Display panel and display device

By setting partition grooves on the isolation column of the OLED display panel and filling in inorganic materials to prevent the entry of water vapor and oxygen, the problem of luminescent unit failure caused by water absorption of the isolation column is solved, and the reliability and service life of the panel are improved.

CN117440714BActive Publication Date: 2024-11-08HKC CORP LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202311577426.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-23
Publication Date
2024-11-08
Estimated Expiration
2043-11-23

AI Technical Summary

Technical Problem

The isolation column of the OLED display panel is prone to absorb water, causing water vapor and oxygen to enter the light emitting unit, causing device failure.

Method used

A partition groove is provided on the isolation column, and a partition part of the inorganic material is filled therein to form a longer water vapor intrusion path to block the entry of external water vapor and oxygen. Using the density of the inorganic material and the absorption effect of the organic light emitting layer, the phase is independently encapsulated The adjacent light emitting unit.

Benefits of technology

Effectively prevent water vapor and oxygen intrusion, avoid regional failure caused by failure of a single light emitting unit, and improve the service life and packaging effect of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117440714B_ABST
    Figure CN117440714B_ABST
Patent Text Reader

Abstract

The present application discloses a display panel and a display device, wherein the display panel comprises a substrate, a pixel definition layer and a plurality of light-emitting units, wherein the pixel definition layer is located on the substrate and is provided with a plurality of pixel openings; wherein the plurality of light-emitting units are located on the substrate and are respectively provided in the plurality of pixel openings; wherein the pixel definition layer comprises a plurality of isolation columns, and at least one of the light-emitting units is provided between adjacent isolation columns; wherein at least one isolation groove is provided on the isolation column, and the isolation groove is provided on the side of the pixel definition layer away from the substrate, and at least one of the isolation grooves is provided around the pixel opening; wherein the isolation groove is filled with an isolation portion, the isolation column is formed of an organic material, and the isolation portion is at least partially formed of an inorganic material. By providing the isolation portion on the isolation column, water vapor intrusion is blocked, the packaging effect of the display panel is improved, and the reliability and yield of the display panel are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a display device. Background Art

[0002] Organic light emitting diodes (OLEDs) have the advantages of surface light source, cold light, energy saving, fast response, flexibility, ultra-lightness and low cost, and their mass production technology is becoming increasingly mature. In order to achieve high resolution and colorization of passive matrix OLEDs and better solve the problems of low cathode template resolution and low device yield, an isolation column structure was introduced in actual research, that is, instead of using a metal template in device preparation, an insulating partition is made on the substrate before evaporating the organic film and the metal cathode, and finally the different pixels of the device are separated to realize a pixel array. Among them, since OLEDs have poor stability and are extremely sensitive to water and oxygen, packaging technology is particularly critical.

[0003] The purpose of encapsulation is mainly to prevent water vapor and oxygen from entering the OLED, and the isolation column also needs to be set under the encapsulation layer. However, the isolation column easily absorbs water during the process and in the water vapor environment, causing the water vapor to extend through the interface between the isolation column and the upper and lower film layers, causing the light-emitting unit to fail. Therefore, the field is in urgent need of a technical solution to solve the problem of the light-emitting unit failing due to the isolation column easily absorbing water. Summary of the invention

[0004] The purpose of the present application is to provide a display panel and a display device, which prevent the intrusion of water vapor by arranging a partition part on the isolation column, thereby improving the packaging effect of the display panel and improving the reliability and yield of the display panel.

[0005] The present application discloses a display panel, which includes a substrate, a pixel definition layer and a plurality of light-emitting units, wherein the pixel definition layer is located on the substrate and is provided with a plurality of pixel openings; the plurality of light-emitting units are located on the substrate and are respectively arranged in the plurality of pixel openings; wherein the pixel definition layer includes a plurality of isolation columns, and at least one of the light-emitting units is arranged between adjacent isolation columns; at least one isolation groove is arranged on the isolation column, and the isolation groove is arranged on a side of the isolation column away from the substrate, and at least one of the isolation grooves is arranged around the pixel opening; the isolation groove is filled with a isolation portion, the isolation column is formed of an organic material, and the isolation portion is at least partially formed of an inorganic material.

[0006] Optionally, the height of the partition portion is consistent with the depth of the partition groove.

