By using opposite electrical ion implantation in shielded gate power semiconductor devices to form depletion-promoting layers and stepped trench designs, the problems of insufficient electric field distribution and polysilicon missing regions are solved, and higher breakdown voltage and lower on-resistance.

CN117334579BActive Publication Date: 2024-11-01SHANGHAI JUNYI INFORMATION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311392824.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-10-25
Publication Date
2024-11-01
Estimated Expiration
2043-10-25

AI Technical Summary

Technical Problem

Existing shielded gate power semiconductor devices have problems such as insufficient peak electric field and gap formation during the electric field distribution and polysilicon filling process, resulting in high on-resistance and leakage.

Method used

The depletion-promoting layer is formed by using opposite electrical ion implantation in the epitaxial layer, the sidewall doping concentration is reduced, and a stepped trench design is adopted to reduce the formation of polysilicon defect regions.

Benefits of technology

It effectively improves the electric field distribution, reduces the on-resistance, and avoids the formation of polysilicon defect regions, thereby increasing the breakdown voltage and filling difficulty of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117334579B_ABST
    Figure CN117334579B_ABST
Patent Text Reader

Abstract

The present invention discloses a shielded gate power semiconductor device and a manufacturing method thereof, comprising the following steps: preparing a substrate, forming an epitaxial layer on the substrate, then etching to form a first groove, then etching to form a second groove, wherein the first groove and the second groove together form a stepped groove; removing the first hard mask layer, generating an oxidation protection layer by thermal oxidation; forming a depletion-promoting layer by ion implantation of opposite electrical properties; removing the oxidation protection layer; forming a field oxide layer, a shielded gate polysilicon, a shielded gate oxide layer, a gate polysilicon and a gate oxide layer in the stepped groove. The present invention forms a depletion-promoting layer by ion implantation of opposite electrical properties in the epitaxial layer, which can effectively reduce the doping concentration of the side wall, change its internal electric field distribution, and is more conducive to reverse depletion. Based on the application of the present invention, the overall doping concentration of the epitaxial layer can be set higher, so the on-resistance of the power semiconductor device can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of semiconductor technology, and in particular relates to a shielded gate power semiconductor device and a manufacturing method thereof. Background Art

[0002] At present, in semiconductor device technology, shielded-gate trench MOSFET (SGT-MOSFET) introduces horizontal depletion on the basis of vertical depletion of PN junction compared with traditional trench MOSFET, changing the device electric field from triangular distribution to approximately rectangular distribution. Under the condition of using epitaxial material specifications with the same doping concentration, the device can obtain a higher breakdown voltage. At the same time, the introduction of the shielded gate structure can greatly reduce the Miller capacitance of MOSFET, which helps to reduce the switching loss during the period.

[0003] In the prior art, there are processes for preparing shielded gate power semiconductor devices, such as Figures 1A to 1G As shown, the existing manufacturing process of the stepped trench semiconductor device includes the following steps:

[0004] Prepare a substrate 1, form an epitaxial layer 2 on the substrate 1, and form a thin oxide layer 3 and a hard mask layer 4 on the epitaxial layer 2. Figure 1A As shown;

[0005] The epitaxial layer 2, the thin oxide layer 3 and the hard mask layer 4 are etched to form a trench 5, and the thin oxide layer 3 and the hard mask layer 4 are removed. Figure 1B As shown;

[0006] A field oxide layer 6 is formed on the surface of the epitaxial layer 2 and the sidewalls and bottom of the trench 5. Figure 1C As shown;

[0007] Depositing the first polysilicon 7 to fill the trench 5, Figure 1D As shown,

[0008] The first polysilicon 7 is etched back to form a shielding gate polysilicon 7-1, and the exposed field oxide layer 6 is removed. Figure 1E As shown (here only the active area trench is back-etched, and those skilled in the art can learn the relevant processing methods of the terminal area trench from other relevant technical documents);

[0009] The oxide layer is regrown and thinned back to form a shielding gate oxide layer 6-1 above the shielding gate polysilicon 7-1. Figure 1F As shown;

[0010] Continue to form a gate oxide layer 6-2 on the sidewall of the trench 5 above the shielding gate oxide layer 6-1, then refill the trench 5 with the second polysilicon, and then etch back to form a gate polysilicon 7-2, as shown in FIG. Figure 1GAs shown;

[0011] Regarding the subsequent processes of other sources and drains, according to the differences in performance requirements of semiconductor devices, technicians in this field can learn the relevant processing methods from other relevant technical documents, which will not be repeated here.

