Yankee dryer and tissue paper machine

By using P690 steel grade or similar cylindrical shell and outer steel covering, combined with weld joint and liquid coating protection, the surface wear and metallization layer of steel Yankee drying cylinder is solved, achieving high wear resistance and reduce production interruption effects.

CN116348626BActive Publication Date: 2024-12-03VALMET AB
View PDF 22 Cites 0 Cited by

Patent Information

Application Number
CN202180072273.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-10-21
Filing Date
2021-10-20
Publication Date
2024-12-03
Estimated Expiration
2041-10-20

AI Technical Summary

Technical Problem

The surface of the steel Yankee dryer is prone to wear due to its low hardness and the metallization layer may break or delaminate, resulting in production interruption and high costs, and may have streak problems when drying paper.

Method used

Using a cylindrical shell made of P690 steel grade or similar steel, a high hardness outer surface is formed by combining circumferential welds and covering the outer steel to avoid the use of hard metallization layers, and a liquid coating device is installed in the paper machine and Hot air blowing device to protect the housing.

Benefits of technology

It significantly reduces the risk of damage to the surface of Yankee dryer, avoids cracks and delamination of the metallized layer, reduces production interruptions, and does not require laser hardening or complex manufacturing processes, improving the steel Yankee dryer Wear resistance and durability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116348626B_ABST
    Figure CN116348626B_ABST
Patent Text Reader

Abstract

The present invention relates to a steel Yankee dryer for a tissue papermaking machine and a tissue papermaking machine using such a steel Yankee dryer, wherein the outer surface (9) of the cylindrical shell of the steel Yankee dryer is formed by steel of grade P690 as defined in European standard EN 10028-6:2017 or similar steel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a steel Yankee dryer and a machine for manufacturing tissue paper comprising such a Yankee dryer. Background Art

[0002] Machines for manufacturing tissue paper usually include a Yankee dryer, which is heated internally by hot steam during operation. In the following, the term "Yankee" will be used for the Yankee dryer. The wet fiber web transferred to the Yankee dryer is dried on the outer surface, the "drying surface" of the Yankee dryer, and is subsequently creped from the drying surface (outer surface) of the Yankee dryer by a creping blade. During the twentieth century, Yankee dryers were usually made of cast iron, but in recent years, Yankee dryers have been made of welded steel. The weight of a steel Yankee dryer is less than that of a cast iron Yankee dryer with the same required strength, so a steel Yankee dryer is considered to be advantageous. An example of a steel Yankee dryer is disclosed in patent document EP2126203B1. As mentioned above, a creping blade is used to crepe the dried fiber web from the surface of the Yankee dryer. In practice, this means that the surface of the Yankee dryer will be subjected to pressure from the doctor blade. Since cast iron generally has an HB hardness (i.e. Brinell hardness) of 220-260, the surface of a cast Yankee dryer has a relatively high hardness. Therefore, the surface is not easily worn by contact with a doctor blade pressed against its surface. However, experience has shown that even Yankee dryers made of cast iron are subject to considerable wear. For this reason, it has long been practice to metallize the surface of the Yankee dryer in order to obtain a harder surface. In the context of the present patent application, the terms "to metallize" and "metallization" refer to a process in which the outer surface (drying surface) of the Yankee dryer is coated with a hard layer, which can be based on an element or alloy or mixture of a metal powder with at least one carbide or nitride or possibly other elements, or a metal matrix containing at least one carbide or nitride or possibly other elements. The coating can usually be applied to the surface of the Yankee dryer by spraying. An example of this technology is disclosed in U.S. Patent No. 4,064,608. Other examples are disclosed in U.S. Pat. No. 5,123,152, U.S. Pat. No. 6,171,657, and U.S. Pat. No. 10,240,291. It should be noted that many different compositions for the hard layer have been proposed. For example, the hard layer can be an iron alloy containing about 20 to about 47 weight percent chromium, about 2.5 to about 6.5 weight percent boron, about 1.7 to about 2.7 weight percent silicon, and less than about 8 weight percent molybdenum, as proposed in the aforementioned U.S. Pat. No. 6,171,657. In the context of a Yankee dryer, it should be noted that the term "coating" may also be used to refer to a liquid coating that is continuously sprayed onto the surface of the Yankee dryer during operation, which is fundamentally different from a hard coating that is applied as part of the manufacturing process.When discussing the application of a hard layer to increase hardness and wear resistance, the technical term commonly used by those skilled in the art is "metallization", and this term and "to metallize" (except when used in reference to other documents cited herein and using the term in a different sense) will be used in this patent application and all patents issued based thereon to refer to the application of a hard and wear-resistant layer permanently bonded to the steel drying surface of the Yankee dryer, regardless of the precise composition of the layer. Such a layer will be referred to below as a "metallized layer". The term "coating" used hereinafter in this patent application will refer to the application of a temporary liquid coating during the operation of a tissue paper machine (except when used in reference to other documents cited herein and using the term in a different sense).

