A special packaging bag for lithium battery negative electrode material and preparation method thereof
By using modified fiber particles and modified resin in the lithium battery negative electrode material packaging bag, an electron flow path and a tight intermolecular structure are formed, which solves the problem of static electricity and leakage during the transportation of lithium battery negative electrode material, and improves the antistatic and Mechanical and chemical resistance properties improve transportation safety and cost-effectiveness.
Patent Information
- Application Number
- CN202410352733.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-03-26
AI Technical Summary
Lithium battery anode materials are prone to static electricity accumulation, discharge and powder material leakage during transportation and packaging. The existing packaging containers have insufficient antistatic properties and sealing properties, resulting in unsafe and high-cost transportation.
A double-layer packaging bag made of PET-based material. The outer protective bag and the inner bag are fixed by heat bonding. Modified fiber particles and modified resin are added to the inner bag. The modified fiber particles are composed of zinc oxide, frame structure and carbon fiber. , forming an electron circulation path to reduce the electron movement speed, and the modified resin increases the tightness between molecules to improve chemical resistance.
It significantly improves the antistatic properties, mechanical properties and chemical resistance of the packaging bag, avoids electrostatic deposition, dust absorption and discharge phenomena, enhances transportation safety and sealing, and reduces transportation costs.
Abstract
Description
Technical Field
[0001] The present application relates to the field of packaging bags, and in particular to a special packaging bag for lithium battery negative electrode materials and a preparation method thereof. Background Art
[0002] In recent years, due to the continuous development of new energy vehicles and the urgent need to replace other old energy forms, the lithium battery industry has developed rapidly, especially the production of lithium batteries has reached its peak in recent years. However, with the rapid development of the lithium battery industry, the additional problems brought by lithium batteries have become increasingly prominent.
[0003] Among them, the transportation and packaging of lithium battery materials and waste has become one of the main problems in various lithium battery-related industries. During the transportation and packaging of existing lithium battery materials, especially negative electrode materials, static electricity and powder material leakage are prone to occur during transportation. In addition, existing packaging and transportation containers mainly use small packages, with limited solvents and high packaging costs. Therefore, how to obtain a large-package product with excellent antistatic and sealing properties to effectively package and transport the negative electrode materials of lithium batteries has become the focus of recent research and development personnel.
[0004] Polyethylene terephthalate (PET) material has been widely used in the field of packaging materials in recent years due to its excellent mechanical properties, heat and cold resistance, and chemical resistance. However, as a packaging material for lithium battery materials, due to the partial insulation of PET material, static electricity accumulation, discharge, and dust absorption are prone to occur during the transportation of lithium battery negative electrode materials, which hinders its application in related environments.
[0005] In order to solve the above problems, the present application provides a PET-based lithium battery negative electrode material special packaging material and its packaging bag, which can overcome the shortcomings of the existing technology and provide a negative electrode material special packaging bag with excellent mechanical properties, weather resistance, corrosion resistance and antistatic properties, avoiding the electrostatic deposition, dust absorption, discharge and other phenomena of the negative electrode material during the transportation and packaging process, and has a very excellent market prospect. Summary of the invention
[0006] In order to solve the above problems, the first aspect of the present application provides a special packaging bag for lithium battery negative electrode materials, which includes an outer protective bag and an inner bag, and the outer protective bag and the inner bag are fixed by heat bonding; the inner bag is used to hold lithium battery negative electrode materials.
[0007] As a preferred solution, the thickness of the outer protective bag is 0.5-1.5 mm.
[0008] As a preferred solution, the thickness of the inner bag is 0.1-0.5 mm.
[0009] As a preferred solution, the outer protective bag comprises, by weight, 90 to 140 parts of PET masterbatch, 10 to 35 parts of reinforcing particles, and 1 to 20 parts of additives.
[0010] As a preferred solution, the mass ratio of the PET masterbatch to the reinforcing particles is (10-12): (1-2.5).
[0011] As a preferred solution, the mass ratio of the PET masterbatch to the reinforced particles is (10-11): (1.5-2).
[0012] As a preferred solution, the reinforcing particles are a composition of metal oxides and modified fiber particles.
[0013] As a preferred solution, the mass ratio of the metal oxide to the modified fiber particles is (0.5-1):(2-4).
[0014] As a preferred solution, the average particle size of the reinforcing particles is 0.1-10 μm.
[0015] As a preferred solution, the metal oxide is at least one of zinc oxide, antimony oxide, aluminum oxide, titanium dioxide, silicon dioxide, and manganese dioxide.
[0016] As a preferred scheme, the preparation method of the modified fiber particles includes the following steps: S1: adding zinc oxide, metal nitrate and organic acid to deionized water and stirring evenly at room temperature, then adding them together into a closed reflux high-pressure reactor, gradually heating up to 180-200°C at a heating rate of 2-3°C / min, then continuously stirring for reaction for 8-12h, naturally cooling to room temperature after the reaction is completed, centrifuging and washing to obtain pretreated solid particles; S2: mixing the pretreated solid particles with ammonia water and adding them to anhydrous ethanol to obtain a mixed solution, preparing an anhydrous ethanol solution of tetraethyl orthosilicate, heating to 50-60°C and dripping the anhydrous ethanol solution of tetraethyl orthosilicate into the mixed solution, and the dripping reaction time is 2-4h; S3: ultrasonically mixing the product solution obtained in S2 with a water-ethanol solution containing carbon fibers for 6-8h, the ultrasonic mixing temperature is 60-65°C, and the ultrasonic power is 200-400W.
