A yield strength testing machine for aluminum alloys without heat treatment for low pressure casting
By setting up placement, detection and alignment devices in the yield strength test machine, the problem of operator contacting fixtures is solved, and safe and efficient removal and placement of aluminum alloy test rods is achieved, ensuring detection accuracy and fault detection, and improving Production safety and efficiency.
Patent Information
- Application Number
- CN202311501201.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-13
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2043-11-13
AI Technical Summary
When conducting the yield strength test of aluminum alloy castings, the operator needs to contact the fixture to pick up and place the test rod, which is at risk of incorrectly operating the start fixture to clamp the hand, which affects production safety.
A heat-free aluminum alloy for low-pressure casting and its manufacturing method are designed. By setting up a placement device, a detection device and a alignment device in the yield strength test machine, the test rod can be removed and placed without the operator touching the fixture, ensuring that Safety and ensure detection accuracy and fault detection through the cooperation of hydraulic cylinder and barrier plate.
It realizes the removal and placement of the test rod without the operator touching the clamp, improves the safety of the test process, and ensures the accuracy of the test results and the timely failure through the precise alignment device and the hydraulic cylinder. Testing avoids waste of labor costs and defective product identification errors.
Smart Images

Figure CN117535566B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum alloy processing, and in particular to a heat-treatment-free aluminum alloy for low-pressure casting and a manufacturing method thereof. Background Art
[0002] Aluminum alloy castings have good strength and good toughness and are widely used in industry. In the existing method of manufacturing aluminum alloy castings, there is a step that requires a yield strength test on a test bar that is sawed off a part of the produced casting product or cast separately, so as to detect whether the product performance is qualified. When testing the test section test bar sawed off the casting, it is necessary to manually put the test bar removed from the casting into a yield strength testing machine. After the test is completed, the test bar is also required to be manually taken out of the yield strength testing machine. Therefore, when taking and placing the test bar, the operator's hand will inevitably come into contact with the clamp that clamps the test bar on the testing machine, so there is a risk of pinching the hand due to misoperation of the starting clamp, thereby affecting production safety. Summary of the invention
[0003] (1) Technical issues to be solved
[0004] The purpose of the present invention is to overcome the shortcomings of the prior art, meet actual needs, and provide a low-pressure casting heat-treatment-free aluminum alloy and a manufacturing method thereof, which can take out and put in the test rod without the operator touching the clamp, thereby conducting a yield strength test more safely, so as to solve the above-mentioned technical problems.
[0005] (2) Technical solution
[0006] In order to achieve the purpose of the present invention, the technical solution adopted by the present invention is:
[0007] A heat-treatment-free aluminum alloy for low-pressure casting comprises 6.5%-8% by weight of silicon, 0.2%-0.35% by weight of magnesium, 0.1%-0.16% by weight of titanium, 0.01%-0.03% by weight of strontium, 0.1%-0.2% by weight of zirconium, and 0.008%-0.03% by weight of manganese; the remainder is aluminum, the weight percentage of impurity iron is no more than 0.2%, the weight percentage of copper is no more than 0.05%, and the weight percentage of zinc is no more than 0.05%.
[0008] A method for manufacturing a heat-treatment-free aluminum alloy for low-pressure casting,
[0009] S1: melting in a tilting crucible furnace, first adding aluminum ingots into the crucible furnace for melting;
[0010] S2: After the aluminum ingot is melted, silicon is added, and the temperature is continued to rise. At the aluminum temperature of 700-720 degrees, slag is removed in the furnace and Mn and
[0011] Mg, then heated to 790 degrees for stirring to confirm the melting of silicon, and then carried out powder spraying and refining;
[0012] S3: putting the solution treated in step S2 into a solution transfer bag, adding aluminum titanium boron rods and aluminum zirconium alloy to the bottom of the solution transfer bag before draining water, degassing and slagging after draining water, adding Sr alloy rods after slagging and letting it stand for 20 minutes, and then taking samples for component testing to confirm whether it is qualified;
[0013] S4: pouring the solution processed in step S3 from the solution transfer bag into a mold for casting a test bar, and casting the test bar using the mold for casting the test bar;
[0014] S4: After 24 hours, the test bar is taken out of the test section test bar by a vertical sawing machine;
[0015] S5: X-ray the test bars to remove the test bars with internal defects;
[0016] S6: Perform a tensile test on the test bar using a yield strength testing machine and obtain the result;
[0017] The yield strength testing machine in step S6 includes a workbench, a working cavity is arranged in the workbench, a working port connected to the working cavity is arranged on the top surface of the workbench, a placing device for placing a test rod, a detection device for detecting the yield strength of the test rod, and a straightening device for straightening the test rod that falls on the detection device are arranged in the working cavity.
