A PCB manufacturing method and PCB

By creating individual windows for each layer of the board before PCB lamination and using deformable structural components made of shape memory alloy, the problem of low cavity structure precision was solved, and the stability of the cavity shape and the improvement of signal transmission were achieved.

CN117412511BActive Publication Date: 2026-11-17DONGGUAN SHENGYI ELECTRONICS
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311636516.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-30
Publication Date
2026-11-17
Estimated Expiration
2043-11-30

AI Technical Summary

Technical Problem

The low precision in the shape and size of cavity structures in current PCB manufacturing leads to unstable signal transmission and product quality issues.

Method used

The deformable structural component made of shape memory alloy is used to create individual windows on each layer of the PCB before PCB lamination. During high-temperature lamination, the shape change of the deformable structural component is used to block the glue flow and support the windows, ensuring that the cavity shape remains unchanged. The deformable structural component can then be removed.

Benefits of technology

It improves the manufacturing precision of the cavity structure, reduces the amount of adhesive used, avoids cavity collapse, and enhances the signal transmission quality and product yield of the PCB.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117412511B_ABST
    Figure CN117412511B_ABST
Patent Text Reader

Abstract

This invention relates to the field of PCB technology and discloses a PCB manufacturing method and a PCB. The PCB manufacturing method includes: creating windows in each target core board / subboard / adhesive sheet, with each window area used for stacking to form a window; providing auxiliary workpieces, including deformable structural components made of shape memory alloys, capable of deforming into a first shape for resisting adhesive and / or supporting the window when heated above the transition temperature, and deforming into a second shape that can be detached from the window when cooled below the transition temperature; stacking the boards, placing the deformable structural components within the window formed by stacking the window areas and controlling the deformable structural components to remain in the first shape; high-temperature pressing; cooling to below the transition temperature, causing the deformable structural components to deform into the second shape, and removing the deformable structural components. This invention utilizes deformable structural components for resisting adhesive and / or supporting the window, which can effectively improve the manufacturing accuracy of through holes, blind holes, embedded holes, or embedded cavities.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of PCB (Printed Circuit Board) technology, and more particularly to a PCB manufacturing method and a PCB. Background Technology

[0002] As the field of communication electronics gradually develops towards higher frequency and higher speed signals, higher requirements are placed on the low-loss transmission of high-frequency and high-speed signals and impedance continuity of signal lines in PCBs.

[0003] Currently, in addition to optimizing the layout design of PCB holes and lines, improving signal transmission speed and reducing losses in PCB manufacturing processes mainly involves using dielectrics with lower Dk (dielectric constant) and Df (dielectric loss factor) as substrates and using conductor layers with lower roughness to fabricate circuits. However, these two directions have gradually encountered bottlenecks in the process of rapid development and will face difficulties in 112G and future high-speed PCB applications.

[0004] Because the Dk and Df values ​​of air are much lower than those of conventional resin-based PCB substrates, if part of the dielectric around the inner layer signal lines is hollowed out, the high-frequency electromagnetic field around the signal lines will partially propagate in the air, thereby increasing signal transmission speed and reducing dielectric loss during transmission. This holds great potential for future high-end high-speed PCB applications. Therefore, the industry typically creates cavities in PCBs. However, the industry generally manufactures PCBs with inner cavities by first creating windows in the low-flowability bonding sheet and inner layer sub-board, and then pressing the core board together. This method has several drawbacks:

[0005] Low-flow adhesive sheets typically have a flow rate of over 10 mil, which can easily lead to abnormal flow and irregular cavities.

[0006] Because the low-flow adhesive sheet flows into the cavity, the dielectric thickness near the cavity will be lower, resulting in a lower cavity height. This will affect the impedance of the transmission line in the cavity, causing it to deviate from the design value.

[0007] When multiple circuits are designed in the same cavity or the cavity is wide, the top of the cavity is prone to collapse due to compression or other external forces, affecting the shape of the cavity. Summary of the Invention

[0008] The purpose of this invention is to provide a PCB manufacturing method and a PCB to solve the problem of low manufacturing accuracy in terms of shape and size of structures such as buried cavities in the prior art.

