A method for calculating the diffusion rate of warm mix synchronously recycled SBS modified asphalt mixture system
Through the diffusion rate calculation formula based on free volume theory, the problem of difficult to accurately predict the diffusion rate and fusion degree in the warm-mixed synchronous regeneration SBS modified asphalt mixing system is solved, and accurate prediction is achieved, ensuring the service performance and anti-slip of the regenerated road surface performance.
Patent Information
- Application Number
- CN202410394052.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-02
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-04-02
AI Technical Summary
The prior art is difficult to accurately predict the diffusion rate and degree of fusion in the warm-mixed synchronous regeneration SBS modified asphalt mixing system, resulting in cracking, peeling, high-temperature rutting, packing, slipping and other diseases during the construction process of the regenerated road surface, which affects it. Service performance.
Based on the free volume theory, the diffusion rate calculation formula of warm-mixed SBS modified asphalt in synchronous regenerated SBS modified asphalt was proposed. Combined with the structural composition and viscosity-temperature characteristics of warm-mixed SBS modified asphalt and synchronous regenerated SBS modified asphalt, the structure composition and viscosity-temperature characteristics of the warm-mixed SBS modified asphalt were combined. Calculate parameters to accurately predict diffusion rate and behavior, reducing errors in routine experiments and numerical simulation calculations.
Accurately predict the diffusion rate at different doping volumes and temperatures, reduce errors, ensure the service performance of regenerative pavement, avoid the occurrence of diseases, and improve the anti-slip performance of the pavement.
Smart Images

Figure CN118230848B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of road engineering, and in particular to a method for calculating the diffusion rate of a warm-mix synchronously regenerated SBS modified asphalt mixing system. Background Art
[0002] Since the unique three-dimensional cross-linked network molecular structure of styrene-butadiene-styrene polymer block molecular chain (SBS) can significantly improve the high temperature performance, low temperature performance, fatigue resistance and temperature sensitivity of the base asphalt itself, SBS modified asphalt is the most widely used modified asphalt product in the current road engineering field. Since the beginning of the 21st century, this high-performance SBS modified asphalt has been widely used in the upper and middle layers of asphalt pavements of my country's highways and urban trunk roads. However, with the increasing proportion of heavy traffic loads and the increase in service life, most of the SBS modified asphalt pavements built in the early days have entered the stage of major and medium repairs. According to statistics, my country produces more than 4 million tons of waste SBS modified asphalt mixtures each year. If it cannot be reasonably recycled, it will cause serious problems such as land occupation and waste of resources.
[0003] In order to achieve efficient recycling of waste SBS modified asphalt mixtures, a variety of two-component regeneration agents have been proposed to simultaneously restore the properties of the SBS polymer component and the matrix asphalt component in aged SBS modified asphalt. For example, CN113817329A discloses a two-component aged SBS modified asphalt regeneration agent composed of epoxidized soybean oil and epoxidized polybutadiene resin, wherein the epoxidized soybean oil is used as a component regulator to restore the colloidal structure balance of the aged matrix asphalt, and the epoxidized polybutadiene resin is used as an SBS molecular chain repair agent to reconnect the aged and broken SBS polymers and restore their three-dimensional cross-linked network structure; CN 104231640A discloses a two-component regeneration agent, including a component regulator composed of heavy oil and catalytic cracking oil slurry and an SBS molecular chain repair agent composed of 1,4-butanediol diglycidyl ether; CN 113583457A discloses a two-component regeneration agent in which the component regulator is aromatic oil and the SBS molecular chain repair agent is mainly diisocyanate and diepoxy substances; in addition, CN 114874635 discloses a two-component regeneration agent in which the component regulator is aromatic oil and the SBS molecular chain repair agent is mainly diisocyanate and diepoxy substances; in addition, CN 114874635 discloses a two-component regeneration agent in which the component regulator is aromatic oil and the SBS molecular chain repair agent is mainly diisocyanate and diepoxy substances. A discloses a two-component regeneration agent, which uses any one or a combination of thiocyanuric acid, genipin, triallyl isocyanurate, and 1-ethyl-(3-dimethylaminopropyl) carbodiimide as an SBS molecular chain repair agent; and any one or a combination of cashew nut shell oil, waste engine oil, waste vegetable oil, and epoxidized soybean oil as a component regulator, and further adds a warm mix agent. The addition of the warm mix agent has been proven to significantly improve the utilization rate of waste SBS modified asphalt mixture by reducing the construction temperature and inhibiting secondary aging.
