Method for preparing lubricating oil composition and regulating or determining its electrical insulation properties
By measuring the nitrogen content in the lubricant and determining the additive formula based on it, the electrical insulation of lubricant for electric vehicle transmissions is controlled, and the problem of insufficient electrical insulation in the prior art is solved, and the comprehensive performance improvement of lubricant is achieved.
Patent Information
- Application Number
- CN202111181496.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-11
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-10-11
AI Technical Summary
The prior art has failed to effectively regulate the electrical insulation of the lubricating oil composition for electric vehicle transmissions, and cannot deeply explore the structure-effect relationship between additive components and oil performance, resulting in insufficient electrical insulation performance of oil products at high temperatures.
By measuring the weight content of nitrogen in the lubricating oil composition, the type and content of additives are determined according to the predetermined nitrogen content, the base oil and additives are mixed to obtain a lubricating oil composition with a specific volume resistivity, and its electrical insulation is regulated, and through The synergistic effect of additives is preferred to improve the overall performance.
It realizes conveniently regulating the electrical insulation of the lubricating oil composition, meets the insulation protection and transmission system lubrication requirements of electric vehicle motors, and improves the copper corrosion inhibition, low-temperature flowability and foam resistance of the oil products.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention relates to the field of lubricating oils, and in particular to a method for preparing a lubricating oil composition and regulating or determining the electrical insulation thereof. Background Art
[0002] The basic structure of electric vehicles is mainly composed of electric drive system, mechanical transmission system and auxiliary working system. Among them, the electric drive system is the "brain center" of electric vehicles, which is also the biggest difference from traditional fuel vehicles. Due to the significant increase in motor speed (generally the input shaft speed is above 10000r / min) and the reduction in volume, the working conditions are more demanding, the operating temperature is higher, and the oil running load is increased. This requires the oil to have excellent electrical insulation performance and excellent heat dissipation and cooling performance under high temperature conditions. At present, the transmission system of electric vehicles is still based on the transmission system of traditional fuel vehicles. In order to make the transmission device compact and improve the transmission efficiency, combined with the design characteristics of electric vehicles themselves, it tends to be "mechatronic" design, that is, the motor and mechanical transmission part share a set of lubrication system, which requires the oil to meet the insulation of the motor and the lubrication of the mechanical transmission system at the same time. At the same time, in order to improve the battery loss of electric vehicles, improve the transmission efficiency, and increase the cruising range, low viscosity oil is the development trend.
[0003] Electric vehicles are equipped with one-speed, two-speed or multi-speed gearboxes. Currently, the market is dominated by one-speed reduction structures. Related products mainly use automatic transmission fluid (ATF) and GL-5 / GL-4 gear oil. The comprehensive properties of oil products such as electrical insulation, copper corrosion inhibition, and anti-foaming properties cannot fully meet the characteristics of electric vehicle gearboxes. CN112930389A discloses a lubricating oil composition, which contains: lubricating oil base oil; (A) calcium salicylate detergent with a calcium content of 0.005-0.03% by mass based on the total amount of the composition; and (B) phosphite compound with a phosphorus content of 0.01-0.06% by mass based on the total amount of the composition. The composition balances the electrical insulation, wear resistance and fatigue resistance of the composition after oxidative degradation of the oil product. The volume resistivity of the oxidatively degraded oil at 80°C is 1.0×10 7 Ω·m or more.
[0004] US2018 / 0100114A discloses a lubricating oil composition for electric vehicles and hybrid vehicles, which lubricating oil comprises at least 80wt% of a lubricating base oil, 0.5-5wt% of one or more dispersants, 0-4wt% of one or more neutral metal detergents, 0-1.5wt% of zinc dialkyl dithiophosphate, 0-0.2wt% of molybdenum dialkyl dithiocarbamate, 0-2wt% of an active viscosity modifier and 0.01-5wt% of one or more other lubricating oil additives, and the conductivity of the composition is between 50-3000pS / m.
