Heterojunction battery and preparation method thereof
By forming a patterned mask on the second surface of the semiconductor substrate layer of the heterojunction battery and making a fleece treatment, the problems of high breakage rate and poor slurry adhesion are solved, and the photoelectric conversion efficiency and reliability are improved.
Patent Information
- Application Number
- CN202310512826.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-08
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2043-05-08
AI Technical Summary
In the existing heterojunction battery preparation process, the high crushing rate of the semiconductor substrate layer leads to low photoelectric conversion efficiency, and poor slurry adhesion leads to poor reliability.
By forming a patterned mask on the second surface of the semiconductor substrate layer and fleece-making treatment is performed on the area where it is not covered by the mask, a structure of comprehensive suede and partial suede is formed, and the flatness is maintained after removing the mask, thereby reducing the thickness of the mask. Crush rate and improve adhesion.
The photoelectric conversion efficiency and battery reliability are improved, the crushing rate of the semiconductor substrate layer is reduced, and the passivation effect and slurry adhesion of the amorphous silicon layer are enhanced.
Smart Images

Figure CN116504877B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of solar cell preparation, and in particular to a heterojunction cell and a preparation method thereof. Background Art
[0002] Against the backdrop of global energy transition and dual-carbon goals, the photovoltaic industry is booming. Heterojunction solar cells have attracted widespread attention due to their advantages such as short manufacturing process, high theoretical efficiency, low-temperature manufacturing, and thin-film fabrication, and are currently one of the key research areas for high-efficiency silicon-based solar cells. Heterojunction solar cells are generally fabricated using N-type monocrystalline silicon wafers with a textured surface and a double-sided pyramid structure. However, the textured surface on the back side can cause uneven deposition of the subsequent amorphous silicon passivation layer, affecting the passivation effect. Furthermore, the textured surface on the back side is not conducive to secondary reflection and absorption of incident light, thus requiring good flatness on the back side. However, with the development of silicon wafer slicing technology, silicon wafers are becoming thinner, which reduces raw material costs, but also increases the processing difficulty.
[0003] Currently, back polishing is a commonly used process in semiconductor substrate fabrication. However, due to the thinning of the semiconductor substrate, the breakage rate increases during back polishing, affecting the photoelectric conversion efficiency of heterojunction solar cells. Secondly, in the fabrication of heterojunction solar cells, the flatness of the back side of the semiconductor substrate, which uses low-temperature silver paste for screen printing, is closely related to the adhesion between the paste and the substrate. Better flatness results in poor paste adhesion, leading to poor contact between the paste and the semiconductor substrate, causing some gate lines to detach and reducing the reliability of the heterojunction solar cell.
[0004] Therefore, there is an urgent need to provide a solution to ensure that the back side of the semiconductor substrate layer has good flatness while reducing the breakage rate of the semiconductor substrate layer, and to ensure the adhesion of the slurry to the back side of the semiconductor substrate layer, thereby improving the photoelectric conversion efficiency and reliability of the heterojunction battery. Summary of the Invention
[0005] Therefore, the technical problem to be solved by the present invention is to overcome the defects in the prior art of low yield due to the large breakage rate of the semiconductor substrate layer, low photoelectric conversion efficiency of the heterojunction battery due to the high cracking rate in the original process, and poor reliability of the heterojunction battery due to the low adhesion of the slurry to the back of the semiconductor substrate layer, thereby providing a method for preparing a heterojunction battery.
[0006] The present invention provides a method for preparing a heterojunction battery, comprising: providing a semiconductor substrate layer, the semiconductor substrate layer comprising a first surface and a second surface relative to each other; forming a patterned mask on the second surface of the semiconductor substrate layer; the patterned mask covering a portion of the second surface; performing a texturing treatment on the first surface and the second surface of the semiconductor substrate layer not covered by the patterned mask; and removing the patterned mask to form a semiconductor substrate layer having a full texturing surface on the first surface and a partial texturing surface on the second surface.
[0007] Optionally, the patterned mask is in a strip shape; there are several patterned masks, and the several patterned masks are parallel to each other and spaced apart; the method of forming the patterned mask includes one or more of screen printing, spraying, photolithography, deposition or physical sputtering.
