A minimally invasive repair method for high-voltage submarine cable breakdown

By using minimally invasive repair methods, the inner and outer layers of high-voltage submarine cables are partially peeled off and repaired layer by layer, solving the problems of material waste and long cycle in traditional repair methods, and achieving efficient and traceless submarine cable repair.

CN117394223BActive Publication Date: 2026-11-10NINGBO ORIENT WIRES & CABLES CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202311541700.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-16
Publication Date
2026-11-10
Estimated Expiration
2043-11-16

AI Technical Summary

Technical Problem

Traditional methods for repairing breakdowns in high-voltage submarine cables result in material waste and long repair cycles. Furthermore, the repair process leaves marks on the cable structure, affecting its performance.

Method used

The minimally invasive repair method involves turning out the steel wire of the armor layer, partially peeling off the sheath and core wire for repair, repairing the inner shielding layer, insulation layer and outer shielding layer layer by layer, using infrared heating technology to melt and fixing with four-way tape and high-temperature tape, and finally restoring the lead sheath and outer sheath.

Benefits of technology

Reduce material waste, shorten the repair period, ensure the integrity and quality of the submarine cable structure, and prevent further breakdown.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117394223B_ABST
    Figure CN117394223B_ABST
Patent Text Reader

Abstract

This invention discloses a minimally invasive repair method for high-voltage submarine cables with insulation breakdown. The steps are as follows: Identify the breakdown location and cut the armor layer; expose the steel wires of the armor layer; peel off the outer sheath; peel off the lead sheath; form the repair area along the breakdown mark; shape the repair area interface along the repair area; repair the core wire surface; process and install the inner shielding repair layer, insulation repair layer, and outer shielding repair layer; bind the repair area interface using PTFE tape, metal materials, and high-temperature tape; melt using infrared heating technology; remove the high-temperature tape, metal materials, and PTFE tape; restore the lead sheath; restore the outer sheath; restore the armor layer. This invention provides a minimally invasive repair method for high-voltage submarine cables with insulation breakdown, shortening the repair period and reducing material waste.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of submarine cable repair, and specifically relates to a minimally invasive repair method for high-voltage submarine cable breakdown. Background Technology

[0002] High-voltage submarine cables are commonly used in the main power transmission lines. With the comprehensive coverage of my country's power grid, the manufacturing process of submarine cables has been continuously improved. However, some micro-defects are still unavoidable during the manufacturing, construction and operation of submarine cables. Micro-defects can easily induce electric treeing, which will cause the insulation layer of the submarine cable to be broken down under the action of overvoltage.

[0003] After insulation breakdown occurs, to ensure the safe use of high-voltage submarine cables, it is necessary to promptly repair the damaged insulation layer and repair the core wires of the cable to prevent further insulation breakdown during subsequent use. Traditional repair methods involve completely stripping the outer layer of the core wires within the circumferential area of ​​the breakdown zone, repairing the core wires, and then wrapping and splicing the outer layer of the core wires to complete the cable repair. However, this process also strips away undamaged outer layers of the cable, resulting in significant material waste, a large workload, and a longer repair cycle. Summary of the Invention

[0004] To address the aforementioned shortcomings, this invention proposes a minimally invasive repair method for high-voltage submarine cables that targets areas where insulation breakdown occurs, shortens the repair period, and reduces material waste.

[0005] The technical solution adopted by this invention to solve the above problems is a minimally invasive repair method for high-voltage submarine cable breakdown, the steps of which are as follows:

[0006] S1: Confirm the location of the cable breakdown and use a cutting machine to cut the armor layer along the breakdown location;

[0007] S2: Flip the steel wires of the armor layer on both sides of the puncture point away from the puncture point, and ensure that the folding radius of the steel wires is greater than the bending elastic limit.

[0008] S3: Strip the outer sheath of the submarine cable, the stripping length of the outer sheath is less than the exposed length of the steel wire;

[0009] S4: Strip the lead sheath of the submarine cable, with the stripping length of the lead sheath being less than the stripping length of the outer sheath.

[0010] S5: Along the breakdown marks, clean up the damaged insulation material at the breakdown location to form the area to be repaired;

[0011] S6: Shape the interface of the repair area along the area to be repaired;

[0012] S7: Repair the surface of the core wire;

[0013] S8: Process the inner shielding repair layer, insulation repair layer, and outer shielding repair layer according to the interface of the repair area;

[0014] S9: Install the inner shielding repair layer, insulation repair layer, and outer shielding repair layer sequentially from the inside out;

[0015] S10: On the outside of the repair area interface, from the inside to the outside, use four-way tape for compression, metal material, and high-temperature tape to bind it;

[0016] S11: Using infrared heating technology, the inner shielding repair layer melts with the original inner shielding layer, the insulation repair layer melts with the original insulation layer, and the outer shielding repair layer melts with the original outer shielding layer.

