A method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester

By using a composite catalyst composed of anhydrous sulfate, α-hydroxy acid and boric acid, the synthesis reaction rate and selectivity of the long-chain fatty acid isoborone esters are improved, and the problems of low reaction rate and catalyst deactivation in the prior art are solved. , achieving an efficient and environmentally friendly production process.

CN115872860BActive Publication Date: 2024-11-29GUANGXI FORESTRY RES INST
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211507588.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-29
Publication Date
2024-11-29
Estimated Expiration
2042-11-29

AI Technical Summary

Technical Problem

In the prior art, the synthesis reaction rate of the long-chain fatty acid isoborone is low, resulting in increased energy consumption, increased side reactions and deepened product color, and the catalyst is quickly deactivated and not easy to regenerate.

Method used

Using a composite catalyst composed of anhydrous sulfate, α-hydroxy acid and boric acid, the reaction temperature is controlled at 80-90°C and the reaction time is 15-24 hours. Through synthesis, filtration, water washing, product purification, solvent recovery and product purification Steps to improve reaction rate and selectivity.

Benefits of technology

It significantly improves the reaction rate and the reusability of the catalyst, reduces energy consumption and cost, and the product selectivity reaches more than 90%, and has excellent color. It is suitable as a green solvent and surfactant.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester, and belongs to the technical field of deep processing of forest chemical products. The method includes steps such as synthesis reaction, filtration, washing, product purification, solvent recovery, and product refining. Due to the large molecular weight of long-chain fatty acids, the reaction rate with camphene is low, which increases energy consumption and power costs. The present invention preferably obtains a composite catalyst composed of sulfate, α-hydroxycarboxylic acid and boric acid, and applies it to the synthesis reaction step to effectively improve the rate of the synthesis reaction of long-chain fatty acid isoborneol ester, and greatly reduce energy consumption costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of deep processing of forest chemical products, and in particular to a method for accelerating the reaction rate of isoborneol ester, a long-chain fatty acid synthesized from camphene. Background Art

[0002] Long-chain fatty acid isoborneol ester can be used as a green solvent, surfactant, plasticizer, etc., and has important applications in the fields of medicine and high-end material manufacturing. The reaction of camphene esterification to prepare long-chain fatty acid isoborneol ester can be divided into homogeneous catalysis and heterogeneous catalysis according to the reaction system. Homogeneous catalysis uses liquid inorganic acids such as sulfuric acid as catalysts. This type of catalytic reaction has problems such as poor selectivity, many by-products, difficulty in subsequent separation, easy corrosion of equipment, and generation of large amounts of acid-containing wastewater. Heterogeneous catalysis uses ion exchange resins, zeolites, molecular sieves, etc. as catalysts, but problems such as rapid catalyst deactivation and difficulty in regeneration are common in industry.

[0003] In order to solve the problems existing in the prior art, technicians are constantly looking for new catalysts to improve the selectivity of the esterification reaction of camphene, increase the reusability and environmental protection of the catalyst. For example, Gu Yuncui et al. used sulfuric acid as a catalyst in their published paper "Factors affecting the esterification reaction of low-level fatty acids and camphene and the preparation of C1-C5 carboxylic acid isoborneol esters", explored the factors affecting the esterification reaction of camphene and low-level fatty acids, and prepared C1-C5 short-chain carboxylic acid isoborneol esters (Fragrances, Fragrances and Cosmetics, 2013, Supplement). Chinese patent application CN201711290727.8 discloses a functionalized polyacid ionic liquid agent and a method for catalyzing the synthesis of isoborneol acetate using the same. The method for catalyzing the synthesis of isoborneol acetate uses camphene and acetic acid as raw materials, and uses a functionalized polyacid ionic liquid as a catalyst to prepare isoborneol acetate through an esterification reaction. Cui Juntao et al. published a paper titled "Study on the synthesis of isoborneol acetate by Lewis acid-catalyzed isoesterification of camphene". They disclosed the use of ferric chloride as a catalyst to catalyze the esterification of camphene with glacial acetic acid to prepare isoborneol acetate. However, ferric chloride is highly irritating and corrosive (Chemistry and Industry of Forest Products, 2018, 38(1)).