[0007] Optionally, the light-emitting unit includes a bottom electrode, a light-emitting layer and a top electrode; the sum of the depth of the partition groove and the thickness of the bottom electrode is greater than or equal to the thickness of the isolation column.

[0008] Optionally, a plurality of partition grooves are provided on the isolation column, and the interval width between adjacent partition grooves is greater than or equal to the radial width of the partition groove; and the radial width of the partition groove gradually increases along the light emitting direction.

[0009] Optionally, a groove is provided on the isolation column, a plurality of the partition grooves are formed at the bottom of the groove, and the depth of the partition groove is greater than the depth of the groove; the radial width of the groove is greater than the sum of the radial widths of the plurality of the partition grooves; the partition portion includes a first inorganic insulating layer, a water vapor absorption layer and a second inorganic insulating layer, the water vapor absorption layer is arranged on the first inorganic insulating layer, and the second inorganic insulating layer is arranged on the water vapor absorption layer; the first inorganic insulating layer and the water vapor absorption layer are arranged in the partition groove; the second inorganic insulating layer extends from the partition groove to the groove and fills the groove.

[0010] Optionally, the interval between adjacent partition grooves is at least 4 um.

[0011] Optionally, the partition portion includes a first inorganic insulating layer, a water vapor absorption layer and a second inorganic insulating layer, the water vapor absorption layer is arranged on the first inorganic insulating layer, and the second inorganic insulating layer is arranged on the water vapor absorption layer; the water vapor absorption layer is used to absorb water vapor.

[0012] Optionally, the water vapor absorption layer includes an organic light-emitting layer, which includes a red organic light-emitting layer, a green organic light-emitting layer or a blue organic light-emitting layer; the display panel also includes an encapsulation layer, which includes a first inorganic encapsulation layer, an organic encapsulation layer and a second inorganic encapsulation layer, the first inorganic encapsulation layer is arranged on the light-emitting unit, the organic encapsulation layer is arranged on the first inorganic encapsulation layer, and the second inorganic encapsulation layer is arranged on the organic encapsulation layer; the second inorganic insulating layer and the first inorganic encapsulation layer are formed using the same material and the same process.

[0013] Optionally, the partition groove is formed by an embossing process; the radial width of the partition groove is greater than or equal to 0.5 um and less than or equal to 1 um; and the radial width of the side wall of the partition groove is greater than or equal to 4 um.

[0014] The present application also discloses a display device, comprising a driving circuit and the above-mentioned display panel, wherein the driving circuit is used to drive the display panel to display.

[0015] The present application provides partition grooves on multiple isolation columns of the pixel definition layer, and partition parts are filled in the partition grooves. The partition parts are formed of inorganic materials, and the density of inorganic materials is used to isolate the extension of water vapor and oxygen in the isolation columns, which can effectively prevent external water vapor and oxygen from entering the light-emitting unit. The side wall contact between the partition part and the partition groove is used to form a longer water vapor invasion path, further reducing the invasion of water vapor and oxygen. In addition, the partition groove is used to make adjacent light-emitting units independently packaged. When a light-emitting unit is invaded by water vapor, water vapor is effectively prevented from invading adjacent light-emitting units, thereby avoiding the failure of one light-emitting unit causing the failure of light-emitting units in an area. The possibility that water vapor and oxygen may cause the failure of the light-emitting unit is greatly improved, and the service life of the display panel is increased. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The included drawings are used to provide a further understanding of the embodiments of the present application, which constitute a part of the specification, are used to illustrate the implementation methods of the present application, and together with the text description, explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. In the drawings:

[0017] Figure 1 is a schematic diagram of a display panel according to a first embodiment of the present application;

[0018] Figure 2 is a schematic diagram of the manufacturing process of the isolation column of the first embodiment of the present application;

[0019] Figure 3 is a schematic diagram of a second display panel of the first embodiment of the present application;

[0020] Figure 4 is a schematic diagram of a display panel according to a second embodiment of the present application;

[0021] Figure 5 is a schematic diagram of a second display panel of a second embodiment of the present application;

[0022] Figure 6 is a schematic diagram of a display device of the present application.

