A production device and method for improving the welding strength of electric fusion pipe fittings
By designing the overmolding mechanism and the oxide film scraping mechanism in the electrofusion pipe fittings production device, the problem of low welding strength in the pre-embedded heating wire process is solved, a thinner overmolding layer and more efficient heat transfer are achieved, which improves the Welding quality and efficiency, avoiding pipeline leaks.
Patent Information
- Application Number
- CN202210998299.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-19
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-08-19
AI Technical Summary
The existing embedded heating wire process electrofusion pipe fittings have low welding strength, leading to pipeline leakage problems. This is mainly due to poor heat transfer and insufficient interface welding strength due to excessive thickness of the plastic-coated wire and incomplete cleaning of the oxide film.
Design a production device, including a molding mechanism and an oxide film scraping mechanism. The molding mechanism forms a plastic coating line with a flat bottom section and a local bulge in the center of the top, increasing the contact area between the plastic coating line and the outer surface of the mold core, and The oxide film scraping mechanism removes the oxide film on the surface of the plastic-coated wire to improve the welding strength.
By removing the oxide film and reducing the thickness of the plastic coating layer, the production quality of the plastic coating line is improved, the welding strength is enhanced, the welding time is shortened, the installation efficiency is improved, and the long-term safe operation of the pipeline is ensured.
Smart Images

Figure CN115366329B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of plastic coating technology, in particular to a production device and method for improving the welding strength of electric fusion pipe fittings. Background Art
[0002] In the current industry, the production processes of electric fusion pipe fittings mainly include pre-embedded heating wire (plastic-coated wire) process electric fusion pipe fittings, secondary injection molding process electric fusion pipe fittings, and post-embedded heating wire process electric fusion pipe fittings. The basic production process of pre-embedded heating wire (plastic-coated wire) process electric fusion pipe fittings is to first use special equipment to coat the heating wire with plastic as a whole. The heating wire after plastic coating has a set structure and thickness. Then the plastic-coated heating wire is wound around the outer cylindrical surface of the mold core and placed in the mold cavity for overall injection molding. After a certain period of time, the mold is opened and the product is taken out.
[0003] The inventors have discovered that after the heating wire of the pre-buried heating wire process electric fusion pipe fitting is coated with plastic, the vertical distance from the heating wire on the inner cylindrical surface of the pipe fitting to the outer cylindrical surface of the pipe will become larger after the plastic pipe is socketed into the inner cylindrical surface of the pipe fitting; after the heating wire is connected to the power supply, the heat transfer efficiency to the outer cylindrical surface of the pipe is low, the melting depth becomes smaller, and the welding strength at the interface is low; at the same time, the plastic is heated at high temperature and reaches a molten state before it can be completely coated on the heating wire, but an oxide film will form on the outer cylindrical surface of the plastic-coated wire during the process of cooling to room temperature. If the oxide film is not thoroughly cleaned during welding, it will block the entanglement between the plastic molecular chains, causing a "cold welding" phenomenon on the interface; due to incomplete cleaning of the oxide layer on the welding surface and the thickness of the coating plastic layer, the heat transfer is poor and the welding strength is insufficient, which ultimately leads to the problem of pipeline leakage always being high, affecting the long-term safe operation of the pipeline. Summary of the invention
[0004] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a production device and method for improving the welding strength of electric fusion pipe fittings, which utilizes a plastic-coating molding mechanism to produce a plastic-coated wire with a flat bottom cross-section and a local bulge at the center of the top, thereby increasing the contact area between the bottom plane of the plastic-coated wire and the outer cylindrical surface of the mold core and reducing the wall thickness of the plastic-coating layer. At the same time, an oxide film scraping mechanism is used to scrape the oxide film on the surface of the plastic-coated wire, thereby greatly improving the production quality of the plastic-coated wire and solving the problem of low welding strength of electric fusion pipe fittings using the existing pre-buried heating wire (plastic-coated wire) process.
[0005] In order to achieve the above object, the present invention is implemented through the following technical solutions:
[0006] In the first aspect, the present invention provides a production device for improving the welding strength of electric fusion pipe fittings, comprising a wire coil support mechanism, a plastic overmolding mechanism, a cooling water trough, an oxide film scraping mechanism and a traction mechanism arranged in sequence from front to back, the top of the plastic overmolding mechanism is fixedly connected to the plasticizing extrusion mechanism, the heating wire on the wire coil support mechanism horizontally passes through the plastic overmolding mechanism, the cooling water trough, the oxide film scraping mechanism in sequence and is connected to the traction mechanism, the heating wire can form a plastic overmolding wire with a flat bottom cross-section and a local bulge at the center of the top in the plastic overmolding mechanism, and the oxide film scraping mechanism is used to scrape off the oxide film on the outer surface of the plastic overmolding wire after cooling.
