A method for fabricating electrospray quartz nozzles based on hydrofluoric acid
By using hydrofluoric acid corrosion and micro-water flow control, the problems of uneven inner diameter and high scrap rate in the manufacturing process of electrospray quartz nozzles were solved, enabling efficient and controllable mass production.
Patent Information
- Application Number
- CN202311156762.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2023-07-24
- Filing Date
- 2023-09-08
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-09-08
AI Technical Summary
Existing methods for manufacturing electrospray quartz nozzles are difficult to achieve rapid, mass production, and the small inner diameter of the conical tip leads to a high scrap rate and makes quality control difficult.
Hydrofluoric acid is used to etch quartz capillaries to form a conical tip. The corrosion process is controlled by the surface tension of the hydrofluoric acid solution and a small amount of water flow to ensure that the inner diameter of the conical tip is consistent with the inner diameter of the capillary, thus avoiding the problem of clogging due to an excessively small inner diameter. A magnetic stirrer is used to ensure the uniformity of corrosion.
It enables rapid, high-volume production of electrospray quartz nozzles, reduces the scrap rate caused by excessively small inner diameter of the conical tip, improves product quality control and repeatability, and avoids spray instability.
Smart Images

Figure CN117228624B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a method for manufacturing an electrospray quartz nozzle, and more particularly to a method for manufacturing an electrospray quartz nozzle based on hydrofluoric acid. Background Technology
[0002] Mass spectrometry, with its outstanding qualitative and quantitative capabilities, is currently the gold standard in various detection and analysis fields, playing an irreplaceable role in major national fields such as proteomics, biomedicine, and clinical diagnostics. Electrospray ionization (ESI), as a highly efficient and convenient continuous ion source technology, has become the mainstream mass spectrometry ion source technology due to its ability to maintain the molecular structure of the analyte during ionization and to allow the sample to carry multiple charges. Nano-liter ESI, by controlling the injection flow rate at the nanoliter level, can further improve the ionization efficiency of the ESI for the analyte, thus also being the most mainstream ESI technology. However, nano-liter ESI places extremely high demands on the ESI nozzle, requiring only an extremely thin outer wall at the nozzle tip. An excessively thick outer wall at the nozzle tip will result in an excessively large Taylor cone angle, leading to instability of the ESI.
[0003] The existing electrospray nozzles are mainly made of quartz, and are also called electrospray quartz nozzles. The existing manufacturing methods for electrospray quartz nozzles mostly involve heating a 1-2 cm long area in the middle of a quartz capillary at high temperature until this area is close to a molten state. Then, the two ends of the quartz capillary are manually pulled, causing the area close to the molten state to lengthen due to the stretching and eventually break off. After the area close to the molten state breaks off, it solidifies to form two conical tips of the electrospray quartz nozzle. Although the electrospray quartz nozzle manufacturing method has an extremely thin outer wall at the very tip (the small end of the conical tip), during the process of pulling the quartz capillary, as the area of the quartz capillary nearing the melting state gradually becomes thinner, the outer and inner diameters of the resulting conical tip also decrease simultaneously. An excessively small inner diameter is prone to clogging during use. In addition, it is difficult to mass-produce by hand, and manually pulling the quartz capillary relies on experience and feel, making it difficult to control product quality. Therefore, when using the current method to select qualified electrospray quartz nozzles through microscopic observation later, a large number of scrapped products with excessively small inner diameters of the conical tip will be found, resulting in a high scrap rate. Summary of the Invention
[0004] The technical problem to be solved by the present invention is to provide a method for manufacturing electrospray quartz nozzles based on hydrofluoric acid, which can quickly and in large quantities produce electrospray quartz nozzles with controllable quality during the manufacturing process and can greatly reduce the high scrap rate caused by the small inner diameter of the conical tip of the electrospray quartz nozzle.
[0005] The technical solution adopted by this invention to solve the above-mentioned technical problems is as follows: a method for manufacturing an electrospray quartz nozzle based on hydrofluoric acid, comprising the following steps:
[0006] Step 1: Select the appropriate quartz capillary tube according to the specifications of the electro-spray quartz nozzle, cut the quartz capillary tube to the required length, and then remove the outer protective film of the quartz capillary tube.
[0007] Step 2: Select any end of the quartz capillary tube to connect to the liquid injection pump. The end of the quartz capillary tube connected to the liquid injection pump is called the liquid injection pump connected end, and the end of the quartz capillary tube not connected to the liquid injection pump is called the liquid injection pump not connected end.
