A carbon fiber composite piston rod surface reinforcement structure

By using a combined structure of engineering plastic outer lining, SiC and BN fillers and diamond-like coating on the surface of the carbon fiber composite piston rod, the wear and fatigue problems of the piston rod in high-pressure environments are solved, achieving high hardness, low friction and good performance. Chemical stability.

CN115742477BActive Publication Date: 2024-10-25BEIJING RES INST OF PRECISE MECHATRONICS CONTROLS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211394120.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-08
Publication Date
2024-10-25
Estimated Expiration
2042-11-08

AI Technical Summary

Technical Problem

Carbon fiber composite piston rods are prone to friction and wear, local pitting corrosion and fatigue cracks under high-pressure, high-load, and high-speed working environments. The existing technology is difficult to meet the surface hardness, roughness, bonding strength of the coating or coating and the carbon fiber matrix, and High requirements for porosity, oil resistance and wear resistance.

Method used

It adopts a combined structure of engineering plastic outer lining, SiC and BN fillers and diamond-like coating. It is bonded by bonding epoxy resin, and uses physical vapor deposition process to prepare the diamond-like coating. The coating temperature is controlled below 170°C. The thickness is 2~4μm.

Benefits of technology

Significantly improves the hardness, wear resistance and low friction coefficient of the piston rod surface, enhances the density and chemical stability of the film layer, and ensures high strength and low friction performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115742477B_ABST
    Figure CN115742477B_ABST
Patent Text Reader

Abstract

A carbon fiber composite piston rod surface enhancement structure includes a polyimide outer lining, SiC and BN fillers and a diamond-like coating; the polyimide outer lining is bonded to the piston rod body, i.e., the carbon fiber material matrix, through epoxy resin, SiC and BN fillers are added to the surface of the polyimide outer lining, and a diamond-like coating is provided on the outer surface of the filler. The carbon fiber piston rod of the present invention uses engineering plastics with excellent mechanical properties as a wear-resistant outer lining, and by adding fillers, the surface hardness and wear resistance of the piston rod outer lining are further improved, and the friction coefficient is reduced. The outer lining and the carbon fiber tube are bonded with high-temperature resistant epoxy resin, and the bonding strength can reach more than 20MPa. The diamond-like coating (DLC) is used as the coating of the piston rod outer lining by adopting a physical vapor deposition (PVD) process method, so as to achieve high hardness, low friction coefficient, excellent film density, good chemical stability and good optical properties on the outer surface of the piston rod.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an electro-hydraulic servo mechanism for a launch vehicle, in particular to a carbon fiber composite material piston rod surface enhancement structure. Background Art

[0002] Lightweighting of onboard equipment is one of the effective ways to improve rocket carrying capacity. The development and application of new high-strength and low-density materials is one of the effective ways to achieve lightweighting. Carbon fiber reinforced composite materials (CFRP) have the advantages of thermal shock resistance, high tensile strength, and corrosion resistance. They have been widely used in robotics, aerospace, engineering equipment and other fields. Using CFRP to prepare hydraulic cylinders can greatly improve the lightweight level of hydraulic systems, help the system reduce energy consumption, and thus achieve higher specific power.

[0003] At present, one of the key technologies in the design of carbon fiber composite piston rods based on lightweight development is the surface enhancement treatment of composite piston rods. Due to the working characteristics of the actuator itself, the piston rod reciprocates in the actuator cylinder. Since the hydraulic piston rod is in a high-pressure, high-load, and high-speed working environment for a long time, its surface is prone to friction and wear, local pitting, and fatigue cracks.

[0004] Therefore, special research is needed on the surface enhancement or surface modification of composite piston rods to meet the high requirements of the piston rod on the outer surface hardness, roughness, bonding strength between the plating or coating and the carbon fiber matrix, porosity, oil resistance and wear resistance, so as to improve the strength, hardness, wear resistance and corrosion resistance of the piston rod surface. Summary of the invention

[0005] The technical problem solved by the present invention is to overcome the deficiencies of the prior art and provide a carbon fiber composite material piston rod surface reinforcement structure.

[0006] The technical solution of the present invention is: a carbon fiber composite piston rod surface enhancement structure, including an engineering plastic outer liner, SiC and BN fillers and a diamond-like coating;

[0007] The engineering plastic outer liner is bonded to the piston rod body, that is, the carbon fiber material matrix, as a whole. SiC and BN fillers are added to the surface of the engineering plastic outer liner, and a diamond-like coating is arranged on the outer surface of the filler.

[0008] Preferably, the gap between the inner diameter of the engineering plastic outer liner and the outer diameter of the piston rod is 0.3-0.8 mm.

[0009] Preferably, the adhesive for bonding the engineering plastic outer lining and the carbon fiber matrix of the piston rod is a high temperature adhesive of the epoxy resin type.

[0010] Preferably, a physical vapor deposition process is used to prepare a diamond-like coating on the outer surface of an engineering plastic outer liner filled with SiC and BN fillers.

[0011] Preferably, the temperature of the diamond-like carbon coating is controlled below 170°C.

[0012] Preferably, the thickness of the diamond-like carbon coating is 2-4 μm.

[0013] Preferably, the engineering plastic outer lining is a polyimide outer lining or a polyurethane outer lining.

