Method for reinforcing a beam of an existing building

By adding temporary supports at the bottom of existing building beams, determining stress points, drilling holes to implant prestressed tendons, and then pouring reinforced concrete, and by using infrared and laser beams to treat cracks, the potential cracks and deformation problems of beams in existing technologies have been solved, improving the safety and performance of the beams.

CN118208064BActive Publication Date: 2026-11-10CHINA CONSTRUCTION INDUSTRIAL & ENERGY ENGINEERING GROUP CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410439437.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-12
Publication Date
2026-11-10
Estimated Expiration
2044-04-12

AI Technical Summary

Technical Problem

Existing methods for reinforcing existing building beams cannot completely eliminate potential cracks and deformations in the beams, leading to safety hazards during use, and the reinforcement effect weakens over time.

Method used

By adding temporary supports at the bottom of the beams, using lasers to determine the dimensions and deformation, estimating the load and identifying the main and auxiliary stress points, drilling holes to insert prestressed tendons, pouring reinforced concrete, accelerating solidification with infrared irradiation, scanning internal cracks with an infrared radiation meter and welding with laser beams, and finally treating the surface to complete the reinforcement.

Benefits of technology

It effectively eliminates cracks and deformations in the beams, improves the load-bearing capacity and stiffness of the beams, ensures the safety and performance of the building structure, extends its service life, reduces the frequency of maintenance and replacement, and reduces energy consumption and environmental pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118208064B_ABST
    Figure CN118208064B_ABST
Patent Text Reader

Abstract

The application provides a method for reinforcing an existing building beam, and belongs to the technical field of reinforcing an existing building beam. The method comprises the following steps: supporting and replacing the bottom of the existing building beam, and increasing temporary support for the existing building beam; a construction worker determines the size and deformation of the existing building beam by comparing a laser with a construction drawing; the load borne by the existing building beam is estimated; the drilling position is determined; after drilling, prestressed reinforcement is placed and then reinforced concrete is poured; the solidification of the reinforced concrete is accelerated by infrared irradiation; and the cracks inside the existing building beam are welded by a laser beam. The method can solve the problem that the existing method for reinforcing an existing building beam cannot completely eliminate potential cracks and deformation of the beam body, resulting in certain safety hazards in the use process of the beam body, and the reinforcing effect will weaken over time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of existing building beam reinforcement technology, specifically, it relates to a method for reinforcing existing building beams. Background Technology

[0002] With the acceleration of urbanization in my country, the renovation and maintenance of existing buildings are receiving increasing attention. Among these efforts, the reinforcement of existing building beams is a crucial task. Building beams are an essential component of the building structure, bearing the building's load and self-weight, and transferring the load to the columns. If beams develop cracks, deformation, or damage, it will affect the overall stability of the building and may even lead to collapse. Therefore, reinforcing existing building beams can ensure the safety of the building structure and extend its service life. Reinforcing existing building beams not only ensures structural safety but also improves the building's performance. Through reinforcement, the beam's load-bearing capacity can be increased, beam deflection reduced, beam deformation minimized, and beam stiffness improved. Simultaneously, reinforced beams can better adapt to the building's usage requirements, enhancing its performance. Non-destructive testing techniques, such as non-destructive testing and infrared thermal imaging, can be used to inspect and diagnose existing building beams, thus avoiding excavation and damage and improving construction efficiency. Meanwhile, reinforced beams can better adapt to the building's usage requirements, reducing the frequency of beam maintenance and replacement, and lowering maintenance costs. Reinforcing existing building beams can reduce the frequency of beam maintenance and replacement, lowering energy consumption and environmental pollution. Furthermore, reinforced beams can better adapt to the building's usage requirements, improving the building's performance and thus increasing its economic value and environmental benefits.

[0003] Existing methods for reinforcing existing building beams cannot completely eliminate potential cracks and deformations in the beams, resulting in certain safety hazards during use. Over time, the reinforcement effect will weaken. Summary of the Invention

[0004] In view of this, the present invention provides a method for reinforcing existing building beams, which can solve the problem that existing methods for reinforcing existing building beams cannot completely eliminate potential cracks and deformations in the beams, resulting in certain safety hazards in the beams during use, and the reinforcement effect weakening over time.

[0005] This invention is implemented as follows:

[0006] This invention provides a method for reinforcing existing building beams, comprising the following steps:

[0007] S10: Replace the bottom support of the existing building beams to add temporary support to the existing building beams;

[0008] S20: Construction workers use lasers to compare with construction drawings to determine the dimensions and deformation of the existing building beams;

[0009] S30: By estimating the load on the existing building beams and corresponding it with the changes in the dimensions of the existing building beams, the direction, angle and size of the deformation and bending, the main stress points and auxiliary stress points of the existing building beams are determined.

[0010] S40: Determine the drilling location, insert prestressed tendons after drilling, and then pour in reinforced concrete. Accelerate the solidification of the reinforced concrete by infrared irradiation.

[0011] S50: Scan the surface of the existing building beams with an infrared radiation meter to determine the internal cracks of the existing building beams, and weld the internal cracks of the existing building beams with a laser beam.