[0005] WO2018 / 067902A discloses a composition for an electric vehicle transmission system, which comprises a lubricating base oil as a main component, an additive composition as a secondary component, and an effective amount of one or more conductive agents as a secondary component. The conductivity of the composition is between 10-20000 pS / m and the dielectric constant ranges from 1.6 to 3.6.
[0006] The above prior art is more about formulating components to improve the electrical insulation of the composition, and does not disclose in depth the method for regulating the electrical insulation of the lubricating oil composition and the structure-activity relationship between the additive components and the oil performance. Therefore, it is still necessary to further investigate the method for regulating the electrical insulation of the composition, so as to obtain a lubricating oil composition with excellent electrical insulation performance, and balance the comprehensive performance of the oil such as copper corrosion inhibition, low temperature fluidity, and anti-foaming. Summary of the invention
[0007] The purpose of the present invention is to overcome the problems existing in the prior art and provide a method for preparing a lubricating oil composition and regulating or determining the electrical insulation thereof.
[0008] The inventors of the present invention have found in their research that the volume resistivity of a lubricating oil composition increases with the decrease of the nitrogen content in the lubricating oil composition. Therefore, in order to achieve the above-mentioned object, the present invention provides a method for preparing a lubricating oil composition, wherein the lubricating oil composition contains a base oil and an additive, and the method comprises:
[0009] (1) According to the predetermined C N Determine the type and content of additives, among which C N Indicates the weight content of nitrogen in the lubricating oil composition;
[0010] (2) The base oil is mixed with the additive selected according to step (1) to obtain a lubricating oil composition having a specific volume resistivity.
[0011] The second aspect of the present invention provides a method, an instrument or a reagent for determining the nitrogen content in a lubricating oil composition and its application in regulating the electrical insulation of the lubricating oil composition.
[0012] A third aspect of the present invention provides a method for determining the electrical insulation of a lubricating oil composition, the method comprising: determining the weight content of nitrogen in the lubricating oil composition to be tested, C N , where C N The smaller the value, the better the electrical insulation property of the lubricating oil composition to be tested.
[0013] A fourth aspect of the present invention provides a method for screening a lubricating oil composition for an electric vehicle gearbox, the method comprising: determining the weight content of nitrogen in the lubricating oil composition to be screened C N , select C N The smaller lubricating oil composition is used as a lubricating oil composition for electric vehicle gearboxes.
[0014] Through the above technical scheme, the present invention can conveniently regulate the electrical insulation (volume resistivity) of the lubricating oil composition, that is, it can obtain a lubricating oil composition with a predetermined electrical insulation (volume resistivity) in a simple and easy-to-operate manner, thereby balancing the key properties of the lubricating oil composition, such as electrical insulation, copper corrosion inhibition, low-temperature fluidity and anti-foaming properties, so as to simultaneously meet the insulation protection requirements of electric vehicle motors and the lubrication requirements of the transmission system. DETAILED DESCRIPTION
[0015] The endpoints and any values of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.
[0016] The present invention provides a method for preparing a lubricating oil composition, wherein the lubricating oil composition contains a base oil and an additive, characterized in that the method comprises:
[0017] (1) According to the predetermined C N Determine the type and content of additives, among which C N Indicates the weight content of nitrogen in the lubricating oil composition;
[0018] (2) The base oil is mixed with the additive selected according to step (1) to obtain a lubricating oil composition having a specific volume resistivity.
[0019] According to a preferred embodiment of the present invention, the volume resistivity of the lubricating oil composition at 25°C satisfies: Y 25 =a·C N +b,Y 25The unit is MΩ·m, a is any value between -3000000 and -1500000, and b is any value between 500 and 2000. According to a specific embodiment of the present invention, Y 25 =-2000000C N +1000.
[0020] According to a preferred embodiment of the present invention, the volume resistivity of the lubricating oil composition at 80°C satisfies Y 80 = k·C N +t,Y 80 The unit is MΩ·m, k is any value between -300000 and -100000, and b is any value between 50 and 200. According to a specific embodiment of the present invention, Y 80 = -200000C N +100.
