Evaporation mask plate and its manufacturing method, and evaporation equipment

By designing the mask body with the same thermal deformation characteristics and the evaporation mask that defines the mask layer, the problem of positional deviation caused by thermal expansion deformation in the vacuum evaporation process is solved, the evaporation accuracy and lamination rate are improved, and the problem is solved Fixed screen color mixing and border issues.

CN115948710BActive Publication Date: 2024-10-18BOE TECHNOLOGY GROUP CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202211287226.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-10-20
Publication Date
2024-10-18
Estimated Expiration
2042-10-20

AI Technical Summary

Technical Problem

In the vacuum evaporation process, thermal expansion and deformation of the substrate and evaporation mask lead to positional deviations, which affects the deposition accuracy of the luminescent material and leads to problems such as poor color mixing on the screen, frame falling off, and frame reduction.

Method used

Design an evaporation mask. The mask body has multiple through holes running through the thickness direction. The through holes correspond to the display panel and have the same thermal deformation characteristics as the substrate. The mask body is provided on one side of the mask body. The defined mask layer is used to form the evaporation pattern. The thickness of the mask body is much larger than the thickness of the defined mask layer. By adjusting the shape and opening size of the through holes, the deformation of the mask layer is reduced and the bonding rate is improved.

Benefits of technology

It effectively reduces the process deformation of the evaporation mask, improves the accuracy and bonding rate of the evaporation pattern, avoids screen color mixing and frame problems, and increases the difficulty of preparing large-size OLED screens.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115948710B_ABST
    Figure CN115948710B_ABST
Patent Text Reader

Abstract

The present invention discloses an evaporation mask plate and a manufacturing method and an evaporation device, wherein the evaporation mask plate comprises: a mask body, wherein the mask body has a plurality of through holes penetrating in the thickness direction, wherein one through hole corresponds to one display panel, and wherein the mask body and the base substrate of the display panel have the same thermal deformation characteristics; a limiting mask layer, which is arranged on one side of the mask body, and wherein the limiting layer mask is used to form the evaporation pattern required for the display panel; and wherein the base substrate is located on a side of the limiting mask layer away from the mask body, and wherein the thickness of the mask body is much greater than the thickness of the limiting mask layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the display field, and in particular to an evaporation mask plate and a manufacturing method thereof, and an evaporation device. Background Art

[0002] Each material layer in the light-emitting device of an active matrix organic light emitting diode (AMOLED) display panel is usually prepared by a vacuum evaporation process.

[0003] The evaporation process is to place the organic material in a crucible under vacuum conditions, and evaporate or sublimate the coating material into gaseous particles through high-temperature heating. The vaporized material particles are deposited on the substrate through the pattern openings defined on the evaporation mask, and form a preset pattern at the corresponding position on the substrate surface. Since the substrate and the evaporation mask are affected by the radiant heat from the crucible heat source and the deposition heat of the evaporation material in the evaporation machine, thermal expansion and deformation will occur, resulting in position deviations of the substrate and mask opening patterns, and offset of the evaporation position of the luminescent material, which in turn causes poor screen color mixing, poor shedding at the frame, and limits the reduction of the screen frame.

[0004] In view of this, how to reduce the process deformation of the evaporation mask has become a technical problem that needs to be solved urgently. Summary of the invention

[0005] The embodiments of the present invention provide an evaporation mask and a manufacturing method thereof, and an evaporation device, so as to solve the above problems existing in the prior art.

[0006] In a first aspect, in order to solve the above technical problems, an embodiment of the present invention provides an evaporation mask, comprising:

[0007] A mask body, wherein the mask body has a plurality of through holes extending through the thickness direction, one through hole corresponds to one display panel, and the mask body and the base substrate of the display panel have the same thermal deformation characteristics;

[0008] A limiting mask layer is arranged on one side of the mask body, and the limiting layer mask is used to form the evaporation pattern required for the display panel; the base substrate is located on the side of the limiting mask layer away from the mask body, and the thickness of the mask body is much greater than the thickness of the limiting mask layer.

[0009] In a possible implementation manner, a cross section of the through hole gradually increases in the thickness direction.

[0010] In a possible implementation manner, the mask body has a first surface and a second surface that are parallel to each other;

[0011] The through hole comprises: a first opening and a second opening arranged opposite to each other, wherein the first opening is located on the first surface, the second opening is located on the second surface, and the area of ​​the first opening is larger than the area of ​​the second opening; and the limiting mask layer is located on the second surface.

[0012] In a possible implementation manner, the second opening completely covers the effective display area of ​​the base substrate.

[0013] In a possible implementation manner, a distance between edges of orthographic projections of the first opening and the second opening on the first surface is greater than 2 mm.

[0014] In a possible implementation manner, the definition mask layer includes:

[0015] A plurality of mask units, each mask unit corresponding to at least one through hole;

[0016] A plurality of gaps are provided, wherein the gaps are located between two adjacent mask units.

[0017] In a possible implementation manner, the mask unit includes a plurality of pixel openings arranged in an array, or a display opening corresponding to an effective display area of ​​the base substrate.

[0018] A possible implementation further includes:

[0019] A plurality of support structures surround the plurality of mask units.

[0020] A possible implementation further includes:

[0021] At least one spacing structure is located between at least part of two adjacent mask units.

[0022] In a possible implementation manner, the shape of the through hole includes:

[0023] Rectangle, square, circle, special shape.

[0024] In a possible implementation manner, through holes of different shapes are arranged in different areas.

[0025] In a possible implementation manner, the material defining the mask layer includes:

[0026] Metal material or polyimide.

[0027] In a possible implementation manner, when the material of the limiting mask layer is the metal material, the evaporation mask further includes:

[0028] The conductive layer is located between the mask body and the definition mask layer, and the conductive layer has the same pattern as that of the definition mask layer.

