Experimental wafer bonding device and method

By combining plasma activation equipment and sealing components in the experimental wafer bonding device, high-quality wafer bonding in non-ideal environments is achieved, solving the reliability of wafer bonding experiments under the lack of ideal cleaning room facilities and Accuracy issues reduce external pollution risks and improve bond success rates.

CN118352251BActive Publication Date: 2024-11-15WUHAN UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410525661.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-29
Publication Date
2024-11-15
Estimated Expiration
2044-04-29

AI Technical Summary

Technical Problem

In the absence of ideal cleaning room facilities, the reliability and accuracy of wafer bonding experiments are affected, especially due to the adverse effects of tiny impurities or particle contamination caused by poor environments on the bonding process, resulting in incomplete experimental results As expected.

Method used

A wafer bonding device for experiments is designed, including plasma activation equipment and experimental devices. The wafer is surface activated in a vacuum environment through wireless control and performs in a sealing environment using sealing components and station switching components. Clean and bond to reduce the risk of external contamination.

Benefits of technology

Improve the reliability and accuracy of the wafer bonding process, ensure the cleaning and activation of the wafer surface, reduce the risk of pollution caused by handling, adapt to different experimental processes, and achieve high-quality wafers in non-ideal environments. Bonding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118352251B_ABST
    Figure CN118352251B_ABST
Patent Text Reader

Abstract

The present invention proposes an experimental wafer bonding device and method, which relates to the field of wafer processing, including plasma activation equipment and experimental equipment; the experimental equipment includes a body, a sealing component and a station switching component, the body has a mounting cavity for mounting the experimental wafer, the station switching component is arranged in the mounting cavity, and has a switchable first station and a second station, the first station is an ion activation station, and the second station is a bonding station, the sealing component is arranged on the body, and the mounting cavity can be opened or closed by wireless control; the plasma activation equipment has a working cavity for accommodating the experimental device, and the surface activation treatment of the experimental wafer in the mounting cavity can be performed under a vacuum environment. The present invention solves the problem of improving the reliability and accuracy of wafer bonding experiments in the absence of ideal clean room facilities, reduces the risk of contamination of the external environment, ensures the activation and bonding of the wafer surface, and thus achieves high-quality wafer bonding under non-ideal cleaning conditions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of wafer processing, and in particular to an experimental wafer bonding device and method. Background Art

[0002] Wafer bonding refers to the process of tightly combining two mirror-polished homogeneous or heterogeneous wafers through chemical and physical effects. After the wafers are bonded, the atoms on the interface react under the action of external forces to form covalent bonds to combine them into one, and the bonding interface reaches a specific bonding strength.

[0003] Wafer surface plasma activation is a surface treatment technology used to improve the chemical properties of the wafer surface for subsequent process steps. The technology uses plasma to activate the wafer surface, making it easier to bond with other wafers.

[0004] Today, experimental conditions are limited in many places, especially in terms of laboratory facilities. The cost of building Class 1000 and Class 100 clean rooms is quite high, which makes it unaffordable for many laboratories. Many researchers have to conduct wafer bonding experiments in less than ideal environments. However, for wafer bonding experiments, the cleanliness of the environment has a huge impact on the experimental results. In these experiments, even tiny impurities or particles may have an adverse effect on the wafer bonding process, resulting in unsatisfactory experimental results. Summary of the invention

[0005] In view of this, the present invention proposes an experimental wafer bonding device and method to solve the problem of how to improve the reliability and accuracy of wafer bonding experiments in the absence of ideal clean room facilities.

[0006] The technical solution of the present invention is achieved in this way:

[0007] In a first aspect, the present invention provides an experimental wafer bonding device, including a plasma activation device and an experimental device;

[0008] The experimental device comprises a body, a sealing component and a station switching component. The surface of the body is provided with an installation cavity for installing the experimental wafer. The station switching component is arranged in the installation cavity and has a switchable first station and a second station. The first station is configured to place the experimental wafer in an ion activation station, and the second station is configured to place the experimental wafer in a bonding station. The sealing component is arranged on the body and can open or close the installation cavity under wireless control.

[0009] The plasma activation equipment has a working chamber for accommodating the experimental device, and can perform surface activation treatment on the experimental wafer in the mounting chamber in an open state under a vacuum environment.

[0010] On the basis of the above technical solution, preferably, the sealing assembly includes a sealing cover, a rotating motor, a battery and a wireless module, the rotating motor, the battery and the wireless module are all fixedly arranged on the main body, the rotating motor is electrically connected to the battery and the wireless module respectively, the sealing cover is horizontally arranged on the top surface of the main body, the rotating motor is used to drive the sealing cover to rotate horizontally to close or open the installation cavity, and the wireless module is used to communicate with the remote control terminal.