[0008] Optionally, the texturing treatment uses an alkaline texturing solution, which includes a KOH solution or a NaOH solution. The mass percentage concentration of the alkaline texturing solution is 0.01%-20%, the texturing treatment temperature is 40°C-80°C, and the texturing treatment time is 60s-300s.
[0009] Optionally, the step of removing the patterned mask includes: placing the semiconductor substrate layer in an acid cleaning solution to perform acid cleaning on the patterned mask to remove the patterned mask, thereby forming a semiconductor substrate layer with the first surface being a full velvet surface and the second surface being a partial velvet surface.
[0010] Optionally, the pickling solution includes an HF solution, the mass percentage concentration of the pickling solution is 0.001%-30%, the temperature of the pickling treatment is 25° C.-30° C., and the time of the pickling treatment is 20s-600s.
[0011] Optionally, the method further includes: before forming a patterned mask on the second surface of the semiconductor substrate layer, performing a pre-cleaning treatment on the first surface and the second surface of the semiconductor substrate layer; the pre-cleaning treatment uses a mixed solution of HF and HCl; the mass percentage concentration of the HF is 0.01%-5%, and the mass percentage concentration of the HCl is 5%-20%; and the volume ratio of HF to HCl in the mixed solution is 0.1-0.3.
[0012] Optionally, it also includes: forming a first gate line on one side of the first surface of the semiconductor substrate layer, and forming a second gate line on one side of the second surface of the semiconductor substrate layer; the second gate line is arranged corresponding to the velvet surface of the second surface, and the first gate line is arranged corresponding to the second gate line; it also includes: after removing the patterned mask, forming a first intrinsic semiconductor layer on the first surface of the semiconductor substrate layer and a second intrinsic semiconductor layer on the second surface of the semiconductor substrate layer; forming a first doped semiconductor layer on the side of the first intrinsic semiconductor layer away from the semiconductor substrate layer and forming a second doped semiconductor layer on the side of the second intrinsic semiconductor layer away from the semiconductor substrate layer; wherein the conductivity type of the second doped semiconductor layer is opposite to the conductivity type of the first doped semiconductor layer; forming a first transparent conductive film on the side of the first doped semiconductor layer away from the semiconductor substrate layer; forming a second transparent conductive film on the side of the second doped semiconductor layer away from the semiconductor substrate layer; after forming the first transparent conductive film and the second transparent conductive film, forming a first gate line on the side of the first transparent conductive film away from the semiconductor substrate layer; forming a second gate line on the side of the second transparent conductive film away from the semiconductor substrate layer.
[0013] The present invention also provides a heterojunction battery, comprising: a semiconductor substrate layer, wherein a first surface of the semiconductor substrate layer is fully velvet-faced, and a second surface of the semiconductor substrate layer is partially velvet-faced.
[0014] Optionally, it also includes: a first gate line located on the first surface side of the semiconductor substrate layer; a second gate line located on the second surface side of the semiconductor substrate layer; the second gate line is arranged corresponding to the velvet surface of the second surface, and the first gate line and the second gate line are arranged correspondingly.
[0015] Optionally, it also includes: a first intrinsic semiconductor layer, located on the first surface of the semiconductor substrate layer, and on the side of the first gate line facing the semiconductor substrate layer; a second intrinsic semiconductor layer, located on the second surface of the semiconductor substrate layer, and on the side of the second gate line facing the semiconductor substrate layer; a first doped semiconductor layer, located on the side of the first intrinsic semiconductor layer facing away from the semiconductor substrate layer, and on the side of the first gate line facing the semiconductor substrate layer; a second doped semiconductor layer, located on the side of the second intrinsic semiconductor layer facing away from the semiconductor substrate layer, and on the side of the second gate line facing the semiconductor substrate layer; a first transparent conductive film, located on the side of the first doped semiconductor layer facing away from the semiconductor substrate layer, and on the side of the first gate line facing the semiconductor substrate layer; a second transparent conductive film, located on the side of the second doped semiconductor layer facing away from the semiconductor substrate layer, and on the side of the second gate line facing the semiconductor substrate layer; wherein the conductivity type of the second doped semiconductor layer is opposite to the conductivity type of the first doped semiconductor layer.