[0004] The above studies provide a variety of two-component rejuvenators for aged SBS modified asphalt, and confirm that these rejuvenators can greatly restore the original performance of aged SBS modified asphalt. However, in the actual construction process, the degree of fusion (DOB) between the diffusion-controlled synchronously regenerated SBS modified asphalt and the warm-mix SBS modified asphalt is the key to determining the service performance of the regenerated pavement. On the one hand, an overestimated DOB value makes the total asphalt content of the regenerated mixture lower than the actual optimal asphalt content, thereby inducing cracking, peeling and other diseases in the regenerated pavement. On the other hand, an overestimated DOB value leads to an excessive total asphalt content in the regenerated mixture, causing high-temperature rutting, lumping, slippage and other diseases in the regenerated pavement, and causing problems such as reduced anti-skid performance of the pavement. In order to ensure the long-term service performance of the warm-mix synchronously regenerated SBS modified asphalt mixture, it is necessary to clarify the diffusion rate of the two, so as to accurately determine the DOB value. Summary of the invention
[0005] In order to address the deficiencies in the prior art, the present invention provides a method for calculating the diffusion rate of a warm-mix synchronously recycled SBS modified asphalt mixture system, which can accurately predict the diffusion rate and diffusion behavior of warm-mix SBS modified asphalt in synchronously recycled SBS modified asphalt at different dosages and temperatures, greatly reducing the inherent errors caused by conventional experiments and numerical simulation calculations.
[0006] To achieve the above object, the present invention provides the following technical solution: a method for calculating the diffusion rate of a warm-mix synchronously regenerated SBS modified asphalt mixture system, and a diffusion rate calculation formula for warm-mix SBS modified asphalt when diffusing in synchronously regenerated SBS modified asphalt based on the free volume theory, as shown in the following formula:
[0007]
[0008] In formula (1), D 1 is the diffusion rate of warm mix SBS modified asphalt, cm 2 / s;D 01 is the pre-exponential factor, cm 2 / s; R is the gas constant; T is the diffusion temperature, K; ξ is the ratio of the critical molar hole free volume required for the migration of warm-mix SBS modified asphalt to the critical molar hole free volume required for the migration of synchronously regenerated SBS modified asphalt jumping units; E * is the critical energy required for warm mix SBS modified asphalt to overcome the attraction of adjacent molecules, cal / mol; and are the critical pore free volumes required for migration of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt, cm 3 / g;w 1 The range of values is 0 to 1, w 2 The range of values is 1-w 1, where w 1 and w 2 They represent the mass fractions of warm-mixed SBS modified asphalt and synchronously recycled SBS modified asphalt in the mixed system respectively; γ is the overlap factor of the mixed system, and its value is between 0.5 and 1, indicating that the same void free volume space can be used for the migration of different motion units; is the average free volume of the mixture system after diffusion, cm 3 / g;
[0009] In formula (1) It represents the dependence of the diffusion process on the free volume, indicating that the free volume of warm-mix SBS modified asphalt and synchronously recycled SBS modified asphalt is evenly distributed in the mixed system, and the value is additive, which can be further expressed as the following formula:
[0010]
[0011] In formula (2), and is the void free volume of warm-mix SBS modified asphalt and synchronously recycled SBS modified asphalt during diffusion, cm 3 / g;
[0012] When the temperature of the mixed system is higher than its glass transition temperature, it can be further expressed as follows:
[0013]
[0014] In formula (3), K 11 , K 21 is the free volume parameter of warm mix SBS modified asphalt, the unit is cm 3 / g·K,K;K 12 , K 22 are the free volume parameters of synchronously regenerated SBS modified asphalt, in cm 3 / g·K,K;T g1 、T g2 are the glass transition temperatures of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt, K;
[0015] Based on equations (1) to (3), the diffusion rate calculation formula of warm mix SBS modified asphalt in synchronously recycled SBS modified asphalt can be further rewritten as follows:
[0016]
[0017] Preferably, and They are respectively equal to the occupied volumes of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt at absolute zero 0K, and are calculated through group contribution.