[0009] To achieve this objective, the present invention adopts the following technical solution:

[0010] A PCB manufacturing method, comprising:

[0011] Each target core board / sub-board / adhesive sheet is pre-cut with windows, and the windowed areas on each target core board / sub-board / adhesive sheet are used to stack and form windows;

[0012] An auxiliary workpiece is provided, the auxiliary workpiece comprising a deformable structural member made of shape memory alloy, the deformable structural member being able to deform into a first shape for resisting adhesive and / or supporting a window when its temperature rises above the transition temperature, and into a second shape that can be detached from the window when its temperature drops below the transition temperature; the transition temperature is lower than a preset bonding temperature;

[0013] At least the target core plates / sub-plates / adhesive sheets are stacked in sequence, and the deformable structural parts of the auxiliary workpiece are placed in the window formed by stacking the window areas of the target core plates / sub-plates / adhesive sheets, and the deformable structural parts are kept in the first shape by heating to above the transformation temperature.

[0014] At the pressing temperature, the stacked plates containing deformable structural members that maintain a first shape are pressed together at high temperature to obtain a pressed plate;

[0015] The laminating plate is cooled below the transition temperature, causing the deformable structural component to deform into a second shape that can be removed from the window. The deformable structural component is then removed from the laminating plate to form a PCB.

[0016] Optionally, after the deformable structural component is removed, the window is specifically formed on the PCB as a through hole, blind hole, embedded hole, or embedded cavity.

[0017] Optionally, the cross-section of the window along the pressing direction is stepped or cylindrical.

[0018] Optionally, it also includes: after opening windows in each target core board / sub-board / adhesive sheet, deburring and removing residual adhesive from the windowed areas of each target core board / sub-board / adhesive sheet.

[0019] Optionally, when the window is specifically formed as an embedded hole or an embedded cavity on the PCB, the step of stacking each target core board / sub-board / adhesive sheet in sequence includes: providing an upper core board and a lower core board, and stacking the upper core board, each target core board / sub-board / adhesive sheet and the lower core board in sequence.

[0020] The PCB manufacturing method further includes: before stacking the boards, pre-opening access channels for taking out and placing deformable structural components on the upper core board and / or the lower core board, which connect to the external space and windows.

[0021] Optionally, the PCB manufacturing method further includes: plugging the holes in the pick-and-place channel after removing the deformable structural component.

[0022] Optionally, the auxiliary workpiece may also include a pick-and-place handle connected to the deformable structural component;

[0023] When the deformable structural component is built into the window, the pick-and-place handle is partially housed within the pick-and-place channel and partially extends outside the pick-and-place channel.

[0024] Optionally, when deformed into the first shape, the outer wall of the deformable structural member placed within the window abuts against the inner wall of the window.

[0025] Optionally, the second shape is columnar.

[0026] A PCB, said PCB being manufactured according to any one of the PCB manufacturing methods described above.

[0027] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0028] In this embodiment of the invention, during the high-temperature pressing process, the window contains a deformable structural component. This component maintains its first shape because the pressing temperature is higher than its transition temperature. The deformable structural component in its first shape can prevent excessive adhesive flow into the window, thus reducing the amount of adhesive flowing into the window. Furthermore, it abuts against the inner wall of the window, preventing deformation of the window shape under high temperature and pressure. In summary, this embodiment of the invention utilizes a deformable structural component made of shape memory alloy, which can effectively improve the manufacturing accuracy of structures such as through holes, blind holes, embedded holes, or embedded cavities. In addition, because windows are individually opened before stacking, it is relatively easy to manufacture various windows with conventional or irregular overall structures, meeting the manufacturing needs of different application scenarios. Attached Figure Description

[0029] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0030] Figure 1 A flowchart of a PCB manufacturing method provided in an embodiment of the present invention;

[0031] Figure 2 A schematic diagram illustrating the deformation of a deformable structural member below the transformation temperature as its temperature increases from below the transformation temperature to above the transformation temperature, provided as an embodiment of the present invention.

