A method for quantitatively characterizing yield stress using heavy oil components

By separating and measuring the contents of the four components in heavy oil, and using multiple regression relationships to calculate the yield stress, the problem of difficulty in characterizing the yield stress of heavy oil in the existing technology is solved, quantitative characterization of heavy oil properties is achieved, and the measurement flow is simplified. The process of changing the curve.

CN116429636BActive Publication Date: 2024-10-11YANGTZE UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310147658.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-02-20
Publication Date
2024-10-11
Estimated Expiration
2043-02-20

AI Technical Summary

Technical Problem

It is difficult to effectively characterize the yield stress of heavy oil with existing technology, mainly due to the difficulty in measuring the yield stress due to the strength of the three-dimensional network structure within the heavy oil colloid system.

Method used

By separating and measuring the relative contents of four components (saturated hydrocarbons, aromatic hydrocarbons, colloids and asphaltenes) in heavy oil, and using multiple regression relationships to calculate the yield stress, we provide an indirect method to obtain the yield stress and simplify the rheology Curve measurement process.

Benefits of technology

The quantitative characterization of the yield stress of heavy oil was achieved. Through multiple regression on the relationship between component content and temperature, the yield stress component formula was obtained. The complex correlation coefficient reached 0.9076, which has good linear correlation and heavy oil performance characterization significance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116429636B_ABST
    Figure CN116429636B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for quantitatively characterizing yield stress using heavy oil components, comprising the following steps: separating and obtaining four components in the original heavy oil, respectively adding the four components to the original heavy oil to obtain a composite heavy oil; separating and determining the relative contents of the four components in the composite heavy oil; determining the rheological curve of the composite heavy oil and obtaining the yield stress; performing multivariate regression on the relative contents, temperature and yield stress of the four components in the composite heavy oil to obtain a yield stress component relationship; using the yield stress component relationship, obtaining the yield stress value corresponding to the heavy oil to be measured. Through the method of the present invention, the component content can be directly measured and then the yield stress can be calculated. This indirect method for obtaining the yield stress eliminates the relatively complex process of measuring the rheological curve; and the complex correlation coefficient in the empirical formula obtained by the present invention reaches 0.9076, and the linear correlation degree is close, which has a good reference significance for the characterization of heavy oil performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of heavy oil component characterization, and in particular to a method for quantitatively characterizing yield stress using heavy oil components. Background Art

[0002] Yield stress is an important parameter to describe the rheological properties of fluids, and is mainly an indicator of the elastic strength of fluids. When a fluid is under shear stress, as the shear stress increases, the fluid changes from a creeping state of plastic deformation to a flowing state of continuous deformation. The critical value of shear stress corresponding to the change from creeping to flowing is called yield stress. The main reason for the existence of yield stress is that it is determined by the strength of the molecular structure inside the fluid system. For heavy oil colloid systems, due to macromolecular substances such as wax crystals, colloids, and asphaltene, the molecules inside the system form a three-dimensional network structure. The strength of this structure is very strong. Only when this three-dimensional network structure is destroyed by external forces, the heavy oil colloid system will flow. Therefore, the yield stress of heavy oil is usually difficult to characterize.

[0003] In addition, the yield stress is related to the fluid structural strength and the dynamic characteristics of the fluid after being stressed. Therefore, it is desirable to obtain a method for quantitatively characterizing the yield stress using heavy oil components, which is of great significance for the characterization of heavy oil properties. Summary of the invention

[0004] The purpose of the present invention is to overcome the above technical deficiencies, provide a method for quantitatively characterizing yield stress using heavy oil components, and solve the technical problem that the yield stress of heavy oil is difficult to characterize in the prior art.