[0017] As a preferred solution, the metal nitrate is at least one of chromium nitrate and nickel nitrate.
[0018] As a preferred solution, the organic acid is terephthalic acid and acetic acid.
[0019] As a preferred solution, the mass ratio of zinc oxide, metal nitrate, terephthalic acid and acetic acid is (1-1.5): (1-1.5): (3-4): (10-15).
[0020] As a preferred solution, the mass ratio of zinc oxide, metal nitrate, terephthalic acid and acetic acid is 1:1.2:3.5:12.
[0021] In the present application, by adding the above-mentioned modified fiber particles to the outer protective bag and the inner bag raw materials, the antistatic performance of the packaging bag can be greatly improved, and the mechanical properties and chemical resistance of the bag can also be greatly improved. This is mainly because the fiber particles obtained by the above-mentioned modification in the present application can rely on the electron flow path formed by zinc oxide, frame structure and carbon fiber, and form a good electron transport and migration track. The connection of this path can greatly reduce the movement speed of electrons in the inner bag and the outer protective bag, and because of the difference in the electron conduction bands of the three, the path will not form a large-scale electron return, so that most of the electrons are directly released on the surface of the bag, thereby avoiding the accumulation of electrons, and because the above-mentioned modified fiber particles are added to the inner and outer bags, the electrons are more smoothly transmitted in the inner and outer bags; on the other hand, the composite structure formed by the fiber particles successfully encapsulates the zinc oxide particles, avoiding the excessive water absorption and hydration caused by the large number of hydroxyl groups on its surface due to the addition of a large number of zinc oxide particles, thereby ensuring the bag's tolerance to the external climate and improving its own strength.
[0022] As a preferred solution, the average particle size of the zinc oxide is 10 to 100 nm.
[0023] As a preferred solution, the average particle size of the zinc oxide is 10 to 30 nm.
[0024] As a preferred solution, the mass ratio of the pretreated solid particles to tetraethyl orthosilicate is (1-2): (0.5-2).
[0025] As a preferred solution, the mass ratio of the pretreated solid particles to tetraethyl orthosilicate is 1.5:1.
[0026] As a preferred solution, the mass ratio of the product in the product solution obtained in S2 to the carbon fiber is (1-1.5):(3-4).
[0027] On the other hand, the applicant has found that further controlling the particle size of zinc oxide particles, as well as the mass ratio of pre-treated solid particles and tetraethyl orthosilicate, can further improve the antistatic and water-resistant and weather-resistant effects. This is mainly because, through the limitation of the above scheme, it is possible to achieve a certain wrapping and adhesion effect of the framework particles on zinc oxide. If the particle size of the zinc oxide particles is too large, it will significantly affect the formation of the framework particles. On the contrary, if it is too small, it will block the microporous space of the framework particles, thereby hindering the adsorption of the framework particles on the water molecules of the bag body internal system, thereby greatly reducing the water resistance. And the above scheme can form a sol-adhesive amorphous silicide on the surface of the frame and zinc oxide composite particles. The presence of the silicide can accelerate the insertion rate and effect of the composite particles in the carbon fiber, thereby in fact forming a fiber-supported linear structure supported by multiple particle points, which can play an obvious supporting and connecting role when the bag body is subjected to external forces.
[0028] As a preferred solution, the auxiliary agent is at least one of a dispersant, a wetting agent, a high temperature resistant agent, a UV resistant agent, a waterproofing agent, and a surfactant.
[0029] As a preferred solution, the auxiliary agent is a dispersant.
[0030] As a preferred solution, the dispersant is ammonium stearate.
[0031] As a preferred solution, the raw materials of the inner bag include, by weight: 80 to 100 parts of PET masterbatch, 10 to 20 parts of modified resin, 10 to 15 parts of modified fiber particles, 5 to 10 parts of flame retardant, 1 to 5 parts of stabilizer, 0.5 to 1 part of defoaming agent, 1 to 3 parts of cross-linking agent, and 1 to 5 parts of polyethylene glycol.
[0032] As a preferred solution, the mass ratio of PET masterbatch, modified resin and modified fiber particles is (8.5-10):(1.5-2):1.
[0033] As a preferred solution, the mass ratio of PET masterbatch, modified resin and modified fiber particles is 8.5:1.5:1.
[0034] As a preferred solution, the modified fiber particles in the inner bag are consistent with the modified fiber particles in the outer protective bag.
[0035] As a preferred scheme, the preparation method of the modified resin includes the following steps: S1: adding terephthalic acid, adipic acid and glutaric acid to a reaction container in sequence, and then adding ethylene glycol and tetrabutyl titanate to the reaction container and mixing evenly; S2: stirring and mixing at a rate of 100 to 200 r / min, heating to 200 to 220°C and reacting for 3 to 4 hours, cooling to 160 to 180°C after completion, adding hydroquinone and tetrabutyl titanate, heating to 220 to 240°C and keeping warm for reaction for 6 to 8 hours; S3: after the reaction is completed, cooling the product to 50 to 60°C, adding succinic anhydride and 3-aminopropyltriethoxysilane, stirring at a rate of 60 to 120 r / min for reaction for 3 to 4 hours, and centrifuging, washing and drying the product after completion to obtain.