[0017] S12: Disassemble high-temperature tape, metal materials, and PTFE tape;

[0018] S13: Restore the lead sheath;

[0019] S14: Restore the outer sheath;

[0020] S15: Restore armor layers.

[0021] Compared with the prior art, the advantages of this invention are as follows: Through steps S1-S4, during the repair process, the steel wires of the armor layer are gently turned out, facilitating the subsequent reuse of the steel wires and preventing waste. The outer sheath and lead sheath are still peeled off using a complete peeling repair method to ensure uniform stress distribution between the outer and lead sheath structures. Simultaneously, by gradually reducing the peeling length from the outside to the inside, it facilitates the connection of subsequent repair materials. Then, through steps S5 and S6, the breakdown area is cleaned according to the breakdown marks, and the repair area is shaped according to the structure of the breakdown area, resulting in a repair area that is easy to operate and has high repair quality. Through step S7, the defects in the core wire are repaired to prevent recurrence of breakdown. Through steps S8-S12, the repair of the inner shielding layer, insulation layer, and outer shielding layer of the core wire is completed, utilizing… Four-way tape ensures the fixation of the inner shielding repair layer, insulation repair layer, and outer shielding repair layer. Metal materials and high-temperature tape ensure uniform heating of these three layers during infrared heating, guaranteeing repair quality. After repair, the high-temperature tape, metal materials, and four-way tape can be removed without affecting the high-voltage submarine cable's structure. This achieves seamless repair of the inner shielding, insulation, and outer shielding layers, maintaining a uniform structure and preventing repair marks that could affect cable performance. Finally, the lead sheath, outer sheath, and armor layer are repaired, completing the minimally invasive repair of the breakdown area. Precise repair of the inner shielding, insulation, and outer shielding layers eliminates the need for extensive stripping, saving significant amounts of repair materials and significantly shortening the repair time.

[0022] As an improvement, in step S2, the steel wires of the armor layers on both sides are turned out to a length of more than 900mm. Through this improvement, a sufficient repair area is created to avoid interference from the steel wires during the repair process.

[0023] As an improvement, in step S3, the peeling length of the outer sheath on one side is more than 150mm shorter than the unfolded length of the steel wire. This improvement provides bending space for the unfolded steel wire, ensuring that the steel wire does not exceed the bending elastic limit during the unfolding process and does not affect the subsequent restoration processing of the outer sheath.

[0024] As an improvement, in step S4, the peeling length of the lead sheath on one side is more than 80mm shorter than the peeling length of the outer sheath. This improvement ensures that sufficient repair space is provided for the lead sheath, ensures the overlap distance of the lead sheath during the repair process, and ensures the metal shielding effect of the lead sheath.

[0025] As an improvement, in step S5, a hollow drill bit is used to drill along the puncture mark towards the core wire. When the hollow drill bit is about to come into contact with the core wire, the forward speed of the hollow drill bit is reduced. While completing the cutting of the original inner shielding layer, the original insulation layer, and the original outer shielding layer, the hollow drill bit is prevented from damaging the core wire. Through this improvement, the hollow drill bit is used for drilling. Taking advantage of the multi-layer structure of the submarine cable, the inner structure of the hollow drill bit can be completely separated after each layer is drilled. The puncture area can be completely separated, which can be used for subsequent research on submarine cable puncture phenomena. Moreover, the effective area of ​​the hollow drill bit is much smaller than that of a solid drill bit of the same diameter. Its drilling efficiency is higher and the power required for drilling is lower. At the end of the drilling, the forward speed of the hollow drill bit is reduced to avoid damage to the core wire, ensure the integrity of the core wire, and avoid burrs on the core wire. The drilling can be stopped when the inner shielding layer is about to break, and the inner shielding layer can be finally peeled off using a suction cup or clamping.

[0026] As an improvement, in step S6, after removing the original inner shielding layer, original insulation layer, and original outer shielding layer, the cylindrical groove processed by the hollow drill bit is widened into a conical groove using a trapezoidal drill bit. With this improvement, the structure of the conical groove is more conducive to observing the quality of the repair during the repair process, thereby ensuring the quality of each layer of repair and avoiding subsequent breakdown. If the cylindrical groove structure is guaranteed for repair, it is easy to perform the insulation repair work when the inner shielding repair layer is not aligned with the original inner shielding layer, resulting in poor flatness of the repaired inner shielding layer and making it very easy for the phenomenon of breakdown to occur again.