[0012] In the prior art, there are the following problems:

[0013] 1) In the traditional SGT structure, such as Figure 2A As shown, the electric field has two peaks a and c, and the middle part b needs to be improved. Only epitaxy with a lighter concentration can be used to achieve the target breakdown voltage, but this cannot achieve a smaller on-resistance. Figure 2B Shows Figure 2A The positions a, b, and c correspond to the specific depth positions of the semiconductor device;

[0014] 2) When the depth-width ratio of conventional SGT trenches is relatively large, gaps are easily generated during the polysilicon filling process. In the subsequent thermal process, the gaps are easily aggregated to form polysilicon missing areas. When the polysilicon missing areas appear on the field oxide sidewalls, leakage will occur. Summary of the invention

[0015] In view of this, the purpose of the present invention is to provide a shielded gate power semiconductor device and a method for manufacturing the same. By forming a depletion-promoting layer in the epitaxial layer through ion implantation of opposite electrical properties, the doping concentration of the side walls can be effectively reduced, and the internal electric field distribution can be changed, which is more conducive to reverse depletion. Based on the application of the present invention, the overall doping concentration of the epitaxial layer can be set higher, thereby reducing the on-resistance of the power semiconductor device.

[0016] To achieve the above object, the present invention provides a method for manufacturing a shielded gate power semiconductor device, comprising the following steps:

[0017] A substrate is prepared, an epitaxial layer is formed on the substrate, a first hard mask layer having a first trench opening is formed on the epitaxial layer, and then a first trench is formed by etching, the first trench opening is expanded into a second trench opening by etching, and then a second trench is formed by etching, wherein the depth of the second trench is smaller than that of the first trench, and the first trench and the second trench together form a stepped trench;

[0018] removing the first hard mask layer and generating an oxidation protection layer by thermal oxidation;

[0019] Forming a depletion-promoting layer in the epitaxial layer adjacent to the oxidation protection layer by ion implantation of opposite electrical polarity;

[0020] Remove the protective oxide layer;

[0021] A field oxide layer, a shielding gate polysilicon, a shielding gate oxide layer, a gate polysilicon and a gate oxide layer are formed in the stepped trench.

[0022] Preferably, forming a field oxide layer, a shielding gate polysilicon, a shielding gate oxide layer, a gate polysilicon and a gate oxide layer in the stepped trench specifically comprises the following steps:

[0023] Generating a field oxide layer in the stepped trench and on the surface of the epitaxial layer;

[0024] Filling the first polysilicon in the stepped trench and on the surface of the epitaxial layer;

[0025] etching back the first polysilicon to form the shielding gate polysilicon;

[0026] removing the exposed field oxide layer;

[0027] After deposition through the HDP process and etching back, a shielding gate oxide layer is formed on the shielding gate polysilicon;

[0028] A gate oxide layer is formed by thermally oxidizing the sidewalls of the second trench over the shielding gate oxide layer.

[0029] The second trench and the surface of the epitaxial layer are filled with second polysilicon, and the second polysilicon is etched back to form the gate polysilicon.

[0030] Preferably, the epitaxial layer includes a first epitaxial layer and a second epitaxial layer, the second epitaxial layer is located above the first epitaxial layer, the doping concentration of the second epitaxial layer is higher than the doping concentration of the first epitaxial layer, and the thickness of the second epitaxial layer is less than the depth of the second trench.