[0018] Preferably, and K 21 -T g1 , and K 22 -T g2 It is calculated by fitting the Williams-Landel-Ferry viscosity-temperature equation of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt; where T g1 and T g2 It was tested by differential scanning calorimetry.
[0019] Preferably, D 01 By analogy with the diffusion rate of pure solvent molecules, it is solved as shown in the following formula:
[0020]
[0021] In formula (5), d 1 is the density of warm mix SBS modified asphalt at temperature T, g / cm 3 ; is the critical molar volume of warm mix SBS modified asphalt, cm 3 / mol, which is equal to the standard molar volume of the gas R is the gas constant; M 1 is the molar mass of warm mix SBS modified asphalt, g / mol; η 1 is the viscosity of warm mix SBS modified asphalt at temperature T, g / cm·s.
[0022] Preferably, ξ is calculated by the following formula:
[0023]
[0024] In formula (6), z is a characteristic parameter of the polymer material, which is usually 0.1, and e=2.718.
[0025] Preferably, E * It is calculated by the Arrhenius equation which describes the relationship between the viscosity and flow activation energy of warm mix SBS modified asphalt.
[0026] The present invention provides a method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system, which has the following beneficial effects compared with the prior art:
[0027] The present invention proposes a method for calculating the diffusion rate of a warm-mix synchronously recycled SBS modified asphalt mixture system, proposes a diffusion rate calculation equation based on the free volume theory, and solves the parameters in the calculation equation by combining the structural composition of warm-mix SBS modified asphalt and synchronously recycled SBS modified asphalt and their viscosity-temperature characteristics. The method can accurately predict the diffusion rate and diffusion behavior of warm-mix SBS modified asphalt in synchronously recycled SBS modified asphalt at different dosages and temperatures, thereby greatly reducing the inherent errors caused by conventional experiments and numerical simulation calculations. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0029] Figure 1 It is a schematic diagram of the main curves of shear modulus and phase angle of warm mix SBS modified asphalt and synchronously regenerated SBS modified asphalt of the present invention;
[0030] Figure 2 It is a schematic diagram of viscosity-temperature curve fitting of warm mix SBS modified asphalt of the present invention;
[0031] Figure 3 This is a schematic diagram of the Arrhenius equation fitting of the viscosity-temperature curve of the warm mix SBS modified asphalt of the present invention;
[0032] Figure 4 This is a graph showing the relationship between the diffusion rate of the warm-mix SBS modified asphalt of the present invention and its dosage;
[0033] Figure 5 It is a relationship diagram between the diffusion rate and the diffusion temperature of the warm mix SBS modified asphalt of the present invention;
[0034] Figure 6 This is a graph showing the relationship between the diffusion rate of the synchronously regenerated SBS modified asphalt and its dosage;
[0035] Figure 7 This is a graph showing the relationship between the diffusion rate and the diffusion temperature of the synchronously regenerated SBS modified asphalt of the present invention. DETAILED DESCRIPTION
[0036] The following examples are used to explain the implementation methods of the present application in detail, so that the implementation process of how the present application uses technical means to solve technical problems and achieve technical effects can be fully understood and implemented accordingly.