[0007] As a further implementation method, the plasticizing extrusion mechanism consists of a vertically arranged barrel, a power unit fixedly arranged on the top of the barrel and connected to the screw inside the barrel, the outside of the barrel is wrapped with a heating ring along its length, and the bottom of the barrel is provided with a mounting port threadedly connected to the overmolding mechanism.
[0008] As a further implementation method, the wire drum support mechanism consists of a first support frame and a first wire drum rotatably arranged on the first support frame; the traction mechanism consists of a second support frame and a second wire drum rotatably arranged on the second support frame, and a driving motor for driving the second wire drum to rotate is fixedly provided on the second support frame.
[0009] As a further implementation method, the overmolding mechanism consists of a mold body, a conical positioning piece arranged inside the mold body, and an overmolding die head. The conical positioning piece is coaxially arranged with the overmolding die head, and the conical end of the conical positioning piece is inserted into the overmolding die head. The conical positioning piece is fixedly connected to the mold body through a first fixing piece, and the overmolding die head is fixedly connected to the mold body through a second fixing piece. The first fixing piece and the second fixing piece are relatively arranged on both sides of the mold body.
[0010] As a further implementation, an injection cavity is provided in the mold body, the conical positioning piece and the overmolding die head are both arranged in the injection cavity, the top end of the mold body is threadedly connected to the plasticizing extrusion mechanism, and the injection cavity is connected to the plasticizing extrusion mechanism.
[0011] As a further implementation method, the first fixing part is composed of a flange and a circular boss fixedly arranged on the flange, the flange is fixedly connected to the mold body, the circular boss is inserted into the injection cavity to block the end of the injection cavity, and the end of the circular boss is provided with a first positioning hole for positioning and installing the conical positioning part. A first channel is also provided in the first fixing part, the first channel runs through the first fixing part, the first channel is coaxially arranged with the first positioning hole, and the diameter of the first channel is the same as the diameter of the heating wire.
[0012] As a further implementation method, one end of the conical positioning piece is threadedly connected to the first positioning hole, and the other end extends into the injection mold. The end of the conical positioning piece inserted into the injection mold is a conical structure. A second channel is provided in the conical positioning piece. The second channel is coaxially arranged with the first channel. The second channel consists of a coaxially arranged flared section and a straight section. The flared section is close to the first channel and is larger than the first channel. The diameter of the straight section is the same as the diameter of the first channel.
[0013] As a further implementation method, the overmolding die head is provided with a coaxially arranged overmolding cavity and a molding cavity. The overmolding cavity is a conical cavity structure. The size of the overmolding cavity is larger than the size of the insertion end of the conical positioning piece. The cross-section of the molding cavity is flat at the bottom and has a local bulge at the center of the top.
[0014] As a further implementation method, the oxide film scraping mechanism is fixedly arranged at the outlet end of the cooling water trough, and is composed of a scraper upper mold, a scraper lower mold and an adjustment screw for adjusting the scraping depth. The scraper upper mold and the scraper lower mold cooperate to form a scraping cavity with the same cross-section as the plastic-coated wire.
[0015] In a second aspect, the present invention provides a working method of a production device for improving the welding strength of an electric fusion pipe fitting, which is specifically as follows:
[0016] Manually lead the heating wire on the first wire drum through the overmolding mechanism, the cooling water tank, the oxide film scraping mechanism in sequence and wind it on the second wire drum;
[0017] The power unit and the driving motor are started, and the molten fluid plastic is transferred from the barrel to the injection molding cavity, and the molten fluid plastic is combined with the outer ring of the heating wire in the overmolding cavity;
[0018] Under the traction of the second wire drum, the plastic-coated wire that has completed the plastic-coating work enters the cooling water tank for cooling and then enters the oxide film scraping mechanism to scrape the surface oxide film. After scraping, the plastic-coating is wound on the second wire drum. At the same time, the heating wire extends from the first wire drum and extends into the plastic-coating molding mechanism under the traction of the second wire drum.
