A method for preparing a crystalline silicon battery electrode and a crystalline silicon battery structure
By preparing the barrier layer step by step in the crystalline silicon battery and accurately controlling the thickness of the sintered barrier layer, the problem of poor thickness control in the existing technology is solved, and the conductive efficiency of the metal electrode and the current extraction performance of the crystalline silicon battery are improved.
Patent Information
- Application Number
- CN202410743727.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-11
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-06-11
AI Technical Summary
The sintering process in the existing technology cannot accurately control the thickness of the barrier layer, resulting in a decrease in the conductive efficiency of the metal electrode and a reduction in the electrical conversion performance of the crystalline silicon battery.
Grooving is performed on the preset metal electrode area of the crystalline silicon battery preform, a first barrier layer of a first preset thickness is prepared and sintering is performed to form a sintered barrier layer, and then a second preset barrier layer is prepared on the surface of the sintered barrier layer The thickness of the second barrier layer ensures precise control of the total barrier layer thickness.
By preparing the barrier layer step by step and accurately controlling the thickness of the sintered barrier layer, the controllability of the barrier layer and the conductive efficiency of the metal electrode are improved, and the current extraction performance of the crystalline silicon photovoltaic cell is improved.
Smart Images

Figure CN118335848B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of photovoltaic cells, and in particular to a method for preparing a crystalline silicon cell electrode and a crystalline silicon cell structure. Background Art
[0002] In the prior art, metal electrodes are prepared in crystalline silicon photovoltaic cells. Before preparing the conductive layer, a barrier layer is prepared on the inner side of the conductive layer close to the crystalline silicon cell sheet, and a portion of the thickness of the barrier layer is sintered at high temperature to form an alloy barrier layer, which can reduce the contact resistance between the metal electrode and the crystalline silicon cell sheet, and at the same time prevent the metal in the conductive layer from diffusing to the inner side of the crystalline silicon cell, and increase the cell tension. However, the sintering process in the prior art cannot guarantee the precise control of the sintering thickness, so that the thickness formed by sintering is too large, which leads to a decrease in the conductive efficiency of the metal electrode and a decrease in the electrical conversion performance of the crystalline silicon cell.
[0003] Therefore, how to accurately control the sintering thickness when sintering the barrier layer using a sintering process is a technical problem that technical personnel in this field need to solve urgently. Summary of the invention
[0004] In view of this, the purpose of the present invention is to provide a method for preparing a crystalline silicon battery electrode and a crystalline silicon battery structure, which solves the problem in the prior art that the sintering process cannot ensure accurate control of the sintering thickness, resulting in a decrease in the conductive efficiency of the metal electrode.
[0005] In order to solve the above technical problems, the present invention provides a method for preparing a crystalline silicon battery electrode, comprising:
[0006] Providing a crystalline silicon cell prefabricated sheet without a metal electrode, and performing a groove process on a preset metal electrode area of the crystalline silicon cell prefabricated sheet to form a grooved area;
[0007] A first barrier layer of a first preset thickness is prepared in the grooved area, and the first barrier layer is sintered to obtain a sintered barrier layer; the first preset thickness is the thickness of a standard sintered barrier layer set according to the total thickness of the barrier layer;
[0008] Preparing a second barrier layer with a second preset thickness on the surface of the sintering barrier layer; the thickness of the second barrier layer is greater than the thickness of the sintering barrier layer;
[0009] A metal conductive layer is prepared on the surface of the second barrier layer to complete the preparation of the crystalline silicon battery electrode.
[0010] Optionally, a first barrier layer with a first preset thickness is prepared in the grooved area by using a chemical plating process.
[0011] Optionally, when the first barrier layer is sintered, the sintering temperature is 300 degrees Celsius to 700 degrees Celsius, and the sintering time is 30 seconds to 8 minutes.
