A design method for a four-axis cloth for blade root

Through the four-axis cloth design method, the yarn layer and surface weight of the blade root are optimized, which solves the problem of insufficient tensile performance of existing materials in ultra-large offshore blades, improves the strength and stability of the blade, and reduces material waste and Manufacturing costs.

CN118332733BActive Publication Date: 2024-10-11CHANGZHOU HONGFA ZONGHENG ADVANCED MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410507006.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-25
Publication Date
2024-10-11
Estimated Expiration
2044-04-25

AI Technical Summary

Technical Problem

The existing blade shell reinforcement layer material has insufficient tensile properties in the design of ultra-large offshore blades, leading to the risk of blade overweight and main engine overloading when strength is increased.

Method used

The four-axis cloth design method is used to obtain the force data of the blade root through numerical simulation and experimental testing, and the angle, weight and modulus of each layer of yarn are balancedly designed, especially the 90° low weight and high modulus fabric layer, optimized The yarn layer and surface weight ensure the mechanical properties of the blade root.

Benefits of technology

It improves the overall strength and stability of the blade root, meets the needs of different blade roots, reduces material waste and manufacturing costs, avoids over- or under-design, and enhances the reliability and durability of the blade.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004810611340000121
    Figure BDA0004810611340000121
  • Figure BDA0004810611340000131
    Figure BDA0004810611340000131
  • Figure FDA0005029506340000011
    Figure FDA0005029506340000011
Patent Text Reader

Abstract

The present invention belongs to the technical field of quad-axial cloth preparation, and specifically relates to a design method for a quad-axial cloth for a blade root, comprising the following steps: determining the angle of each layer of yarn of the quad-axial cloth; determining a mechanical performance index according to the mechanical performance requirements of the blade root; determining the category of each layer of yarn of the quad-axial cloth according to the range of the mechanical performance index; determining the initial surface weight in grams of each layer of yarn of the quad-axial cloth according to the category of each layer of yarn of the quad-axial cloth, and obtaining an initial design scheme of the quad-axial cloth; adjusting the surface weight in grams of each layer of yarn in the initial design scheme of the quad-axial cloth according to the mechanical performance index, and obtaining a final design scheme of the quad-axial cloth.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of four-axis cloth preparation, and in particular relates to a design method of a four-axis cloth for a blade root. Background Art

[0002] The development of offshore wind power requires the manufacture of supporting large blades. The current mainstream 4MW, 5MW, and 6MW models have gradually failed to meet market demand, and the requirements for blade length are also rising. Large offshore wind power blades have enough advantages, but also enough research difficulties: material selection, aerodynamic considerations, reliability of design structure, blade quality requirements, cost economic considerations, and even the selection of manufacturing sites and transportation issues for ultra-long blades, etc., are all pain points and difficulties that need to be comprehensively considered.

[0003] The blade shell reinforcement layer materials currently used in the industry, although they generally show good performance, have insufficient tensile properties for the design requirements of super-large offshore blades. Traditional methods such as increasing the layer or increasing the thickness of fiberglass can improve the strength of the blade, but also bring the risk of blade overweight and main engine overload.

[0004] As a special fiber cloth, quad-axial cloth is composed of two layers of bidirectional fibers with perpendicular polarization directions, and has higher tensile strength and modulus. This design enables the quad-axial cloth to better resist bidirectional forces and effectively disperse the stress at the root of the blade, thereby improving the overall strength and stability of the blade. How to design the quad-axial cloth accordingly according to different blade root requirements is currently a difficult problem to solve. Summary of the invention

[0005] The purpose of the present invention is to provide a design method for a quad-axial cloth for the root of a blade, and the stress conditions of the root of a blade under actual working conditions, including mechanical properties such as tension, compression, and torsion. Through numerical simulation or experimental testing, the force data of the root of the blade is obtained to provide a basis for the design of the quad-axial cloth, and the angle, gram weight, modulus, and yarn type of each layer are balanced. In particular, a low-gram weight and high-modulus fabric layer is used at 90°. This design method can effectively improve the performance in the 90° direction and ensure the mechanical properties of the root of the blade.