[0021] According to the present invention, 0.01 wt % ≤ C N ≤0.25 wt%. It can be measured with reference to NB / SH / T 0704-2010 (Determination of nitrogen content in petroleum and petroleum products, boat sampling chemiluminescence method).
[0022] According to the present invention, the additive can be an additive commonly used in lubricating oil in the art, for example, the additive is selected from at least one of a viscosity index improver, a dispersant, an extreme pressure antiwear agent, an antioxidant, a metal passivator and an antifoaming agent.
[0023] According to the present invention, there is no particular requirement for the content of each additive in the lubricating oil composition. Based on the total weight of the lubricating oil composition, the amount of the viscosity index improver can be 2-10 wt % (such as 2 wt %, 3 wt %, 4 wt %, 4.5 wt %, 5.5 wt %, 6 wt %, 7 wt %, 8 wt %, 9 wt %, 10 wt % or any value in between), preferably 3-8 wt %.
[0024] Based on the total weight of the lubricating oil composition, the amount of the dispersant can be 0.5-10 wt % (e.g., 0.6 wt %, 0.7 wt %, 0.8 wt %, 1.2 wt %, 2.5 wt %, 3.8 wt %, 4 wt %, 4.5 wt %, 5.5 wt %, 6 wt %, 7 wt %, 8 wt %, 9 wt %, 10 wt % or any value therebetween), preferably 0.5-5 wt %.
[0025] Based on the total weight of the lubricating oil composition, the amount of the extreme pressure anti-wear agent can be 0.1-5 weight % (such as 0.6 weight %, 0.7 weight %, 0.9 weight %, 1.2 weight %, 2.5 weight %, 3.8 weight %, 4 weight %, 4.5 weight %, 5 weight % or any value in between the above values), preferably 0.5-2 weight %.
[0026] Based on the total weight of the lubricating oil composition, the antioxidant can be used in an amount of 0.5-10 wt % (e.g., 0.6 wt %, 0.7 wt %, 0.8 wt %, 1.2 wt %, 2.5 wt %, 3.8 wt %, 4 wt %, 4.5 wt %, 5.5 wt %, 6 wt %, 7 wt %, 8 wt %, 9 wt %, 10 wt % or any value therebetween), preferably 0.5-3 wt %.
[0027] Based on the total weight of the lubricating oil composition, the amount of the metal passivator can be 0.01-2 weight % (such as 0.06 weight %, 0.08 weight %, 0.12 weight %, 0.15 weight %, 0.5 weight %, 0.6 weight %, 0.8 weight %, 1 weight %, 2 weight % or any value in between the above values), preferably 0.02-0.5 weight %.
[0028] Based on the total weight of the lubricating oil composition, the amount of the antifoaming agent can be 0.001-0.1 wt % (such as 0.002 wt %, 0.005 wt %, 0.008 wt %, 0.01 wt %, 0.05 wt %, 0.08 wt %, 0.1 wt % or any value in between), preferably 0.001-0.01 wt %.
[0029] According to the present invention, the viscosity index improver is a substance capable of improving (increasing) the viscosity index, and may be any of the various viscosity index improvers commonly used in the art, but preferably, the viscosity index improver is selected from at least one of polymethacrylate (PMA) and polyisobutylene (PIB). More preferably, the kinematic viscosity of the polymethacrylate at 100° C. is 500-1500 mm 2 More preferably, the number average molecular weight of the polyisobutylene is 1000-3400.