[0012] Optionally, the second barrier layer is formed on the surface of the sintered barrier layer by chemical plating, electroplating or vapor deposition process;
[0013] A metal conductive layer is formed on the surface of the second barrier layer by using chemical plating, electroplating or vapor deposition process to complete the preparation of the crystalline silicon battery electrode.
[0014] Optionally, an anti-oxidation protective layer is formed on the surface of the metal conductive layer by chemical plating, electroplating or vapor deposition process.
[0015] Optionally, the crystalline silicon battery electrode forming the anti-oxidation protection layer is subjected to an annealing treatment; the temperature of the annealing treatment is lower than the temperature of the sintering treatment.
[0016] Optionally, a laser grooving process is used to perform grooving in a preset metal electrode region of the crystalline silicon cell prefabricated sheet, and a deoxidation treatment is performed on the grooved portion to form the grooved region.
[0017] Optionally, the grooved area is deoxidized by using a slow-release hydrofluoric acid process to form the grooved area.
[0018] A crystalline silicon battery structure, prepared by the above-mentioned crystalline silicon battery electrode preparation method, comprising:
[0019] Crystalline silicon cell prefabricated sheets and crystal silicon cell electrodes;
[0020] A grooved area is formed in the preset metal electrode area of the crystalline silicon cell prefabricated sheet;
[0021] The crystalline silicon battery electrode comprises a sintered barrier layer, a second barrier layer and a metal conductive layer which are sequentially arranged along the back of the crystalline silicon battery prefabricated sheet corresponding to the grooved area;
[0022] The thickness of the sintering barrier layer is smaller than the thickness of the second barrier layer.
[0023] Optionally, the sintering barrier layer is a nickel-silicon alloy barrier layer, and the second barrier layer is a nickel barrier layer;
[0024] The thickness of the nickel-silicon alloy barrier layer is 5 nanometers to 500 nanometers, and the total thickness of the nickel-silicon alloy barrier layer and the nickel barrier layer is greater than or equal to 200 nanometers.
[0025] It can be seen that the method for preparing crystalline silicon battery electrodes provided by the present invention provides a crystalline silicon battery prefabricated sheet without metal electrodes, performs a groove treatment on the preset metal electrode area of the crystalline silicon battery prefabricated sheet to form a grooved area, prepares a first barrier layer of a first preset thickness in the grooved area, and sinters the first barrier layer to obtain a sintered barrier layer. By controlling the value of the first preset thickness, the problem of accurately controlling the sintering process parameters is achieved by accurately controlling the deposition thickness of the first barrier layer. Subsequently, a second barrier layer is prepared on the surface of the sintered barrier layer. At this time, in the total barrier layer structure formed by the sintered barrier layer and the second barrier layer, the thickness of the sintered barrier layer can be accurately controlled to be the thickness of the set standard sintered barrier layer. While ensuring the preparation efficiency, the controllability of the thickness of the barrier layer after sintering is improved, thereby ensuring the current extraction efficiency of the crystalline silicon photovoltaic cell.
[0026] In addition, the present invention also provides a crystalline silicon battery structure prepared by the above-mentioned crystalline silicon battery electrode preparation method, which also has the above-mentioned beneficial effects. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.
[0028] Figure 1 A flow chart of a method for preparing a crystalline silicon battery electrode provided by an embodiment of the present invention;
[0029] Figure 2 A schematic diagram of a crystalline silicon cell structure provided by an embodiment of the present invention;
[0030] Figure 2 In the figure, the reference numerals are described as follows:
[0031] 10-crystalline silicon cell prefabricated sheet;
[0032] 21 - sintering barrier layer, 22 - second barrier layer, 23 - metal conductive layer, 24 - anti-oxidation protection layer. DETAILED DESCRIPTION
[0033] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0034] In the prior art, in the process of preparing metal electrodes in crystalline silicon photovoltaic cells, in order to prevent the prepared metal conductive layer from diffusing into the crystalline silicon cell prefabricated sheet in the crystalline silicon cell, a barrier layer is set between the metal conductive layer and the crystalline silicon cell prefabricated sheet, and in order to further improve the diffusion inhibition of the metal conductive layer by the barrier layer, a part of the thickness of the barrier layer is subjected to high-temperature sintering. However, if the thickness of the sintered barrier layer is too small, it will not be conducive to the diffusion inhibition of the metal conductive layer. If the thickness is too large, the resistivity of the metal electrode will be increased, thereby reducing the current extraction efficiency. Therefore, the thickness of the sintered barrier layer is precisely controlled, but the prior art cannot effectively achieve precise control of the sintered thickness while ensuring the preparation efficiency.
