Methods for reducing the ion content on the surface of solder resist layer, backlight module and its manufacturing method
By subjecting the photosensitive dry film to two rounds of ultraviolet light irradiation and heat treatment, a cyclized acrylic resin solder resist layer is formed, which solves the corrosion and short circuit problems caused by ion migration in the backlight module and improves the module's service life.
Patent Information
- Application Number
- CN202210650908.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-09
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-06-09
AI Technical Summary
During manufacturing and use, backlight modules may experience corrosion, open circuits, and short circuits due to the migration of residual conductive ions, affecting their lifespan, especially with high-density LED components and small-pitch solder pads.
The photosensitive dry film is treated with ultraviolet light of different wavelengths and energies twice. First, it is pre-cured, and then cyclized acrylic resin is formed through cyclization reaction to form a solder resist layer, reducing the surface ion content. Finally, it is cured by heating.
It effectively reduces the ion content on the surface of the solder resist layer, reduces the migration of anions and cations, improves the curing degree of the solder resist layer, enhances the protective effect, and extends the service life of the backlight module.
Smart Images

Figure CN117255495B_ABST
Abstract
Description
Technical Field
[0001] This application relates to a method for reducing the ion content on the surface of a solder resist layer, a backlight module, and a method for manufacturing the same. Background Technology
[0002] Mini LEDs refer to LEDs with a chip size of approximately tens of micrometers. As a new generation of LED display technology, they can be applied to small-pitch backlight modules with a pitch of less than millimeters.
[0003] Generally, to improve light reflectivity, both sides of the backlight module need to be covered with a white photosensitive dry film. However, with the increase in LED component density and the decrease in the spacing between adjacent solder pads, problems such as corrosion, open circuits, and short circuits often occur in the backlight module during manufacturing, testing, and use due to the migration of residual conductive ions, thereby reducing the lifespan of the backlight module. Therefore, reducing the residual conductive ions on the surface of the white photosensitive dry film has become particularly important. Summary of the Invention
[0004] In view of the above, it is necessary to provide a method for reducing the ion content on the surface of the solder resist layer in order to solve the above problems.
[0005] In addition, it is necessary to provide a backlight module.
[0006] In addition, it is necessary to provide a method for manufacturing a backlight module.
[0007] A method for reducing the surface ion content of a solder resist layer includes the steps of: irradiating a photosensitive dry film with a first ultraviolet light to obtain an exposure medium, wherein the photosensitive dry film and the exposure medium comprise acrylate; irradiating the exposure medium with a second ultraviolet light, wherein the acrylate in the exposure medium undergoes cyclization to form a cyclized acrylic resin, thereby obtaining the solder resist layer, wherein the surface ion content of the solder resist layer is less than 7 × 10⁻⁶. -3 Grams per square meter. Wherein, the wavelength of the second ultraviolet light is shorter than the wavelength of the first ultraviolet light.
[0008] Furthermore, it also includes: developing the exposed body to obtain a solder resist intermediate and irradiating the solder resist intermediate with the second ultraviolet light to obtain the solder resist layer.
[0009] Furthermore, the wavelength of the first ultraviolet light is 300–480 nm, and the energy density of the first ultraviolet light is 150–650 mJ / cm². 2 The wavelength of the second ultraviolet light is 300–370 nm, and the energy density of the first ultraviolet light is 1200–1800 mJ / cm². 2 .
[0010] Furthermore, the method also includes the step of heating the solder resist layer, wherein the heating temperature is 120-180°C and the heating time is 60-80 minutes.
[0011] Furthermore, the photosensitive dry film also includes a photoinitiator, a colorant, and a filler.
[0012] A method for manufacturing a backlight module includes the following steps: providing a circuit board, the circuit board including a plurality of solder pads; forming a solder resist layer on the circuit board according to the method described above, the solder resist layer having a plurality of openings through it, the solder pads being exposed at the bottom of the openings; and forming light-emitting elements on the solder pads to obtain the backlight module.
[0013] Furthermore, before the step "depositing the light-emitting element on the solder pad", the method further includes: depositing a protective layer on the solder pad, and depositing the light-emitting element on the protective layer.
[0014] Furthermore, the circuit board includes multiple alternating conductive layers and multiple dielectric layers, the outermost conductive layer includes multiple solder pads, the circuit board has a hollow conductor, and the solder resist layer is filled into the hollow conductor.
