A stress corrosion experimental device for polar environments

By using the hot end and cold end of the semiconductor refrigeration chip to work simultaneously in the polar environment stress corrosion experimental device, combined with the neural network fuzzy controller and PID controller, the stable temperature adjustment and the improvement of heat dissipation efficiency are achieved, solving the existing problem. The problem of temperature instability and vibration noise in the technology meets the experimental needs of multi-factor coupling in polar environment.

CN117367941BActive Publication Date: 2024-10-18JIANGSU UNIV OF SCI & TECH
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202311510549.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-14
Publication Date
2024-10-18
Estimated Expiration
2043-11-14

AI Technical Summary

Technical Problem

Existing polar environment stress corrosion experimental equipment has problems such as temperature instability, loud vibration and noise, unstable experimental equipment, and limited selectivity of low-temperature media in low-temperature environments, making it difficult to implement multi-factor coupling experiments.

Method used

A polar environment stress corrosion experimental device including a low-temperature environment box, a low-temperature medium box and a corrosive medium box is designed. The hot end and cold end of the semiconductor refrigeration piece are used to work simultaneously, and real-time monitoring of temperature is achieved through the heating system and temperature control unit. and adjustment, combining the neural network fuzzy controller and PID controller, using thermal conductive silicone grease and cooling fans to improve heat dissipation efficiency, and allowing the use of solid or gaseous low-temperature media.

Benefits of technology

It achieves the stability of the temperature in the corrosive medium box, simulates the operating environment of polar equipment, reduces external influences, improves the stability of the experimental device and the selectivity of low-temperature media, solves the problem of vibration and noise, enhances the refrigeration capacity, and meets the requirements Experimental requirements for multi-factor coupling effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117367941B_ABST
    Figure CN117367941B_ABST
Patent Text Reader

Abstract

The invention discloses a stress corrosion experimental device for polar environment, comprising a low temperature environment box, a low temperature medium box located in the low temperature environment box and containing a low temperature medium, a corrosive medium box located in the low temperature medium box and used for placing a sample and containing a corrosive medium, and a heating system located on the side walls of the corrosive medium box and the low temperature medium box, wherein the heating system comprises a first heat dissipation component, a semiconductor cooling sheet and a second heat dissipation component stacked in sequence from the inside to the outside, wherein the hot end of the semiconductor cooling sheet provides heat to the corrosive medium box through the first heat dissipation component, and the cold end of the semiconductor cooling sheet provides cold to the low temperature environment box through the second heat dissipation component. The cold end and the hot end of the semiconductor cooling sheet of the invention work simultaneously, so that the temperature in the low temperature environment box is much lower than the temperature of the outside air, reducing the influence of the outside high temperature environment on the low temperature medium, so that the temperature of the low temperature medium remains relatively stable, thereby ensuring the stability of the experimental temperature in the corrosive medium box.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of stress corrosion, and in particular to a stress corrosion experimental device for polar environments. Background Art

[0002] Stress corrosion is a material destruction process caused by the combined effects of strain and corrosion caused by residual or applied stress. Stress corrosion cracking refers to the phenomenon that materials under stress produce delayed cracking or even delayed fracture in a specific corrosive environment. The polar regions are rich in oil and gas resources and polar waterway resources, but the operating environment of polar equipment is harsh and complex. Polar equipment will experience stress corrosion under the coupling of multiple factors such as corrosive environment, ambient temperature and operating load.

[0003] At present, most experiments that require low-temperature environments are temperature-controlled through cryogenic boxes. Cryogenic boxes are external equipment and are large in size. At the same time, cryogenic boxes are in a closed state when working, and cannot be used in conjunction with universal testing machines, making it difficult to complete low-temperature stress corrosion experiments under the coupling of multiple factors. There are also smaller cryogenic boxes on the market. Unlike the compressor refrigeration of large cryogenic boxes, small cryogenic boxes use semiconductor refrigeration chips for refrigeration. Semiconductor refrigeration chips have cold ends and hot ends. After the semiconductor refrigeration chips are powered on, both ends work at the same time. Therefore, this type of cryogenic box can only use the cold end of the semiconductor refrigeration chip for refrigeration, and cannot use the heating function of the hot end of the semiconductor refrigeration chip to carry out production work at the same time. It is even necessary to consider solving the heat dissipation problem of the semiconductor refrigeration chip, because under the same control conditions, the higher the heat dissipation efficiency of the hot end of the semiconductor refrigeration chip, the lower the temperature that the cold end can reach. However, even if the heat dissipation problem is solved, it is difficult for semiconductor refrigeration chips to achieve ultra-low temperatures such as in polar environments due to their own refrigeration capacity.