[0030] According to the present invention, the dispersant is a substance capable of improving the dispersibility of the lubricating oil composition, preferably an ashless dispersant. The ashless dispersant is selected from at least one of succinimide-type ashless dispersants, phenolic amine-type ashless dispersants (such as phenolic amine-type condensates), aromatic amine-type ashless dispersants and benzylamine-type ashless dispersants, and more preferably selected from at least one of monopolyisobutylene succinimide, dipolyisobutylene succinimide, high molecular weight polyisobutylene succinimide and boronized polyisobutylene succinimide. The above-mentioned ashless dispersant can be obtained by commercial purchase or prepared by itself. For example, dipolyisobutylene succinimide and high molecular weight polyisobutylene succinimide can generally be prepared by sequentially hydrocarbonizing and aminating polyisobutylene. Boronized polyisobutylene succinimide includes boron-modified monopolyisobutylene succinimide, boron-modified dipolyisobutylene succinimide and boron-modified high molecular weight polyisobutylene succinimide. Phenolic amine condensates are generally prepared by the Mannich reaction of alkylphenol formaldehyde and amine. Aromatic amine ashless dispersants generally refer to ashless dispersants containing at least one aromatic structure. The preparation method can be found in Gieselman MD, Pudeiski JK, Raguz MG, et al. Lubricating Composition Containing a Carboxylic Function-alised Polymer and Dispersant: US, 8569217 [P]. 2013.
[0031] According to the present invention, the extreme pressure anti-wear agent is a substance capable of improving the extreme pressure anti-wear property of the lubricating oil composition, and various extreme pressure anti-wear agents commonly used in the art can be used. However, preferably, the extreme pressure anti-wear agent is selected from at least one of alkyl dithiophosphates, phosphates and phosphate amine salts, and more preferably selected from at least one of di-n-butyl phosphite, tricresyl phosphate, isooctyl phosphate octadecylamine salt and dialkyl dithiophosphates.
[0032] According to the present invention, the antioxidant is a substance capable of improving the oxidation stability of the lubricating oil composition. Preferably, the antioxidant is selected from at least one of aminothioesters, alkylated diphenylamines, N-phenyl-α-naphthylamine and shielded phenols, and more preferably selected from at least one of N-phenyl-α-naphthylamine, 2,6-di-tert-butyl-p-cresol, 2,6-di-tert-butylphenol, 2,6-di-tert-butyl-4-hydroxyphenylpropionate and di-n-octyl dithiocarbamate.
[0033] According to the present invention, the metal passivator is a catalytic agent capable of inhibiting the catalytic effect of metal (especially copper) on the oxidation of the lubricating oil composition, and can be various metal passivators commonly used in the art. Preferably, the metal passivator is selected from at least one of benzotriazole derivatives (alkylaminomethylenebenzotriazole) and thiadiazole polysulfide, and more preferably selected from at least one of N,N-di-n-butylaminomethylenebenzotriazole and thiadiazole alkylthiol peroxide condensate. The above metal passivator can be obtained by commercial purchase or prepared by itself. The alkylaminomethylenebenzotriazole can be obtained by benzotriazole and di-n-butylamine undergoing Mannich and condensation reactions in the presence of formaldehyde, then adding water to settle and adding an acidifying agent to neutralize, and finally by solvent extraction, water washing, and distillation. The thiadiazole polysulfide can be synthesized by using hydrazine hydrate, carbon disulfide and sodium hydroxide as raw materials to synthesize 2,5-disulfide thiadiazole sodium salt, and then adding mercaptan and hydrogen peroxide to couple after acidification, and then extracting, washing, and distilling to obtain.
[0034] According to the present invention, the antifoaming agent is a substance that can inhibit the generation of foam in the lubricating oil. It can be a conventional selection, but preferably, the antifoaming agent is selected from at least one of silicone oil and non-silicone antifoaming agents, and more preferably selected from at least one of polymethyl silicone oil, dimethyl silicone oil, methyl silicone ester, polysiloxane, polyacrylate and polyacrylate.
[0035] According to the present invention, by using the additives in the preferred embodiment described above, various additives can work synergistically to further improve the comprehensive performance of the lubricating oil composition, such as electrical insulation, copper corrosion inhibition, low temperature fluidity and anti-foaming properties.
