Fiber optic sensor combination, strain discrimination, and concrete structure deformation inversion method
By combining fiber optic sensors with overall bonding and point fixing, and using a crack response strain differentiation formula, the problem of deformation monitoring and data analysis of large hydraulic concrete structures was solved, realizing quantitative monitoring and stress form analysis of hydraulic concrete structures.
Patent Information
- Application Number
- CN202410188668.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-20
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2044-02-20
AI Technical Summary
Existing technologies are insufficient for quantitative monitoring and data analysis of deformation in large hydraulic concrete structures. They cannot optimize the arrangement of fiber optic sensors for specific deformation characteristics of the structure, cannot distinguish between fiber optic signals of cracks and strain in hydraulic concrete structures, and cannot analyze the stress patterns of hydraulic concrete structures.
A combination of fiber optic sensors, employing both integral bonding and point fixing, and incorporating formulas to differentiate crack response strain from concrete strain, is used to achieve deformation monitoring and data analysis of hydraulic concrete structures through fiber optic strain field analysis and inversion.
It enables quantitative monitoring and data analysis of large-scale hydraulic concrete structures, optimizes the arrangement of fiber optic sensors, distinguishes between crack and strain fiber optic signals, and performs stress mode analysis of hydraulic concrete structures.
Smart Images

Figure CN118031835B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of optical fiber signal processing technology, and more specifically, relates to an optical fiber sensor combination, strain differentiation, and concrete structure deformation inversion method. Background Technology
[0002] Inverting structural strain fields using fiber optic core strain has become a current research hotspot. Some scholars have conducted extensive research on structural deformation using fiber optic strain data, finding that strain field reconstruction methods based on fiber optic strain sensing technology can obtain strain and internal stress information of the monitored object, offering comprehensive, intuitive, and intelligent features, and are widely used in several key fields such as aerospace and medicine. However, shape reconstruction methods are not widely used in concrete engineering.
[0003] However, the above studies still have some shortcomings: First, during service, hydraulic concrete structures may experience both concrete strain and crack propagation simultaneously, and existing studies do not consider the impact of cracks on the deformation inversion results when performing structural deformation inversion; second, the accuracy of the structural deformation inversion methods proposed in existing studies is affected by calculation errors, and the more iterations are performed in the shape deformation inversion process, the greater the impact of iteration errors on the deformation inversion results; finally, most existing structural deformation inversion techniques are used in linear engineering such as pipelines, and the materials monitored are mostly homogeneous materials such as steel and plastics, so the existing studies have limited guiding role in the strain field monitoring of hydraulic concrete structures.
[0004] Some existing patents monitor the deformation of the substrate structure through a dense arrangement of optical fibers. However, the number of dense optical fiber sensors used is insufficient for monitoring the deformation of large hydraulic concrete structures. A representative example is CN104257363B, which only uses 1*6 FBG measuring points and cannot be called "dense," but rather "concentrated." Some patents simply set more fiber optic grating measuring points on a single optical fiber, which cannot actually represent a surface with a line. Therefore, most of them are pasted on the surface of the reinforcing steel, limiting their ability to monitor critical structural defects (cracks). For example, CN113026829B uses a single-strand armored fiber. Some patents employ dense fiber grating strings, which are then attached to the surface of reinforcing steel. Others utilize fiber optic sensing arrays, enabling regionalized structural strain monitoring through densely distributed fiber grating sensing points. However, these methods are ineffective for cracks that randomly appear on large hydraulic concrete structures, such as CN116164858A, which describes a multi-parameter detection system and method based on dense fiber gratings. This system uses a single fiber to simultaneously sense multiple parameters, including temperature, strain, and vibration, but does not cover cracks. Some patents, such as CN108548548B, only study the demodulation method of array-type dense fiber grating sensing arrays, without explaining the application of array technology, thus failing to confirm the practicality of the technology.
[0005] Therefore, it is evident that there is currently a lack of a deformation inversion method for hydraulic concrete structures based on densely arranged fiber optic networks. The shortcomings are as follows:
[0006] 1. Existing methods are insufficient for quantitative monitoring and data analysis of deformation in large hydraulic concrete structures.