[0012] S60: The surface of the existing building beams is treated to complete the reinforcement of the existing building beams.

[0013] The technical effects of the existing building beam reinforcement method provided by this invention are as follows: Temporary support is added to the existing building beam by supporting and replacing the bottom of the beam; construction personnel determine the dimensions and deformation of the existing building beam by laser comparison with construction drawings; the main and auxiliary stress points of the existing building beam are determined by estimating the load on the beam and corresponding it with changes in the beam's dimensions, the direction, angle, and size of deformation and bending; drilling locations are determined, prestressed tendons are inserted after drilling, and reinforced concrete is poured in; the solidification of the reinforced concrete is accelerated by infrared irradiation; the surface of the existing building beam is scanned with an infrared radiation instrument to determine the internal cracks, and the internal cracks are welded using a laser beam; the surface of the existing building beam is treated to complete the reinforcement; this method solves the problem that existing building beam reinforcement methods cannot completely eliminate potential cracks and deformations in the beam, resulting in certain safety hazards during use and a weakening reinforcement effect over time.

[0014] Based on the above technical solution, the method for reinforcing existing building beams of the present invention can be further improved as follows:

[0015] The specific steps of determining the drilling location, inserting prestressed tendons after drilling, pouring reinforced concrete, and accelerating the solidification of the reinforced concrete by infrared irradiation include:

[0016] The first step is to determine the arrangement direction and quantity of the prestressing tendons based on the main and auxiliary stress points of the existing building beams.

[0017] The second step is to drill a hole at an angle at the auxiliary stress point, and continue drilling along the straight line between the drilling position and the main stress point, so that the length of the drilling hole passes through and extends out of the main stress point and the auxiliary stress point.

[0018] The third step is to insert the prestressed tendons into the borehole and tension them to the designed prestress value;

[0019] The fourth step is to pour reinforced concrete into the borehole and compact it thoroughly.

[0020] The fifth step is to evenly arrange infrared radiators above the reinforced concrete surface to irradiate the surface and accelerate the solidification of the reinforced concrete.

[0021] The specific steps of uniformly arranging infrared radiators above the reinforced concrete surface to irradiate the surface and accelerate the solidification of the reinforced concrete include:

[0022] The first step is to smooth the surface of the reinforced concrete at the drilled position where it contacts the existing building beams.

[0023] The second step is to evenly arrange the infrared radiators above the surface of the existing building beams filled with the reinforced concrete, at a distance of about 20-30cm from the concrete surface.

[0024] The third step is to turn on the infrared radiator to start heating the reinforced concrete surface and continue heating for 12-24 hours.

[0025] The fourth step is to use a thermometer to monitor the temperature of the reinforced concrete surface and maintain the temperature of the reinforced concrete surface at 40-60℃.

[0026] Fifth, after heating is complete, continue curing the reinforced concrete to ensure its strength and durability;

[0027] After the heating process is completed, the specific steps for continuing to cure the reinforced concrete to ensure its strength and durability include:

[0028] The first step is to maintain the concrete at the target temperature specified in the heating curve for the specified holding time after heating is completed.

[0029] The second step is to cool the concrete slowly and in a controlled manner after the insulation period ends, at a rate of 15-30°C per hour.

[0030] The third step, during the cooling process, involves keeping the concrete surface moist by spraying water, covering it with damp cloths, or using plastic film to prevent moisture evaporation and cracking.

[0031] Furthermore, the specific steps for determining the arrangement direction and quantity of the prestressing tendons based on the main and auxiliary stress points of the existing building beams include:

[0032] The prestressing tendons are arranged in the direction of the line connecting the main stress point and the auxiliary stress point; the number of prestressing tendons is equal to the number of auxiliary stress points.

[0033] The specific steps of drilling an oblique hole at the auxiliary stress point, and continuously drilling along the straight line between the drilling position and the main stress point, such that the length of the drilling hole passes through and extends to both the main stress point and the auxiliary stress point, include:

[0034] The first step is to drill a hole at a defined angle and depth, with the inner diameter of the hole being larger than the outer diameter of the prestressing tendon.

[0035] The second step is to use compressed air to remove dust and debris from the drill hole;

[0036] The third step is to insert the prestressed steel bars into the drilled hole and ensure that they extend to the main stress point and extend to a certain length.

[0037] The fourth step is to use anchorages to anchor the prestressed steel bars in the borehole.

[0038] Furthermore, the specific steps of pouring reinforced concrete into the borehole and compacting it include:

[0039] The first step is to mix the concrete according to the specified ratio and then pump it into the borehole, controlling the pouring speed and volume to ensure the quality of the pouring.

[0040] The second step is to eliminate air bubbles in the reinforced concrete.

[0041] The third step is to fix the sealing baffle.

[0042] The specific steps for eliminating air bubbles in the reinforced concrete include:

[0043] The first step is to aim the UV lamp at the surface of the reinforced concrete filling the borehole along the drilling direction;

[0044] The second step is to turn on the ultraviolet lamp after shielding the area, so that the light shines into the interior of the reinforced concrete along the drilling direction to eliminate air bubbles.