[0036] As a preferred solution, the mass ratio of terephthalic acid, adipic acid and glutaric acid is (14-16): (1-2): (3-5).
[0037] As a preferred solution, the mass ratio of terephthalic acid to ethylene glycol is (14-16):(9-10).
[0038] As a preferred solution, the added amounts of succinic anhydride and 3-aminopropyltriethoxysilane are (5-10wt%) and (3-5wt%) of the mass of the S2 product, respectively.
[0039] In this application, the addition of the modified resin can greatly improve the chemical resistance and mechanical properties of the packaging bag. This is mainly because the modified resin prepared by the above modification method in this application can use its more branched long chains to form a good internal network system with other raw materials, thereby greatly increasing the intermolecular tightness of the internal system of the inner bag, having suitable steric hindrance between active molecules, reducing the flow and collision efficiency of active molecules, and thus providing greater resistance to the penetration of external chemical molecules; on the other hand, the tighter intermolecular connection can also play a better intermolecular bonding role when the outside world acts, thereby effectively enhancing the mechanical strength of the inner bag; and the stronger intermolecular bonding effect can further enhance the fitting strength of the inner bag and the outer protective bag, thereby greatly improving the performance of the packaging bag.
[0040] As a preferred solution, the flame retardant is at least one of molybdenum trioxide, magnesium oxide, and aluminum oxide.
[0041] As a preferred solution, the cross-linking agent is polyisocyanate.
[0042] As a preferred solution, the polyethylene glycol is polyethylene glycol 200 and polyethylene glycol 800.
[0043] As a preferred solution, the mass ratio of polyethylene glycol 200 to polyethylene glycol 800 is (1-3): (1-3).
[0044] The second aspect of the present application provides a method for preparing the above-mentioned special packaging bag for lithium battery negative electrode materials, and the preparation method includes the following steps: S1: melt-mixing and drawing the raw materials of the outer protective bag into a film bag; S2: melt-mixing and blow-forming the raw materials of the inner bag; S3: adding and fixing the outer protective bag and the inner bag by means of heat bonding, and the bag is obtained after completion.
[0045] The beneficial effects of this application are:
[0046] 1. The special packaging bag for lithium battery negative electrode materials provided in this application can overcome the shortcomings of the existing technology and at the same time has excellent mechanical properties, weather resistance, corrosion resistance and antistatic properties, avoiding electrostatic deposition, dust absorption, discharge and other phenomena of negative electrode materials during transportation and packaging, and has very excellent market prospects.
[0047] 2. A special packaging bag for lithium battery negative electrode materials provided in the present application can greatly improve the antistatic performance of the packaging bag while also greatly improving the mechanical properties and chemical resistance of the bag body by adding modified fiber particles; the modified fiber particles can rely on the electron flow path formed by zinc oxide, frame structure and carbon fiber to form a good electron transport and migration track, and the connection of this path can greatly reduce the movement speed of electrons in the inner bag and the outer protective bag body, and because of the difference in the electron conduction bands of the three, the path will not form a large-scale electron migration, so that most of the electrons are directly released on the surface of the bag body, thereby avoiding the accumulation of electrons, and because the above-mentioned modified fiber particles are added to the inner and outer bags, the transmission of electrons between the inner and outer bags is smoother.
[0048] 3. A special packaging bag for lithium battery negative electrode materials provided in the present application can further improve the antistatic and water-resistant and weather-resistant effects by controlling the particle size of zinc oxide particles and the mass ratio of pre-treated solid particles and tetraethyl orthosilicate; under the above scheme, the modified fiber particles can achieve a certain wrapping and adhesion effect of the framework particles on zinc oxide. If the particle size of the zinc oxide particles is too large, it will significantly affect the formation of the framework particles. On the contrary, if it is too small, it will block the microporous space of the framework particles, thereby hindering the adsorption of moisture molecules in the bag body system by the framework particles, thereby greatly reducing water resistance. And the above scheme can form a sol-adhesive amorphous silicide on the surface of the framework and zinc oxide composite particles. The presence of the silicide can accelerate the insertion rate and effect of the composite particles in the carbon fiber, thereby forming a fiber-supported linear structure supported by multiple particles.
[0049] 4. A special packaging bag for lithium battery negative electrode materials provided in this application can greatly improve the chemical resistance and mechanical properties of the packaging bag by adding modified resin. This is mainly because the modified resin prepared by the above-mentioned modification method in this application can use its more branched long chains to form a good internal network system with other raw materials, thereby greatly increasing the intermolecular tightness of the internal system of the inner bag, having suitable steric hindrance between active molecules, reducing the flow and collision efficiency of active molecules, and thus providing greater resistance to the penetration of external chemical molecules; on the other hand, tighter intermolecular connections can also play a better intermolecular bonding role when the outside world acts, thereby effectively enhancing the mechanical strength of the inner bag; and stronger intermolecular bonding can further enhance the fitting strength of the inner bag and the outer protective bag, thereby greatly improving the performance of the packaging bag.
[0050] 5. The special packaging bag for lithium battery negative electrode materials provided in this application has a simple preparation method and is easy to operate. It does not involve complex and highly polluting chemical reactions and is not obviously corrosive to equipment. Therefore, it can effectively control the labor and equipment maintenance costs of production during large-scale production and has excellent market value. DETAILED DESCRIPTION
[0051] The following will further explain and demonstrate the technical solutions in the above invention content of this application in the form of specific implementation schemes. The following embodiments are only practical examples used to illustrate and explain the contents of the technical solutions in the specification, and should not limit the scope of the claims to be protected by this application. All technical products based on the technical solutions described in the invention content of this application should be included in the scope to be protected by this application.