[0007] 2. Existing methods are too wasteful and do not optimize the arrangement of fiber optic sensors for the specific deformation characteristics of the structure.
[0008] 3. Existing methods have difficulty distinguishing between fiber optic signals of cracks and strain in hydraulic concrete structures.
[0009] 4. Existing methods are insufficient for analyzing the stress patterns of hydraulic concrete structures. Summary of the Invention
[0010] This invention addresses the aforementioned problems in the prior art. Therefore, there is a need for a fiber optic sensor combination, strain differentiation, and concrete structure deformation inversion method.
[0011] According to a first aspect of the present invention, a method for combining fiber optic sensors to monitor both matrix strain and cracks is provided, the method comprising:
[0012] Fiber optic cables are installed using a complete bonding process.
[0013] Fixed-point installation of optical fiber;
[0014] A combined fiber optic sensor is formed by combining optical fibers that are integrally bonded and installed and optical fibers that are fixed at points.
[0015] The integral adhesive mounting of the optical fiber includes: bonding the optical fiber along its entire length to the surface of the structure;
[0016] The point-fixed installation of the optical fiber includes fixing the optical fiber at spaced points.
[0017] Furthermore, the strain transmissivity (STR) of the fiber optic cable in integrally bonded installation... OB and average strain transmissibility ASTR OB As shown in equations (1) and (2):
[0018]
[0019]
[0020] Where, ε m (x) is the matrix strain, ε f (x) is the fiber core strain, L is the fiber bonding length, λ is the shear hysteresis coefficient, and G... a It is the shear modulus of epoxy resin, G p It is the shear modulus of the sheath, rf It is the radius of the fiber core, r p It's the thickness of the sheath, E f is the elastic modulus of the fiber core, and x is the fiber position. It is the strain distribution of the fiber core.
[0021] Furthermore, the strain transmissivity STR of point-fixed fiber optic cables PF and average strain transmissibility ASTR PF As shown in equations (3) and (4).
[0022]
[0023]
[0024] Where w is the crack width.
[0025] According to a second aspect of the present invention, a method for distinguishing between crack response strain and concrete strain is provided, characterized in that it is based on a combined fiber optic sensor constructed using the method described above, the method comprising:
[0026] The signals of concrete cracks and concrete strain are extracted using a formula that distinguishes between crack response strain and concrete strain.
[0027] The formula for distinguishing between crack response strain and concrete strain is as follows:
[0028]
[0029] Where ε0(x) is the strain level of the concrete matrix, c1 and c2 are coefficients to be determined, λ1 is the shear hysteresis coefficient of the optical fiber, a is the crack coefficient, usually 10, C is the location of the crack strain peak, and COD is the crack width.
[0030] According to a third aspect of the present invention, a deformation inversion method for hydraulic concrete structures is provided. Based on the method described above, strain field analysis and inversion are performed on cracked hydraulic structures under different structural stress states to determine the fiber optic strain caused by the cracked hydraulic structures.
[0031] Furthermore, when the strain of the concrete matrix is a bilinear strain field, the strain of the concrete matrix is expressed as:
[0032]
[0033] Where A is the starting point of the strain field, B is the ending point of the strain field, C is the ending point of the strain field, and ε0 is the peak value of the strain field.
[0034] The expressions for fiber core strain are:
[0035]
[0036]
[0037] Among them, c 11 c 12 c 21 c 22 It is a constant term;
[0038] The boundary conditions are expressed as follows:
[0039]
[0040] Where, ε f (C - ) and ε f (C + () is the derivative to the left and right of point C;
[0041] The coefficients are obtained from the fiber strain field and the boundary conditions according to formula (6.2):
[0042]
[0043]
[0044]
[0045]
[0046] By shifting the coordinate axes so that C = 0, the coefficients are obtained as follows:
[0047]
[0048]
[0049]
[0050]
[0051] Based on the crack response strain, the fiber core strain caused by the hydraulic concrete structure is:
[0052]
[0053] Where 'a' is the crack coefficient.