[0029] In a possible implementation manner, the definition mask layer completely covers the conductive layer.

[0030] In a possible implementation manner, the edge of the limiting mask layer is a curved surface.

[0031] In a possible implementation manner, the metal material includes:

[0032] Any one or any combination of iron, nickel and cobalt; the material of the conductive layer includes:

[0033] Any one of indium tin oxide, titanium, platinum, and silver.

[0034] In a possible implementation manner, the thickness of the mask body is the same as the thickness of the substrate;

[0035] The mask body and the substrate are made of the same material.

[0036] In a possible implementation manner, the thickness of the limiting mask layer ranges from 5 um to 30 um.

[0037] In a second aspect, an embodiment of the present invention provides a method for manufacturing an evaporation mask based on the first aspect, comprising:

[0038] providing a mask body;

[0039] The mask body is patterned to form a mask body, wherein the mask body has a plurality of through holes extending through the thickness direction, one through hole corresponds to one display panel, and the mask body and the base substrate of the display panel have the same thermal deformation characteristics;

[0040] Forming a filling layer in a through hole of the mask body; the filling layer at least fills the plurality of through holes to make the surface of the mask body flat;

[0041] A limiting mask layer is formed on one side of the filling layer; wherein the limiting mask layer is used to form the evaporation pattern required for the display panel, and the thickness of the limiting mask layer is much smaller than the thickness of the mask body;

[0042] The filling layer is peeled off.

[0043] In a possible implementation manner, forming the limiting mask layer on one side of the filling layer includes:

[0044] Depositing a metal layer on the side where the second surface of the mask body is located; the second surface is the side with the smallest opening area of ​​the through hole;

[0045] Patterning the metal layer to form a conductive layer consistent with the vapor deposition pattern;

[0046] The defining mask layer is formed by electrodeposition on a surface of the conductive layer which is away from the mask body.

[0047] In a possible implementation manner, forming the limiting mask layer on one side of the filling layer includes:

[0048] A polyimide layer is coated on the side where the second surface of the mask body is located; the second surface is the side with the smallest opening area of ​​the through hole;

[0049] curing the polyimide layer;

[0050] The cured polyimide layer is patterned to obtain the defined mask layer.

[0051] In a third aspect, an embodiment of the present invention provides an evaporation device, comprising the evaporation mask as described in the first aspect. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] Figure 1 It is a schematic diagram of the film structure of an OLED light-emitting device in the related art;

[0053] Figure 2 A top view of a vapor-deposited metal mask in the related art;

[0054] Figure 3 for Figure 2 Cross-sectional view along the AA' direction;

[0055] Figure 4 A schematic diagram showing the comparison of the sagging amount of the metal mask and the base substrate of the display panel in the related art;

[0056] Figure 5 It is a schematic diagram for comparing the offset between the deposition of light-emitting materials on a substrate and the display area of ​​the substrate in the related art;

[0057] Figure 6 A schematic top view of an evaporation mask provided by an embodiment of the present invention;

[0058] Figure 7 A method provided by an embodiment of the present invention Figure 6 Cross-sectional view of middle BB';

[0059] Figure 8 A method provided by an embodiment of the present invention Figure 6 A cross-sectional view of the middle mask body at BB';

[0060] Fig. 9 Another embodiment of the present invention provides Figure 6 A cross-sectional view of the middle mask body at BB';

[0061] Fig.10 A schematic structural diagram of an evaporation mask provided by an embodiment of the present invention;

[0062] Fig.11 A schematic diagram of an orthographic projection of a first opening and a second opening on a first surface provided by an embodiment of the present invention;

[0063] Fig.12 A top view of a limiting mask layer provided in an embodiment of the present invention;

[0064] Fig.13 and Fig.14 A top view of another definition mask layer provided in an embodiment of the present invention;

[0065] Fig.15 A top view of a mask unit provided by an embodiment of the present invention;

[0066] Fig.16 A top view of another mask evaporation plate provided by an embodiment of the present invention;

[0067] Fig.17 and Fig.18 A top view of another vapor deposition mask provided by an embodiment of the present invention;

[0068] Fig.19 A schematic diagram of the arrangement of mask units in an evaporation mask provided by an embodiment of the present invention;

[0069] Figure 20 to Figure 22 A schematic structural diagram of another vapor deposition mask provided by an embodiment of the present invention;

[0070] Fig.23 A cross-sectional view of an edge position of a vapor deposition mask provided by an embodiment of the present invention;

[0071] Fig.24 A schematic structural diagram of another vapor deposition mask provided by an embodiment of the present invention;

[0072] Fig.25 A flow chart of a method for manufacturing an evaporation mask provided by an embodiment of the present invention;

[0073] Fig.26 A schematic diagram of forming a mask body provided by an embodiment of the present invention;

[0074] Fig. 27 A schematic diagram of another method of forming a mask body provided by an embodiment of the present invention;

[0075] Fig.28 and Fig.29 A schematic diagram of the structure of a filling layer provided in an embodiment of the present invention;

[0076] Fig.30 A schematic diagram of manufacturing a vapor deposition mask provided by an embodiment of the present invention;

[0077] Fig.31 FIG. 1 is a top view of a mask unit provided by an embodiment of the present invention;

[0078] Fig.32 A schematic diagram of manufacturing another evaporation mask provided by an embodiment of the present invention;

[0079] Fig.33 A top view of another mask unit provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0080] The embodiments of the present invention provide an evaporation mask and a manufacturing method thereof, and an evaporation device, so as to solve the above problems existing in the prior art.

