Integrated titanium dioxide nanomaterial microfluidic chip and its preparation and application
By integrating a titanium dioxide nanomaterial microfluidic chip and using electrospray-electrospinning technology to prepare a microchannel structure, the problem of sEVs separation is solved and efficient, fast, and low-cost extracellular vesicle capture and separation is achieved, which is suitable for early diagnosis of cancer. and treatment monitoring.
Patent Information
- Application Number
- CN202210962828.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-11
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-08-11
AI Technical Summary
It is difficult to efficiently separate and enrich low-content extracellular vesicles (sEVs) with existing technology, especially in trace samples. Traditional methods have long processing times, low purity, and risk of damage.
Using an integrated titanium dioxide nanomaterial microfluidic chip, single-sided concave TiO2 nanospheres or fibers are prepared through electrospray-electrospinning technology, and combined with microchannel templates to form microchannels with a convex structure to achieve efficient capture and separation of sEVs, and Modifications such as antibodies and aptamers can be made to specifically capture pathogens.
It achieves fast, simple, and efficient separation and enrichment of sEVs, reduces experimental costs and reagent consumption, does not require large instruments, improves capture efficiency, and supports subsequent nucleic acid analysis.
Smart Images

Figure CN115318349B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of electrospray-electrospinning technology and microfluidic technology, and more specifically, relates to an integrated titanium dioxide nanomaterial microfluidic chip and its preparation and application. Background Art
[0002] The use of electrohydrodynamic jet technology to prepare monodisperse micro / nano particles and ultrafine fibers has become one of the research hotspots. According to the different morphologies of the products, electrostatic jet can be divided into two forms: electrospraying and electrospinning. The former can prepare monodisperse micro / nano particles, while the latter can prepare continuous nanofibers. At present, electrospray-electrospinning technology has broad application prospects in many fields such as high-performance adsorption, protection, filtration, and biomedicine.
[0003] As one of the main markers of "liquid biopsy", sEVs are one of the current research hotspots. Due to the high content of sEVs and their continued presence in all physiological and disease stages, and the inherent stability of sEVs that ensures the integrity of the biological molecules they carry, sEVs have received widespread attention in the early diagnosis of cancer and monitoring of cancer treatment efficacy. If sEVs are to be used for early diagnosis of cancer and monitoring of cancer recurrence, sEVs must first be separated from biological samples with complex matrices for subsequent analysis. At present, a variety of technologies have been developed for the separation of sEVs. Although traditional sEVs separation methods are widely used in scientific research, they cannot handle trace samples, have long processing times, have low purity of sEVs, and have the risk of sEVs being damaged. Microfluidics technology provides a new technical platform for the separation of sEVs from trace samples, in which micron or nano-fabricated channels and structures can be used to handle small amounts of liquid. This method has unique advantages, including low reagent and sample consumption, fast separation and analysis speed, and miniaturized integration. Therefore, microfluidic technology is increasingly being used for the rapid separation and analysis of sEVs to achieve the purpose of early diagnosis of cancer and monitoring of recurrence after treatment. Summary of the invention
[0004] The present invention solves the technical difficulties in separating and enriching low-content sEVs from specimens in the prior art, and provides a simple method for preparing and using a titanium dioxide nanomaterial microfluidic chip for extracellular vesicle separation and downstream nucleic acid analysis. The device is small in size and can be manufactured in batches. The method is simple, fast, efficient, and low in cost. It does not require modification of antibodies, aptamers, short peptides, etc., and no large instruments are required during the entire separation process. At the same time, the device can also be modified with antibodies, aptamers, short peptides, etc. to achieve the purpose of specifically capturing a certain type of sEVs, circulating tumor cells, viruses, bacteria and other pathogens.