[0015] A backlight module includes a circuit board, a solder resist layer, and multiple light-emitting components. The circuit board has multiple solder pads. The solder resist layer is disposed on the circuit board and has a through-hole, through which the solder pads are exposed at the bottom. The surface ion content of the solder resist layer is less than 7 × 10⁻⁶. -3 Grams per square meter. Multiple of the aforementioned light-emitting elements are connected to the bonding pads.
[0016] Furthermore, the light-emitting element includes an LED.
[0017] The method for reducing the surface ion content of the solder resist layer provided in this application involves cross-linking and cyclizing the acrylic resin in the photosensitive dry film through two different ultraviolet light irradiations. This cyclized acrylic resin can, on the one hand, increase the degree of cross-linking of the acrylic resin, thereby increasing the curing degree of the solder resist layer and helping to hinder the migration of anions (e.g., sulfate ions, nitrate ions, chloride ions). On the other hand, the cyclized acrylic resin has a strongly polar oxygen-containing group, which adsorbs cations (e.g., sodium ions, ammonium ions), reducing cation migration. Attached Figure Description
[0018] Figure 1 This is a cross-sectional schematic diagram of the photosensitive dry film provided in the embodiments of this application.
[0019] Figure 2 First ultraviolet light irradiation Figure 1 The diagram shows a cross-section of the photosensitive dry film.
[0020] Figure 3 For development Figure 2 The diagram shows a cross-sectional view of the photosensitive dry film after it has been used to form a solder resist intermediate.
[0021] Figure 4 Second ultraviolet light irradiation Figure 3 The diagram shows a cross-sectional view of the intermediate anti-weld material.
[0022] Figure 5 This is a cross-sectional schematic diagram of a backlight module provided in an embodiment of this application.
[0023] Figure 6 for Figure 5 A top view of the backlight module shown.
[0024] Figure 7 for Figure 1 The photosensitive dry film shown Figure 3 The solder resist intermediate shown, and Figure 4 The Fourier transform infrared spectrum of the solder resist layer is shown.
[0025] Explanation of main component symbols
[0026] Photosensitive dry film 10
[0027] Exposure Body 11
[0028] Open window 111
[0029] Intermediate anti-weld material 12
[0030] Solder resist layer 13
[0031] Circuit board 100
[0032] Conductive layer 101
[0033] Dielectric layer 102
[0034] Hollow Conductor 103
[0035] solder pad 104
[0036] Backlight module 200
[0037] Protective layer 202
[0038] Light-emitting component 203
[0039] Thickness direction D
[0040] First ultraviolet light I
[0041] Second ultraviolet light J
[0042] The following detailed description, in conjunction with the accompanying drawings, will further illustrate this application. Detailed Implementation
[0043] The technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments.
[0044] Please see Figures 1 to 4 One embodiment of this application provides a method for reducing the ion content on the surface of a solder resist layer, comprising the steps of:
[0045] S1: Please see Figure 1 A photosensitive dry film 10 is provided, the photosensitive dry film 10 comprising a photosensitive resin, a photoinitiator, a colorant, and a filler. The photosensitive resin is selected from acrylate resins and acrylates. The photoinitiator is TOP (Diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide). The colorant is selected from titanium dioxide and aluminum hydroxide. The filler is selected from diatomaceous earth, aluminum hydroxide, silica, and barium sulfate.
[0046] S2: Please see Figure 2 A portion of the photosensitive dry film 10 is irradiated with a first ultraviolet light I to form an exposure body 11. When the first ultraviolet light irradiates the photosensitive dry film 10, the photoinitiator within the photosensitive dry film 10 generates free radicals, which promote cross-linking of the photosensitive resin, thereby causing the photosensitive dry film 10 to initially cure to form the exposure body 11, wherein the exposure body 11 contains a portion of the photosensitive resin that has not undergone cross-linking.
[0047] In this embodiment, the wavelength of the first ultraviolet light I is 300–480 nm, and the energy density of the first ultraviolet light I is 150–650 mJ / cm². 2 .
[0048] S3: Please see Figure 3 The exposed body 11 is developed, causing the exposed portion of the photosensitive dry film 10 to be removed, thereby forming multiple windows 111 to obtain a solder resist intermediate 12. The solder resist intermediate 12 further includes acrylate. Specifically, developing the exposed body involves immersing and washing away the exposed portion of the photosensitive dry film 10 with a developing solution. The developing solution comprises, by weight fraction, 0.8%–5% of an alkali source, 0.05%–0.3% of a surfactant, and the balance being water. The alkali source is selected from at least one of sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, sodium hydroxide, and potassium hydroxide. The surfactant includes at least one of sodium sulfonate surfactants, sodium benzenesulfonate surfactants, sodium phosphate surfactants, ammonium chloride surfactants, potassium benzenesulfonate surfactants, or potassium phosphate surfactants.
