and simplifies the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115125771B_ABST
    Figure CN115125771B_ABST
Patent Text Reader

Abstract

This invention discloses a crack-free production process for high-hardness cardboard, comprising the following steps: Crushing: Crushing straw; Mixing: Adding materials and water to the crushed straw and mixing them thoroughly; Forming: Applying a release cloth to the bottom of the hot press chamber and another release cloth to the bottom of the pressing plate; Passing the mixed slurry into the cavity formed by the pressing plate and the bottom of the hot press chamber; Hot pressing: Hot pressing the slurry in the cavity, then slowly raising the pressing plate to separate it from the formed cardboard; Subsequent processing: After the cardboard cools to room temperature, opening the sealing plate and quickly removing the formed cardboard through the discharge port; Pressing with a heavy object for 1-2 hours to obtain the formed cardboard. This invention removes air bubbles by having the scraper below the scraper contact the slurry, thereby increasing the cardboard's hardness and preventing cracking after forming.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of paperboard production, and in particular to a high-hardness paperboard without cracking production process. Background Art

[0002] Cardboard is a thick paper sheet made of various pulps and interwoven with fibers. The difference between cardboard and paper is usually based on the basis weight and thickness. Generally, cardboard is defined as paper with a basis weight of more than 200g / ㎡ and a thickness greater than 0.5mm. Cardboard is mainly used for packaging cartons, packaging materials or printing materials.

[0003] During the current cardboard production process, some places are stretched and folded, and some places are broken. This causes different stresses in the folded and folded parts of the cardboard, resulting in different strengths. There are hidden scratches inside the loaded cardboard, which will cause wrinkles and breaks, and cracks in the cardboard, resulting in reduced performance of the cardboard. Summary of the invention

[0004] The purpose of the present invention is to provide a high-hardness paperboard without cracking production process to solve the following technical problems:

[0005] During the current production process of cardboard, some parts are stretched and folded, and some parts are broken, which causes different stresses in the folded parts of the cardboard folding box, resulting in different strengths.

[0006] The purpose of the present invention can be achieved through the following technical solutions:

[0007] A high-hardness paperboard crack-free production process comprises the following steps:

[0008] S1. Crushing: crush the straw to a particle size of 20-40 mesh;

[0009] S2, stirring treatment: adding the material and water to the crushed straw, mixing the three evenly, and the stirring treatment time is 20-40 minutes;

[0010] S3, embryo processing: stick a layer of release cloth on the bottom of the hot press box, and also stick a layer of release cloth under the pressing plate, and pass the mixed slurry into the cavity formed by the pressing plate and the bottom of the hot press box;

[0011] S4, hot pressing treatment: hot pressing treatment is performed on the slurry in the cavity, the hot pressing time is 10-30 minutes, the pressure is maintained for 4-7 minutes, and then the pressing plate is slowly lifted to separate the pressing plate from the formed paperboard. The hot pressing temperature in the hot pressing treatment is 100°C;

[0012] S5. Subsequent processing: After the paperboard is cooled to room temperature, the sealing plate is opened, the formed paperboard is quickly taken out through the discharge port, and pressed with a heavy object for 1-2 hours to obtain the formed paperboard.

[0013] Preferably, the crushing process in step S1 is as follows:

[0014] S11, adding the straw into the crushing chamber of the processing cylinder through the feed port;

[0015] S12, starting the driving motor, which drives the crushing blades to rotate through the rotating rod, and the crushing blades crush the straw, and the crushed straw particles fall through the sieve holes under the action of gravity.

[0016] Preferably, the stirring process in step S2 is as follows:

[0017] S22, the crushed straw falls into the mixing chamber, external water is transported to the rotating shaft through the water inlet pipe, water is sprayed into the mixing chamber through the spray hole, and the material is transported into the mixing chamber through the feed pipe;

[0018] S23, the rotating rod drives the main gear to rotate through the belt and the pulley during the rotation process, and the main gear drives the rotating shaft and the stirring rod to rotate through the sub-gear, thereby mixing water, materials and straw particles to form slurry;

[0019] S24, when the slurry is mixed, the main gear drives the scraper to move horizontally in the mixing chamber by meshing with the rack plate during rotation, and the scraper hairs arranged under the scraper come into contact with the slurry to remove bubbles;

[0020] S25. Open the control valve, and the slurry falls from the discharge port into the static box. After static treatment for 30-50 minutes, open the valve to transport the slurry into the cavity through the discharge pipe.