[0005] According to a first aspect of the present invention, a method for preparing a microfluidic chip integrated with titanium dioxide nanomaterials is provided, comprising the following steps:
[0006] (1) using tetra-n-butyl titanate as a raw material and adopting an electrospraying method to prepare single-sided concave TiO2 nanospheres, or using tetra-isopropyl titanate as a raw material and adopting an electrospinning method to prepare TiO2 nanofibers;
[0007] (2) preparing a microchannel template, wherein the microchannel template has a continuous convex structure as a whole and an uneven surface; pouring a prepolymer onto the microchannel template fixed in a container, removing bubbles and then curing to obtain a microchannel;
[0008] (3) The microchannel obtained in step (2) is adhered to the single-sided concave TiO2 nanospheres or TiO2 nanofibers obtained in step (1) by using a prepolymer, thereby obtaining an integrated titanium dioxide nanomaterial microfluidic chip.
[0009] Preferably, the specific preparation process of step (2) is: using a coating machine to evenly cover the photoresist on the silicon wafer, and after masking and negative photoresist development, a microchannel template is obtained; the microchannel template is fixed in a culture dish, and a liquid prepolymer is poured into the culture dish by an in-situ reaction molding method. After the prepolymer is solidified, the polymer is demolded to obtain a microchannel.
[0010] Preferably, the microchannel is S-shaped as a whole.
[0011] Preferably, after step (3), the integrated titanium dioxide nanomaterial microfluidic chip is further modified, specifically, biotin-linked bovine serum albumin, streptavidin and biotin-linked antibody are injected into the integrated titanium dioxide nanomaterial microfluidic chip, or biotin-linked bovine serum albumin, streptavidin and biotin-linked aptamer are injected, or biotin-linked bovine serum albumin, streptavidin and biotin-linked polypeptide are injected, so that TiO2 is linked to bovine serum albumin and streptavidin is linked to biotin, so as to modify the integrated titanium dioxide nanomaterial microfluidic chip.
[0012] According to another aspect of the present invention, there is provided an integrated titanium dioxide nanomaterial microfluidic chip prepared by the method.
[0013] According to another aspect of the present invention, there is provided an application of the integrated titanium dioxide nanomaterial microfluidic chip for separating extracellular vesicles.
[0014] According to another aspect of the present invention, a modified integrated titanium dioxide nanomaterial microfluidic chip prepared by the method is provided.
[0015] According to another aspect of the present invention, there is provided an application of the modified integrated titanium dioxide nanomaterial microfluidic chip for specific separation of extracellular vesicles, tumor cells, bacteria or viruses.
[0016] In general, the above technical solution conceived by the present invention has the following technical advantages compared with the prior art:
[0017] (1) The present invention realizes the preparation of single-sided concave TiO2 spheres and TiO2 fibers only by electrospray-electrospinning. The manufacturing process and method are simple, low-cost, and size controllable. By utilizing the interaction between TiO2 and phospholipids on the lipid bilayer, sEVs can be easily captured. No other antibodies, aptamers or short peptides are required for modification, which simplifies the modification of materials and greatly simplifies the experimental process and cost.
[0018] (2) The single-sided concave TiO2 spheres synthesized in the present invention have a pore size (30-200 nm) that is consistent with the size of sEVs and have a certain size effect. Compared with TiO2 fibers, they greatly improve the capture efficiency of sEVs.
[0019] (3) The "fishbone" shaped structure (uneven structure) chip used in the present invention has a vortex mixing effect, which can promote the collision between sEVs in the sample and the TiO2 substrate, increase the probability of binding between the substrate and the target, and thus improve the capture efficiency.
[0020] (4) The integrated TiO2 ball microfluidic chip prepared by the present invention can be post-modified to achieve the specific capture of a certain type of sEVs, circulating tumor cells, viruses, bacteria and other pathogens by modifying antibodies, aptamers, short peptides, etc. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 (a) is a natural light image of TiO2 spheres and proves that they are light-transmissive (a'). Figure 1 (b) is a natural light image of the TiO2 fiber and demonstrates its light transmittance (b').
[0022] Figure 2 This is the XRD pattern of TiO2 spheres.
[0023] Figure 3 (a, b) are optical microscope images (a) and SEM images (b) of TiO2 spheres; (c, d) are optical microscope images (c) and SEM images (d) of TiO2 fibers.