[0031] On the other hand, the present invention discloses a shielded gate power semiconductor device, comprising an epitaxial layer, a stepped groove arranged on a surface of the epitaxial layer, a stepped field oxide layer arranged along the side wall of the stepped groove, and a depletion-promoting layer arranged outside the field oxide layer, wherein shielding gate polysilicon, shielding gate oxide layer, gate polysilicon and gate oxide layer are arranged in the stepped groove, the effective doping electrical property of the depletion-promoting layer is the same as the doping electrical property of the epitaxial layer, and the effective doping concentration of the depletion-promoting layer is lower than the doping concentration of the epitaxial layer.

[0032] Preferably, the shielding gate polysilicon is arranged at the bottom and the step portion of the stepped trench, the shielding gate oxide layer is arranged above the shielding gate polysilicon, the gate polysilicon is arranged above the shielding gate oxide layer, the gate oxide layer is arranged on the side walls of the stepped trench at a depth corresponding to the gate polysilicon, and the field oxide layer is arranged on the side walls and bottom walls of the stepped trench at a depth corresponding to the shielding gate polysilicon.

[0033] Preferably, the shielded gate power semiconductor device is a shielded gate trench field effect transistor.

[0034] Preferably, the shielded gate power semiconductor device is manufactured using the above-mentioned manufacturing method.

[0035] The beneficial effects of the present invention are:

[0036] (1) The present invention forms a depletion-promoting layer in the epitaxial layer by ion implantation of opposite electrical properties, which can effectively reduce the doping concentration of the sidewalls and change the internal electric field distribution, which is more conducive to reverse depletion. Based on the application of the present invention, the overall doping concentration of the epitaxial layer can be set higher, thereby reducing the on-resistance of the power semiconductor device;

[0037] (2) The present invention generates an oxidation protection layer before ion implantation, which can effectively prevent ion implantation from damaging the surface of the epitaxial layer and also plays a sacrificial oxidation role, thereby repairing etching damage;

[0038] (3) The trench width of the present invention is designed to be larger at the top and smaller at the bottom. When the trench depth and width are relatively large, the difficulty of filling polysilicon can be greatly reduced, and the formation of polysilicon missing areas can be avoided. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0040] Figures 1A to 1G A schematic diagram of a process for preparing a shielded gate power semiconductor device in the prior art;

[0041] FIG. 2A to FIG. 2B It is a schematic diagram of the electric field distribution of the SGT structure in the prior art;

[0042] Figures 3A to 3P It is a schematic diagram of a flow chart of an embodiment of the present invention;

[0043] FIG. 4A to FIG. 4B This is a comparison diagram of the effects of the embodiment of the present invention and the prior art;

[0044] in:

[0045] 1 substrate; 2 epitaxial layer; 2-1 first epitaxial layer; 2-2 second epitaxial layer; 3 thin oxide layer; 4 hard mask layer; 5 trench; 5-1 first trench; 5-2 second trench; 5-3 stepped trench; 6 field oxide layer; 6-1 shielding gate oxide layer; 6-2 gate oxide layer; 7 polysilicon; 7-1 shielding gate polysilicon; 7-2 gate polysilicon; 8 oxidation protection layer; 9 depletion-promoting layer. DETAILED DESCRIPTION

[0046] The core of the present invention is to provide a shielded gate power semiconductor device and a method for manufacturing the same. By forming a depletion-promoting layer in the epitaxial layer through ion implantation of opposite electrical properties, the doping concentration of the side wall can be effectively reduced, and the internal electric field distribution can be changed, which is more conducive to reverse depletion. Based on the application of the present invention, the overall doping concentration of the epitaxial layer can be set higher, thereby reducing the on-resistance of the power semiconductor device.

[0047] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0048] Embodiment 1

[0049] Figures 3A to 3P A shielded gate power semiconductor device and a manufacturing method thereof provided in this embodiment are shown, comprising the following steps:

[0050] S1: prepare a substrate 1, form a first epitaxial layer 2-1 and a second epitaxial layer 2-2 on the substrate 1, the second epitaxial layer 2-2 is located above the first epitaxial layer 2-1, the doping concentration of the second epitaxial layer 2-2 is higher than the doping concentration of the first epitaxial layer 2-1, form a first hard mask layer 4-1 with a first trench opening on the second epitaxial layer 2-2, then etch to form a first trench 5-1, expand the first trench opening to a second trench opening by etching, then etch to form a second trench 5-2, the depth of the second trench 5-2 is less than the first trench 5-1, the depth of the second trench 5-2 is greater than the thickness of the second epitaxial layer 2-2, the first trench 5-1 and the second trench 5-2 together form a stepped trench 5-3, such as FIG. 3A to FIG. 3D In some other embodiments, those skilled in the art can set the layering position of the epitaxial layer and the relationship between the doping concentration of each layer according to actual needs, which is not limited here.