[0006] The above technical objectives of the present invention are achieved through the following technical solutions:

[0007] The present invention provides a method for designing a four-axis cloth for a blade root, comprising the following steps:

[0008] Determine the angle of each layer of yarn in the quad-axial cloth;

[0009] Determine the mechanical performance index according to the mechanical performance requirements of the blade root;

[0010] Determine the type of yarn in each layer of the quad-axial cloth according to the range of mechanical performance indicators;

[0011] Determine the initial surface weight of each layer of yarn of the quad-axial cloth according to the type of each layer of yarn of the quad-axial cloth, and obtain the initial design scheme of the quad-axial cloth;

[0012] The surface weight of each layer of yarn in the initial design of the quad-axial cloth is adjusted according to the mechanical performance index to obtain the final design of the quad-axial cloth.

[0013] Furthermore, the warp and weft yarn layers are arranged in sequence from top to bottom, the first layer is a warp yarn layer in the first angle direction; the second layer is a weft yarn layer at the second angle, the third layer is a warp yarn layer at the third angle, and the fourth layer is a weft yarn layer at the fourth angle. The first angle and the third angle are perpendicular to each other, and the second angle and the fourth angle are equally divided by the first angle yarn.

[0014] Furthermore, the first angle range is 0 to 90 degrees, and the second angle range is 30 to -60 degrees.

[0015] Furthermore, the mechanical performance index is determined according to the mechanical performance requirements of the blade root, including any one or more of tensile strength, compressive strength, bending stiffness or fatigue life.

[0016] Furthermore, the type of yarn of each layer of the quad-axial cloth is determined according to the range of the mechanical performance index, including: selecting the type of yarn that can meet the mechanical performance index according to the maximum and minimum values ​​of the mechanical performance index.

[0017] Furthermore, the initial surface weight of each layer of yarn of the quad-axial cloth is determined according to the category of each layer of yarn of the quad-axial cloth, including: the surface weight of each layer of yarn adopts the sensitive surface weight of the category of this layer of yarn.

[0018] Furthermore, the sensitivity surface weight interval is generated by clustering the point values ​​of historical data.

[0019] Furthermore, the surface weight of each layer of yarn in the initial design of the quad-axial fabric is adjusted according to the mechanical performance index, including:

[0020] According to the initial design plan of the quad-axial cloth, a quad-axial cloth sample is prepared;

[0021] Test the mechanical properties data of the four-axis cloth samples;

[0022] Adjust the surface weight according to the difference between the mechanical performance data and the mechanical performance indicators.

[0023] Further, the surface weight is adjusted according to the difference between the mechanical performance data and the mechanical performance index, including: dividing the mechanical performance index into a warp yarn layer mechanical performance index and a weft yarn layer mechanical performance index;

[0024] Adjust the surface weight of the warp yarn layer according to the difference between the mechanical property data of the warp yarn layer and the mechanical property index of the warp yarn layer;

[0025] The surface weight of the weft yarn layer is adjusted according to the difference between the mechanical property data of the weft yarn layer and the mechanical property index of the weft yarn layer.

[0026] Furthermore, the surface weight is adjusted according to the difference between the mechanical performance data and the mechanical performance index, including: if the mechanical performance data is less than the mechanical performance index, the surface weight is increased; if the mechanical performance data exceeds the mechanical performance index by 10%, the surface weight is reduced.

[0027] Furthermore, the basis for adjusting the surface weight is to test the surface weight, angle and tensile strength data of different yarn types, fit the curve, and determine the tensile strength that can be improved at different angles for every increase of 1 gram in weight based on the fitting curve.