[0021] Preferably, the hot pressing process in step S4 is as follows:

[0022] S41, start the cylinder to push the pressing plate down to press the slurry evenly, and the hot pressing pressure is 1.2-1.8MP;

[0023] S42, starting the heater to perform hot pressing molding on the slurry.

[0024] Preferably, the material comprises the following raw materials in parts by weight: 20-30 parts of calcium carbonate, 40-50 parts of polypropylene resin, 20-30 parts of starch, 10-15 parts of bone glue, 2-7 parts of plasticizer and 3-6 parts of toughening agent.

[0025] Preferably, the plasticizer is diisopropyl 1,2-cyclohexanedicarboxylate;

[0026] Preferably, the toughening agent is polyoxypropylene glyceryl ether.

[0027] Preferably, the weight ratio of the straw, material and water is 2:1:10.

[0028] Beneficial effects of the present invention:

[0029] (1) The present invention provides a defoaming mechanism. When the slurry is mixed, the main gear drives the scraper to move horizontally in the mixing chamber by meshing with the rack plate during rotation. The scraper hairs arranged under the scraper contact the slurry to remove bubbles, thereby improving the hardness of the paperboard and preventing cracking of the paperboard after forming.

[0030] (2) The present invention adjusts the pressure of the pressing plate through the cylinder, thereby increasing the stress and strength of the paperboard, achieving crack-free production, simple production process, soft and tough paper, and improving the quality of the paperboard. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] The present invention will be further described below in conjunction with the accompanying drawings.

[0032] Figure 1 This is a three-dimensional structure diagram of a processing box in a high-hardness paperboard crack-free production process of the present invention. Figure 1 ;

[0033] Figure 2 This is a three-dimensional structure diagram of a processing box in a high-hardness paperboard crack-free production process of the present invention. Figure 2 ;

[0034] Figure 3 It is a structural schematic diagram of a processing cylinder in a high-hardness paperboard crack-free production process of the present invention;

[0035] Figure 4 The present invention is a schematic structural diagram of a hot press box in a high-hardness paperboard crack-free production process.

[0036] In the figure: 1. processing box; 2. driving motor; 3. static box; 4. hot press box; 5. feeding pipe; 6. processing cylinder; 7. mixing chamber; 101. feeding port; 102. working table; 201. belt; 301. discharge pipe; 401. heater; 402. cylinder; 403. discharge port; 404. pressing plate; 405. cavity; 601. crushing chamber; 602. crushing blade; 603. rotating rod; 604. sieve hole; 605. sieve plate; 701. water inlet pipe; 702. rotating shaft; 703. stirring rod; 704. sub gear; 705. main gear; 706. scraper; 707. scraper; 708. slide plate; 709. discharge port; 710. control valve; 711. rack plate; 712. spray hole. DETAILED DESCRIPTION

[0037] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example 1

[0038] The present invention is a high-hardness paperboard crack-free production process, comprising the following steps:

[0039] S1. Crushing: crush the straw to a particle size of 20 mesh;

[0040] S2, stirring treatment: adding the material and water to the crushed straw, mixing the three evenly, and the stirring treatment time is 20 minutes;

[0041] S3, embryo processing: a layer of demoulding cloth is pasted on the bottom of the hot press box 4, and a layer of demoulding cloth is also pasted under the pressing plate 404, and the mixed slurry is passed into the cavity 405 formed by the pressing plate 404 and the hot press box 4;

[0042] S4, hot pressing treatment: hot pressing treatment is performed on the slurry in the cavity 405, the hot pressing time is 10 minutes, the pressure is maintained for 4 minutes, and then the pressing plate 404 is slowly raised to separate the pressing plate 404 from the formed paperboard, and the hot pressing temperature in the hot pressing treatment is 100°C;

[0043] S5, subsequent processing: After the paperboard is cooled to room temperature, the sealing plate is opened, the formed paperboard is quickly taken out through the discharge port 403, and pressed with a heavy object for 1 hour to obtain the formed paperboard.