[0018] The placing device includes a mounting groove arranged in the workbench, the top wall and the bottom wall of the mounting groove are both arranged as inclined surfaces, and the top wall and the bottom wall remain parallel, the mounting groove is connected to the working chamber, a reciprocating placing plate is arranged in the mounting groove, an electromagnet is fixedly arranged on the inner wall of the mounting groove, a magnet is fixedly arranged on the side surface of the placing plate facing the electromagnet, and a connecting spring is fixedly arranged between the electromagnet and the magnet.
[0019] The alignment device includes a through groove arranged at the bottom of the working chamber, and a rotating shaft is rotatably arranged on the side walls of the through groove along the length direction, and an alignment rod is fixedly arranged on the rotating shaft. A torsion spring is sleeved on each rotating shaft, one end of the torsion spring is fixedly connected to the rotating shaft, and the other end of the torsion spring is fixedly connected to the side wall of the through groove, and the bottom surface of the placement plate is provided with a first groove and a second groove.
[0020] The detection device includes two detection components arranged on both sides of the working chamber; the detection component includes a support plate fixedly arranged on the inner wall of the working chamber, a first hydraulic cylinder is fixedly arranged on the support plate, a long plate is fixedly arranged on the piston rod of the first hydraulic cylinder, a first vertical plate is fixedly arranged at one end of the long plate, a second vertical plate is fixedly arranged at the other end of the long plate, a bearing plate is fixedly arranged on the bottom surface of the first vertical plate and the long plate, a second hydraulic cylinder is fixedly arranged on the second vertical plate, and a pressure plate is fixedly arranged on the piston rod of the second hydraulic cylinder.
[0021] A first blocking plate is fixedly disposed on the bottom surface of the placement plate, and a second blocking plate is fixedly disposed on the top surface of the pressing plate.
[0022] Two long strip marks are arranged on the top surface of the placement plate.
[0023] The working port is rotatably provided with a rotating shaft, and a transparent plastic plate is fixedly provided on the rotating shaft.
[0024] (3) Beneficial effects:
[0025] A. By setting up the placement device and the detection device, the test rod can be taken out and put in without the operator touching the fixture, so that the yield strength test can be carried out more safely.
[0026] B. By setting up the alignment device, the length direction of the test rod can be kept parallel to the length direction of the first hydraulic cylinder, so that the force direction during the test can be parallel to the length direction of the test rod, making the test result more accurate.
[0027] C. By setting the first blocking plate and the second blocking plate, when the straightening device fails and the side wall of the first groove cannot push the straightening rod to flip and push the two ends of the test rod flat, the placement plate will be unable to move further because the side wall of the first groove and the straightening rod are stuck near the end of the through groove. At this time, the first blocking plate cannot move upward along with the oblique upward movement of the placement plate. At this time, when the second hydraulic cylinder pushes the pressure plate to move, the second blocking plate above the pressure plate will be against the first blocking plate, and the pressure plate cannot continue to move to clamp the test rod (when the straightening device is not faulty, when the placement plate moves to the oblique upward limit position , the bottom surface of the first obstruction plate is located above the top surface of the second obstruction plate, so the first obstruction plate will not offset the second obstruction plate), so that when the straightening device fails, the test rod cannot be clamped, and the first hydraulic cylinder cannot break the test rod when it is started. When the operator sees that a complete test rod falls from the load-bearing plate when the first hydraulic cylinder is started to pull the load-bearing plate to move, it can be determined in time that the straightening device has failed, so that timely maintenance can be carried out before measurement, thereby avoiding the waste of labor costs caused by continuing to measure the yield strength when the straightening device fails, and the inability to distinguish defective products based on the measured data. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 It is a schematic diagram of the three-dimensional structure of the heat-treatment-free aluminum alloy for low-pressure casting of the present invention;
[0029] Figure 2 It is a front view of the present invention;
[0030] Figure 3 for Figure 2 Schematic diagram of the cross-sectional structure at AA in FIG.
[0031] Figure 4 for Figure 2 Schematic diagram of the cross-sectional structure at BB in FIG.