[0028] Furthermore, for different types of yarns, their surface weight, angle and tensile strength data are tested, and a curve is fitted. Based on the fitted curve, it is determined how much the tensile strength can be increased by every 1 gram increase in weight at a certain angle. This data is used to adjust the surface weight according to the difference between the mechanical property data and the mechanical property indicators.

[0029] Furthermore, the mechanical performance indicators include: tensile strength and compressive strength.

[0030] Furthermore, the surface weight is adjusted according to the difference between the mechanical performance data and the mechanical performance index, and the surface weight is adjusted according to the following calculation formula:

[0031] Among them, ΔM is the difference between the mechanical property data and the mechanical property index, and M is the mechanical property index.

[0032] Furthermore, the types of yarn include TM+ yarn, ECT yarn, Twaron yarn, Technora yarn or Vectran yarn.

[0033] In summary, the present invention has the following beneficial effects:

[0034] The design method of the quad-axial cloth for the root of the blade provided by the present invention can realize the accurate design of the quad-axial cloth by determining the mechanical performance index according to the mechanical performance requirements of the root of the blade, and determining the type and angle of each layer of yarn of the quad-axial cloth according to these indexes, so as to ensure that it meets the actual mechanical performance requirements of the root of the blade. At the same time, the initial design scheme is determined according to the range of mechanical performance indexes and the type of each layer of yarn, and then the initial design scheme is adjusted according to actual requirements to obtain the final design scheme, and the quad-axial cloth can be customized according to specific conditions to optimize the structural performance of the root of the blade to the greatest extent. DETAILED DESCRIPTION

[0035] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined purpose of the invention, a design method for a four-axis cloth for a blade root proposed by the present invention, its specific implementation method, characteristics and effects are described in detail as follows.

[0036] The present specific implementation provides a method for designing a quad-axis cloth for a blade root, comprising the following steps:

[0037] S1. Determine the angle of each layer of yarn of the quad-axial cloth;

[0038] S2. Determine the mechanical performance index according to the mechanical performance requirements of the blade root;

[0039] S3. Determine the type of yarn of each layer of the quad-axial cloth according to the range of mechanical performance indicators;

[0040] S4, determining the initial surface weight of each layer of yarn of the quad-axial cloth according to the type of each layer of yarn of the quad-axial cloth, and obtaining an initial design scheme of the quad-axial cloth;

[0041] S5. According to the mechanical performance index, the surface weight of each layer of yarn in the initial design of the quad-axial cloth is adjusted to obtain the final design of the quad-axial cloth.

[0042] In some preferred specific embodiments, the warp and weft yarn layers are arranged in sequence from top to bottom, the first layer is a warp yarn layer at a first angle; the second layer is a weft yarn layer at a second angle, the third layer is a warp yarn layer at a third angle, and the fourth layer is a weft yarn layer at a fourth angle. The first angle and the third angle are perpendicular to each other, and the second angle and the fourth angle are equally divided by the first angle yarn. Specifically, if the first angle range is 0 to 90°, the second angle range is 30 to -60°.

[0043] The above method can make the blade have higher strength and stability in multiple directions by setting yarn layers in different directions. The fiber layers in different directions are staggered with each other, which can effectively offset the external stress and improve the overall structural strength of the blade. At the same time, setting longitudinal and transverse crossed yarn layers can improve the tensile performance of the blade. The perpendicular arrangement of the yarn layers can increase the tensile strength of the blade in different directions and improve the durability and reliability of the blade.

[0044] In some preferred embodiments, the mechanical performance indexes determined according to the mechanical performance requirements of the blade root include: any one or more of tensile strength, compressive strength, bending stiffness or fatigue life; preferably tensile strength and compressive strength. The above performance indexes can make the quad-axial cloth have excellent tensile properties and strength, and can improve the strength of the blade while realizing the lightweight design of the blade, reducing the dead weight of the blade and reducing the risk of overloading the wind turbine host.