[0045] Furthermore, the specific steps of scanning the surface of the existing building beams with an infrared radiation meter to determine the internal cracks of the existing building beams, and then welding the internal cracks of the existing building beams with a laser beam, include:

[0046] The first step is to scan the surface of the existing building beams with an infrared radiation meter to determine the extent of cracks inside the beams.

[0047] The second step is to determine the location and length of the cracks that need to be welded based on the scanning results.

[0048] The third step is to use laser beam welding equipment to weld the cracks inside the beam that need to be welded.

[0049] The fourth step is to cool the welded area after welding to prevent thermal stress from forming.

[0050] The specific steps for using laser beam welding equipment to weld cracks inside the beam include:

[0051] The first step is to determine the direction and path of welding based on the location of the crack;

[0052] The second step is to preheat the welding area before the actual welding.

[0053] The third step is to weld the crack using a laser beam welding device after preheating.

[0054] The fourth step is to inspect the welding quality after welding is completed.

[0055] Furthermore, the specific steps for treating the surface of the existing building beams to reinforce them include:

[0056] The first step is to use a vacuum cleaner to clean the surface of the beams, removing dust, debris, and loose carbonized material.

[0057] The second step is to use an electric sander and coarse sandpaper to sand the surface of the existing building beams along the extension direction to remove the carbonized material on the surface.

[0058] The third step is to remove the carbonized material from the surface of the existing building beams using hydrofluoric acid to produce glass.

[0059] The fourth step is to gradually use finer sandpaper to polish the surface as the carbonized material is removed, in order to obtain a smoother surface.

[0060] The fifth step is to apply anti-rust paint to extend the service life of the existing building beams.

[0061] Furthermore, the specific steps for inserting the prestressing tendons into the borehole and tensioning them to the designed prestress value include:

[0062] The first step is to insert one end of the prestressed tendon into the anchoring device and then pass it through the drill hole;

[0063] The second step is to fix the anchoring device to one end of the borehole and connect the jack to the other end of the prestressing tendon.

[0064] The third step is to slowly and evenly pump the jack oil to tension the prestressed tendons;

[0065] The fourth step is to use a pressure gauge to monitor the tension of the prestressing tendons to ensure that the design prestress value is reached;

[0066] Fifth, once the design prestress value is reached, maintain the tension for a period of time to allow the prestressing tendons to stabilize.

[0067] Step 6: Use wedges to fix the prestressed tendons to the anchoring device;

[0068] Step 7: Slowly release the jack to release the tension.

[0069] Furthermore, the specific steps for adding temporary supports to the existing building beams by supporting and replacing the bottom supports are as follows:

[0070] The first step is to inspect the condition of the existing beams to determine the areas that need support and the type of support required.

[0071] The second step is to place jacks at the bottom of the beam where support is needed, ensuring that the jacks are placed on a solid surface and perpendicular to the beam.

[0072] The third step is to place shims between the jack and the beam to distribute the load and protect the beam surface.

[0073] The fourth step is to slowly and evenly pump the jacks to lift the roof beams;

[0074] Fifth step, place the timber at the bottom of the roof beam, parallel to the roof beam;

[0075] The sixth step is to wedge the support tightly to the bottom of the beam with wedges to provide additional support;

[0076] Step 7: Secure the support to the roof beam using bolts;

[0077] Step 8: Slowly and evenly release the jacks to transfer the weight of the roof beam to the temporary supports.

[0078] Furthermore, the specific steps by which the construction personnel determine the dimensions and deformation of the existing building beams by comparing them with the construction drawings using laser technology include:

[0079] The first step is to set up the measuring equipment on site according to the location of the roof beams on the construction drawings, including determining the location, height and angle of the measuring points, as well as the lines connecting the measuring equipment;

[0080] The second step is to calibrate the measuring equipment, including calibrating it using a standard reference surface or reference object, and performing multiple measurements and calculating the average value.

[0081] The third step is to align the calibrated measuring equipment with the roof beam, perform multiple measurements, and record the coordinates, elevation, and angle information of each measuring point.

[0082] The fourth step is to process the measured data, including calculating the dimensions and deformation of the beams.

[0083] The fifth step is to compare the completed measurement results with the construction drawings.

[0084] Furthermore, the specific steps for determining the main and auxiliary stress points of the existing building beams by estimating the loads on the beams and correlating this with changes in the beams' dimensions, the direction, angle, and size of deformation and bending include:

[0085] The first step is to determine the dead load and live load information of the existing building beams by examining the structures that are in direct and indirect contact with them, and to determine the direction of the load.

[0086] The second step is for construction workers to estimate the load based on the structural information.

[0087] The third step is to construct a stress analysis diagram based on the dimensions and deformation of the existing building beams, as well as the direction and magnitude of the loads, to determine the maximum stress point of the existing building beams. The location of the maximum stress point is the main stress point of the existing building beams.

[0088] The fourth step is to construct a stress analysis diagram based on the dimensions and deformation of the existing building beams, as well as the direction and magnitude of the loads, to determine the locations of stress points in the existing building beams that are less than the maximum stress point, and to select the five points with the greatest stress among these locations as auxiliary stress points.