[0019] The beneficial effects of the present invention are as follows:
[0020] (1) In the continuous production process of the coated plastic, the heating wire of the present invention is always fixed in position and is always in a horizontal moving state, which effectively ensures the uniformity of the plastic coating layer on the outer circle of the heating wire and the uniformity of the scraping of the oxide layer, greatly improves the production quality of the plastic-coated wire, and controls the thickness of the plastic-coated wire to be the thinnest. The thinner the plastic coating layer of the plastic-coated wire, the faster the speed of heat transfer to the surface of the pipe per unit welding time, the higher the welding efficiency, shortens the welding time, and improves the installation efficiency.
[0021] (2) The present invention uses an oxide film scraping mechanism to remove the oxide film generated on the outer cylindrical surface of the plastic-coated wire during high-temperature extrusion molding. After the oxide film of the plastic-coated wire is removed, power is turned on and heat is generated, and the polyethylene on the inner cylindrical surface of the connector and the outer cylindrical surface of the pipe changes from a solid state to a molten fluid state, and entanglement and penetration are formed between the polyethylene molecular chains. In this way, the welding surface is integrated after cooling to room temperature, meeting the welding strength requirements.
[0022] (3) The cross-section of the plastic-coated wire of the present invention is a flat bottom structure with a local bulge at the center of the top, which increases the contact area between the bottom plane of the plastic-coated wire and the outer cylindrical surface of the mold core, avoiding the displacement of the plastic-coated wire due to the high injection pressure during the production process of the injection molded product, and at the same time reduces the wall thickness of the plastic-coated layer. When the heating wire is energized, the heat is transferred and diffused to the surrounding more efficiently. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The accompanying drawings in the specification, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.
[0024] Figure 1 It is a schematic diagram of the overall structure of a production device for improving the welding strength of electric fusion pipe fittings according to one or more embodiments of the present invention;
[0025] Figure 2 is a schematic structural diagram of an overmolding mechanism according to one or more embodiments of the present invention;
[0026] Figure 3 is a schematic structural diagram of a mold body according to one or more embodiments of the present invention;
[0027] Figure 4 is a schematic diagram of a main structural cross-section of a first fixing member according to one or more embodiments of the present invention;
[0028] Figure 5 is a schematic side structural view of a first fixing member according to one or more embodiments of the present invention;
[0029] Figure 6 is a schematic cross-sectional structure diagram of a conical positioning member according to one or more embodiments of the present invention;
[0030] Figure 7 is a schematic diagram of a main structural cross-section of an overmolding die head according to one or more embodiments of the present invention;
[0031] Figure 8 is a schematic side view of the structure of an overmolding die according to one or more embodiments of the present invention;
[0032] Fig. 9is a schematic structural diagram of a second fixing member according to one or more embodiments of the present invention;
[0033] Fig.10 is a schematic cross-sectional view of a plastic-coated wire according to one or more embodiments of the present invention;
[0034] Fig.11 is a schematic cross-sectional structure diagram of an oxide film scraping mechanism according to one or more embodiments of the present invention;
[0035] In the figure: the distances or sizes between parts are exaggerated to show the positions of the parts, and the schematic diagram is for illustration only;
[0036] Among them, 1. plasticizing extrusion mechanism; 1.1. power unit; 1.2. barrel; 1.3. screw; 1.4. installation port; 2. wire drum support mechanism; 3. plastic molding mechanism; 3.1. mold body; 3.1.1. injection cavity; 3.2. first fixing member; 3.2.1. first channel; 3.2.2. first positioning hole; 3.3. conical positioning member; 3.3.1. connecting part; 3.3.2. positioning part; 3.3.3. guiding part; 3.3.4. second channel; 3. .4. Overmolding die; 3.4.1. First fixing part; 3.4.2. Second fixing part; 3.4.3. Overmolding cavity; 3.4.4. Molding cavity; 3.5. Second fixing piece; 3.5.1. Positioning cavity; 3.5.2. Second positioning hole; 4. Cooling water trough; 5. Oxide film scraping mechanism; 5.1. Scraper upper die; 5.2. Scraper lower die; 5.3. Adjusting screw; 5.4. Scraping cavity; 6. Traction mechanism; 7. Overmolding wire; 7.1. Overmolding layer; 7.2. Heating wire. DETAILED DESCRIPTION
[0037] It should be noted that the following detailed descriptions are illustrative and intended to provide further explanation of the present invention. Unless otherwise specified, all technical and scientific terms used in the present invention have the same meanings as those commonly understood by those skilled in the art to which the present invention belongs.