[0081] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and understandable, the present invention will be further described below with reference to the accompanying drawings and examples. However, the exemplary embodiments can be implemented in various forms and should not be understood as being limited to the embodiments described herein; on the contrary, these embodiments are provided to make the present invention more comprehensive and complete, and to fully convey the concepts of the exemplary embodiments to those skilled in the art. The same figure marks in the figures represent the same or similar structures, and thus their repeated descriptions will be omitted. The words expressing position and direction described in the present invention are all explained using the accompanying drawings as examples, but changes can be made as needed, and the changes made are all included in the scope of protection of the present invention. The drawings of the present invention are only used to illustrate the relative position relationship and do not represent the true proportions.

[0082] It should be noted that specific details are described in the following description to facilitate a full understanding of the present invention. However, the present invention can be implemented in a variety of other ways different from those described herein, and those skilled in the art can make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below. The subsequent description of the specification is a preferred embodiment of the present application, but the description is for the purpose of illustrating the general principles of the present application and is not intended to limit the scope of the present application. The scope of protection of the present application shall be determined by the definition of the attached claims.

[0083] The basic structure of an organic light-emitting diode (OLED) is composed of a pair of electrodes and an organic material layer. Figure 1Schematic diagram of the film structure of an OLED light-emitting device in the related art. The film layers of the OLED light-emitting device include an anode 001, a hole injection layer 002, a hole transport layer 003, a hole blocking layer 004, a light-emitting layer 005, an electron blocking layer 006, an electron transport layer 007, an electron injection layer 008, a cathode 009, and a light extraction layer 010, which are stacked in sequence.

[0084] When making yellow, green and blue light-emitting layers, the light-emitting materials need to be evaporated onto the base substrate of the display panel through a high-precision metal mask, while other organic film layers are usually evaporated onto the base substrate of the display panel through a full-opening metal mask.

[0085] See also Figure 2 and Figure 3 , Figure 2 It is a top view of a vapor-deposited metal mask in the related art. Figure 3 for Figure 2 Cross-sectional view along the AA' direction.

[0086] Figure 2 The vapor deposition metal mask in the embodiment includes a metal frame S1, a metal mask S2, and a metal eye mask S2 having a plurality of openings SK, the openings SK corresponding to the display panel, and in a high-precision metal mask, the pattern of the openings SK corresponds to the pattern of the light-emitting pixels of the display panel. Usually, the thickness of the metal mask S2 ranges from 20 to 150 um, and the metal frame S1 plays the role of fixing and supporting the metal mask S2, and the thickness of the metal frame is usually several tens of millimeters.

[0087] See also Figure 4 It is a schematic diagram comparing the sagging amount of the metal mask and the base substrate of the display panel in the related art.

[0088] Since the metal mask S2 is relatively thin and will be stretched during the assembly process with the metal frame S1, its droop is much smaller than the size of the base substrate 100. Depending on the basic size, the difference in the droop between the two will gradually increase. For example, as the size of the base substrate 100 increases, the difference in the droop between the two ranges from several hundred microns to several millimeters. The droop difference between the base substrate 100 and the metal mask S2 is large. When the two need to be aligned and bonded during the evaporation process, there will be problems such as failure to fully bond and match well, local gaps or position shifts, which will cause shadow effects or position shifts in the evaporation pattern, causing poor color mixing on the screen.

[0089] See also Figure 5 It is a schematic diagram comparing the offset between the deposition of light-emitting material on a substrate and the display area of ​​the substrate in the related art.

[0090] When the evaporation material of the organic film layer is deposited in the evaporation chamber, the base substrate 100 and the metal mask S2 are affected by the radiation heat from the crucible heat source and the deposition heat of the evaporation material in the evaporation chamber, and thermal expansion deformation will occur, resulting in deviations in the positions of the display area AA of the base substrate 100 and the opening pattern (luminescent material EL) on the metal mask S2. If the base substrate is a glass substrate, the thermal expansion coefficient of the glass substrate is about 3 times greater than that of the metal mask S2, and the thermal expansion size of the glass substrate is larger than that of the metal mask S2. Therefore, the pattern of the evaporated luminescent material EL will gradually shrink from the edge to the center as a whole compared to the glass substrate (such as Figure 5 shown).

[0091] When the temperature increases or the size of the evaporation mask increases, the relative position deviation between the substrate and the opening pattern of the metal mask S2 will be aggravated. In addition, because the metal mask S2 is assembled through the meshing process, the different positions of the metal mask S2 will be affected by mechanics and will also produce certain deformations compared with the design. After being affected by temperature, the deformation of the metal mask will be affected by the combined effects of mechanics and heat. This makes the evaporation process of large-size OLEDs very difficult.

[0092] At the same time, when the size of the evaporation mask becomes larger, the stretching deformation and flatness of the metal mask S2 will be difficult to control, which will also make the stretching process very difficult. After the stretching is completed, the metal mask S2 sags due to gravity and the amount of sag of the glass substrate is also very different, which makes the glass substrate and the metal mask not fit well. The presence of gaps or wrinkles will also cause the deposition of the evaporation material to shift, the pattern to be incomplete, or the shadow to be bad.

[0093] Therefore, how to reduce the process deformation of the evaporation mask, especially the process deformation of the large-size evaporation mask, has become a technical problem that needs to be solved urgently.

[0094] In order to solve the above problems, an embodiment of the present invention provides an evaporation mask and a manufacturing method thereof, and an evaporation device, which are described in detail as follows.

