A preparation method of hydroquinone dihydroxyethyl ether (HQEE)
Through the reaction of hydroquinone with an alkaline catalyst and liquid ethylene oxide, combined with inert gas protection and activated carbon decolorization, the problems of low yield and high cost in the preparation process of HQEE are solved, and high-purity and efficient products are achieved preparation, simplifying the process and reducing environmental pollution.
Patent Information
- Application Number
- CN202211458410.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-17
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-11-17
AI Technical Summary
The existing preparation method of hydroquinone dihydroxyethyl ether (HQEE) has problems such as low yield, long preparation time, high raw material cost, complex production process and environmental pollution, resulting in low industrialization value and low competitiveness.
Mix hydroquinone, water and alkaline catalyst, react with liquid ethylene oxide under the protection of inert gas, control the temperature and pressure, then neutralize and filter, use activated carbon to decolorize and wash, and finally pass through hot filtration and drying Obtain high purity HQEE.
Efficient preparation of HQEE has been achieved, with a product yield of over 99.5%, simplifying the process route, reducing wastewater generation, improving product quality and safety, and controlling the platinum-cobalt chromaticity below 10.
Abstract
Description
Technical Field
[0001] The invention relates to the field of polyurethane chain extenders, in particular to a method for preparing hydroquinone dihydroxyethyl ether (HQEE). Background Art
[0002] Hydroquinone dihydroxyethyl ether (HQEE for short) is a symmetrical aromatic diol chain extender with no toxicity or irritation. HQEE is mainly used as a chain extender for polyurethane elastomers and a crosslinker for mixing, casting and thermoplastic polyurethane elastomers. It can improve the stability of products and improve various physical properties such as tear strength, heat resistance, hardness, elasticity, compression deformation, etc. It can be especially used in MDI series products and has good compatibility with MDI, which can effectively extend the life of the kettle and facilitate operation.
[0003] There are three main preparation routes for hydroquinone dihydroxyethyl ether (HQEE for short).
[0004] Patent PL100649 reports that hydroquinone is first salted with sodium hydroxide and then reacted with chloroethanol to form an ether to prepare HQEE, with a product yield of about 79%. This route has a low yield for preparing HQEE, a long preparation time, sodium hydroxide as a raw material, not a catalyst, and chloroethanol is expensive, resulting in a high cost of raw materials. This route has basically no industrial value.
[0005] Japanese patent JP2011148886 reported that hydroquinone and ethylene carbonate were reacted to prepare HQEE under potassium carbonate catalysis using DMF as a reaction solvent. This route uses DMF, the reaction temperature is too high to reach 160°C, carbon dioxide is produced during the reaction, the post-processing is cumbersome, and the operation steps are increased, which not only pollutes the environment, but also has high production costs. This route is not very competitive.
[0006] Chinese patent CN101244989 reports that in the sodium carbonate catalyst, hydroquinone and ethylene oxide react, there are three treatment methods after the reaction. One treatment method obtains molten HQEE after dehydration, and the product appearance is pink. The HQEE content obtained by this treatment method cannot reach more than 99.5%. The second treatment method adds water to cool down and obtains HQEE. The product appearance is pink and the product quality is not good. The third treatment method, in order to obtain a product with good appearance, adds sodium sulfite for protection, and obtains white HQEE. The protection effect of sodium sulfite is not so good. According to this method, good quality HQEE cannot be obtained. Summary of the invention
[0007] The present invention aims to provide a method for preparing hydroquinone dihydroxyethyl ether (HQEE).
[0008] To achieve the above purpose, the present invention adopts the following technical solution:
[0009] A method for preparing hydroquinone dihydroxyethyl ether (HQEE),
[0010] The hydroquinone, water and alkaline catalyst are mixed, and liquid ethylene oxide is added under the protection of inert gas. After sealing, the temperature is raised to 70-75°C for reaction, and the reaction pressure is between 0.2-0.6Mpa (preferably 0.2-0.4Mpa). After the reaction is completed, the system is vented, and then acid is added for neutralization, and then the temperature is lowered and filtered to obtain a wet filter cake, which is hydroquinone dihydroxyethyl ether; the wet filter cake, solvent and activated carbon are mixed, and the temperature is raised to 60-100°C for decolorization, and then hot filtration is performed while hot to remove the activated carbon, and the filtrate is cooled under stirring, filtered, washed, and dried to obtain the refined qualified HQEE.