[0032] Figure 3 A comparison diagram of the shape of the deformable structural component provided in the embodiment of the present invention before and after entering the window. Detailed Implementation

[0033] To make the objectives, features, and advantages of this invention more apparent and understandable, the technical solutions of the embodiments of this invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the embodiments described below are only some embodiments of this invention, and not all embodiments. Based on the embodiments of this invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this invention.

[0034] Shape memory alloys (SMAs) are materials composed of two or more metallic elements that exhibit shape memory effect (SME) through thermoelastic and martensitic phase transformations and their inverse transformations. SMAs are the materials with the best shape memory performance among shape memory materials. To date, more than 50 alloys exhibiting shape memory effect have been discovered.

[0035] Components made of shape memory alloys possess both a high-temperature phase shape and a low-temperature phase shape. The deformation recovery capability of shape memory alloy components is due to the thermoelastic martensitic phase transformation that occurs within the material during deformation. Shape memory alloys contain two phases: a high-temperature austenitic phase and a low-temperature martensitic phase. Shape memory alloys can remember different shapes in different phases and recover the high-temperature phase shape upon heating and the low-temperature phase shape upon cooling. Therefore, components made of shape memory alloys can exhibit two shapes depending on different thermodynamic loading conditions.

[0036] For example, a nickel-titanium alloy wire is sintered into a spring, then straightened in cold water or cast into square, triangular, or other shapes, and then placed in hot water above 40°C, at which point the alloy wire returns to its original spring shape.

[0037] To improve the manufacturing precision of the internal window of the PCB, this embodiment of the invention utilizes the characteristics of shape memory alloys to create deformable structural components. During the lamination process, the deformable structural components, which are deformed to a first shape, act as a barrier and / or support for the pre-opened and stacked window, thereby reducing the amount of adhesive flowing into the window and / or preventing window deformation. After lamination, the deformable structural components are further deformed to a second shape that makes it easier to remove them from the window. The deformable structural components are then removed from the window to obtain the PCB.

[0038] For details, please refer to Figures 1 to 3 The PCB manufacturing method provided in this embodiment of the invention includes:

[0039] S1. Pre-open windows on each target core board / sub-board / adhesive sheet. The windowed areas on each target core board / sub-board / adhesive sheet are used to stack and form a window.

[0040] In this step, the target core board / sub-board / adhesive sheet that needs to be opened is first determined according to the depth position of the window in the PCB. Then, windows are opened on each target core board / sub-board / adhesive sheet according to the specifications of the window.

[0041] Because the process involves individually opening windows in the target core board / sub-board / adhesive sheet before lamination, the window depth is relatively small. Therefore, it is easier to control the size, position, and shape of the windows, thereby initially ensuring the accuracy of the window assembly formed by the subsequent overlapping of windowed areas in each layer.

[0042] S2. Provide auxiliary workpieces, including deformable structural parts made of shape memory alloys. The deformable structural parts can deform into a first shape for resisting adhesive and / or supporting the window when their temperature rises above the transition temperature, and deform into a second shape that can be detached from the window when their temperature drops below the transition temperature; the transition temperature is lower than the preset pressing temperature.

[0043] Based on the properties of shape memory alloys, deformable structural components can be controlled to deform into a first or second shape by adjusting the temperature.

[0044] In practical applications, the pressing temperature is relatively high, typically around 220 degrees Celsius. At this pressing temperature, the adhesive sheets layered between the core boards will melt to achieve the bonding function between the upper and lower core boards. The transition temperature can be a specific temperature value below the pressing temperature, such as 40 degrees Celsius, or a certain temperature range; there is no specific limitation.

[0045] S3. Stack each target core board / sub-board / adhesive sheet in sequence, place the deformable structural component of the auxiliary workpiece in the window formed by stacking the window areas of each target core board / sub-board / adhesive sheet, and keep the deformable structural component in the first shape by heating it to above the transformation temperature.