[0044] The crushing process in step S1 is as follows:

[0045] S11, adding the straw into the crushing chamber 601 of the processing cylinder 6 through the feed port 101;

[0046] S12, start the driving motor 2, the driving motor 2 drives the crushing blade 602 to rotate through the rotating rod 603, the crushing blade 602 crushes the straw, and the crushed straw particles fall through the sieve hole 604 under the action of gravity.

[0047] The stirring process in step S2 is as follows:

[0048] S22, the crushed straw falls into the mixing chamber 7, the external water is transported to the rotating shaft 702 through the water inlet pipe 701, the water is sprayed into the mixing chamber 7 through the spray hole 712, and the material is transported into the mixing chamber 7 through the feed pipe 5;

[0049] S23, the rotating rod 603 drives the main gear 705 to rotate through the belt 201 and the pulley during the rotation process, and the main gear 705 drives the rotating shaft 702 and the stirring rod 703 to rotate through the sub-gear 704, thereby mixing water, materials and straw particles to form slurry;

[0050] S24, when the slurry is mixed, the main gear 705 drives the scraper 706 to move horizontally in the mixing chamber 7 by meshing with the rack plate 711 during the rotation process, and the scraper 707 arranged under the scraper 706 contacts the slurry to remove the bubbles;

[0051] S25, open the control valve 710, the slurry falls from the discharge port 709 into the static box 3, and after being statically treated for 30-50 minutes, open the valve to transport the slurry into the cavity 405 through the discharge pipe 301;

[0052] The hot pressing process in step S4 is as follows:

[0053] S41, start the cylinder 402 to push the pressing plate 404 downward to press the slurry evenly, and the hot pressing pressure is 1.2MP;

[0054] S42, start the heater 401 to perform hot pressing molding on the slurry.

[0055] The material includes the following raw materials in parts by weight: 20 parts of calcium carbonate, 40 parts of polypropylene resin, 20 parts of starch, 10 parts of bone glue, 2 parts of plasticizer and 3 parts of toughening agent.

[0056] The plasticizer is diisopropyl 1,2-cyclohexanedicarboxylate; and the toughening agent is polyoxypropylene glycerol ether.

[0057] The weight ratio of the straw, the material and the water is 2:1:10.

[0058] See also Figure 1 As shown, a processing cylinder 6 is arranged in the processing box 1, and a feeding port 101 connected to the processing cylinder 6 is arranged on the top of the processing box 1. A crushing chamber 601 for crushing straw is arranged above the processing cylinder 6, and a rotating rod 603 is rotatably arranged in the crushing chamber 601. A plurality of groups of crushing blades 602 are evenly arranged on the rotating rod 603. The rotating rod 603 is fixedly connected to the output end of the driving motor 2 arranged outside the processing box 1;

[0059] A sieve plate 605 for screening straw is provided at the bottom of the crushing chamber 601, and a plurality of sieve holes 604 are evenly provided on the sieve plate 605;

[0060] The straw is added into the crushing chamber 601 of the processing cylinder 6 through the feed port 101, and the driving motor 2 is started. The driving motor 2 drives the crushing blade 602 to rotate through the rotating rod 603, and the crushing blade 602 crushes the straw. The crushed straw particles fall through the sieve hole 604 under the action of gravity;

[0061] See also Figure 2 A mixing chamber 7 is arranged below the crushing chamber 601, a rotating shaft 702 is arranged in the mixing chamber 7, stirring rods 703 for mixing and stirring the materials are evenly arranged on the rotating shaft 702, the rotating rod 603 is connected to the main gear 705 arranged in the mixing chamber 7 through the belt 201 and the pulley, and the end of the rotating shaft 702 is fixedly connected to a sub-gear 704 meshing with the main gear 705;