[0023] Among them, 100, display panel; 110, substrate; 102, pixel opening; 120, pixel definition layer; 121, isolation column; 122, partition groove; 123, groove; 130, partition part; 131, first inorganic insulating layer; 132, water vapor absorption layer; 133, second inorganic insulating layer; 140, light-emitting unit; 141, bottom electrode; 142, light-emitting layer; 143, top electrode; 150, encapsulation layer; 151, first inorganic encapsulation layer; 152, organic encapsulation layer; 153, second inorganic encapsulation layer; 200, display device; 210, driving circuit. DETAILED DESCRIPTION

[0024] It should be understood that the terms used herein, the specific structures and functional details disclosed are only for describing specific embodiments and are representative, but the present application can be implemented in many alternative forms and should not be construed as being limited to only the embodiments described herein.

[0025] In the description of the present application, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating relative importance or implicitly indicating the number of technical features indicated. Therefore, unless otherwise specified, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features; "multiple" means two or more. In addition, the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicating orientation or positional relationships are described based on the orientation or relative positional relationships shown in the accompanying drawings, and are only for the convenience of describing the simplified description of the present application, rather than indicating that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to the specific circumstances.

[0026] The present application is described in detail below with reference to the accompanying drawings and optional embodiments.

[0027] Figure 1 is a schematic diagram of a display panel of the first embodiment of the present application, see Figure 1As shown, the present application discloses a display panel 100, which includes a substrate 110, a pixel definition layer 120 and a plurality of light-emitting units 140, wherein the pixel definition layer 120 is located on the substrate 110 and is provided with a plurality of pixel openings 102; the plurality of light-emitting units 140 are located on the substrate 110 and are respectively arranged in the plurality of pixel openings 102; wherein the pixel definition layer 120 includes a plurality of isolation columns 121, and at least one of the light-emitting units 140 is arranged between adjacent isolation columns 121; at least one partition groove 122 is arranged on the isolation column 121, and the partition groove 122 is arranged on a side of the isolation column 121 away from the substrate 110, and at least one of the partition grooves 122 is arranged around the pixel opening 102; the partition groove 122 is filled with a partition portion 130, the isolation column 121 is formed of an organic material, and the partition portion 130 is at least partially formed of an inorganic material.

[0028] The present application provides partition grooves 122 on a plurality of isolation columns 121 of the pixel definition layer 120, and partition portions 130 are filled in the partition grooves 122. The partition portions 130 are formed of inorganic materials, and the compactness of the inorganic materials is used to isolate the extension of water vapor and oxygen in the isolation columns 121, so as to effectively prevent external water vapor and oxygen from entering the light-emitting unit 140. The sidewalls of the partition portions 130 and the partition grooves 122 are in contact to form a longer water vapor intrusion path, further reducing the intrusion of water vapor and oxygen. In addition, the partition grooves 122 are used to make adjacent light-emitting units 140 be independently packaged. When a light-emitting unit 140 is invaded by water vapor, water vapor is effectively prevented from invading adjacent light-emitting units 140, thereby avoiding the failure of one light-emitting unit 140 leading to the failure of light-emitting units 140 in an area. The possibility that water vapor and oxygen may cause the light-emitting unit 140 to fail is greatly improved, and the service life of the display panel 100 is improved.

[0029] The isolation columns 121 are used to separate adjacent light-emitting units 140, and a plurality of isolation columns 121 are connected vertically and horizontally to form a pixel definition layer 120. The area without the isolation columns 121 is the pixel opening 102, also known as the opening area of ​​the display panel 100, and the corresponding area with the isolation columns 121 is the non-opening area. This solution mainly improves the isolation columns 121 in the non-opening area to solve the problem that the isolation columns 121 absorb water and are not waterproof and oxygen-proof.

[0030] It is understandable that the light-emitting unit 140 in the OLED display panel 100 is susceptible to degradation caused by internal factors and degradation caused by external factors, such as degradation caused by the reaction between the light-emitting layer 142 and the film layer interface, such as degradation of the electrode and the light-emitting layer 142 caused by water vapor and oxygen. Generally speaking, the thickness of the isolation column 121 will be higher than the height of the light-emitting unit 140, and relatively speaking, the thickness of the isolation column 121 will be thicker. In practice, it is impossible to select an inorganic insulating material with good compactness to form it, and the film thickness of the inorganic insulating layer cannot meet this height requirement. Therefore, the isolation column 121 is generally formed by an organic material, but the compactness of the organic material is not as good as that of the inorganic material, resulting in the existence of water absorption characteristics. Therefore, when water vapor enters the isolation column 121, the water vapor will extend through the interface between the isolation column 121 and the upper and lower film layers, or directly extend through the inside of the organic material film layer. The paths of these two extension methods are both short, and it is easy to cross the isolation column 121 and enter the adjacent light-emitting unit 140, causing damage to the device. In this regard, the present solution utilizes the partition groove 122 and the partition portion 130 to solve the above problem.