[0051] S2: removing the first hard mask layer and generating an oxidation protection layer 8 by thermal oxidation, such as FIG. 3E to FIG. 3FAs shown, the oxidation protection layer 8 is used to prevent ion implantation from damaging the surface of the epitaxial layer, and also plays a sacrificial oxidation role, which is removed in step S4 to repair the etching damage.

[0052] S3: by ion implantation of opposite electrical properties, a depletion-promoting layer 9 is formed in the epitaxial layer (including the first epitaxial layer 2-1 and the second epitaxial layer 2-2) adjacent to the oxidation protection layer 8, such as Figure 3G Specifically, when the epitaxial layers are all doped with N-type ions, this step is P-type ion implantation, thereby reducing the effective doping concentration of the depletion-promoting layer 9 (ie, forming an N- depletion-promoting layer on the N- epitaxial layer), and vice versa.

[0053] S4: removing the oxide protection layer 8, such as Figure 3H shown.

[0054] S5: Generate a field oxide layer 6 in the stepped trench 5-3 and on the surface of the epitaxial layer, such as Fig. 3I shown.

[0055] S6: Fill the first polysilicon 7 in the stepped trench 5-3 and on the surface of the epitaxial layer, such as Figure 3J shown.

[0056] S7: Etching back the first polysilicon 7 to form shielding gate polysilicon 7-1, such as Figure 3K As shown:

[0057] S8: removing the exposed field oxide layer 6, such as Figure 3L shown.

[0058] S9: After HDP process deposition and back etching, a shielding gate oxide layer 6-1 is formed on the shielding gate polysilicon 7-1, such as Figure 3M to Figure 3N shown.

[0059] S10: Forming a gate oxide layer 6-2 on the sidewall of the second trench 5-2 above the shielding gate oxide layer 6-1 by thermal oxidation. Fig.3O As shown;

[0060] S11: Fill the second polysilicon in the second trench 5-2 and on the surface of the epitaxial layer, and etch back the second polysilicon to form gate polysilicon 7-2, such as Figure 3P shown.

[0061] On the other hand, this embodiment discloses a shielded gate power semiconductor device, such as Figure 3PAs shown, the shielded gate power semiconductor device includes an epitaxial layer, a stepped groove 5-3 arranged on a surface of the epitaxial layer, a stepped field oxide layer 6 arranged along the sidewall of the stepped groove 5-3, and a depletion-promoting layer 9 arranged outside the field oxide layer. The stepped groove 5-3 is provided with a shielding gate polysilicon 7-1, a shielding gate oxide layer 6-1, a gate polysilicon 7-2 and a gate oxide layer 6-2. The shielding gate polysilicon 7-1 is arranged at the bottom and the stepped portion of the stepped groove 5-3. The oxide layer 6-1 is arranged above the shielding gate polysilicon 7-1, the gate polysilicon 7-2 is arranged above the shielding gate oxide layer 6-1, the gate oxide layer 6-2 is arranged on the sidewalls of the stepped trench of the corresponding depth of the gate polysilicon 7-2, the field oxide layer 6 is arranged on the sidewalls and bottom walls of the stepped trench of the corresponding depth of the shielding gate polysilicon 7-1, the effective doping electrical property of the depletion-promoting layer 9 is the same as the doping electrical property of the epitaxial layer, and the effective doping concentration of the depletion-promoting layer 9 is lower than the doping concentration of the epitaxial layer. The shielding gate power semiconductor device can be manufactured by the above manufacturing method.

[0062] The shielded gate power semiconductor device of this embodiment is described by taking a shielded gate trench field effect transistor device as an example. In some other embodiments, this is not used as a limitation.