[0054] Furthermore, when the strain in the concrete matrix is a linear strain field with compressive strain, the strain in the concrete matrix is expressed as:
[0055]
[0056] Where A is the starting point of the strain field, B is the ending point of the strain field, and C is the ending point of the strain field. and These are the two peak values at both ends of the strain field;
[0057] The expression for fiber core strain is:
[0058]
[0059]
[0060] Among them, c 11 c 12 c 21 c 22 It is a constant term;
[0061] The boundary conditions are expressed as follows:
[0062]
[0063] The coefficients are obtained from the fiber strain field and the boundary conditions according to formula (7.2):
[0064]
[0065]
[0066]
[0067]
[0068] By shifting the coordinate axes so that C = 0, the coefficients are obtained as follows:
[0069]
[0070]
[0071]
[0072]
[0073] The fiber core strain caused by the crack response strain is expressed as:
[0074]
[0075] Where 'a' is the crack coefficient.
[0076] Furthermore, in the case where the concrete matrix strain is a complex linear strain field composed of multiple linear strain segments, the concrete matrix strain is expressed as:
[0077]
[0078] The expression for fiber core strain is:
[0079]
[0080] Among them, c 11 c 12 c 21 c 22 c 31 c 32 c 41 c 42 It is a constant term;
[0081] The fiber core strain caused by the combination of crack response strain is shown below:
[0082]
[0083] Where 'a' is the crack coefficient.
[0084] Furthermore, when the strain in the concrete matrix is a nonlinear strain field under a uniformly distributed load, the strain in the concrete matrix is expressed as:
[0085]
[0086] The expression for fiber core strain is:
[0087]
[0088]
[0089] Among them, c 11 c 12 It is a constant term;
[0090] The boundary conditions are:
[0091]
[0092] The fiber core strain caused by the crack response strain is shown below:
[0093]
[0094] Where 'a' is the crack coefficient.
[0095] Furthermore, when the strain in the concrete matrix is a periodic nonlinear strain field under a uniformly distributed load, the strain in the concrete matrix is expressed as:
[0096]
[0097] The expression for fiber core strain is:
[0098]
[0099]
[0100] Among them, c 11 c 12 It is a constant term;
[0101] The boundary conditions are:
[0102] ε f (A)=ε f (B)=ε f (C)=0 (10.4)
[0103] The fiber core strain caused by the crack response strain is shown below:
[0104]
[0105] Where 'a' is the crack coefficient.
[0106] The present invention has at least the following beneficial effects:
[0107] 1. It can realize quantitative monitoring and data analysis of deformation of large hydraulic concrete structures.
[0108] 2. Optimize the arrangement of fiber optic sensors based on the specific deformation characteristics of the structure.
[0109] 3. It can distinguish between cracks and strain in hydraulic concrete structures using fiber optic signals.
[0110] 4. It can analyze the stress patterns of hydraulic concrete structures. Attached Figure Description
[0111] Figure 1 A schematic diagram of the integral bonding method according to an embodiment of the present invention is shown;
[0112] Figure 2 A schematic diagram of the point fixing method according to an embodiment of the present invention is shown;
[0113] Figure 3 A schematic diagram of the minimum fiber optic sensing unit according to an embodiment of the present invention is shown;
[0114] Figure 4 A schematic diagram of a method for distinguishing between strain in a concrete matrix and crack response according to an embodiment of the present invention is shown.
[0115] Figure 5 A schematic diagram of an optical fiber mesh type according to an embodiment of the present invention is shown;
[0116] Figure 6A schematic diagram of the bilinear strain field of cracked concrete according to an embodiment of the present invention is shown;
[0117] Figure 7 A schematic diagram of the linear strain field of cracked concrete according to an embodiment of the present invention is shown;
[0118] Figure 8 A schematic diagram of a complex linear strain field in cracked concrete according to an embodiment of the present invention is shown;
[0119] Figure 9 A schematic diagram of the nonlinear strain field of cracked concrete according to an embodiment of the present invention is shown;
[0120] Figure 10 A schematic diagram of the strain field of a cracked concrete pipe according to an embodiment of the present invention is shown;
[0121] Figure 11 A schematic diagram of the sensor arrangement on a concrete beam according to an embodiment of the present invention is shown;
[0122] Figure 12 A schematic diagram of the concrete beam loading process according to an embodiment of the present invention is shown;
[0123] Figure 13 A schematic diagram of the test results of the OB method according to an embodiment of the present invention is shown;
[0124] Figure 14 A schematic diagram of the test results of the PF method according to an embodiment of the present invention is shown;
[0125] Figure 15 A schematic diagram of the three-point bending beam test results according to an embodiment of the present invention is shown;
[0126] Figure 16 A schematic diagram showing the results of resolving the matrix strain and crack width according to an embodiment of the present invention is provided.