[0011] Further, preferably, a sealing member is fixedly provided at the opening of the installation cavity.

[0012] On the basis of the above technical solution, preferably, a rubber plug is fixedly provided on the sealing cover, so that when the sealing cover closes the mounting cavity, a syringe filled with deionized water can pierce the rubber plug to clean the experimental wafer after the surface activation treatment.

[0013] On the basis of the above technical solution, preferably, the workstation switching assembly includes a first loading block, a second loading block, a first driving unit and a second driving unit, the first loading block and the second loading block are arranged in parallel and spaced apart on the bottom surface of the installation cavity, the first loading block and the second loading block have opposite sides for installing experimental wafers, respectively, a side of the first loading block away from the second loading block is connected to the first driving unit, a side of the second loading block away from the first loading block is connected to the second driving unit, the first driving unit is used to drive the first loading block to flip or translate, and the second driving unit is used to drive the second loading block to flip or translate.

[0014] Further, preferably, the first driving unit and the second driving unit have the same structure, wherein the first driving unit includes a rotating rod, a pushing rod and a connecting seat, the connecting seat is fixedly arranged on a side of the first loading block away from the experimental wafer mounting surface, one end of the pushing rod is located in the mounting cavity, and the other end moves through the outside of the main body, the pushing rod is perpendicular to the length direction of the first loading block, one end of the pushing rod is located in the mounting cavity and is rotatably connected to the connecting seat, one end of the rotating rod is located in the mounting cavity, and the other end moves through the outside of the main body, the rotating rod is perpendicular to the pushing rod, one end of the rotating rod is located in the mounting cavity, and the other end moves through the outside of the main body, the rotating rod is perpendicular to the pushing rod, and one end of the rotating rod is located in the mounting cavity is detachably connected to the connecting seat, and the rotating rod can drive the connecting seat and the first loading block to flip relative to the end of the pushing rod.

[0015] On the basis of the above technical solution, preferably, a first positioning portion is fixedly provided on a side of the first loading block away from the first driving unit, and a second positioning portion corresponding to the position of the first positioning portion is fixedly provided on a side of the second loading block away from the second driving unit, and the first positioning portion and the second positioning portion are respectively used for positioning the experimental wafer.

[0016] Further, preferably, mutually connected positioning protrusions and positioning grooves are provided between the surfaces of the first material loading block and the second material loading block that are in contact with the bottom surface of the installation cavity.

[0017] Preferably, a movable channel is provided on the main body for the rotating rod and the pushing rod to pass through, and dynamic sealing members are provided between the rotating rod and the pushing rod and the movable channel.

[0018] In a second aspect, the present invention discloses an experimental wafer bonding method, which utilizes the experimental wafer bonding device described in the first aspect, and is characterized in that it comprises the following steps:

[0019] S1. Two experimental wafers are respectively fixed vertically on the first loading block and the opposite side of the second loading block, and the first driving unit drives the first loading block to flip so that the experimental wafers on the first loading block are in a horizontal state, and the second driving unit drives the second loading block to flip so that the experimental wafers on the second loading block are in a horizontal state;

[0020] S2. Place the experimental device in a plasma activation device, and keep the mounting cavity on the body in an open state;

[0021] S3, setting a vacuum environment through a plasma activation device, and performing surface activation treatment on the experimental wafer in the mounting cavity;

[0022] S4. When the plasma activation treatment on the surface of the experimental wafer is completed, the wirelessly controlled rotary motor rotates so that the sealing cover closes the installation cavity;

[0023] S5, taking the experimental device out of the plasma activation device, and cleaning the experimental wafer in the mounting cavity by piercing the rubber stopper on the sealing cover with a syringe filled with deionized water;

[0024] S6. After the cleaning is completed, the first driving unit drives the first loading block to flip, and the second driving unit drives the second loading block to flip, so as to ensure that the experimental wafers on the first loading block and the second loading block are arranged vertically opposite to each other;

[0025] S7, the first driving unit drives the first loading block to translate, and the second driving unit drives the second loading block to translate, so that the experimental wafers on the first loading block and the experimental wafers on the second loading block are contacted and bonded.

[0026] Compared with the prior art, the present invention has the following beneficial effects:

[0027] (1) The experimental wafer bonding device disclosed in the present invention can greatly improve the reliability and accuracy of the wafer bonding process even in a non-ideal environment by combining the plasma activation equipment and the experimental device. In particular, after plasma activation, the mounting cavity is quickly sealed by a wirelessly controlled sealing component, and the activated wafer surface can be sealed and protected before it is exposed to the external environment, greatly reducing the possibility of re-contamination of the surface and improving the success rate of bonding and the interface quality.