[0003] The hardness of the steel used to make steel Yankee dryers is significantly lower than that of cast iron. Typical values ​​for the hardness of such steels may be of the order of about 140 HB, or may be in the range of 120-170 HB.

[0004] Since the steel grades used for Yankee dryers usually have a significantly lower hardness (of the order of 140 HB) than cast iron (220-260 HB), it is required that Yankee dryers made of steel be metallized. Different metallization layers for steel Yankee dryers have been proposed. From a 2007 paper, Mr. Luca Mignani discussed a steel Yankee dryer with a "metal coating" whose surface hardness was said to be twice that of cast iron ("Application of a Steel Yankee in Tissue Machines", TAPPI Yankee Dryer Safety Committee, Jacksonville 10 / 23 / 07), although no details were given as to the exact composition. In a 2008 paper by Mr. Luca Mignani ("Advances with Steel Yankee Dryers", TISSUE WORLD, Asia 2008), Mr. Mignani proposed a steel Yankee dryer that could be provided with a "metal coating" (i.e., a metallized layer) and the "metal coating" could be, for example, an alloy with a high content of Cr and Ni and having a hardness of 60 HRC. Although hardness measured in terms of HRC does not directly correspond to Brinell hardness, a value of 60 HRC can be said to correspond to about 600 HB. In the same paper, Mr. Mignani also proposed that a is a trademark owned by the company Valmet and relates to the metallization of Yankee dryers with thermally sprayed metal coatings. The paper by Mr. Mignani gives hardness values ​​in this case of "50 to 60 HRC", ie of the order of about 500-600 HB.

[0005] As an alternative to metallization, it has been proposed to harden the outer shell of a steel Yankee dryer by laser, and this solution is disclosed in patent document AT 519 996 A2. According to this document, hardness values ​​of up to 400 HB can be achieved.

[0006] However, the currently known techniques of metallization and possibly hardening by laser represent further steps in the Yankee dryer manufacturing process, which makes the manufacturing process more complicated.

[0007] With regard to metallized steel Yankee dryers, the inventors of the present invention have also noticed that streaks may occur in paper that has been dried on such dryers.

[0008] The inventors have also seen that the metallization layer of the Yankee dryer may crack and / or delaminate, which makes it necessary to stop production and shut down the machine. When this happens, production is severely disrupted and its costs can be very high.

[0009] It is therefore an object of the present invention to provide a Steel Yankee dryer which is suitably protected against surface wear and which can also be manufactured in a simple manner, and to provide a machine having such a Steel Yankee dryer. Another object of the present invention is to provide a Steel Yankee dryer which prevents or reduces the appearance of streaks in paper dried on the machine. Summary of the invention

[0010] The present invention relates to a steel Yankee dryer comprising a cylindrical shell having two axial ends. An end wall is joined to each axial end by means of a circumferential weld. The cylindrical shell also has an outer surface and an inner surface, in which an inner surface circumferential groove is formed. According to an embodiment of the invention, the cylindrical shell is completely made of steel of the P690 steel series as defined in European standard EN 10028-6:2017 or a similar steel, so that the outer surface of the shell is formed by such steel, i.e. the outer surface of the shell is formed by steel of P690 steel grade or a similar steel having the composition defined in claim 1. In another embodiment of the invention, the cylindrical shell is made of steel of different grades and an outer layer made of P690 grade steel or a similar steel is applied to the outer cylindrical surface of the cylindrical shell.