[0052] In the following examples, unless otherwise specified, the raw materials are all commercially available products, or can be prepared by methods well known to those skilled in the art.
[0053] Example 1
[0054] Embodiment 1 provides a first aspect of a special packaging bag for negative electrode materials of lithium batteries, which includes an outer protective bag and an inner bag, and the outer protective bag and the inner bag are fixed by heat bonding; the inner bag is used to hold negative electrode materials of lithium batteries.
[0055] The thickness of the outer protective bag is 1mm; the thickness of the inner bag is 0.3mm.
[0056] The outer protective bag, calculated by weight, includes the following raw materials: 105 parts of PET masterbatch, 20 parts of reinforcing particles, and 5 parts of additives.
[0057] The reinforcing particles are titanium dioxide and modified fiber particles, and the mass ratio of the two is 1:3.
[0058] The average particle size of titanium dioxide is 0.15 μm; the average particle size of modified fiber particles is 5.2 μm.
[0059] The preparation method of modified fiber particles comprises the following steps, calculated by mass: S1: 1 part of zinc oxide (average particle size 20 nm), 1.2 parts of metal nitrate (chromium nitrate: nickel nitrate = 2:1), 3.5 parts of terephthalic acid and 12 parts of acetic acid are added to 100 parts of deionized water and stirred evenly at room temperature, and then added together into a closed reflux autoclave, and the temperature is gradually increased to 200°C at a rate of 2°C / min, and then the reaction is continued with stirring for 10 hours. After the reaction is completed, the temperature is naturally lowered to room temperature, and the pre-filtered fiber particles are centrifuged and washed to obtain the pre-filtered fiber particles. Treat solid particles; S2: Mix 1.5 parts of pretreated solid particles with 2 parts of ammonia water (concentration 20wt%) and add them to 50 parts of anhydrous ethanol to obtain a mixed solution, prepare an anhydrous ethanol solution containing 1 part of tetraethyl orthosilicate in a total of 10 parts, heat the temperature to 60°C and drop the anhydrous ethanol solution of tetraethyl orthosilicate into the mixed solution, and the dropwise reaction time is 2h; S3: Ultrasonic mix the product solution obtained in S2 with a water-ethanol solution containing carbon fibers for 6h, the ultrasonic mixing temperature is 60°C, and the ultrasonic power is 300W.
[0060] The mass ratio of the product to the carbon fiber in the product solution obtained in S2 is 1:3.
[0061] The carbon fiber was purchased from chopped carbon fiber products sold by Shanghai Lishuo Composite Materials Technology Co., Ltd. and was chopped to a length of 5 μm.
[0062] The auxiliary agent is the dispersant ammonium stearate.
[0063] The raw materials of the inner bag, calculated by mass, include: 85 parts of PET masterbatch, 15 parts of modified resin, 10 parts of modified fiber particles, 6 parts of flame retardant, 2 parts of stabilizer, 0.5 parts of defoaming agent, 2 parts of cross-linking agent, and 4 parts of polyethylene glycol.
[0064] The modified fiber particles in the inner bag are consistent with the modified fiber particles in the outer protective bag.
[0065] The PET masterbatch in the inner bag is consistent with the PET masterbatch in the outer protective bag, purchased from China Resources Polyester (Changzhou) Co., Ltd., 8863.
[0066] The preparation method of the modified resin comprises the following steps, calculated by mass: S1: 15 parts of terephthalic acid, 2 parts of adipic acid and 4 parts of glutaric acid are added to a reaction container in sequence, and then 9 parts of ethylene glycol and 0.1 parts of tetrabutyl titanate are added to the reaction container and mixed evenly; S2: the mixture is stirred and mixed at a rate of 200 r / min, the temperature is raised to 220°C and the reaction is carried out for 3 hours, after the mixture is cooled to 180°C, 2 parts of hydroquinone and 0.1 parts of tetrabutyl titanate are added, the temperature is raised to 240°C and the reaction is kept for 6 hours; S3: after the reaction is completed, the product is cooled to 55°C, succinic anhydride (product 5wt%) and 3-aminopropyltriethoxysilane (product 3wt%) are added, the reaction is stirred at a rate of 100 r / min for 3 hours, and the product is centrifugally washed and dried to obtain the product.
[0067] The flame retardant is magnesium oxide; the stabilizer is dibutyltin dilaurate; the defoamer is BYK-A500; and the cross-linking agent is polyisocyanate.
[0068] The polyethylene glycol is polyethylene glycol 200 and polyethylene glycol 800, and the mass ratio is 1:1.
[0069] The second aspect of this embodiment provides a method for preparing the above-mentioned special packaging bag for lithium battery negative electrode materials, and the preparation method includes the following steps: S1: melt-mixing and drawing the raw materials of the outer protective bag into a film bag; S2: melt-mixing and blow-forming the raw materials of the inner bag; S3: adding and fixing the outer protective bag and the inner bag by means of heat bonding, and the bag is obtained after completion.
[0070] Example 2
[0071] Embodiment 2 The first aspect provides a special packaging bag for negative electrode materials of lithium batteries, which includes an outer protective bag and an inner bag, and the outer protective bag and the inner bag are fixed by heat bonding; the inner bag is used to hold negative electrode materials of lithium batteries.