[0036] According to the present invention, there is no particular limitation on the amount of the base oil, and the lubricating oil composition can be prepared in a manner that the balance is the base oil. However, according to a preferred embodiment of the present invention, based on the total weight of the lubricating oil composition, the amount of the base oil can be 63-96.5% by weight, preferably 85-95% by weight.
[0037] According to the present invention, the base oil can be selected from the base oil commonly used in the art for lubricating oil, and can be at least one of mineral base oil, synthetic base oil and biological base oil, preferably at least one of Class II hydrogenated base oil, Class III hydrogenated base oil, poly-α-olefin, alkylbenzene and alkylnaphthalene. The kinematic viscosity of the base oil at 100°C can be 1-10 mm 2 / s, preferably 3-6mm 2 / s. “Kinematic viscosity” can be measured by GB / T 265 method.
[0038] According to the present invention, the content of metal elements in the lubricating oil composition is less than 0.01% by weight, and preferably contains no metal elements. In other words, the raw material for preparing the lubricating oil composition is a raw material that substantially contains no metal elements.
[0039] According to a preferred embodiment of the present invention, the lubricating oil composition consists only of the base oil and additives as described above.
[0040] According to a preferred embodiment of the present invention, in addition to the ashless dispersant, the total nitrogen content of other additives in the composition, such as antioxidants and metal passivators, is relatively small, and can be ignored in the actual preparation process. N Mainly refers to the percentage of nitrogen in the dispersant to the total weight of the lubricating oil composition. Therefore, in this case, the method preferably includes:
[0041] (a) Calculate the nitrogen content in the nitrogen-containing ashless dispersant;
[0042] (b) An ashless dispersant having a specific nitrogen content and other additives are selected and mixed with a base oil to obtain a lubricating oil composition having a specific volume resistivity.
[0043] According to the method of the present invention, a volume resistivity of 10×10 7 Ω·m or more, volume resistivity at 80℃ reaches 1×10 7 Furthermore, a lubricating oil composition with a volume resistivity of 50×10 7 Ω·m or more, volume resistivity at 80℃ reaches 5×10 7 Furthermore, a lubricating oil composition with a volume resistivity of 60×10 7 Ω·m or more, volume resistivity at 80℃ reaches 6×10 7 Lubricating oil composition with a value of Ω·m or more.
[0044] According to one embodiment of the present invention, the mixing method may include: mixing a viscosity index improver, an antifoaming agent and a base oil, heating to 65-75° C. and stirring for 2-5 hours; then mixing with a dispersant, an antioxidant, an extreme pressure antiwear agent and a metal passivator, and continuing to stir at 65-75° C. (about 2-5 hours) until the mixture is uniform and transparent.
[0045] The present invention also provides a method for determining the nitrogen content in a lubricating oil composition, and the use of an instrument or reagent in regulating the electrical insulation of the lubricating oil composition. The inventors of the present invention have found in their research that the volume resistivity of the lubricating oil composition increases with the decrease of the nitrogen content in the lubricating oil composition (especially within the additive formulation range listed in the preferred embodiment of the present invention). Therefore, by pre-determining the nitrogen content, the electrical insulation (volume resistivity) of the lubricating oil composition to be prepared can be determined according to the nitrogen content determination result, thereby conveniently and quickly preparing a lubricating oil composition with a predetermined electrical insulation (volume resistivity). The method for determining the nitrogen content in the lubricating oil composition can be NB / SH / T0704-2010 or NB / SH / T 0656-2017.
[0046] The present invention also provides a method for determining the electrical insulation of a lubricating oil composition, characterized in that the method comprises: determining the weight content of nitrogen in the lubricating oil composition to be tested, C N , where C N The smaller the volume resistivity of the lubricating oil composition, the better the electrical insulation of the lubricating oil composition to be tested. N The method of the present invention is particularly suitable for lubricating oil compositions containing nitrogen as a main element, especially lubricating oil compositions as described in the above preferred embodiments.