[0089] Compared with existing technologies, the beneficial effects of the reinforcement method for existing building beams provided by this invention are as follows: Temporary support is added to the existing building beams by supporting and replacing the bottom of the beams; construction personnel determine the dimensions and deformation of the existing building beams by comparing them with construction drawings using laser; the main and auxiliary stress points of the existing building beams are determined by estimating the load on the beams and corresponding it with changes in the beams' dimensions, the direction, angle, and size of deformation and bending; drilling locations are determined, prestressed tendons are inserted after drilling, and reinforced concrete is poured in; the solidification of the reinforced concrete is accelerated by infrared irradiation; the surface of the existing building beams is scanned using an infrared radiation instrument to determine the internal cracks, and the internal cracks are welded using a laser beam; the surface of the existing building beams is treated to complete the reinforcement; this method solves the problem that existing methods for reinforcing existing building beams cannot completely eliminate potential cracks and deformations in the beams, resulting in certain safety hazards during use and a weakening of the reinforcement effect over time. Attached Figure Description

[0090] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the description of the embodiments of the present invention will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0091] Figure 1 This is a flowchart illustrating the operation of a method for reinforcing the beams of an existing building. Detailed Implementation

[0092] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings.

[0093] like Figure 1 The diagram shows an operation flowchart of a method for reinforcing existing building beams provided by this invention. The method includes the following steps:

[0094] S10: Replace the bottom support of the existing building beams to add temporary support to the existing building beams;

[0095] S20: Construction workers use lasers to compare with construction drawings to determine the dimensions and deformation of existing building beams;

[0096] S30: By estimating the load on the existing building beams and corresponding it with the changes in the dimensions of the existing building beams, the direction, angle and size of the deformation and bending, the main stress points and auxiliary stress points of the existing building beams are determined.

[0097] S40: Determine the drilling location, insert prestressed tendons after drilling, and then pour in reinforced concrete. Use infrared irradiation to accelerate the solidification of the reinforced concrete.

[0098] S50: The surface of the existing building beams is scanned by an infrared radiation meter to determine the internal cracks of the existing building beams, and the internal cracks of the existing building beams are welded by a laser beam.

[0099] S60: To treat the surface of existing building beams and reinforce them.

[0100] During use, temporary supports are added to the bottom of the existing building beams. Construction workers use lasers to compare with construction drawings to determine the dimensions and deformation of the existing building beams. By estimating the load on the existing beams and correlating it with changes in dimensions, the direction, angle, and size of deformation and bending, the main and auxiliary stress points of the existing building beams are determined. Drilling locations are determined, prestressed tendons are inserted after drilling, and reinforced concrete is poured in. Infrared irradiation accelerates the solidification of the reinforced concrete. An infrared radiation instrument scans the surface of the existing building beams to identify internal cracks, which are then welded using a laser beam. Finally, the surface of the existing building beams is treated to complete the reinforcement.

[0101] In the above technical solution, the specific steps of determining the drilling location, inserting prestressed tendons after drilling, pouring reinforced concrete, and accelerating the solidification of the reinforced concrete by infrared irradiation include:

[0102] The first step is to determine the arrangement direction and quantity of prestressing tendons based on the main and auxiliary stress points of the existing building beams;

[0103] The second step is to drill a hole at an angle at the auxiliary stress point, and continue drilling along the straight line between the drilling position and the main stress point, so that the length of the drilling hole passes through and extends to the main stress point and the auxiliary stress point.

[0104] The third step is to insert the prestressed tendons into the borehole and tension them to the designed prestress value;

[0105] The fourth step is to pour reinforced concrete into the borehole and compact it thoroughly.

[0106] The fifth step is to evenly arrange infrared radiators above the reinforced concrete surface to irradiate the surface and accelerate the solidification of the reinforced concrete.

[0107] The specific steps for uniformly arranging infrared radiators above the reinforced concrete surface to irradiate the surface and accelerate the solidification of the reinforced concrete include:

[0108] The first step is to smooth the surface of the drilled holes where the reinforced concrete meets the existing building beams.

[0109] The second step is to evenly place the infrared radiators above the surface of the existing building beam filled with reinforced concrete, about 20-30cm away from the concrete surface.

[0110] The third step is to turn on the infrared radiator to start heating the reinforced concrete surface and continue heating for 12-24 hours.

[0111] The fourth step is to use a thermometer to monitor the temperature of the reinforced concrete surface and maintain the temperature of the reinforced concrete surface at 40-60℃.

[0112] Fifth, after heating is complete, continue curing the reinforced concrete to ensure its strength and durability;

[0113] After heating, the specific steps for continuing to cure the reinforced concrete to ensure its strength and durability include:

[0114] The first step is to maintain the concrete at the target temperature specified in the heating curve for the specified holding time after heating is completed.

[0115] The second step is to cool the concrete slowly and in a controlled manner after the insulation period ends, at a rate of 15-30°C per hour.

[0116] The third step, during the cooling process, involves keeping the concrete surface moist by spraying water, covering it with damp cloths, or using plastic film to prevent moisture evaporation and cracking.