[0004] In addition to refrigeration through a cryogenic box, a low-temperature constant-temperature water bath device can also be used to meet the low-temperature requirements of the experiment. The prior art (CN110646314A) uses the low-temperature medium in the low-temperature circulation box to refrigerate, so that the space in the sample loading module at the bottom of the environmental simulation box reaches the experimental temperature. In addition, the low-temperature circulation box is connected to the external device low-temperature constant-temperature bath through two low-temperature circulation pipes. After the low-temperature medium reaches a low-temperature constant-temperature state under the action of the low-temperature constant-temperature bath, the low-temperature medium is introduced into the low-temperature circulation box through the low-temperature circulation pipe, and the low-temperature medium is returned to the low-temperature constant-temperature bath through another low-temperature circulation pipe. However, the low-temperature circulation box in the patent will inevitably be affected after being connected to the low-temperature thermostatic bath of the external device through the low-temperature circulation pipe. The working principle of the low-temperature thermostatic bath is similar to that of the low-temperature box. Both are refrigerated by the compressor. When the compressor is refrigerating, it will generate large vibration and noise. Therefore, the overall experimental device of the patent will resonate due to the operation of the low-temperature circulation tank. The vibration of the experimental device will affect the experiment. For example, when conducting stress corrosion related experiments, the pins that fix the sample may fall off, resulting in the failure of the experiment. In addition, some experiments require the operator to supervise and guard. The noise generated by the low-temperature thermostatic bath is not conducive to human physical and mental health. At the same time, the inflow and outflow of the low-temperature medium in the low-temperature circulation box will exert force on the side wall of the low-temperature circulation box, which may cause the overall experimental device to shake left and right. In summary, the patent cannot guarantee the stability of the overall experimental device, thereby affecting the experiment. At the same time, the noise generated by the external equipment endangers the physical and mental health of the human body, and requires that the low-temperature medium must be a liquid low-temperature medium with high fluidity. Only a liquid low-temperature medium with high fluidity can achieve a circulating flow state in the low-temperature circulation box and the low-temperature thermostatic bath, which greatly limits the selectivity of the low-temperature medium.

[0005] Therefore, it is urgent to solve the above problems. Summary of the invention

[0006] Purpose of the invention: The purpose of the present invention is to provide a stress corrosion test device for polar environments that can effectively ensure the experimental temperature stability in the corrosive medium box.

[0007] Technical solution: To achieve the above objectives, the present invention discloses a stress corrosion experimental device for polar environments, comprising a low-temperature environment box, a low-temperature medium box located in the low-temperature environment box and containing a low-temperature medium, a corrosive medium box located in the low-temperature medium box and used for placing a sample and containing a corrosive medium, and a heating system located on the corrosive medium box and the side walls of the low-temperature medium box, wherein the heating system comprises a first heat dissipation component, heat insulation cotton, a semiconductor refrigeration sheet and a second heat dissipation component stacked in sequence from the inside to the outside, wherein the hot end of the semiconductor refrigeration sheet supplies heat to the corrosive medium box through the first heat dissipation component, and the cold end of the semiconductor refrigeration sheet supplies cooling to the low-temperature environment box through the second heat dissipation component.

[0008] Among them, the heating system also includes a temperature sensor and a temperature control unit arranged in the corrosive medium box. The temperature sensor monitors the temperature in the corrosive medium box in real time, and transmits the monitored temperature data to the temperature control unit for processing and analysis. The output signal of the temperature control unit controls the heating of the hot end of the semiconductor refrigeration plate.

[0009] Preferably, the temperature control unit includes a neural network fuzzy controller and a PID controller, the neural network fuzzy controller includes a first calculation module and a PID parameter acquisition module, the first calculation module is used to obtain the temperature error e(t) and the error change rate ec between the expected temperature and the measured temperature in the corrosive medium box, and the PID parameter acquisition module is used to perform neural network fuzzification, neural network fuzzy reasoning and neural network clarification on the error e and the error change rate ec to obtain the real-time adjusted PID control parameter change ΔK p , ΔK i and ΔK d , and then the initial PID control parameter K p0 , K i0 and K d0 Add the PID control parameter change to get the real-time PID control parameter K p , K i and K d , and set the PID control parameter K p , K i and K d The data is transmitted to the PID controller to control the heating of the hot end of the semiconductor refrigeration plate.

[0010] Furthermore, the PID parameter acquisition module takes the temperature error e(t) and the error change rate ec as input variables, and defines the basic domain of the input variable e(t) as [e l ,e h ], the fuzzy domain is [-p e ,p e ], the quantization factor is Define the basic domain of the input variable ec as [ec l ,ec h ], the fuzzy domain is [-p ec ,p ec ], the quantization factor is The PID control parameter change ΔK p , ΔK i and ΔK d As the output variable, the basic domain of the output variable is defined as [ΔK l ,ΔK h ], ΔK p The fuzzy domain is [-m p ,m p ], the quantization factor is ΔK i The fuzzy domain is [-m i ,m i ], the quantization factor is ΔK d The fuzzy domain is [-m d ,m d ], the quantization factor is The fuzzy subsets of input variables and output variables are set to seven levels: NB, NM, NS, ZO, PS, PM and PB, and Gaussian function is used as the membership function. Fuzzy control performs fuzzy reasoning according to the fuzzy rule table to obtain the fuzzy subsets of output variables. After clarification processing, the output control quantity is obtained.