[0005] In order to achieve the above technical objectives, the technical solution of the present invention provides a method for quantitatively characterizing yield stress using heavy oil components:

[0006] The following steps are involved:

[0007] S1, separating and obtaining four components in the original heavy oil, and respectively adding the four components to the original heavy oil to obtain a composite heavy oil;

[0008] S2. Separating and determining the relative contents of the four components in the compound heavy oil; determining the rheological curve of the compound heavy oil and obtaining the yield stress;

[0009] S3, performing multivariate regression on the relative contents, temperature and yield stress of the four components in the composite heavy oil to obtain the yield stress component relationship;

[0010] S4, using the yield stress component relationship, obtaining a yield stress value corresponding to the heavy oil to be tested.

[0011] Furthermore, the four components are saturated hydrocarbons, aromatic hydrocarbons, resins and asphaltenes.

[0012] Furthermore, the separation in step S1 and step S2 both adopts a four-component separation method.

[0013] Furthermore, the specific steps of the four-component separation method include:

[0014] (1) Using n-heptane to treat the original heavy oil or the compounded heavy oil to separate asphaltene and soluble matter;

[0015] (2) The soluble substances are separated by an activated Al2O3 adsorption chromatographic column. Saturated hydrocarbons are obtained by washing with n-heptane, aromatic hydrocarbons are obtained by washing with benzene, and colloids are obtained by washing with benzene-ethanol.

[0016] Furthermore, in step S2, the relative contents of the four components in the composite heavy oil are obtained by drying and weighing after separation.

[0017] Furthermore, the yield stress component relationship includes the empirical formula:

[0018] lnτ=1687.01*Sa+1687.10*Ar+1688.08*Rs+1688.79*As-0.6541*T-168698.3

[0019] Wherein, τ is the yield stress; Sa is the saturated hydrocarbon content, %; Ar is the aromatic hydrocarbon content, %; Rs is the colloid content, %; As is the asphaltene content, %; T is the temperature, ℃.

[0020] Furthermore, in step S1, during the preparation of the compounded heavy oil, the addition amount of the four components is 2-20% of the mass of the original heavy oil.

[0021] Furthermore, in step S2, a rheometer is used to measure the rheological curve of the compounded heavy oil at room temperature to 70°C.

[0022] Furthermore, in step S3, multiple regression is performed using matlab software.

[0023] Compared with the prior art, the beneficial effects of the present invention include:

[0024] The present invention studies the relationship between component content, temperature and yield stress, and then performs multiple regression on the relationship between yield stress, component and temperature, quantitatively characterizes the relationship between heavy oil components and yield stress, and substitutes component and temperature data of different oil fields into the characterization relationship to calculate the yield stress. Through the method of the present invention, the component content can be directly measured and then the yield stress can be calculated. This method of indirectly obtaining the yield stress eliminates the relatively complex process of measuring the rheological curve; and the complex correlation coefficient in the empirical formula obtained by the present invention reaches 0.9076, the linear correlation degree is close, and it has good reference significance for the characterization of heavy oil performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a flowchart of the present invention;

[0026] Figure 2 It is a four-component separation flow chart of the present invention;

[0027] Figure 3 is the relationship curve between saturated hydrocarbon content and yield stress at different temperatures of the present invention;

[0028] Figure 4 is the relationship curve between aromatic hydrocarbon content and yield stress;

[0029] Figure 5 It is the relationship curve between colloid content and yield stress;

[0030] Figure 6 It is a graph showing the relationship between asphaltene content and yield stress;

[0031] Figure 7 These are the calculated values ​​and measured values ​​of the component formula of the present invention. DETAILED DESCRIPTION

[0032] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0033] The yield stress value can be measured directly by a rheometer, but the rheometer itself is expensive and easily restricted by the site. In comparison, the determination of the heavy oil components can be directly separated by the four-component separation method and then obtained by weighing, which is a simple step.

[0034] Based on this, the present invention provides a method for quantitatively characterizing yield stress using heavy oil components, which mainly studies the relationship between the yield value of heavy oil and viscosity, components, and temperature. Since there are many methods for obtaining the yield stress value, and the yield stress values ​​obtained by each method are very different, the yield stress value in the present invention is mainly obtained by fitting and regression using the Bingham rheological equation. The characterization formula for yield stress is obtained by multi-factor regression based on the regression fitting result of the Bingham rheological equation to ensure the linear correlation of the final formula.