[0117] Furthermore, in the above technical solution, the specific steps for determining the arrangement direction and quantity of prestressing tendons based on the main and auxiliary stress points of the existing building beams include:

[0118] The direction of the prestressing tendons is the direction of the line connecting the main stress points and the auxiliary stress points; the number of prestressing tendons is the number of auxiliary stress points.

[0119] The specific steps for drilling at an angle at the auxiliary stress point, and continuing to drill along the straight line between the drill hole and the main stress point, so that the length of the drill hole passes through and extends to both the main stress point and the auxiliary stress point, include:

[0120] The first step is to drill holes at a defined angle and depth, with the inner diameter of the holes being larger than the outer diameter of the prestressing tendons.

[0121] The second step is to use compressed air to remove dust and debris from the drill hole;

[0122] The third step is to insert the prestressed steel bars into the drilled hole and ensure that they extend to the main stress point and extend to a certain length.

[0123] The fourth step is to use anchorages to anchor the prestressed steel bars in the borehole.

[0124] Furthermore, in the above technical solution, the specific steps for pouring reinforced concrete into the borehole and compacting it include:

[0125] The first step is to mix the concrete according to the specified ratio and then pump it into the borehole, controlling the pouring speed and volume to ensure the quality of the pouring.

[0126] The second step is to eliminate air bubbles in the reinforced concrete.

[0127] The third step is to fix the sealing baffle.

[0128] The specific steps for eliminating air bubbles in reinforced concrete include:

[0129] The first step is to aim the UV lamp at the surface of the reinforced concrete filling the borehole along the drilling direction;

[0130] The second step is to turn on the ultraviolet lamp after shielding the area, so that the light shines into the interior of the reinforced concrete along the drilling direction to eliminate air bubbles.

[0131] Furthermore, in the above technical solution, the specific steps of scanning the surface of the existing building beams with an infrared radiation meter to determine the internal cracks of the existing building beams, and welding the internal cracks of the existing building beams with a laser beam include:

[0132] The first step is to scan the surface of the existing building beams with an infrared radiation meter to determine the extent of cracks inside the beams.

[0133] The second step is to determine the location and length of the cracks that need to be welded based on the scanning results.

[0134] The third step is to use laser beam welding equipment to weld the cracks inside the beam that need to be welded.

[0135] The fourth step is to cool the welded area after welding to prevent thermal stress from forming.

[0136] The specific steps for welding inside a beam using laser beam welding equipment include:

[0137] The first step is to determine the direction and path of welding based on the location of the crack;

[0138] The second step is to preheat the welding area before the actual welding.

[0139] The third step is to weld the crack using a laser beam welding device after preheating.

[0140] The fourth step is to inspect the welding quality after welding is completed.

[0141] Furthermore, in the above technical solution, the specific steps for treating the surface of the existing building beams to reinforce them include:

[0142] The first step is to use a vacuum cleaner to clean the surface of the beams, removing dust, debris, and loose carbonized material.

[0143] The second step is to use an electric sander and coarse sandpaper to sand the surface of the existing building beams along the extension direction to remove the carbonized material on the surface.

[0144] The third step involves removing the carbonized material from the surface of existing building beams using hydrofluoric acid to produce glass.

[0145] The fourth step is to gradually use finer sandpaper to polish the surface as the carbonized material is removed, in order to obtain a smoother surface.

[0146] The fifth step is to apply anti-rust paint to extend the service life of existing building beams.

[0147] Furthermore, in the above technical solution, the specific steps for inserting the prestressing tendons into the borehole and tensioning them to the designed prestress value include:

[0148] The first step is to insert one end of the prestressed tendon into the anchoring device and then pass it through the drill hole;

[0149] The second step is to fix the anchoring device to one end of the borehole and connect the jack to the other end of the prestressing tendon.

[0150] The third step is to slowly and evenly pump the jack oil to tension the prestressed tendons;

[0151] The fourth step is to use a pressure gauge to monitor the tension of the prestressing tendons to ensure that the design prestress value is reached;

[0152] Fifth, once the design prestress value is reached, maintain the tension for a period of time to allow the prestressing tendons to stabilize.

[0153] Step 6: Use wedges to fix the prestressed tendons to the anchoring device;

[0154] Step 7: Slowly release the jack to release the tension.

[0155] Furthermore, in the above technical solution, the specific steps for providing temporary support to the existing building beams are added, specifically regarding the bottom support replacement of the existing building beams:

[0156] The first step is to inspect the condition of the existing beams to determine the areas that need support and the type of support required.

[0157] The second step is to place jacks at the bottom of the beam where support is needed, ensuring that the jacks are placed on a solid surface and perpendicular to the beam.

[0158] The third step is to place shims between the jack and the beam to distribute the load and protect the beam surface.

[0159] The fourth step is to slowly and evenly pump the jacks to lift the roof beams;

[0160] Fifth step, place the timber at the bottom of the roof beam, parallel to the roof beam;

[0161] The sixth step is to wedge the support tightly to the bottom of the beam with wedges to provide additional support;

[0162] Step 7: Secure the support to the roof beam using bolts;

[0163] Step 8: Slowly and evenly release the jacks to transfer the weight of the roof beam to the temporary supports.