[0046] S4. At the pressing temperature, the stacked plates containing the deformable structural components that maintain the first shape are pressed together at high temperature to obtain the pressed plate.

[0047] S5. Cool the laminating plate to below the transition temperature, so that the deformable structural component can be deformed into a second shape that can be removed from the window. Remove the deformable structural component from the laminating plate to form a PCB.

[0048] In the above method, during the high-temperature pressing process, the window contains a deformable structural component. This component maintains its first shape because the pressing temperature is higher than its transition temperature. Furthermore, the deformable structural component in its first shape acts as a barrier and support for the window. Therefore, the deformable structural component, on the one hand, prevents excessive flow of molten adhesive sheets into the window, reducing the amount of adhesive flowing into the window; on the other hand, it abuts against the inner wall of the window, preventing deformation of the window's shape under high temperature and pressure. In summary, this embodiment of the invention utilizes a deformable structural component made of shape memory alloy, which can effectively improve the manufacturing precision of the window.

[0049] Furthermore, because the windows are individually opened before the laminates are stacked, it is relatively easy to manufacture windows with various overall conventional or irregular structures to meet the production needs of different application scenarios. For example, the cross-section of the window along the pressing direction is stepped or cylindrical.

[0050] From another perspective, after removing the deformable structural component, the window on the PCB is formed into different types such as through holes, blind vias, buried vias, or buried cavities. It should be noted that in this field, buried cavities are generally used to improve signal insertion loss; through holes, blind vias, and buried vias are signal conduction holes. The specific manufacturing requirements for buried cavities, through holes, blind vias, and buried vias differ not only in size and shape but also in whether the inner wall is metallized. Therefore, the above manufacturing process may require additional related steps to meet these requirements. For example, after removing the deformable structural component, the window may undergo copper plating and electroplating to obtain through holes with metallized inner walls. The specific implementation of this step is the same as conventional methods and will not be elaborated here.

[0051] If the window is specifically formed as a through-hole on the PCB, since it penetrates the top and bottom surfaces of the PCB, the core boards and bonding sheets of all layers of the PCB can be identified as the target objects for windowing. When opening windows, each core board and bonding sheet can be opened individually, or the core boards and bonding sheets can be grouped, and multiple core boards and / or bonding sheets in each group can be opened individually. This approach appropriately improves windowing efficiency while ensuring good windowing accuracy, as long as the windows are opened in multiple stages. This embodiment of the invention does not impose specific limitations on this.

[0052] Especially for through holes and blind holes with high depth-to-diameter ratios, the conventional manufacturing process involves first bonding the core boards together at high temperature with an adhesive sheet, and then drilling with a high-precision drill bit. This not only places high demands on the drill bit and increases processing costs, but also generates a large amount of burrs and adhesive residue inside the hole during the high-speed and long-term rotation of the drill bit. These residues are difficult to remove completely, resulting in poor hole shape and even affecting the subsequent copper plating effect, ultimately causing product quality problems and affecting the defect rate. In contrast, the embodiment of this invention uses a method of individually opening windows on each board before stacking and then stacking the boards. Compared with the conventional method of drilling after stacking and pressing, since each board is individually opened, the opening depth is smaller. This not only helps to ensure the accuracy of the hole diameter and position, but also produces fewer burrs and adhesive residue that are easier to remove. Furthermore, it does not require high-end processing tools and has lower manufacturing costs.

[0053] To further improve manufacturing precision, after opening windows in each target core board / sub-board / adhesive sheet, deburring and residual adhesive treatment can be performed on the windowed areas of each target core board / sub-board / adhesive sheet. Conventional methods can be used for deburring and residual adhesive treatment, and no specific limitations are imposed.