[0035] See also Figure 1 , the method of the present invention comprises the following steps:

[0036] S1. Using a four-component separation method to obtain four components of saturated hydrocarbons, aromatic hydrocarbons, colloids and asphaltene in the original heavy oil, the four components are added to the original heavy oil in a certain proportion to obtain a composite heavy oil;

[0037] S2. Separating and determining the relative contents of four components in the compound heavy oil by a four-component separation method; determining the rheological curve of the compound heavy oil, and obtaining the yield stress from the rheological curve;

[0038] S3, performing multiple regression on the relative content, temperature and yield stress of the four components in the compound heavy oil to obtain the yield stress component relationship formula;

[0039] S4, using the yield stress component relationship, obtaining a yield stress value corresponding to the heavy oil to be tested.

[0040] Preferably, the four-component separation method of the original heavy oil in step S1 and the four-component separation method of the composite heavy oil in step S2 both adopt the four-component separation method of the chromatographic column, and the reference standard is NB / SH / T 0509-2010 petroleum asphalt four-component determination method; and in step S2, the relative contents of saturated hydrocarbons, aromatic hydrocarbons, colloids and asphaltene in the heavy oil are obtained by drying and weighing after separation, such as Figure 2 As shown, the specific steps include:

[0041] (1) Using n-heptane to treat heavy oil to separate asphaltene (insoluble matter) and soluble matter (filtrate);

[0042] (2) Soluble substances are separated by an activated Al2O3 adsorption column, washed with n-heptane to obtain saturated hydrocarbons, washed with benzene to obtain aromatic hydrocarbons, and washed with benzene-ethanol to obtain colloids;

[0043] (3) The collected components are subjected to solvent distillation, dried, weighed, and the content is calculated.

[0044] Preferably, in step S1, the added amount of each component in the composite heavy oil is 2-20% of the mass of the original heavy oil; more preferably, 5-20%.

[0045] Preferably, in step S2, a rheometer is used to measure the rheological curve of the compounded heavy oil at room temperature to 70°C.

[0046] Preferably, in step S3, multiple regression is performed using matlab software.

[0047] The present invention is further described in detail below through specific examples.

[0048] The experimental instruments mainly used in the embodiments of the present invention are:

[0049] Rheometer: MCR301 Anton Paar rheometer.

[0050] Example 1

[0051] S1. After separating the heavy oil from oil field A by using a four-component separation method using a chromatographic column, the heavy oil was re-compounded according to the different component ratios shown in Table 1. During compounding, each component was added incrementally to obtain 13 different component compounded heavy oil samples, which were numbered 1# to 13# oil samples.

[0052] The addition of saturated hydrocarbons, aromatic hydrocarbons, colloids and asphaltene is shown in Table 1.

[0053] S2. The relative contents of the four components of the compounded oil samples 1# to 13# were measured, and the measurement results are shown in Table 2. In addition, the oil samples 14# to 17# in Table 2 are from other oil fields in China that are different from the A oil field, and are mainly used to verify the applicability of the yield stress calculation formula.

[0054] The rheological curves of the heavy oil samples were measured at room temperature to 70°C using a rheometer, and the yield stress of each compounded heavy oil sample was obtained from the rheological curves.

[0055] Table 1 Source information of experimental heavy oil samples

[0056]

[0057]

[0058] Table 2 Four components of compound samples

[0059]

[0060] As can be seen from Table 2, after adding different pure components, molecular interactions will occur, which will in turn affect the content of the components. Therefore, it is uncertain whether other components will decrease or increase after adding the components. Therefore, the content of each component needs to be re-measured, and cannot be calculated based on the actual amount added.

[0061] S3. Effect of heavy oil components on yield stress

[0062] Firstly, the influence relationship between the four components of heavy oil and yield stress was studied. Matlab software was used to perform multivariate regression on heavy oil saturated hydrocarbons, aromatic hydrocarbons, colloids, asphaltene, temperature and yield stress, and the relevant empirical formula was obtained and analyzed.