[0011] The invention also relates to a tissue papermaking machine comprising a steel Yankee dryer according to the invention and a creping doctor having a creping blade arranged to act on the outer surface of the Yankee dryer.

[0012] In an embodiment of the present invention, the tissue papermaking machine further comprises a device for applying the liquid coating onto the outer surface of the Yankee dryer.

[0013] The paper machine may also optionally comprise a Yankee dryer hood arranged to be able to blow hot air onto the outer surface of the cylindrical shell over a portion of the circumference of the shell.

[0014] In an embodiment of the invention, the cleaning blade may be arranged to act on the outer surface of the housing at a position after the creping blade but before the coating device in the direction of rotation of the Yankee dryer.

[0015] According to a first embodiment, the machine may additionally comprise at least one ventilated dryer. In this embodiment, the embossing fabric will be an air-permeable fabric arranged to carry the fiber web over a portion of the circumference of the at least one ventilated dryer and to carry the fiber web from the at least one ventilated dryer to a transfer nip formed between the press roll and the Yankee dryer. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 is a schematic cross-sectional view of a Yankee dryer.

[0017] Figure 2 yes Figure 1 A magnified view of a portion of .

[0018] Figure 3 is a schematic side view of a tissue papermaking machine according to the present invention during operation.

[0019] Figure 4 Schematic diagram of the creping blade acting on the Yankee dryer.

[0020] Figure 5 is a schematic side view showing how a tissue paper machine has a Yankee dryer hood. DETAILED DESCRIPTION

[0021] Reference Figure 1The Yankee dryer 2 of the present invention is a steel Yankee dryer comprising a cylindrical shell 3 having two axial ends 4, 5. It should be understood that the cylindrical shell 3 is a cylindrical shell. The end walls 6, 7 are joined to each axial end 4, 5 by means of at least one circumferential weld 8. A single weld may be applied from the inside of the shell or, more preferably, from the outside of the shell. If two welds are used, the first weld may be applied from the outside of the shell and the second weld may be applied from the inside of the shell, or, alternatively, the first weld may be applied from the inside of the shell and the second weld may be applied from the outside of the shell. The shell may be joined to the end wall in a manner such as disclosed in patent documents EP2920360B1 or EP2126203B1. The end wall may optionally be provided with a thermal insulation portion, such as disclosed in patent documents EP2475819B1 or WO2016 / 026662A1. As Figure 2 As shown, the cylindrical housing 3 has an outer surface 9 and an inner surface 10. Figure 2 Preferably, a circumferential groove 11 is formed in the inner surface 10 of the cylindrical housing 3. In the groove 11, condensed water will accumulate during operation, and the Yankee dryer 2 is preferably provided with means for draining condensed water from the groove 11, for example, as disclosed in US Pat. No. 5,090,135 or EP 2 614 182 B1.

[0022] Further references Figure 3 The Yankee dryer 2 of the present invention is used in a tissue paper machine 1. When the Yankee dryer is used in the machine 1, a creping doctor 12 is used. The creping doctor 12 has a creping blade 13 which is arranged to act on the outer surface 9 of the housing 3 of the Yankee dryer 2. Figure 3 In the figure, the Yankee dryer is shown as being along the direction of arrow R, i.e. Figure 3 In the "clockwise" direction, it rotates around its rotation axis A. Figure 3 It can be understood that the housing has a cylindrical shape. The Yankee dryer is arranged in a tissue paper machine so that it can rotate about an axis of rotation A.