[0031] Figure 2 is a schematic diagram of the process of manufacturing the isolation column of the first embodiment of the present application, see Figure 2 As shown, the partition groove 122 of the present application is formed by an imprinting process. Imprinting technology is to complete the transfer of graphics through contact imprinting, which is equivalent to the exposure and development process in optical exposure technology, and then use the etching transfer process to transfer the structure to other materials. Among them, nanoimprinting technology overcomes the resolution limit problem caused by the light diffraction phenomenon in optical exposure technology, and demonstrates the unique advantages of ultra-high resolution, high efficiency, low cost, and suitability for industrial production. The latest nanoimprinting (NIL) overlay accuracy has reached a circuit line width of 5nm. Currently, the three common nanoimprinting technologies are hot pressing, ultraviolet and molding. This proposal uses hot pressing technology as an example to illustrate the preparation process of the special structure of the water vapor absorption layer in the isolation column 121. The imprinting material is a high-transmittance resin, that is, a common organic resin such as the pixel definition layer 120.

[0032] The specific process includes forming a pixel definition layer 120 on a substrate 110; secondly, using a printing film to perform hot stamping on the pixel definition layer 120, and performing a demolding process after the stamping is completed, so as to form a pixel opening 102, form an isolation column 121 in a non-opening area, and form a partition groove 122 on the isolation column 121; it can be understood that using printing films of different widths can realize the simultaneous process of the pixel opening 102 and the partition groove 122 of different widths. After demolding, a specific reactive ion etching can be used to remove the residual glue at the edge of the pattern.

[0033] In this solution, the film layer quality of the partition groove 122 formed by the printed film is better and has higher precision. In addition, it can be processed synchronously with the pixel opening 102, and batch processing can be performed using a mold, reducing the complexity and resource requirements of the manufacturing process. The cross-sectional shape of the isolation column 121 in this application can be a standing trapezoid or an inverted trapezoidal overhanging structure. In this solution, only the standing trapezoidal isolation column 121 is used as an example for description, and is not limited to the standing trapezoidal isolation column 121.

[0034] Specifically, the light-emitting unit 140 includes a bottom electrode 141, a light-emitting layer 142 and a top electrode 143, wherein the light-emitting layer 142 is disposed on the bottom electrode 141, and the top electrode 143 is disposed on the light-emitting layer 142. Generally speaking, the bottom electrode 141 partially overlaps with the isolation column 121 in the projection of the substrate 110, while the isolation groove 122 does not overlap with the orthographic projection of the bottom electrode 141 in the substrate 110.

[0035] Specifically, the sum of the depth of the partition groove 122 and the thickness of the bottom electrode 141 is greater than or equal to the thickness of the isolation column 121. The depth of the partition groove 122 in this solution is deeper, and the depth of the partition groove 122 is at least greater than the thickness of the light-emitting layer 142 of the light-emitting unit 140 and the top electrode 143. In other words, the bottom height of the partition groove 122 is not higher than the upper surface of the bottom electrode 141, or the bottom height of the partition groove 122 is consistent with the height of the bottom electrode 141.

[0036] The depth of the partition groove 122 formed by the embossing process in this solution can be deeper, so that the material of the partition part 130 filled into the partition groove 122 is sufficient to prevent the intrusion of water vapor, and the water vapor intrusion path inside the organic material film layer is interrupted by the partition part 130 to the maximum extent. It is worth mentioning that in this solution, in the direction parallel to the substrate 110, a stacked arrangement of organic layers, inorganic layers and organic layers is actually formed, and the inorganic layer sandwiched between the organic layers is used to prevent the intrusion of water vapor, thereby improving the packaging effect of the display panel 100. It can be understood that the oxygen intrusion path is roughly the same as the water vapor path. In this application, water vapor intrusion is mainly used as an example for illustration. Relatively speaking, the ability to block water vapor intrusion also has the function of blocking oxygen intrusion, which will not be elaborated here.

[0037] Specifically, the height of the partition portion 130 is consistent with the depth of the partition groove 122 , the radial width of the partition groove 122 is greater than or equal to 0.5 um and less than or equal to 1 um; the radial width of the side wall of the partition groove 122 is greater than or equal to 4 um.