[0063] 301. Effect of heavy oil components on yield stress

[0064] (1) Effect of saturated hydrocarbons on yield stress

[0065] Figure 3 It is a curve showing the relationship between saturated hydrocarbon content and yield stress at different temperatures, where the vertical axis is plotted in a semi-logarithmic coordinate.

[0066] pass Figure 3It can be seen from the experimental results that with the increase of saturated hydrocarbon content, the yield stress gradually decreases. This is mainly because saturated hydrocarbons have a solvating effect, which reduces the interaction force between heavy oil macromolecules and weakens the strength of the three-dimensional spatial network structure, thus leading to a decrease in yield stress.

[0067] (2) Effect of aromatic hydrocarbons on yield stress

[0068] Figure 4 This is the relationship curve between the aromatic hydrocarbon content and the yield stress at different temperatures, where the vertical axis is plotted in a semi-logarithmic coordinate.

[0069] pass Figure 4 It can be seen from the experimental results that with the increase of aromatic hydrocarbon content, the yield stress shows an overall trend of increasing first and then gradually decreasing. This is mainly because in the early stage of the gradual increase of aromatic hydrocarbon content, the dipole-dipole effect between aromatic hydrocarbons and colloids is dominant, which weakens the interaction force (dispersion effect) between aromatic hydrocarbons and asphaltene, thus causing asphaltene aggregation. The formation of macromolecules will increase the strength of the three-dimensional network structure. With the continuous increase of aromatic hydrocarbon content, the dispersion effect of aromatic hydrocarbons gradually strengthens, reducing the interaction force between heavy oil macromolecules, weakening the strength of the three-dimensional network structure, and thus reducing the yield stress.

[0070] (3) Effect of colloid on yield stress

[0071] Figure 5 It is the relationship curve between colloid content and yield stress at different temperatures, where the vertical axis is plotted in semi-logarithmic coordinates.

[0072] pass Figure 5 It can be seen from the experimental results that with the increase of gum content, the overall trend of yield stress gradually increases. This is mainly due to the charge transfer, hydrogen bonding and dipole effects between gum and asphaltene molecules. Under the influence of these effects, asphaltene forms larger aggregates under the wrapping of gum. At this time, the strength of the three-dimensional spatial network structure of the molecules is enhanced, which leads to an increase in yield stress.

[0073] (4) Effect of asphaltene on yield stress

[0074] Figure 6 This is the relationship curve between asphaltene content and yield stress at different temperatures, where the vertical axis is plotted in a semi-logarithmic coordinate.

[0075] pass Figure 6The experimental results show that with the increase of asphaltene content, the yield stress first decreases and then increases. The decrease in yield stress caused by asphaltene is mainly due to the fact that the asphaltene entering the colloid system first combines with the colloid outside the micelle to form aggregates, breaking up the associations formed by the colloid asphaltene micelles. At this time, the strength of the three-dimensional network structure is weakened and the yield stress decreases. When the asphaltene content continues to increase, the asphaltene molecules have an association effect, resulting in the formation of aggregates with larger molecular weight and stronger structural strength. Therefore, the structural mechanical properties of the heavy oil are stronger and the yield stress increases.

[0076] 302. Quantitative characterization of yield stress, composition and temperature

[0077] The relationship between different components and yield stress was analyzed by multivariate regression using MATLAB software, and the empirical formula for calculating yield stress using components and temperature and the complex correlation coefficient were obtained as shown below.

[0078] lnτ=1687.01*Sa+1687.10*Ar+1688.08*Rs+1688.79*As-0.6541*T-168698.37(1)

[0079] Among them, the complex correlation coefficient is: 0.9076 (the calculated value is the horizontal axis, the experimental value is the vertical axis, and the curve is drawn by linear fitting). The complex correlation coefficient obtained by the present invention is large, indicating that the linear correlation between the elements or variables of formula (1) is close.