[0004] Since long-chain fatty acids have large molecular weight and low reactivity, it often takes a long time to react with camphene, which increases energy consumption and power costs, and also causes more side reactions and darker product colors. Therefore, screening for suitable catalysts has become a new research direction. Summary of the invention

[0005] The invention provides a method for accelerating the reaction rate of synthesizing long-chain fatty acid isoborneol ester in order to overcome the problem of low reaction rate in the synthesis of long-chain fatty acid isoborneol ester.

[0006] In order to achieve the above objectives, the present invention is implemented through the following technical solutions:

[0007] A method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester comprises the following steps: synthesis reaction, filtration, water washing, product purification, solvent recovery, and product refining. In the synthesis reaction step, the following steps are included:

[0008] Add camphene and long-chain fatty acids in a molar ratio of 1:1.2-1.6 and a composite catalyst to camphene in a mass ratio of 0.05-0.3:1 into a reactor, start stirring, control the reaction temperature to 80-90°C and the reaction time to 15-24h; the composite catalyst is composed of anhydrous sulfate, α-hydroxy acid and boric acid in a mass ratio of 1:1:0.5-1.

[0009] Preferably, the anhydrous sulfate includes one or more of iron sulfate, zirconium sulfate and titanium sulfate.

[0010] Preferably, the α-hydroxycarboxylic acid includes one or more of tartaric acid, citric acid, malic acid, mandelic acid, lactic acid, and glycolic acid.

[0011] Preferably, the boric acid is dehydrated boric acid heated at a temperature of 105-110° C. for 1 hour.

[0012] Preferably, the filtering step is as follows: after the reaction is completed, the liquid product is allowed to stand, filtered and moved into a water washing tank, and then an organic solvent is added to the reactor to wash the solid catalyst at the bottom of the reactor, and the washing liquid is filtered and moved into the water washing tank.

[0013] Preferably, the water washing step is as follows: adding a certain mass of water and controlling the water temperature for washing to obtain a mixture of long-chain fatty acids and long-chain fatty acid isoborneol esters.

[0014] Preferably, the product purification step is as follows: adding an organic solvent to the mixture obtained by water washing to dissolve it, then dropping an alkaline solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution.

[0015] Preferably, the alkaline solution includes one of a potassium hydroxide solution and a sodium hydroxide solution.

[0016] Preferably, the solvent recovery step is as follows: recovering the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester.

[0017] Preferably, the product refining step is as follows: the crude long-chain fatty acid isoborneol ester obtained in the solvent recovery step is subjected to vacuum distillation to remove light components such as camphene and terpinene to obtain fine long-chain fatty acid isoborneol ester.

[0018] Compared with the prior art, the advantages and beneficial effects of the present invention are:

[0019] 1. The composite catalyst used in the present invention has the advantages of easy and simple preparation of raw materials, good repeatability, non-toxicity, low corrosiveness, and easy industrial production. The catalytic activity is more than 1 times higher than that of a single component.

[0020] 2. The composite catalyst used in the present invention can reduce the reaction temperature to only 80-90° C. without increasing the amount of catalyst, which can greatly save energy consumption, but can accelerate the reaction rate, and the reaction can be completed within 24 hours.

[0021] 3. the composite catalyst used by the present invention, target product selectivity ≥ 90%. Side reactions such as isomerization and polymerization do not occur in camphene, which is beneficial to the preparation of high-quality long-chain fatty acid isoborneol ester products. Using concentrated sulfuric acid as catalyst, product color is black, and using composite catalyst of the present invention, product color is light yellow, high quality, can omit decolorization step, reduce cost.

[0022] 4. The composite catalyst of the method of the present invention can be recovered and reused after the reaction is completed.

[0023] 5. The purity of the long-chain fatty acid isoborneol ester prepared by the present invention can reach more than 99%, and it can be used as a green solvent, surfactant, and plasticizer, and has a high value for promotion and application.

[0024] 6. because the molecular weight of long-chain fatty acid is larger, and the reaction rate with amphene is low, energy consumption and power cost are increased, the present invention, by preferably obtaining the composite catalyst of sulfate, alpha-hydroxycarboxylic acid and boric acid composition, applies it to be used in the long-chain fatty acid isoborneol ester building-up reaction and can effectively improve the speed of building-up reactions, and greatly reduces energy consumption cost. DETAILED DESCRIPTION

[0025] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as limiting the present invention, but should be understood as a more detailed description of certain aspects, features, and embodiments of the present invention.

[0026] It should be understood that the terms described in the present invention are only for describing special embodiments and are not intended to limit the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper and lower limits of the scope is also specifically disclosed. Each smaller range between the intermediate value in any stated value or stated range and any other stated value or intermediate value in the described range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.