[0095] See also Figure 6 and Figure 7 , Figure 6 A schematic top view of a vapor deposition mask provided by an embodiment of the present invention, Figure 7 A method provided by an embodiment of the present invention Figure 6 The cross-sectional view of BB' in FIG. The evaporation mask includes:

[0096] The mask body 1 has a plurality of through holes H extending in the thickness direction Y, one through hole H corresponding to one display panel, and the mask body 1 and the substrate of the display panel ( Figure 6The through holes H in the mask body 1 may have the same thermal deformation characteristics as those in the substrate to be evaporated (not shown in the figure, and may also be referred to as the substrate to be evaporated); the shapes of the through holes H include rectangular, square, circular, and irregular shapes. The shapes of the multiple through holes H in the mask body 1 may be completely the same, partially the same, or different, and there is no specific limitation.

[0097] The mask body 1 and the substrate have the same thermal deformation characteristics, which means that the thickness and material properties of the mask body 1 match the sagging deformation and thermal expansion of the substrate, so that even if the size of the substrate increases, it can fit well with the substrate mask and maintain the same deformation.

[0098] In some embodiments, the mask body 1 and the substrate can be made of the same material, such as glass, so that the thermal deformation and mechanical deformation of the mask body 1 and the substrate can be kept consistent, so that the two can fit well during evaporation and match thermal deformation.

[0099] In some embodiments, the thickness of the mask body 1 is 0.1-1 mm.

[0100] In some other embodiments, the thickness of the mask body 1 and the base substrate may also be the same, so that the thermal deformation characteristics of the mask body 1 and the base substrate can be kept consistent.

[0101] The limiting mask layer 2 is arranged on one side of the mask body 1, and the limiting layer mask is used to form the evaporation pattern required for the display panel; the base substrate is located on the side of the limiting mask layer 2 away from the mask body 1, and the thickness d1 of the mask body 1 is much larger than the thickness d2 of the limiting mask layer 2.

[0102] like Figure 7 As shown, since the thickness d1 of the mask body 1 is much larger than the thickness d2 of the limiting mask layer 2 for forming the vapor deposition pattern, and the mask body 1 has a plurality of through holes H extending through the thickness direction Y, the limiting mask layer 2 for forming the vapor deposition pattern arranged on one side of the mask body 1 can be effectively supported by the mask body 1 in the area outside the through holes H, thereby reducing the deformation of the limiting mask layer 2. At the same time, since the thermal deformation characteristics of the mask body 1 and the base substrate are the same, the mask body 1 and the base substrate can maintain the same deformation, so that the deformation of the mask body 1 will not affect the bonding between the limiting mask layer 2 and the base substrate, thereby improving the bonding rate between the limiting mask layer 2 and the base substrate, and making the vapor deposition mask plate and the base substrate bond well.

[0103] See also Figure 8 and Fig. 9 , Figure 8 A method provided by an embodiment of the present invention Figure 6 The cross-sectional view of the middle mask body at BB', Fig. 9 Another embodiment of the present invention provides Figure 6The cross section S of the through hole H gradually increases in the thickness direction Y.

[0104] like Figure 8 As shown, the side wall of the through hole H may be a slope, or, as shown in FIG. Fig. 9 As shown, the side wall of the through hole H is a curved surface.

[0105] In the embodiment provided by the present invention, the cross section S of the through hole H is set to gradually increase in the thickness direction Y, which facilitates the process implementation.

[0106] See also Fig.10 A schematic structural diagram of an evaporation mask provided in an embodiment of the present invention.

[0107] The mask body 1 has a first surface 11 and a second surface 12 which are parallel to each other;

[0108] The through hole H includes: a first opening K1 and a second opening K2 arranged opposite to each other, the first opening K1 is located on the first surface 11, the second opening K2 is located on the second surface 12, and the area of ​​the first opening K1 is larger than the area of ​​the second opening K2; the limiting mask layer 2 is located on the second surface 12. When performing evaporation, the substrate is arranged on the side of the limiting mask layer 2 away from the mask body 1, and the evaporation material enters from the first opening. The shape of the first opening K1 is consistent with the shape of the second opening K2, that is, they have the same shape but different sizes.

[0109] By arranging the limiting mask layer 2 on the second surface of the mask body 1 where the through hole H has a smaller opening area, it is possible to avoid the mask body 1 with a relatively thick limiting mask from blocking the evaporated material in the thickness direction Y, thereby improving the quality of the formed pattern.

[0110] The size of the second opening may be the same as the effective display area of ​​the base substrate.

[0111] In some embodiments, the second opening can completely cover the effective display area of ​​the base substrate, so that the mask layer 2 can be defined to have a stress release area, so that a transition is made between the boundary of the effective display area and the mask body 1, thereby ensuring the accuracy of the evaporation area.

[0112] See also Fig.11 Schematic diagram of the orthographic projection of the first opening and the second opening on the first surface provided by the embodiment of the present invention. The edge spacing d3 of the orthographic projection of the first opening K1 and the second opening K2 on the first surface 11 is greater than 2 mm.

[0113] By setting the edge distance d3 of the orthographic projection of the first opening K1 and the second opening K2 on the first surface 11 to be greater than 2 mm, it is possible to effectively avoid the mask body 1 from blocking the evaporated material in the thickness direction Y during the evaporation process.

[0114] See also Figure 12 to Figure 14 , Fig.12 A top view of a limiting mask layer provided in an embodiment of the present invention, Fig.13 and Fig.14 A top view of another definition mask layer provided in an embodiment of the present invention.

[0115] The mask layer 2 is defined, comprising:

[0116] A plurality of mask units 21, each mask unit 21 corresponds to at least one through hole H;

[0117] A plurality of gaps 22 are provided, wherein the gap 22 is located between two adjacent mask units 21 .

[0118] Fig.12 It is a top view of the mask layer 2 for defining other organic film layers except the light-emitting layer in the light-emitting device. Assuming that one mask unit 21 corresponds to one through hole H, the opening in the mask unit 21 (the white area in the mask unit 21) corresponds to the second opening K2. Fig.12 It is assumed that one mask unit 21 corresponds to 10 through holes H, and the mask unit 21 has 10 openings, one opening corresponding to one display panel; Fig.14 2 is a top view of the mask layer 2 for limiting the light-emitting layer, and the dotted frame in the mask unit 21 corresponds to the second opening K2.