[0027] As an improvement, in step S8, the inner shielding repair layer, the insulation repair layer, and the outer shielding repair layer are selected according to the trapezoidal drill bit structure. The inner shielding repair layer, the insulation repair layer, and the outer shielding repair layer can all be pre-produced according to the structure of the trapezoidal drill bit. Through this improvement, after the pre-production of the inner shielding repair layer, the insulation repair layer, and the outer shielding repair layer is completed, they can be directly used during repair, thereby greatly increasing the repair efficiency. Furthermore, the quality of the inner shielding repair layer, the insulation repair layer, and the outer shielding repair layer can be detected in advance, thereby ensuring the quality of the repaired layer.

[0028] As an improvement, in step S9, when the inner and outer shielding repair layers are installed, a second grinding process is performed based on the installation allowance to ensure the flatness of the connection between the inner and outer shielding repair layers and the original inner shielding layer, and the connection between the outer and outer shielding repair layers and the original outer shielding layer. Through this improvement, after the repair is completed, it is necessary to ensure the flatness of the connection between the inner and outer shielding repair layers and the original inner shielding layer, in order to avoid the possibility of breakdown problems in this area again. However, because the inner shielding repair layer needs to be pressed and shaped along the core wire during repair and installation, and the outer shielding repair layer needs to be pressed and shaped along the insulation repair layer during repair and installation, especially since the connection surface structure of the inner shielding repair layer is more complex, with the side near the core wire being a near-flat arc surface and the side near the insulation repair layer being a large arc surface, the pressing and shaping is poor, and a second grinding process is required to correct the allowance.

[0029] As an improvement, in step S9, the insulation repair layer is formed using an injection mold. The injection mold has an injection cavity, the side of which has the same structure as the side of the trapezoidal drill bit. The lower end face of the injection mold is the same as the outer side of the original inner shielding layer, and the upper end face of the injection mold is the same as the inner side of the original outer shielding layer. In step S11, an insulation preheating block with the same structure as the insulation repair layer is formed using the injection mold, and an outer shielding preheating block with the same structure as the outer shielding repair layer is pre-produced. The surfaces of the insulation preheating block and the outer shielding preheating block are then repeatedly polished until smooth. When the inner shielding repair layer is fused with the original inner shielding layer, the outer side of the inner shielding repair layer is filled with insulating preheating blocks and outer shielding preheating blocks; when the insulation repair layer is fused with the original insulation layer, the outer side of the insulation repair layer is filled with outer shielding preheating blocks. Through these improvements, a high-precision insulation repair layer can be manufactured using injection molds. This not only ensures high-quality repair of the insulation repair layer but also serves as a quality inspection tool for the inner shielding repair layer. When the inner shielding repair layer is not installed properly, the alignment difference of the insulation repair layer can be easily detected during the installation process. Therefore, the inner shielding repair layer needs to be repaired again. In step S11, the inner shielding repair layer, insulation repair layer, and outer shielding repair layer have different melting temperatures. If all three are melted simultaneously for repair, a higher temperature is required to repair the inner shielding repair layer, which would cause excessive heat damage to the outer shielding repair layer. Therefore, the best solution for the three-layer structure is to use layered melting. During the repair of the inner shielding repair layer, insulation preheating blocks and outer shielding preheating blocks are used for filling. This not only allows for the assessment of the flatness of the inner shielding repair layer but also ensures... The tight compression of the inner shielding repair layer ensures the repair quality of the inner shielding repair layer. At the same time, during the melting process of the inner shielding repair layer, the insulation preheating block and the outer shielding preheating block will also heat up, which can preheat the repair surface of the original insulation layer and the original outer shielding layer, activate the activity of the original insulation layer and the original outer shielding layer materials, and improve the efficiency of subsequent repair work of the original insulation layer and the original outer shielding layer while ensuring high repair quality. Similarly, when repairing the insulation repair layer, the outer shielding preheating is used for filling and preheating, which requires repeated binding and unbinding of high temperature tape, metal materials and PTFE tape.