[0072] The thickness of the outer protective bag is 1mm; the thickness of the inner bag is 0.3mm.
[0073] The raw materials of the outer protective bag, calculated by weight, include: 120 parts of PET masterbatch, 10 parts of reinforcing particles, and 5 parts of additives.
[0074] The reinforcing particles are titanium dioxide and modified fiber particles, and the mass ratio of the two is 1:3.
[0075] The average particle size of titanium dioxide is 0.15 μm; the average particle size of modified fiber particles is 3.2 μm.
[0076] The preparation method of modified fiber particles comprises the following steps, calculated by mass: S1: 1 part of zinc oxide (average particle size 20 nm), 1.2 parts of metal nitrate (chromium nitrate: nickel nitrate = 2:1), 3.5 parts of terephthalic acid and 12 parts of acetic acid are added to 100 parts of deionized water and stirred evenly at room temperature, and then added together into a closed reflux autoclave, and the temperature is gradually increased to 200°C at a rate of 2°C / min, and then the reaction is continued with stirring for 10 hours. After the reaction is completed, the temperature is naturally lowered to room temperature, and the pre-filtered fiber particles are centrifuged and washed to obtain the pre-filtered fiber particles. Treat solid particles; S2: Mix 1.5 parts of pretreated solid particles with 2 parts of ammonia water (concentration 20wt%) and add them to 50 parts of anhydrous ethanol to obtain a mixed solution, prepare an anhydrous ethanol solution containing 1 part of tetraethyl orthosilicate in a total of 10 parts, heat the temperature to 60°C and drop the anhydrous ethanol solution of tetraethyl orthosilicate into the mixed solution, and the dropwise reaction time is 2h; S3: Ultrasonic mix the product solution obtained in S2 with a water-ethanol solution containing carbon fibers for 6h, the ultrasonic mixing temperature is 60°C, and the ultrasonic power is 300W.
[0077] The mass ratio of the product to the carbon fiber in the product solution obtained in S2 is 1.5:4.
[0078] The carbon fiber was purchased from chopped carbon fiber products sold by Shanghai Lishuo Composite Materials Technology Co., Ltd. and was chopped to a length of 5 μm.
[0079] The auxiliary agent is the dispersant ammonium stearate.
[0080] The raw materials of the inner bag, calculated by weight, include: 100 parts of PET masterbatch, 20 parts of modified resin, 10 parts of modified fiber particles, 6 parts of flame retardant, 2 parts of stabilizer, 0.5 parts of defoaming agent, 2 parts of cross-linking agent, and 4 parts of polyethylene glycol.
[0081] The modified fiber particles in the inner bag are consistent with the modified fiber particles in the outer protective bag.
[0082] The PET masterbatch in the inner bag is consistent with the PET masterbatch in the outer protective bag, purchased from China Resources Polyester (Changzhou) Co., Ltd., 8863.
[0083] The preparation method of the modified resin comprises the following steps, calculated by mass: S1: 15 parts of terephthalic acid, 2 parts of adipic acid and 4 parts of glutaric acid are added to a reaction container in sequence, and then 9 parts of ethylene glycol and 0.1 parts of tetrabutyl titanate are added to the reaction container and mixed evenly; S2: the mixture is stirred and mixed at a rate of 200 r / min, the temperature is raised to 220°C and the reaction is carried out for 3 hours, after the mixture is cooled to 180°C, 2 parts of hydroquinone and 0.1 parts of tetrabutyl titanate are added, the temperature is raised to 240°C and the reaction is kept for 6 hours; S3: after the reaction is completed, the product is cooled to 55°C, succinic anhydride (product 5wt%) and 3-aminopropyltriethoxysilane (product 3wt%) are added, the reaction is stirred at a rate of 100 r / min for 3 hours, and the product is centrifugally washed and dried to obtain the product.
[0084] The flame retardant is magnesium oxide; the stabilizer is dibutyltin dilaurate; the defoamer is BYK-A500; and the cross-linking agent is polyisocyanate.
[0085] The polyethylene glycol is polyethylene glycol 200 and polyethylene glycol 800, and the mass ratio is 1:1.
[0086] The second aspect of this embodiment provides a method for preparing the above-mentioned special packaging bag for lithium battery negative electrode materials, and the preparation method includes the following steps: S1: melt-mixing and drawing the raw materials of the outer protective bag into a film bag; S2: melt-mixing and blow-forming the raw materials of the inner bag; S3: adding and fixing the outer protective bag and the inner bag by means of heat bonding, and the bag is obtained after completion.
[0087] Example 3
[0088] Embodiment 3 provides a first aspect of a special packaging bag for negative electrode materials of lithium batteries, which includes an outer protective bag and an inner bag, and the outer protective bag and the inner bag are fixed by heat bonding; the inner bag is used to contain negative electrode materials of lithium batteries.
[0089] The thickness of the outer protective bag is 1mm; the thickness of the inner bag is 0.3mm.
[0090] The outer protective bag, calculated by weight, includes the following raw materials: 105 parts of PET masterbatch, 20 parts of reinforcing particles, and 5 parts of additives.
[0091] The reinforcing particles are titanium dioxide and modified fiber particles, and the mass ratio of the two is 1:2.