[0164] Furthermore, in the above technical solution, the specific steps by which construction workers determine the dimensions and deformation of existing building beams by comparing them with construction drawings using lasers include:

[0165] The first step is to set up the measuring equipment on site according to the location of the roof beams on the construction drawings, including determining the location, height and angle of the measuring points, as well as the lines connecting the measuring equipment;

[0166] The second step is to calibrate the measuring equipment, including calibrating it using a standard reference surface or reference object, and performing multiple measurements and calculating the average value.

[0167] The third step is to align the calibrated measuring equipment with the roof beam, perform multiple measurements, and record the coordinates, elevation, and angle information of each measuring point.

[0168] The fourth step is to process the measured data, including calculating the dimensions and deformation of the beams.

[0169] The fifth step is to compare the completed measurement results with the construction drawings.

[0170] Furthermore, in the above technical solution, the specific steps for determining the main and auxiliary stress points of the existing building beams by estimating the loads on them and corresponding them with the changes in the dimensions, deformation, bending direction, angle, and size of the existing building beams include:

[0171] The first step is to determine the dead load and live load information of the existing building beams by examining the structures that are in direct and indirect contact with them, and to determine the direction of the load.

[0172] The second step is for construction workers to estimate the load based on the structural information.

[0173] The third step is to construct a stress analysis diagram based on the dimensions, deformation, load direction, and magnitude of the existing building beams, and determine the maximum stress point of the existing building beams. The location of the maximum stress point is the main stress point of the existing building beams.

[0174] The fourth step is to construct a stress analysis diagram based on the dimensions, deformation, load direction, and magnitude of the existing building beams, determine the locations of stress points in the existing building beams that are less than the maximum stress point, and select the five points with the greatest stress among these locations as auxiliary stress points.

[0175] Example 1:

[0176] The existing building beams are supported and temporarily supported at their base. Construction workers use laser pointers to compare with construction drawings to determine the dimensions and deformation of the existing beams. By estimating the load on the existing beams and correlating this with changes in dimensions, the direction, angle, and size of deformation and bending, the main and auxiliary stress points are identified. Based on these points, the arrangement direction and quantity of prestressing tendons are determined. Holes are drilled obliquely at the auxiliary stress points, continuing along the straight line between the auxiliary and main stress points, extending the borehole length to both the main and auxiliary stress points. Prestressing tendons are inserted into the boreholes and tensioned to the design prestress value. Reinforced concrete is then poured. Soil was poured into the borehole and compacted. Reinforced concrete was then filled into the existing building beam, and the surface of the borehole was leveled. Infrared radiators were evenly positioned above the reinforced concrete filling area of ​​the existing building beam, approximately 20 cm away from the concrete surface. The infrared radiators were turned on to heat the reinforced concrete surface for 12 hours. The temperature of the reinforced concrete surface was monitored using a thermometer and maintained at 40°C. After heating, the concrete was kept at the target temperature specified in the heating curve for the prescribed holding time. After the holding period, the concrete was cooled slowly and in a controlled manner at a rate of 15°C per hour. During cooling, the concrete surface was kept moist by spraying water, covering with damp cloths, and using plastic film to prevent moisture evaporation and cracking. The surface of the existing building beam was scanned using an infrared radiator to determine the internal cracks. These cracks were then welded using a laser beam. The surface of the existing building beam was then treated to complete the reinforcement of the existing building beam.

[0177] Example 2:

[0178] The existing building beams are supported and temporarily supported at their base. Construction workers use laser pointers to compare with construction drawings to determine the dimensions and deformation of the existing beams. By estimating the load on the existing beams and correlating this with changes in dimensions, the direction, angle, and size of deformation and bending, the main and auxiliary stress points are identified. Based on these points, the arrangement direction and quantity of prestressing tendons are determined. Holes are drilled obliquely at the auxiliary stress points, continuing along the straight line between the auxiliary and main stress points, extending the borehole length to both the main and auxiliary stress points. Prestressing tendons are inserted into the boreholes and tensioned to the design prestress value. Reinforced concrete is then poured. Soil was poured into the borehole and compacted. Reinforced concrete was then filled into the existing building beam, and the surface of the borehole was leveled. Infrared radiators were evenly positioned above the reinforced concrete filling area of ​​the existing building beam, approximately 30 cm away from the concrete surface. The infrared radiators were turned on to heat the reinforced concrete surface for 24 hours. The temperature of the reinforced concrete surface was monitored using a thermometer and maintained at 60°C. After heating, the concrete was kept at the target temperature specified in the heating curve for the prescribed holding time. After the holding period, the concrete was cooled slowly and in a controlled manner at a rate of 30°C per hour. During cooling, the concrete surface was kept moist by spraying water, covering with damp cloths, and using plastic film to prevent moisture evaporation and cracking. The surface of the existing building beam was scanned using an infrared radiator to determine the internal cracks. These cracks were then welded using a laser beam. The surface of the existing building beam was then treated to complete the reinforcement of the existing building beam.