[0038] As introduced in the background technology, after the plastic pipe is socketed into the inner cylindrical surface of the pre-buried heating wire process electric fusion pipe fittings, the vertical distance from the heating wire on the inner cylindrical surface of the pipe fitting to the outer cylindrical surface of the pipe becomes larger; after the heating wire is connected to the power supply, the heat transfer efficiency to the outer cylindrical surface of the pipe is low, the melting depth becomes smaller, and the welding strength at the interface is low. At the same time, the oxide layer on the welding surface is not thoroughly cleaned, and the thickness of the coating plastic layer causes poor heat transfer and insufficient welding strength, which ultimately leads to the problem of pipeline leakage that is always high and affects the long-term safe operation of the pipeline. In order to solve the above technical problems, the present invention proposes a production device and method for improving the welding strength of electric fusion pipe fittings.
[0039] Example 1
[0040] In a typical embodiment of the present invention, Figure 1-Figure 11 As shown, a production device for improving the welding strength of electric fusion pipe fittings is proposed, comprising: Figure 1 Taking the shown example as an example, with the front-to-back direction being from left to right, a wire drum supporting mechanism 2, an overmolding mechanism 3, a cooling water trough 4, an oxide film scraping mechanism 5 and a traction mechanism 6 are sequentially arranged in the same plane, wherein the overmolding mechanism 3 is connected to the plasticizing extrusion mechanism 1, and the molding cavity 3.4.4 on the overmolding mechanism 3 is coaxially arranged with the scraping cavity 5.4 on the oxide film scraping mechanism 5, so as to control the thickness and uniformity of the overmolding layer 7.1 on the outer surface of the heating wire 7.2.
[0041] like Figure 1 As shown, the plasticizing extrusion mechanism 1 is composed of a power unit 1.1, a barrel 1.2, a screw 1.3 and a die head connection unit 1.4, wherein the barrel 1.2 is vertically arranged, the power unit 1.1 is fixedly arranged on the top of the barrel 1.2 and connected to the screw 1.3 in the barrel 1.2 to drive the rotation of the screw 1.3, the screw 1.3 and the barrel 1.2 are coaxially arranged, and the bottom of the barrel 1.2 has a mounting port 1.4 for connecting to the overmolding mechanism 3, the mounting port 1.4 is connected to the inside of the barrel 1.2 and the inner wall of the mounting port is provided with an internal thread, and the outside of the barrel 1.2 is wrapped with a heating coil along its length.
[0042] The overmolding mechanism 3 is fixedly connected to the mounting opening 1.4 at the bottom of the barrel 1.2 by means of a threaded connection. Figure 2 As shown, the overmolding mechanism 3 is composed of a mold body 3.1, a first fixing member 3.2, a conical positioning member 3.3, an overmolding die head 3.4 and a second fixing member 3.5, wherein the conical positioning member 3.3 is fixedly arranged in the mold body 3.1 through the first fixing member 3.2, the overmolding die head 3.4 is fixedly arranged in the mold body 3.1 through the second fixing member 3.5, and the conical positioning member 3.3 is coaxially arranged with the overmolding die head 3.4, and is mainly used for overmolding of the heating wire 7.2.
[0043] Specific as Figure 3 As shown, an injection cavity 3.1.1 is provided in the mold body 3.1, and the injection cavity 3.1.1 is a three-way cavity, wherein a conical positioning member 3.3 and an overmolding die head 3.4 are both arranged in the injection cavity 3.1.1, and a first fixing member 3.2 and a second fixing member 3.5 are relatively arranged on both sides of the mold body 3.1;
[0044] An external thread is arranged on the outer side wall of the top of the mold body 3.1. The top of the mold body 3.1 is fixedly connected to the barrel 1.2 by threaded connection. The inside of the barrel 1.2 is connected to the top of the injection cavity 3.1.1, and the overmolding material can be injected into the injection cavity 3.1.1.
[0045] like Figure 4-Figure 5 As shown, the first fixing member 3.2 is a boss flange structure, which consists of a flange plate and a circular boss fixed on the flange plate. The flange plate and the circular boss are coaxially arranged, and the flange plate is fixedly connected to the mold body 3.1 by bolting. The circular boss is inserted into the injection cavity 3.1.1 from the left side to block the left end of the injection cavity 3.1.1. A first positioning hole 3.2.2 is provided at the end of the circular boss. The diameter of the first positioning hole 3.2.2 is the same as the diameter of the connecting portion of the conical positioning member 3.3, and is used for the positioning and installation of the conical positioning member 3.3.