[0062] A feed pipe 5 for adding mixed materials is arranged on one side of the mixing chamber 7, and a water inlet pipe 701 is rotatably connected to the end of the rotating shaft 702, wherein the rotating shaft 702 is a hollow structure, and a plurality of groups of spray holes 712 are evenly arranged on the rotating shaft 702;

[0063] See also Figure 3 The crushed straw falls into the mixing chamber 7, and the external water is transported to the rotating shaft 702 through the water inlet pipe 701, and the water is sprayed into the mixing chamber 7 through the spray hole 712. The material is transported into the mixing chamber 7 through the feeding pipe 5. The rotating shaft 702 drives the main gear 705 to rotate through the belt 201 and the pulley during the rotation process. The main gear 705 drives the rotating shaft 702 and the stirring rod 703 to rotate through the sub-gear 704, thereby mixing the water, the material and the straw particles to form a slurry;

[0064] See also Figure 4 A defoaming mechanism is also provided in the mixing chamber 7. The defoaming mechanism includes a scraper 706 arranged above the mixing chamber 7. A plurality of scraper bristles 707 are evenly arranged below the scraper 706. A rack plate 711 meshing with the main gear 705 is fixedly installed at the end of the scraper 706. The rack plate 711 is slidably connected to a slide plate 708 fixedly installed on one side of the mixing chamber 7.

[0065] When water, materials and straw particles are mixed to form slurry, bubbles are easily generated. The existence of bubbles not only affects the aesthetics of the paperboard after forming, but also seriously affects the strength and quality of the paperboard. The present invention provides a defoaming mechanism. When the slurry is mixed, the main gear 705 drives the scraper 706 to move horizontally in the mixing chamber 7 by meshing with the rack plate 711 during the rotation process. The scraper 707 arranged under the scraper 706 contacts the slurry to remove the bubbles.

[0066] A discharge port 709 is provided at the bottom of the mixing chamber 7, a control valve 710 is provided between the discharge ports 709, and a static box 3 is arranged at the bottom of the processing box body 1, and the static box 3 is used to statically store the slurry discharged from the discharge port 709;

[0067] A workbench 102 is arranged on one side of the processing box 1, a hot press box 4 is arranged on the workbench 102, a heater 401 is arranged on the hot press box 4, a pressing plate 404 is arranged in the hot press box 4, the pressing plate 404 is fixedly connected to a cylinder 402 arranged on the top of the hot press box 4, the pressing plate 404 and the bottom wall of the hot press box 4 are enclosed to form a cavity 405 for hot pressing the slurry, one end of the cavity 405 is connected to the static box 3 through a discharge pipe 301, and a discharge port 403 is arranged at the other end, a sealing plate is rotatably arranged in the discharge port 403, and a valve is arranged between the discharge pipe 301;

[0068] After the slurry is left to stand in the still box 3 for a period of time, the valve is opened to transport the slurry to the cavity 405 through the discharge pipe 301, and then the cylinder 402 pushes the pressing plate 404 downward to press the slurry evenly, and the heater 401 is started to hot-press the slurry, and the formed paperboard is discharged from the discharge port 403; the present invention adjusts the pressure of the pressing plate 404 by the cylinder 402, thereby increasing the stress and strength of the paperboard, achieving crack-free production, simple production process, soft and tough paper, and improving the quality of the paperboard. Example 2

[0069] A high-hardness paperboard crack-free production process comprises the following steps:

[0070] S1. Crushing: crush the straw to a particle size of 30 mesh;

[0071] S2, stirring treatment: adding the material and water to the crushed straw, mixing the three evenly, and the stirring treatment time is 30 minutes;

[0072] S3, embryo processing: a layer of demoulding cloth is pasted on the bottom of the hot press box 4, and a layer of demoulding cloth is also pasted under the pressing plate 404, and the mixed slurry is passed into the cavity 405 formed by the pressing plate 404 and the hot press box 4;

[0073] S4, hot pressing treatment: hot pressing treatment is performed on the slurry in the cavity 405, the hot pressing time is 20 minutes, the pressure is maintained for 6 minutes, and then the pressing plate 404 is slowly raised to separate the pressing plate 404 from the formed paperboard. The hot pressing temperature in the hot pressing treatment is 100°C;

[0074] S5, subsequent processing: After the paperboard is cooled to room temperature, the sealing plate is opened, the molded paperboard is quickly taken out through the discharge port 403, and pressed with a heavy object for 1.5 hours to obtain the molded paperboard.