[0049] In other embodiments of this application, depending on the specific composition of the photosensitive dry film 10, the developing solution may also remove the unexposed portion of the photosensitive dry film 10.
[0050] In other embodiments of this application, if the window 111 does not need to be formed, step S3 can be omitted.
[0051] S4: Please see Figure 4 The solder resist intermediate 12 is irradiated with a second ultraviolet light J, causing the acrylic resin in the solder resist intermediate 12 to cyclize to form a cyclized acrylic resin, thereby obtaining the solder resist layer 13. The surface ion content of the solder resist layer 13 is less than 7 × 10⁻⁶ ions, as tested by an ion contamination tester. -3 Grams per square meter. Wherein, the wavelength of the second ultraviolet light J is shorter than the wavelength of the first ultraviolet light I. Wherein, the acrylic resin undergoes a cyclization reaction under the influence of the second ultraviolet light J, the reaction formula is as follows:
[0052]
[0053] The cyclized acrylic resin can, on the one hand, increase the degree of cross-linking of the acrylic resin, thereby improving the curing degree of the solder resist layer 13 and helping to hinder the migration of anions (e.g., sulfate ions, nitrate ions, chloride ions). On the other hand, the cyclized acrylic resin has a highly polar oxygen-containing group, which adsorbs cations (e.g., sodium ions, ammonium ions), reducing cation migration.
[0054] In this embodiment, the wavelength of the second ultraviolet light J is 300–370 nm, and the energy density of the second ultraviolet light J is 1200–1800 mJ / cm². 2 That is, the energy density of the second ultraviolet light J is greater than that of the first ultraviolet light I, and the photon energy of the second ultraviolet light J is also greater than that of the first ultraviolet light I. This approach has the following two advantages: (i) the exposure of the photosensitive dry film by the low-energy first ultraviolet light I is conducive to the development process, and (ii) the exposure of the solder resist intermediate 12 by the high-energy second ultraviolet light J is conducive to the cyclization reaction.
[0055] S5: Heat the solder resist layer 13, wherein the heating temperature is 120-180°C and the heating time is 60-80 minutes, so that the solder resist layer 13 completes final curing.
[0056] This application embodiment also provides a method for manufacturing a backlight module 200, including the following steps:
[0057] S6: Please see Figure 5A circuit board 100 is provided, the circuit board 100 having a thickness direction D, the circuit board 100 including a plurality of conductive layers 101, a plurality of dielectric layers 102, and a plurality of hollow conductors 103. The conductive layers 101 and the dielectric layers 102 are alternately arranged at intervals along the thickness direction D. The outermost conductive layer 101 has a plurality of solder pads 104. The hollow conductors 103 pass through the conductive layers 101 and the dielectric layers 102 along the thickness direction D. The hollow conductors 103 connect the plurality of conductive layers 101 to achieve interlayer conductivity among the plurality of conductive layers 101.
[0058] S7: Please see Figure 5 The photosensitive dry film 10 is pressed onto the front and back outer surfaces of the circuit board 100 respectively (see Figure 1 A portion of the photosensitive dry film 10 is filled into the hollow conductive body 103. The photosensitive dry film 10 includes a first photosensitive dry film (not shown) and a second photosensitive dry film (not shown). The components and proportions of the first photosensitive dry film, by mass fraction, are: titanium dioxide, 1-5 parts; TOP, 1-5 parts; acrylic resin, 35-45 parts; acrylate resin, 5-15 parts; aluminum hydroxide, 0.1-1 part; silica, 15-25 parts; barium sulfate, 15-25 parts; and diatomaceous earth, 1-5 parts. The components and proportions of the second photosensitive dry film, by mass fraction, are: titanium dioxide, 45-55 parts; TOP, 1-5 parts; acrylic resin, 25-35 parts; acrylate resin, 5-15 parts; aluminum hydroxide, 0.1-1 part; silica, 1-5 parts; barium sulfate, 1-5 parts; and diatomaceous earth, 1-5 parts. The type and location of the photosensitive dry film 10 are selected according to Table 1.