[0127] Figure 17 A schematic diagram of the optical fiber network on the front surface of the first board according to an embodiment of the present invention is shown;
[0128] Figure 18 A schematic diagram of the optical fiber network on the bottom surface of the first board according to an embodiment of the present invention is shown;
[0129] Figure 19 A schematic diagram of an optical fiber network on the surface of a second plate according to an embodiment of the present invention is shown;
[0130] Figure 20 A diagram illustrating the location and trajectory of a crack according to an embodiment of the present invention is shown. Detailed Implementation
[0131] To enable those skilled in the art to better understand the technical solutions of the present invention, the present invention will be described in detail below with reference to the accompanying drawings and specific embodiments. The embodiments of the present invention will be further described in detail below with reference to the accompanying drawings and specific examples, but this is not intended to limit the present invention. If there is no necessary sequential relationship between the various steps described herein, the order in which they are described as examples should not be considered a limitation. Those skilled in the art should understand that the order can be adjusted, as long as it does not disrupt the logical consistency between them and render the entire process impossible.
[0132] This invention provides a method for combining fiber optic sensors that takes into account both matrix strain and crack monitoring, including a method for designing the minimum fiber optic sensing unit.
[0133] The minimum fiber optic sensing unit (LPP) includes: integral bonding (OB) mounting method, point fixing (PF) mounting method, and combination method.
[0134] The minimum fiber optic sensing unit (LPP) includes: integral bonding (OB) mounting method, point fixing (PF) mounting method, and combination method.
[0135] The integral bonding (OB) mounting method is a method of bonding the optical fiber along its entire length to the surface of the structure, such as... Figure 1 As shown.
[0136] The adhesive used in the integral bonding (OB) installation method is typically an adhesive or glue such as epoxy resin.
[0137] The strain transfer rate STR and average strain transfer rate ASTR of the integral bond (OB) mounting method are shown in Equations (1) and (2).
[0138]
[0139]
[0140] Where, ε m (x) is the matrix strain, ε f (x) is the fiber core strain, L is the fiber bonding length, λ is the shear hysteresis coefficient, and G... a It is the shear modulus of epoxy resin, G p It is the shear modulus of the sheath, r f It is the radius of the fiber core, r p It's the thickness of the sheath, E f It is the elastic modulus of the fiber core.
[0141] The point-fixed (PF) installation method is as follows: the optical fiber is fixed at spaced points, such as... Figure 2 As shown.
[0142] The point-fixed (PF) installation method is as follows: the fiber at the endpoint is fixed using a clamping fixture, clamping clip or other fixing device.
[0143] The strain transfer rate STR and average strain transfer rate ASTR of the point-fixed (PF) installation method are shown in equations (3) and (4).
[0144]
[0145]
[0146] The method for combining the minimum fiber optic sensing unit (LPP) is as follows: Figure 3 As shown.
[0147] like Figure 4 As shown, this embodiment of the invention provides a method for distinguishing between crack response strain and concrete strain, including extracting the signals of concrete cracks and concrete strain using a formula for distinguishing between crack response strain and concrete strain.
[0148] The formula for distinguishing between crack response strain and concrete strain is as follows:
[0149]
[0150] Where ε0(x) is the strain level of the concrete matrix, c1 and c2 are coefficients to be determined, which are related to the structural characteristics and will be introduced according to the specific structural form in the embodiments, λ is the shear hysteresis coefficient of the optical fiber, a is the crack coefficient, which is usually 10, and C is the location of the crack strain peak.
[0151] The embodiments of the present invention provide a method for strain field analysis and inversion of cracked hydraulic structures under different structural stress states, including specific embodiments 2 to 6.