[0045] In some preferred embodiments, the type of yarn of each layer of the quad-axial cloth is determined according to the range of mechanical performance indicators, including: selecting the type of yarn that can meet the mechanical performance indicators according to the maximum and minimum values ​​of the mechanical performance indicators. For example: when ECT yarn is selected in the first angle direction or the third angle direction, if the tensile strength required by the target is to be achieved, the surface weight in grams needs to be greatly increased. Therefore, when the tensile strength requirement in the first angle direction or the third angle direction is high, TM+ yarn or other yarn with higher tensile strength is selected.

[0046] In this specific embodiment, the initial surface weight of each layer of yarn of the quad-axial cloth is determined according to the category of each layer of yarn of the quad-axial cloth, including: the surface weight of each layer of yarn adopts the sensitive surface weight of the category of this layer of yarn.

[0047] Specifically, the sensitivity surface weight range of the yarn category is generated by clustering the point values ​​of the historical data. The specific operation steps are as follows:

[0048] S41. Collect data: collect yarn categories and corresponding tensile strength data.

[0049] S42. Data preprocessing: clean the data and process missing values ​​and outliers.

[0050] S43. Feature selection and conversion: Identify yarn type and tensile strength as key features affecting sensitivity surface weight.

[0051] S44. Cluster analysis: Cluster the data using a clustering algorithm to identify clusters of data points under different yarn categories and tensile strength conditions.

[0052] S45. Determine the sensitivity surface weight range: calculate the average or median of the sensitivity surface weight for each cluster, and determine the range.

[0053] S46, generating a corresponding sensitivity surface weight range according to the type of yarn and the tensile strength, and selecting the median in the weight range as the initial surface weight. In some preferred embodiments, adjusting the surface weight of each layer of yarn in the initial design of the quad-axial cloth according to the mechanical performance index includes:

[0054] S51, preparing a four-axis cloth sample according to the initial design plan of the four-axis cloth;

[0055] S52, test the mechanical properties data of the four-axis cloth sample;

[0056] S53. Adjust the surface weight in grams according to the difference between the mechanical property data and the mechanical property index.

[0057] The above method, by adjusting the surface weight of the four-axis cloth according to the mechanical performance data of the actual test, can ensure that the mechanical performance indicators of the blade can meet the design requirements, effectively improve the structural strength, stiffness and stability of the blade, and ensure that it has good performance during use. At the same time, according to the difference between the mechanical performance data and the mechanical performance indicators, the surface weight of the four-axis cloth is adjusted to optimize the structural design of the blade, improve the reliability, durability and safety of the blade, reduce the failure rate and maintenance cost, avoid over-design or under-design, maximize the use of material resources and reduce waste.

[0058] In some preferred embodiments, the surface weight is adjusted according to the difference between the mechanical property data and the mechanical property index, including:

[0059] S531, dividing the mechanical performance index into a warp yarn layer mechanical performance index and a weft yarn layer mechanical performance index;

[0060] S532, adjusting the surface weight of the warp yarn layer according to the difference between the mechanical property data of the warp yarn layer and the mechanical property index of the warp yarn layer;

[0061] S533. Adjust the surface weight of the weft yarn layer according to the difference between the mechanical property data of the weft yarn layer and the mechanical property index of the weft yarn layer.

[0062] The above method subdivides the mechanical performance index into the mechanical performance index of the warp yarn layer and the weft yarn layer. The warp yarn layer and the weft yarn layer play different roles in different directions of the blade, so the targeted adjustment of the surface weight in each direction can ensure that the mechanical properties of the blade in all directions can meet the design requirements; among them, the warp yarn layer usually plays the main role in the longitudinal load and tensile strength of the blade, so the surface weight of the warp yarn layer needs to be adjusted according to the mechanical performance index of the warp yarn layer.