[0027] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials associated with the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.

[0028] It will be apparent to those skilled in the art that various modifications and variations may be made to the specific embodiments of the present invention description without departing from the scope or spirit of the present invention. Other embodiments derived from the present invention description will be apparent to those skilled in the art. The present application description and examples are exemplary only.

[0029] The words “include,” “including,” “have,” “contain,” etc. used in this document are open-ended terms, meaning including but not limited to.

[0030] Example or control sample analysis test method

[0031] Analytical instrument: Aglient7890A gas chromatograph, Agilent, USA; Chromatographic column: AT-35, quartz capillary column (60m×0.25mm×0.25μm). GC analysis conditions: Carrier gas, high-purity nitrogen; Program temperature: 70℃ (2min), increase to 150℃ at 50℃ / min, stay for 3min, increase to 230℃ at 30℃ / min, stay for 40min; Injection port temperature: 250℃, total flow rate 130.5ml / min, split ratio 50:1, septum purge 3ml / min; FID detection, detection port temperature: 250℃, hydrogen flow rate 40ml / min, air 450ml / min, nitrogen purge, 25ml / min. Injection volume 0.2ul.

[0032] The area normalization method was used to approximate the conversion amount of camphene by subtracting the GC content of camphene in the product from the GC content of camphene in the raw material.

[0033] Camphene conversion rate = (GC content of camphene in the raw material - GC content of camphene in the product) / GC content of camphene in the raw material.

[0034] Example 1

[0035] A method for accelerating the synthesis reaction rate of isoborneol laurate, comprising the following steps:

[0036] (1) Synthesis reaction: camphene and long-chain fatty acids are added into a reactor in a molar ratio of 1:1.6 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 80°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1;

[0037] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice, and the washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0038] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0039] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0040] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0041] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0042] Because lauric acid feeding is excessive, need to weigh the degree of reaction by the conversion situation of amphene.The amphene used in the experiment is industrial amphene, and the GC content of amphene is 86%, and the GC content of tricyclic alkene is 13% (same as the following embodiment).After reaction finishes, analyze by product, the transformation efficiency of amphene is 88%; The GC content of isoborneol laurate after product refining is 93.5%, and the GC content of fenchyl laurate is 3.9% and pine laurate 2.6%.

[0043] Example 2

[0044] A method for accelerating the synthesis reaction rate of isoborneol laurate, comprising the following steps:

[0045] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 80°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous ferric sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1;

[0046] (2) Filtration: After the reaction of step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice, and the washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is methyl acetate;

[0047] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0048] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0049] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0050] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0051] Since the lauric acid feed is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 90% through product analysis; the GC content of isoborneol laurate after refining is 96.5%, the GC content of fenchyl laurate is 1.8% and the GC content of pinyl laurate is 2.7%.

[0052] Example 3

[0053] A method for accelerating the synthesis reaction rate of isoborneol laurate, comprising the following steps:

[0054] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene in a mass ratio of 0.25:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 80°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous titanium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:0.5;

[0055] (2) Filtration: After the reaction of step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate and hexane in a mass ratio of 1:1;

[0056] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0057] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0058] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0059] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0060] Since the lauric acid feed is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 90% through product analysis; the GC content of isoborneol laurate after refining is 97.5%, the GC content of fenchyl laurate is 1.5% and the GC content of pinyl laurate is 1.0%.

[0061] Example 4

[0062] A method for accelerating the synthesis reaction rate of isoborneol laurate, comprising the following steps:

[0063] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.25:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 80°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:0.5; the boric acid is dehydrated boric acid heated at 105°C for 1 hour;

[0064] (2) Filtration: After the reaction of step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is hexane;

[0065] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0066] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is anhydrous ethanol;

[0067] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0068] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0069] Since the lauric acid feed is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 90% through product analysis; the GC content of isoborneol laurate after refining is 98.5%, the GC content of fenchyl laurate is 0.8% and the GC content of pinyl laurate is 0.7%.