[0011] Furthermore, the neural network structure of the PID parameter acquisition module consists of an input layer, a fuzzification layer, a fuzzy reasoning layer, and an output layer. The function of the input layer is to input the temperature error e(t) and the error change rate ec. Its function expression is:

[0012] f1(T i )=T i (i=1,2)

[0013] Where, T1 = e(t), T2 = ec;

[0014] The fuzzy layer fuzzifies the input variables, creates fuzzy subsets of the input variables, and selects the Gaussian function as its membership function. Its function expression is:

[0015]

[0016] Where c ij is the middle value of the Gaussian membership function, b ij is the basis width of the Gaussian membership function;

[0017] The fuzzy reasoning layer performs fuzzy reasoning according to the fuzzy rule table, and its function expression is:

[0018]

[0019]

[0020] Where f3(i,j) is the fuzzy inference function, N i is the level number of the fuzzy subset of the input variable;

[0021] The output layer clarifies the fuzzy quantity after fuzzy reasoning and obtains the PID control parameter change ΔK P , ΔK i and ΔK d , its function expression is:

[0022]

[0023] Where w is the conversion weight;

[0024] Finally, the initial PID control parameter K p0 , K i0 and K d0 Add the PID control parameter change to get the real-time PID control parameter K p , K i and K d .

[0025] Preferably, the PID controller controls the hot end heating of the semiconductor refrigeration plate according to the temperature error information and the PID control parameters, and its function expression is:

[0026]

[0027] Where u(t) is the output of the PID controller, K p is the PID proportional control parameter, K i is the PID integral control parameter, K d is the PID differential control parameter.

[0028] Furthermore, the first heat dissipation component includes a first heat dissipation block connected to the hot end of the semiconductor refrigeration plate through thermal grease and semiconductor refrigeration plate bonding glue, and a first heat dissipation fan fixed to the first heat dissipation block with one side of the fin facing the corrosive medium box.

[0029] Furthermore, the second heat dissipation component includes a second heat dissipation block connected to the cold end of the semiconductor refrigeration plate through thermal grease and semiconductor refrigeration plate bonding glue, and a second heat dissipation fan fixed to the second heat dissipation block with one side of the fin facing the low temperature environment box.

[0030] Preferably, the periphery of the semiconductor refrigeration plate is covered with thermal insulation cotton.

[0031] Furthermore, the cryogenic medium box is provided with a conduit for introducing and discharging liquid cryogenic medium, and the conduit is provided with a switch valve.

[0032] Beneficial effects: Compared with the prior art, the present invention has the following significant advantages:

[0033] (1) The cold source of the corrosive medium box of the present invention is a low-temperature medium, and the heat source is a hot end of a semiconductor refrigeration chip. The low-temperature medium is used to create an ultra-low temperature environment in the corrosive medium box, and the hot end of the semiconductor refrigeration chip is used to adjust and maintain the temperature in the corrosive medium box. The cold end of the semiconductor refrigeration chip works as a cold source of the low-temperature environment box and works simultaneously with the hot end of the semiconductor refrigeration chip, so that the temperature in the low-temperature environment box is much lower than the temperature of the outside air, reducing the influence of the outside high-temperature environment on the low-temperature medium, so that the temperature of the low-temperature medium remains relatively stable, thereby ensuring the stability of the experimental temperature in the corrosive medium box;

[0034] (2) The present invention can simulate the real environment of polar equipment operation, add different corrosive media into the corrosive medium box as needed, and provide different experimental loads by the universal testing machine, thereby realizing stress corrosion experiment of the sample under the coupling effect of multiple factors such as corrosive environment, ambient temperature and operating load;

[0035] (3) The cold source of the corrosive medium box in the present invention is a low-temperature medium, and the heat source is the hot end of the semiconductor refrigeration sheet. The low-temperature medium is used to create an ultra-low temperature environment in the corrosive medium box, and the hot end of the semiconductor refrigeration sheet is used to adjust and maintain the temperature in the corrosive medium box. This solves the problem that the semiconductor refrigeration sheet is limited by its own refrigeration capacity and is difficult to achieve ultra-low temperatures in polar environments. At the same time, the present invention fully utilizes the hot and cold ends of the semiconductor refrigeration sheet for production work, solving the problem that only the cold end of the semiconductor refrigeration sheet can be used for cooling in a small low-temperature box, but the heating function of the hot end of the semiconductor refrigeration sheet cannot be used for production work;