[0037] Example 1
[0038] In this example, a linear SBS polymer with a polystyrene and polybutadiene block (S / B) ratio of 3:7 is used as a base asphalt modifier to obtain SBS modified asphalt. The molecular formula of the SBS polymer can be expressed as C 104 H 134 The amount is 5% of the base asphalt mass ratio. Warm mix SBS modified asphalt is made by further mixing SBS modified asphalt with warm mix agent Sasobit. The molecular formula of Sasobit can be expressed as C n H 2n+2 (n=65), and its dosage is 3% of the mass ratio of SBS modified asphalt. Synchronous regeneration SBS modified asphalt is an artificial aged asphalt prepared by rotating thin film oven aging (RTFO) + pressure aging vessel (PAV), and the product obtained by the joint repair of SBS molecular chain repair agent (triallyl isocyanurate) and base asphalt component regulator (aromatic oil). The molecular formulas of triallyl isocyanurate and aromatic oil are C 12 H 15 N 3 O 3 and C 30 H 40 The addition amounts are 3% and 5% of the mass ratio of aged SBS modified asphalt respectively.
[0039] In addition, in the mixed system, the warm-mix SBS modifier can be regarded as the diffusing substance, and the synchronously regenerated SBS modified asphalt can be regarded as the diffused substance.
[0040] A method for calculating the diffusion rate of a warm mix synchronously recycled SBS modified asphalt mixture system is provided. The parameter solving process of the calculation equation is as follows:
[0041] (1) Determine the critical void free volume of the warm-mix synchronously recycled SBS modified asphalt mixture system and The values are equal to the occupied volumes of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt at absolute zero 0K, respectively, and are calculated by group contribution. With reference to the asphalt chemical four-component test specified in the "Testing Procedures for Asphalt and Asphalt Mixtures for Highway Engineering" (JTG E20-2011), the distribution of the chemical four components (including saturated components, aromatic components, colloids and asphaltene) of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt is determined. At the same time, based on the molecular structure composition of the two asphalts and with reference to the molar volume parameters of different groups at 0K shown in Table 1, the molar volumes of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt at 0K are calculated, respectively, as shown in Tables 2 and 3 below.
[0042] Table 1 Molar volume parameters of different groups at 0K in the group contribution method
[0043]
[0044]
[0045] Table 2 Calculation results of molar volume of warm mix SBS modified asphalt
[0046]
[0047] Table 3 Calculation results of molar volume of synchronously regenerated SBS modified asphalt
[0048]
[0049]
[0050] Combining the contents of each component of warm-mix SBS modified asphalt and the molar volume of its average component at 0K in Tables 1 and 2, the critical void free volume of warm-mix SBS modified asphalt is Average component molar volume = single component molar volume × molecular number ratio, taking saturated components as an example, Single component molar volume = molecular group contribution volume / molecular weight. Taking Hopane molecule in saturated fraction as an example, the single component molar volume of Hopane molecule = (35×1.1+62×6.7+0.6×4+1.8) / 482 = 0.950cm 3 / g.
[0051] Similarly, referring to the calculation steps of the critical free volume of warm-mix SBS modified asphalt, the critical free volume of synchronously regenerated SBS modified asphalt is
[0052] (2) Determine the void free volume parameters of the warm mix synchronously recycled SBS modified asphalt mixture system and in, and K 21 , and K 22 Corresponds to the constant in the Williams-Landel-Ferry (WLF) viscosity-temperature equation for warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt, where K 21 =C 21 , K 22 =C 22 , (C 1i and C2i , i = 1 or 2 represents warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt respectively), glass transition temperature T g1 and T g2 It was tested by differential scanning calorimetry.
[0053] The dynamic rheological shear (DSR) frequency sweep test of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt was carried out. The test temperature was 10-70℃, the temperature gradient was 10℃, and the test frequency was 0.1-10Hz. After the frequency sweep test was completed, the test data was constrained by WLF equation movement and CAM model fitting to obtain the shear modulus and phase angle master curves of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt, such as Figure 1 As shown in Table 4 below, the corresponding master curve fitting parameters are shown in Table 4 below.