[0024] Figure 4(a) and SEM images (b) of the “fishbone” shaped chip, as well as the optical microscope image and natural light image of the integrated TiO2 ball and TiO2 fiber microfluidic chip; (c, e) are the optical microscope image (c) and natural light image (e) of the integrated TiO2 fiber microfluidic chip; (d, f) are the optical microscope image (d) and natural light image (f) of the integrated TiO2 ball microfluidic chip.
[0025] Figure 5 Immunofluorescence and SEM were used to verify the capture of sEVs on the integrated TiO2 sphere and TiO2 fiber microfluidic chips, respectively; (a, b) are the immunofluorescence images (a) and SEM images (b) of sEVs captured by the integrated TiO2 sphere microfluidic chip, and (c, d) are the immunofluorescence images (c) and SEM images (d) of sEVs captured by the integrated TiO2 fiber microfluidic chip.
[0026] Figure 6 The capture efficiency of sEVs by the integrated TiO2 ball microfluidic chip at different flow rates.
[0027] Figure 7 Capture efficiency of sEVs by integrated TiO2 sphere microfluidic chip synthesized with different electrospinning times.
[0028] Figure 8 Comparison of sEVs capture efficiency between integrated TiO2 sphere and TiO2 fiber microfluidic chips at optimal flow rate and electrospinning time.
[0029] Fig. 9 To extract nucleic acids from captured sEVs in situ, agarose gel electrophoresis was used to verify the CK19 mRNA gene fragment amplified by RT-PCR (left) and the EGFR DNA gene fragment amplified by PCR (right).
[0030] Fig.10 qPCR was used to detect the EGFR exon 19 deletion mutation in the mock samples.
[0031] Fig.11 To verify the stability of Biotin-BSA and SA modification on TiO2 spheres using SA-Cy3, the figure shows the changes in fluorescence intensity of the blank control and after 1, 2, 5, 7, and 10 washes with HEPES.
[0032] Fig.12 The schematic diagram of the present invention is to synthesize single-sided concave TiO2 nanospheres and TiO2 fibers by using electrospray-electrospinning technology. DETAILED DESCRIPTION
[0033] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0034] The present invention utilizes electrospray-electrospinning technology to synthesize single-sided concave TiO2 nanospheres and TiO2 fibers ( Fig.12 As a schematic diagram), the integrated TiO2 microfluidic chip is prepared by the "stamp-stick-adhesion" method, including the following steps:
[0035] (1) Synthesize single-sided concave TiO2 spheres and TiO2 fibers on glass slides by electrospray-electrospinning technology;
[0036] (2) using photoresist to prepare a template having a "fishbone" structure;
[0037] (3) using a polymer to replicate the template having a "fishbone" structure obtained in step (2) to obtain a polymer having a "fishbone" structure;
[0038] (4) The single-sided concave TiO2 spheres or TiO2 fibers obtained in step (1) and the polymer containing a "fishbone" structure obtained in step (3) are used to prepare an integrated TiO2 microfluidic chip through a "stamp-stick-adhesion" method.
[0039] In some embodiments, the specific preparation process of step (1) is:
[0040] (1-1) Single-side concave TiO2 spheres and TiO2 fiber solutions were prepared using tetra-n-butyl titanate and tetra-isopropyl titanate as raw materials, respectively;
[0041] (1-2) connecting a high voltage power supply to a syringe pump to form a circuit, performing electrospray-electrospinning at a constant flow rate, and vacuum drying and calcining the spun TiO2 spheres and TiO2 fibers;
[0042] In some embodiments, the specific preparation process of step (2) is:
[0043] Use a coating machine to evenly cover the clean silicon wafer with photoresist. After masking and negative photoresist development, you can get a silicon wafer with a "fishbone" structure.
[0044] In some embodiments, the specific preparation process of step (3) is:
[0045] The silicon wafer with a "fishbone" structure is fixed in a culture dish with tape, and the liquid prepolymer is poured into the culture dish using an in-situ reaction molding method. After the prepolymer is solidified, the polymer is demolded.
[0046] In some embodiments, the polymer is an elastomeric polymer or a thermoplastic polymer;
[0047] Preferably, the elastomeric polymer is polydimethylsiloxane; and the thermoplastic polymer is polymethyl methacrylate, polycarbonate or polystyrene.