[0152] Example 1: Implementation methods of fiber optic sensor networks with different structures and variations
[0153] Based on the minimum fiber optic sensing unit proposed above, fiber optic mesh layout schemes are designed for concrete structures with different structural forms, working conditions, failure modes, and monitoring requirements. Among them, Figure 5 In the middle (a), (d), and (e), there are orthogonal grids, which are general solutions suitable for situations where the crack orientation and crack density cannot be determined. Figure 5 In the middle (b), (f), and (g), there are oblique meshes, which are suitable for a single-direction densification scheme when the general direction of the crack can be determined, thereby increasing the number of points where the optical fiber intersects with the crack; Figure 5 (c) represents the scheme where the optical fiber is orthogonal to the crack when it can be determined that the crack is developing in a single direction; Figure 5(d) and (f) are crack monitoring schemes for large-volume concrete structures. In this case, the crack spacing is large, the probability of two or more cracks appearing between two adjacent bonding points is small, and the crack width is usually large. Using this scheme can improve monitoring accuracy and reduce fiber optic loss rate. Figure 5 (e) and (g) are crack monitoring schemes for small-volume concrete structures. The cracks are relatively dense and the crack width is small, which can accurately determine the number and width of cracks. Figure 5 (a), (b), and (c) represent cases of relatively small-volume concrete structures with large crack widths, which are applicable to destructive testing of concrete structures.
[0154] Example 2: Inversion Analysis of Bilinear Strain Field in Cracked Concrete
[0155] like Figure 6 As shown. The strain in the concrete matrix is a bilinear strain field, which can be expressed as:
[0156]
[0157] Therefore, the expression for the fiber core strain is:
[0158]
[0159]
[0160] According to formula (6.2), the fiber strain field is as follows: Figure 6 As shown in (d), according to the boundary conditions, we have:
[0161]
[0162] The coefficients are obtained as follows:
[0163]
[0164]
[0165]
[0166]
[0167] To simplify the calculation, we can first shift the coordinate axes so that C = 0, and then obtain the coefficients as follows:
[0168]
[0169]
[0170]
[0171]
[0172] Combining crack response strain, such as Figure 6 As shown in (c), the resulting fiber core strain is:
[0173]
[0174] The fiber core strain caused by the crack response strain is as follows: Figure 6 As shown in (e).
[0175] Example 3: Linear strain field analysis of cracked concrete with compressive strain
[0176] When the strain in the concrete matrix is a linear strain field with compressive strain, the matrix strain can be expressed as:
[0177]
[0178] Therefore, the expression for the fiber core strain is:
[0179]
[0180]
[0181] According to formula (7.2), the fiber strain field is as follows: Figure 7 As shown in (d), according to the boundary conditions, we have:
[0182]
[0183] The coefficients are obtained as follows:
[0184]
[0185]
[0186]
[0187]
[0188] To simplify the calculation, we can first shift the coordinate axes so that C = 0, and then obtain the coefficients as follows:
[0189]
[0190]
[0191]
[0192]
[0193] The fiber core strain caused by the crack response strain is as follows: Figure 7As shown in (e).
[0194]
[0195] Example 4: Analysis of Complex Linear Strain Field in Cracked Concrete
[0196] When the strain of the concrete matrix is a complex linear strain field composed of multiple linear strain segments, the matrix strain is:
[0197]
[0198] Therefore, the expression for the fiber core strain is as follows: Figure 8 In (d), we have:
[0199]
[0200] The fiber core strain caused by the crack response strain is as follows: Figure 8 As shown in (e).
[0201]
[0202] Example 5: Parabolic Strain Field Analysis of Cracked Concrete
[0203] When the strain in the concrete matrix is a nonlinear strain field under a uniformly distributed load, the matrix strain can be expressed as:
[0204]
[0205] Therefore, the expression for the fiber core strain is:
[0206]
[0207]
[0208] According to equation (9.2), the fiber strain field is as follows: Figure 9 As shown in (d), according to the boundary conditions, we have:
[0209]
[0210] The fiber core strain caused by the crack response strain is as follows: Figure 9 As shown in (e).