[0008] Step 3: Use hydrofluoric acid to corrode the section of the quartz capillary tube that is not connected to the liquid injection pump to form a tapered tip. The specific process is as follows:
[0009] S3.1 Prepare a hydrofluoric acid solution with a volume concentration of 20%–99%, and place a magnetic stirrer at the bottom of the hydrofluoric acid solution. Fix a quartz capillary tube vertically above the hydrofluoric acid solution, with the unconnected end facing down and the connected end facing up. Immerse a 0.5–1.0 cm section of the quartz capillary tube completely in the hydrofluoric acid solution. Due to the surface tension between the hydrofluoric acid solution and the quartz capillary tube, the hydrofluoric acid solution around the immersed section rises by 2–3 mm. Furthermore, the surface tension between the hydrofluoric acid solution and the quartz capillary tube increases with increasing height. As the height increases, the amount of hydrofluoric acid solution rising around the section of the quartz capillary immersed in the hydrofluoric acid solution gradually decreases. That is, hydrofluoric acid solution is also present around the outer wall of a portion of the quartz capillary 2-3 mm above the section immersed in the hydrofluoric acid solution, and the contact amount between this portion of the quartz capillary and the hydrofluoric acid solution decreases from bottom to top. While the quartz capillary is immersed in the hydrofluoric acid solution, water is continuously injected into the quartz capillary from the end connected to the liquid injection pump using a liquid injection pump. The water flow rate is 0.01 μL / min to 10 μL / min. The injected water flows out from the end of the quartz capillary not connected to the liquid injection pump and enters the hydrofluoric acid solution.
[0010] S3.2 Using a magnetic stirrer, stir at a speed not exceeding 30 revolutions per minute at the bottom of the hydrofluoric acid solution. The outer wall of the section of quartz capillary completely immersed in the hydrofluoric acid solution is uniformly corroded by the hydrofluoric acid solution. The outer wall of the section of quartz capillary above the section of quartz capillary completely immersed in the hydrofluoric acid solution is also corroded by the hydrofluoric acid solution around it, and the degree of corrosion decreases from bottom to top.
[0011] S3.3 When it is observed that the quartz capillary below the hydrofluoric acid solution level is completely corroded, the tension between the hydrofluoric acid solution surface and the quartz capillary disappears, the hydrofluoric acid solution level is normal, and the contact between the hydrofluoric acid solution and the quartz capillary is completely cut off. At this time, a section of the quartz capillary with a height of 2-3 mm above the hydrofluoric acid solution level forms a perfect conical tip on its outer wall. The inner diameter of this conical tip is still equal to the inner diameter of the quartz capillary. At this time, the liquid injection pump is turned off, and water is stopped being injected into the quartz capillary.
[0012] Step 4: Remove the liquid injection pump from the quartz capillary and add a hydrophobic protective layer to the tapered tip of the quartz capillary to obtain an electro-spray quartz nozzle.
[0013] In step (1), the specific steps for selecting a quartz capillary of the appropriate specification according to the specifications of the electro-spray quartz nozzle, cutting the quartz capillary to the required length, and then removing the outer protective film of the quartz capillary are as follows:
[0014] S1.1. Using a capillary cutter, select a quartz capillary of the appropriate specification and cut it to obtain a quartz capillary of the required length.
[0015] S1.2. Immerse the cut quartz capillary tube completely into a saturated sodium hydroxide solution at a temperature of 100 degrees Celsius until the saturated sodium hydroxide solution completely corrodes away the outer protective film of the quartz capillary tube.
[0016] S1.3 Clean the quartz capillary tube obtained in step S1.2 with clean water and let it dry.
[0017] In step (2), the end of the quartz capillary connected to the liquid injection pump is connected to the injection needle on the liquid injection pump via a reducing adapter.
[0018] The specific process of adding a hydrophobic protective layer to the conical tip of the quartz capillary in step (4) is as follows: the conical tip of the quartz capillary is immersed in the silicone waterproofing agent for 1 second and then quickly pulled out and left to stand. When the silicone waterproofing agent attached to the surface of the conical tip dries, a hydrophobic protective layer is formed on the surface of the conical tip of the quartz capillary.