[0063] In this specific embodiment, by increasing or decreasing the surface weight of the warp yarn layer, the tensile strength and stiffness of the blade in the longitudinal direction can be accurately controlled to ensure that it can withstand external loads such as wind; the weft yarn layer usually bears the main role of the lateral load and bending strength of the blade, so by adjusting the surface weight of the weft yarn layer according to the mechanical performance indicators of the weft yarn layer, the bending strength and stability of the blade in the lateral direction can be accurately controlled to ensure that it can remain stable in a complex airflow environment.

[0064] By fine-tuning the surface weight of the warp and weft yarn layers, the structural design of the blade can be optimized to the greatest extent possible so that it can meet the design requirements in all directions while avoiding unnecessary over-design or under-design. This method of fine-tuning can improve the performance and reliability of the blade, reduce material waste, and improve the controllability and predictability of engineering implementation.

[0065] Specifically, the surface weight is adjusted according to the difference between the mechanical performance data and the mechanical performance index, including: if the mechanical performance data is less than the mechanical performance index, the surface weight is increased; if the mechanical performance data exceeds the mechanical performance index by 10%, the surface weight is reduced; specifically, the surface weight is adjusted according to the following calculation formula: Among them, ΔM is the difference between the mechanical property data and the mechanical property index, and M is the mechanical property index.

[0066] Taking tensile strength as an example, if the sample prepared by the initial design of the quad-axial cloth is tested, the tensile strength of the warp yarn layer of the sample is N T , and the tensile strength index M T The difference between T , then according to Determine whether the sample prepared by the initial design of the four-axis cloth meets the target requirements. If not, according to the relationship between tensile strength and surface weight, according to ΔM T The value of is used to adjust the surface weight.

[0067] The specific adjustment plan can be to test the surface weight, angle and tensile strength data of different yarn categories, fit the curve, and determine how much MPa the tensile strength can be increased by each gram increase in weight at a certain angle based on the fitting curve. T The value of the surface weight is adjusted; for example, every increase of 1 gram can increase the tensile strength CMPa; according to the formula The calculation requires increasing or decreasing the P surface weight.

[0068] The above method tests different types of yarns and fits the relationship curve between surface weight, angle and tensile strength, so as to more accurately understand the influence of different parameters on tensile strength, greatly improve the design accuracy, and make the mechanical properties of the blade more in line with actual needs; among them, by determining the tensile strength that can be improved by each increase of 1 gram in weight based on the fitting curve, the surface weight of the yarn can be better adjusted during the design process, and by optimizing the surface weight of the yarn, the amount of material used can be minimized while ensuring the strength of the blade, thereby reducing the manufacturing cost of the blade and achieving the purpose of lightweighting.

[0069] In some embodiments, the type of yarn includes TM+ yarn, Twaron yarn, Technora yarn, or Vectran yarn.

[0070] Embodiment: A method for designing a four-axis cloth for a blade root comprises the following steps:

[0071] S1. Determine the angle of each layer of yarn of the quad-axial cloth, including: the warp and weft yarn layers arranged in sequence from top to bottom, the first layer is the warp yarn layer in the 0° direction; the second layer is the weft yarn layer in the +45° direction; the third layer is the warp yarn layer in the 90° direction; and the fourth layer is the weft yarn layer in the -45° direction.

[0072] S2. Determine the mechanical performance index according to the mechanical performance requirements of the blade root. The mechanical performance index is determined according to the blade root material performance test results and ANSYS simulation analysis (see Table 1).

[0073] Table 1. Mechanical properties

[0074] Mechanical properties T0 / MPa T90 / MPa C0 / MPa VNS / MPa Target value 750 300 550 150

[0075] S3. Determine the type of yarn in each layer of the quad-axial cloth according to the range of mechanical performance indicators; According to Table 1, the yarns in the 0° and 90° directions have higher requirements for tensile strength. Therefore, the warp and weft yarn layers of the quad-axial cloth are arranged in sequence from top to bottom. The first layer uses TM+ yarn; the second layer uses ECT yarn; the third layer uses TM+ yarn; and the fourth layer uses ECT yarn.