[0046] A first channel 3.2.1 is also provided in the first fixing member 3.2. The first channel 3.2.1 penetrates the first fixing member 3.2. The first channel 3.2.1 is coaxially arranged with the first positioning hole 3.2.2, and one end of the first channel 3.2.1 is connected with the first positioning hole 3.2.2, and is mainly used for the passage of the heating wire 7.2. The diameter of the first channel 3.2.1 is the same as the diameter of the heating wire 7.2 to prevent the heating wire 7.2 from bending.
[0047] like Figure 6 As shown, the conical positioning member 3.3 is composed of a coaxially arranged connecting portion 3.3.1, a positioning portion 3.3.2 and a guiding portion 3.3.3, and the connecting portion 3.3.1, the positioning portion 3.3.2 and the guiding portion 3.3.3 are integrally formed, wherein the outer wall of the connecting portion 3.3.1 has an external thread, and the first positioning hole 3.2.2 is provided with an internal thread matching therewith, and the connecting portion 3.3.1 is fixedly connected to the first positioning hole 3.2.2 by a threaded connection, and the diameter of the positioning portion 3.3.2 is greater than the diameter of the connecting portion 3.3.1, which can limit the depth of the connecting portion 3.3.1 extending into the first positioning hole 3.2.2, and the guiding portion 3.3.3 is a conical structure, which can be extended into the injection mold head 3.4 to guide the heating wire 7.2 to prevent the heating wire 7.2 from bending during the overmolding process.
[0048] A second channel 3.3.4 is provided in the conical positioning member 3.3. The second channel 3.3.4 runs through the conical positioning member 3.3 and is mainly used for guiding the heating wire 7.2. The second channel 3.3.4 is coaxially arranged with the first channel 3.2.1. The second channel 3.3.4 is a variable cross-section structure, consisting of a coaxially arranged flared section and a straight section, wherein the flared section is close to the first channel 3.2.1, and the size of one end of the flared section close to the first channel 3.2.1 is larger than the first channel 3.2.1, so that the heating wire 7.2 extending from the first channel 3.2.1 can enter the second channel 3.3.4, and the diameter of the straight section is the same as the diameter of the first channel 3.2.1, so as to further ensure the straightness of the heating wire 7.2.
[0049] like Figure 7-Figure 8As shown, the overmolding die 3.4 is a circular boss structure, and the overmolding die 3.4 is composed of a first fixing part 3.4.1 and a second fixing part 3.4.2 which are coaxially arranged, wherein the outer diameter of the first fixing part 3.4.1 is larger than the second fixing part 3.4.2, and the outer diameter of the first fixing part 3.4.1 is slightly smaller than the diameter of the end of the injection cavity 3.1.1 connected thereto, so as to facilitate assembly, and the outer diameter of the second fixing part 3.4.2 is the same as the diameter of the second positioning hole 3.5.2 on the second fixing member 3.5, so as to ensure the positioning effect.
[0050] The overmolding die head 3.4 is also provided with an overmolding cavity 3.4.3 and a molding cavity 3.4.4, which are coaxially arranged and connected with each other, wherein the overmolding cavity 3.4.3 is a conical cavity structure, the size of the overmolding cavity 3.4.3 is larger than the size of the guide portion 3.3.3 of the conical positioning piece 3.3, the guide portion 3.3.3 is inserted into the overmolding cavity 3.4.3, and the heating wire 7.2 can be combined with the overmolding material in the overmolding cavity 3.4.3.
[0051] The molding cavity 3.4.4 has a flat bottom cross section and a partially raised structure at the top center. The heating wire 7.2 molded in the molding cavity 3.4.3 can be molded into a molding wire 7 with the same cross section as the molding cavity 3.4.4 under the action of the molding cavity 3.4.4.
[0052] like Fig.10 As shown, the plastic-coated wire 7 has a flat bottom section and a local bulge at the center of the top. The outermost layer is a plastic-coated layer 7.1, which is polyethylene plastic. The interior of the plastic-coated layer 7.1 is a heating wire 7.2. When the plastic-coated wire 7 of this structure is wound onto the outer cylindrical surface of the mold core at an equal pitch under a certain tensioning force, the contact area between the bottom plane of the plastic-coated wire 7 and the outer cylindrical surface of the mold core is large, which can avoid the plastic-coated wire shifting site due to the high injection pressure during the production process of the injection molded product, which directly affects the product quality in serious cases. At the same time, the local bulge design on the top of the plastic-coated wire 7 can accommodate the heating wire 7.2 and realize the wrapping of the heating wire 7.2 under the thinnest plastic-coated cross-section. When the heating wire 7.2 is energized, the heat is transferred and diffused to the surrounding more efficiently.