[0035] The present invention divides the barrier layer into a barrier layer that needs to be sintered and a barrier layer that does not need to be sintered according to its thickness, and prepares the barrier layer that needs to be sintered and the barrier layer that does not need to be sintered in steps. After the barrier layer that needs to be sintered is prepared, it is first sintered to obtain a sintered barrier layer, and then the barrier layer that does not need to be sintered is prepared on the surface of the sintered barrier layer. By utilizing the above-mentioned step-by-step preparation method, the thickness of the sintered barrier layer can be accurately controlled while ensuring the preparation efficiency.
[0036] Please refer to Figure 1 , Figure 1 A flow chart of a method for preparing a crystalline silicon battery electrode provided by an embodiment of the present invention. The method may include:
[0037] S101: providing a crystalline silicon cell prefabricated sheet without metal electrodes, and performing a groove process on a preset metal electrode area of the crystalline silicon cell prefabricated sheet to form a grooved area.
[0038] The execution subject of this embodiment is a crystalline silicon battery electrode preparation device. The crystalline silicon battery prefabricated sheet provided in this embodiment can be a conventional crystalline silicon battery prefabricated sheet without metal electrodes in existing crystalline silicon batteries, that is, the surface of the emitter and base formed in the corresponding crystalline silicon battery prefabricated sheet is provided with a grooved area obtained by groove processing, and the grooved area is the area corresponding to the subsequent metal electrode. It should be explained that in this embodiment, the surface of the preset metal electrode in the crystalline silicon battery prefabricated sheet is provided with a dielectric layer, and the groove processing is performed, that is, the dielectric layer corresponding to the preset metal electrode area in the crystalline silicon battery component to be grooved is removed to form the grooved area.
[0039] Furthermore, in order to improve the efficiency of the groove processing, the groove processing is performed on the preset metal electrode area of the crystalline silicon cell prefabricated sheet to form the groove area, which may include:
[0040] The laser grooving process is used to perform grooving processing on the preset metal electrode area of the crystalline silicon cell prefabricated sheet, and the grooving area is deoxidized to form the grooving area.
[0041] In this embodiment, the laser grooving process is used to remove the dielectric layer of the preset metal electrode area, which can increase the preparation rate, and there is no need to set a pre-step before laser irradiation, thereby improving the preparation efficiency. It should be further explained that in this embodiment, after the laser grooving process is used to perform grooving treatment and the grooving area is formed, oxidation will occur in the laser irradiation area, so it is necessary to perform deoxidation treatment on the laser irradiation area (i.e., the grooving area) to ensure the conductivity of the metal electrode. In this embodiment, the laser can be selected from one of the picosecond, femtosecond 266nm or 355nm lasers, or a combination of multiple lasers to achieve the above-mentioned dielectric layer removal.
[0042] Furthermore, in order to ensure the efficiency of the deoxidation treatment, a slow-release hydrofluoric acid process may be used to perform deoxidation treatment on the grooved area to form the grooved area.
[0043] It should be noted that in this embodiment, a slow-release hydrofluoric acid process is used to remove the oxide layer formed in the laser irradiation area. The slow-release hydrofluoric acid process controls the release rate of hydrofluoric acid by certain physical or chemical means, thereby achieving the purpose of extending the action time, reducing the frequency of use, and improving the effect, and can effectively remove the formed oxide layer. In the specific slow-release hydrofluoric acid process performed in this embodiment, the control parameters can be customized according to the needs.