[0092] The average particle size of titanium dioxide is 0.15 μm; the average particle size of modified fiber particles is 3.2 μm.
[0093] The preparation method of modified fiber particles comprises the following steps, calculated by mass: S1: 1.5 parts of zinc oxide (average particle size 25 nm), 1.5 parts of metal nitrate (chromium nitrate: nickel nitrate = 2:1), 3 parts of terephthalic acid and 12 parts of acetic acid are added to 100 parts of deionized water and stirred evenly at room temperature, and then added together into a closed reflux autoclave, and the temperature is gradually increased to 200°C at a rate of 2°C / min, and then the reaction is continued with stirring for 10 hours. After the reaction is completed, the temperature is naturally lowered to room temperature, and centrifuged and washed to obtain a pre- Treat solid particles; S2: Mix 1.5 parts of pretreated solid particles with 2 parts of ammonia water (concentration 20wt%) and add them to 50 parts of anhydrous ethanol to obtain a mixed solution, prepare an anhydrous ethanol solution containing 1 part of tetraethyl orthosilicate in a total of 10 parts, heat the temperature to 60°C and drop the anhydrous ethanol solution of tetraethyl orthosilicate into the mixed solution, and the dropwise reaction time is 2h; S3: Ultrasonic mix the product solution obtained in S2 with a water-ethanol solution containing carbon fibers for 6h, the ultrasonic mixing temperature is 60°C, and the ultrasonic power is 300W.
[0094] The mass ratio of the product to the carbon fiber in the product solution obtained in S2 is 1.5:3.
[0095] The carbon fiber was purchased from chopped carbon fiber products sold by Shanghai Lishuo Composite Materials Technology Co., Ltd. and was chopped to a length of 5 μm.
[0096] The auxiliary agent is the dispersant ammonium stearate.
[0097] The raw materials of the inner bag, calculated by mass, include: 85 parts of PET masterbatch, 15 parts of modified resin, 10 parts of modified fiber particles, 6 parts of flame retardant, 2 parts of stabilizer, 0.5 parts of defoaming agent, 2 parts of cross-linking agent, and 4 parts of polyethylene glycol.
[0098] The modified fiber particles in the inner bag are consistent with the modified fiber particles in the outer protective bag.
[0099] The PET masterbatch in the inner bag is consistent with the PET masterbatch in the outer protective bag, purchased from China Resources Polyester (Changzhou) Co., Ltd., 8863.
[0100] The preparation method of the modified resin comprises the following steps, calculated by mass: S1: 14 parts of terephthalic acid, 1.5 parts of adipic acid and 5 parts of glutaric acid are added to a reaction container in sequence, and then 10 parts of ethylene glycol and 0.1 parts of tetrabutyl titanate are added to the reaction container and mixed evenly; S2: the mixture is stirred and mixed at a rate of 200 r / min, the temperature is raised to 220°C and the reaction is carried out for 3 hours, after the mixture is cooled to 180°C, 2.5 parts of hydroquinone and 0.1 parts of tetrabutyl titanate are added, the temperature is raised to 240°C and the reaction is kept for 6 hours; S3: after the reaction is completed, the product is cooled to 55°C, succinic anhydride (product 6wt%) and 3-aminopropyltriethoxysilane (product 4wt%) are added, the reaction is stirred at a rate of 100 r / min for 3 hours, and the product is centrifugally washed and dried to obtain the product.
[0101] The flame retardant is magnesium oxide; the stabilizer is dibutyltin dilaurate; the defoamer is BYK-A500; and the cross-linking agent is polyisocyanate.
[0102] The polyethylene glycol is polyethylene glycol 200 and polyethylene glycol 800, and the mass ratio is 2:1.
[0103] The second aspect of this embodiment provides a method for preparing the above-mentioned special packaging bag for lithium battery negative electrode materials, and the preparation method includes the following steps: S1: melt-mixing and drawing the raw materials of the outer protective bag into a film bag; S2: melt-mixing and blow-forming the raw materials of the inner bag; S3: adding and fixing the outer protective bag and the inner bag by means of heat bonding, and the bag is obtained after completion.
[0104] Comparative Example 1
[0105] The specific implementation of this comparative example is basically the same as that of Example 1, except that the reinforcing particles are titanium dioxide and carbon fibers, and the mass ratio of the two is 1:3.
[0106] Comparative Example 2
[0107] The specific implementation of this comparative example is basically the same as that of Example 1, except that: the preparation method of the modified fiber particles comprises the following steps, measured by mass: S1: 1 part of zinc oxide (average particle size 20 nm), 1.2 parts of metal nitrate (chromium nitrate: nickel nitrate = 2:1), 3.5 parts of terephthalic acid and 12 parts of acetic acid are added to 100 parts of deionized water and stirred evenly at room temperature, and then added together into a closed reflux high-pressure reactor, and the temperature is gradually increased to 200°C at a heating rate of 2°C / min, and then the reaction is continuously stirred for 10 hours. After the reaction is completed, the temperature is naturally lowered to room temperature, and the pretreated solid particles are obtained by centrifugation and washing; S2: 1.5 parts of the pretreated solid particles are ultrasonically mixed with a water-ethanol solution containing 5 parts of carbon fibers (a total of 80 parts) for 6 hours, the ultrasonic mixing temperature is 60°C, and the ultrasonic power is 300W.