[0014] The beneficial effects of the present invention compared with the prior art are:

[0015] The carbon fiber piston rod of the present invention adopts engineering plastics with excellent mechanical properties as the wear-resistant outer lining, and by adding fillers, the surface hardness and wear resistance of the piston rod outer lining are further improved, and the friction coefficient is reduced. The outer lining and the carbon fiber tube are bonded with high-temperature resistant epoxy resin, and the bonding strength can reach more than 20MPa. The physical vapor deposition (PVD) process method is adopted to use diamond-like coating (DLC) as the coating of the piston rod outer lining. This enhanced structural design including high-strength engineering plastic outer lining, SiC and BN fillers and diamond-like coating effectively ensures the high hardness (HV3500 or above) of the outer surface of the piston rod, low friction coefficient (0.08), excellent film density and good chemical stability. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 Schematic diagram of the surface enhancement structure of the carbon fiber composite piston rod; DETAILED DESCRIPTION

[0017] The present invention is described in detail below with reference to the accompanying drawings and examples.

[0018] Carbon fiber composite piston rod structure Figure 1 As shown, the piston rod body is a carbon fiber material matrix 1, and the piston rod surface reinforcement structure is composed of a polyimide outer lining 3, SiC and BN fillers 4 and a diamond-like carbon DLC coating 5.

[0019] The adhesive for the polyimide outer lining and the carbon fiber matrix of the piston rod can be selected from high-temperature adhesives such as epoxy resins. The present invention uses high-temperature resistant epoxy resin 2 to bond the carbon fiber material matrix 1 as a whole. In order to ensure firm and convenient bonding, a certain gap should be reserved between the inner diameter of the polyimide outer lining 3 and the outer diameter of the piston rod. The gap is designed to be 0.3 to 0.8 mm in the present invention.

[0020] SiC and BN fillers 4 are added to the surface of the polyimide outer lining 3. Polyimide outer lining test pieces with added SiC and BN fillers 4, conventional metal outer lining test pieces and conventional polyimide outer lining test pieces were respectively made, and friction comparison tests were carried out. Both the metal test pieces and the conventional polyimide outer lining test pieces showed clear wear marks and produced obvious wear debris. There are almost no wear marks on the surface of the polyimide outer lining test piece to which SiC and BN fillers 4 are added according to the present invention. The test results show that the addition of SiC and BN fillers 4 has a good effect on reducing the friction coefficient of the outer surface of the polyimide outer lining and improving the hardness and wear resistance of the outer surface of the polyimide outer lining. After the outer surface of the polyimide outer lining is filled with SiC and BN fillers, the hardness and wear resistance can be greatly improved compared with ordinary polyimide materials.

[0021] On the outer surface of the polyimide liner 3 filled with SiC and BN fillers 4, a coating is prepared by a physical vapor deposition (PVD) process. This process can deposit a film layer on the outer surface of the liner, improve the interface of the film substrate, and increase the deposition rate.

[0022] The coating is diamond-like coating (DLC) 5. In order to prevent the epoxy resin bonding between the outer lining and the carbon fiber tube and the epoxy resin inside the carbon fiber from failing at high temperature, the temperature of the DLC coating is controlled below 170°C. Through a preliminary test, the DLC coating on the polyimide surface can reach 2 to 3 μm. The diamond-like coating of the present invention is designed on the outermost layer of the reinforcement structure, which ensures that the outer lining surface has excellent film density and good chemical stability. Compared with the surface roughness of plasma sprayed aluminum oxide coating, electroplated nickel and special resin on the carbon fiber surface, which is difficult to reduce and the film density is insufficient, the diamond-like coating (DLC) 5 has many excellent characteristics: high hardness (HV3500 or above); low friction coefficient (0.08); excellent film density; good chemical stability and good optical properties. The present invention selects diamond-like coating (DLC) 5 as the outermost material of the piston rod surface reinforcement structure, which ensures that the outer surface of the piston rod has a low friction coefficient and high film density, and further strengthens the hardness of the reinforcement structure.

[0023] In addition, the surface reinforcement combination of SiC, BN filler and diamond-like coating in the present invention is universal and suitable for use in combination with a variety of high-strength engineering plastics as a reinforcement structure. Other high-strength engineering plastics such as polyurethane can be used to replace the polyimide outer lining to form a reinforcement structure.

[0024] The contents not described in detail in the specification of the present invention belong to the common knowledge of the professionals in this field.

Claims

1. A carbon fiber composite piston rod surface enhancement structure, Features: Including engineering plastic lining, SiC and BN fillers and diamond-like coating; The engineering plastic outer lining is bonded to the piston rod body, i.e., the carbon fiber material matrix, as a whole, SiC and BN fillers are added to the surface of the engineering plastic outer lining, and a diamond-like coating is provided on the outer surface of the filler; The gap between the inner diameter of the engineering plastic outer lining and the outer diameter of the piston rod is 0.3-0.8 mm; the adhesive between the engineering plastic outer lining and the carbon fiber matrix of the piston rod is selected from epoxy resin high temperature glue; the engineering plastic outer lining is a polyimide outer lining or a polyurethane outer lining.

2. The carbon fiber composite piston rod surface enhancement structure according to claim 1, Features: A diamond-like coating is prepared on the outer surface of an engineering plastic liner filled with SiC and BN fillers by using a physical vapor deposition process.

3. The carbon fiber composite piston rod surface enhancement structure according to claim 1, Features: The temperature of the diamond-like carbon coating is controlled below 170°C.