[0044] S102: preparing a first barrier layer with a first preset thickness in the grooved area, and sintering the first barrier layer to obtain a sintered barrier layer.
[0045] In this embodiment, the first preset thickness is the thickness of the standard sintered barrier layer set according to the total thickness of the barrier layer. In this embodiment, a first barrier layer of a first preset thickness is first prepared on the surface of the electrode lead-out region, and the first preset thickness is set to the thickness of the standard sintered barrier layer set according to the total thickness of the barrier layer, that is, the first preset thickness is the thickness of the barrier layer that needs to be sintered. By controlling the thickness of the first barrier layer prepared by deposition, the thickness of the barrier layer that needs to be sintered in the total barrier layer is precisely controlled without changing the sintering process and ensuring the preparation efficiency. It should be further explained that the specific method of preparing the first barrier layer is not limited here, for example, it can be prepared by any method in the electroplating process, chemical plating process or deposition process, wherein the electroplating process can be prepared by light-induced electroplating, forward bias electroplating and other processes, and the deposition process can be prepared by physical vapor deposition process. This embodiment does not limit the specific material of the first barrier layer, as long as it can inhibit the diffusion of the outer metal conductive layer. For example, the material of the barrier layer can be selected from one or more of cobalt, nickel, zinc and bismuth.
[0046] Further, in order to improve the accuracy of the thickness of the sintered barrier layer, the above-mentioned preparation of the first barrier layer with a first preset thickness on the surface of the electrode lead-out region may include:
[0047] A first barrier layer with a first preset thickness is prepared in the grooved area by using a chemical plating process.
[0048] It should be noted that in this embodiment, the first barrier layer is prepared by chemical plating process. Since the chemical plating preparation rate is slow, the preparation can be completed more timely, which is convenient for controlling the thickness of the prepared first barrier layer, and further improving the accuracy of the thickness of the prepared sintered barrier layer. In actual preparation, this embodiment can further use a slow chemical plating process for preparation to further optimize the sintered barrier layer thickness preparation process.
[0049] Furthermore, in order to ensure that the sintering process is completed smoothly and the functionality of the barrier layer is ensured, the sintering process of the first barrier layer to obtain the sintered barrier layer may include:
[0050] The sintering temperature is set to 300 degrees Celsius to 700 degrees Celsius, the sintering time is set to 30 seconds to 8 minutes, and the nickel barrier layer is sintered in a nitrogen atmosphere to obtain a sintered barrier layer.
[0051] It should be noted that in this embodiment, the material of the barrier layer is set to nickel metal, and the nickel barrier layer is sintered using the above-mentioned specific preparation parameters, which can ensure the smooth preparation of the sintered barrier layer while ensuring the preparation cost and efficiency. In this embodiment, the sintering treatment time is set to between 30 seconds and 8 minutes, but because the first barrier layer prepared at this time is all a barrier layer that needs to be sintered, the sintering treatment time will not cause the barrier layer to fail due to reasons such as untimely treatment, thereby improving the fault tolerance of the preparation steps.
[0052] S103: preparing a second barrier layer with a second preset thickness on the surface of the sintering barrier layer; the thickness of the second barrier layer is greater than the thickness of the sintering barrier layer.
[0053] In this embodiment, after the first barrier layer is sintered to obtain the sintered barrier layer, a second barrier layer with a second preset thickness is prepared on the surface of the sintered barrier layer to achieve the preparation of the entire barrier layer. At this time, the sintered barrier layer and the second barrier layer together form the total barrier layer. Accordingly, this embodiment does not limit the specific method for preparing the second barrier layer. In order to ensure the preparation cost, the preparation method of the second barrier layer can be set to be the same as the preparation method of the first barrier layer.