[0076] S4. Determine the sensitive surface weight of each layer of yarn of the quad-axial cloth according to the type of each layer of yarn of the quad-axial cloth, and obtain the initial design scheme of the quad-axial cloth, wherein the surface weight of each layer of yarn is shown in Table 2.

[0077] The specific method is:

[0078] S41. Collect data: collect yarn categories and corresponding tensile strength data.

[0079] S42. Data preprocessing: clean the data and process missing values ​​and outliers.

[0080] S43. Feature selection and conversion: Identify yarn type and tensile strength as key features affecting sensitivity surface weight.

[0081] S44. Cluster analysis: Cluster the data using a clustering algorithm to identify clusters of data points under different yarn categories and tensile strength conditions.

[0082] S45. Determine the sensitivity surface weight range: calculate the average or median of the sensitivity surface weight for each cluster, and determine the range.

[0083] S46. Generate a corresponding sensitivity surface weight range according to the type of yarn and the tensile strength, and select the median in the range as the initial surface weight.

[0084] Table 2. Initial design of the four-axis cloth

[0085] Yarn direction 0° +45° 90° -45° Yarn category TM+468GS ECT468GS TM+468GS ECT468GS <![CDATA[Yarn surface weight / g / cm 2 > 1039 200 250 200

[0086] S5. Adjust the surface weight of each layer of yarn in the initial design of the quad-axial fabric according to the mechanical performance index;

[0087] Specifically, the samples were formed according to the initial design of the initial four-axis cloth, and a full set of static performance tests were performed. The test results are shown in Table 3:

[0088] Table 3. Performance test results of the initial design of the four-axis cloth

[0089]

[0090] According to the table above, the 0° surface T0 strength is 127MPa higher than the target value, and the 90° surface T90 is 34MPa lower than the target value. According to the calculation formula: Among them, ΔM is the difference between the mechanical performance data and the mechanical performance index, and M is the mechanical performance index. It is necessary to reduce the surface weight of the 0° surface and increase the surface weight of the 90° surface.

[0091] For ECT yarn, in the 90° direction, the tensile strength can be increased by 30MPa for every 50g increase in surface weight, and in the 0° direction, the tensile strength can be increased by 40MPa for every 50g increase in surface weight; for TM+ yarn, in the 0° direction, the tensile strength can be increased by 34MPa for every 50g increase in surface weight, and in the 90° direction, the tensile strength can be increased by 44MPa for every 50g increase in surface weight.

[0092] According to the formula Calculation: The surface weight of the yarn in the 0° direction needs to be reduced by 94 g / cm 2 , the surface weight of the yarn in the 90° direction needs to be increased by 51g / cm 2 .

[0093] According to the difference between the measured value and the target value, the tensile strength in the 0° direction overflows compared with the target value, and the overflow rate is greater than 10%, and the tensile strength in the 90° direction is significantly lower than the target value. Therefore, the surface weight of the yarn in the 0° direction is reduced, the surface weight of the yarn in the 90° direction is increased, and the surface weights of the yarns in the other two directions remain unchanged, and the adjusted four-axis cloth design is obtained, as shown in Table 4.

[0094] Table 4. Adjusted four-axis cloth design

[0095] Yarn direction 0° +45° 90° -45° Yarn category TM+468GS ECT468GS TM+468GS ECT468GS <![CDATA[Yarn surface weight / g / cm 2 > 945 200 301 200

[0096] Samples were prepared according to the adjusted four-axis cloth design scheme and a full set of static performance tests were performed. The test results are shown in Table 5.

[0097] Table 5. Performance test results of the adjusted four-axis cloth design

[0098]

[0099] After comparison, it can be seen that the performance test results of the adjusted four-axis cloth design scheme have all met the target value requirements, thus obtaining the final four-axis cloth design scheme.