[0016] The beneficial effects of the present invention are:
[0017] The present invention provides a method for preparing a heterojunction cell. A full textured surface is formed on the first surface of a semiconductor substrate layer. When light is irradiated from the first surface of the heterojunction cell, the amount of incident sunlight reflected by the semiconductor substrate layer is reduced, thereby allowing more sunlight incident from the first surface of the heterojunction cell to enter the semiconductor substrate layer. The area where the patterned mask is formed on the second surface of the semiconductor substrate layer is not affected by the textured process and becomes partially polished after the patterned mask is removed. This facilitates long-wave absorption by the semiconductor substrate layer, preventing recombination of photogenerated carriers on the second surface of the semiconductor substrate layer and increasing the lifetime of minority carriers. Furthermore, it facilitates maintaining the flatness of the second surface of the semiconductor substrate layer, improving the uniformity of the subsequently formed amorphous silicon layer and enhancing the passivation effect of the amorphous silicon layer. Furthermore, it eliminates the need for a back-polishing process, thereby reducing the breakage rate of the semiconductor substrate layer and improving the photoelectric conversion efficiency of the heterojunction cell. Furthermore, the partial textured surface formed on the second surface of the semiconductor substrate layer facilitates improved adhesion of a subsequently printed paste to the semiconductor substrate layer, preventing debonding of a subsequently formed second gate line and improving the reliability of the heterojunction cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the specific embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0019] Figure 1 Flowchart of the method for preparing a heterojunction battery in Example 1 of the present invention;
[0020] Figures 2 to 10 Schematic diagram of the structure of each process in the method for preparing a heterojunction battery in Example 1 of the present invention;
[0021] Description of reference numerals:
[0022] 1-semiconductor substrate layer; 2-patterned mask; 4-first intrinsic semiconductor layer; 5-second intrinsic semiconductor layer; 6-first doped semiconductor layer; 7-second doped semiconductor layer; 8-first transparent conductive film; 9-second transparent conductive film; 10-first gate line; 11-second gate line. DETAILED DESCRIPTION
[0023] The technical solution of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the embodiments described are only some embodiments of the present invention, not all embodiments. All other embodiments obtained by ordinary technicians in this field based on the embodiments of the present invention without making any creative efforts shall fall within the scope of protection of the present invention.
[0024] In the description of the present invention, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings and are intended solely to facilitate and simplify the description of the present invention. They are not intended to indicate or imply that the devices or components referred to must have, be constructed, or operate in a specific orientation, and therefore should not be construed as limitations on the present invention. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.
[0025] In the description of the present invention, it should be noted that, unless otherwise expressly specified or limited, the terms "mounted," "connected," and "connected" should be understood in a broad sense. For example, they may refer to fixed, detachable, or integral connections; mechanical or electrical connections; direct or indirect connections through an intermediate medium; and internal communication between two components. Those skilled in the art will understand the specific meanings of the above terms in the present invention based on the specific circumstances.
[0026] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0027] Example 1
[0028] This invention provides a method for preparing a heterojunction solar cell, as described in the following embodiments. Figure 1 , the method comprising:
[0029] S1: A semiconductor substrate layer is provided, the semiconductor substrate layer including opposing first and second surfaces;
[0030] S2: A patterned mask is formed on the second surface of the semiconductor substrate layer; the patterned mask covers a portion of the second surface;
[0031] S3: Texturing is performed on the areas of the first and second surfaces of the semiconductor substrate that are not covered by the patterned mask;
[0032] S4: Remove the patterned mask to form a semiconductor substrate layer with a fully textured first surface and a partially textured second surface.