[0032] Figure 5 It is a structural schematic diagram of the straightening device;
[0033] Figure 6 is a schematic diagram of the three-dimensional structure of the placement plate;
[0034] Figure 7 This is a schematic diagram of the position of the placement plate after it moves when the electromagnet is activated;
[0035] Figure 8 It is a schematic diagram of the position of the long strip mark 500;
[0036] Fig. 9 It is the finished mold product after casting in step S4 (the dashed box in the figure shows the test bar for subsequent yield strength test after cutting). DETAILED DESCRIPTION
[0037] The following is combined with Figure 1-9 The present invention is further described with examples:
[0038] In this embodiment, a heat-free aluminum alloy for low-pressure casting includes 6.5%-8% silicon by weight, 0.2%-0.35% magnesium by weight, 0.1%-0.16% titanium by weight, 0.01%-0.03% strontium by weight, 0.1%-0.2% zirconium by weight, and 0.008%-0.03% manganese by weight; the balance is aluminum, and the weight percentage of impurity iron is not more than 0.2%, the weight percentage of copper is not more than 0.05%, and the weight percentage of zinc is not more than 0.05%. (Impurity iron, copper, and zinc are all impurities contained in the raw materials used in the preparation of aluminum alloys).
[0039]
[0040] After conducting experiments on multiple samples, it can be seen that the samples with the components of each material within the range included in the aluminum alloy of this embodiment have higher tensile strength than the samples not within the range when the tensile strength is tested. The tensile strength can reach more than 190Mpa, and the elongation is more than 10%. Therefore, the tensile strength and elongation of the heat-free aluminum alloy for low-pressure casting in this embodiment are better.
[0041] A method for manufacturing a heat-treatment-free aluminum alloy for low-pressure casting,
[0042] S1: melting in a tilting crucible furnace, first adding aluminum ingots into the crucible furnace for melting;
[0043] S2: After the aluminum ingot is melted, silicon is added and the temperature is continued to rise. At an aluminum temperature of 700-720 degrees, slag is removed in the furnace and Mn and Mg are added. Then the temperature is raised to 790 degrees for stirring to confirm the melting of silicon, and powder spraying and refining are performed.
[0044] S3: putting the solution treated in step S2 into a solution transfer bag, adding aluminum titanium boron rods and aluminum zirconium alloy to the bottom of the solution transfer bag before draining water, degassing and slagging after draining water, adding Sr alloy rods after slagging and letting it stand for 20 minutes, and then taking samples for component testing to confirm whether it is qualified;
[0045] S4: pouring the solution processed in step S3 from the solution transfer bag into a mold for casting a test bar, and casting the test bar using the mold for casting the test bar;
[0046] S4: After 24 hours, the test bar is taken out of the test section test bar by a vertical sawing machine;
[0047] S5: X-ray the test bars to remove the test bars with internal defects;
[0048] S6: Perform a tensile test on the test bar using a yield strength testing machine and obtain the result;
[0049] The yield strength testing machine in step S6 includes a workbench 1, a work chamber 2 is provided in the workbench 1, a work port 3 connected to the work chamber 2 is provided on the top surface of the workbench 1, a placement device 4 for placing a test bar and a detection device 5 for detecting the yield strength of the test bar are provided in the work chamber 2.
[0050] And a straightening device 6 for straightening the test rod that falls on the detection device.
[0051] The placing device 4 includes a mounting groove 40 arranged in the workbench 1, the top wall and the bottom wall of the mounting groove 40 are both set as inclined surfaces, and the top wall and the bottom wall are kept parallel, the mounting groove 40 is communicated with the working chamber 2, a reciprocating placing plate 41 is arranged in the mounting groove 40, an electromagnet 42 is fixedly arranged on the inner wall of the mounting groove 40, a magnet 43 is fixedly arranged on the side of the placing plate 41 facing the electromagnet 42, and a connecting spring 44 is fixedly arranged between the electromagnet 42 and the magnet 43 (the setting of the connecting spring 44 can slow down the moving speed of the magnet 43 and the second groove 65 when the magnet 43 is attracted by the electromagnet 42, so that there is enough time for the test rod to roll onto the supporting plate 354 before the straightening device starts working).
[0052] The alignment device 6 includes a through slot 60 arranged at the bottom of the working chamber 2, and a rotating shaft 61 is rotatably arranged on the side walls of the through slot 60 along the length direction. A straightening rod 62 is fixedly arranged on the rotating shaft 61, and a torsion spring is sleeved on each rotating shaft 61. One end of the torsion spring is fixedly connected to the rotating shaft 61, and the other end of the torsion spring is fixedly connected to the side wall of the through slot 60. The bottom surface of the placement plate 41 is provided with a first groove 64 and a second groove 65.