[0054] S104: preparing a metal conductive layer on the surface of the second barrier layer to complete the preparation of the crystalline silicon battery electrode.
[0055] In this embodiment, a metal conductive layer is prepared on the surface of the prepared second barrier layer to complete the preparation of the crystalline silicon battery electrode. This embodiment also does not limit the preparation method of the above-mentioned metal conductive layer. The preparation methods of the metal conductive layer, the above-mentioned first barrier layer and the second barrier layer can also be set to be the same.
[0056] Furthermore, in order to ensure that the second barrier layer and the metal conductive layer are successfully prepared, the second barrier layer having a second preset thickness is prepared on the surface of the sintered barrier layer, which may include:
[0057] forming a second barrier layer on the surface of the sintered barrier layer by chemical plating, electroplating or vapor deposition process;
[0058] Accordingly, preparing a metal conductive layer on the surface of the second barrier layer to complete the preparation of the crystalline silicon battery electrode may include:
[0059] A metal conductive layer is formed on the surface of the second barrier layer by chemical plating, electroplating or vapor deposition process to complete the preparation of the crystalline silicon battery electrode.
[0060] It should be noted that, in this embodiment, the electroplating may include light-induced electroplating and forward bias electroplating, and the vapor deposition process may utilize a physical vapor deposition process.
[0061] Furthermore, in order to ensure that the metal conductive layer is not easily damaged by corrosion, after forming the metal conductive layer on the surface of the second barrier layer by chemical plating, electroplating or vapor deposition process, the method may further include:
[0062] An anti-oxidation protective layer is formed on the surface of the metal conductive layer by chemical plating, electroplating or vapor deposition process.
[0063] It should be noted that in this embodiment, an anti-oxidation protective layer is prepared on the surface of the metal conductive layer, which can protect the metal conductive layer. In this embodiment, electroplating can also include light-induced electroplating and forward bias electroplating, and the vapor deposition process can also be a physical vapor deposition process. To ensure the convenience of preparation, in this embodiment, the preparation processes of the anti-oxidation protective layer, the metal conductive layer, the second barrier layer, and the first barrier layer are all the same.
[0064] Furthermore, in order to ensure the structural stability of the metal electrode, after forming the anti-oxidation protective layer on the surface of the metal conductive layer by chemical plating, electroplating or vapor deposition process, the method may further include:
[0065] The crystalline silicon battery electrode with the anti-oxidation protection layer formed thereon is subjected to annealing treatment; the temperature of the annealing treatment is lower than the temperature of the sintering treatment.
[0066] In this embodiment, after the barrier layer, metal conductive layer and anti-oxidation protective layer are prepared, annealing treatment is uniformly performed to ensure the stability of the formed crystalline silicon battery electrode structure. It should be noted that in this embodiment, the annealing temperature can be set as low as possible to reduce the impact of the annealing treatment on the barrier layer.
[0067] The crystalline silicon battery electrode preparation method provided in the embodiment of the present invention is applied, by providing a crystalline silicon battery prefabricated sheet without metal electrodes, performing a groove processing on the preset metal electrode area of the crystalline silicon battery prefabricated sheet to form a grooved area, preparing a first barrier layer of a first preset thickness in the grooved area, and sintering the first barrier layer to obtain a sintered barrier layer. By controlling the value of the first preset thickness, the problem of accurately controlling the sintering process parameters is achieved by accurately controlling the deposition thickness of the first barrier layer. Subsequently, a second barrier layer is prepared on the surface of the sintered barrier layer. At this time, in the total barrier layer structure formed by the sintered barrier layer and the second barrier layer, the thickness of the sintered barrier layer can be accurately controlled to be the thickness of the set standard sintered barrier layer. While ensuring the preparation efficiency, the controllability of the thickness of the barrier layer after sintering is improved, thereby ensuring the current extraction efficiency of the crystalline silicon photovoltaic cell.