[0033] In this embodiment, a full textured surface is formed on the first surface of the semiconductor substrate layer. When light is irradiated from the first surface of the heterojunction cell, the amount of incident sunlight reflected by the semiconductor substrate layer is reduced, thereby allowing more sunlight incident from the first surface of the heterojunction cell to enter the semiconductor substrate layer. The area on the second surface of the semiconductor substrate layer where the patterned mask is formed is not affected by the textured process and becomes partially polished after the patterned mask is removed. Firstly, this facilitates long-wavelength absorption by the semiconductor substrate layer, preventing recombination of photogenerated carriers on the second surface of the semiconductor substrate layer and increasing the minority carrier lifetime. Secondly, it facilitates maintaining the flatness of the second surface of the semiconductor substrate layer, improving the uniformity of the subsequently formed amorphous silicon layer, and enhancing the passivation effect of the amorphous silicon layer. Thirdly, it eliminates the need for a back-polishing process, thereby reducing the breakage rate of the semiconductor substrate layer and improving the photoelectric conversion efficiency of the heterojunction cell. Furthermore, the partial textured surface on the second surface of the semiconductor substrate layer facilitates improved adhesion of the subsequently printed paste to the semiconductor substrate layer, preventing debonding of the subsequently formed second gate line, and improving the reliability of the heterojunction cell.
[0034] The method for preparing the heterojunction battery further includes: before forming a patterned mask on the second surface of the semiconductor substrate layer, performing a pre-cleaning process on the first surface and the second surface of the semiconductor substrate layer.
[0035] Refer to the following Figures 2 to 10 The preparation method of heterojunction battery is introduced in detail.
[0036] refer to Figure 2 , providing a semiconductor substrate layer 1.
[0037] The semiconductor substrate layer 1 includes a first surface and a second surface opposite to each other.
[0038] Specifically, the first surface of the semiconductor substrate layer 1 is the front surface of the semiconductor substrate layer 1, and the second surface of the semiconductor substrate layer 1 is the back surface of the semiconductor substrate layer 1. In other embodiments, the first surface of the semiconductor substrate layer may be the back surface of the semiconductor substrate layer, and the second surface of the semiconductor substrate layer may be the front surface of the semiconductor substrate layer.
[0039] The material of the semiconductor substrate layer 1 includes single crystal silicon. In other embodiments, the material of the semiconductor substrate layer is other semiconductor materials, such as silicon or silicon germanium. The material of the semiconductor substrate layer can also be other semiconductor materials.
[0040] In this embodiment, the conductivity type of the semiconductor substrate layer is N-type, for example, it can be an N-type silicon wafer, which is suitable for the preparation of heterojunction batteries.
[0041] refer to Figure 3 , pre-cleaning treatment is performed on the first surface and the second surface of the semiconductor substrate layer 1.
[0042] The functions of the pre-cleaning treatment include: removing organic matter and metal contaminants on the first surface and the second surface of the semiconductor substrate layer 1 .
[0043] In this embodiment, a mixed solution of HF and HCl is used for the pre-cleaning process; the mass percentage concentration of HF is 0.01%-5%, for example, 0.01%, 1%, 3% or 5%, and the mass percentage concentration of HCl is 5%-20%, for example, 5%, 10%, 15% or 20%; the volume ratio of HF to HCl in the mixed solution is 0.1-0.3, for example, 0.1, 0.2 or 0.3.
[0044] In this embodiment, after the first surface and the second surface of the semiconductor substrate layer 1 are pre-cleaned, the first surface and the second surface of the semiconductor substrate layer 1 are subjected to a first drying process (not shown in the figure).
[0045] refer to Figure 4 , forming a patterned mask 2 on the second surface of the semiconductor substrate layer 1 .
[0046] In this embodiment, after a first drying treatment is performed on the first and second surfaces of the semiconductor substrate layer 1, a patterned mask 2 is formed on the second surface of the semiconductor substrate layer 1. The patterned mask 2 is alkali-resistant but not acid-resistant. Since the subsequent texturing treatment uses an alkaline texturing solution, the area of the semiconductor substrate layer 1 blocked by the patterned mask 2 undergoes the texturing treatment and becomes partially polished after the patterned mask 2 is removed. This eliminates the need for a back-polishing process, reduces the occurrence of cracks in the original process, lowers the breakage rate of the semiconductor substrate layer 1, improves product yield, and simultaneously enhances the photoelectric conversion efficiency of the heterojunction cell. Secondly, in the subsequent step of removing the patterned mask 2, it can be directly removed only during the acid washing process of the semiconductor substrate layer 1, eliminating the need for an additional cleaning process and reducing process production costs.