[0070] Example 5

[0071] A method for accelerating the synthesis reaction rate of isoborneol myristate, comprising the following steps:

[0072] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene in a mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:0.5;

[0073] (2) Filtration: After the reaction of step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate and petroleum ether, and the mass ratio thereof is 1:1;

[0074] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0075] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is anhydrous ethanol;

[0076] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0077] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0078] Since the amount of myristic acid added is excessive, the degree of reaction is measured by the conversion of camphene. After the reaction is completed, the product is analyzed and the conversion rate of camphene is 80%; the GC content of the refined product is 97.5% of isoborneol myristate, 1.6% of fenchyl myristate, and 0.9% of pinyl myristate.

[0079] Example 6

[0080] A method for accelerating the synthesis reaction rate of isoborneol myristate, comprising the following steps:

[0081] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene in a mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90° C., and the reaction time is 24 h; the composite catalyst is composed of anhydrous zirconium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:0.5; the boric acid is dehydrated boric acid heated at 105° C. for 1 h;

[0082] (2) Filtration: After the reaction of step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate and toluene in a mass ratio of 2:1;

[0083] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0084] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0085] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0086] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0087] Since the amount of myristic acid added is excessive, the degree of reaction is measured by the conversion of camphene. After the reaction is completed, the product is analyzed and the conversion rate of camphene is 90%; the GC content of the refined product is 98.5% of isoborneol myristate, 1.0% of fenchyl myristate, and 0.5% of pinyl myristate.

[0088] Example 7

[0089] A method for accelerating the synthesis reaction rate of isoborneol myristate, comprising the following steps:

[0090] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.6 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:0.5; the boric acid is dehydrated boric acid heated at 105°C for 1 hour;

[0091] (2) Filtration: After the reaction of step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is methyl acetate and toluene, and the mass ratio thereof is 1:1;

[0092] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0093] (4) Product purification: adding 2 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is anhydrous ethanol;

[0094] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0095] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0096] Since the amount of myristic acid added is excessive, the degree of reaction is measured by the conversion of camphene. After the reaction is completed, the product is analyzed and the conversion rate of camphene is 90%; the GC content of the refined product is 98.5% of isoborneol myristate, 1.0% of fenchyl myristate, and 0.5% of pinyl myristate.

[0097] Example 8

[0098] A method for accelerating the synthesis reaction rate of isoborneol myristate, comprising the following steps:

[0099] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.6 and a composite catalyst and camphene mass ratio of 0.15:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90° C., and the reaction time is 24 h; the composite catalyst is composed of anhydrous ferric sulfate, tartaric acid and boric acid in a mass ratio of 1:1:0.5; the boric acid is dehydrated boric acid heated at 105° C. for 1 h;

[0100] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice, and the washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0101] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0102] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0103] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0104] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0105] Since the amount of myristic acid added is excessive, the degree of reaction is measured by the conversion of camphene. After the reaction is completed, the product is analyzed and the conversion rate of camphene is 75%; the GC content of the refined product is 98.5% of isoborneol myristate, 1.0% of fenchyl myristate, and 0.5% of pinyl myristate.

[0106] Example 9

[0107] A method for accelerating the synthesis reaction rate of myristyl isoborneol, comprising the following steps:

[0108] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.2 and a composite catalyst and camphene mass ratio of 0.05:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90° C., and the reaction time is 24 h; the composite catalyst is composed of anhydrous ferric sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 105° C. for 1 h;

[0109] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice, and the washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0110] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, washing 3, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0111] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0112] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0113] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0114] Since the amount of myristic acid added is excessive, the degree of reaction is measured by the conversion of camphene. After the reaction is completed, the product is analyzed and the conversion rate of camphene is 55%. After the product is refined, the GC content of isoborneol myristate is 98.5%, fenchyl myristate is 1.0%, and pinyl myristate is 0.5%.

[0115] Example 10

[0116] A method for accelerating the synthesis reaction rate of isoborneol myristate, comprising the following steps:

[0117] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.2 and a composite catalyst and camphene mass ratio of 0.05:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90° C., and the reaction time is 24 h; the composite catalyst is composed of anhydrous ferric sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 105° C. for 1 h;

[0118] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor twice, and the washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0119] (3) washing: add water of 100% of amphene quality, water temperature 60 ℃, wash 3 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0120] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0121] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0122] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0123] Since the amount of myristic acid added is excessive, the degree of reaction is measured by the conversion of camphene. After the reaction is completed, the product is analyzed and the conversion rate of camphene is 55%. After the product is refined, the GC content of isoborneol myristate is 98.5%, fenchyl myristate is 1.0%, and pinyl myristate is 0.5%.