[0048] The integrated TiO2 microfluidic chip prepared by the present invention is used for label-free capture of sEVs.
[0049] The integrated TiO2 microfluidic chip prepared by the present invention can modify antibodies, aptamers, short peptides, etc. in the chip to achieve the purpose of specifically capturing a certain type of sEVs, circulating tumor cells, viruses, bacteria and other pathogens.
[0050] In the present invention, antibodies, aptamers, short peptides, etc. are modified in the chip, and the specific modification steps are that TiO2 can be used to non-specifically adsorb bovine serum albumin (BSA) modified with biotin, and then streptavidin (SA) is modified according to the affinity of biotin and streptavidin (SA), and then the biotinylated antibodies, short peptides, aptamers, etc. can be modified.
[0051] The present invention utilizes electrospray-electrospinning technology and microfluidic technology to prepare an integrated TiO2 microfluidic chip, using the following steps:
[0052] (1) Prepare TiO2 ball solution, dissolve polyvinyl pyrrolidone in anhydrous ethanol by ultrasonic, and then stir magnetically. Mix tetrabutyl titanate with anhydrous ethanol, and after stirring, pour the solution into the polyvinyl pyrrolidone ethanol solution prepared above and continue stirring;
[0053] (2) Prepare TiO2 fiber solution, dissolve polyvinyl pyrrolidone in anhydrous ethanol by ultrasonic, and then stir magnetically. Mix tetraisopropyl titanate with anhydrous ethanol, and after stirring, pour the solution into the polyvinyl pyrrolidone ethanol solution prepared above and continue stirring;
[0054] (3) Add the TiO2 ball solution and TiO2 fiber solution prepared above into a syringe respectively, and connect them to a high-voltage power supply through a syringe pump to form a passage. After adjusting the distance between the needle and the receiver, place the glass slide on the surface of the receiver table, adjust the working voltage and the flow rate of the syringe pump, and perform electrospray-electrospinning. After vacuum drying and calcination, the obtained TiO2 balls and TiO2 fibers are naturally cooled to room temperature for use;
[0055] (4) Pour the prepolymer onto the template silicon wafer fixed on the culture dish, completely remove the bubbles, place it in an oven to solidify, and then carefully cut it off with a blade for later use.
[0056] (5) Fixing the polymer with a "fishbone" structure obtained in step (4) and the TiO2 obtained in step (3) by means of a liquid prepolymer, thereby preparing an integrated TiO2 microfluidic chip.
[0057] In some embodiments, the polymer material is an elastomeric polymer such as polydimethylsiloxane (PDMS) or a thermoplastic material such as polymethyl methacrylate (PMMA), polycarbonate (PC), polystyrene (PS), and the like.
[0058] (6) Depending on the application purpose, antibodies, aptamers, short peptides, etc. can be modified on the integrated TiO2 microfluidic chip. Biotin-BSA, SA, Biotin-antibody (Biotin-aptamer, Biotin-short peptide) are injected into the chip for a certain period of time to modify antibodies, short peptides, aptamers, etc. in the chip.
[0059] Example 1
[0060] The following is a detailed description of the manufacturing method and application of the integrated TiO2 microfluidic chip through examples.
[0061] The specific steps are as follows:
[0062] (1) Prepare TiO2 ball solution: dissolve 2g polyvinyl pyrrolidone in 3mL anhydrous ethanol by ultrasonication, and then stir magnetically for about 10 minutes. Mix 3g tetra-n-butyl titanate with 3mL anhydrous ethanol, stir for 5 minutes, and then pour this solution into the polyvinyl pyrrolidone ethanol solution prepared above and continue stirring for 10 minutes.
[0063] (2) Prepare TiO2 fiber solution: dissolve 2g polyvinyl pyrrolidone in 3mL anhydrous ethanol by ultrasonication, and then stir magnetically for about 10 minutes. Mix 3g tetraisopropyl titanate with 3mL anhydrous ethanol, stir for 5 minutes, and pour the solution into the polyvinyl pyrrolidone ethanol solution prepared above, and continue stirring for 10 minutes.