[0036] (4) The cold source of the corrosion medium box in the present invention is the cryogenic medium in the cryogenic medium box. The cryogenic medium box in the present invention is not connected to external equipment such as a cryogenic constant temperature bath, and there is no problem of the flow of liquid cryogenic medium in the cryogenic medium box causing the experimental device to shake. The present invention can also use solid or gaseous cryogenic media for cooling, such as solid carbon dioxide (dry ice), etc.; the vibration and noise problems generated when the experimental device in the comparative document is working are solved, and the selectivity of the cryogenic medium is greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is a schematic diagram of the process of the present invention;

[0038] Figure 2 It is a schematic diagram of the framework of the temperature control unit in the present invention;

[0039] Figure 3 It is a structural schematic diagram of the neural network fuzzy controller in the present invention;

[0040] Figure 4 It is a front view schematic diagram of the present invention;

[0041] Figure 5It is a structural schematic diagram of the present invention;

[0042] Figure 6 It is an explosion schematic diagram of the present invention;

[0043] Figure 7 It is a schematic diagram of the structure of the corrosive medium box, the low-temperature medium box and some devices of the heating system in the present invention. DETAILED DESCRIPTION

[0044] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.

[0045] like Figure 5 and Figure 6 As shown, the stress corrosion experimental device for polar environment in the present invention comprises a corrosive medium box 1, a low temperature medium box 2, a low temperature environment box 3 and a heating system, wherein the corrosive medium box 1, the low temperature medium box 2 and the low temperature environment box 3 are sequentially arranged from the inside to the outside, and the innermost corrosive medium box 1 comprises a detachable corrosive medium box cover 4, and a circular hole 10 is opened on the corrosive medium box cover 4, and a fixture mounting hole 8 is provided on the bottom of the corrosive medium box 1 and the corrosive medium box cover 4, and a heating system mounting hole 11 is provided on the upper right side of the corrosive medium box 1. Figure 4As shown, the cryogenic medium box 2 located in the middle layer includes a detachable cryogenic medium box cover 5, and a conduit 7 is provided on the bottom of the cryogenic medium box 2 and the cryogenic medium box cover 5. The conduit 7 is provided with a switch valve. The cryogenic medium box 2 contains ultra-low temperature cryogenic medium, and the cryogenic medium is used to create a low-temperature environment in the corrosive medium box 1. The cryogenic medium is a low-temperature object such as silicone oil or anhydrous ethanol, wherein silicone oil is a colorless, odorless, non-toxic, non-volatile liquid, and the freezing point of silicone oil is low, and its freezing point can reach minus 70°C, and the freezing point of anhydrous ethanol is as high as minus 114°C. The conduit 7 is used to pass in and out the liquid cryogenic medium, and the conduit 7 is provided with a switch valve. A heating system installation hole 11 is also provided on the upper right side of the cryogenic medium box 2. The low-temperature environment box 3 located in the outermost layer includes a detachable low-temperature environment box cover 6, and the heating system is provided on the upper right side of the corrosive medium box 1 and the cryogenic medium box 2. Considering factors such as heat transfer performance and corrosion resistance, the side wall of the corrosive medium box 1 of the present invention is made of pure copper, the bottom of the corrosive medium box 1, the low temperature environment box 3 and the low temperature medium box 2 are made of vacuum stainless steel, the side wall and the bottom of the corrosive medium box 1 are connected by welding, and the corrosive medium box cover 4, the low temperature environment box cover 6 and the low temperature medium box cover 5 are made of vacuum stainless steel. A sample 18 is placed in the corrosive medium box 1, and the corrosive medium box 1 is filled with corrosive medium. The fixture 9 is installed on the fixture installation hole 8, and the sample 18 is set in the corrosive medium box 1 through the fixture 9. The upper and lower ends of the fixture 9 are connected to the universal testing machine, and the universal testing machine provides the experimental load. The experimental section of the sample 18 is exposed in the corrosive medium box 1. Corrosive medium, such as polar seawater, polar ice-water mixture, polar sea ice, etc., is added to the corrosive medium box 1 according to experimental requirements. The fixture 9 can use existing technology, such as the chuck assembly in CN110646297A.