[0047] In one embodiment, the patterned mask 2 is strip-shaped; the number of patterned masks 2 is several, and the several patterned masks 2 are parallel to each other and spaced apart.
[0048] In one embodiment, the method of forming the patterned mask 2 includes one or more of screen printing, spraying, photolithography, deposition or physical sputtering. In other embodiments, the method of forming the patterned mask includes other methods.
[0049] In other embodiments, the first drying process is not required; after the first surface and the second surface of the semiconductor substrate layer 1 are pre-cleaned, a patterned mask is formed on the second surface of the semiconductor substrate layer.
[0050] refer to Figure 5 The first and second surfaces of the semiconductor substrate 1 are texturized.
[0051] After forming a patterned mask 2 on the second surface of the semiconductor substrate 1, the first and second surfaces of the semiconductor substrate 1 are texturized.
[0052] After the texturing process, the first surface of the semiconductor substrate layer 1 is fully textured. When light is irradiated from the first surface of the heterojunction cell, the amount of incident sunlight reflected by the semiconductor substrate layer 1 is reduced, allowing more sunlight incident from the first surface of the heterojunction cell to enter the semiconductor substrate layer 1. The second surface of the semiconductor substrate layer 1, where the patterned mask 2 is not formed, has a partial textured surface, which helps improve the adhesion of the subsequently printed paste to the semiconductor substrate layer, prevents the subsequent second gate line from decoupling, and improves the reliability of the heterojunction cell.
[0053] In one embodiment, the nap is pyramidal in shape. In other embodiments, the nap may also be other shapes, without limitation.
[0054] In one embodiment, a pyramid light-recessed velvet surface is formed by alkali texturing. The texturing treatment uses an alkaline texturing solution, and the alkaline texturing solution includes a KOH solution or a NaOH solution. The mass percentage concentration of the alkaline texturing solution is 0.01%-20%, for example, 0.01%, 2%, 4%, 6%, 8%, 10%, 15% or 20%; the texturing treatment temperature is 40°C-80°C, for example, 40°C, 50°C, 60°C, 70°C or 80°C, and the texturing treatment time is 60s-300s, for example, 60s, 100s, 150s, 200s, 250s or 300s.
[0055] refer to Figure 6 , remove the patterned mask 2 to form a semiconductor substrate layer with a first surface that is a full textured surface and a second surface that is a partial textured surface.
[0056] After texturing the first surface and the second surface of the semiconductor substrate layer 1 , the patterned mask 2 is removed.
[0057] Specifically, the step of removing the patterned mask 2 includes: placing the semiconductor substrate layer 1 in an acid cleaning solution to acid-clean the patterned mask 2 to remove the patterned mask, thereby forming a semiconductor substrate layer 1 with a full velvet surface on the first surface and a partial velvet surface on the second surface.
[0058] In one embodiment, the pickling solution comprises an HF solution, and the mass percentage concentration of the pickling solution is 0.001%-30%, for example, 0.001%, 5%, 10%, 15%, 20%, or 30%; the pickling temperature is 25°C-30°C, for example, 25°C, 28°C, or 30°C; and the pickling time is 20s-600s, for example, 20s, 100s, 200s, 300s, 400s, 500s, or 600s.
[0059] In this embodiment, after removing the patterned mask 2, the first and second surfaces of the semiconductor substrate 1 are rinsed; after rinsing the first and second surfaces of the semiconductor substrate 1, the first and second surfaces of the semiconductor substrate 1 are dried.
[0060] refer to Figure 7 A first intrinsic semiconductor layer 4 is formed on the first surface of the semiconductor substrate layer 1 , and a second intrinsic semiconductor layer 5 is formed on the second surface of the semiconductor substrate layer 1 .
[0061] After the first surface and the second surface of the semiconductor substrate layer 1 are subjected to a second baking process, a first intrinsic semiconductor layer 4 is formed on the first surface of the semiconductor substrate layer 1 and a second intrinsic semiconductor layer 5 is formed on the second surface of the semiconductor substrate layer 1 .