[0011] Hydroquinone, water and alkaline catalyst are added into a high-pressure reactor. After the inert gas replacement is completed, liquid ethylene oxide is added under the protection of the inert gas. After sealing, the temperature is controlled to rise to 70-75° C. for 1-2 hours and the reaction is carried out for 6-10 hours. The reaction pressure is between 0.2-0.6Mpa. Among them, the amount of water added is 3-8 times (preferably 4-6 times) the weight of hydroquinone, and the amount of alkaline catalyst added is 1-10% (preferably 1.5-4%) of the molar amount of hydroquinone; the molar ratio of ethylene oxide to hydroquinone is 2-2.6:1, preferably 2.2-2.4:1.
[0012] The inert gas is nitrogen or argon, preferably nitrogen;
[0013] The alkaline catalyst is sodium hydroxide or potassium hydroxide, preferably sodium hydroxide.
[0014] After the reaction is completed, the system is emptied, acid is added for full neutralization, and then the temperature is lowered according to the cooling program, filtered, and washed to obtain a wet HQEE product with a solid content of about 80%. The filtrate is collected for standby use.
[0015] The cooling procedure is as follows: first cool to 55-60°C, stir until a large amount of material precipitates, then slowly cool to 20-25°C and stir for 2 hours, then cool to 2-6°C with chilled brine and stir for 2 hours.
[0016] The wet filter cake, solvent and activated carbon are mixed, heated to 60-100°C for decolorization for 1-4 hours, then hot filtered to remove the activated carbon while hot, and the filter cake is washed and the filtrate is combined.
[0017] The obtained filtrate is subjected to a cooling program, filtered, washed and dried to obtain qualified HQEE with a content greater than 99.5% and a platinum-cobalt chromaticity of less than 10.
[0018] The cooling procedure is as follows: first cool to 55-60°C, stir until a large amount of material precipitates, then slowly cool to 20-25°C and stir for 2 hours, then cool to 2-6°C with chilled brine and stir for 2 hours.
[0019] The solvent is one or more of water, methanol aqueous solution (wherein the methanol concentration is 0-100%) or 0-100% ethanol aqueous solution (wherein the ethanol concentration is 0-100%), preferably water or 5-20% methanol aqueous solution; the amount of solvent used is 2-6 times the dry amount of HQEE wet product; the amount of activated carbon used is 0.1-10% of the dry amount of HQEE wet product.
[0020] During the preparation and purification process, the mother liquor is collected by filtration and can be used separately.
[0021] The advantages of the present invention are:
[0022] The preparation and purification method of hydroquinone dihydroxyethyl ether (HQEE) of the present invention has the characteristics of simple process route, easy industrial implementation, high product yield, etc. compared with the existing route. The preparation and post-treatment process of hydroquinone dihydroxyethyl ether (HQEE) of the present invention does not generate waste water, and the mother liquor generated by the preparation and post-treatment can be used after recovery, and the use does not affect the product quality. The preparation process uses water as a reaction solvent to greatly improve the safety of the reaction, and uses activated carbon, water or an aqueous solution of alcohol as a post-treatment method to greatly improve the product quality. The product content can reach more than 99.5%, and the content of the final product in the embodiment is greater than 99.5%, and the platinum cobalt chromaticity can be controlled below 10. DETAILED DESCRIPTION
[0023] The present invention is further described in detail by the following examples, but the present invention is by no means limited thereto. In the following examples, the content of hydroquinone used is greater than 99%, and the content of ethylene oxide is greater than 98%.
[0024] Example 1
[0025] 44g hydroquinone, 0.8g sodium hydroxide and 270g water were added to the autoclave in sequence. After nitrogen replacement was completed three times, 40.5g ethylene oxide was added at one time through the balance tube, and the temperature was raised to 70-75°C within 1h, and the mixture was kept warm and stirred for 6h at this temperature. The maximum reaction pressure was 0.35Mpa. After completion, the system was emptied, 2.1g hydrochloric acid was added to fully neutralize, and the central control sampling showed that there was no raw material, and the product selectivity reached 98.7%. The temperature was lowered to 55-60°C while stirring until a large amount of material precipitated, and then slowly cooled to 20-25°C and stirred for 2 hours, and then cooled to 6°C with frozen brine and stirred for 2h. Filtered and washed to obtain 90g of gray-white wet cake with a GC normalized content of 99.4%. 267.7g of the preparation mother liquor was obtained by filtration.