[0023] like Figure 3As shown, a fiber web W (shown schematically and incompletely in dashed and solid lines) is formed in the forming section 17 between a forming fabric 18 and a fabric 24, which may be a water-absorbing felt. The fiber web W is formed by the slurry injected from the headbox 19. The newly formed fiber web W is carried on the felt 24 to the nip N between the press roll 21 and the Yankee dryer 2. The press roll 21 used in the nip for the Yankee dryer may be, for example, a shoe roll of the design disclosed in U.S. Pat. No. 7,527,708, U.S. Pat. No. 9,885,153 or EP 2 085 513 B1, but other rolls than shoe rolls may also be considered. The wet fiber web W may be subjected to a certain degree of dewatering in the nip N, which is then used as a dewatering press nip. The nip N may also be essentially just a transfer nip in which essentially no dewatering occurs. The nip N may optionally be before the suction turning roll 20. The fibrous web W is transferred onto the heated outer surface 9 of the cylindrical shell 3 of the Yankee dryer 2, and then the fibrous web W is dried by heat from hot steam supplied into the Yankee dryer 3. Subsequently, the dried fibrous web W is creped from the Yankee dryer by a doctor blade 12 and sent to a reel 25.

[0024] During operation, the tissue machine may be run at a speed in the range of 1200 m / min-2000 m / min. However, higher speeds are also contemplated, and machine speeds in the range of 2000 m / min-2300 m / min may also be used, or even speeds of up to 2400 m / min may be used. In all embodiments of the invention, the diameter of the Yankee dryer may be in the range of, for example, 2 m to more than 7 m. Some diameters are more common than others, such as 3.5 m, 3.66 m, 4.88 m or 5.5 m. The width of the Yankee dryer 2 may be in the range of, for example, 0.6 m for a pilot machine up to more than 7 m. For example, the width may be 3 m or 5 m. However, the Yankee dryer may also have other dimensions than those described above.

[0025] Reference Figure 4 The doctor blade 12 preferably comprises a blade holder 23 holding the creping blade 13. During operation, the creping blade 13 will act on the outer surface 9 of the housing 3 to crepe the dried fiber web from the outer surface 9.

[0026] Reference Figure 5 , the tissue paper machine can be provided with a Yankee dryer hood 16, which is arranged to be able to blow hot air onto the outer surface 10 of the cylindrical shell 3 over a portion of the circumference of the cylindrical shell 3. The Yankee dryer hood can be, for example, a Yankee dryer hood disclosed in patent document EP2963176B1, but other Yankee dryer hoods can also be considered, and the machine of the present invention can also be operated without a Yankee dryer hood. Figure 5 A further scraper 12' is shown in . This further scraper is optional and may be a cleaning scraper for scraping off fiber residues from the Yankee dryer.

[0027] The tissue paper machine preferably also includes a device 14 for applying a liquid coating to the outer surface 9 of the Yankee dryer 2. The liquid coating generally includes polyvinyl alcohol and other chemical reagents. The applied coating may include, for example, 50-65 weight percent polyvinyl alcohol (PVOH), 15-30 weight percent adhesive constituting the coating, 5-30 weight percent modifier / release agent constituting the coating, and preferably also includes phosphate. The phosphate used for this coating may be, for example, monoammonium phosphate, diammonium phosphate, trisodium phosphate or tetraphosphate. Instead of the above-mentioned phosphate (or with one or more combinations thereof), phosphoric acid may be used in the coating. The supply system for supplying the liquid coating is symbolically represented by reference numeral 26.

[0028] During operation, the creping doctor 12 can act on the outer surface 9 of the cylindrical housing 3 with a linear load, which can be as high as 10 kN / m in some cases. This means that the cylindrical housing 3 is subject to wear. For Yankee dryers made of steel, this can be a very serious problem, and it is already standard procedure to provide them with a protective layer, a so-called "metallization layer" of a hard material resistant to coating. However, cracks can appear in such a hard layer, which can quickly lead to delamination of the entire layer, making it necessary to interrupt the operation of the machine. In addition, the doctor blade can be damaged due to cracks and delamination. When a crack catches the doctor blade, the doctor blade can be deformed, which can be the source of streaks in the paper. Therefore, from a process point of view, it is actually desirable to eliminate the metallization layer.