[0054] Table 4 Master curve fitting parameters of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt
[0055]
[0056] At the same time, the glass transition temperatures of the two asphalts were further tested. The test instrument used was DSC-2500, the test temperature was -50 to 50°C, the heating rate was 5°C / min, and the ventilation gas flow was nitrogen. The test results showed that the glass transition temperatures of warm-mixed SBS modified asphalt and synchronously recycled SBS modified asphalt were 2.13°C and 0.01°C, respectively.
[0057] Based on the master curve parameter fitting results of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt and the glass transition temperature test results, the calculation results of the void free volume parameters of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt are K 21 -T g =135.22-275.28=-140.06K and K 22 -T g2 =123.74-273.16=-149.42K.
[0058] (3) Solving the pre-exponential factor D of the warm mix synchronously recycled SBS modified asphalt mixture system 01 , analogous to the semi-empirical prediction equation for the diffusion rate of miscible solvent molecules When the amount of warm-mix SBS modified asphalt in the mixed system is w 1 =1, while synchronously regenerated SBS modified asphalt w 2 =0, formula (4) can be further rewritten as follows:
[0059]
[0060] When 1 →1, in the mixed system E * The effect on diffusion is small. 01 Therefore, combined with the semi-empirical prediction equation, equation (7) can be further rewritten as follows:
[0061]
[0062] After logarithmic processing on both sides, we can get the following formula:
[0063]
[0064] The density of warm mix SBS modified asphalt is d 1 =1.0341g / cm 3 , molar mass M 1 =506.50g / cm 3 Substituting into formula (9) we can get:
[0065]
[0066] By analogy fitting the viscosity-temperature curve of warm-mix SBS modified asphalt, the pre-exponential factor D of the warm-mix SBS modified asphalt of the mixed system can be obtained: 01 ,like Figure 2 As shown, the final calculated result is 0.00201cm 2 / s.
[0067] (4) Calculate the critical molar volume ratio ξ of the warm mix synchronously recycled SBS modified asphalt mixture system. According to formula (6), it can be calculated that the critical molar volume ratio ξ of the warm mix synchronously recycled SBS modified asphalt is 0.7091.
[0068] (5) Determine the diffusion energy parameter E of the warm mix synchronously recycled SBS modified asphalt mixture system * , which is calculated by the Arrhenius equation describing the relationship between the viscosity and flow activation energy of warm-mix SBS modified asphalt, as shown in the following formula:
[0069]
[0070] In formula (11), η 1 is the viscosity of warm mix SBS modified asphalt, mPa·s; A is the Arrhenius equation constant; R is the gas constant; E a is the activation energy of warm mix SBS modified asphalt, kJ / mol, equivalent to E * ; T is absolute temperature, K.
[0071] Taking the logarithm of both sides of formula (11) yields the following formula:
[0072]
[0073] The energy parameter E of the mixed system was determined by fitting the viscosity-temperature data of warm-mix SBS modified asphalt. * is 2041.94 cal / mol, such as Figure 3 shown.
[0074] Combined with the calculation results of the above parameters, it can be seen that when warm-mix SBS modified asphalt is used as the diffusion material, the diffusion rate calculation equation of the warm-mix synchronously recycled SBS modified asphalt mixed system is shown as follows:
[0075]
[0076] The diffusion rate of warm-mix SBS modified asphalt in the mixed system at different dosages and different diffusion temperatures can be calculated by formula (13), as follows: Figure 4 (diffusion temperature 413.15K) and Figure 5 (Warm mix SBS modified asphalt content: warm mix synchronously recycled SBS modified asphalt content = 0.5: 0.5). Figure 4 It can be seen that as the amount of warm-mix SBS modified asphalt in the mixed system increases, its diffusion rate decreases instead, which is obviously inconsistent with the diffusion behavior described in the conventional Fick's law, that is, diffusion always tends to proceed from the high-concentration side to the low-concentration side. As the content of warm-mix SBS modified asphalt increases, its diffusion rate should increase. The opposite change law in this embodiment can be attributed to the fact that it is not reasonable to simply use warm-mix SBS modified asphalt as a diffusion material. After synchronous regeneration, the two asphalts may complete fusion through mutual diffusion. In addition, Figure 5 It shows that with the increase of diffusion temperature, the diffusion of warm-mixed SBS modified asphalt in the mixed system increases rapidly. This is because the irregular movement of molecules accelerates as the temperature increases, making diffusion more likely to occur.