[0119] In the embodiment provided by the present invention, by setting the limiting mask layer 2 to a plurality of mask units 21 corresponding to the plurality of through holes H one by one, and setting a gap 22 between two adjacent mask units 21, the unit mask unit 21 can be made smaller in size than the evaporation mask in the prior art, so that the internal stress of the mask unit 21 is smaller, and is easy to release, and is not prone to uneven deformation; when the evaporation process is subjected to heat, the gap 22 is provided between two adjacent mask units 21, so that the mask units 21 are separated from each other and do not affect each other, which can effectively reduce the thermal deformation of the mask unit 21, and will not cause relative deformation due to the difference between the thermal deformation of the mask unit 21 and the mask body 1, and will not be affected by the gradual increase in the thermal expansion size of the limiting mask layer 2. In addition, since the thickness of the limiting mask layer 2 is much smaller than the thickness of the mask body 1, when the evaporation process is performed, the mask unit 21 of the limiting mask layer 2 changes with the deformation of the mask body 1, and always matches the deformation of the glass substrate, so that a higher graphic accuracy can be achieved. At the same time, since there are gaps 22 between the multiple mask units 21 separated from each other on the limited mask layer 2, the influence of particles on the evaporation process can also be reduced, allowing some particles to fall into the gaps between the mask units 21, so that they will not be sandwiched between the base substrate and the evaporation mask to cause bonding gaps and poor evaporation.

[0120] See also Fig.15A top view of a mask unit provided in an embodiment of the present invention.

[0121] The mask unit 21 includes a plurality of pixel openings arranged in an array, or display openings corresponding to the effective display area of ​​the base substrate.

[0122] When the mask unit 21 is used to form the pattern required for the light-emitting layer, the mask unit 21 includes: Fig.15 The multiple pixel openings K arranged in an array are shown, one pixel opening corresponds to one pixel or sub-pixel, and if one pixel opening K corresponds to one pixel, then the pixel opening K also includes multiple sub-pixel openings. The orthographic projection of the multiple pixel openings K arranged in an array on the second surface of the mask body 1 is located within the second opening K2.

[0123] When the mask unit 21 is used to form other organic film layers in the light-emitting device, the mask unit 21 includes a display opening (eg, Fig.12 The orthographic projection of the display opening on the second surface of the mask body 1 is located within the second opening K2.

[0124] See also Fig.16 A top view of another mask evaporation plate provided in an embodiment of the present invention, wherein the evaporation mask plate further includes:

[0125] A plurality of support structures 3 , wherein the support structures 3 surround the plurality of mask units 21 .

[0126] The shape of the support structure 3 at the corner position among the multiple support structures 3 is different from the shape of the shapes at other positions. The shape of the support structure 3 at the corner position is consistent with the shape of the corresponding corner, so that the mask unit 21 close to the corner position can be effectively supported to prevent poor bonding.

[0127] In the embodiment provided by the present invention, by arranging multiple support structures 3 around multiple mask units 21, the edge of the mask layer 2 can be supported when the mask layer 2 is bonded to the base substrate, thereby preventing poor edge bonding.

[0128] The support structure 3 is provided in the same layer and with the same material as the limiting mask layer 2 .

[0129] See also Fig.17 and Fig.18 A top view of another vapor deposition mask provided by an embodiment of the present invention.

[0130] The evaporation mask further includes: at least one spacing structure 4 , and the spacing structure 4 is located between at least part of two adjacent mask units 21 .

[0131] like Fig.17As shown, the spacing structure 4 can be arranged between two mask units 21 adjacent to each other in the transverse direction, or can be arranged as shown in FIG. Fig.18 As shown, it is arranged between any two adjacent mask units 21 .

[0132] In the embodiment provided by the present invention, by providing a spacing structure 4 between at least some adjacent mask units 21 , the stress between the plurality of mask units 21 can be balanced, so that the stress distribution in the evaporation mask is balanced, thereby reducing the deformation of the mask unit 21 .

[0133] See also Fig.19 A schematic diagram of the arrangement of mask units in a vapor deposition mask provided by an embodiment of the present invention, in Fig.19 One mask unit 21 corresponds to one through hole H, among the multiple through holes H in the mask body 1, a part of the through holes H are rectangular in shape, and the corresponding mask unit 21 is also rectangular in shape, another part of the through holes H are circular in shape, and the corresponding mask unit 21 can be square in shape, and another part of the through holes H are irregular in shape, and the shapes corresponding to these irregular through holes are not completely the same, and the shapes of the mask units corresponding to these irregular through holes are consistent with the shapes of the corresponding through holes H.

[0134] By arranging the mask units 21 corresponding to display panels of different shapes and sizes in the same defined mask layer 21, the space of the defined mask layer 2 can be fully utilized, and the mask units 21 can be arranged to the maximum extent, thereby effectively reducing the investment cost.

[0135] In some embodiments, the material defining the mask layer 2 includes a metal material or polyimide. The metal material includes any one or any combination of iron, nickel, and cobalt.

[0136] See also Figure 20 to Figure 22 A schematic structural diagram of another vapor deposition mask provided by an embodiment of the present invention, when the material of the mask layer 2 is limited to a metal material, the vapor deposition mask further includes:

[0137] The conductive layer 5 is located between the mask body 1 and the limiting mask layer 2 , and the conductive layer 5 has the same pattern as that of the limiting mask layer 2 .