[0059] Table 1: Selection and placement of 10 types of photosensitive dry films in three embodiments
[0060]
[0061] S8: The photosensitive dry film 10 is processed according to steps S1 to S4 to obtain a backlight module intermediate (not shown). The solder pad 104 is exposed at the bottom of the window 111.
[0062] S9: Please see Figure 5 A protective layer 202 is formed on the solder pad 104 by nickel plating.
[0063] S10: Please refer to Figure 5 and Figure 6 A light-emitting element 203, including an LED, is disposed on the protective layer 202 to obtain the backlight module 200.
[0064] In comparison, this application also provides three comparative examples. Compared with the above three embodiments, the type and placement of the photosensitive dry film in the comparative examples are the same as those in each embodiment. The difference is that each comparative example does not perform a second ultraviolet J exposure treatment on the developed solder resist intermediate 12. Ion contamination tests (see Table 2) and Fourier transform infrared spectroscopy detection (see Table 3) of the three embodiments and three comparative examples were compared and analyzed. Figure 7 ).
[0065] Table 2: Ion contamination test results of the examples and comparative examples
[0066]
[0067] By comparing and analyzing the ion contamination test results, it can be found that the total anion content on the surface of the solder resist layer 13 generally decreases after development and irradiation with the second ultraviolet light J.
[0068] Comparative analysis of Fourier transform infrared spectroscopy results revealed that after development and irradiation with the second ultraviolet light J, the wavenumber ranged from 1392 to 1417 cm⁻¹. -1 The characteristic peak height of the acrylic resin decreased, and the content of the acrylic resin decreased after the second ultraviolet light irradiation.
[0069] Please see again Figure 5 This application also provides a backlight module 200, which includes a circuit board 100, a solder resist layer 13, and a plurality of light-emitting elements 203. The surface of the circuit board 100 is provided with a plurality of solder pads 104, and the solder resist layer 13 is provided with a plurality of openings 111, with the solder pads 104 exposed at the bottom of the openings 111. The light-emitting elements 203 are disposed on the solder pads 104. The surface ion content of the solder resist layer 13 is less than 7 × 10⁻⁶. -3 Grams per square meter. The light-emitting element 203 includes LEDs.
[0070] In addition, those skilled in the art may make other changes within the spirit of this application. Of course, all such changes made in accordance with the spirit of this application should be included within the scope of protection claimed in this application.
Claims
1. A method for reducing the ion content on the surface of a solder resist layer, characterized in that, Including the following steps: A photosensitive dry film is irradiated with a first ultraviolet light to obtain an exposed body, wherein the photosensitive dry film and the exposed body comprise acrylate; cycloacrylate resin, to obtain the anti-solder layer, wherein the surface ion content of the anti-solder layer is less than 7 x 10 -3 grams per square meter, the wavelength of the second ultraviolet light being less than the wavelength of the first ultraviolet light; Develop the exposed body to obtain a solder resist intermediate; and The solder resist intermediate is irradiated with the second ultraviolet light to obtain the solder resist layer; The wavelength of the first ultraviolet light is 300~480nm, and the energy density of the first ultraviolet light is 150~650mJ / cm². 2 The wavelength of the second ultraviolet light is 300~370nm, and the energy density of the second ultraviolet light is 1200~1800mJ / cm². 2 ; The solder resist layer is heated at a temperature of 120-180°C for 60-80 minutes.
2. The method for reducing the ion content on the surface of the solder resist layer as described in claim 1, characterized in that, The photosensitive dry film also includes a photoinitiator, a colorant, and a filler.
3. A method for manufacturing a backlight module, characterized in that, Including the following steps: A circuit board is provided, the circuit board including a plurality of solder pads; The solder resist layer is provided on the circuit board. The solder resist layer is prepared by the method as described in claim 1 or 2. The solder resist layer is provided with a plurality of openings, and the solder pads are exposed at the bottom of the openings. A light-emitting element is disposed on the solder pad to obtain the backlight module.
4. The manufacturing method as described in claim 3, characterized in that, The step of "providing the light-emitting element on the solder pad" includes the following steps before: A protective layer is provided on the solder pad, and The light-emitting element is disposed on the protective layer.
5. The manufacturing method as described in claim 3, characterized in that, The circuit board includes multiple alternating conductive layers and multiple dielectric layers. The outermost conductive layer includes multiple solder pads. The circuit board has a hollow conductor, and the solder resist layer is filled into the hollow conductor.
Citation Information
Patent Citations
Photosensitive resin composition, solder resist film using said photosensitive resin composition, flexible printed wiring board, and image display device
CN110268323A