[0179] Specifically, the principle of this invention is as follows: A temporary support is added to the bottom of the existing building beams; construction workers determine the dimensions and deformation of the existing building beams by comparing them with construction drawings using laser; the load on the existing building beams is estimated and correlated with changes in dimensions, the direction, angle, and size of deformation and bending to determine the main and auxiliary stress points; drilling locations are determined, prestressed tendons are inserted after drilling, and reinforced concrete is poured in; infrared irradiation accelerates the solidification of the reinforced concrete; the surface of the existing building beams is scanned using an infrared radiation instrument to determine the internal cracks, and laser beams are used to weld these cracks; the surface of the existing building beams is treated to complete the reinforcement of the existing building beams.

Claims

1. A method for reinforcing existing building beams, characterized in that, Includes the following steps: S10: Replace the bottom support of the existing building beams to add temporary support to the existing building beams; S20: Construction workers use lasers to compare with construction drawings to determine the dimensions and deformation of the existing building beams; S30: By estimating the load on the existing building beams and corresponding it with the changes in the dimensions of the existing building beams, the direction, angle and size of the deformation and bending, the main stress points and auxiliary stress points of the existing building beams are determined. S40: Determine the drilling location, insert prestressed tendons after drilling, and then pour in reinforced concrete. Accelerate the solidification of the reinforced concrete by infrared irradiation. S50: Scan the surface of the existing building beams with an infrared radiation meter to determine the internal cracks of the existing building beams, and weld the internal cracks of the existing building beams with a laser beam. S60: The surface of the existing building beams is treated to complete the reinforcement of the existing building beams; The specific steps of determining the drilling location, inserting prestressed tendons after drilling, pouring reinforced concrete, and accelerating the solidification of the reinforced concrete by infrared irradiation include: The first step is to determine the arrangement direction and quantity of the prestressing tendons based on the main and auxiliary stress points of the existing building beams. The second step is to drill a hole at an angle at the auxiliary stress point, and continue drilling along the straight line between the drilling position and the main stress point, so that the length of the drilling hole passes through and extends out of the main stress point and the auxiliary stress point. The third step is to insert the prestressed tendons into the borehole and tension them to the designed prestress value; The fourth step is to pour reinforced concrete into the borehole and compact it thoroughly. The fifth step is to evenly arrange infrared radiators above the reinforced concrete surface to irradiate the surface and accelerate the solidification of the reinforced concrete. The specific steps of uniformly arranging infrared radiators above the reinforced concrete surface to irradiate the surface and accelerate the solidification of the reinforced concrete include: The first step is to smooth the surface of the reinforced concrete at the drilled position where it contacts the existing building beams. The second step is to evenly arrange the infrared radiators above the surface of the existing building beams filled with the reinforced concrete, at a distance of about 20-30cm from the concrete surface. The third step is to turn on the infrared radiator to start heating the reinforced concrete surface and continue heating for 12-24 hours. The fourth step is to use a thermometer to monitor the temperature of the reinforced concrete surface and maintain the temperature of the reinforced concrete surface at 40-60℃. Fifth, after heating is complete, continue curing the reinforced concrete to ensure its strength and durability; The specific steps for estimating the load on the existing building beams and corresponding it with the changes in the dimensions, direction, angle, and size of the deformation and bending of the existing building beams to determine the main and auxiliary stress points of the existing building beams include: The first step is to determine the dead load and live load information of the existing building beams by examining the structures that are in direct and indirect contact with them, and to determine the direction of the load. The second step is for construction workers to estimate the load based on the structural information. The third step is to construct a stress analysis diagram based on the dimensions and deformation of the existing building beams, as well as the direction and magnitude of the loads, to determine the maximum stress point of the existing building beams. The location of the maximum stress point is the main stress point of the existing building beams. The fourth step is to construct a stress analysis diagram based on the dimensions and deformation of the existing building beams, as well as the direction and magnitude of the loads, to determine the locations of stress points in the existing building beams that are less than the maximum stress point, and to select the five points with the greatest stress among these locations as auxiliary stress points.

2. The method for reinforcing existing building beams according to claim 1, characterized in that, After the heating process is completed, the specific steps for continuing to cure the reinforced concrete to ensure its strength and durability include: The first step is to maintain the concrete at the target temperature specified in the heating curve for the specified holding time after heating is completed. The second step is to cool the concrete slowly and in a controlled manner after the insulation period ends, at a rate of 15-30°C per hour. The third step, during the cooling process, involves keeping the concrete surface moist by spraying water, covering it with damp cloths, or using plastic film to prevent moisture evaporation and cracking.

3. The method for reinforcing existing building beams according to claim 2, characterized in that, The specific steps for determining the arrangement direction and quantity of the prestressing tendons based on the main and auxiliary stress points of the existing building beams include: The prestressing tendons are arranged in the direction of the line connecting the main stress point and the auxiliary stress point; the number of prestressing tendons is equal to the number of auxiliary stress points. The specific steps of drilling a hole obliquely at the auxiliary stress point, and continuously drilling along the straight line between the drilling position and the main stress point, so that the length of the drilling hole passes through and extends to the main stress point and the auxiliary stress point, include: The first step is to drill a hole at a defined angle and depth, with the inner diameter of the hole being larger than the outer diameter of the prestressing tendon. The second step is to use compressed air to remove dust and debris from the drill hole; The third step is to insert the prestressed steel bars into the drilled hole and ensure that they extend to the main stress point and extend to a certain length. The fourth step is to use anchorages to anchor the prestressed steel bars in the borehole.