[0211]
[0212] Example 6: Periodic Nonlinear Strain Field Analysis of Cracked Concrete
[0213] When the strain in the concrete matrix is a periodic nonlinear strain field under a uniformly distributed load, the matrix strain can be expressed as:
[0214]
[0215] Therefore, the expression for the fiber core strain is:
[0216]
[0217]
[0218] According to equation (10.2), the fiber strain field is as follows: Figure 10 As shown in (d), according to the boundary conditions, we have:
[0219] ε f (A)=ε f (B)=ε f (C)=0 (10.4)
[0220] The fiber core strain caused by the crack response strain is as follows: Figure 10 As shown in (e).
[0221]
[0222] Example 7: Strain Monitoring of Reinforced Concrete Beams Based on Minimum Sensing Units
[0223] like Figure 11 and Figure 12 As shown, the deformation of a concrete beam was monitored using fiber optic sensor networks with different spacings, and the results are as follows. Figure 13 and Figure 14 As shown.
[0224] Example 8: Strain Monitoring of Reinforced Concrete Beams Based on Fiber Optic Strain and Crack Resolution
[0225] like Figure 15 As shown, the bending deformation signal of the concrete beam was analyzed using a matrix strain and crack monitoring differentiation method. The strain and crack width of the concrete were successfully calculated, and the results are as follows. Figure 16 As shown.
[0226] Example 9: Deformation Monitoring of Hydropower Station Powerhouse Floor Based on Fiber Optic Sensor Network
[0227] like Figures 17-19 As shown, a fiber optic sensor network was used to analyze the deformation signal of the hydropower station powerhouse floor slab, and the width and direction of concrete cracks were successfully calculated. The results are as follows. Figure 20 As shown in Tables 1 to 3.
[0228] Table 1 Crack width data for the first plate (10 -2 mm)
[0229]
[0230] Table 2 Crack width data for the second plate (10 -2 mm)
[0231]
[0232] Table 3 Crack width data for the second plate (10 -2 mm)
[0233]
[0234] The above description is intended to be illustrative and not restrictive. For example, the above examples (or one or more of them) can be used in combination with each other. Other embodiments can be used by those skilled in the art when reading the above description. Furthermore, in the above detailed description, various features may be grouped together to simplify the invention. This should not be construed as an intention that a feature of an unclaimed invention is necessary for any claim. Rather, the subject matter of the invention may be less than all the features of a particular embodiment of the invention. Thus, the following claims are incorporated herein by reference as examples or embodiments, wherein each claim is an independent, separate embodiment, and these embodiments are contemplated to be combined with each other in various combinations or arrangements. The scope of the invention should be determined by reference to the appended claims and the full scope of their equivalents.
Claims
1. A method for distinguishing between crack response strain and concrete strain, characterized in that, Based on a combined optical fiber sensor, the method of combining the combined optical fiber sensor includes: integrally bonding and installing optical fibers; point fixing and installing optical fibers; combining the integrally bonded and installed optical fibers and the point fixing and installed optical fibers to form a combined optical fiber sensor; the integrally bonded and installed optical fibers include: bonding the optical fibers along their entire length to the surface of the structure; the point fixing and installed optical fibers include: fixing the optical fibers at spaced points. The method for distinguishing between crack response strain and concrete strain includes: The signals of concrete cracks and concrete strain are extracted using a formula that distinguishes between crack response strain and concrete strain. The formula for distinguishing between crack response strain and concrete strain is as follows: (5) in, ε f ( x ) is the fiber core strain, ε 0( x () represents the strain level of the concrete matrix. c 1 and c 2 is the coefficient to be determined. λ 1 is the shear hysteresis coefficient of the optical fiber. a It is the crack coefficient. C It indicates the location of the peak crack strain, and COD is the crack width. x It refers to the location of the optical fiber; Based on the strain level of the concrete matrix and the coefficients to be determined, determine the fiber core strain caused by the strain of the concrete matrix: ; The fiber core strain caused by the strain of the concrete matrix is derived from the fiber core strain. Subtracting from the middle, we obtain the core strain caused by the crack response strain: ; This allows for the differentiation between signals from concrete cracks and signals from concrete strain.