[0124] Embodiment 11

[0125] A method for accelerating the synthesis reaction rate of isoborneol palmitate comprises the following steps:

[0126] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous ferric sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 hour;

[0127] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0128] (3) washing: add water of 100% of amphene quality, water temperature 70 ℃, wash 4 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0129] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0130] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0131] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0132] Since the palmitic acid feed is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 88% through product analysis; the GC content of the refined product isoborneol palmitate is 99.7%, fenchyl palmitate is 0.2%, and pinyl palmitate is 0.1%.

[0133] Example 12

[0134] A method for accelerating the synthesis reaction rate of isoborneol palmitate comprises the following steps:

[0135] (1) Synthesis reaction: adding camphene and long-chain fatty acids in a molar ratio of 1:1.5 and a composite catalyst to camphene in a mass ratio of 0.3:1 to a reactor, starting stirring, rotating at 500 rpm, controlling the reaction temperature to 90°C and the reaction time to 24 h; the composite catalyst is composed of anhydrous titanium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 h;

[0136] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0137] (3) washing: add water of 100% of amphene quality, water temperature 70 ℃, wash 4 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0138] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0139] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0140] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0141] Since the palmitic acid feed is excessive, the degree of reaction needs to be measured according to the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 87.9% through product analysis; the GC content of isoborneol palmitate after refining is 99.7%, fenchyl palmitate is 0.2%, and pinyl palmitate is 0.1%.

[0142] Embodiment 13

[0143] A method for accelerating the synthesis reaction rate of isoborneol palmitate comprises the following steps:

[0144] (1) Synthesis reaction: adding camphene and long-chain fatty acid in a molar ratio of 1:1.5 and a composite catalyst to camphene in a mass ratio of 0.3:1 to a reactor, starting stirring, rotating at 500 rpm, controlling the reaction temperature to 90°C and the reaction time to 24 h; the composite catalyst comprises anhydrous zirconium sulfate, citric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 h;

[0145] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0146] (3) washing: add water of 100% of amphene quality, water temperature 70 ℃, wash 4 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0147] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0148] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0149] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0150] Since the amount of palmitic acid added is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 86.8% through product analysis; the GC content of isoborneol palmitate after refining is 99.4%, fenchyl palmitate is 0.3%, and pinyl palmitate is 0.3%.

[0151] Embodiment 14

[0152] A method for accelerating the synthesis reaction rate of isoborneol palmitate comprises the following steps:

[0153] (1) Synthesis reaction: adding camphene and long-chain fatty acids in a molar ratio of 1:1.5 and a composite catalyst to camphene in a mass ratio of 0.3:1 to a reactor, starting stirring, rotating at 500 rpm, controlling the reaction temperature to 90°C and the reaction time to 24 h; the composite catalyst comprises anhydrous zirconium sulfate, mandelic acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 h;

[0154] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0155] (3) washing: add water of 100% of amphene quality, water temperature 70 ℃, wash 4 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0156] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0157] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0158] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0159] Since the palmitic acid feed is excessive, the degree of reaction needs to be measured according to the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 87.5% through product analysis; the GC content of isoborneol palmitate after refining is 99.6%, fenchyl palmitate is 0.3%, and pinyl palmitate is 0.1%.

[0160] Embodiment 15

[0161] A method for accelerating the synthesis reaction rate of isoborneol palmitate comprises the following steps:

[0162] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, citric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 hour;

[0163] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0164] (3) washing: add water of 100% of amphene quality, water temperature 70 ℃, wash 4 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0165] (4) Product purification: adding 3 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0166] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0167] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0168] Since the palmitic acid feed is excessive, the degree of reaction needs to be measured according to the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 87% through product analysis; the GC content of isoborneol palmitate after refining is 99.5%, fenchyl palmitate is 0.3%, and pinyl palmitate is 0.2%.

[0169] Example 16

[0170] A method for accelerating the synthesis reaction rate of isoborneol stearate, comprising the steps of:

[0171] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, citric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 hour;

[0172] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0173] (3) washing: add water of 100% of amphene quality, water temperature 80 ℃, wash 5 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0174] (4) Product purification: adding 4 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0175] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0176] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0177] Since the stearic acid feed is excessive, the degree of reaction needs to be measured according to the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 87.3% through product analysis; the GC content of isoborneol stearate after refining is 99.7%, fenchyl stearate 0.2%, and pine stearate 0.1%.