[0047] The present invention also provides a method for screening a lubricating oil composition for an electric vehicle gearbox, characterized in that the method comprises: determining the weight content of nitrogen in the lubricating oil composition to be screened C N , select C N The smaller lubricating oil composition is used as a lubricating oil composition for electric vehicle gearboxes. The method of the present invention is particularly suitable for lubricating oil compositions containing nitrogen as the main element, especially lubricating oil compositions as described in the above preferred embodiments.
[0048] In the present invention, the additives and base oil in the lubricating oil composition are as described above and will not be described in detail herein.
[0049] The present invention will be described in detail below by way of examples. In the following examples:
[0050] Non-dispersible PMA viscosity index improver, 100℃ kinematic viscosity 575mm 2 / s, produced by Lanzhou Lubrizol Additives Company;
[0051] Bis(isobutylene) succinimide T154A, dispersibility SDT≥55, nitrogen content ~1.1% by weight, produced by Yangzi Petrochemical Company;
[0052] Monoisobutylene succinimide T151, dispersibility SDT ≥ 55, nitrogen content ~ 2.1% by weight, produced by Yangzi Petrochemical Company;
[0053] High molecular weight polyisobutylene succinimide T161, dispersibility SDT ≥ 55, nitrogen content ~ 1.5% by weight, produced by Yangzi Petrochemical Company;
[0054] Phenolic antioxidant T512 (2,6-di-tert-butyl-4-hydroxyphenyl propionate), density 0.95g / cm 3 , 100℃ kinematic viscosity 7.2mm 2 / s, produced by Beijing Xingpu Fine Chemical Technology Development Co., Ltd.;
[0055] Aminothioester antioxidant T323 (thiocarbamate), density 950-1150g / cm 3 , 100℃ kinematic viscosity 15mm 2 / s, produced by Changsha Wangcheng Petrochemical Co., Ltd.;
[0056] Tricresol phosphate T306, acid value less than 0.1mgKOH / g, produced by Zibo Huihua Petrochemical Company;
[0057] Thiadiazole polysulfide T561, kinematic viscosity at 100℃, 15.5mm 2 / s, produced by Zibo Huihua Petrochemical Company;
[0058] Dimethyl silicone oil, 25℃ kinematic viscosity 12500mm 2 / s, pour point -46℃, produced by Dow Corning;
[0059] Type III hydrogenated base oil, kinematic viscosity at 100°C 4.45 mm 2 / s, viscosity index 125, produced by Maoming Petrochemical.
[0060] Examples 1-18
[0061] The lubricating oil composition was prepared according to the weight percentage of the base oil and the lubricating oil shown in Tables 1, 3 and 4. The preparation process included: adding the viscosity index improver, the antifoaming agent and the base oil into a blending kettle with a stirrer in proportion, heating to 70°C and stirring for 3 hours, blending the ashless dispersant, the antioxidant, the extreme pressure antiwear agent and the metal passivator in proportion, and then adding them to the blending kettle, and continuing to stir at 70°C for 3 hours until the mixture is uniform and transparent.
[0062] The properties and volume resistivity (ρ) of the obtained lubricating oil composition were tested according to the methods described in Table 2.
[0063] In Table 1, the nitrogen content is calculated by the nitrogen content in the feed, and the theoretical ρ is expressed according to the formula Y25 =-2000000C N +1000 and Y 80 =-200000C N +100 calculated theoretical volume resistivity value.
[0064] In Table 3, the nitrogen content is calculated by the nitrogen content in the feed, and the theoretical ρ is expressed according to the formula Y 25 =-2000000C N +1000 and Y 80 =-200000C N +100 calculated theoretical volume resistivity value.
[0065] In Table 4, the nitrogen content is calculated by the nitrogen content in the feed, and the theoretical ρ is expressed according to the formula Y 25 =-1500000C N +950 and Y 80 =-150000C N +100 calculated theoretical volume resistivity value.