[0075] The crushing process in step S1 is as follows:

[0076] S11, adding the straw into the crushing chamber 601 of the processing cylinder 6 through the feed port 101;

[0077] S12, start the driving motor 2, the driving motor 2 drives the crushing blade 602 to rotate through the rotating rod 603, the crushing blade 602 crushes the straw, and the crushed straw particles fall through the sieve hole 604 under the action of gravity.

[0078] The stirring process in step S2 is as follows:

[0079] S22, the crushed straw falls into the mixing chamber 7, the external water is transported to the rotating shaft 702 through the water inlet pipe 701, the water is sprayed into the mixing chamber 7 through the spray hole 712, and the material is transported into the mixing chamber 7 through the feed pipe 5;

[0080] S23, the rotating rod 603 drives the main gear 705 to rotate through the belt 201 and the pulley during the rotation process, and the main gear 705 drives the rotating shaft 702 and the stirring rod 703 to rotate through the sub-gear 704, thereby mixing water, materials and straw particles to form slurry;

[0081] S24, when the slurry is mixed, the main gear 705 drives the scraper 706 to move horizontally in the mixing chamber 7 by meshing with the rack plate 711 during the rotation process, and the scraper 707 arranged under the scraper 706 contacts the slurry to remove the bubbles;

[0082] S25, open the control valve 710, the slurry falls from the discharge port 709 into the static box 3, and after being statically treated for 40 minutes, open the valve to transport the slurry into the cavity 405 through the discharge pipe 301;

[0083] The hot pressing process in step S4 is as follows:

[0084] S41, start the cylinder 402 to push the pressing plate 404 downward to press the slurry evenly, and the hot pressing pressure is 1.2MP;

[0085] S42, start the heater 401 to perform hot pressing molding on the slurry.

[0086] The material includes the following raw materials in parts by weight: 25 parts of calcium carbonate, 45 parts of polypropylene resin, 25 parts of starch, 13 parts of bone glue, 4 parts of plasticizer and 4 parts of toughening agent.

[0087] The plasticizer is diisopropyl 1,2-cyclohexanedicarboxylate; and the toughening agent is polyoxypropylene glycerol ether.

[0088] The weight ratio of the straw, the material and the water is 2:1:10. Example 3

[0089] A high-hardness paperboard crack-free production process comprises the following steps:

[0090] S1. Crushing: crush the straw to a particle size of 40 mesh;

[0091] S2, stirring treatment: adding the material and water to the crushed straw, mixing the three evenly, and the stirring treatment time is 40 minutes;

[0092] S3, embryo processing: a layer of demoulding cloth is pasted on the bottom of the hot press box 4, and a layer of demoulding cloth is also pasted under the pressing plate 404, and the mixed slurry is passed into the cavity 405 formed by the pressing plate 404 and the hot press box 4;

[0093] S4, hot pressing treatment: hot pressing treatment is performed on the slurry in the cavity 405, the hot pressing time is 30 minutes, the pressure is maintained for 7 minutes, and then the pressing plate 404 is slowly raised to separate the pressing plate 404 from the formed paperboard, and the hot pressing temperature in the hot pressing treatment is 100°C;

[0094] S5, subsequent processing: After the paperboard is cooled to room temperature, the sealing plate is opened, the formed paperboard is quickly taken out through the discharge port 403, and pressed with a heavy object for 2 hours to obtain the formed paperboard.

[0095] The crushing process in step S1 is as follows:

[0096] S11, adding the straw into the crushing chamber 601 of the processing cylinder 6 through the feed port 101;

[0097] S12, start the driving motor 2, the driving motor 2 drives the crushing blade 602 to rotate through the rotating rod 603, the crushing blade 602 crushes the straw, and the crushed straw particles fall through the sieve hole 604 under the action of gravity.