[0062] In other embodiments, no second drying process or rinsing process is required; after removing the patterned mask, a first intrinsic semiconductor layer is formed on the first surface of the semiconductor substrate and a second intrinsic semiconductor layer is formed on the second surface of the semiconductor substrate.
[0063] The process for forming the first intrinsic semiconductor layer 4 includes a vapor deposition process. The process for forming the second intrinsic semiconductor layer 5 also includes a vapor deposition process. By forming the first intrinsic semiconductor layer 4 and the second intrinsic semiconductor layer 5, the dangling bonds of the semiconductor substrate layer 1 can be effectively hydrogenated and surface defects reduced, thereby improving minority carrier lifetime, increasing open-circuit voltage, and ultimately improving the efficiency of the heterojunction cell.
[0064] refer to Figure 8 A first doped semiconductor layer 6 is formed on the side of the first intrinsic semiconductor layer 4 away from the semiconductor substrate layer 1, and a second doped semiconductor layer 7 is formed on the side of the second intrinsic semiconductor layer 5 away from the semiconductor substrate layer 1.
[0065] After forming a first intrinsic semiconductor layer 4 on the first surface of the semiconductor substrate layer 1 and a second intrinsic semiconductor layer 5 on the second surface of the semiconductor substrate layer 1, a first doped semiconductor layer 6 is formed on a side of the first intrinsic semiconductor layer 4 facing away from the semiconductor substrate layer 1, and a second doped semiconductor layer 7 is formed on a side of the second intrinsic semiconductor layer 5 facing away from the semiconductor substrate layer 1. The conductivity type of the second doped semiconductor layer 7 is opposite to that of the first doped semiconductor layer 6.
[0066] In this embodiment, the conductivity type of the first doped semiconductor layer 6 is N-type and the conductivity type of the second doped semiconductor layer 7 is P-type, as an example.
[0067] The process for forming the first doped semiconductor layer 6 includes a vapor deposition process. The process for forming the second doped semiconductor layer 7 also includes a vapor deposition process.
[0068] refer to Figure 9 A first transparent conductive film 8 is formed on the side of the first doped semiconductor layer 6 away from the semiconductor substrate layer 1; and a second transparent conductive film 9 is formed on the side of the second doped semiconductor layer 7 away from the semiconductor substrate layer 1.
[0069] After a first doped semiconductor layer 6 is formed on the first surface of the first intrinsic semiconductor layer 4 facing away from the semiconductor substrate layer 1 and a second doped semiconductor layer 7 is formed on the second surface of the second intrinsic semiconductor layer 5 facing away from the semiconductor substrate layer 1, a first transparent conductive film 8 is formed on the side of the first doped semiconductor layer 6 facing away from the semiconductor substrate layer 1; and a second transparent conductive film 9 is formed on the side of the second doped semiconductor layer 7 facing away from the semiconductor substrate layer 1.
[0070] refer to Figure 10 A first gate line 10 is formed on the side of the first transparent conductive film 8 facing away from the semiconductor substrate layer 1 ; and a second gate line 11 is formed on the side of the second transparent conductive film 9 facing away from the semiconductor substrate layer 1 .
[0071] A first transparent conductive film 8 is formed on the side of the first doped semiconductor layer 6 facing away from the semiconductor substrate layer 1; after a second transparent conductive film 9 is formed on the side of the second doped semiconductor layer 7 facing away from the semiconductor substrate layer 1, a first gate line 10 is formed on the side of the first transparent conductive film 8 facing away from the semiconductor substrate layer 1; and a second gate line 11 is formed on the side of the second transparent conductive film 9 facing away from the semiconductor substrate layer 1.
[0072] Specifically, the second gate lines 11 are arranged corresponding to the velvet surface of the second surface, and the first gate lines 10 are arranged corresponding to the second gate lines 11 .
[0073] Example 2
[0074] This embodiment provides a heterojunction battery, referring to Figure 10 ,include:
[0075] The semiconductor substrate layer 1 has a first surface that is fully textured, and a second surface that is partially textured.