[0077] Example 2
[0078] In this embodiment, the warm mix SBS modified asphalt and synchronously regenerated SBS modified asphalt in Example 1 are still used. The difference compared with Example 1 is that the synchronously regenerated SBS modified asphalt in the mixed system is used as the diffusing substance, and the warm mix SBS modified asphalt is used as the diffused substance.
[0079] A method for calculating the diffusion rate of a warm mix synchronously recycled SBS modified asphalt mixture system is provided. The parameter solving process of the calculation equation is as follows:
[0080] (1) Determine the critical void free volume of the warm-mix synchronously recycled SBS modified asphalt mixture system and The solution process is the same as in Example 1. The critical free volume of the synchronously regenerated SBS modified asphalt is The final calculated result is 0.7919cm 3 / g, critical void free volume of warm mix SBS modified asphalt The final calculated result is 0.7422cm 3 / g.
[0081] (2) Determine the void free volume parameters of the warm mix synchronously recycled SBS modified asphalt mixture system and The solution process is the same as that in Example 1. The final calculated results of the free volumes of the cavities of the synchronously recycled SBS modified asphalt and the warm mix SBS modified asphalt are 2.6637×10 -4 cm 3 / g·K, -149.42K and 2.0639×10 -4 cm 3 / g·K, -140.06K.
[0082] (3) Solving the pre-exponential factor D of the warm mix synchronously recycled SBS modified asphalt mixture system 01 By analogy fitting the viscosity-temperature curve of synchronously regenerated SBS modified asphalt, the pre-exponential factor of synchronously regenerated SBS modified asphalt in the mixed system can be solved to be 0.000212 cm 2 / s.
[0083] (4) The critical molar volume ratio ξ of the warm-mix synchronously recycled SBS modified asphalt mixture system is calculated by the formula It can be calculated that the critical molar volume ratio ξ of warm mix synchronously recycled SBS modified asphalt is 0.728.
[0084] (5) Determine the diffusion energy parameter E of the warm mix synchronously recycled SBS modified asphalt mixture system * , calculated using the Arrhenius equation describing the relationship between the viscosity and flow activation energy of warm mix synchronously recycled SBS modified asphalt, it is 2189.48 cal / mol.
[0085] Combined with the calculation results of the above parameters, it can be seen that when synchronously regenerated SBS modified asphalt is used as the diffusion material, the diffusion rate calculation equation of the warm-mix synchronously regenerated SBS modified asphalt mixed system is shown as follows:
[0086]
[0087] The diffusion rate of synchronously regenerated SBS modified asphalt in the mixed system at different dosages and different diffusion temperatures can be calculated by formula (14), as follows: Figure 6(diffusion temperature 413.15K) and Figure 7 (Warm mix synchronously recycled SBS modified asphalt content: warm mix SBS modified asphalt content = 0.5: 0.5). Figure 6 It can be seen that with the increase of the synchronously regenerated SBS modified asphalt in the mixed system, its diffusion rate decreases instead, which also does not conform to the diffusion behavior described in the conventional Fick's law. Figure 4 The change in diffusion rate can further infer that after synchronous regeneration, the two asphalts can be fused through mutual diffusion, so the expected degree of fusion is high. In addition, Figure 7 It shows that with the increase of diffusion temperature, the diffusion of synchronously regenerated SBS modified asphalt in the mixed system increases rapidly. This is because the irregular movement of molecules accelerates with the increase of temperature, making diffusion easier to occur. Figure 5 The phenomenon is consistent with .