[0030] As an improvement, in step S13, the lead sheath used for repair overlaps with the original lead sheath by more than 40mm and is then welded back; in step S14, the outer sheath used for repair is wrapped around the lead sheath using a strip made of the same material as the original outer sheath, and then heated and melted; in step S15, the exposed original steel wire is re-woven, and when re-woven to the cut section, the steel wire used for repair is interwoven into the original steel wire, connecting the original steel wires at both ends of the cut, and then welded and fixed. Through these improvements, the overall metal shielding of the lead sheath, the high-strength connection between the outer sheath and the armor layer are achieved, and the overall repair work is completed. The main function of these three layers is to isolate the submarine cable from the external environment, and more importantly, to ensure sealing and structural strength. Attached Figure Description

[0031] Figure 1 This is a schematic diagram of the submarine cable structure after steps S1-S4 of the present invention.

[0032] Figure 2 This is a schematic diagram of the cross-sectional structure of the submarine cable after step S5 of the present invention.

[0033] Figure 3 This is a schematic diagram of the cross-sectional structure of the submarine cable after step S6 of the present invention.

[0034] Figure 4 This is a schematic diagram of the cross-sectional structure of the submarine cable after step S6 of the present invention.

[0035] Figure 5 This is a schematic diagram of the cross-sectional structure of the submarine cable after step S12 of the present invention.

[0036] Figure 6 This is a schematic diagram of the cross-sectional structure of the submarine cable after step S12 of the present invention.

[0037] The diagram shows: 1. Armor layer, 1.1. Steel wire, 2. Outer sheath, 3. Lead sheath, 4. Original outer shielding layer, 5. Original insulation layer, 6. Original inner shielding layer, 7. Core wire, 8. Hollow drill bit, 9. Trapezoidal drill bit, 10. Cylindrical groove, 11. Conical groove, 12. Outer shielding repair layer, 13. Insulation repair layer, 14. Inner shielding repair layer. Detailed Implementation

[0038] The embodiments of the present invention will be further described below with reference to the accompanying drawings.

[0039] Example 1:

[0040] like Figure 1-6 As shown, a minimally invasive repair method for high-voltage submarine cable breakdown includes the following steps:

[0041] S1: Confirm the location of the cable puncture, and use a cutting machine to cut the armor layer 1 along the puncture location;

[0042] S2: Turn the steel wires 1.1 of the armor layer 1 on both sides of the puncture position outwards in a direction away from the puncture position, and ensure that the turning radius of the steel wires 1.1 is greater than the bending elastic limit. The steel wires 1.1 of the armor layer 1 on both sides are turned outwards by 1000mm in length.

[0043] S3: Strip the outer sheath 2 of the submarine cable. The stripping length of the outer sheath 2 is less than the exposed length of the steel wire 1.1. The puncture point is the stripping length of 800mm from the center to both sides.

[0044] S4: Strip the lead sheath 3 of the submarine cable. The stripping length of the lead sheath 3 is less than the stripping length of the outer sheath 2. The breakdown point is the length of 700mm stripped from the center to both sides.

[0045] S5: Along the breakdown marks, clean up the damaged insulation material at the breakdown location to form the area to be repaired;

[0046] S6: Shape the interface of the repair area along the area to be repaired;

[0047] S7: Repair the surface of core wire 7;

[0048] S8: Process the inner shielding repair layer 14, the insulation repair layer 13, and the outer shielding repair layer 12 according to the interface of the repair area;

[0049] S9: Install the inner shielding repair layer 14, the insulation repair layer 13, and the outer shielding repair layer 12 sequentially from the inside out;

[0050] S10: On the outside of the repair area interface, from the inside to the outside, use four-way tape for compression, metal material, and high-temperature tape to bind it;

[0051] S11: Using infrared heating technology, the inner shielding repair layer 14 is melted with the original inner shielding layer 6, the insulation repair layer 13 is melted with the original insulation layer 5, and the outer shielding repair layer 12 is melted with the original outer shielding layer 4.

[0052] S12: Disassemble high-temperature tape, metal materials, and PTFE tape;

[0053] S13: Restore lead sheath 3;

[0054] S14: Restore outer sheath 2;

[0055] S15: Restore armor layer 1.

[0056] In step S5, a hollow drill bit 8 is used to drill a hole along the puncture mark towards the core wire 7. When the hollow drill bit 8 is about to come into contact with the core wire 7, the forward speed of the hollow drill bit 8 is reduced. While completing the cutting of the original inner shielding layer 6, the original insulation layer 5, and the original outer shielding layer 4, the hollow drill bit 8 is prevented from damaging the core wire 7. In step S6, after removing the cut-off original inner shielding layer 6, the original insulation layer 5, and the original outer shielding layer 4, the cylindrical groove 10 processed by the hollow drill bit 8 is widened into a conical groove 11 using a trapezoidal drill bit 9. The conical groove 11 is used to shape the interface of the repair area. The cut surfaces of the original inner shielding layer 6, the original insulation layer 5, and the original outer shielding layer 4 are ground into smooth bevels using sandpaper. There should be no step phenomenon, otherwise it will affect the repair melting effect.