[0066] Comparative Example 1
[0067] The conventional oil is prepared by blending a Class III hydrogenated base oil with a composite additive purchased from Lubrizol Corporation, with the contents of the base oil and the composite additive being 89 weight % and 11 weight %, respectively.
[0068] Table 1
[0069]
[0070] Table 2
[0071]
[0072] Table 3
[0073]
[0074]
[0075] Table 4
[0076]
[0077] It can be seen from the results in Tables 1-4 that the theoretical volume resistivity obtained by the method of the present invention is close to the measured volume resistivity. Therefore, the electrical insulation of a lubricating oil composition of unknown composition can be obtained only by a simple nitrogen content test, thereby conveniently realizing the screening of lubricating oil compositions and the regulation of electrical insulation.
[0078] As shown in Table 2, the electric vehicle transmission oil compositions obtained in Examples 1-6 have excellent electrical insulation, a breakdown voltage exceeding 60 kV, and a volume resistivity of 10×10 7 Ω·m or more, volume resistivity at 80℃ reaches 1×10 7 Ω·m or more, which indicates that the oil has excellent electrical insulation properties. At the same time, as the amount of nitrogen-containing ash-free dispersant in the lubricating oil composition decreases, the volume resistivity of the lubricating oil composition at 25°C and 80°C both show an increasing trend, and there is a linear relationship between the volume resistivity of the oil and the nitrogen content in the composition. In addition, the lubricating oil compositions obtained in Examples 1-6 have excellent copper corrosion inhibition, and the copper corrosion grade reaches 1b after heating at 150°C for 3h, and the anti-foaming and high-temperature anti-foaming properties are excellent. The apparent viscosity at -40°C is less than 10000mPa·s, and it has good low-temperature fluidity. The kinematic viscosity at 100°C is 5mm 2 / s, and the low viscosity oil characteristics are conducive to increasing the heat dissipation of the oil and improving the transmission efficiency of electric vehicles. Therefore, the lubricating oil composition finally obtained in the embodiment of the present invention has excellent electrical insulation, and the electrical insulation performance of the oil can be regulated by changing the amount of nitrogen-containing ashless dispersant added in the composition, and the key properties of the composition such as copper corrosion inhibition, low temperature fluidity and anti-foaming are balanced.
[0079] Similarly, Examples 7-18 exhibited key properties such as copper corrosion inhibition, low temperature fluidity and anti-foaming properties similar to those of Examples 1-6. Specifically, Examples 7-11 and 13-17, 100°C kinematic viscosity ≈5.0 mm 2 / s, pour point is lower than -40℃, viscosity index>150, apparent viscosity at -40℃ is not higher than 10000mPa·s, copper sheet corrosion inhibition performance is at 150℃, after 3h, the copper sheet grade is not greater than grade 2, DKA oxidation test is passed, and anti-foaming performance is excellent.
[0080] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.
Claims
1. A method for determining the volume resistivity of a lubricating oil composition, characterized in that The method comprises: determining the weight content of nitrogen in the lubricating oil composition to be tested C N , where C N The smaller the value, the higher the volume resistivity of the lubricating oil composition to be tested; The lubricating oil composition contains a base oil and an additive, wherein the additive is selected from at least one of a viscosity index improver, a dispersant, an extreme pressure anti-wear agent, an antioxidant, a metal passivator and an anti-foaming agent; the dispersant is selected from at least one of a succinimide-type ashless dispersant, a phenalkamine-type ashless dispersant, an aromatic amine-type ashless dispersant and a benzylamine-type ashless dispersant; the base oil is selected from at least one of a Class II hydrogenated base oil, a Class III hydrogenated base oil, a poly-α-olefin, an alkylbenzene and an alkylnaphthalene; the viscosity index improver is selected from at least one of a polymethacrylate and a polyisobutylene; the extreme pressure anti-wear agent is selected from at least one of an alkyl dithiophosphate, a phosphate ester and an amine salt of a phosphate ester; the antioxidant is selected from at least one of an aminothioester, an alkylated diphenylamine, an N-phenyl-α-naphthylamine and a shielded phenol; the metal passivator is selected from at least one of an alkylaminomethylenetriazole and a thiadiazole polysulfide; the anti-foaming agent is selected from at least one of a silicone oil and a non-silicon anti-foaming agent; The volume resistivity of the lubricating oil composition at 25°C satisfies: Y 25 =a•C N +b,Y 25 The unit is MΩ•m, a is any value between -3000000 and -1500000, and b is any value between 500 and 2000; the volume resistivity of the lubricating oil composition at 80°C satisfies Y 80 =k•C N +t,Y 80 The unit is MΩ•m, k is any value between -300000 and -100000, and t is any value between 50 and 200; where 0≤C N ≤0.25% by weight.