[0064] (3) The TiO2 ball solution and TiO2 fiber solution prepared above were added to 1 mL syringes respectively, and connected to a high voltage power supply through a syringe pump. After adjusting the distance between the needle and the receiver, the glass slide was placed on the surface of the receiver table, the working voltage was adjusted to 5 KV, the flow rate of the syringe pump was adjusted to 1 mL / h, and electrospray-electrospinning was performed. The obtained TiO2 balls and TiO2 fibers were vacuum dried at 80°C overnight, calcined at 600°C for 5 hours, and naturally cooled to room temperature. Figure 1(a) is a natural light image of TiO2 spheres and proves that they are light-transmissive (a'). Figure 1 (b) is a natural light image of the TiO2 fiber and demonstrates its light transmittance (b'). Figure 2 This is the XRD pattern of TiO2 spheres. Figure 3 (a) and (b) are optical microscope images and SEM images of TiO2 spheres, respectively. Figure 3 (c) and (d) are optical microscope images and SEM images of TiO2 fibers, respectively.
[0065] (4) Place a clean silicon wafer on a coater and adjust the coater speed to 1500 rpm for 30 seconds. Pour SU-82015 negative photoresist onto the silicon wafer and obtain a 25 μm thick photoresist master through the coater. Align the chip channel mask with the silicon wafer, irradiate with UV light for 15 seconds, and bake at 65°C and 95°C for 3 minutes. Use a coater to prepare a second layer of 25 μm thick SU-82015 photoresist on the above silicon wafer. Align the mask with a fishbone structure with the chip channel and expose it to UV light for 15 seconds, then bake at 65°C for 3 minutes and 95°C for 5 minutes. Finally, develop in SU-8 developer.
[0066] (5) The "fishbone" chip model prepared on the silicon wafer was glued to a 15 cm plastic dish, and the PDMS component A and component B were mixed evenly at a ratio of 10:1 (wt / wt), and the mixture was vacuumed to remove air bubbles, and then poured into the plastic dish. After being placed at room temperature for a period of time, the remaining air bubbles were removed with an ear bulb, and the mixture was placed in a 75°C oven for 3 h. The cured PDMS "fishbone" chip (with an uneven surface) was cut from the plastic dish, and the PDMS chip was punched with a hole puncher for later use. Figure 4 (a) and (b) are optical microscope images and SEM images of PDMS with a "fishbone" structure, respectively.
[0067] (6) Prepare an integrated TiO2 microfluidic chip using the "stamp-stick-adhesion" method. Mix a certain amount of PMDS component A and component B at a ratio of 10:1 (wt / wt) and pour them onto a clean silicon wafer. Adjust the homogenizer to an appropriate speed and time, and use the homogenization effect of the homogenizer to evenly shake the PDMS on the silicon wafer to obtain a PDMS thin layer of appropriate thickness. Finally, place the punched PDMS chip on the silicon wafer, dip a small amount of undried PDMS, quickly bond it to the above-mentioned TiO2 micro-nano material, and leave it at room temperature overnight. Figure 4 (c) and (d) are optical microscope images of integrated TiO2 fiber and TiO2 ball microfluidic chips, respectively. Figure 4 (e) and (f) are natural light images of the integrated TiO2 fiber and TiO2 ball microfluidic chips, respectively.
[0068] Figure 5 Immunofluorescence and SEM were used to verify the capture of sEVs on the integrated TiO2 sphere and TiO2 fiber microfluidic chips, respectively. (The specific method is: 1. Immunofluorescence method, the sEVs standard sample obtained by ultracentrifugation is allowed to react with the chip at a constant flow rate through a syringe pump, and then blocked with 5% bovine serum albumin. Then the biotin-modified anti-CD9 antibody is injected into the chip to react with sEVs, and then blocked with 5% bovine serum albumin, and finally injected with SA-Cy3, and the fluorescence is observed with an inverted fluorescence microscope. 2. SEM method, the sEVs standard sample obtained by ultracentrifugation is allowed to react with the chip at a constant flow rate through a syringe pump, and then fixed with 2.5% (V / V) glutaraldehyde overnight, and then dehydrated step by step with ethanol solutions with a concentration gradient of 30%, 50%, 70%, 90%, 95%, and 100% for 15 minutes. After fixation, wash with deionized water to remove excess salt, dry at room temperature and take SEM photos.) (a, b) are the immunofluorescence images (a) and SEM images (b) of the integrated TiO2 ball microfluidic chip capturing sEVs, both of which indicate that this chip can successfully capture sEVs. (c, d) are the immunofluorescence images (c) and SEM images (d) of the integrated TiO2 fiber microfluidic chip capturing sEVs, both of which show that this chip can successfully capture sEVs. Comparing the capture effects of the integrated TiO2 ball microfluidic chip and the integrated TiO2 fiber microfluidic chip, it can be found that the integrated TiO2 ball microfluidic chip has a better capture effect.