[0057] Simultaneously, the unbroken original inner shielding layer 6 can be peeled off and polished. This not only ensures the smoothness of the cut surface of the inner shielding layer after cutting, but also exposes the core wire 7, facilitating step S7 and completing the repair of the core wire 7 surface. Figure 4 , Figure 6 As shown, the original inner shielding layer 6 has a different structure, which is changed by grinding after peeling off the inner shielding layer in the repair area.

[0058] In step S6, after removing the original inner shielding layer 6, original insulation layer 5, and original outer shielding layer 4 that were cut off, the cylindrical groove 10 processed by the hollow drill bit 8 is widened into a conical groove 11 using a trapezoidal drill bit 9.

[0059] In step S8, the inner shielding repair layer 14, the insulation repair layer 13, and the outer shielding repair layer 12 are selected according to the structure of the trapezoidal drill bit 9. The inner shielding repair layer 14, the insulation repair layer 13, and the outer shielding repair layer 12 can all be pre-produced according to the structure of the trapezoidal drill bit 9. In step S9, when the inner shielding repair layer 14 and the outer shielding repair layer 12 are installed, they are subjected to secondary grinding processing according to the installation allowance to ensure the flatness of the connection between the inner shielding repair layer 14 and the original inner shielding layer 6, and the outer shielding repair layer 12 and the original outer shielding layer 4. The insulation repair layer 13 is formed by injection molding. The injection mold has an injection cavity. The side of the injection cavity is the same as the side structure of the trapezoidal drill bit. The lower end face of the injection cavity is the same as the outer side face of the original inner shielding layer 6, and the upper end face of the injection cavity is the same as the inner side face of the original outer shielding layer 4.

[0060] In step S13, the lead sheath 3 used for repair overlaps with the original lead sheath 3 by more than 40mm and is then welded back together.

[0061] In step S14, the outer sheath 2 for repair is wrapped around the lead sheath 3 by using a strip made of the same material as the original outer sheath 2, and then heated and melted.

[0062] In step S15, the exposed original steel wire 1.1 is re-woven. When re-weaving to the cut section, the repair steel wire 1.1 is interwoven into the original steel wire 1.1 to connect the original steel wires 1.1 at both ends of the cut section and welded to fix them.

[0063] In step S10, the metal material is a heating coil made of coiled copper wire.

[0064] Example 2:

[0065] A minimally invasive repair method for high-voltage submarine cable breakdown, the steps of which are as follows:

[0066] S1: Confirm the location of the cable puncture, and use a cutting machine to cut the armor layer 1 along the puncture location;

[0067] S2: Turn the steel wires 1.1 of the armor layer 1 on both sides of the puncture position outwards in a direction away from the puncture position, and ensure that the turning radius of the steel wires 1.1 is greater than the bending elastic limit. The steel wires 1.1 of the armor layer 1 on both sides are turned outwards by 1000mm in length.

[0068] S3: Strip the outer sheath 2 of the submarine cable. The stripping length of the outer sheath 2 is less than the exposed length of the steel wire 1.1. The puncture point is the stripping length of 800mm from the center to both sides.

[0069] S4: Strip the lead sheath 3 of the submarine cable. The stripping length of the lead sheath 3 is less than the stripping length of the outer sheath 2. The breakdown point is the length of 700mm stripped from the center to both sides.

[0070] S5: Along the breakdown marks, clean up the damaged insulation material at the breakdown location to form the area to be repaired;

[0071] S6: Shape the interface of the repair area along the area to be repaired;

[0072] S7: Repair the surface of core wire 7;

[0073] S8: Process the inner shielding repair layer 14, insulation repair layer 13, outer shielding repair layer 12, insulation preheating block, and outer shielding preheating block according to the interface of the repair area;

[0074] S9-1: Install the inner shielding repair layer 14, the insulation preheating block 3, and the outer shielding preheating block in sequence from the inside out;

[0075] S10-1: On the outside of the repair area interface, from the inside to the outside, use four-way tape for compression, metal material, and high-temperature tape for binding;

[0076] S11-1: The inner shielding repair layer 14 is fused with the original inner shielding layer 6 by infrared heating technology;

[0077] S12-1: Disassemble the high-temperature tape, metal materials and 4F tape, and observe the repair quality of the inner shielding repair layer 14. If there are any repair defects, grind and repair them in time.