[0046] like Figure 7As shown, the heating system includes a first heat dissipation component, heat insulation cotton 14, semiconductor cooling sheet 15, second heat dissipation component, temperature sensor and temperature control unit. The first heat dissipation component, semiconductor cooling sheet 15 and second heat dissipation component are stacked from inside to outside, wherein the hot end of semiconductor cooling sheet 15 provides heat to the corrosive medium box 1 through the first heat dissipation component, and the cold end of semiconductor cooling sheet 15 provides cold to the low temperature environment box 3 through the second heat dissipation component. The semiconductor cooling sheet 15 is covered with heat insulation cotton 14 on the periphery, and the first heat dissipation component includes a first heat dissipation block 13 and a first heat dissipation fan 12. The first heat dissipation block 13 is connected to the hot end of the semiconductor cooling sheet 15 through thermal grease and semiconductor cooling sheet bonding glue, and the first heat dissipation fan 12 is fixed to one side of the fin of the first heat dissipation block 13, and the first heat dissipation fan 12 faces the corrosive medium box 1. The second heat dissipation assembly includes a second heat dissipation block 16 and a second heat dissipation fan 17. The second heat dissipation block 16 is connected to the cold end of the semiconductor cooling sheet 15 through thermal grease and semiconductor cooling sheet bonding glue. The second heat dissipation fan 17 is fixed to one side of the fin of the second heat dissipation block 16, and the second heat dissipation fan 17 faces the low temperature environment box 3. The temperature sensor is arranged in the corrosive medium box 1. The round hole 10 on the corrosive medium box cover 4 is mainly used to lead out the wires of the test elements such as the temperature sensor. The temperature sensor monitors the temperature in the corrosive medium box 1 in real time, and transmits the monitored temperature data to the temperature control unit for processing and analysis. The output signal of the temperature control unit controls the heating of the hot end of the semiconductor cooling sheet 15. The heating system includes a first heat dissipation fan 12, a first heat dissipation block 13, heat insulation cotton 14, a plurality of semiconductor cooling sheets 15, a second heat dissipation block 16, a second heat dissipation fan 17, a temperature sensor and a temperature control unit. The temperature control unit includes a neural network fuzzy controller and a PID controller. The temperature control unit is used to control the heating of the hot end of the semiconductor cooling sheet 15. The heat generated by the hot end of the semiconductor refrigeration plate 15 is transferred to the corrosive medium box 1 through the first heat sink 13 and the first heat dissipation fan 12, so that the temperature in the corrosive medium box 1 increases. The cold temperature generated by the cold end of the semiconductor refrigeration plate 15 is transferred to the low temperature environment box 3 through the second heat sink 16 and the second heat dissipation fan 17, so that the temperature in the low temperature environment box 3 decreases.

[0047] Installation of the heating system: The semiconductor refrigeration sheet 15 has a cold end and a hot end. After the semiconductor refrigeration sheet 15 is powered on, the cold end and the hot end work simultaneously. The periphery of the semiconductor refrigeration sheet 15 is covered with thermal insulation cotton 14. The hot end of the semiconductor refrigeration sheet 15 is adhered to the first heat sink 13 by thermal conductive silicone grease and semiconductor refrigeration sheet bonding adhesive. The first cooling fan 12 is fixed to the fin side of the first heat sink 13 by bolts. The cold end of the semiconductor refrigeration sheet 15 is adhered to the second heat sink 16 by thermal conductive silicone grease and semiconductor refrigeration sheet bonding adhesive. The second cooling fan 17 is fixed to the fin side of the second heat sink 16 by bolts. The hot end side of the semiconductor refrigeration sheet 15 is installed facing the corrosive medium box 1, and the cold end side of the semiconductor refrigeration sheet 15 is installed facing the low-temperature environment box 3. The temperature sensor is installed in the corrosive medium box 1.

[0048] Temperature control in the corrosive medium box 1: cooling is performed by the low-temperature medium in the low-temperature medium box 2, and the temperature of the low-temperature medium is much lower than the temperature required in the corrosive medium box 1, that is, much lower than the simulated polar environment temperature; heating is performed by the hot end of the semiconductor refrigeration plate 15. Since the refrigeration of the low-temperature medium is affected by its own temperature, and the low-temperature medium inevitably transfers heat with the external environment, it is impossible to ensure that the temperature of the low-temperature medium will never change. In order to control the temperature in the corrosive medium box 1 to remain stable or maintain it in a certain temperature range for a long time, the temperature in the corrosive medium box 1 is monitored in real time by the temperature sensor in the corrosive medium box 1, and the monitored temperature information is transmitted to the temperature control unit. The heating temperature of the hot end of the semiconductor refrigeration plate 15 is controlled by the temperature control unit, that is, as the temperature of the low-temperature medium itself changes, the heating temperature of the hot end of the semiconductor refrigeration plate 15 is also adjusted accordingly, so that the temperature in the corrosive medium box 1 remains stable or maintains it in a certain temperature range for a long time.

[0049] like Figure 1 and Figure 2 As shown, the temperature control unit includes a neural network fuzzy controller and a PID controller. The neural network fuzzy controller includes a first calculation module and a PID parameter acquisition module. The first calculation module is used to obtain the temperature error e(t) and the error change rate ec between the expected temperature and the measured temperature in the corrosive medium box 1. The PID parameter acquisition module is used to perform neural network fuzzification, neural network fuzzy reasoning and neural network clarification on the error e and the error change rate ec to obtain the real-time adjusted PID control parameter change ΔK p , ΔK i and ΔK d , and then the initial PID control parameter K p0 , K i0 and K d0 Add the PID control parameter change to get the real-time PID control parameter K p , K i and K d, and set the PID control parameter K p , K i and K d The PID parameter acquisition module of the neural network fuzzy controller can obtain the PID control parameter K p , K i and K d The adaptive adjustment makes up for the defect of the single control parameter of the traditional PID algorithm and improves the adaptability of the temperature control unit, so that the temperature in the corrosive medium box 1 can be quickly and stably controlled to reach the expected experimental temperature again during the temperature change of the low-temperature medium.