[0054] Furthermore, to achieve both good adhesive resistance and good support, the first shape of the deformable structural member can be designed to perfectly match the internal structure of the window, so that when deformed into the first shape, the outer wall of the deformable structural member placed inside the window abuts against the inner wall of the window. Of course, in other embodiments, the first shape can be flexibly designed according to actual needs, as long as it can provide a certain degree of support or adhesive resistance.

[0055] In actual processing, the order of the stacking process and the deformation process of deformed structural parts is determined according to the actual situation of the PCB.

[0056] If, after removing the deformable structural component, the window is specifically formed as a through-hole or blind via on the PCB, and at least one side of the through-hole or blind via penetrates the outer layer of the PCB, then the window area will be directly exposed after stacking, and the removal and placement of the deformable structural component will be unobstructed. In this case, the following two placement methods can be used:

[0057] The first method involves heating the material and maintaining it above the transformation temperature to deform the deformable structural component and keep it in its first shape. Then, the plates are stacked, and the deformable structural component is placed directly into the window formed after the plates are stacked. When using this method, the window area on the target core plate / sub-plate / adhesive sheet does not need to reserve too much space for the deformable structural component. As long as the deformable structural component, which is in its first shape (in an expanded state), is placed into the window, the deformable structural component will be locked and fixed.

[0058] The second method involves first stacking plates at room temperature, then placing the deformable structural component in its second shape into the window formed after stacking the plates; then raising the temperature and maintaining it above the transformation temperature to deform the deformable structural component into its first shape.

[0059] Meanwhile, since the window is exposed, the deformable structural component can extend freely beyond it. Therefore, when it needs to be removed, simply cooling it below its transformation temperature will allow the component to gradually shrink inward and deform into its second shape, extending beyond the window during the deformation process, making it easy to remove. In practical applications, the length or markings can be used to confirm whether the deformable structural component has completed its deformation; once confirmed, it can be removed.

[0060] If the window is specifically formed as an embedded hole or an embedded cavity on the PCB after the deformable structural component is removed, at least the target core board / sub-board / adhesive sheet should be stacked in sequence, including: providing an upper core board and a lower core board, and stacking the upper core board, each target core board / sub-board / adhesive sheet and the lower core board in sequence.

[0061] Since the embedded holes or cavities do not penetrate the outer layer of the PCB, the window area will be blocked by the outer core board after stacking. To enable the placement and removal of deformable structural components, the PCB manufacturing method provided in this embodiment further includes: before stacking, pre-creating a placement and removal channel on the upper core board and / or lower core board, which connects to the external space and the window, for placing and removing deformable structural components. Based on this, the placement and removal of deformable structural components within the window can be accomplished through the placement and removal channel.

[0062] Meanwhile, to facilitate pick-and-place operations, the auxiliary workpiece also includes a pick-and-place handle that connects to the deformable structural component. When the deformable structural component is built into the form, the pick-and-place handle is partially housed within the pick-and-place channel and partially extends outside the channel. This allows workers or robotic arms to easily grasp the pick-and-place handle to perform pick-and-place operations on the deformable structural component.

[0063] The shape of the pick-and-place handle matches the shape of the pick-and-place channel. For example, the pick-and-place channel is a small-diameter hole, and the shape of the pick-and-place handle and the second shape of the deformable structure are both columnar shapes that match the pick-and-place channel.

[0064] At this point, the following two insertion methods can be used:

[0065] The first method involves heating the material and maintaining it above the transformation temperature to deform the deformable structural component and keep it in the first shape. Then, the target core boards / sub-boards / adhesive sheets with windows are stacked, and the deformable structural component is placed directly into the window formed after stacking. Then, the upper core board and the lower core board are stacked. During the stacking process, the pick-and-place handle connected to the deformable structural component is passed through the pick-and-place channel opened on the upper core board and / or the lower core board.

[0066] The second method involves first stacking all the core boards at room temperature, then raising the temperature and maintaining it above the transformation temperature. The deformable structural components, originally in the second shape, are gradually inserted into the window through the pick-and-place channel. During the process of insertion, the deformable structural components gradually deform into the first shape.