[0108] Comparative Example 3
[0109] The specific implementation of this comparative example is basically the same as that of Example 1, except that: the preparation method of the modified fiber particles comprises the following steps, calculated by mass: S1: 3 parts of zinc oxide (average particle size 150 nm), 1 part of chromium nitrate, 1.5 parts of terephthalic acid and 3 parts of acetic acid are added to 50 parts of deionized water and stirred evenly at room temperature, then added together into a closed reflux autoclave, gradually heated to 200°C at a rate of 2°C / min, then stirred and reacted for 10 hours, cooled naturally to room temperature after the reaction was completed, and centrifuged to wash S2: Mix 2 parts of pretreated solid particles with 0.5 parts of ammonia water (concentration 20wt%) and add them to 50 parts of anhydrous ethanol to obtain a mixed solution, prepare an anhydrous ethanol solution containing 0.5 parts of tetraethyl orthosilicate in a total of 10 parts, heat to 60°C and drop the anhydrous ethanol solution of tetraethyl orthosilicate into the mixed solution, and the dropwise reaction time is 2h; S3: Ultrasonic mix the product solution obtained in S2 with the water-ethanol solution containing carbon fibers for 6h, the ultrasonic mixing temperature is 60°C, and the ultrasonic power is 300W, to obtain.
[0110] Comparative Example 4
[0111] The specific implementation of this comparative example is basically the same as that of Example 1, except that no modified resin is added to the inner bag, and the modified resin portion is filled by PET masterbatch.
[0112] Comparative Example 5
[0113] The specific implementation method of this comparative example is basically the same as that of Example 1, except that: the preparation method of the modified resin includes the following steps, in parts by mass: S1: 20 parts of terephthalic acid, 1.5 parts of adipic acid and 5 parts of glutaric acid are added to a reaction container in sequence, and then 10 parts of ethylene glycol and 0.1 parts of tetrabutyl titanate are added to the reaction container and mixed evenly: S2: Stirring and mixing at a rate of 200r / min, heating to 220°C and reacting for 3h, cooling to 180°C after completion, adding 2.5 parts of hydroquinone and 0.1 parts of tetrabutyl titanate, heating to 240°C and keeping warm for 6h, filtering, washing and drying after the reaction is completed.
[0114] Comparative Example 6
[0115] The specific implementation of this comparative example is basically the same as that of Example 1, except that: the preparation method of the modified resin comprises the following steps, measured in parts by mass: S1: 20 parts of terephthalic acid are added to a reaction container in sequence, and then 10 parts of ethylene glycol and 0.1 parts of tetrabutyl titanate are added to the reaction container and mixed evenly: S2: the temperature is raised to 220°C at a rate of 200 r / min for reaction for 3 hours, and after completion, the temperature is lowered to 180°C, 2.5 parts of hydroquinone and 0.1 parts of tetrabutyl titanate are added, the temperature is raised to 240°C for reaction for 6 hours; S3: after the reaction is completed, the product is cooled to 55°C, succinic anhydride (product 4wt%) and 3-aminopropyltriethoxysilane (product 1wt%) are added, the reaction is stirred at a rate of 100 r / min for 3 hours, and the product after completion is centrifuged, washed and dried to obtain.
[0116] Performance Evaluation
[0117] Tensile strength: The packaging bag samples prepared in the embodiments and comparative examples were subjected to a tensile strength test. The testing instrument was a universal tensile machine. The sample size was 3×3 cm. The average value of 10 test results was recorded in Table 1.
[0118] Water vapor permeability: The water vapor permeability of the packaging bag samples prepared in the embodiments and comparative examples was tested with reference to the standard GB / T 1037. The average value of the test results for 10 times was recorded in Table 1.
[0119] Antistatic property: The packaging bag samples prepared in the embodiments and comparative examples were subjected to surface resistance test, the test surface was the inner surface of the inner bag (the surface in contact with the negative electrode material), and the average value of 10 test results was recorded in Table 1.
[0120] Table 1
[0121] Example Tensile strength MPa <![CDATA[Water vapor transmission rate g / m 2 ·24h]]> Surface resistance Ω Example 1 44.6 2.45 <![CDATA[2.5×10 7 ]]> Example 2 41.8 3.14 <![CDATA[3.5×10 7 ]]> Example 3 44.9 2.98 <![CDATA[3.1×10 7 ]]> Comparative Example 1 32.4 8.45 <![CDATA[2.2×10 8 ]]> Comparative Example 2 33.4 9.14 <![CDATA[7.5×10 7 ]]> Comparative Example 3 31.9 9.66 <![CDATA[8.1×10 7 ]]> Comparative Example 4 36.4 10.14 <![CDATA[4.5×10 7 ]]> Comparative Example 5 37.2 8.63 <![CDATA[3.5×10 7 ]]> Comparative Example 6 35.7 9.27 <![CDATA[4.1×10 7 ]]>
[0122] From the examples and comparative examples of the present application and the data results in Table 1, it can be seen that the examples 1 to 3 which adopt the necessary technical solutions given in the present application have achieved excellent results in the performance tests of mechanical properties, antistatic properties, and water vapor permeability. This is mainly due to the specific modified fiber particles and modified resins in the examples 1 to 3 playing a conductive and supporting connection role in the packaging bag material, overcoming the technical problems of discharge, electrostatic deposition, dust absorption, etc. existing in the packaging and transportation of the existing lithium battery negative electrode material packaging bags. However, because the comparative examples 1 to 6 did not fully adopt the necessary technical solutions described by the applicant, they were significantly worse than the corresponding test results of the examples 1 to 3, which better proves the irreplaceable nature of the specific technical solutions of the present application in achieving technical effects and solving technical problems.