[0098] The stirring process in step S2 is as follows:

[0099] S22, the crushed straw falls into the mixing chamber 7, the external water is transported to the rotating shaft 702 through the water inlet pipe 701, the water is sprayed into the mixing chamber 7 through the spray hole 712, and the material is transported into the mixing chamber 7 through the feed pipe 5;

[0100] S23, the rotating rod 603 drives the main gear 705 to rotate through the belt 201 and the pulley during the rotation process, and the main gear 705 drives the rotating shaft 702 and the stirring rod 703 to rotate through the sub-gear 704, thereby mixing water, materials and straw particles to form slurry;

[0101] S24, when the slurry is mixed, the main gear 705 drives the scraper 706 to move horizontally in the mixing chamber 7 by meshing with the rack plate 711 during the rotation process, and the scraper 707 arranged under the scraper 706 contacts the slurry to remove the bubbles;

[0102] S25, open the control valve 710, the slurry falls from the discharge port 709 into the static box 3, and after being statically treated for 30-50 minutes, open the valve to transport the slurry into the cavity 405 through the discharge pipe 301;

[0103] The hot pressing process in step S4 is as follows:

[0104] S41, start the cylinder 402 to push the pressing plate 404 downward to press the slurry evenly, and the hot pressing pressure is 1.2-1.8MP;

[0105] S42, start the heater 401 to perform hot pressing molding on the slurry.

[0106] The material includes the following raw materials in parts by weight: 30 parts of calcium carbonate, 50 parts of polypropylene resin, 30 parts of starch, 15 parts of bone glue, 7 parts of plasticizer and 6 parts of toughening agent.

[0107] The plasticizer is diisopropyl 1,2-cyclohexanedicarboxylate; and the toughening agent is polyoxypropylene glycerol ether.

[0108] The weight ratio of the straw, the material and the water is 2:1:10.

[0109] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, and a specific direction structure and operation, and therefore, cannot be understood as a limitation of the present invention. In addition, "first" and "second" are only for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.

[0110] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", etc. should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0111] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.