[0080] Where: τ is the yield stress;

[0081] Sa is the saturated hydrocarbon content, %;

[0082] Ar is the aromatic hydrocarbon content, %;

[0083] Rs is the colloid content, %;

[0084] As is asphaltene content, %;

[0085] T is temperature, °C.

[0086] 303. Verification of Yield Stress Component Formula

[0087] The calculation results were verified using the above 14#~17# heavy oil samples. The viscosity of the heavy oil at different temperatures was directly measured by a viscometer. The calculation results using the component formula were compared with the actual yield stress results as follows: Figure 7 shown.

[0088] See also Figure 7According to the calculation results of the above component formula, it can be seen that the average deviation of the yield stress component formula calculation results is 32.45%. This is mainly due to the limitation of the number of heavy oil samples in the fitting process of the yield stress component calculation formula, resulting in a large deviation. However, the present invention provides a new quantitative characterization method, which can indirectly obtain the yield stress by determining the component content, and has a good reference significance for the characterization of heavy oil performance. In the future, more heavy oil samples from different oil fields can be expanded to update the database in real time to improve the empirical formula and enhance universality.

[0089] The present invention first studies the relationship between components, temperature and yield stress, and then uses matlab software to perform multiple regression on the relationship between yield stress, components and temperature to obtain formula (1), that is, the relationship formula (1) between different component values, temperature values ​​and yield stress; then, the component and temperature data of different oil fields are substituted into formula (1) to calculate the yield stress. The present invention can directly calculate the yield stress by measuring the component content, eliminating the process of measuring the rheological curve.

[0090] The specific implementation of the present invention described above does not constitute a limitation on the protection scope of the present invention. Any other corresponding changes and modifications made based on the technical concept of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. A method for quantitatively characterizing yield stress using heavy oil components, characterized in that: The following steps are involved: S1. Separating and obtaining four components from the original heavy oil, and adding the four components to the original heavy oil to obtain a composite heavy oil; the four components are saturated hydrocarbons, aromatic hydrocarbons, colloids and asphaltene; S2. Separating and determining the relative contents of the four components in the compound heavy oil; determining the rheological curve of the compound heavy oil and obtaining the yield stress; S3, performing multivariate regression on the relative contents, temperature and yield stress of the four components in the composite heavy oil to obtain the yield stress component relationship; S4, using the yield stress component relationship, obtaining a yield stress value corresponding to the heavy oil to be tested.

2. The method for quantitatively characterizing yield stress using heavy oil components according to claim 1, characterized in that: The separation in both step S1 and step S2 adopts a four-component separation method.

3. The method for quantitatively characterizing yield stress using heavy oil components according to claim 2, characterized in that: The specific steps of the four-component separation method include: (1) Using n-heptane to treat the original heavy oil or compound heavy oil to separate asphaltene and soluble matter; (2) The soluble substances are separated by an activated Al2O3 adsorption chromatographic column. Saturated hydrocarbons are obtained by washing with n-heptane, aromatic hydrocarbons are obtained by washing with benzene, and colloids are obtained by washing with benzene-ethanol.

4. The method for quantitatively characterizing yield stress using heavy oil components according to claim 1, characterized in that: In step S2, the relative contents of the four components in the composite heavy oil are obtained by drying and weighing after separation.

5. The method for quantitatively characterizing yield stress using heavy oil components according to claim 1, characterized in that: The yield stress component relationship includes the empirical formula: in, is the yield stress; Sa is the saturated hydrocarbon content, %; Ar is the aromatic hydrocarbon content, %; Rs is the resin content, %; As is the asphaltene content, %; and T is the temperature, ℃.

6. The method for quantitatively characterizing yield stress using heavy oil components according to claim 1, characterized in that: In step S1, during the preparation of the composite heavy oil, the addition amount of the four components is 2-20% of the mass of the original heavy oil.

7. The method for quantitatively characterizing yield stress using heavy oil components according to claim 1, characterized in that: In step S2, a rheometer is used to measure the rheological curve of the compounded heavy oil at room temperature to 70°C.