[0068] In addition, the embodiment of the present invention prepares the first barrier layer by utilizing a chemical plating process, thereby facilitating the control of the thickness of the prepared first barrier layer and further improving the accuracy of the thickness of the prepared sintered barrier layer; the material of the barrier layer is set to nickel metal, and the sintering treatment temperature is set to 300 degrees Celsius to 700 degrees Celsius, the sintering treatment time is 30 seconds to 8 minutes, and the nickel barrier layer is sintered in a nitrogen atmosphere, which can ensure the smooth preparation of the sintered barrier layer while ensuring the preparation cost and efficiency; an anti-oxidation protective layer is prepared on the surface of the metal conductive layer, which can protect the metal conductive layer; after the barrier layer, the metal conductive layer and the anti-oxidation protective layer are prepared, annealing treatment is performed uniformly, which can ensure the stability of the formed crystalline silicon battery electrode structure, and at the same time, the annealing treatment temperature is set lower than the sintering treatment temperature to reduce the influence of the annealing treatment on the barrier layer.
[0069] In a specific embodiment, taking TOPCon battery preparation as an example, the front material TOPCon blue film may include the following steps:
[0070] Step S1: providing a crystalline silicon cell prefabricated sheet without metal electrodes, and performing a groove process on a preset metal electrode area of the crystalline silicon cell prefabricated sheet to form a grooved area.
[0071] Step S2: Prepare a nickel barrier layer of a first preset thickness in the grooved area by using a chemical plating process, set the sintering temperature to 300 degrees Celsius to 700 degrees Celsius, and the sintering time to 30 seconds to 8 minutes. Sinter the nickel barrier layer in a nitrogen atmosphere to obtain a sintered barrier layer; the first preset thickness is the thickness of a standard sintered barrier layer set according to the total thickness of the barrier layer.
[0072] Step S4: forming a second barrier layer on the surface of the sintering barrier layer by chemical plating, electroplating or vapor deposition process; the thickness of the second barrier layer is greater than the thickness of the sintering barrier layer.
[0073] Step S5: forming a metal conductive layer on the surface of the second barrier layer by chemical plating, electroplating or vapor deposition process, thereby completing the preparation of the crystalline silicon battery electrode.
[0074] Step S6: forming an anti-oxidation protective layer on the surface of the metal conductive layer by using chemical plating, electroplating or vapor deposition process.
[0075] Step S7: annealing the crystalline silicon battery electrode with the anti-oxidation protection layer formed thereon; the temperature of the annealing treatment is lower than the temperature of the sintering treatment.
[0076] The crystalline silicon cell structure provided by the embodiment of the present invention is introduced below. The crystalline silicon cell structure described below is prepared by the above-mentioned crystalline silicon cell electrode preparation method, and can be referred to in correspondence with the crystalline silicon cell electrode preparation method described above.
[0077] Please refer to Figure 2 , Figure 2 A schematic structural diagram of a crystalline silicon cell structure provided in an embodiment of the present invention may include:
[0078] Crystalline silicon cell prefabricated sheet 10 and crystal silicon cell electrodes;
[0079] A grooved area is formed in the preset metal electrode area in the crystalline silicon cell prefabricated sheet 10;
[0080] The crystalline silicon cell electrode comprises a sintered barrier layer 21, a second barrier layer 22 and a metal conductive layer 23 which are sequentially arranged along the back of the crystalline silicon cell prefabricated sheet corresponding to the grooved area;
[0081] The thickness of the sintering barrier layer 21 is smaller than that of the second barrier layer 22 , and the thickness of the sintering barrier layer 21 is the thickness of a standard sintering barrier layer set according to the total thickness of the barrier layer.