[0019] Compared with the prior art, the advantage of this invention lies in that by first connecting one end of a quartz capillary to a liquid injection pump, and then using hydrofluoric acid to corrode the section of the quartz capillary starting from the end not connected to the liquid injection pump, a conical tip is formed. During the formation of the conical tip, the section of the quartz capillary starting from the end not connected to the liquid injection pump is completely immersed in the hydrofluoric acid solution. Due to the surface tension between the hydrofluoric acid solution and the quartz capillary, the hydrofluoric acid solution around the section of the quartz capillary immersed in the solution rises by 2-3 mm under the surface tension. Furthermore, due to the surface tension between the hydrofluoric acid solution and the quartz capillary, the hydrofluoric acid solution around the immersed section rises by 2-3 mm with increasing height. As the height of the quartz capillary immersed in the hydrofluoric acid solution gradually decreases, the amount of hydrofluoric acid solution rising around the section of the capillary immersed in the hydrofluoric acid solution also decreases. Specifically, a portion of the capillary above the section immersed in the hydrofluoric acid solution, about 2-3 mm high, also has hydrofluoric acid solution around its outer wall, and the contact amount between this portion of the capillary and the hydrofluoric acid solution decreases from bottom to top. Simultaneously, while the capillary is immersed in the hydrofluoric acid solution, a small amount of water is continuously injected into the capillary from the end connected to the liquid injection pump using a liquid injection pump. The water flows into the hydrofluoric acid solution from the end of the capillary not connected to the liquid injection pump, and the water flow rate is only 0.The water flow rate of 0.01 μL / min to 10 μL / min is far less than the corrosion rate of hydrofluoric acid solution on quartz capillaries. During the corrosion process, the amount of water entering the hydrofluoric acid solution is negligible. Therefore, the water injected using a liquid injection pump will not significantly affect the concentration or level of the hydrofluoric acid solution, and will also prevent the hydrofluoric acid solution from entering the interior of the quartz capillary due to capillary action. This ensures that the subsequent hydrofluoric acid solution will only corrode the outer wall of the quartz capillary, without affecting the inner wall. Furthermore, using a magnetic stirrer to stir the hydrofluoric acid solution at the bottom at a speed not exceeding 30 rpm ensures the uniformity of the hydrofluoric acid solution without significantly affecting its surface, thus guaranteeing the effectiveness of the immersion process. The corrosion uniformity of a quartz capillary segment in a hydrofluoric acid solution was observed during stirring. The outer wall of the segment completely immersed in the hydrofluoric acid solution was uniformly corroded. Because this segment had more thorough contact with the hydrofluoric acid solution, the corrosion rate was faster. The upper portion of the quartz capillary segment, also completely immersed, was gradually corroded by the surrounding hydrofluoric acid solution. However, because this portion only came into contact with a small amount of hydrofluoric acid solution, the corrosion rate was slower. Furthermore, the amount of hydrofluoric acid solution surrounding this portion of the capillary gradually decreased with increasing height, meaning the contact amount between this portion of the capillary and the hydrofluoric acid solution decreased from bottom to top. Therefore, the corrosion rate of this portion of the capillary... The degree of corrosion on the outer wall decreases from bottom to top. When the section of the quartz capillary completely immersed in the hydrofluoric acid solution is completely corroded, the tension between the surface of the hydrofluoric acid solution and the quartz capillary disappears. There is no hydrofluoric acid solution rising due to tension, and the surface of the hydrofluoric acid solution is at a normal horizontal level. The contact between the hydrofluoric acid solution and the quartz capillary is completely severed. The portion of the quartz capillary wall corroded by the hydrofluoric acid solution, which was above the horizontal level of the hydrofluoric acid solution due to surface tension, forms a perfect conical tip. The inner diameter of this conical tip is still equal to the inner diameter of the quartz capillary. Therefore, in the process of forming the conical tip, this invention only requires fixing the quartz capillary above the hydrofluoric acid solution according to the height requirement of the conical tip. By pre-setting a location, a conical tip can be formed through corrosion with hydrofluoric acid solution. This allows for the rapid and mass production of electrospray quartz nozzles with controllable quality and good repeatability. Simultaneously, a trace amount of water is injected into the quartz capillary via a liquid injection pump, ensuring that the hydrofluoric acid solution only corrodes the outer wall of the capillary and does not affect the inner wall. This avoids the instability of subsequent electrospray spraying caused by an excessively large inner diameter of the conical tip. Because the inner diameter of the conical tip matches the inner diameter of the quartz capillary, it is less prone to clogging during subsequent use, significantly reducing the high scrap rate caused by an excessively small inner diameter of the conical tip in electrospray quartz nozzles. Testing shows that the wall thickness of the small end of the conical tip obtained using this method is only 1-2 micrometers. Attached Figure Description
[0020] Figure 1 This is an initial schematic diagram of the quartz capillary tube, starting from the end not connected to the liquid injection pump, being completely immersed in the hydrofluoric acid solution in the electrospray quartz nozzle manufacturing method based on hydrofluoric acid of the present invention.