[0069] Figure 6 The capture efficiency of sEVs by the integrated TiO2 ball microfluidic chip at different flow rates. (The specific method is: at different flow rates (1, 10, 20, 30 and 40 μL / min), the sEVs standard sample is passed into the integrated TiO2 ball microfluidic chip to be captured to investigate the effect of flow rate on the capture efficiency of sEVs. The capture efficiency is calculated by measuring the change in protein content of sEVs before and after capture using the BCA method microprotein concentration determination kit.)
[0070] Figure 7 The capture efficiency of sEVs by the integrated TiO2 ball microfluidic chip synthesized at different electrospinning times. (The specific method is: the TiO2 ball solution is synthesized by the electrospray-electrospinning device at different times (15, 30, 45, 60, 75min), and then the sEVs solution is passed into the integrated TiO2 ball microfluidic chip for capture, and the capture efficiency of sEVs by the integrated TiO2 ball microfluidic chip at different synthesis times is investigated.)
[0071] Figure 8Comparison of the capture efficiency of sEVs by integrated TiO2 sphere and TiO2 fiber microfluidic chips under the optimal flow rate and synthesis time. It can be found that the capture effect of sEVs by integrated TiO2 sphere microfluidic chip is significantly better than that by integrated TiO2 fiber microfluidic chip.
[0072] Fig. 9 To extract nucleic acids from captured sEVs in situ, agarose gel electrophoresis was used to verify the CK19 mRNA gene fragment amplified by RT-PCR (left) and the EGFR DNA gene fragment amplified by PCR (right). (The specific method is: according to the instructions, the Nucleozol reagent is used to extract the sEVs RNA captured by the integrated TiO2 ball microfluidic chip in situ, and then the CK19 gene coding region is amplified by RT-PCR. The reverse transcription reaction system is shown in Table 1. The CK19 specific primers are shown in Table 2 (346bp). The PCR system is shown in Table 3. The amplification program is shown in Table 4. In addition, according to the instructions, the QIAamp DNA MicroKit is used to extract the sEVs DNA captured by the integrated TiO2 ball microfluidic chip in situ, and then the EGFR gene coding region is amplified by PCR technology. The EGFR specific primers are shown in Table 5 (285bp). The PCR system is shown in Table 6. The amplification program is shown in Table 7. Finally, 2% agarose gel electrophoresis is used to characterize the CK19 mRNA gene fragment and the EGFR DNA gene fragment, respectively.) As can be seen from the figure, the target bands can be detected at 346bp and 285bp respectively, proving that the sEVs captured by this chip can be used for nucleic acid analysis.
[0073] Table 1 Reverse transcription reaction system *
[0074]
[0075] *Operate on ice
[0076] Table 2 CK 19 specific primer sequences
[0077]
[0078] Table 3 PCR amplification reaction system for the coding region of CK 19 gene
[0079]
[0080] Table 4 PCR amplification reaction procedure for the coding region of CK 19 gene
[0081]
[0082] Table 5 EGFR specific primer sequences
[0083]
[0084] Table 6 PCR amplification reaction system of EGFR gene coding region
[0085]
[0086] Table 7 PCR amplification reaction procedure for the EGFR gene coding region
[0087]
[0088] Fig.10 To detect the EGFR exon 19 deletion mutation in the simulated sample by qPCR. (The specific method is: 10 μL PC9 cell-derived sEVs standard is added to 500 μL healthy human serum to simulate clinical samples, and then the sEVs in the simulated sample are captured by an integrated TiO2 ball microfluidic chip, followed by in situ DNA extraction, and finally the human EGFR gene mutation detection kit is used to detect EGFR-related mutations according to the instructions provided by the manufacturer. The judgment standard for the detection of EGFR exon 19 deletion mutation is ΔCt < 6 (ΔCt = mutation detection Ct-quality control detection Ct.) Fig.10 To simulate the detection results of the sample, it can be seen from the figure that the sEVs captured by this chip can be successfully used for downstream mutation analysis.