[0053] If a circular plastic-coated wire 7 is used, the contact surface between the plastic-coated wire 7 and the outer cylindrical surface of the mold core is very small, and the entire wire is easily displaced due to the injection pressure during the injection molding process, causing product appearance problems and even product quality problems; at the same time, in order to ensure the thinner plastic coating thickness of the heating wire, the outer diameter of the circular plastic-coated wire must be small, and the pitch between the plastic-coated wires wound on the outer cylindrical surface of the mold core is small. When the heating wire is energized and the conductor is subjected to the current load, vibration will occur (the greater the current, the greater the vibration of the heating wire). At this time, the small pitch can easily cause adjacent heating wires to overlap, causing the electric fusion component to short-circuit or even break, and welding cannot be continued. At this time, the pipe joint needs to be scrapped, removed, and replaced;
[0054] If other regular structures of plastic-coated wires (such as square) are used, the cross-sectional area of the plastic-coated wire will increase, and the thickness of the coated plastic layer will increase. During the injection molding process, the bonding strength between the molten fluid plastic and the plastic-coated wire with a larger cross-section (solid cold material) will be poor, which is cold material bonding and has product quality defects. At the same time, the larger the cross-section, the lower the heat transfer efficiency.
[0055] like Fig. 9 As shown, the second fixing member 3.5 is provided with a positioning cavity 3.5.1 and a second positioning hole 3.5.2, and the positioning cavity 3.5.1 is coaxially arranged with the second positioning hole 3.5.2, wherein the diameter of the positioning cavity 3.5.1 is larger than the diameter of the second positioning hole 3.5.2, and an internal thread is provided in the positioning cavity 3.5.1 for cooperating with the thread on the outer surface of the end portion on the right side of the mold body 3.1, and the diameter of the second positioning hole 3.5.2 is the same as the outer diameter of the second fixing portion 3.4.2 of the overmolding die 3.4, and the second fixing portion 3.4.2 can pass through the positioning cavity 3.5.1 and be inserted into the second positioning hole 3.5.2 to achieve positioning.
[0056] A heating module is fixedly provided on the outside of the overmolding structure 3. The heating module can be a heating wire or other structure, which is used to heat the overmolding structure 3 as a whole to control the temperature within a fixed range, so that the molten plastic can smoothly enter the overmolding structure 3 and achieve continuous extrusion.
[0057] The wire drum supporting mechanism 2 is composed of a first wire drum and a first supporting frame. The first wire drum is rotatably arranged on the first supporting frame and is mainly used for accommodating and releasing the heating wire 7.2.
[0058] The cold water trough 4 is an existing trough structure, with through holes on both sides allowing the plastic-coated wire 7 to pass through. The shape and size of the through holes are the same as those of the molding cavity 3.4.4 and are coaxially arranged with the molding cavity 3.4.4 to ensure that the plastic-coated wire 7 enters the cooling water trough 4 horizontally, and the cooling water will not leak out from the through holes during the cooling process of the plastic-coated wire 7.
[0059] The oxide film scraping mechanism 5 is fixedly arranged at the outlet end of the cooling water tank 4, and is mainly used to scrape off the oxide film on the surface of the plastic coated wire 7. Fig.11 As shown, the oxide film scraping mechanism 5 is composed of a scraper upper mold 5.1, a scraper lower mold 5.2 and an adjustment screw 5.3 for adjusting the scraping depth. The scraper upper mold 5.1 is located above the scraper lower mold 5.2, and the two cooperate in the middle position to form a scraping cavity 5.4 with the same shape as the molding cavity 3.4.4. The scraping cavity 5.4 is coaxially arranged with the molding cavity 3.4.4, and the size of the scraping cavity 5.4 is smaller than that of the molding cavity 3.4.4. In this embodiment, the scraping cavity 5.4 is 0.1mm-0.2mm smaller than the molding cavity 3.4.4, that is, 0.1mm-0.2mm is cut off from the outer surface of the plastic-coated wire 7.
[0060] Since the oxide film prevents the entanglement and penetration between molecular chains, the oxide film barrier causes a "cold weld" between the connector and the pipe, affecting the safe operation of the pipeline. Therefore, the oxide film generated on the outer cylindrical surface of the plastic-coated wire during high-temperature extrusion molding is removed by the oxide film scraping mechanism 5 by 0.1mm-0.2mm; after the oxide film of the plastic-coated wire is removed, the polyethylene on the inner cylindrical surface of the connector and the outer cylindrical surface of the pipe is transformed from a solid state to a molten fluid state by power-on and heat-generation, and the polyethylene molecular chains are entangled and penetrated, so that the weld surface is integrated after cooling to room temperature, meeting the welding strength requirements.