[0029] The inventors of the present invention have now discovered that by manufacturing the cylindrical outer shell 3 using steel of grade P690 or similar steel having the composition and properties as described below, such that the outer surface of the outer shell 3 is formed of steel of grade P690 or similar steel, the use of a hard metallized layer can be avoided entirely. In a first embodiment of the invention, the cylindrical outer shell is formed of steel of grade P690 or similar steel. In a second embodiment of the invention, the cylindrical outer shell is formed of an inner cylindrical outer shell made of steel and covered with a continuous outer layer of steel of grade P690 or similar steel. Such a continuous outer layer of steel of grade P690 or similar steel may consist of an annular or spiral strip of steel of grade P690 or similar steel, which is welded to the underlying steel shell, for example, by its edges and / or by through holes drilled through the strip. Alternatively, the continuous outer layer of steel of grade P690 or similar steel may be formed of a plurality of plates of steel of grade P690 or similar steel, which are welded to the inner cylindrical outer shell by their edges and / or by through holes drilled through the plates.

[0030] The hardness of the outer surface of P690 grade steel or similar steel is preferably equal to or greater than 770 MPa and equal to or less than 940 MPa.

[0031] In each embodiment, the surface on which the doctor blade 13 acts will be formed from steel of grade P690 or similar steel. This is possible without laser hardening as proposed in patent document AT519996A2. It has been found that the wear resistance of grade P690 is so high that it does not require any metallization layer and similar steels will have the same wear resistance. In addition, it has the properties required for Yankee dryers in terms of welding, strength and heat transfer.

[0032] The P690 steel grade or similar steel used in the present invention has the following composition in weight percentage:

[0033] C is equal to or greater than 0.12% and equal to or less than 0.20%

[0034] Si is equal to or more than 0.10% and equal to or less than 0.80%

[0035] Mn is equal to or more than 1.00% and equal to or less than 1.70%

[0036] Cr is equal to or more than 0.10% and equal to or less than 1.50%

[0037] Mo is equal to or more than 0.30% and equal to or less than 0.70%

[0038] V is equal to or greater than 0.005% and equal to or less than 0.12%

[0039] Nb is equal to or more than 0.005% and equal to or less than 0.060%

[0040] B is equal to or greater than 0.0006% and equal to or less than 0.005%

[0041] P is equal to or less than 0.025%

[0042] S is equal to or less than 0.010%

[0043] N is equal to or less than 0.015%

[0044] Cu is equal to or less than 0.30%

[0045] Ni is equal to or less than 2.50%

[0046] Ti is equal to or less than 0.05%

[0047] Zr is equal to or less than 0.15%

[0048] Al is equal to or less than 0.01%

[0049] The remainder is iron and impurities.

[0050] Preferably, in P690 grade steel or similar steel, the weight percentage of Nb, Ti, V, Zr is equal to or greater than 0.015%.

[0051] Optionally, if aluminum is present, the sum of V, Ti, Nb and Al is equal to or greater than 0.02%

[0052] Preferably, for products made of P690 grade steel or similar steel with a maximum thickness equal to or less than 50 mm, the upper yield strength (ReH) of P690 measured by ISO 6892-1:2019 is equal to or greater than 690 MPa, and the corresponding tensile strength measured by ISO6892-1:2019 is preferably equal to or greater than 770 MPa and equal to or less than 940 MPa.

[0053] Preferably, for products made of P690 grade steel with a thickness greater than 50 mm and a thickness equal to or less than 100 mm, the yield strength of P690 measured by ISO 6892-1:2019 is equal to or greater than 670 MPa, and the corresponding tensile strength measured by ISO 6892-1:2019 is preferably equal to or greater than 770 MPa and equal to or less than 940 MPa.

[0054] Preferably, for products with a thickness greater than 100 mm made of P690 grade steel, the yield strength of P690 measured by ISO 6892-1:2019 is equal to or greater than 630 MPa, and the corresponding tensile strength measured by ISO 6892-1:2019 is preferably equal to or greater than 770 MPa and equal to or less than 940 MPa.

[0055] Thanks to the invention, the risk of having to shut down the machine due to damage to the drying surface of the Yankee dryer is significantly reduced.