[0078] S9-2: Install the insulation repair layer 13 and the outer shielding preheating block sequentially from the inside out;

[0079] S10-2: On the outside of the repair area interface, from the inside to the outside, use four-way tape for compression, metal material, and high-temperature tape for binding;

[0080] S11-2: The insulation repair layer 13 and the original insulation layer 5 are melted together by infrared heating technology;

[0081] S12-2: Disassemble the high-temperature tape, metal materials and PTFE tape, and observe the repair quality of the insulation repair layer 13. If there are any repair defects, grind and repair them in time.

[0082] S9-3: Install the outer shielding repair layer 12 sequentially from the inside out;

[0083] S10-3: On the outside of the repair area interface, from the inside to the outside, use four-way tape for compression, metal material, and high-temperature tape to bind it;

[0084] S11-3: The outer shielding repair layer 12 is fused with the original outer shielding layer 4 using infrared heating technology;

[0085] S12-3: Disassemble the high-temperature tape, metal materials and fluoropolymer tape, and observe the repair quality of the outer shielding repair layer 12. If there are any repair defects, grind and repair them in time.

[0086] S13: Restore lead sheath 3;

[0087] S14: Restore outer sheath 2;

[0088] S15: Restore armor layer 1.

[0089] In step S5, a hollow drill bit 8 is used to drill a hole along the puncture mark towards the core wire 7. When the hollow drill bit 8 is about to come into contact with the core wire 7, the forward speed of the hollow drill bit 8 is reduced. While completing the cutting of the original inner shielding layer 6, the original insulation layer 5, and the original outer shielding layer 4, the hollow drill bit 8 is prevented from damaging the core wire 7. In step S6, after removing the cut-off original inner shielding layer 6, the original insulation layer 5, and the original outer shielding layer 4, the cylindrical groove 10 processed by the hollow drill bit 8 is widened into a conical groove 11 using a trapezoidal drill bit 9. The conical groove 11 is used to shape the interface of the repair area. The cut surfaces of the original inner shielding layer 6, the original insulation layer 5, and the original outer shielding layer 4 are ground into smooth bevels using sandpaper. There should be no step phenomenon, otherwise it will affect the repair melting effect.

[0090] Simultaneously, the unbroken original inner shielding layer 6 can be peeled off and polished. This not only ensures the smoothness of the cut surface of the inner shielding layer after cutting, but also exposes the core wire 7, facilitating step S7 and completing the repair of the core wire 7 surface. Figure 4 , Figure 6 As shown, the original inner shielding layer 6 has a different structure, which is changed by grinding after peeling off the inner shielding layer in the repair area.

[0091] In step S6, after removing the original inner shielding layer 6, original insulation layer 5, and original outer shielding layer 4 that were cut off, the cylindrical groove 10 processed by the hollow drill bit 8 is widened into a conical groove 11 using a trapezoidal drill bit 9.

[0092] In step S8, the inner shielding repair layer 14, the insulation repair layer 13, and the outer shielding repair layer 12 are selected according to the structure of the trapezoidal drill bit 9. The inner shielding repair layer 14, the insulation repair layer 13, and the outer shielding repair layer 12 can all be pre-produced according to the structure of the trapezoidal drill bit 9. In step S9, when the inner shielding repair layer 14 and the outer shielding repair layer 12 are installed, they are subjected to secondary grinding processing according to the installation allowance to ensure the flatness of the connection between the inner shielding repair layer 14 and the original inner shielding layer 6, and the outer shielding repair layer 12 and the original outer shielding layer 4.