[0038] In one embodiment, the partition portion 130 may include an inorganic insulating layer, that is, the partition groove 122 is completely filled with the inorganic insulating layer.

[0039] Figure 3 It is a schematic diagram of the second display panel of the first embodiment of the present application. In this embodiment, the partition portion 130 includes a first inorganic insulating layer 131, a water vapor absorption layer 132 and a second inorganic insulating layer 133. The water vapor absorption layer 132 is arranged on the first inorganic insulating layer 131, and the second inorganic insulating layer 133 is arranged on the water vapor absorption layer 132; the water vapor absorption layer 132 is used to absorb water vapor.

[0040] In this solution, the partition groove 122 is not completely filled with inorganic materials. A water vapor absorption layer 132 is set between the inorganic insulating layers, wherein the water vapor absorption layer 132 can be an organic material. Then, a laminated structure of inorganic materials, organic materials and inorganic materials is formed in the vertical direction of the substrate 110, forming a laminated structure in the light emitting direction to prevent water vapor from invading. Moreover, since the partition groove 122 in this solution is deeper, more inorganic materials are needed to completely fill the partition groove 122. Therefore, by adopting a laminated setting, the inorganic film layer does not need to be particularly thick, and can be formed simultaneously with other inorganic film layers in the display panel 100 process, such as the first inorganic encapsulation layer 151 in the encapsulation layer 150.

[0041] Specifically, the display panel 100 further includes an encapsulation layer 150, the encapsulation layer 150 includes a first inorganic encapsulation layer 151, an organic encapsulation layer 152 and a second inorganic encapsulation layer 153, the first inorganic encapsulation layer 151 is disposed on the light-emitting unit 140, and the organic encapsulation layer 152 is disposed on the first inorganic encapsulation layer 151. The display panel 100 further includes a light shielding layer, which is disposed on the pixel definition layer 120 and does not overlap with the pixel opening 102 on the orthographic projection of the substrate 110. The second inorganic encapsulation layer 153 is disposed on the organic encapsulation layer 152; the second inorganic insulating layer 133 and the first inorganic encapsulation layer 151 are formed using the same material and the same process.

[0042] In this embodiment, after the first inorganic insulating layer 131 and the water vapor absorption layer 132 are formed in the partition groove 122, the step of forming the light-emitting unit 140 can be carried out. When the light-emitting unit 140 is packaged after formation, the partition groove 122 can be filled with the first inorganic packaging layer 151 as the second inorganic insulating layer 133.

[0043] In another embodiment, the water vapor absorption layer 132 can also be an organic light-emitting layer, and the organic light-emitting layer includes a red organic light-emitting layer, a green organic light-emitting layer or a blue organic light-emitting layer. The entire isolation column 121 of this solution includes a multi-layer film layer interface. After entering the organic outer wall of the isolation column 121, the water vapor will extend inward along the interface. Since there are interfaces between the organic film layer and the inorganic film layer inside, the water vapor will preferentially extend along these interfaces, and the extension path can be extended many times. At the same time, the middle organic light-emitting layer can also effectively absorb water and oxygen, and act as a water and oxygen absorption layer. When the subsequent packaging fails, the water vapor entering will be absorbed and stored, which can further improve the packaging life of the device. In this solution, the organic light-emitting layer has the function of absorbing water vapor and oxygen as a depletion layer. When water vapor or oxygen enters the interior of the isolation column 121, the organic light-emitting layer set here can be used as an absorbent to absorb water vapor or oxygen to prevent further diffusion of water vapor and oxygen.

[0044] Relatively speaking, this solution can be formed synchronously with the light-emitting layer 142 in the light-emitting unit 140 during the process of the light-emitting unit 140. After the process of the top electrode 143 of the light-emitting unit 140 is completed, the first inorganic encapsulation layer 151 can be used as the second inorganic insulating layer 133 to fill the partition groove 122. In this embodiment, the first inorganic insulating layer 131 mentioned above can be omitted, and only the organic light-emitting layer and the second inorganic insulating layer 133 are provided in the partition groove 122.