[0021] Figure 2 This is a schematic diagram showing that half of the quartz capillary in contact with the hydrofluoric acid solution is corroded in the hydrofluoric acid-based electrospray quartz nozzle manufacturing method of the present invention.
[0022] Figure 3 This is a schematic diagram illustrating the process of fabricating a hydrofluoric acid-based electrospray quartz nozzle according to the present invention, in which the quartz capillary in contact with the hydrofluoric acid solution is etched to form a conical tip. Detailed Implementation
[0023] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments.
[0024] Example 1: A method for manufacturing an electrospray quartz nozzle based on hydrofluoric acid, characterized by the following steps:
[0025] Step 1: Select the appropriate quartz capillary tube according to the specifications of the electro-spray quartz nozzle, cut the quartz capillary tube to the required length, and then remove the outer protective film of the quartz capillary tube.
[0026] Step 2: Select any end of the quartz capillary tube to connect to the liquid injection pump to form the end connected to the liquid injection pump. The end of the quartz capillary tube not connected to the liquid injection pump is called the end not connected to the liquid injection pump.
[0027] Step 3: Use hydrofluoric acid to corrode the section of the quartz capillary tube that is not connected to the liquid injection pump to form a tapered tip. The specific process is as follows:
[0028] S3.1 Prepare a 40% hydrofluoric acid solution and place a magnetic stirrer at the bottom of the solution. Fix a quartz capillary tube vertically above the hydrofluoric acid solution, with the unconnected end facing down and the connected end facing up. Immerse a 0.8cm section of the capillary tube completely in the hydrofluoric acid solution. Due to the surface tension between the hydrofluoric acid solution and the capillary tube, the hydrofluoric acid solution around the immersed section rises by 2-3mm. Furthermore, the surface tension between the hydrofluoric acid solution and the capillary tube increases with increasing height. As the height increases, the amount of hydrofluoric acid solution rising around the section of the quartz capillary immersed in the hydrofluoric acid solution gradually decreases. That is, hydrofluoric acid solution is also present around the outer wall of a portion of the quartz capillary 2-3 mm above the section immersed in the hydrofluoric acid solution, and the contact amount between this portion of the quartz capillary and the hydrofluoric acid solution decreases from bottom to top. While the quartz capillary is immersed in the hydrofluoric acid solution, water is continuously injected into the quartz capillary from the end connected to the liquid injection pump using a liquid injection pump. The water flow rate is 0.01 μL / min. The injected water flows out from the end of the quartz capillary not connected to the liquid injection pump and enters the hydrofluoric acid solution.
[0029] S3.2 Using a magnetic stirrer, the bottom of the hydrofluoric acid solution is stirred at a speed of 30 rpm. The outer wall of the section of quartz capillary completely immersed in the hydrofluoric acid solution is uniformly corroded by the hydrofluoric acid solution. The outer wall of the section of quartz capillary above the section of quartz capillary completely immersed in the hydrofluoric acid solution is also corroded by the hydrofluoric acid solution around it, and the degree of corrosion decreases from bottom to top.
[0030] S3.3 When it is observed that the quartz capillary below the hydrofluoric acid solution level is completely corroded, the tension between the hydrofluoric acid solution surface and the quartz capillary disappears, the hydrofluoric acid solution level is normal, the contact between the hydrofluoric acid solution and the quartz capillary is completely cut off, and the outer wall of the section of the quartz capillary corroded by the hydrofluoric acid solution above the hydrofluoric acid solution level under the action of the surface tension of the hydrofluoric acid solution forms a perfect conical tip. The inner diameter of the conical tip is still equal to the inner diameter of the quartz capillary. At this time, the liquid injection pump is turned off and water is stopped being injected into the quartz capillary.
[0031] Step 4: Remove the liquid injection pump from the quartz capillary and add a hydrophobic protective layer to the tapered tip of the quartz capillary to obtain an electro-spray quartz nozzle.