[0138] The material of the conductive layer 5 includes any conductive material among indium tin oxide (ITO), titanium (Ti), platinum (Pt), and silver (Ag). The conductive layer 5 is used as a cathode when the defining mask layer 2 is made on the substrate by an electrochemical deposition process. By setting the conductive layer 5 to be consistent with the pattern of the defining mask layer 2, the pattern of the defining mask layer 2 can be grown on the conductive layer 5 by electrodeposition.

[0139] like Fig. 20 FIG. 2 is a cross-sectional view of a light-emitting layer without a plurality of mask units 21 in the limiting mask layer 2. Fig.21A cross-sectional view of a mask layer 2 for defining a light-emitting layer, including a plurality of mask units 21 and gaps 22, Fig. 22 The mask layer 2 for defining other organic film layers in the light-emitting device includes a cross-sectional view of a plurality of mask units 21 and gaps 22 .

[0140] like Figure 20 to Figure 22 As shown, the limiting mask layer 2 completely covers the conductive layer 5. The outer contour of the limiting mask layer 2 is larger than that of the conductive layer 5, and increases with the increase of the deposition thickness of the limiting mask layer 2. By allowing the limiting mask layer 2 to completely cover the conductive layer 5, the limiting mask layer 2 can form a pattern consistent with the opening of the conductive layer 5.

[0141] In the embodiment provided by the present invention, by providing a conductive layer 5 consistent with the pattern of the defined mask layer 2 between the mask body 1 and the defined mask layer 2, the conductive layer 5 can be used as a cathode, and the defined mask layer 2 is electrodeposited and grown on the conductive layer 5 by an electrochemical deposition process, thereby improving the pattern accuracy of the defined mask layer 2. In addition, since the pattern accuracy of the defined mask layer 2 produced by electrodeposition is high, and the pattern is not restricted and can be formed into any shape or sharp corners, it can not only effectively improve the resolution of the display panel to achieve a high pixel unit (Pixels Per Inch, PPI), but also can adapt to the evaporation pattern requirements of various display panels, and improve the application range is very wide.

[0142] The evaporation mask prepared by the wet etching technology used in the prior art is usually 20 to 100um thick, which is difficult to thin and the opening size is also difficult to reduce, and cannot correspond to high PPI display panels; and the etching process cannot produce sharp corners due to the diffusion characteristics of the etching solution, and all graphic openings have different degrees of rounded corners. However, the limiting mask layer 2 in the embodiment of the present invention is prepared by the electrodeposition process using the conductive layer 5, and its thickness can be arbitrarily controlled, and a thinner film thickness can be achieved, such as the thickness of the limiting mask layer 2 can be controlled to 5um to 30um.

[0143] See also Fig.23 A cross-sectional view of the edge position of a vapor deposition mask provided by an embodiment of the present invention. The edge of the mask layer 2 is limited to be a curved surface. That is, the curvature of the edge of the mask layer 2 is limited to surround the conductive layer 5.

[0144] When the vapor deposition mask plate includes a supporting structure 3 and / or a spacing structure 4 arranged around the limiting mask layer 2, the supporting structure 3 and the spacing structure 4 are composed of the same layer and material as the conductive layer 5 and the limiting mask layer 2, and the edges of the parts of the supporting structure 3 and the spacing structure 4 that are of the same layer and material as the limiting mask layer 2 are also arc surfaces.

[0145] The process is easy to implement by setting the edge of the limiting mask layer 2 as a curved surface.

[0146] like Fig.16 or Fig.17 As shown, when the material of the limiting mask layer 2 is polyamide (ie, there is no conductive layer 5), the support structure 3 and the spacing structure 4 are made of the same material as the limiting mask layer 2, that is, they are formed by patterning the same film layer once; Fig.24 FIG. 1 is a schematic diagram of the structure of another vapor deposition mask provided by an embodiment of the present invention, wherein the material of the mask layer 2 is a metal material and the vapor deposition mask includes a conductive layer 5. Fig.24 It is a vapor deposition mask for other organic film layers other than the light-emitting layer in the light-emitting device. At this time, the support structure 3 and the spacer structure 4 are made of the same material as the limiting mask layer 2 and the conductive layer 5, that is, the support structure 3 and the spacer structure 4 are formed by patterning one side of the same film layer corresponding to the conductive layer 5 to form a part in the same layer as the conductive layer 5, and are formed together with the same process for forming the limiting mask layer 2.

[0147] Based on the same inventive concept, an embodiment of the present invention provides a method for manufacturing a vapor deposition mask. The specific structure of the vapor deposition mask can be found in the description of the above embodiment. Fig.25 A flow chart of a method for manufacturing a vapor deposition mask provided by an embodiment of the present invention, the manufacturing method comprising:

[0148] Step S10: providing a mask body;

[0149] Step S12: patterning the mask body to form a mask body, wherein the mask body has a plurality of through holes extending through the thickness direction, one through hole corresponding to one display panel, and the mask body and the base substrate of the display panel have the same thermal deformation characteristics;

[0150] There are two options for forming the mask body:

[0151] Solution 1: Preparation by etching.

[0152] See also Fig.26 A schematic diagram of forming a mask body provided by an embodiment of the present invention.

[0153] A photoresist is coated on the surface of the mask body, and the through-hole pattern is prepared by known etching processes such as exposure, development, etching and stripping, as follows:

[0154] Step S20: coating photoresist.

[0155] A photoresist is coated on one side of the mask body.

[0156] Step S21: placing an exposure mask.

[0157] An exposure mask is arranged on a side of the photoresist away from the mask body.

[0158] Step 22: Expose and develop to form a mask body.

[0159] Exposure and development are performed from the side where the exposure mask is placed to form through holes in the mask body.