[0045] Specifically, along the light emitting direction, the radial width of the partition groove 122 gradually increases. The light emitting direction is perpendicular to the substrate 110 and is the direction from the substrate 110 to the pixel definition layer 120. When forming the first inorganic insulating layer 131, since the sidewall of the partition groove 122 has a certain inclination angle, it is not completely perpendicular to the substrate 110. Therefore, a thin first inorganic layer is also formed on the sidewall of the partition groove 122, and the first inorganic layer can protect the internal organic light emitting layer to a certain extent.

[0046] Figure 4 is a schematic diagram of a display panel of the second embodiment of the present application, see Figure 4As shown, the present application also discloses a display panel 100, the display panel 100 includes a substrate 110, a pixel definition layer 120 and a plurality of light-emitting units 140, the pixel definition layer 120 is located on the substrate 110 and is provided with a plurality of pixel openings 102; the plurality of light-emitting units 140 are located on the substrate 110 and are respectively provided in the plurality of pixel openings 102; wherein the pixel definition layer 120 includes a plurality of isolation columns 121, at least one of the light-emitting units 140 is provided between adjacent isolation columns 121; a plurality of partition grooves 122 are provided on the isolation columns 121, the partition grooves 122 are provided on the side of the pixel definition layer 120 away from the substrate 110, and at least one of the partition grooves 122 is provided around the pixel opening 102. A plurality of partition grooves 122 are provided on the isolation columns 121, and the interval width between adjacent partition grooves 122 is greater than or equal to the radial width of the partition grooves 122.

[0047] In this solution, a plurality of partition grooves 122 are arranged on the isolation column 121 corresponding to the same non-opening area position, and each partition groove 122 is filled with at least inorganic material. In the direction parallel to the substrate 110, the inorganic material in the plurality of partition grooves 122 and the organic material between the plurality of partition grooves 122 form a multilayer stacking structure of inorganic material and organic material. The inorganic and organic multilayer stacking arrangement can prevent water vapor from extending from one light-emitting unit 140 to another light-emitting unit 140 to the greatest extent. This prevents the failure of one light-emitting unit 140 from causing the failure of light-emitting units 140 in an area. The possibility that water vapor and oxygen may cause the light-emitting unit 140 to fail is greatly improved, and the service life of the display panel 100 is improved.

[0048] Specifically, the interval between adjacent partition grooves 122 is at least 4 um, and the radial width of the partition groove 122 is greater than or equal to 0.5 um and less than or equal to 1 um. The width of the partition groove 122 should be greater than the minimum precision of nano-imprinting, which can generally be about 0.5 um.

[0049] The wall thickness between the partition grooves 122 should be more than 4um to ensure sufficient support strength, and the number can be set according to the width of the isolation column 121. After the partition grooves 122 are formed by trenching, the first inorganic insulating layer 131 material is filled by inkjet printing, and the filling height is 1 to 2um. After the first inorganic insulating layer 131 is filled, the inkjet printing process of the light-emitting layer 142 is carried out on the entire panel, and the deep grooves will also be filled with the corresponding light-emitting layer 142. All light-emitting layer 142 film layers or several of them can be selectively filled. The film layer that is easy to absorb water and oxygen can be preferred, and the filling height can be determined according to the amount of ink at that position. After the light-emitting layer 142 is filled, the second inorganic insulating layer 133 is filled to fill the trench plane and provide a film layer interface between organic materials and inorganic materials. In this embodiment, after the first inorganic insulating layer 132 and the organic material are formed in the partition groove 122, the step of forming the light-emitting unit 140 can be performed. When the light-emitting unit 140 is packaged after formation, the partition groove 122 can be filled with the first inorganic packaging layer 151 as the second inorganic insulating layer 133.

[0050] In another embodiment, the water vapor absorption layer 132 can also be an organic light-emitting layer. The organic light-emitting layer includes a red organic light-emitting layer, a green organic light-emitting layer or a blue organic light-emitting layer. At the same isolation column 121 position, organic light-emitting layers of different colors can be formed in different partition grooves 122. The entire isolation column 121 of this solution includes a multi-layer film layer interface. After entering the organic outer wall of the isolation column 121, the water vapor will extend inward along the interface. Since there are interfaces between the organic film layer and the inorganic film layer inside, the water vapor will preferentially extend along these interfaces, and the extension path can be extended many times. At the same time, the middle organic light-emitting layer can also effectively absorb water and oxygen, and act as a water and oxygen absorption layer. When the subsequent packaging fails, the water vapor entering will be absorbed and stored, which can further improve the packaging life of the device. In this solution, the organic light-emitting layer has the function of absorbing water vapor and oxygen as a depletion layer. When there is water vapor or oxygen entering the interior of the isolation column 121, the organic light-emitting layer set here can be used as an absorbent to absorb water vapor or oxygen to prevent further diffusion of water vapor and oxygen.