2. The method according to claim 1, wherein: The kinematic viscosity of the base oil at 100°C is 1-10 mm 2 / s.
3. The method according to claim 1, wherein: Based on the total weight of the lubricating oil composition, the viscosity index improver is used in an amount of 2-10 wt %, or the dispersant is used in an amount of 0.5-10 wt %, or the extreme pressure antiwear agent is used in an amount of 0.1-5 wt %, or the antioxidant is used in an amount of 0.5-10 wt %, or the metal passivator is used in an amount of 0.01-2 wt %, or the antifoaming agent is used in an amount of 0.001-0.1 wt %.
4. The method according to claim 1, wherein: Based on the total weight of the lubricating oil composition, the viscosity index improver is used in an amount of 3-8% by weight, or the dispersant is used in an amount of 0.5-8% by weight, or the extreme pressure anti-wear agent is used in an amount of 0.5-2% by weight, or the antioxidant is used in an amount of 0.5-3% by weight, or the metal passivator is used in an amount of 0.02-0.5% by weight, or the anti-foaming agent is used in an amount of 0.001-0.01% by weight.
5. The method according to claim 1, wherein: The kinematic viscosity of the base oil at 100°C is 3-6 mm 2 / s.
6. The method according to claim 1, wherein: The kinematic viscosity of the polymethacrylate at 100°C is 500-1500 mm 2 / s; And / or, the number average molecular weight of the polyisobutylene is 1000-3400; and / or, the dispersant is selected from at least one of monopolyisobutylene succinimide, dipolyisobutylene succinimide, high molecular weight polyisobutylene succinimide and boronated polyisobutylene succinimide; and / or, the extreme pressure anti-wear agent is selected from at least one of di-n-butyl phosphite, tricresyl phosphate, isooctyl phosphate octadecylamine salt and dialkyl dithiophosphate; And / or, the antioxidant is selected from at least one of N-phenyl-α-naphthylamine, 2,6-di-tert-butyl-p-cresol, 2,6-di-tert-butylphenol, 2,6-di-tert-butyl-4-hydroxyphenylpropionate and di-n-octyl dithiocarbamate; and / or, the metal passivator is selected from at least one of N,N-di-n-butylaminomethylenebenzotriazole and thiadiazolidinyl mercaptan hydroperoxide condensate; And / or, the anti-foaming agent is selected from at least one of polymethyl silicone oil, dimethyl silicone oil, methyl silicone ester, polysiloxane, polyacrylate and polyacrylate.
7. Use of a method, an apparatus or a reagent for determining the nitrogen content in a lubricating oil composition in regulating the electrical insulation properties of the lubricating oil composition, wherein: The additives and base oil in the lubricating oil composition are the additives and base oil in the method according to any one of claims 1 to 6.
8. A method for screening a lubricating oil composition for an electric vehicle gearbox, characterized in that: The method comprises: determining the weight content of nitrogen in the lubricating oil composition to be screened C N , select C N A smaller lubricating oil composition is used as a lubricating oil composition for electric vehicle gearboxes, wherein the additives and base oil in the lubricating oil composition are the additives and base oil in the method described in any one of claims 1 to 6.