[0061] The traction mechanism 6 is located at the outlet end of the oxide film scraping mechanism 5. The traction mechanism 6 is composed of a second wire drum, a second support frame and a driving motor. The second wire drum is rotatably arranged on the second support frame. The driving motor is fixedly arranged on the second support frame and connected to the second wire drum. The second wire drum can be driven to rotate by the driving motor, thereby driving the heating wire 7.2 to move in one direction at a uniform speed. Specifically, the heating wire 7.2 is introduced from the first wire drum into the overmolding mechanism 3 for overmolding, and the overmolded wire 7 is led out of the overmolding mechanism 3 for cooling, oxide film scraping and storage.
[0062] Example 2
[0063] In another typical embodiment of the present invention, a working method of a production device for improving the welding strength of electric fusion pipe fittings is provided, which is specifically as follows:
[0064] The heating wire 7.2 on the first wire drum of the wire drum support mechanism 2 is manually led out and sequentially passes through the first fixing member 3.2, the conical positioning member 3.3, the overmolding die head 3.4, the second fixing member 3.5, the cooling water tank 4, the oxide film scraping mechanism 5 and is wound on the second wire drum of the traction mechanism 6;
[0065] Start the power unit 1.1 and the driving motor on the traction mechanism 6. Under the action of the screw 1.3, the molten fluid plastic is transferred from the inside of the barrel 1.2 to the injection cavity 3.1.1 and flows into the overmolding cavity 3.4.3 of the overmolding die 3.4. The molten fluid plastic combines with the outer ring of the heating wire 7.2 in the overmolding cavity 3.4.3.
[0066] The second wire drum is driven by the driving motor to rotate to store the plastic-coated wire 7. Under the traction of the second wire drum, the plastic-coated wire 7 that has completed the plastic-coating work enters the cooling water tank 4 for cooling and then enters the oxide film scraping mechanism 5 to scrape the surface oxide film. After scraping, the plastic-coated wire 7 is wound on the second wire drum. At the same time, the heating wire 7.2 is pulled out from the first wire drum and extends into the plastic-coating molding mechanism 3 under the traction of the second wire drum to realize the unidirectional uniform movement of the heating wire 7.2.
[0067] Since the first channel 3.2.1, the second channel 3.3.4, the molding cavity 3.4.4 and the scraping cavity 5.4 are coaxially arranged, the heating wire 7.2 is always fixed in position and is always in a horizontal moving state during the continuous production process of the coated plastic, which effectively ensures the uniformity of the outer circle plastic coating layer 7.1 of the heating wire 7.2 and the uniformity of the scraping of the oxide layer, greatly improves the production quality of the plastic-coated wire 7, and controls the thickness of the plastic-coated wire 7 to be the thinnest. The thinner the plastic coating layer 7.1 of the plastic-coated wire 7, the faster the heat is transferred to the surface of the pipe per unit welding time, the higher the welding efficiency, shortens the welding time and improves the installation efficiency.
[0068] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A production device for improving the welding strength of electric fusion pipe fittings, It is characterized in that It includes a wire drum support mechanism, a plastic molding mechanism, a cooling water trough, an oxide film scraping mechanism and a traction mechanism which are arranged in sequence from front to back. The top of the plastic molding mechanism is fixedly connected to the plasticizing extrusion mechanism. The heating wire on the wire drum support mechanism horizontally passes through the plastic molding mechanism, the cooling water trough, the oxide film scraping mechanism in sequence and is connected to the traction mechanism. The heating wire can form a plastic-coated wire with a flat bottom cross-section and a local bulge at the center of the top in the plastic molding mechanism. The outermost layer of the plastic-coated wire is a plastic coating layer, which is polyethylene plastic. The inside of the plastic coating layer is the heating wire. The top of the plastic-coated wire adopts a local bulge design to accommodate the heating wire. The oxide film scraping mechanism is used to scrape off the oxide film on the outer surface of the plastic-coated wire after cooling; the oxide film scraping mechanism is fixedly arranged at the outlet end of the cooling water trough, and is composed of a scraper upper mold, a scraper lower mold and an adjustment screw for adjusting the scraping depth. The scraper upper mold and the scraper lower mold cooperate to form a scraping cavity with the same cross-section as the plastic-coated wire.