[0051] Relatively speaking, this solution can be formed synchronously with the light-emitting layer 142 in the light-emitting unit 140 during the process of the light-emitting unit 140. After the process of the top electrode 143 of the light-emitting unit 140 is completed, the first inorganic encapsulation layer 151 can be used as the second inorganic insulating layer 133 to fill the partition groove 122. In this embodiment, the first inorganic insulating layer 131 mentioned above can be omitted, and only the organic light-emitting layer and the second inorganic insulating layer 133 are provided in the partition groove 122.

[0052] Specifically, along the light emitting direction, the radial width of the partition groove 122 gradually increases, and the cross-sectional shape of the partition groove 122 is a trapezoid.

[0053] In another embodiment, the cross-sectional shape of the partition groove 122 may also be rectangular, and the bottom of the partition groove 122 may also be arc-shaped, etc. The present application may adopt hot stamping technology to produce various shapes.

[0054] Figure 5 is a schematic diagram of a second display panel of the second embodiment of the present application, see Figure 5 As shown, in another embodiment, a groove 123 is provided on the isolation column 121, a plurality of the partition grooves 122 are formed at the bottom of the groove 123, and the depth of the partition groove 122 is greater than the depth of the groove 123; the radial width of the groove 123 is greater than the sum of the radial widths of the plurality of the partition grooves 122; the partition portion 130 includes a first inorganic insulating layer 131, a water vapor absorption layer 132 and a second inorganic insulating layer 133, the water vapor absorption layer 132 is provided on the first inorganic insulating layer 131, and the second inorganic insulating layer 133 is provided on the water vapor absorption layer 132; the first inorganic insulating layer 131 and the water vapor absorption layer 132 are provided in the partition groove 122; the second inorganic insulating layer 133 extends from the partition groove 122 to the groove 123 and fills the groove 123.

[0055] In this solution, the groove 123 is mainly filled with the first inorganic encapsulation layer 151, and a larger area of ​​the first inorganic encapsulation layer 151 can be formed in the groove 123, and a larger inorganic material is formed for the isolation column 121. In accordance with the main concept of the present application, the isolation column 121 of organic material is used as a frame, and the inorganic material is filled in the partition groove 122 of the isolation column 121 to form a seal.

[0056] In the top view of the isolation column 121, the partition groove 122 can be in the shape of a Chinese character "Yu" or a strip. Both solutions are based on the premise that the outer wall of the isolation column 121 needs to be closed, that is, the annular partition groove 122 and the independent multiple strip-shaped partition grooves 122 solution. Both solutions can extend the extension path of water vapor to the greatest extent, and provide multiple water vapor extension paths at the same time to avoid rapid extension under a single path.

[0057] Figure 6 is a schematic diagram of the display device of the present application, see Figure 6 As shown, the present application also discloses a display device 200 , which includes a driving circuit 210 and a display panel 100 described in any one of the above embodiments, wherein the driving circuit 210 drives the display panel 100 to display, and the display panel 100 is an organic light-emitting display panel 100 .

[0058] The present application provides partition grooves 122 on a plurality of isolation columns 121 of the pixel definition layer 120, and partition portions 130 are filled in the partition grooves 122. The partition portions 130 are formed of inorganic materials, and the compactness of the inorganic materials is used to isolate the extension of water vapor and oxygen in the isolation columns 121, so as to effectively prevent external water vapor and oxygen from entering the light-emitting unit 140. The sidewalls of the partition portions 130 and the partition grooves 122 are in contact to form a longer water vapor intrusion path, further reducing the intrusion of water vapor and oxygen. In addition, the partition grooves 122 are used to make adjacent light-emitting units 140 be independently packaged. When a light-emitting unit 140 is invaded by water vapor, water vapor is effectively prevented from invading adjacent light-emitting units 140, thereby avoiding the failure of one light-emitting unit 140 leading to the failure of light-emitting units 140 in an area. The possibility that water vapor and oxygen may cause the light-emitting unit 140 to fail is greatly improved, and the service life of the display panel 100 is improved.