[0026] The HQEE wet cake was put into 160g water and 5g activated carbon was added, and the mixture was stirred and decolorized at 85-90℃ for 4 hours, filtered while hot, and the activated carbon cake was rinsed with 10g hot water. The combined filtrate was put into a crystallization bottle, cooled to 55-60℃ with stirring until a large amount of material precipitated, and then slowly cooled to 20-25℃ and stirred for 2 hours, and then cooled to 6℃ with frozen brine and stirred for 2h, filtered, washed, and vacuum dried to obtain 67.5g of pure white solid with a normalized content of 99.8% and a platinum-cobalt chromaticity of 7. 147.6g of post-treatment mother liquor was obtained by filtration.
[0027] Taking HQEE produced by Solvay as a standard sample, the quantitative content of HQEE prepared above is 100.5%, the melting point is 107.8-108.0°C, and the platinum-cobalt chromaticity of HQEE produced by Solvay is 28.
[0028] Example 2
[0029] 44g hydroquinone, 1.3g potassium hydroxide and 220g water were added to the autoclave in sequence. After nitrogen replacement was completed three times, 42.5g ethylene oxide was added at one time through the balance tube, and the temperature was raised to 70-75°C within 1.5h, and the mixture was kept warm and stirred for 8h at this temperature. The maximum reaction pressure was 0.37Mpa. After completion, the system was emptied, 3.3g hydrochloric acid was added to fully neutralize, and the sampling control showed that the raw material was absent and the product selectivity reached 98.5%. The temperature was lowered to 55-60°C while stirring until a large amount of material precipitated, and then slowly cooled to 20-25°C and stirred for 2 hours, and then cooled to 4°C with frozen brine and stirred for 2h. Filtered and washed to obtain 95g of gray-white wet cake with a GC normalized content of 99.2%.
[0030] Put the HQEE wet cake into 150g water and add 3g activated carbon, keep warm and stir at 85-90℃ for 3 hours to decolorize, filter while hot, rinse the activated carbon cake with 10g hot water, combine the filtrate and put it into a crystallization bottle, cool down to 55-60℃ with stirring until a large amount of material precipitates, then slowly cool down to 20-25℃ and stir for 2 hours, then cool down to 4℃ with frozen brine and stir for 2h, filter, wash and vacuum dry to obtain 70.3g of pure white solid with a normalized content of 99.7% and a platinum-cobalt chromaticity of 9.
[0031] Taking HQEE produced by Solvay as a standard sample, the quantitative content of HQEE prepared above is 100.1%, and the platinum-cobalt chromaticity of HQEE produced by Solvay is 28.
[0032] Example 3
[0033] 44g hydroquinone, 2.2g sodium hydroxide and 240g water were added to the autoclave in sequence. After nitrogen replacement was completed three times, 38.8g ethylene oxide was added at one time through a balance tube. The temperature was raised to 70-75°C within 2 hours, and the mixture was stirred at this temperature for 9 hours. The maximum reaction pressure was 0.33Mpa. After completion, the system was emptied, 5.6g hydrochloric acid was added to fully neutralize, and sampling was performed. The raw material was free, and the product selectivity reached 98.1%. The temperature was lowered to 55-60°C while stirring until a large amount of material precipitated, and then slowly cooled to 20-25°C and stirred for 2 hours, and then cooled to 4°C with frozen brine and stirred for 2 hours. Filtered and washed to obtain 85g of gray-white wet cake with a GC normalized content of 99.1%.
[0034] The HQEE wet cake was put into 160g methanol aqueous solution (methanol concentration 15%), and 2.5g activated carbon was added, and the mixture was stirred and decolorized at 85-90°C for 2 hours, filtered while hot, and the activated carbon cake was rinsed with 10g hot water. The combined filtrate was put into a crystallization bottle, cooled to 55-60°C with stirring until a large amount of material precipitated, and then slowly cooled to 20-25°C and stirred for 2 hours, and then cooled to 4°C with frozen brine and stirred for 2h. After filtering, washing and vacuum drying, 64.1g of pure white solid was obtained, with a normalized content of 99.9% and a platinum-cobalt chromaticity of 2.