Claims

1. A steel Yankee dryer (2) comprising a cylindrical housing (3) having two axial ends (4, 5); an end wall (6, 7) joined to each axial end (4, 5) by means of a circumferential weld (8), the cylindrical housing (3) also having an outer surface (9) and an inner surface (10), characterized in that The outer surface (9) of the cylindrical housing (3) is formed of steel of grade P690 as defined in European standard EN 10028-6:2017 or of a steel having the following weight composition: C is equal to or greater than 0.12% and equal to or less than 0.20%, Si is equal to or greater than 0.10% and equal to or less than 0.80%, Mn is equal to or greater than 1.00% and equal to or less than 1.70%, Cr is equal to or greater than 0.10% and equal to or less than 1.50%, Mo is equal to or greater than 0.30% and equal to or less than 0.70%, V is equal to or greater than 0.005% and equal to or less than 0.12%, Nb is equal to or greater than 0.005% and equal to or less than 0.060%, B is equal to or greater than 0.0006% and equal to or less than 0.005%, P is equal to or less than 0.025%, S is equal to or less than 0.010%, N is equal to or less than 0.015%, Cu is equal to or less than 0.30%, Ni is equal to or less than 2.50%, Ti is equal to or less than 0.05%, Zr is equal to or less than 0.15%, Al is equal to or less than 0.01%, The remainder is iron and impurities; For products made of P690 grade steel or steel of the above weight composition with a maximum thickness equal to or less than 50 mm, the upper yield strength measured by ISO 6892-1:2019 is equal to or greater than 690 MPa, and the corresponding tensile strength measured by ISO 6892-1:2019 is equal to or greater than 770 MPa and equal to or less than 940 MPa, For products made of P690 grade steel or steel of the above weight composition with a thickness greater than 50 mm and a thickness equal to or less than 100 mm, the upper yield strength measured by ISO 6892-1:2019 is equal to or greater than 670 MPa, and the corresponding tensile strength measured by ISO6892-1:2019 is equal to or greater than 770 MPa and equal to or less than 940 MPa, For products made of P690 grade steel or steel of the above weight composition with a thickness greater than 100 mm, the upper yield strength measured by ISO 6892-1:2019 is equal to or greater than 630 MPa, and the corresponding tensile strength measured by ISO 6892-1:2019 is equal to or greater than 770 MPa and equal to or less than 940 MPa.

2. The steel Yankee dryer according to claim 1, characterized in that: The cylindrical housing (3) is made of P690 grade steel or a steel having the following weight composition: C is equal to or greater than 0.12% and equal to or less than 0.20%, Si is equal to or greater than 0.10% and equal to or less than 0.80%, Mn is equal to or greater than 1.00% and equal to or less than 1.70%, Cr is equal to or greater than 0.10% and equal to or less than 1.50%, Mo is equal to or greater than 0.30% and equal to or less than 0.70%, V is equal to or greater than 0.005% and equal to or less than 0.12%, Nb is equal to or greater than 0.005% and equal to or less than 0.060%, B is equal to or greater than 0.0006% and equal to or less than 0.005%, P is equal to or less than 0.025%, S is equal to or less than 0.010%, N is equal to or less than 0.015%, Cu is equal to or less than 0.30%, Ni is equal to or less than 2.50%, Ti is equal to or less than 0.05%, Zr is equal to or less than 0.15%, Al is equal to or less than 0.01%, The remainder is iron and impurities.

3. The steel Yankee dryer according to claim 1 or 2, characterized in that: The sum of weight percentages of Nb, Ti, V and Zr in the steel is equal to or greater than 0.015%.

4. The steel Yankee dryer according to claim 1 or 2, characterized in that: The sum of weight percentages of V, Ti, Nb and Al in the steel is equal to or greater than 0.02%.

5. A tissue papermaking machine (1) comprising a steel Yankee dryer (2) according to any one of claims 1 to 4 and a corrugating doctor (12) having a corrugating blade (13), the corrugating blade being arranged to act on the outer surface (9) of the Yankee dryer (2).

6. The household papermaking machine (1) according to claim 5, wherein: The papermaking machine (1) further comprises means (14) for applying a liquid coating to the outer surface (9) of the Yankee dryer (2).