[0059] It should be noted that the inventive concept of the present application can form a large number of embodiments, but the length of the application document is limited and it is impossible to list them one by one. Therefore, under the premise of no conflict, the embodiments or technical features described above can be arbitrarily combined to form new embodiments. After the embodiments or technical features are combined, the original technical effects will be enhanced.

[0060] The above content is a further detailed description of the present application in combination with specific optional implementation methods, and it cannot be determined that the specific implementation of the present application is limited to these descriptions. For ordinary technicians in the technical field to which the present application belongs, several simple deductions or substitutions can be made without departing from the concept of the present application, which should be deemed to fall within the scope of protection of the present application.

Claims

1. A display panel, characterized in that: include: substrate; A pixel definition layer, located on the substrate, and provided with a plurality of pixel openings; as well as A plurality of light emitting units are located on the substrate and are respectively arranged in the plurality of pixel openings; Wherein, the pixel definition layer includes a plurality of isolation columns, and at least one light-emitting unit is arranged between adjacent isolation columns; At least one partition groove is disposed on the isolation column, the partition groove is disposed on a side of the isolation column away from the substrate, and at least one of the partition grooves is disposed around the pixel opening; The partition groove is filled with a partition part, the isolation column is formed of an organic material, and the partition part is at least partially formed of an inorganic material; The light-emitting unit comprises a bottom electrode, a light-emitting layer and a top electrode; the sum of the depth of the partition groove and the thickness of the bottom electrode is greater than or equal to the thickness of the isolation column.

2. The display panel according to claim 1, characterized in that: The height of the partition portion is consistent with the depth of the partition groove.

3. The display panel according to claim 1, characterized in that: A plurality of partition grooves are arranged on each of the isolation columns, and the interval width between adjacent partition grooves is greater than or equal to the radial width of the partition groove; along the light emitting direction, the radial width of the partition groove gradually increases.

4. The display panel according to claim 3, characterized in that: The isolation column is provided with a groove, a plurality of the partition grooves are formed at the bottom of the groove, and the depth of the partition groove is greater than the depth of the groove; the radial width of the groove is greater than the sum of the radial widths of the plurality of the partition grooves; The partition portion includes a first inorganic insulating layer, a water vapor absorbing layer, and a second inorganic insulating layer, wherein the water vapor absorbing layer is disposed on the first inorganic insulating layer, and the second inorganic insulating layer is disposed on the water vapor absorbing layer; The first inorganic insulating layer and the water vapor absorption layer are arranged in the partition groove; the second inorganic insulating layer extends from the partition groove to the groove and fills the groove.

5. The display panel according to claim 3, characterized in that: The interval between adjacent partition grooves is at least 4 um.

6. The display panel according to claim 1, characterized in that: The partition portion includes a first inorganic insulating layer, a water vapor absorption layer and a second inorganic insulating layer, the water vapor absorption layer is arranged on the first inorganic insulating layer, and the second inorganic insulating layer is arranged on the water vapor absorption layer; the water vapor absorption layer is used to absorb water vapor.

7. The display panel according to claim 6, characterized in that: The water vapor absorption layer includes an organic light-emitting layer, and the organic light-emitting layer includes a red organic light-emitting layer, a green organic light-emitting layer or a blue organic light-emitting layer; The display panel further includes an encapsulation layer, the encapsulation layer including a first inorganic encapsulation layer, an organic encapsulation layer, and a second inorganic encapsulation layer, the first inorganic encapsulation layer is disposed on the light emitting unit, the organic encapsulation layer is disposed on the first inorganic encapsulation layer, and the second inorganic encapsulation layer is disposed on the organic encapsulation layer; The second inorganic insulating layer and the first inorganic encapsulation layer are formed by using the same material and the same process.

8. The display panel according to claim 1, characterized in that: The partition groove is formed by an embossing process; the radial width of the partition groove is greater than or equal to 0.5um and less than or equal to 1um; the radial width of the side wall of the partition groove is greater than or equal to 4um.

9. A display device, characterized in that: It comprises a driving circuit and the display panel according to any one of claims 1 to 8, wherein the driving circuit is used to drive the display panel to display.

Citation Information

Patent Citations

  • Display panel and display screen

    CN108538899A

  • Display panel, preparation method thereof and display device

    CN110828519A

  • Display panel and preparation method thereof and display device

    CN111725422A

  • Display panel and preparation method thereof

    CN115498126A

  • Display panel and display device

    WO2023092672A1