[0178] Embodiment 17

[0179] A method for accelerating the synthesis reaction rate of isoborneol stearate, comprising the steps of:

[0180] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.4 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous titanium sulfate, tartaric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 hour;

[0181] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0182] (3) washing: add water of 100% of amphene quality, water temperature 80 ℃, wash 5 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0183] (4) Product purification: adding 4 times the mass of organic solvent b to the mixture of step (3) to dissolve, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is anhydrous ethanol and ethyl acetate, and the mass ratio thereof is 1:2;

[0184] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0185] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0186] Since stearic acid is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is finished, the conversion rate of camphene is 88% through product analysis; the GC content of isoborneol stearate after the product is refined is 99.7%, fenchyl stearate 0.2%, and pine stearate 0.1%.

[0187] Embodiment 18

[0188] A method for accelerating the synthesis reaction rate of isoborneol oleate, comprising the following steps:

[0189] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, citric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 hour;

[0190] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor four times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0191] (3) washing: add water of 100% of amphene quality, water temperature 80 ℃, wash 5 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0192] (4) Product purification: add 4 times the mass of organic solvent b to the mixture of step (3) to dissolve, then add sodium hydroxide solution dropwise, filter out the generated soap, and finally wash with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is anhydrous ethanol and ethyl acetate, and the mass ratio thereof is 1:5;

[0193] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0194] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0195] Since the oleic acid feed is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 87.2% through product analysis; the GC content of the refined product isoborneol oleate is 97.8%, fenchyl oleate is 1.2%, and pinyl oleate is 1.0%.

[0196] Embodiment 19

[0197] A method for accelerating the synthesis reaction rate of isoborneol linoleate, comprising the following steps:

[0198] (1) Synthesis reaction: camphene and long-chain fatty acids are added to a reactor in a molar ratio of 1:1.5 and a composite catalyst and camphene mass ratio of 0.3:1, stirring is started, the speed is 500 rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24 hours; the composite catalyst is composed of anhydrous zirconium sulfate, citric acid and boric acid in a mass ratio of 1:1:1; the boric acid is dehydrated boric acid heated at 110°C for 1 hour;

[0199] (2) Filtration: After the reaction in step (1) is completed, the reaction is allowed to stand, the liquid product is filtered and then transferred to a water washing tank, and then an organic solvent a is added to the reactor to wash the solid catalyst at the bottom of the reactor three times. The washing liquid is filtered and then transferred to a water washing tank, wherein the organic solvent a is ethyl acetate;

[0200] (3) washing: add water of 100% of amphene quality, water temperature 80 ℃, wash 5 times, must contain the mixture of long-chain fatty acid and long-chain fatty acid isoborneol ester;

[0201] (4) Product purification: adding 4 times the mass of organic solvent b to the mixture of step (3) to dissolve it, then dropping sodium hydroxide solution, filtering out the generated soap, and finally washing with water to obtain layered long-chain fatty acid isoborneol ester and long-chain fatty acid sodium aqueous solution, wherein the organic solvent b is ethyl acetate;

[0202] (5) Solvent recovery: recover the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester;

[0203] (6) Product purification: The crude long-chain fatty acid isoborneol ester obtained in step (5) is fractionated to remove unreacted camphene and light components such as isomeric terpinene, thereby obtaining high-purity long-chain fatty acid isoborneol ester.

[0204] Since the amount of linoleic acid added is excessive, the degree of reaction needs to be measured by the conversion of camphene. After the reaction is completed, the conversion rate of camphene is 86% through product analysis; the GC content of the refined product is 98.5% of isoborneol linoleate, 1.0% of fenchyl linoleate, and 0.5% of pinyl linoleate.

[0205] Comparative Example 1

[0206] Blank experiment. Synthesis reaction: camphene and oleic acid are added to the reactor in a molar ratio of 1:1.5, stirring is started, the speed is 500rpm, the reaction temperature is controlled to be 90℃, and the reaction time is 24h; no catalyst. After the reaction is completed, samples are taken for GC analysis. The GC content of camphene in the product is 86%, the GC content of tricyclic olefins is 13%, and oleyl isoborneol is not detected. It can be seen that camphene does not react with oleic acid without a catalyst.