Claims
1. A special packaging bag for lithium battery negative electrode materials, characterized in that: A special packaging bag for lithium battery negative electrode materials, comprising an outer protective bag and an inner bag, wherein the outer protective bag and the inner bag are fixed by heat bonding; the inner bag is used to hold the lithium battery negative electrode materials; The thickness of the outer protective bag is 0.5 to 1.5 mm; The thickness of the inner bag is 0.1 to 0.5 mm; The outer protective bag comprises, by weight, 90 to 140 parts of PET masterbatch, 10 to 35 parts of reinforcing particles, and 1 to 20 parts of additives; The mass ratio of the PET masterbatch to the reinforcing particles is (10-12): (1-2.5); The reinforcing particles are a combination of metal oxide and modified fiber particles; the mass ratio of the metal oxide to the modified fiber particles is (0.5-1):(2-4); The average particle size of the reinforcing particles is 0.1 to 10 μm; The metal oxide is at least one of zinc oxide, antimony oxide, aluminum oxide, titanium dioxide, silicon dioxide, and manganese dioxide; The preparation method of the modified fiber particles comprises the following steps: S1: adding zinc oxide, metal nitrate and organic acid into deionized water and stirring them evenly at room temperature, then adding them into a closed reflux high-pressure reactor, gradually heating the temperature to 180-200°C at a heating rate of 2-3°C / min, then continuously stirring and reacting for 8-12 hours, naturally cooling the temperature to room temperature after the reaction is completed, and centrifuging and washing to obtain pretreated solid particles; S2: mixing the pretreated solid particles with ammonia water and adding them into anhydrous ethanol to obtain a mixed solution, preparing an anhydrous ethanol solution of tetraethyl orthosilicate, heating the temperature to 50-60°C, and dripping the anhydrous ethanol solution of tetraethyl orthosilicate into the mixed solution, and the dripping reaction time is 2-4 hours; S3: ultrasonically mixing the product solution obtained in S2 with a water-ethanol solution containing carbon fibers for 6-8 hours, the ultrasonic mixing temperature is 60-65°C, and the ultrasonic power is 200-400W, to obtain the obtained solid particles.
2. The special packaging bag for lithium battery negative electrode materials according to claim 1, characterized in that: The metal nitrate is at least one of chromium nitrate and nickel nitrate.
3. The special packaging bag for lithium battery negative electrode materials according to claim 2, characterized in that: The organic acids are terephthalic acid and acetic acid; the mass ratio of the zinc oxide, metal nitrate, terephthalic acid and acetic acid is (1-1.5): (1-1.5): (3-4): (10-15).
4. The special packaging bag for lithium battery negative electrode materials according to claim 3, characterized in that: The average particle size of the zinc oxide is 10 to 100 nm.
5. The special packaging bag for lithium battery negative electrode materials according to claim 4, characterized in that: The mass ratio of the pretreated solid particles to tetraethyl orthosilicate is (1-2): (0.5-2).
6. The special packaging bag for lithium battery negative electrode materials according to claim 5, characterized in that: The inner bag comprises, by weight, 80 to 100 parts of PET masterbatch, 10 to 20 parts of modified resin, 10 to 15 parts of modified fiber particles, 5 to 10 parts of flame retardant, 1 to 5 parts of stabilizer, 0.5 to 1 part of defoamer, 1 to 3 parts of crosslinking agent, and 1 to 5 parts of polyethylene glycol.
7. The special packaging bag for lithium battery negative electrode materials according to claim 6, characterized in that: In the inner bag, the mass ratio of the PET masterbatch, the modified resin and the modified fiber particles is (8.5-10):(1.5-2):
1.
8. The special packaging bag for lithium battery negative electrode materials according to claim 7, characterized in that: The preparation method of the modified resin comprises the following steps: S1: adding terephthalic acid, adipic acid and glutaric acid into a reaction container in sequence, and then adding ethylene glycol and tetrabutyl titanate into the reaction container and mixing evenly; S2: stirring and mixing at a rate of 100 to 200 r / min, heating to 200 to 220°C for reaction for 3 to 4 hours, cooling to 160 to 180°C after completion, adding hydroquinone and tetrabutyl titanate, heating to 220 to 240°C and keeping the temperature for reaction for 6 to 8 hours; S3: after the reaction is completed, cooling the product to 50 to 60°C, adding succinic anhydride and 3-aminopropyltriethoxysilane, stirring at a rate of 60 to 120 r / min for reaction for 3 to 4 hours, and centrifuging, washing and drying the product after completion to obtain the product.
9. The special packaging bag for lithium battery negative electrode materials according to claim 8, characterized in that: The mass ratio of terephthalic acid, adipic acid and glutaric acid is (14-16): (1-2): (3-5).
10. A method for preparing a special packaging bag for lithium battery negative electrode materials according to any one of claims 1 to 9, characterized in that: Preparation method The following steps are involved: S1: melt and mix the raw materials of the outer protective bag and draw and weave them into a film bag; S2: mix and melt the raw materials of the inner bag and blow film to form; S3: fix the outer protective bag and the inner bag by means of heat bonding and fixing, and the bag is obtained after completion.