[0050] The first calculation module of the neural network fuzzy controller in the temperature control unit is based on the formula:

[0051] e(t)=ry(t)

[0052] The temperature error e(t) is obtained, where e(t) is the temperature error, r is the expected temperature, and y(t) is the measured temperature;

[0053] According to the formula:

[0054]

[0055] The error change rate ec is obtained, where ec is the error change rate, y(t) is the current measured temperature, and y(t l ) is the temperature measured last time, tt l For the time interval.

[0056] The PID parameter acquisition module takes the temperature error e(t) and the error change rate ec as input variables, and defines the basic domain of the input variable e(t) as [e l ,e h ], the fuzzy domain is [-p e ,p e ], the quantization factor is Define the basic domain of the input variable ec as [ec l ,ec h ], the fuzzy domain is [-p ec ,p ec ], the quantization factor is The PID control parameter change ΔK p , ΔK i and ΔK d As the output variable, the basic domain of the output variable is defined as [ΔK l ,ΔK h ], ΔK p The fuzzy domain is [-m p ,mp ], the quantization factor is ΔK i The fuzzy domain is [-m i ,m i ], the quantization factor is ΔK d The fuzzy domain is [-m d ,m d ], the quantization factor is The fuzzy subsets of input variables and output variables are set to seven levels: NB, NM, NS, ZO, PS, PM and PB, and Gaussian function is used as the membership function. Fuzzy control performs fuzzy reasoning according to the fuzzy rule table to obtain the fuzzy subsets of output variables. After clarification processing, the output control quantity is obtained.

[0057] The fuzzy rule table satisfies: When the temperature error e is large, a larger ΔK is output p , so that the experimental temperature rises rapidly; when the temperature error e is small, a smaller ΔK is output p , output a larger ΔK i and ΔK d , so that the experimental temperature remains stable.

[0058] The PID parameter acquisition module of the neural network fuzzy controller applies the neural network algorithm to the fuzzy control process. The neural network algorithm can adaptively adjust the membership function of the fuzzy control algorithm to approach the ideal control rule.

[0059] like Figure 3 As shown in the figure, the neural network structure of the PID parameter acquisition module consists of an input layer, a fuzzification layer, a fuzzy reasoning layer and an output layer. The function of the input layer is to input the temperature error e(t) and the error change rate ec. Its function expression is:

[0060] f1(T i )=T i (i=1,2)

[0061] Where, T1 = e(t), T2 = ec;

[0062] The fuzzy layer fuzzifies the input variables, creates fuzzy subsets of the input variables, and selects the Gaussian function as its membership function. Its function expression is:

[0063]

[0064] Where c ij is the middle value of the Gaussian membership function, b ij is the basis width of the Gaussian membership function;

[0065] The fuzzy reasoning layer performs fuzzy reasoning according to the fuzzy rule table, and its function expression is:

[0066]

[0067]

[0068] Where f3(i,j) is the fuzzy inference function, N i is the level number of the fuzzy subset of the input variable;

[0069] The output layer clarifies the fuzzy quantity after fuzzy reasoning and obtains the PID control parameter change ΔK P , ΔK i and ΔK d , its function expression is:

[0070]

[0071] Where w is the conversion weight;

[0072] Finally, the initial PID control parameter K p0 , K i0 and K d0 Add the PID control parameter change to get the real-time PID control parameter K p , K i and K d .

[0073] The neural network algorithm uses the gradient descent method to adjust the parameter b of the membership function. ij 、c ij And the conversion weight w is adaptively adjusted to approach the ideal control rule. The function expression of the output layer performance index function is:

[0074]

[0075] In the formula, r (k) is the ideal output, y (k) is the actual output, k is the number of iterations;

[0076]

[0077] Where w(k) is the conversion weight of the kth iteration, and α is the learning rate;

[0078]

[0079]

[0080] In the formula, α is the learning rate, β is the learning habit factor;

[0081] The PID controller controls the heating of the hot end of the semiconductor refrigeration plate 15 according to the temperature error information and the PID control parameters, and its function expression is:

[0082]

[0083] Where u(t) is the output of the PID controller, K p is the PID proportional control parameter, K i is the PID integral control parameter, K d is the PID differential control parameter.