7. The household papermaking machine (1) according to claim 5 or 6, wherein: The papermaking machine further comprises a Yankee dryer hood (16) arranged to be able to blow hot air onto the outer surface (9) of the cylindrical shell (3) over a portion of the circumference of the cylindrical shell (3).

8. A cylindrical housing (3) for a steel Yankee dryer, characterized in that The cylindrical housing comprises an outer surface (9) made of P690 grade steel as defined in European Standard EN 10028-6:2017 or a steel having the following weight composition: C is equal to or greater than 0.12% and equal to or less than 0.20%, Si is equal to or greater than 0.10% and equal to or less than 0.80%, Mn is equal to or greater than 1.00% and equal to or less than 1.70%, Cr is equal to or greater than 0.10% and equal to or less than 1.50%, Mo is equal to or greater than 0.30% and equal to or less than 0.70%, V is equal to or greater than 0.005% and equal to or less than 0.12%, Nb is equal to or greater than 0.005% and equal to or less than 0.060%, B is equal to or greater than 0.0006% and equal to or less than 0.005%, P is equal to or less than 0.025%, S is equal to or less than 0.010%, N is equal to or less than 0.015%, Cu is equal to or less than 0.30%, Ni is equal to or less than 2.50%, Ti is equal to or less than 0.05%, Zr is equal to or less than 0.15%, Al is equal to or less than 0.01%, The remainder is iron and impurities; For products made of P690 grade steel or steel of the above weight composition with a maximum thickness equal to or less than 50 mm, the upper yield strength measured by ISO 6892-1:2019 is equal to or greater than 690 MPa, and the corresponding tensile strength measured by ISO 6892-1:2019 is equal to or greater than 770 MPa and equal to or less than 940 MPa, For products made of P690 grade steel or steel of the above weight composition with a thickness greater than 50 mm and a thickness equal to or less than 100 mm, the upper yield strength measured by ISO 6892-1:2019 is equal to or greater than 670 MPa, and the corresponding tensile strength measured by ISO6892-1:2019 is equal to or greater than 770 MPa and equal to or less than 940 MPa, For products made of P690 grade steel or steel of the above weight composition with a thickness greater than 100 mm, the upper yield strength measured by ISO 6892-1:2019 is equal to or greater than 630 MPa, and the corresponding tensile strength measured by ISO 6892-1:2019 is equal to or greater than 770 MPa and equal to or less than 940 MPa.

9. The cylindrical housing (3) for a steel Yankee dryer according to claim 8, characterized in that The cylindrical shell is made of P690 grade steel or steel having the following weight composition composition: C is equal to or greater than 0.12% and equal to or less than 0.20%, Si is equal to or greater than 0.10% and equal to or less than 0.80%, Mn is equal to or greater than 1.00% and equal to or less than 1.70%, Cr is equal to or greater than 0.10% and equal to or less than 1.50%, Mo is equal to or greater than 0.30% and equal to or less than 0.70%, V is equal to or greater than 0.005% and equal to or less than 0.12%, Nb is equal to or greater than 0.005% and equal to or less than 0.060%, B is equal to or greater than 0.0006% and equal to or less than 0.005%, P is equal to or less than 0.025%, S is equal to or less than 0.010%, N is equal to or less than 0.015%, Cu is equal to or less than 0.30%, Ni is equal to or less than 2.50%, Ti is equal to or less than 0.05%, Zr is equal to or less than 0.15%, Al is equal to or less than 0.01%, The remainder is iron and impurities.

10. The cylindrical housing for a steel Yankee dryer according to claim 8 or 9, characterized in that The sum of weight percentages of Nb, Ti, V and Zr in the steel is equal to or greater than 0.015%.

11. The cylindrical shell for a steel Yankee dryer according to claim 8 or 9, characterized in that The sum of weight percentages of V, Ti, Nb and Al in the steel is equal to or greater than 0.02%.

Citation Information

Patent Citations

  • method of surface treatment of a steel yankee

    AT519996A2

  • Pressing unit

    EP2085513B1

  • Yankee cylinder for a paper producing machine

    EP2126203B1

  • Thermally insulated yankee cylinder

    EP2475819B1

  • Steam-heated drying cylinder

    EP2614182B1