[0100] The above description is only a preferred embodiment of the present invention and does not constitute any form of limitation to the present invention. Although the present invention has been presented as a preferred embodiment as above, it is not intended to limit the present invention. Any technician familiar with the profession can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the scope of the technical solution of the present invention.

Claims

1. A design method for a four-axis cloth for a blade root, characterized in that: The steps include: Determine the angle of each layer of yarn in the quad-axial cloth; Determine the mechanical performance index according to the mechanical performance requirements of the blade root; Determine the type of yarn in each layer of the quad-axial cloth according to the range of mechanical performance indicators; Determine the initial surface weight of each layer of yarn of the quad-axial cloth according to the type of each layer of yarn of the quad-axial cloth, and obtain the initial design scheme of the quad-axial cloth; The surface weight of each layer of yarn in the initial design of the quad-axial cloth is adjusted according to the mechanical performance index to obtain the final design of the quad-axial cloth; The method of adjusting the surface weight of each layer of yarn in the initial design of the quad-axial fabric according to the mechanical performance index includes: According to the initial design scheme of the four-axis cloth, a four-axis cloth sample is prepared; Test the mechanical properties data of the four-axis fabric samples; Adjust the surface weight in grams according to the difference between the mechanical performance data and the mechanical performance index; The adjusting the surface weight in grams according to the difference between the mechanical performance data and the mechanical performance index includes: if the mechanical performance data is less than the mechanical performance index, increasing the surface weight in grams; if the mechanical performance data exceeds the mechanical performance index by 10%, reducing the surface weight in grams; The surface weight is adjusted according to the difference between the mechanical performance data and the mechanical performance index, and the surface weight is adjusted according to the following calculation formula: Among them, △M is the difference between the mechanical property data and the mechanical property index, and M is the mechanical property index; The basis for adjusting the surface weight is to test the surface weight, angle and tensile strength data of different yarn types, fit the curve, and determine the tensile strength that can be improved at different angles for every increase of 1 gram in weight based on the fitting curve.

2. The design method of a quad-axis cloth for blade root according to claim 1, characterized in that: The method for determining the angle of each layer of yarn of the quad-axial cloth includes: warp and weft yarn layers arranged in sequence from top to bottom, the first layer is a warp yarn layer at a first angle; the second layer is a weft yarn layer at a second angle, the third layer is a warp yarn layer at a third angle, and the fourth layer is a weft yarn layer at a fourth angle, the first angle and the third angle are perpendicular to each other, and the second angle and the fourth angle are equally divided by the yarn at the first angle.

3. The design method of a quad-axis cloth for a blade root according to claim 1, characterized in that: The mechanical performance index includes: any one or more of tensile strength, compressive strength, bending stiffness or fatigue life.

4. The design method of a quad-axis cloth for a blade root according to claim 1, characterized in that: Determining the type of yarn of each layer of the quad-axial cloth according to the range of the mechanical performance index includes: selecting the type of yarn that can meet the mechanical performance index according to the maximum and minimum values ​​of the mechanical performance index.

5. The design method of a quad-axial cloth for blade root according to claim 1, characterized in that: Determining the initial surface weight of each layer of yarn of the quad-axial cloth according to the category of each layer of yarn of the quad-axial cloth includes: the surface weight of each layer of yarn adopts the sensitive surface weight of the category of this layer of yarn.

6. The design method of a quad-axis cloth for a blade root according to claim 1, characterized in that: The adjusting the surface weight in grams according to the difference between the mechanical performance data and the mechanical performance index comprises: dividing the mechanical performance index into a warp yarn layer mechanical performance index and a weft yarn layer mechanical performance index; Adjust the surface weight of the warp yarn layer according to the difference between the mechanical property data of the warp yarn layer and the mechanical property index of the warp yarn layer; The surface weight of the weft yarn layer is adjusted according to the difference between the mechanical property data of the weft yarn layer and the mechanical property index of the weft yarn layer.