[0084] It is not difficult to see from the above temperature control principle that the slower the heat transfer rate between the cryogenic medium in the cryogenic medium box 2 and the external environment, the slower the temperature change of the cryogenic medium, the smaller the working pressure of the temperature control unit, and the more stable the temperature in the corrosive medium box 1. The temperature change of the cryogenic medium not only affects the temperature control in the corrosive medium box 1, but also relates to the single use time of the cryogenic medium. When the temperature of the cryogenic medium rises to a certain extent, the temperature in the corrosive medium box 1 will exceed the expected experimental temperature. At this time, the temperature control cannot be performed through the hot end of the semiconductor refrigeration plate 15. In order to continue to complete the subsequent experiments, the cryogenic medium needs to be discharged through the conduit 7 at the bottom of the cryogenic medium box 2, and a new pre-cooled cryogenic medium is introduced through the conduit 7 of the cryogenic medium box cover 5. Since the temperature of the replaced cryogenic medium drops sharply, the hot end of the semiconductor refrigeration plate 15 can re-control the temperature in the corrosive medium box 1, but frequent replacement of the cryogenic medium is not only time-consuming, but also not conducive to stable control of the temperature in the corrosive medium box 1; therefore, the present invention can extend the use time of the cryogenic medium in the cryogenic medium box 2 and reduce the replacement frequency.

[0085] The temperature of the low-temperature medium is kept relatively stable, which is not only conducive to the stable control of the temperature in the corrosive medium box 1, but also prolongs the single use time of the low-temperature medium itself. Since the hot end and the cold end of the semiconductor refrigeration chip 15 work simultaneously after being powered on, a low-temperature environment box 3 is set on the periphery of the low-temperature medium box 2. While the hot end of the semiconductor refrigeration chip 15 controls the temperature in the corrosive medium box 1 in real time, the cold temperature generated by the cold end of the semiconductor refrigeration chip 15 is transmitted to the low-temperature environment box 3 through the second heat sink 16 and the second heat dissipation fan 17, so that the temperature in the low-temperature environment box 3 is reduced. Under the condition that other control conditions such as the voltage flowing through the semiconductor refrigeration chip 15 are the same, the higher the heat dissipation efficiency of the hot end of the semiconductor refrigeration chip 15, the stronger the refrigeration capacity of the cold end of the semiconductor refrigeration chip 15. The hot end of the semiconductor refrigeration chip 15 of the present invention works in a low-temperature environment simulating the polar temperature in the corrosive medium box 1. Compared with the refrigeration equipment on the market that places the hot end of the semiconductor refrigeration chip 15 in the air for heat dissipation, the heat dissipation efficiency of the hot end of the semiconductor refrigeration chip 15 of the present invention is improved, and the refrigeration capacity of the cold end of the semiconductor refrigeration chip 15 is enhanced accordingly, which is specifically manifested in that the temperature in the low-temperature environment box 3 is much lower than the temperature of the outside air. Although the low-temperature medium box 2 is made of a material with a heat-insulating effect, the low-temperature medium will inevitably be affected by the external environment. Compared with the temperature change caused by heat transfer between the low-temperature medium and the high-temperature environment of the outside air, the low-temperature environment in the low-temperature environment box 3 can better ensure that the temperature of the low-temperature medium remains relatively stable.

[0086] The low temperature environment in the corrosive medium box 1 provides good working conditions for the hot end of the semiconductor refrigeration chip 15, resulting in a higher heat dissipation efficiency of the hot end of the semiconductor refrigeration chip 15, and the refrigeration capacity of the cold end of the semiconductor refrigeration chip 15 is enhanced accordingly, which is specifically manifested in that the temperature in the low temperature environment box 3 is much lower than the temperature of the outside air. The cold source of the corrosive medium box 1 is the low temperature medium, and the heat source is the hot end of the semiconductor refrigeration chip 15. The ultra-low temperature environment in the corrosive medium box 1 is created by the low temperature medium, and the temperature in the corrosive medium box 1 is adjusted and constant by the hot end of the semiconductor refrigeration chip 15. The cold end of the semiconductor refrigeration chip 15 works simultaneously with the hot end of the semiconductor refrigeration chip 15 as the cold source of the low temperature environment box 3, so that the temperature in the low temperature environment box 3 is much lower than the temperature of the outside air, reducing the influence of the external high temperature environment on the low temperature medium, and keeping the temperature of the low temperature medium relatively stable, thereby ensuring the stability of the experimental temperature in the corrosive medium box 1.

[0087] The preferred implementation modes of the present invention are described in detail above, but the design concept of the present invention is not limited thereto. Within the technical concept of the present invention, various equivalent transformations can be made to the technical scheme of the present invention, and these equivalent transformations all belong to the protection scope of the present invention.

Claims

1. A stress corrosion test device for polar environments, characterized in that: The invention comprises a low temperature environment box (3), a low temperature medium box (2) located in the low temperature environment box and containing a low temperature medium, a corrosive medium box (1) located in the low temperature medium box and used for placing a sample (18) and containing a corrosive medium, and a heating system located on the corrosive medium box and the side wall of the low temperature medium box, wherein the heating system comprises a first heat dissipation component, a semiconductor cooling plate (15) and a second heat dissipation component which are stacked in sequence from the inside to the outside, wherein the hot end of the semiconductor cooling plate (15) supplies heat to the corrosive medium box through the first heat dissipation component, and the cold end of the semiconductor cooling plate (15) supplies cold to the low temperature environment box through the second heat dissipation component; the heating system also comprises a temperature sensor and a temperature control unit arranged in the corrosive medium box, wherein the temperature sensor monitors the temperature in the corrosive medium box in real time, transmits the monitored temperature data to the temperature control unit for processing and analysis, and controls the heating of the hot end of the semiconductor cooling plate through the output signal of the temperature control unit.