[0063] As shown in Table 1, Figure 4A and Figure 4B As shown, compared with the conventional technology, the shielded gate power semiconductor device of this embodiment reduces the on-resistance of the power semiconductor device and also improves the breakdown voltage of the power semiconductor device.

[0064] Table 1

[0065]

[0066]

[0067] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0068] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for manufacturing a shielded gate power semiconductor device, characterized in that: The steps include: A substrate is prepared, an epitaxial layer is formed on the substrate, a first hard mask layer having a first trench opening is formed on the epitaxial layer, and then a first trench is formed by etching, the first trench opening is expanded into a second trench opening by etching, and then a second trench is formed by etching, wherein the depth of the second trench is smaller than that of the first trench, and the first trench and the second trench together form a stepped trench; removing the first hard mask layer and generating an oxidation protection layer by thermal oxidation; Forming a depletion-promoting layer in the epitaxial layer adjacent to the oxidation protection layer by ion implantation of opposite electrical polarity; Remove the protective oxide layer; forming a field oxide layer, a shielding gate polysilicon, a shielding gate oxide layer, a gate polysilicon and a gate oxide layer in the stepped trench; The epitaxial layer includes a first epitaxial layer and a second epitaxial layer, the second epitaxial layer is located above the first epitaxial layer, the doping concentration of the second epitaxial layer is higher than the doping concentration of the first epitaxial layer, and the thickness of the second epitaxial layer is less than the depth of the second trench; The shielding gate polysilicon is arranged at the bottom and the step portion of the stepped trench.

2. The method according to claim 1, characterized in that: The step of forming a field oxide layer, a shielding gate polysilicon, a shielding gate oxide layer, a gate polysilicon and a gate oxide layer in the stepped trench specifically comprises the following steps: Generating a field oxide layer in the stepped trench and on the surface of the epitaxial layer; Filling the first polysilicon in the stepped trench and on the surface of the epitaxial layer; etching back the first polysilicon to form the shielding gate polysilicon; removing the exposed field oxide layer; After deposition through the HDP process and etching back, a shielding gate oxide layer is formed on the shielding gate polysilicon; A gate oxide layer is formed by thermally oxidizing the sidewalls of the second trench over the shielding gate oxide layer. The second trench and the surface of the epitaxial layer are filled with second polysilicon, and the second polysilicon is etched back to form the gate polysilicon.

3. A shielded gate power semiconductor device, characterized in that: It comprises an epitaxial layer, a stepped trench arranged on a surface of the epitaxial layer, a stepped field oxide layer arranged along the sidewall of the stepped trench, and a depletion-promoting layer arranged outside the field oxide layer, wherein shielding gate polysilicon, shielding gate oxide layer, gate polysilicon and gate oxide layer are arranged in the stepped trench, the effective doping electrical property of the depletion-promoting layer is the same as the doping electrical property of the epitaxial layer, and the effective doping concentration of the depletion-promoting layer is lower than the doping concentration of the epitaxial layer; The epitaxial layer includes a first epitaxial layer and a second epitaxial layer, the second epitaxial layer is located above the first epitaxial layer, the doping concentration of the second epitaxial layer is higher than the doping concentration of the first epitaxial layer, and the thickness of the second epitaxial layer is less than the depth of the second trench; The shielding gate polysilicon is arranged at the bottom and the step portion of the stepped trench, the shielding gate oxide layer is arranged above the shielding gate polysilicon, the gate polysilicon is arranged above the shielding gate oxide layer, the gate oxide layer is arranged on the side walls of the stepped trench of the corresponding depth of the gate polysilicon, and the field oxide layer is arranged on the side walls and bottom walls of the stepped trench of the corresponding depth of the shielding gate polysilicon.

4. The shielded gate power semiconductor device according to claim 3, characterized in that: The shielded gate power semiconductor device is a shielded gate trench field effect transistor.

5. The shielded gate power semiconductor device according to claim 3, characterized in that: The shielded gate power semiconductor device is manufactured by the manufacturing method according to any one of claims 1 to 2.