[0076] In this embodiment, the first surface of the semiconductor substrate layer 1 is fully textured. When light is irradiated from the first surface of the heterojunction cell, the amount of incident sunlight reflected by the semiconductor substrate layer 1 is reduced, thereby allowing more sunlight incident from the first surface of the heterojunction cell to enter the semiconductor substrate layer 1. The second surface of the semiconductor substrate layer 1 is partially textured, which helps improve the adhesion of the subsequently printed paste to the semiconductor substrate layer, prevents the subsequent formation of a second gate line debonding, and improves the reliability of the heterojunction cell.
[0077] The heterojunction battery further includes: a first gate line 10 located on a first surface side of the semiconductor substrate layer 1 ; and a second gate line 11 located on a second surface side of the semiconductor substrate layer 1 .
[0078] In one embodiment, the second gate line 11 is disposed corresponding to the textured surface of the second surface, and the first gate line 10 is disposed corresponding to the second gate line 11. Since the textured structure helps maintain the adhesion of the printed paste to the semiconductor substrate, it can prevent the first gate line 10 and the second gate line 11 from detaching, thereby improving the reliability of the heterojunction cell.
[0079] The heterojunction battery also includes: a first intrinsic semiconductor layer 4, located on the first surface of the semiconductor substrate layer 1, and on the side of the first gate line 10 facing the semiconductor substrate layer 1; a second intrinsic semiconductor layer 5, located on the second surface of the semiconductor substrate layer 1, and on the side of the second gate line 11 facing the semiconductor substrate layer 1; a first doped semiconductor layer 6, located on the side of the first intrinsic semiconductor layer 4 facing away from the semiconductor substrate layer 1, and on the side of the first gate line 10 facing the semiconductor substrate layer 1; a second doped semiconductor layer 7, located on the side of the second intrinsic semiconductor layer 5 facing away from the semiconductor substrate layer 1, and on the side of the second gate line 11 facing the semiconductor substrate layer 1; a first transparent conductive film 8, located on the side of the first doped semiconductor layer 6 facing away from the semiconductor substrate layer 1, and on the side of the first gate line 10 facing the semiconductor substrate layer 1; and a second transparent conductive film 9, located on the side of the second doped semiconductor layer 7 facing away from the semiconductor substrate layer 1, and on the side of the second gate line 11 facing the semiconductor substrate layer 1.
[0080] The conductivity type of the second doped semiconductor layer 7 is opposite to that of the first doped semiconductor layer 6. In this embodiment, the conductivity type of the first doped semiconductor layer 6 is N-type and the conductivity type of the second doped semiconductor layer 7 is P-type, as an example.
[0081] The present invention is different from the prior art in that the back surface of the semiconductor substrate layer is polished by reacting the alkaline solution with the entire area of the back surface of the semiconductor substrate layer, while the entire area of the front surface is not reacted due to the protection of the oxide layer, so that the back surface of the semiconductor substrate layer can form a back-polished surface with good flatness. Specifically, the first surface mentioned in the present invention is the front surface of the semiconductor substrate layer, and the second surface is the back surface of the semiconductor substrate layer; the area on the back surface of the semiconductor substrate layer 1 of the present invention where the patterned mask is formed is subjected to a texturing treatment, and is partially polished after the patterned mask is removed, without the need to add a back-polishing process, which can reduce the breakage rate of the semiconductor substrate layer 1, improve the product yield, and reduce the cracking situation in the original process, thereby improving the photoelectric conversion efficiency of the heterojunction battery by about 0.05%-0.2%; at the same time, the area on the semiconductor substrate layer 1 where the patterned mask 2 is not formed is subjected to a texturing treatment to form a partial velvet surface, which is beneficial to improving the adhesion of the subsequently printed slurry to the semiconductor substrate layer 1, avoiding the subsequent formation of the first gate line 10 and the second gate line 11 being off the gate, and improving the reliability of the heterojunction battery.
[0082] Obviously, the above embodiments are merely examples for clarity of explanation and are not intended to limit the implementation methods. Those skilled in the art will readily appreciate that other variations or modifications based on the above descriptions are possible. It is not necessary and impossible to enumerate all implementation methods here. Obvious variations or modifications arising therefrom remain within the scope of protection of the present invention.