2. The stress corrosion test device for polar environment according to claim 1, characterized in that: The temperature control unit includes a neural network fuzzy controller and a PID controller. The neural network fuzzy controller includes a first calculation module and a PID parameter acquisition module. The first calculation module is used to obtain the temperature error e(t) and the error change rate ec between the expected temperature and the measured temperature in the corrosive medium box. The PID parameter acquisition module is used to perform neural network fuzzification, neural network fuzzy reasoning and neural network clarification on the error e and the error change rate ec to obtain the real-time adjusted PID control parameter change amount. , and , and then the initial PID control parameters , and Add the PID control parameter change to get the real-time PID control parameter , and , and set the PID control parameters , and The data is transmitted to the PID controller to control the heating of the hot end of the semiconductor refrigeration plate.

3. The stress corrosion test device for polar environment according to claim 2, characterized in that: The PID parameter acquisition module takes the temperature error e(t) and the error change rate ec as input variables, and defines the basic domain of the input variable e(t) as , the fuzzy domain is , the quantization factor is , define the basic domain of the input variable ec as , the fuzzy domain is , the quantization factor is , change the PID control parameter , and As an output variable, the basic domain of the output variable is defined as , The fuzzy domain is , the quantization factor is , The fuzzy domain is , the quantization factor is , The fuzzy domain is , the quantization factor is The fuzzy subsets of input variables and output variables are set to seven levels of NB, NM, NS, ZO, PS, PM and PB respectively, and Gaussian function is used as the membership function. Fuzzy control performs fuzzy reasoning according to the fuzzy rule table to obtain the fuzzy subsets of output variables. After clarification processing, the output control quantity is obtained.

4. The stress corrosion test device for polar environment according to claim 3, characterized in that: The neural network structure of the PID parameter acquisition module consists of an input layer, a fuzzification layer, a fuzzy reasoning layer and an output layer. The function of the input layer is to input the temperature error e(t) and the error change rate ec. Its function expression is: , In the formula, , ; The fuzzy layer fuzzifies the input variables, creates fuzzy subsets of the input variables, and selects the Gaussian function as its membership function. Its function expression is: , In the formula is the middle value of the Gaussian membership function, is the basis width of the Gaussian membership function; The fuzzy reasoning layer performs fuzzy reasoning according to the fuzzy rule table, and its function expression is: , , In the formula is the fuzzy inference function, is the level number of the fuzzy subset of the input variable; The output layer clarifies the fuzzy quantity after fuzzy reasoning to obtain the change of PID control parameters. , and , its function expression is: , In the formula is the conversion weight; Finally, the initial PID control parameters , and Add the PID control parameter change to get the real-time PID control parameter , and .

5. The stress corrosion test device for polar environment according to claim 4, characterized in that: The PID controller controls the hot end heating of the semiconductor refrigeration plate according to the temperature error information and the PID control parameters, and its function expression is: , In the formula, is the output of the PID controller, is the PID proportional control parameter, is the PID integral control parameter, is the PID differential control parameter.

6. The stress corrosion test device for polar environment according to claim 1, characterized in that: The first heat dissipation component comprises a first heat dissipation block (13) connected to the hot end of the semiconductor cooling sheet (15) via thermally conductive silicone grease and semiconductor cooling sheet bonding adhesive, and a first heat dissipation fan (12) fixed to the first heat dissipation block with one side of the fin facing the corrosive medium box.

7. The stress corrosion test device for polar environment according to claim 1, characterized in that: The second heat dissipation component comprises a second heat dissipation block (16) connected to the cold end of the semiconductor refrigeration sheet (15) via thermally conductive silicone grease and semiconductor refrigeration sheet bonding adhesive, and a second heat dissipation fan (17) fixed to the second heat dissipation block with one side of the fin facing the low-temperature environment box.

8. The stress corrosion test device for polar environment according to claim 1, characterized in that: The semiconductor refrigeration sheet (15) is covered with heat insulation cotton (14) on its periphery.

9. The stress corrosion test device for polar environment according to claim 1, characterized in that: The cryogenic medium box is provided with a conduit (7) for introducing and discharging liquid cryogenic medium, and the conduit is provided with a switch valve.

Citation Information

Patent Citations

  • High-temperature water environment fracture toughness testing device

    CN110646297A

  • Low-temperature stress corrosion experimental device

    CN110646314A

  • Indoor semiconductor cooling and dehumidification device

    CN103697551A

  • Temperature-controllable magnesium alloy stress corrosion test device

    CN219245251U