[0207] Comparative Example 2

[0208] Sulfuric acid is used as a catalyst. Synthesis reaction: Add camphene and stearic acid in a molar ratio of 1:1.5 and a mass ratio of sulfuric acid to camphene of 0.3:1 into a reactor, start stirring, the speed is 500rpm, the reaction temperature is controlled to be 90°C, and the reaction time is 24h. After the reaction is completed, the product color is black. After the reaction is completed, the product can be directly sampled, washed with water to neutrality, dissolved in ethyl acetate and then analyzed by GC. By performing GC analysis on the product, it is found that there are more isomeric limonene and polymerization by-products. The selectivity of isoborneol stearate is 60%, which is lower than the selectivity of the target product of the present invention.

[0209] Comparative Example 3

[0210] Titanium sulfate is used alone as a catalyst. Synthesis reaction: Add camphene and stearic acid in a molar ratio of 1:1.5 and a mass ratio of titanium sulfate to camphene of 0.3:1 into the reactor, start stirring, the speed is 500rpm, the reaction temperature is controlled to be 80℃, and the reaction time is 24h. After the reaction is completed, the product can be directly sampled, washed with water to neutrality, and GC analysis is performed after dissolving in ethyl acetate. By GC analysis of the product, the conversion rate of camphene is 65%. Under the same reaction conditions, the conversion rate of camphene is 86% using a composite catalyst of titanium sulfate, tartaric acid and boric acid (the mass ratio is 1:1:0.5). It can be seen that the conversion rate of camphene is improved by using a composite catalyst. In addition, compared with a composite catalyst, the advantage of using titanium sulfate alone as a catalyst is that the catalyst is easy to prepare and easy to recycle, and the disadvantage is that the reaction rate is slow.

[0211] The above contents are further detailed descriptions of the present invention in combination with specific / preferred implementations, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, they can also make several substitutions or modifications to these described embodiments without departing from the concept of the present invention, and these substitutions or modifications should be regarded as belonging to the protection scope of the present invention.

Claims

1. A method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester, comprising the following steps: synthesis reaction, filtration, water washing, product purification, solvent recovery, product refining, characterized in that: The synthesis reaction step includes the following steps: Add camphene and long-chain fatty acids in a molar ratio of 1:1.2-1.6 and a composite catalyst to camphene in a mass ratio of 0.3:1 into a reactor, start stirring, control the reaction temperature to 80-90°C and the reaction time to 15-24h; the composite catalyst is composed of anhydrous sulfate, α-hydroxy acid and boric acid in a mass ratio of 1:1:0.5-1; The anhydrous sulfate is selected from one or more of iron sulfate, zirconium sulfate and titanium sulfate; The α-hydroxycarboxylic acid is selected from one or more of tartaric acid, citric acid, malic acid, mandelic acid, lactic acid, and glycolic acid; The filtering step is as follows: after the reaction is completed, the liquid product is allowed to stand, the liquid product is filtered and then moved into a water washing tank, and then an organic solvent is added to the reactor to wash the solid catalyst at the bottom of the reactor, and the washing liquid is filtered and then moved into a water washing tank; The water washing step is as follows: adding a certain mass of water and controlling the water temperature for washing to obtain a mixture of long-chain fatty acids and long-chain fatty acid isoborneol esters; The product purification steps are as follows: adding an organic solvent to the mixture obtained by washing with water to dissolve it, then dropping an alkali solution, filtering out the generated soap, and finally washing with water to obtain a layered long-chain fatty acid isoborneol ester and a long-chain fatty acid sodium aqueous solution; The product refining step is as follows: the crude long-chain fatty acid isoborneol ester obtained in the solvent recovery step is subjected to vacuum distillation to remove the light components of camphene and terpinene to obtain the fine long-chain fatty acid isoborneol ester.

2. The method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester according to claim 1, characterized in that: The boric acid is dehydrated boric acid heated at a temperature of 105-110° C. for 1 hour.

3. The method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester according to claim 1, characterized in that: The alkaline solution is selected from one of potassium hydroxide solution and sodium hydroxide solution.

4. The method for accelerating the synthesis reaction rate of long-chain fatty acid isoborneol ester according to claim 1, characterized in that: The solvent recovery step is as follows: recovering the solvent by distillation under reduced pressure to obtain a crude product of long-chain fatty acid isoborneol ester.

Citation Information

Patent Citations

  • A functionalized polyacid ionic liquid catalyst, its preparation method, and a method for catalyzing the synthesis of isoborneol acetate using the same catalyst.

    CN107899612B

  • Method for synthesizing isobornyl acetate by camphene

    CN108863779A