[0082] It should be noted that in this embodiment, the sintered barrier layer 21 obtained by sintering treatment in the crystalline silicon battery electrode and the prepared second barrier layer 22 are prepared in steps, which can ensure the thickness of the sintered barrier layer 21 obtained during the sintering treatment and improve the accuracy of the thickness of the sintered barrier layer 21 prepared in the crystalline silicon battery electrode. It should be noted that the above-mentioned metal conductive layer 23 can be made of metal materials such as nickel, aluminum, copper, titanium, tungsten, etc., and the total thickness of the metal conductive layer 23 is not less than 3 microns. Furthermore, in this embodiment, an anti-oxidation protective layer 24 can be prepared on the outside of the metal conductive layer 23. The anti-oxidation protective layer 24 can be made of materials such as tin and silver, and the thickness is also not less than 3 microns.
[0083] Furthermore, in order to ensure the barrier layer's effect of inhibiting the diffusion of the metal conductive layer and to avoid the sintered barrier layer 21 being too thick to increase the electrode resistivity, the sintered barrier layer 21 may be a nickel-silicon alloy barrier layer, and the second barrier layer 22 may be a nickel barrier layer;
[0084] The thickness of the nickel-silicon alloy barrier layer is 5 nanometers to 500 nanometers, and the total thickness of the nickel-silicon alloy barrier layer and the nickel barrier layer is greater than or equal to 200 nanometers.
[0085] It should be noted that in this embodiment, the first barrier layer is set as a nickel barrier layer, and the first barrier layer is sintered to obtain the above-mentioned nickel-silicon alloy barrier layer as the sintered barrier layer 21. In this embodiment, the total thickness of the nickel-silicon alloy barrier layer and the nickel barrier layer is set to be greater than or equal to 200 nanometers, and the thickness of the nickel-silicon alloy barrier layer is set to 5 nanometers to 500 nanometers, which can improve the diffusion inhibition effect on the metal conductive layer 23, while reducing the contact resistance with the crystalline silicon battery prefabricated sheet 10, and at the same time avoid the nickel-silicon alloy barrier layer after the sintering process. The thickness is too large to affect the current extraction efficiency.
[0086] The crystalline silicon battery structure provided by the embodiment of the present invention is applied. The sintered barrier layer 21 to be obtained by sintering in the crystalline silicon battery electrode and the prepared second barrier layer 22 are prepared in steps. The barrier layer of the specified thickness is first prepared, and the sintered barrier layer 21 is obtained by sintering, and then the barrier layer of the remaining thickness is prepared. The accuracy of the thickness of the sintered barrier layer 21 obtained during the sintering process can be guaranteed, and the accuracy of the thickness of the sintered barrier layer 21 prepared in the crystalline silicon battery electrode can be improved. In addition, the embodiment of the present invention sets the sintered barrier layer 21 as a nickel-silicon alloy barrier layer, sets the second barrier layer 22 as a nickel barrier layer, and sets the total thickness of the nickel-silicon alloy barrier layer and the nickel barrier layer to be greater than or equal to 200 nanometers, and sets the thickness of the nickel-silicon alloy barrier layer to be 5 nanometers to 500 nanometers, which can improve the diffusion inhibition effect on the metal conductive layer 23, reduce the contact resistance with the crystalline silicon battery prefabricated sheet 10, and avoid the excessive thickness of the nickel-silicon alloy barrier layer after the sintering process to affect the current extraction efficiency.
[0087] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.
[0088] The professionals may further appreciate that the examples described in conjunction with the embodiments disclosed herein can be implemented with electronic hardware, computer software, or a combination of the two. In order to clearly illustrate the interchangeability of hardware and software, the composition and steps of each example have been generally described in terms of function in the above description. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professionals and technicians may use different methods to implement the described functions for each specific application, but such implementation should not be considered beyond the scope of the present invention.
[0089] Finally, it should be noted that, in this article, relationships such as first and second, etc. are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprises" or any other variations are intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0090] The above is a detailed introduction to a crystalline silicon battery electrode preparation method and a crystalline silicon battery structure provided by the present invention. Specific examples are used in this article to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea; at the same time, for general technical personnel in this field, according to the idea of the present invention, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.