[0093] The insulation repair layer 13 is formed by injection molding. The injection mold has an injection cavity. The side surface of the injection cavity is the same as the side surface of the trapezoidal drill bit. The lower end surface of the injection cavity is the same as the outer side surface of the original inner shielding layer 6, and the upper end surface of the injection cavity is the same as the inner side surface of the original outer shielding layer 4. In step S11, an insulation preheating block with the same structure as the insulation repair layer 13 is formed by injection molding, and an outer shielding preheating block with the same structure as the outer shielding repair layer 12 is pre-produced. The insulation preheating block and the outer shielding repair layer 12 are then processed. The surface of the shielding preheating block is polished multiple times until smooth; when the inner shielding repair layer 14 is melted with the original inner shielding layer 6, the outer side of the inner shielding repair layer 14 is filled with insulating preheating blocks and outer shielding preheating blocks; when the insulating repair layer 13 is melted with the original insulating layer 5, the outer side of the insulating repair layer 13 is filled with outer shielding preheating blocks. In step S11, the melting temperatures of the inner shielding repair layer 14, insulating repair layer 13, and outer shielding repair layer 12 are different. If the three are melted simultaneously... For the repair of the inner shielding repair layer 14, a high temperature is required. However, this temperature would cause excessive damage to the outer shielding repair layer 12. Therefore, the optimal solution for the three-layer structure is to use layered melting. During the repair of the inner shielding repair layer 14, insulation preheating blocks and outer shielding preheating blocks are used for filling. This not only allows for the assessment of the flatness of the repaired inner shielding repair layer 14 but also ensures the compaction effect of the inner shielding repair layer 14, guaranteeing the repair quality of the inner shielding repair layer 14. At the same time, during the melting process of the inner shielding repair layer 14, the insulation preheating blocks and outer shielding preheating blocks will also heat up, which can preheat the repair surfaces of the original insulation layer 5 and the original outer shielding layer 4, activating the material activity of the original insulation layer 5 and the original outer shielding layer 4. This ensures high repair quality while improving the efficiency of subsequent repair work of the original insulation layer 5 and the original outer shielding layer 4. Similarly, when repairing the insulation repair layer, the outer shielding preheating is used for filling and preheating, which requires repeated binding and disassembly of high-temperature tape, metal materials, and four-way tape.

[0094] Both the aforementioned insulation preheating block and outer shielding preheating block are made of aluminum metal. Aluminum metal has a melting point of 660 degrees Celsius and can be molded using the same injection mold as the insulation repair layer. It will not melt during the subsequent infrared heating process. At the same time, aluminum metal has good thermal conductivity, which can quickly achieve the effect of heat conduction during infrared heating, so that the inner shielding repair layer 14 and the original inner shielding layer 6 can melt quickly, and the original insulation layer 5 can be quickly activated, which facilitates the subsequent melting and repair work of the insulation repair layer 13 and the original insulation layer 5.

[0095] In step S13, the lead sheath 3 used for repair overlaps with the original lead sheath 3 by more than 40mm and is then welded back together.

[0096] In step S14, the outer sheath 2 for repair is wrapped around the lead sheath 3 by using a strip made of the same material as the original outer sheath 2, and then heated and melted.

[0097] In step S15, the exposed original steel wire 1.1 is re-woven. When re-weaving to the cut section, the repair steel wire 1.1 is interwoven into the original steel wire 1.1 to connect the original steel wires 1.1 at both ends of the cut section and welded to fix them.

[0098] In step S10, the metal material is a heating coil made of coiled copper wire.

[0099] Compared with traditional repair methods, the minimally invasive repair method of the present invention has lower repair costs and shorter repair time, and is more suitable for outdoor repair. It also has lower requirements for outdoor repair equipment. Correspondingly, it requires higher repair standards, with higher requirements for the detailed alignment of the inner shielding repair layer 14 with the original inner shielding layer 6, the insulation repair layer 13 with the original insulation layer 5, and the outer shielding repair layer 12 with the original outer shielding layer 4. However, through the interface design of the conical groove 11, the alignment of the three can be better calibrated, thus ensuring the repair quality.

[0100] The above description only illustrates the preferred embodiments of the present invention and should not be construed as limiting the scope of the claims. The present invention is not limited to the above embodiments, and variations in its specific structure are permitted. All variations made within the scope of the independent claims of this invention are also within the scope of protection of this invention.