2. The method according to claim 1, characterized in that, STR of fiber strain transmissivity in integrally bonded installation OB and average strain transmissibility ASTR OB As shown in equations (1) and (2): (1) (2) in, ε m ( x ) is matrix strain, L It refers to the fiber optic cable bonding length. λ It is the shear hysteresis coefficient. G a It is the shear modulus of epoxy resin. G p It is the shear modulus of the sheath. r f It is the radius of the fiber core. r p It's the thickness of the sheath. E f It is the elastic modulus of the fiber core. It is the strain distribution of the fiber core.
3. A method for deformation inversion of hydraulic concrete structures, characterized in that, Based on the method described in claim 1, strain field analysis and inversion are performed on cracked hydraulic structures under different structural stress states to determine the fiber optic strain caused by the cracked hydraulic structures.
4. The method according to claim 3, characterized in that, When the strain of the concrete matrix is a bilinear strain field, the strain of the concrete matrix is expressed as: (6.1) Where A is the starting point of the strain field and B is the ending point of the strain field. It is the peak value of the strain field; The expressions for fiber core strain are: (6.2) (6.3) in, c 11 , c 12 , c 21 , c 22 It is a constant term; The boundary conditions are expressed as follows: (6.4) in, (C - )and (C + () is the derivative to the left and right of point C; The coefficients are obtained from the fiber strain field and the boundary conditions according to formula (6.2): (6.5) (6.6) (6.7) (6.8) By shifting the coordinate axes so that C=0, the coefficients are obtained as follows: (6.8-1) (6.8-2) (6.8-3) (6.8-4) Based on the crack response strain, the fiber core strain caused by the hydraulic concrete structure is: (6.9) in, a It is the crack coefficient.
5. The method according to claim 3, characterized in that, When the strain in the concrete matrix is a linear strain field with compressive strain, the strain in the concrete matrix is expressed as: (7.1) Where A is the starting point of the strain field and B is the ending point of the strain field. and These are the two peak values at both ends of the strain field; The expression for fiber core strain is: (7.2) (7.3) in, c 11 , c 12 , c 21 , c 22 It is a constant term; The boundary conditions are expressed as follows: (7.4) The coefficients are obtained from the fiber strain field and the boundary conditions according to formula (7.2): (7.5) (7.6) (7.7) (7.8) By shifting the coordinate axes so that C=0, the coefficients are obtained as follows: (7.9-1) (7.9-2) (7.9-3) (7.9-4) The fiber core strain caused by the crack response strain is expressed as: (7.10) in, a It is the crack coefficient.
6. The method according to claim 3, characterized in that, In the case where the strain of the concrete matrix is a complex linear strain field composed of multiple linear strain segments, the strain of the concrete matrix is expressed as: (8.1) The expression for fiber core strain is: (8.2) in, c 11 , c 12 , c 21 , c 22 , c 31 , c 32 , c 41 , c 42 It is a constant term; The fiber core strain caused by the combination of crack response strain is shown below: (8.3) in, a It is the crack coefficient.
7. The method according to claim 3, characterized in that, When the strain in the concrete matrix is a nonlinear strain field under a uniformly distributed load, the strain in the concrete matrix is expressed as: (9.1) The expression for fiber core strain is: (9.2) (9.3) in, c 11 , c 12 It is a constant term; The boundary conditions are: (9.4) The fiber core strain caused by the crack response strain is shown below: (9.5) in, a It is the crack coefficient.
8. The method according to claim 3, characterized in that, When the strain in the concrete matrix is a periodic nonlinear strain field under a uniformly distributed load, the strain in the concrete matrix is expressed as: (10.1) The expression for fiber core strain is: (10.2) (10.3) in, c 11 , c 12 It is a constant term; The boundary conditions are: (10.4) The fiber core strain caused by the crack response strain is shown below: (10.5) in, a It is the crack coefficient.
Citation Information
Patent Citations
Optical fiber grating pulse diagnosis sensor probe and dense array fiber optic pulse diagnosis instrument
CN104257363B
Demodulation method based on dense identical grating partition sensing
CN108548548B
Device and Method for Integrity Detection of Cast-in-Place Piles Based on Densely Distributed Fiber Bragg Grating Temperature Sensing Technology
CN113026829B
Multi-parameter detection system and method based on dense fiber bragg grating
CN116164858A