[0032] In this embodiment, the initial schematic diagram of the quartz capillary tube, starting from the end not connected to the liquid injection pump, being completely immersed in the hydrofluoric acid solution in the electrospray quartz nozzle fabrication method based on hydrofluoric acid of the present invention is shown below. Figure 1 As shown in the diagram, in the method for manufacturing an electrospray quartz nozzle based on hydrofluoric acid of the present invention, a schematic diagram of half-corrosion of the quartz capillary in contact with the hydrofluoric acid solution is shown. Figure 2 As shown in the schematic diagram of the method for manufacturing a hydrofluoric acid-based electrospray quartz nozzle of the present invention, the quartz capillary in contact with the hydrofluoric acid solution is corroded to form a conical tip. Figure 3 As shown.
[0033] analyze Figure 1 It can be seen that when a quartz capillary is immersed in a hydrofluoric acid solution, due to the surface tension of the hydrofluoric acid solution, the height of the hydrofluoric acid solution around the quartz capillary will be slightly higher than the horizontal level of the hydrofluoric acid solution, typically 2–3 mm higher. Analysis Figure 2 It can be seen that under the corrosive effect of hydrofluoric acid solution, the outer wall of the quartz capillary is gradually corroded. The quartz capillary below the hydrofluoric acid solution level corrodes faster, while the amount of hydrofluoric acid solution above the solution level, due to surface tension, is smaller and thus corrodes the outer wall of the contacting quartz capillary more slowly. Analysis Figure 3 It can be seen that when the quartz capillary below the hydrofluoric acid solution level is completely corroded, the contact between the hydrofluoric acid solution and the quartz capillary is completely cut off, while a small part of the outer wall of the quartz capillary above the hydrofluoric acid solution level is corroded by a small part of the hydrofluoric acid to form a perfect conical tip.
[0034] Example 2: This example is basically the same as Example 1, except that: in this example, the volume concentration of the hydrofluoric acid solution is 20%, the length of the quartz capillary tube completely immersed in the hydrofluoric acid solution is 0.5 cm, and the water flow rate is 0.01 μL / min.
[0035] Example 3: This example is basically the same as Example 1, except that: in this example, the volume concentration of the hydrofluoric acid solution is 99%, the length of the quartz capillary completely immersed in the hydrofluoric acid solution is 1.0 cm, and the water flow rate is 5 μL / min.
[0036] Example 4: This example is basically the same as Example 1, except that in this example, the specific steps of selecting the appropriate specification of quartz capillary tube according to the specifications of the electro-spray quartz nozzle in step (1), cutting the required length of quartz capillary tube, and then removing the outer protective film of the quartz capillary tube are as follows:
[0037] S1.1. Using a capillary cutter, select a quartz capillary of the appropriate specification and cut it to obtain a quartz capillary of the required length.
[0038] S1.2. Immerse the cut quartz capillary tube completely into a saturated sodium hydroxide solution at a temperature of 100 degrees Celsius until the saturated sodium hydroxide solution completely corrodes away the outer protective film of the quartz capillary tube.
[0039] S1.3 Clean the quartz capillary tube obtained in step S1.2 with clean water and let it dry.
[0040] Example 5: This example is basically the same as Example 1, except that in this example, in step (2), the end of the quartz capillary connected to the liquid injection pump is connected to the injection needle on the liquid injection pump through a reducing adapter.
[0041] Example 6: This example is basically the same as Example 1. The difference is that in this example, the specific process of adding a hydrophobic protective layer to the conical tip of the quartz capillary in step (4) is as follows: the conical tip of the quartz capillary is immersed in the silicone waterproofing agent for 1 second and then quickly pulled out and left to stand. When the silicone waterproofing agent attached to the surface of the conical tip dries, a hydrophobic protective layer is formed on the surface of the conical tip of the quartz capillary.