2. A production device for improving the welding strength of electric fusion pipe fittings according to claim 1, It is characterized in that The plasticizing extrusion mechanism consists of a vertically arranged barrel, a power unit fixedly arranged on the top of the barrel and connected to the screw inside the barrel, the outside of the barrel is wrapped with a heating ring along its length, and the bottom of the barrel is provided with a mounting port threadedly connected to the overmolding mechanism.
3. A production device for improving the welding strength of electric fusion pipe fittings according to claim 2, It is characterized in that The wire drum support mechanism consists of a first support frame and a first wire drum rotatably arranged on the first support frame; the traction mechanism consists of a second support frame and a second wire drum rotatably arranged on the second support frame, and a driving motor for driving the second wire drum to rotate is fixedly provided on the second support frame.
4. A production device for improving the welding strength of electric fusion pipe fittings according to claim 3, It is characterized in that The overmolding mechanism consists of a mold body, a conical positioning piece arranged inside the mold body, and an overmolding die head. The conical positioning piece is coaxially arranged with the overmolding die head, and the conical end of the conical positioning piece is inserted into the overmolding die head. The conical positioning piece is fixedly connected to the mold body through a first fixing piece, and the overmolding die head is fixedly connected to the mold body through a second fixing piece. The first fixing piece and the second fixing piece are relatively arranged on both sides of the mold body.
5. A production device for improving the welding strength of electric fusion pipe fittings according to claim 4, It is characterized in that An injection cavity is arranged in the mold body, and the conical positioning piece and the overmolding die head are arranged in the injection cavity. The top end of the mold body is threadedly connected with the plasticizing extrusion mechanism, and the injection cavity is communicated with the plasticizing extrusion mechanism.
6. A production device for improving the welding strength of electric fusion pipe fittings according to claim 5, It is characterized in that The first fixing part is composed of a flange and a circular boss fixedly arranged on the flange. The flange is fixedly connected to the mold body. The circular boss is inserted into the injection cavity to block the end of the injection cavity. The end of the circular boss is provided with a first positioning hole for positioning and installing the conical positioning part. A first channel is also provided in the first fixing part. The first channel runs through the first fixing part. The first channel is coaxially arranged with the first positioning hole. The diameter of the first channel is the same as the diameter of the heating wire.
7. A production device for improving the welding strength of electric fusion pipe fittings according to claim 6, It is characterized in that One end of the conical positioning piece is threadedly connected to the first positioning hole, and the other end extends into the injection mold. The end of the conical positioning piece inserted into the injection mold is a conical structure. A second channel is provided in the conical positioning piece. The second channel is coaxially arranged with the first channel. The second channel consists of a coaxially arranged flared section and a straight section. The flared section is close to the first channel and is larger in size than the first channel. The diameter of the straight section is the same as the diameter of the first channel.
8. A production device for improving the welding strength of electric fusion pipe fittings according to claim 7, It is characterized in that The overmolding die head is provided with a coaxially arranged overmolding cavity and a molding cavity. The overmolding cavity is a conical cavity structure. The size of the overmolding cavity is larger than the size of the insertion end of the conical positioning piece. The cross-section bottom of the molding cavity is flat and there is a local bulge at the center of the top.
9. A method for operating the production device for improving the welding strength of electric fusion pipe fittings as claimed in claim 8, It is characterized in that The details are as follows: Manually lead the heating wire on the first wire drum through the overmolding mechanism, the cooling water tank, the oxide film scraping mechanism in sequence and wind it on the second wire drum; The power unit and the driving motor are started, and the molten fluid plastic is transferred from the barrel to the injection molding cavity, and the molten fluid plastic is combined with the outer ring of the heating wire in the overmolding cavity; Under the traction of the second wire drum, the plastic-coated wire that has completed the plastic-coating work enters the cooling water tank for cooling and then enters the oxide film scraping mechanism to scrape the surface oxide film. After scraping, the plastic-coating is wound on the second wire drum. At the same time, the heating wire extends from the first wire drum and extends into the plastic-coating molding mechanism under the traction of the second wire drum.
Citation Information
Patent Citations
Reinforcing flexible guide pipe secondary coating extrusion device and molding process
CN103465454A
Electric heater band
CN103476159A
Electric smelting pipe fitting welding heating wire cladding die head device
CN205021952U
Rubber-coated wire and electric melting pipe fitting with same
CN215721593U
Manufacture of foaming insulation wire
JP1994295631A