[0160] Since the above process uses the same equipment as the conventional OLED substrate preparation process, there is no need for additional equipment investment, which can effectively save equipment costs.

[0161] Solution 2: Use laser equipment to prepare through holes in the mask body.

[0162] See also Fig. 27 Another schematic diagram of forming a mask body provided by an embodiment of the present invention is to directly form the required through holes on the mask body by laser processing to obtain the mask body.

[0163] It should be understood that other processes may also be used to achieve this, and the specific process used to prepare the mask body is not limited here.

[0164] Step S13: forming a filling layer in the through holes of the mask body; the filling layer at least fills up a plurality of through holes to make the surface of the mask body flat;

[0165] The material of the filling layer may be photoresist, and the filling layer may be formed by the following methods:

[0166] Place the side with the smaller opening (i.e., the second opening) of the through hole of the mask body on the platform, and apply photoresist on the side with the larger opening (i.e., the first opening) of the through hole. After the photoresist is applied evenly, it is exposed and heat-treated to transform it into a solid state, and tightly bonded to the mask body to form a whole.

[0167] See also Fig.28 and Fig.29 A schematic diagram of the structure of the filling layer provided in an embodiment of the present invention is shown in FIG. Fig.28 As shown in the figure, the filling layer 6 can just fill the through hole H of the mask body 1, or it can be Fig.29 The filling layer 6 shown is slightly higher than the through hole H, but the higher portion of the filling layer 6 needs to be kept flat as a whole.

[0168] By forming a filling layer in the through hole of the mask body, it is convenient to form a pattern defining the mask layer at a position corresponding to the through hole of the mask body.

[0169] Step S14: forming a limiting mask layer on one side of the filling layer; wherein the limiting mask layer is used to form the vapor deposition pattern required for the display panel, and the thickness of the limiting mask layer is much smaller than the thickness of the mask body;

[0170] Step S15: peeling off the filling layer.

[0171] In some embodiments, forming the limiting mask layer on one side of the filling layer can be achieved by the following methods:

[0172] A polyimide layer is coated on the side where the second surface of the mask body is located; the second surface is the side with the smallest through hole opening area; the polyimide layer is cured; and the cured polyimide layer is patterned to obtain a defined mask layer.

[0173] Taking the evaporation mask for forming the organic film layer other than the light-emitting layer in the light-emitting device as an example, the production process of the evaporation mask is explained. Fig.30 A schematic diagram of manufacturing a vapor deposition mask provided by an embodiment of the present invention.

[0174] Step S30: forming a mask body.

[0175] The through hole H in the mask body 1 may be formed by the aforementioned process. The opening of the through hole H is the largest on the first surface 11 of the mask body 1 , and the opening of the through hole H is the smallest on the second surface 12 of the mask body 1 .

[0176] Step S31: forming a filling layer.

[0177] The filling layer is filled in from the side with a larger opening (ie, the second surface side) of the through hole H of the mask body 1 .

[0178] Step S32: forming a definition mask layer.

[0179] A polyimide layer is coated on one side of the second surface of the mask body, and the polyimide layer is cured; and the cured polyimide layer is patterned to form a defined mask layer. Fig.30 The limiting mask layer in the embodiment includes a plurality of mask units 21, and a gap 22 is provided between two adjacent mask units 21. In addition, a support structure 3 is provided around the plurality of mask units 21. The support structure 3 is provided in the same layer and with the same material as the mask units 21. Fig.31 FIG. 1 is a top view of a mask unit provided by an embodiment of the present invention. Fig.31 It is the production process of the vapor deposition mask of other organic film layers other than the light-emitting layer in the light-emitting device. Fig.31 The middle mask unit 21 and the conductive layer 5 have only one display opening corresponding to the effective display area of ​​the display panel, through which the filling layer 6 below can be observed.

[0180] Step 33: Peel off the filling layer.

[0181] The filling layer may be stripped using a stripping process, such as using an organic solvent to dissolve the solidified photoresist (the material of the filling layer) to form a final evaporation mask.

[0182] When the above-mentioned evaporation mask is used to implement the evaporation process, the base substrate of the display panel is set on the side where the second surface of the mask body is located. The evaporation material moves from the first surface 11 of the mask body to the second surface 12, and is finally precisely controlled by the limited mask to deposit on the base substrate with the evaporation size and pattern.

[0183] In some other embodiments, forming a limiting mask layer on one side of the filling layer may also be achieved by the following methods:

[0184] A metal layer is deposited on the side where the second surface of the mask body is located; the second surface is the side with the smallest through-hole opening area; the metal layer is patterned to form a conductive layer consistent with the vapor deposition pattern; and a limiting mask layer is formed by electro-deposition on the side surface of the conductive layer away from the mask body.

[0185] Taking the conductive layer made of indium tin oxide as an example, an ITO film layer can be formed on the second surface of the mask body by chemical vapor deposition (CVD) or magnetron sputtering, and a vapor deposition pattern required for the display panel (i.e., consistent with the pattern of the defined mask layer) can be formed on the ITO film layer through processes such as exposure, development, and stripping. The method of forming a conductive layer with other materials is similar and will not be repeated here.

[0186] Taking the evaporation mask of the light-emitting layer of the light-emitting device as an example, the production process of the evaporation mask is explained. Fig.32 A schematic diagram of manufacturing another evaporation mask provided by an embodiment of the present invention.

[0187] Step S40: forming a mask body.

[0188] Step S41: forming a filling layer.

[0189] The filling layer is formed in the same manner as described above and will not be described in detail herein.

[0190] Step S42: forming a conductive layer.

[0191] On the side where the second surface 12 of the mask body 1 is located, a conductive layer 5 consistent with a desired evaporation pattern is formed.

[0192] Step S43: forming a definition mask layer by electroplating.