Claims
1. A method for preparing a heterojunction battery, It is characterized in that include: Providing a semiconductor substrate layer, the semiconductor substrate layer comprising a first surface and a second surface opposite to each other; Performing a pre-cleaning process on the first surface and the second surface of the semiconductor substrate layer; A patterned mask is formed on the second surface of the semiconductor substrate layer; the patterned mask covers a portion of the second surface; the patterned mask is in a strip shape, the number of the patterned masks is a plurality of strips, and the plurality of patterned masks are parallel to each other and spaced apart; Performing texturing treatment on the areas of the first surface and the second surface of the semiconductor substrate layer that are not covered by the patterned mask to form a semiconductor substrate layer in which the first surface is fully textured and the second surface is partially textured; The patterned mask is removed by pickling, so that a smooth surface is formed on the second surface at a position corresponding to the patterned mask.
2. The method for preparing a heterojunction battery according to claim 1, It is characterized in that The method of forming the patterned mask includes one or more of screen printing, spraying, photolithography, deposition or physical sputtering.
3. The method for preparing a heterojunction battery according to claim 1, It is characterized in that The texturing treatment uses an alkaline texturing solution, which includes a KOH solution or a NaOH solution. The mass percentage concentration of the alkaline texturing solution is 0.01%-20%. The texturing treatment temperature is 40° C.-80° C., and the texturing treatment time is 60s-300s.
4. The method for preparing a heterojunction battery according to claim 1, Features: The step of removing the patterned mask by pickling includes placing the semiconductor substrate layer in a pickling solution and performing the pickling treatment on the patterned mask to remove the patterned mask so that a smooth surface is formed on the second surface at a position corresponding to the patterned mask.
5. The method for preparing a heterojunction battery according to claim 4, It is characterized in that The pickling solution includes HF solution, the mass percentage concentration of the pickling solution is 0.001%-30%, the temperature of the pickling treatment is 25°C-30°C, and the time of the pickling treatment is 20s-600s.
6. A method for preparing a heterojunction battery according to any one of claims 1 to 5, It is characterized in that The pre-cleaning treatment uses a mixed solution of HF and HCl; the mass percentage concentration of the HF is 0.01%-5%, the mass percentage concentration of the HCl is 5%-20%; the volume ratio of HF to HCl in the mixed solution is 0.1-0.
3.
7. The method for preparing a heterojunction battery according to any one of claims 1 to 5, It is characterized in that Also includes: A first gate line is formed on one side of the first surface of the semiconductor substrate layer, and a second gate line is formed on one side of the second surface of the semiconductor substrate layer; the second gate line is arranged corresponding to the velvet surface of the second surface, and the first gate line is arranged corresponding to the second gate line; Correspondingly, after removing the patterned mask, the preparation method further comprises: after removing the patterned mask, forming a first intrinsic semiconductor layer on the first surface of the semiconductor substrate layer and forming a second intrinsic semiconductor layer on the second surface of the semiconductor substrate layer; Forming a first doped semiconductor layer on a side of the first intrinsic semiconductor layer away from the semiconductor substrate layer and forming a second doped semiconductor layer on a side of the second intrinsic semiconductor layer away from the semiconductor substrate layer; wherein the conductivity type of the second doped semiconductor layer is opposite to that of the first doped semiconductor layer; A first transparent conductive film is formed on a side of the first doped semiconductor layer away from the semiconductor substrate layer; a second transparent conductive film is formed on a side of the second doped semiconductor layer away from the semiconductor substrate layer; after forming the first transparent conductive film and the second transparent conductive film, a first gate line is formed on a side of the first transparent conductive film away from the semiconductor substrate layer; and a second gate line is formed on a side of the second transparent conductive film away from the semiconductor substrate layer.
Citation Information
Patent Citations
High efficiency N-type double-faced solar cell and preparation method thereof
CN104733555A
Mono-crystalline silicon double-sided solar cell and preparation method thereof
CN105826405A
Selective emitter black silicon battery and manufacturing method thereof
CN108074999A
Method for fabricating selective textured surface and emitter of silicon solar cell by laser
CN109346535A
Crystalline silicon solar battery and method for producing same
CN109690791A