[0088] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system, characterized in that: Based on the free volume theory, a formula for calculating the diffusion rate of warm-mix SBS modified asphalt in synchronously recycled SBS modified asphalt is proposed, as shown below: In formula (1), D1 is the diffusion rate of warm-mix SBS modified asphalt, cm 2 / s;D 01 is the pre-exponential factor, cm 2 / s; R is the gas constant; T is the diffusion temperature, K; ξ is the ratio of the critical molar hole free volume required for the migration of warm-mix SBS modified asphalt to the critical molar hole free volume required for the migration of synchronously regenerated SBS modified asphalt jumping units; E * is the critical energy required for warm mix SBS modified asphalt to overcome the attraction of adjacent molecules, cal / mol; and are the critical pore free volumes required for migration of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt, cm 3 / g; the range of w1 is 0-1, and w2 can be expressed as 1-w1, where w1 and w2 represent the mass fractions of warm-mixed SBS modified asphalt and synchronously recycled SBS modified asphalt in the mixed system, respectively; γ is the overlap factor of the mixed system, and its value is between 0.5 and 1, indicating that the same free volume space of the cavity can be used for the migration of different motion units; is the average free volume of the mixture system after diffusion, cm 3 / g; In formula (1) It represents the dependence of the diffusion process on the free volume, indicating that the free volume of warm-mix SBS modified asphalt and synchronously recycled SBS modified asphalt is evenly distributed in the mixed system, and the value is additive, which can be further expressed as the following formula: In formula (2), and is the void free volume of warm-mix SBS modified asphalt and synchronously recycled SBS modified asphalt during diffusion, cm 3 / g; When the temperature of the mixed system is higher than its glass transition temperature, it can be further expressed as follows: In formula (3), K 11 , K 21 is the free volume parameter of warm mix SBS modified asphalt, the unit is cm 3 / g·K,K;K 12 , K 22 are the free volume parameters of synchronously regenerated SBS modified asphalt, in cm 3 / g·K,K;T g1 、T g2 are the glass transition temperatures of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt, K; Based on equations (1) to (3), the diffusion rate calculation formula of warm mix SBS modified asphalt in synchronously recycled SBS modified asphalt can be further rewritten as follows:
2. The method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system according to claim 1, characterized in that: and They are respectively equal to the occupied volumes of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt at absolute zero 0K, and are calculated through group contribution.
3. The method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system according to claim 1, characterized in that: and K 21 -T g1 , and K 22 -T g2 It is calculated by fitting the Williams-Landel-Ferry viscosity-temperature equation of warm mix SBS modified asphalt and synchronously recycled SBS modified asphalt; where T g1 and T g2 It was tested by differential scanning calorimetry.
4. The method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system according to claim 1, characterized in that: D 01 By analogy with the diffusion rate of pure solvent molecules, it is solved as shown in the following formula: In formula (5), d1 is the density of warm mix SBS modified asphalt at temperature T, g / cm 3 ; is the critical molar volume of warm mix SBS modified asphalt, cm 3 / mol, which is equal to the standard molar volume of the gas R is the gas constant; M1 is the molar mass of warm-mix SBS modified asphalt, g / mol; η1 is the viscosity of warm-mix SBS modified asphalt at temperature T, g / cm·s.
5. The method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system according to claim 1, characterized in that: ξ is calculated by the following formula: In formula (6), z is a characteristic parameter of the polymer material, which is taken as 0.1, and e=2.
718.
6. The method for calculating the diffusion rate of a warm mix synchronously regenerated SBS modified asphalt mixture system according to claim 1, characterized in that: E * It is calculated by the Arrhenius equation which describes the relationship between the viscosity and flow activation energy of warm mix SBS modified asphalt.