[0193] The conductive layer 5 is used as a cathode, and a limiting mask layer 2 is electro-deposited and grown on the conductive layer 5 by an electrochemical deposition process. The limiting mask layer 2 completely covers the conductive layer 5, so that the pattern of the limiting mask layer 2 is consistent with the pattern of the conductive layer 5. The limiting mask layer 2 includes a plurality of mask units 21, and adjacent mask units 21 have gaps 22. A support structure 3 is arranged around the plurality of mask units 21. Here, the support structure 3 is composed of the conductive layer 5 and the edge portion of the limiting mask layer 2. Each mask unit 21 includes a plurality of pixel openings arranged in an array, through which the filling layer 6 under the conductive layer 5 can be observed, such as Fig.33 , which is a top view of another mask unit provided by an embodiment of the present invention.

[0194] Step S44: peeling off the filling layer.

[0195] The stripping method of the filling layer 5 is the same as that described above, and will not be repeated here.

[0196] Based on the same inventive concept, an embodiment of the present invention further provides an evaporation device, including the evaporation mask as described above.

[0197] The evaporation device can evaporate various organic film layers of the light-emitting device in the OLED display panel.

[0198] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.

[0199] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A vapor deposition mask, characterized in that: include: A mask body, wherein the mask body has a plurality of through holes extending through the thickness direction, one through hole corresponds to one display panel, and the mask body and the base substrate of the display panel have the same thermal deformation characteristics; A limiting mask layer is arranged on one side of the mask body; The substrate is located at a side of the limiting mask layer away from the mask body, and the thickness of the mask body is much greater than the thickness of the limiting mask layer; the material of the limiting mask layer is a metal material; A conductive layer is located between the mask body and the limiting mask layer. The conductive layer is consistent with the vapor deposition pattern required for the display panel. The conductive layer is used as a cathode when the limiting mask layer is made by an electrochemical deposition process. The limiting mask layer is grown on the conductive layer by electro-deposition to form a pattern consistent with the conductive layer.

2. The vapor deposition mask according to claim 1, characterized in that: The cross section of the through hole gradually increases in the thickness direction.

3. The vapor deposition mask according to claim 2, characterized in that: The mask body has a first surface and a second surface which are parallel to each other; The through hole comprises: a first opening and a second opening which are arranged opposite to each other, the first opening is located on the first surface, the second opening is located on the second surface, and the area of ​​the first opening is larger than the area of ​​the second opening; The limiting mask layer is located on the second surface.

4. The vapor deposition mask according to claim 3, characterized in that: The second opening completely covers the effective display area of ​​the base substrate.

5. The vapor deposition mask according to claim 3, characterized in that: The edge spacing between the orthographic projections of the first opening and the second opening on the first surface is greater than 2 mm.

6. The vapor deposition mask according to claim 1, characterized in that: The limiting mask layer comprises: A plurality of mask units, each mask unit corresponding to at least one through hole; A plurality of gaps are provided, wherein the gaps are located between two adjacent mask units.

7. The vapor deposition mask according to claim 6, characterized in that: The mask unit includes a plurality of pixel openings arranged in an array, or a display opening corresponding to an effective display area of ​​the base substrate.

8. The vapor deposition mask according to claim 6, characterized in that: Also includes: A plurality of support structures surround the plurality of mask units.

9. The vapor deposition mask according to claim 8, characterized in that: Also includes: At least one spacing structure is located between at least part of two adjacent mask units.

10. The vapor deposition mask according to any one of claims 1 to 9, characterized in that: The shape of the through hole includes: Rectangle, square, circle, special shape.

11. The vapor deposition mask according to claim 10, characterized in that: Through holes of different shapes are arranged in different areas.

12. The vapor deposition mask according to any one of claims 1 to 9, characterized in that: The definition mask layer completely covers the conductive layer.

13. The vapor deposition mask according to claim 12, characterized in that: The edge of the limiting mask layer is a curved surface.

14. The vapor deposition mask according to any one of claims 1 to 9, characterized in that: The metal material comprises: Any one or any combination of iron, nickel and cobalt; the material of the conductive layer includes: Any one of indium tin oxide, titanium, platinum, and silver.

15. The vapor deposition mask according to any one of claims 1 to 9, characterized in that: The thickness of the mask body is the same as the thickness of the substrate; The mask body and the substrate are made of the same material.

16. The vapor deposition mask according to any one of claims 1 to 9, characterized in that: The thickness of the limiting mask layer ranges from 5um to 30um.

17. A method for making a vapor deposition mask, characterized in that: include: providing a mask body; The mask body is patterned to form a mask body, wherein the mask body has a plurality of through holes extending through the thickness direction, one through hole corresponds to one display panel, and the mask body and the base substrate of the display panel have the same thermal deformation characteristics; forming a filling layer in a through hole of the mask body; The filling layer at least fills the plurality of through holes to make the surface of the mask body flat; Depositing a metal layer on the side where the second surface of the mask body is located; the second surface is the side with the smallest opening area of ​​the through hole; Patterning the metal layer to form a conductive layer consistent with the vapor deposition pattern; On a surface of the conductive layer away from the mask body, a limiting mask layer consistent with the pattern of the conductive layer is formed by electrodeposition; wherein the thickness of the limiting mask layer is much smaller than the thickness of the mask body; The filling layer is peeled off.

18. A vapor deposition device, characterized in that: It comprises the vapor deposition mask as described in any one of claims 1 to 16.

Citation Information

Patent Citations

  • Mask plate and preparation method thereof

    CN103777461A

  • Mask and evaporation device

    CN111850466A

  • Metal mask for manufacturing organic el element and manufacturing method for organic el

    JP2003077660A

  • Shadow mask and method of making the same

    KR1020030049964A