[0089] Fig.11 In order to verify the stability of Biotin-BSA and SA modification on TiO2 balls with SA-Cy3, (the specific method is: inject Biotin-BSA and SA-Cy3 into the chip for 30 minutes in succession, and for the blank control, only inject SA-Cy3 into the chip for 30 minutes, and observe the fluorescence after clearing with HEPES). It can be seen from the figure that the blank control has no fluorescence, indicating that TiO2 balls cannot directly adsorb SA. The fluorescence intensity does not change much after washing with HEPES 1, 2, 5, 7, and 10 times, which proves that the stability of SA modified by Biotin-BSA adsorption is better.
[0090] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing a microfluidic chip integrated with titanium dioxide nanomaterials, characterized in that: The following steps are involved: (1) using tetra-n-butyl titanate as a raw material and adopting an electrospraying method to prepare single-sided concave TiO2 nanospheres, wherein the pore size of the single-sided concave TiO2 nanospheres is 30-200 nm; (2) preparing a microchannel template, wherein the microchannel template has a continuous convex structure as a whole and an uneven surface; pouring a prepolymer onto the microchannel template fixed in a container, removing bubbles and then curing to obtain a microchannel; (3) The microchannel obtained in step (2) is adhered to the single-sided concave TiO2 nanosphere obtained in step (1) by using a prepolymer, thereby obtaining an integrated titanium dioxide nanomaterial microfluidic chip.
2. The method for preparing an integrated titanium dioxide nanomaterial microfluidic chip according to claim 1, characterized in that: The specific preparation process of step (2) is as follows: using a coating machine to evenly cover the silicon wafer with photoresist, and after masking and negative photoresist development, a microchannel template is obtained; the microchannel template is fixed in a culture dish, and a liquid prepolymer is poured into the culture dish using an in-situ reaction molding method. After the prepolymer is solidified, the polymer is demolded to obtain a microchannel.
3. The method for preparing an integrated titanium dioxide nanomaterial microfluidic chip according to claim 1 or 2, characterized in that: The microchannel is S-shaped as a whole.
4. The method for preparing an integrated titanium dioxide nanomaterial microfluidic chip according to claim 1 or 2, characterized in that: After step (3), the method further includes modifying the integrated titanium dioxide nanomaterial microfluidic chip, specifically, injecting biotin-linked bovine serum albumin, streptavidin and biotin-linked antibody, or injecting biotin-linked bovine serum albumin, streptavidin and biotin-linked aptamer, or injecting biotin-linked bovine serum albumin, streptavidin and biotin-linked polypeptide into the integrated titanium dioxide nanomaterial microfluidic chip, so that TiO2 is linked to bovine serum albumin and streptavidin is linked to biotin, so as to modify the integrated titanium dioxide nanomaterial microfluidic chip.
5. An integrated titanium dioxide nanomaterial microfluidic chip prepared by the method according to any one of claims 1 to 3.
6. Use of the integrated titanium dioxide nanomaterial microfluidic chip as claimed in claim 5 for separating extracellular vesicles.
7. The modified integrated titanium dioxide nanomaterial microfluidic chip prepared by the method according to claim 4.
8. Use of the modified integrated titanium dioxide nanomaterial microfluidic chip as claimed in claim 7 for specific separation of extracellular vesicles, tumor cells, bacteria or viruses.
Citation Information
Patent Citations
Biomolecule recovering device and method, and biomolecule analyzing device and method
CN113597559A