[0035] Taking HQEE produced by Solvay as the standard sample, the quantitative content of homemade HQEE is 100.6%, and the platinum-cobalt chromaticity of HQEE produced by Solvay is 28.
[0036] Example 4
[0037] The wet filter cake was prepared according to the operation of Example 1.
[0038] The HQEE wet cake was put into 160g ethanol aqueous solution (ethanol concentration 15%), and 2.5g activated carbon was added, and the mixture was stirred and decolorized at 85-90°C for 1 hour, filtered while hot, and the activated carbon cake was rinsed with 10g hot water. The combined filtrate was put into a crystallization bottle, cooled to 55-60°C with stirring until a large amount of material precipitated, and then slowly cooled to 20-25°C and stirred for 2 hours, and then cooled to 2°C with frozen brine and stirred for 2h. After filtering, washing and vacuum drying, 66.4g of pure white solid was obtained, with a normalized content of 99.9% and a platinum-cobalt chromaticity of 3.
[0039] Taking HQEE produced by Solvay as the standard sample, the quantitative content of homemade HQEE is 100.4%, and the platinum-cobalt chromaticity of HQEE produced by Solvay is 28.
[0040] Example 5
[0041] 267.7 g of the preparation mother liquor and 147.6 g of the post-treatment mother liquor obtained in Example 1 were respectively subjected to reduced pressure to recover water, and the obtained water was then applied to the preparation and post-treatment processes respectively according to the dosage and conditions recorded in Example 1 (the water loss part was supplemented with fresh water), and 68.4 g of qualified HQEE was obtained, with a content of 99.7% and a platinum-cobalt chromaticity of 8.
Claims
1. A method for preparing hydroquinone dihydroxyethyl ether (HQEE), characterized in that: Mix hydroquinone, water and alkaline catalyst, add liquid ethylene oxide under the protection of inert gas, seal, heat to 70-75°C for reaction, reaction pressure is between 0.2-0.6Mpa, after the reaction is completed, vent the system, then add acid for neutralization, then cool down, filter to obtain wet cake, which is hydroquinone dihydroxyethyl ether; mix the wet cake, solvent and activated carbon, heat to 60-100°C for decolorization, then filter to remove activated carbon while hot, cool the filtrate under stirring, filter, wash and dry to obtain refined qualified HQEE; The amount of water added is 3-8 times the weight of hydroquinone, the amount of alkaline catalyst added is 1-10% of the molar amount of hydroquinone; the molar ratio of ethylene oxide to hydroquinone is 2-2.6:1; After the reaction is completed, the system is emptied, acid is added for full neutralization, and then the temperature is lowered according to the cooling program, filtered, and washed to obtain a wet HQEE product with a solid content of 80%, and the filtrate is collected for standby use; The wet filter cake, solvent and activated carbon are mixed, heated to 60-100°C for decolorization for 1-4 hours, then hot filtered to remove the activated carbon while hot, and the filter cake is washed and the filtrate is combined; The cooling procedure is as follows: first cool to 55-60°C, stir until a large amount of material precipitates, then slowly cool to 20-25°C and stir for 2 hours, then cool to 2-6°C with frozen brine and stir for 2 hours; The solvent is one or more of water, methanol aqueous solution or 0-100% ethanol aqueous solution, wherein the methanol concentration is 0-100%, and the ethanol concentration is 0-100%; the amount of solvent used is 2-6 times the dry HQEE wet product; the amount of activated carbon used is 0.1-10% of the dry HQEE wet product.
2. The method for preparing hydroquinone dihydroxyethyl ether (HQEE) according to claim 1, characterized in that: The inert gas is nitrogen or argon; The alkaline catalyst is sodium hydroxide or potassium hydroxide.
3. The method for preparing hydroquinone dihydroxyethyl ether (HQEE) according to claim 1, characterized in that: The obtained filtrate is cooled by a cooling program, filtered, washed and dried to obtain qualified HQEE with a content greater than 99.5% and a platinum-cobalt chromaticity controlled below 10.
4. The method according to claim 1, characterized in that During the preparation and refining process, the mother liquor is collected by filtration and can be used separately.