Claims

1. A high-hardness paperboard crack-free production process, characterized in that: The steps include: S1. Crushing: crush the straw to a particle size of 20-40 mesh; S2, stirring treatment: adding the material and water to the crushed straw, mixing the three evenly, and the stirring treatment time is 20-40 minutes; S3, embryo processing: a layer of demoulding cloth is pasted on the bottom of the hot press box (4), and a layer of demoulding cloth is also pasted under the pressing plate (404), and the mixed slurry is passed into the cavity (405) formed by the pressing plate (404) and the bottom of the hot press box (4); S4, hot pressing treatment: hot pressing treatment is performed on the slurry in the cavity (405), the hot pressing time is 10-30 minutes, the pressure is maintained for 4-7 minutes, and then the pressing plate (404) is slowly lifted to separate the pressing plate (404) from the formed paperboard, and the hot pressing temperature in the hot pressing treatment is 100° C.; S5, subsequent processing: after the paperboard is cooled to room temperature, the sealing plate is opened, the formed paperboard is quickly taken out through the discharge port (403), and pressed with a heavy object for 1-2 hours to obtain the formed paperboard; The crushing process in step S1 is as follows: S11, adding straw into the pulverizing chamber (601) of the processing cylinder (6) through the feed inlet (101); S12, starting the driving motor (2), the driving motor (2) drives the crushing blades (602) to rotate via the rotating rod (603), the crushing blades (602) crush the straw, and the crushed straw particles fall through the sieve holes (604) under the action of gravity; The stirring process in step S2 is as follows: S22, the crushed straw falls into the mixing chamber (7), external water is transported to the rotating shaft (702) through the water inlet pipe (701), the water is sprayed into the mixing chamber (7) through the spray hole (712), and the material is transported into the mixing chamber (7) through the feed pipe (5); S23, the rotating rod (603) drives the main gear (705) to rotate via the belt (201) and the pulley during the rotation process, and the main gear (705) drives the rotating shaft (702) and the stirring rod (703) to rotate via the sub-gear (704), thereby mixing water, materials and straw particles to form slurry; S24, when the slurry is mixed, the main gear (705) drives the scraper (706) to move horizontally in the mixing chamber (7) by meshing with the rack plate (711) during rotation, and the scraper (707) arranged below the scraper (706) contacts the slurry to remove bubbles; S25, opening the control valve (710), allowing the slurry to fall from the discharge port (709) into the static box (3), and after being statically treated for 30-50 minutes, opening the valve to transport the slurry into the mold cavity (405) through the discharge pipe (301); The processing cylinder (6) is arranged in the processing box (1), and a feeding port (101) connected to the processing cylinder (6) is arranged at the top of the processing box (1). A crushing chamber (601) for crushing straw is arranged at the top of the processing cylinder (6), and a rotating rod (603) is rotatably arranged in the crushing chamber (601). A plurality of groups of crushing blades (602) are evenly arranged on the rotating rod (603), and the rotating rod (603) is fixedly connected to the output end of a driving motor (2) arranged outside the processing box (1); A sieve plate (605) for screening straw is provided at the bottom of the grinding chamber (601), and a plurality of groups of sieve holes (604) are evenly arranged on the sieve plate (605); A mixing chamber (7) is arranged below the pulverizing chamber (601), a rotating shaft (702) is arranged in the mixing chamber (7), stirring rods (703) for mixing and stirring materials are evenly arranged on the rotating shaft (702), the rotating rods (603) are connected to a main gear (705) rotatably arranged in the mixing chamber (7) via a belt (201) and a pulley, and a secondary gear (704) meshing with the main gear (705) is fixedly connected to the end of the rotating shaft (702); A feed pipe (5) for adding mixed materials is arranged on one side of the mixing chamber (7), and a water inlet pipe (701) is rotatably connected to the end of the rotating shaft (702), wherein the rotating shaft (702) is a hollow structure, and a plurality of groups of spray holes (712) are evenly arranged on the rotating shaft (702); A defoaming mechanism is also provided in the mixing chamber (7), the defoaming mechanism comprising a scraper (706) arranged at the top of the mixing chamber (7), a plurality of groups of scraping hairs (707) evenly arranged below the scraper (706), a rack plate (711) meshing with the main gear (705) fixedly mounted at the end of the scraper (706), the rack plate (711) being slidably connected to a slide plate (708) fixedly mounted on one side of the mixing chamber (7).

2. A high-hardness paperboard crack-free production process according to claim 1, characterized in that: The hot pressing process in step S4 is as follows: S41, start the cylinder (402) to push the pressing plate (404) downward to press the slurry evenly, and the hot pressing pressure is 1.2-1.8MP; S42, starting the heater (401) to perform hot pressing molding on the slurry.

3. The high-hardness paperboard crack-free production process according to claim 1, characterized in that: The material comprises the following raw materials in parts by weight: 20-30 parts of calcium carbonate, 40-50 parts of polypropylene resin, 20-30 parts of starch, 10-15 parts of bone glue, 2-7 parts of plasticizer and 3-6 parts of toughening agent.

4. A high-hardness paperboard crack-free production process according to claim 3, characterized in that: The plasticizer is diisopropyl 1,2-cyclohexanedicarboxylate.

5. The high-hardness paperboard crack-free production process according to claim 3, characterized in that: The toughening agent is polyoxypropylene glyceryl ether.

6. The high-hardness paperboard crack-free production process according to claim 1, characterized in that: The weight ratio of the straw, the material and the water is 2:1:10.

Citation Information

Patent Citations

  • High-abrasion resistance paperboard and production technology thereof

    CN105401483A

  • Straw ecological plastic master batch and preparation method thereof

    CN107722433A

  • High-performance paperboard non-cracking production process

    CN109333955A

  • Straw processing and recycling treatment method and treatment system

    CN111922052A

  • Agricultural straw crushing device

    CN211430147U