Claims
1. A method for preparing a crystalline silicon battery electrode, characterized in that: include: Providing a crystalline silicon cell prefabricated sheet without a metal electrode, and performing a groove process on a preset metal electrode area of the crystalline silicon cell prefabricated sheet to form a grooved area; A first barrier layer of a first preset thickness is prepared in the grooved area, and the first barrier layer is sintered to obtain a sintered barrier layer; the first preset thickness is the thickness of the barrier layer to be sintered; the first barrier layer is entirely a barrier layer to be sintered; Preparing a second barrier layer with a second preset thickness on the surface of the sintering barrier layer; the thickness of the second barrier layer is greater than the thickness of the sintering barrier layer; Preparing a metal conductive layer on the surface of the second barrier layer to complete the preparation of the crystalline silicon battery electrode; The sintered barrier layer is a nickel-silicon alloy barrier layer, and the second barrier layer is a nickel barrier layer; The thickness of the nickel-silicon alloy barrier layer is 5 nanometers to 500 nanometers, and the total thickness of the nickel-silicon alloy barrier layer and the nickel barrier layer is greater than or equal to 200 nanometers.
2. The method for preparing a crystalline silicon battery electrode according to claim 1, characterized in that: A first barrier layer with a first preset thickness is prepared in the grooved area by using a chemical plating process.
3. The method for preparing a crystalline silicon battery electrode according to claim 1, characterized in that: When the first barrier layer is sintered, the sintering temperature is 300 degrees Celsius to 700 degrees Celsius, and the sintering time is 30 seconds to 8 minutes.
4. The method for preparing a crystalline silicon battery electrode according to claim 1, characterized in that: Forming the second barrier layer on the surface of the sintered barrier layer by chemical plating, electroplating or vapor deposition process; A metal conductive layer is formed on the surface of the second barrier layer by using chemical plating, electroplating or vapor deposition process to complete the preparation of the crystalline silicon battery electrode.
5. The method for preparing a crystalline silicon battery electrode according to claim 4, characterized in that: An anti-oxidation protective layer is formed on the surface of the metal conductive layer by chemical plating, electroplating or vapor deposition process.
6. The method for preparing a crystalline silicon battery electrode according to claim 5, characterized in that: The crystalline silicon battery electrode forming the anti-oxidation protection layer is subjected to annealing treatment; the temperature of the annealing treatment is lower than the temperature of the sintering treatment.
7. The method for preparing a crystalline silicon battery electrode according to claim 1, characterized in that: The laser grooving process is used to perform grooving processing on the preset metal electrode area of the crystalline silicon cell prefabricated sheet, and the grooving area is deoxidized to form the grooving area.
8. The method for preparing a crystalline silicon battery electrode according to claim 7, characterized in that: The grooved area is deoxidized by using a slow-release hydrofluoric acid process to form the grooved area.
9. A crystalline silicon battery structure, characterized in that: Prepared by the method for preparing a crystalline silicon battery electrode according to any one of claims 1 to 8, comprising: Crystalline silicon cell prefabricated sheets and crystal silicon cell electrodes; A grooved area is formed in the preset metal electrode area of the crystalline silicon cell prefabricated sheet; The crystalline silicon battery electrode comprises a sintered barrier layer, a second barrier layer and a metal conductive layer which are sequentially arranged along the back of the crystalline silicon battery prefabricated sheet corresponding to the grooved area; The thickness of the sintered barrier layer is less than that of the second barrier layer, and the thickness of the sintered barrier layer is the thickness of the barrier layer required to be sintered; the first barrier layer is completely sintered to obtain the sintered barrier layer; The sintered barrier layer is a nickel-silicon alloy barrier layer, and the second barrier layer is a nickel barrier layer; The thickness of the nickel-silicon alloy barrier layer is 5 nanometers to 500 nanometers, and the total thickness of the nickel-silicon alloy barrier layer and the nickel barrier layer is greater than or equal to 200 nanometers.