Claims

1. A minimally invasive repair method for high-voltage submarine cable breakdown, characterized in that, The steps are as follows: S1: Confirm the location of the cable breakdown and use a cutting machine to cut the armor layer (1) along the breakdown location; S2: Turn the steel wires (1.1) of the armor layer (1) on both sides of the puncture position outwards in a direction away from the puncture position, and ensure that the turning radius of the steel wires (1.1) is greater than the bending elastic limit. S3: Strip the outer sheath (2) of the submarine cable, the stripping length of the outer sheath (2) is less than the exposed length of the steel wire (1.1); S4: Strip the lead sheath (3) of the submarine cable, the stripping length of the lead sheath (3) is less than the stripping length of the outer sheath (2); S5: Use a hollow drill bit (8) to drill a hole along the puncture mark toward the core wire (7), clean up the damaged insulation material at the puncture location, and reduce the forward speed of the hollow drill bit (8) when it is about to come into contact with the core wire (7). While completing the cutting of the original inner shielding layer (6), the original insulation layer (5), and the original outer shielding layer (4), avoid the hollow drill bit (8) from damaging the core wire (7) and forming an area to be repaired. S6: Shape the interface of the repair area along the area to be repaired, and take out the original inner shielding layer (6), original insulation layer (5), and original outer shielding layer (4) that were cut off. Then, use a trapezoidal drill bit (9) to enlarge the cylindrical groove (10) processed by the hollow drill bit (8) into a conical groove (11). S7: Repair the surface of the core wire (7); S8: Select the inner shielding repair layer (14), insulation repair layer (13), and outer shielding repair layer (12) according to the structure of the trapezoidal drill bit (9). The inner shielding repair layer (14), insulation repair layer (13), and outer shielding repair layer (12) can all be pre-produced according to the structure of the trapezoidal drill bit (9). S9: Install the inner shielding repair layer (14), the insulation repair layer (13), and the outer shielding repair layer (12) sequentially from the inside to the outside. The insulation repair layer (13) is formed by injection molding. The injection mold has an injection cavity. The side of the injection cavity is the same as the side structure of the trapezoidal drill bit (9). The lower end face of the injection cavity is the same as the outer side face of the original inner shielding layer (6). The upper end face of the injection cavity is the same as the inner side face of the original outer shielding layer (4). S10: On the outside of the repair area interface, from the inside to the outside, use four-way tape for compression, metal material, and high-temperature tape to bind it; S11: Using infrared heating technology, the inner shielding repair layer (14) is melted with the original inner shielding layer (6), the insulation repair layer (13) is melted with the original insulation layer (5), and the outer shielding repair layer (12) is melted with the original outer shielding layer (4). An insulation preheating block with the same structure as the insulation repair layer (13) is formed using an injection mold, and an outer shielding preheating block with the same structure as the outer shielding repair layer (12) is pre-produced. The surfaces of the insulation preheating block and the outer shielding preheating block are polished multiple times until smooth. When the inner shielding repair layer (14) is melted with the original inner shielding layer (6), the outer side of the inner shielding repair layer (14) is filled with insulation preheating blocks and outer shielding preheating blocks. When the insulation repair layer (13) is melted with the original insulation layer (5), the outer side of the insulation repair layer (13) is filled with outer shielding preheating blocks. S12: Disassemble high-temperature tape, metal materials, and PTFE tape; S13: Restore the lead sheath (3); S14: Restore the outer sheath (2); S15: Restore armor layer (1).

2. The method for minimally invasive repair of high-voltage submarine cable breakdown according to claim 1, characterized in that: In step S2, the steel wires (1.1) of the two sides of the armor layer (1) are turned out to a length of more than 900mm.

3. The method for minimally invasive repair of high-voltage submarine cable breakdown according to claim 1, characterized in that: In step S3, the peeling length of the single-sided outer sheath (2) is more than 150 mm shorter than the unfolded length of the steel wire (1.1).

4. The method for minimally invasive repair of high-voltage submarine cable breakdown according to claim 1, characterized in that: In step S4, the peel length of the single-sided lead sheath (3) is more than 80 mm shorter than the peel length of the outer sheath (2).

5. The method for minimally invasive repair of high-voltage submarine cable breakdown according to claim 1, characterized in that: In step S9, when the inner shielding repair layer (14) and the outer shielding repair layer (12) are installed, they are subjected to secondary grinding processing according to the installation allowance to ensure the flatness of the connection between the inner shielding repair layer (14) and the original inner shielding layer (6), and the outer shielding repair layer (12) and the original outer shielding layer (4).

6. The method for minimally invasive repair of high-voltage submarine cable breakdown according to claim 1, characterized in that: In step S13, the lead sheath (3) used for repair overlaps with the original lead sheath (3) by more than 40mm and is then welded back together. In step S14, the outer sheath (2) for repair is wrapped around the lead sheath (3) by using a strip of the same material as the original outer sheath (2), and then heated and melted. In step S15, the exposed original steel wire (1.1) is re-woven. When re-woven to the cut section, the repair steel wire (1.1) is interlaced and woven into the original steel wire (1.1) to connect the original steel wires (1.1) at both ends of the cut section and welded to fix them.

Citation Information

Patent Citations

  • Hot-melt type cable middle connection mounting technology

    CN109616962A

  • Middle-high voltage cross-linked polyethylene insulation fault repair power cable and repair method

    CN115065009A

  • Emergency recovery method for power cable

    JP1993344626A