[0067] Conversely, the method for removing deformable structural components from the form is as follows: cool the temperature to below the transformation temperature so that the deformable structural component gradually deforms into the first shape, and at the same time, use the pick-and-place handle to gradually remove the deformable structural component.

[0068] After removing the deformable structural component, the access channels can be plugged. Strongly adhesive resins or glues can be used to seal the access channels. The amount of plugging material can be determined based on the depth and diameter of the access channels, and conventional plugging processes can be selected.

[0069] Based on the same inventive concept, this embodiment of the invention also provides a PCB, which is manufactured according to the PCB manufacturing method described above. Due to the adoption of the above manufacturing method, the manufacturing precision of the window on the PCB of this embodiment is greatly improved, thereby effectively increasing product yield.

[0070] The above-described embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A PCB manufacturing method, characterized in that, include: Each target core board / sub-board / adhesive sheet is pre-windowed, and the windowed areas on each target core board / sub-board / adhesive sheet are used to stack and form a window; An auxiliary workpiece is provided, the auxiliary workpiece comprising a deformable structural member made of shape memory alloy, the deformable structural member being able to deform into a first shape for resisting adhesive and supporting the window when its temperature rises above the transition temperature, and into a second shape that can be detached from the window when its temperature drops below the transition temperature; the transition temperature is lower than a preset pressing temperature; At least the target core plates / sub-plates / adhesive sheets are stacked in sequence, and the deformable structural parts of the auxiliary workpiece are placed in the window formed by stacking the window areas of the target core plates / sub-plates / adhesive sheets, and the deformable structural parts are kept in the first shape by heating to above the transformation temperature. At the pressing temperature, the stacked plates containing deformable structural members that maintain a first shape are pressed together at high temperature to obtain a pressed plate; The laminating plate is cooled to below the transition temperature, causing the deformable structural component to deform into a second shape that can be removed from the window. The deformable structural component is then removed from the laminating plate to form a PCB.

2. The PCB manufacturing method according to claim 1, characterized in that, After the deformable structural component is removed, the window is specifically formed on the PCB as a through hole, blind hole, embedded hole, or embedded cavity.

3. The PCB manufacturing method according to claim 1, characterized in that, The cross-section of the window along the pressing direction is stepped or cylindrical.

4. The PCB manufacturing method according to claim 1, characterized in that, Also includes: After opening windows in each target core board / sub-board / adhesive sheet, deburring and residual adhesive treatment are performed on the windowed areas of each target core board / sub-board / adhesive sheet.

5. The PCB manufacturing method according to claim 2, characterized in that, When the window is specifically formed as an embedded hole or an embedded cavity on the PCB, the step of stacking each target core board / subboard / adhesive sheet in sequence includes: providing an upper core board and a lower core board, and stacking the upper core board, each target core board / subboard / adhesive sheet and the lower core board in sequence. The PCB manufacturing method further includes: before stacking the boards, pre-opening access channels for taking out and placing deformable structural components on the upper core board and / or the lower core board, which connect to the external space and windows.

6. The PCB manufacturing method according to claim 5, characterized in that, The PCB manufacturing method further includes: plugging the holes in the pick-and-place channel after removing the deformable structural component.

7. The PCB manufacturing method according to claim 5, characterized in that, The auxiliary workpiece also includes a pick-and-place handle connected to the deformable structural component; When the deformable structural component is built into the window, the pick-and-place handle is partially housed within the pick-and-place channel and partially extends outside the pick-and-place channel.

8. The PCB manufacturing method according to claim 1, characterized in that, When deformed into its first shape, the outer wall of the deformable structural member placed within the window abuts against the inner wall of the window.

9. The PCB manufacturing method according to claim 1, characterized in that, The second shape is columnar.

10. A PCB, characterized in that, The PCB is manufactured according to the PCB manufacturing method as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Circuit board with heat dissipation structure and manufacturing method thereof

    CN115776756A

  • Flexible circuit board

    CN205305224U