[0053] The detection device 5 includes two detection components arranged on both sides of the working chamber 2; the detection component includes a support plate 50 fixedly arranged on the inner wall of the working chamber 2, a first hydraulic cylinder 51 is fixedly arranged on the support plate 50, a long plate 52 is fixedly arranged on the piston rod of the first hydraulic cylinder 51, a first vertical plate 53 is fixedly arranged at one end of the long plate 52, a second vertical plate 54 is fixedly arranged at the other end of the long plate 52, a bearing plate 354 is fixedly arranged on the bottom surface of the first vertical plate 53 and the long plate 52, a second hydraulic cylinder 55 is fixedly arranged on the second vertical plate 54, a pressure plate 56 is fixedly arranged on the piston rod of the second hydraulic cylinder 55, a through hole 57 is arranged on the long plate 52, and a push rod 58 that can move back and forth in the through hole 57 is fixedly arranged on the support plate 50.
[0054] A first blocking plate 80 is fixedly disposed on the bottom surface of the placement plate 41 , and a second blocking plate 81 is fixedly disposed on the top surface of the pressing plate 56 .
[0055] Two long strip marks 500 are arranged on the top surface of the placement plate 41. The arrangement of the marks 500 makes it easy for people to identify the placement position of the test rod. The long strip marks can be drawn by a spray gun.
[0056] The working port 3 is rotatably provided with a rotating shaft 90, and a transparent plastic plate 91 is fixedly provided on the rotating shaft 90. The transparent plastic plate can be closed when testing the yield strength to prevent the debris from splashing out when the test rod breaks and causing injuries to the operator next to the equipment; the transparent setting makes it easier for the operator to observe the situation inside the equipment.
[0057] The workbench 1 is provided with a communication port communicating with the working chamber 2, and an electric control door 777 is fixedly provided in the communication port. By opening the electric control door 777, the test rod falling on the bottom of the working chamber 2 can be taken out.
[0058] The working principle of the present invention includes the following process:
[0059] The test rod is placed between the two long strip marks 500, and then the transparent plastic plate 91 is turned down 90 degrees, the working port 3 is closed, and the electromagnet 42 is started. Since the relative polarities between the electromagnet 42 and the magnet 43 are opposite, the magnet 43 will move toward the direction of the electromagnet 42 according to the attraction of opposite poles, and the magnet 43 will move with the placement plate 41. Since the placement plate 41 is located in the installation groove 40, the top wall and the bottom wall of the installation groove 40 are inclined, so the top surface of the placement plate 41 is also inclined. Therefore, when the placement plate 41 is moved away from the top of the carrier plate 354, the placement plate 41 is located at the placement plate 41. The test tube on the top surface of the plate 41 will roll down onto the left and right supporting plates 354 along the inclined surface (at this time, the two supporting plates 354 are located directly below the two long strip marks 500). As the placement plate 41 continues to move toward the electromagnet 42, the side wall of the second groove 65 will abut against the alignment rod 62, and then the alignment rod 62 will flip. The flipping of the two alignment rods 62 will make the end away from the rotating shaft 61 abut against the two ends of the test tube, so that the test tube can be pushed and aligned (that is, the length direction of the test rod is kept parallel to the length direction of the first hydraulic cylinder 51, so that the force direction during detection can be consistent with the length of the test rod). The length direction is parallel to make the test result more accurate), and then as the placement plate 41 continues to move, the end of the straightening rod 62 close to the rotating shaft 61 is located in the second groove 65, so that after losing the resistance, the straightening rod 62 will return to its original state under the action of the torsion spring and no longer abut against the test rod, thereby avoiding affecting the test result due to the abutment between the straightening rod 62 and the test rod during the test, and then after a preset time of 5S (that is, the placement plate 41 has moved to the limit position and no longer moves), the second hydraulic cylinder 55 is started to clamp the test rod. After clamping, the first hydraulic cylinder 51 is started to clamp the test rod. Pull the long plate 52 to both sides to test the yield strength (during the yield strength test, the long plate 52 will not move to a position where the push rod can enter the perforation when moving in the direction close to the support plate 50). After the test is completed, the second hydraulic cylinder 55 is started to move the pressure plate 56 away from the test rod and release the test rod. Then the first hydraulic cylinder 51 continues to drive the long plate 52 to move in the direction close to the support plate 50. Only then will the push rod pass through the perforation and push down the broken test rod that has not fallen off the load-bearing plate 354. Therefore, there is no need to manually remove the broken test rod that has not fallen off the load-bearing plate 354 from the fixture, thereby making the detection process safer.