4. The method for reinforcing existing building beams according to claim 3, characterized in that, The specific steps for pouring reinforced concrete into the borehole and compacting it include: The first step is to mix the concrete according to the specified ratio and then pump it into the borehole, controlling the pouring speed and volume to ensure the quality of the pouring. The second step is to eliminate air bubbles in the reinforced concrete. The third step is to fix the sealing baffle. The specific steps for eliminating air bubbles in the reinforced concrete include: The first step is to aim the UV lamp at the surface of the reinforced concrete filling the borehole along the drilling direction; The second step is to turn on the ultraviolet lamp after shielding the area, so that the light shines into the interior of the reinforced concrete along the drilling direction to eliminate air bubbles.

5. A method for reinforcing existing building beams according to claim 4, characterized in that, The specific steps of scanning the surface of the existing building beams with an infrared radiation meter to determine the internal cracks of the existing building beams, and then welding the internal cracks of the existing building beams with a laser beam include: The first step is to scan the surface of the existing building beams with an infrared radiation meter to determine the extent of cracks inside the beams. The second step is to determine the location and length of the cracks that need to be welded based on the scanning results. The third step is to use laser beam welding equipment to weld the cracks inside the beam that need to be welded. The fourth step is to cool the welded area after welding to prevent thermal stress from forming. The specific steps for using laser beam welding equipment to weld cracks inside the beam include: The first step is to determine the direction and path of welding based on the location of the crack; The second step is to preheat the welding area before the actual welding. The third step is to weld the crack using a laser beam welding device after preheating. The fourth step is to inspect the welding quality after welding is completed.

6. The method for reinforcing existing building beams according to claim 5, characterized in that, The specific steps for treating the surface of the existing building beams to reinforce them include: The first step is to use a vacuum cleaner to clean the surface of the beams, removing dust, debris, and loose carbonized material. The second step is to use an electric sander and coarse sandpaper to sand the surface of the existing building beams along the extension direction to remove the carbonized material on the surface. The third step is to remove the carbonized material from the surface of the existing building beams using hydrofluoric acid to produce glass. The fourth step is to gradually use finer sandpaper to polish the surface as the carbonized material is removed, in order to obtain a smoother surface. The fifth step is to apply anti-rust paint to extend the service life of the existing building beams.

7. A method for reinforcing existing building beams according to claim 6, characterized in that, The specific steps for inserting the prestressing tendons into the borehole and tensioning them to the designed prestress value include: The first step is to insert one end of the prestressed tendon into the anchoring device and then pass it through the drill hole; The second step is to fix the anchoring device to one end of the borehole and connect the jack to the other end of the prestressing tendon. The third step is to slowly and evenly pump the jack oil to tension the prestressed tendons; The fourth step is to use a pressure gauge to monitor the tension of the prestressing tendons to ensure that the design prestress value is reached; Fifth, once the design prestress value is reached, maintain the tension for a period of time to allow the prestressing tendons to stabilize. Step 6: Use wedges to fix the prestressed tendons to the anchoring device; Step 7: Slowly release the jack to release the tension.

8. A method for reinforcing existing building beams according to claim 7, characterized in that, The specific steps for adding temporary supports to the existing building beams by supporting and replacing the bottom supports are as follows: The first step is to inspect the condition of the existing beams to determine the areas that need support and the type of support required. The second step is to place jacks at the bottom of the beam where support is needed, ensuring that the jacks are placed on a solid surface and perpendicular to the beam. The third step is to place shims between the jack and the beam to distribute the load and protect the beam surface. The fourth step is to slowly and evenly pump the jacks to lift the roof beams; Fifth step, place the timber at the bottom of the roof beam, parallel to the roof beam; The sixth step is to wedge the support tightly to the bottom of the beam with wedges to provide additional support; Step 7: Secure the support to the roof beam using bolts; Step 8: Slowly and evenly release the jacks to transfer the weight of the roof beam to the temporary supports.

9. A method for reinforcing existing building beams according to claim 8, characterized in that, The specific steps by which construction workers determine the dimensions and deformation of the existing building beams by comparing them with construction drawings using lasers include: The first step is to set up the measuring equipment on site according to the location of the roof beams on the construction drawings, including determining the location, height and angle of the measuring points, as well as the lines connecting the measuring equipment; The second step is to calibrate the measuring equipment, including calibrating it using a standard reference surface or reference object, and performing multiple measurements and calculating the average value. The third step is to align the calibrated measuring equipment with the roof beam, perform multiple measurements, and record the coordinates, elevation, and angle information of each measuring point. The fourth step is to process the measured data, including calculating the dimensions and deformation of the beams. The fifth step is to compare the completed measurement results with the construction drawings.

Citation Information

Patent Citations

  • Prestressed reinforced concrete beam transforming and reinforcing method

    CN113622703A

  • Rapid maintenance and reinforcement method for stand column type concrete structure

    CN117144820A