Claims
1. A method for fabricating an electrospray quartz nozzle based on hydrofluoric acid, characterized in that... Includes the following steps: Step 1: Select the appropriate quartz capillary tube according to the specifications of the electro-spray quartz nozzle, cut the quartz capillary tube to the required length, and then remove the outer protective film of the quartz capillary tube. Step 2: Select any end of the quartz capillary tube to connect to the liquid injection pump. The end of the quartz capillary tube connected to the liquid injection pump is called the liquid injection pump connected end, and the end of the quartz capillary tube not connected to the liquid injection pump is called the liquid injection pump not connected end. Step 3: Use hydrofluoric acid to corrode the section of the quartz capillary tube that is not connected to the liquid injection pump to form a tapered tip. The specific process is as follows: S3.1 Prepare a hydrofluoric acid solution with a volume concentration of 20%–99%, and place a magnetic stirrer at the bottom of the hydrofluoric acid solution. Fix a quartz capillary tube vertically above the hydrofluoric acid solution, with the unconnected end facing down and the connected end facing up. Immerse a 0.5–1.0 cm section of the quartz capillary tube completely in the hydrofluoric acid solution. Due to the surface tension between the hydrofluoric acid solution and the quartz capillary tube, the hydrofluoric acid solution around the immersed section rises by 2–3 mm. Furthermore, the surface tension between the hydrofluoric acid solution and the quartz capillary tube increases with increasing height. As the height increases, the amount of hydrofluoric acid solution rising around the section of the quartz capillary immersed in the hydrofluoric acid solution gradually decreases. That is, hydrofluoric acid solution is also present around the outer wall of a portion of the quartz capillary 2-3 mm above the section immersed in the hydrofluoric acid solution, and the contact amount between this portion of the quartz capillary and the hydrofluoric acid solution decreases from bottom to top. While the quartz capillary is immersed in the hydrofluoric acid solution, water is continuously injected into the quartz capillary from the end connected to the liquid injection pump using a liquid injection pump. The water flow rate is 0.01 μL / min to 10 μL / min. The injected water flows out from the end of the quartz capillary not connected to the liquid injection pump and enters the hydrofluoric acid solution. S3.2 Using a magnetic stirrer, stir at a speed not exceeding 30 revolutions per minute at the bottom of the hydrofluoric acid solution. The outer wall of the section of quartz capillary completely immersed in the hydrofluoric acid solution is uniformly corroded by the hydrofluoric acid solution. The outer wall of the section of quartz capillary above the section of quartz capillary completely immersed in the hydrofluoric acid solution is also corroded by the hydrofluoric acid solution around it, and the degree of corrosion decreases from bottom to top. S3.3 When it is observed that the quartz capillary below the hydrofluoric acid solution level is completely corroded, the tension between the hydrofluoric acid solution surface and the quartz capillary disappears, the hydrofluoric acid solution level is normal, and the contact between the hydrofluoric acid solution and the quartz capillary is completely cut off. At this time, a section of the quartz capillary with a height of 2-3 mm above the hydrofluoric acid solution level forms a perfect conical tip on its outer wall. The inner diameter of this conical tip is still equal to the inner diameter of the quartz capillary. At this time, the liquid injection pump is turned off, and water is stopped being injected into the quartz capillary. Step 4: Remove the liquid injection pump from the quartz capillary and add a hydrophobic protective layer to the tapered tip of the quartz capillary to obtain an electro-spray quartz nozzle.
2. The method for fabricating a hydrofluoric acid-based electrospray quartz nozzle according to claim 1, characterized in that... In step (1), the specific steps for selecting a quartz capillary of the appropriate specification according to the specifications of the electro-spray quartz nozzle, cutting the quartz capillary to the required length, and then removing the outer protective film of the quartz capillary are as follows: S1.
1. Using a capillary cutter, select a quartz capillary of the appropriate specification and cut it to obtain the required length of quartz capillary. S1.
2. Immerse the cut quartz capillary tube completely into a saturated sodium hydroxide solution at a temperature of 100 degrees Celsius until the saturated sodium hydroxide solution completely corrodes away the outer protective film of the quartz capillary tube. S1.3 Clean the quartz capillary tube obtained in step S1.2 with clean water and let it dry.
3. The method for fabricating a hydrofluoric acid-based electrospray quartz nozzle according to claim 1, characterized in that... In step (2), the end of the quartz capillary connected to the liquid injection pump is connected to the injection needle on the liquid injection pump via a reducing adapter.
4. The method for manufacturing an electrospray quartz nozzle based on hydrofluoric acid according to claim 1, characterized in that... The specific process of adding a hydrophobic protective layer to the conical tip of the quartz capillary in step (4) is as follows: the conical tip of the quartz capillary is immersed in the silicone waterproofing agent for 1 second and then quickly pulled out and left to stand. When the silicone waterproofing agent attached to the surface of the conical tip dries, a hydrophobic protective layer is formed on the surface of the conical tip of the quartz capillary.
Citation Information
Patent Citations
Method for preparing quartz needle by etching capillary tube by hydrofluoric acid
CN106486336A
Silicon needle array preparation method and disinfection factor generation device
CN114804014A