[0060] By setting the first blocking plate and the second blocking plate, when the straightening device fails and the side wall of the first groove cannot push the straightening rod to flip and push the two ends of the test rod flat, the placement plate 41 will be unable to move further because the side wall of the first groove and the straightening rod are stuck at one end of the through groove 60. At this time, the first blocking plate 80 cannot move obliquely upward with the oblique upward movement of the placement plate 41. At this time, when the second hydraulic cylinder 55 pushes the pressing plate 56 to move, the second blocking plate 81 above the pressing plate 56 abuts against the first blocking plate 80, and the pressing plate 56 cannot continue to move to clamp the test rod (when the straightening device has no failure, when the placement plate 41 moves to the oblique upward limit When the straightening device is in the right position, the bottom surface of the first obstruction plate 80 is located above the top surface of the second obstruction plate 81, so the first obstruction plate 80 will not offset the second obstruction plate 81), so that when the straightening device fails, the test rod cannot be clamped, and the test rod cannot be broken when the first hydraulic cylinder is started. When the operator sees that a complete test rod falls from the load-bearing plate 354 when the first hydraulic cylinder is started to pull the load-bearing plate 354 to move, it can be determined in time that the straightening device has failed, so that timely maintenance can be carried out before measurement, thereby avoiding the waste of labor costs caused by continuing to measure the yield strength when the straightening device fails, and the inability to distinguish defective products based on the measured data.
[0061] The embodiments of the present invention disclose preferred embodiments, but are not limited thereto. A person skilled in the art can easily understand the spirit of the present invention based on the above embodiments and make different extensions and changes. However, as long as they do not deviate from the spirit of the present invention, they are all within the protection scope of the present invention.
Claims
1. A yield strength testing machine for low-pressure casting aluminum alloy without heat treatment, characterized in that: The invention comprises a workbench (1), wherein a working chamber (2) is arranged in the workbench (1), a working port (3) connected to the working chamber (2) is arranged on the top surface of the workbench (1), and a placing device (4) for placing a test bar, a detection device (5) for detecting the yield strength of the test bar, and a straightening device (6) for straightening the test bar that falls on the detection device are arranged in the working chamber (2); the placing device (4) comprises a mounting groove (40) arranged in the workbench (1), and the mounting groove ( The top wall and bottom wall of the mounting groove (40) are both arranged as inclined surfaces, and the top wall and the bottom wall remain parallel, the mounting groove (40) is connected to the working chamber (2), a reciprocating placement plate (41) is arranged in the mounting groove (40), an electromagnet (42) is fixedly arranged on the inner wall of the mounting groove (40), a magnet (43) is fixedly arranged on the side surface of the placement plate (41) facing the electromagnet (42), and a connecting spring (44) is fixedly arranged between the electromagnet (42) and the magnet (43).
2. A yield strength testing machine for low pressure casting aluminum alloy without heat treatment as claimed in claim 1, characterized in that: The alignment device (6) comprises a through slot (60) arranged at the bottom of the working chamber (2); a rotating shaft (61) is rotatably arranged on the side walls of both sides of the through slot (60) along the length direction; a aligning rod (62) is fixedly arranged on the rotating shaft (61); a torsion spring is sleeved on each rotating shaft (61); one end of the torsion spring is fixedly connected to the rotating shaft (61); the other end of the torsion spring is fixedly connected to the side wall of the through slot (60); and a first groove (64) and a second groove (65) are arranged on the bottom surface of the placement plate (41).
3. A yield strength testing machine for low pressure casting aluminum alloy without heat treatment as claimed in claim 2, characterized in that: The detection device (5) comprises two detection components arranged on both sides of the working chamber (2); the detection component comprises a support plate (50) fixedly arranged on the inner wall of the working chamber (2), a first hydraulic cylinder (51) fixedly arranged on the support plate (50), a long plate (52) fixedly arranged on the piston rod of the first hydraulic cylinder (51), a first vertical plate (53) fixedly arranged on one end of the long plate (52), a second vertical plate (54) fixedly arranged on the other end of the long plate (52), a bearing plate (354) fixedly arranged on the bottom surface of the first vertical plate (53) and the long plate (52), a second hydraulic cylinder (55) fixedly arranged on the second vertical plate (54), and a pressure plate (56) fixedly arranged on the piston rod of the second hydraulic cylinder (55).
4. A yield strength testing machine for aluminum alloys without heat treatment for low pressure casting as claimed in claim 3, characterized in that: A first blocking plate (80) is fixedly disposed on the bottom surface of the placement plate (41), and a second blocking plate (81) is fixedly disposed on the top surface of the pressing plate (56).
5. The yield strength testing machine for aluminum alloy without heat treatment for low pressure casting according to claim 3, characterized in that: Two long strip marks (500) are arranged on the top surface of the placement plate (41).
6. A yield strength testing machine for aluminum alloys without heat treatment for low pressure casting as claimed in claim 2, characterized in that: The working port (3) is rotatably provided with a rotating shaft (90), and a transparent plastic plate (91) is fixedly provided on the rotating shaft (90).