[0028] (2) By designing a rubber plug on the sealing cover, after the wafer surface is activated, it can be directly cleaned with deionized water in a sealed environment without moving the wafer out of the experimental device. This structural setting reduces the handling of the wafer during the processing process and reduces the risk of contamination caused by handling. At the same time, it can ensure that the wafer has a high-quality surface state before bonding, improve the success rate and surface quality of wafer bonding, and thus effectively control the wafer bonding experiment.

[0029] (3) By controlling the flipping or translation of the carrier block through the built-in drive unit, the wafer can be moved in a closed environment, reducing the risk of contamination or damage during movement. Since the carrier block can be flipped or translated, the device can adapt to different experimental processes and provide flexibility for experimental wafer surface activation and bonding experiments.

[0030] (4) The present invention solves the problem of improving the reliability and accuracy of wafer bonding experiments in the absence of ideal clean room facilities by performing plasma activation and cleaning of the wafer in a sealed mounting chamber and using a precisely controlled flipping and translational mechanical device to align the wafer. This method reduces the risk of contamination from the external environment and ensures the cleanliness and activation of the wafer surface, thereby achieving high-quality wafer bonding even under non-ideal cleaning conditions. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0032] Figure 1 It is a structural schematic diagram of a wafer disclosed in the present invention being in an ion activation station in an experimental device;

[0033] Figure 2 It is a structural schematic diagram of a wafer disclosed in the present invention being in a bonding station in an experimental device;

[0034] Figure 3 A schematic diagram of the state of the experimental device disclosed in the present invention in a plasma activation device;

[0035] Figure 4 It is a schematic diagram of the three-dimensional structure from a first perspective of the workstation switching assembly disclosed in the present invention;

[0036] Figure 5 It is a schematic diagram of the stereoscopic structure of the workstation switching assembly disclosed in the present invention from a second viewing angle;

[0037] Figure 6 It is a schematic diagram of the planar structure of the experimental device disclosed in the present invention;

[0038] Figure 7 It is a schematic diagram of a wafer in a cleaning state in an experimental device disclosed in the present invention;

[0039] Figure 8 It is a schematic diagram of the wafer bonding state in the experimental device disclosed in the present invention;

[0040] Reference numerals:

[0041] 1. Plasma activation equipment; 2. Experimental device; 21. Main body; 22. Sealing assembly; 23. Workstation switching assembly; 11. Working chamber; 211. Installation chamber; 221. Sealing cover; 222. Rotating motor; 223. Battery; 224. Wireless module; S1. Sealing member; 2210. Rubber plug; 231. First loading block; 232. Second loading block; 233. First driving unit; 234. Second driving unit; 2331. Rotating rod; 2332. Pushing rod; 2333. Connecting seat; 2311. First positioning part; 2321. Second positioning part; D1. Positioning protrusion; D2. Positioning groove; 212. Movable channel; S2. Dynamic sealing member; P. Experimental wafer; Q. Injector. DETAILED DESCRIPTION

[0042] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0043] like Figure 1 As shown, combined Figure 2-3 An embodiment of the present invention discloses an experimental wafer bonding device, including a plasma activation device 1 and an experimental device 2.

[0044] Among them, the plasma activation equipment 1 is used to perform plasma activation treatment on the wafer surface under a vacuum environment. The equipment can select a more conventional small plasma activation equipment 1 on the market, as long as the experimental device 2 can be placed inside it to meet the vacuum environment and plasma treatment operations.

[0045] The experimental device 2 is used to provide components for loading the experimental wafer P and bonding operations. In the present embodiment, the experimental device 2 loaded with the experimental wafer P is placed in the working chamber 11 of the plasma activation equipment 1. The plasma activation equipment 1 performs a vacuum treatment so that the experimental device 2 loaded with the wafer is placed in a vacuum environment. This can ensure that the wafer is in an ideal experimental environment, facilitating subsequent surface activation treatments and bonding operations.

[0046] The experimental device 2 of this embodiment includes a body 21, a sealing component 22 and a station switching component 23. The body 21 is the basis of the entire experimental device 2, which can be set as a box or a square structure. The surface of the body 21 has a mounting cavity 211 for mounting the experimental wafer P, which provides a fixed and protected environment for the wafer to ensure the accuracy and repeatability of the experiment. Preferably, the entire body 21 can be made of transparent plastic material, which is convenient for observing the wafer in the body 21 during activation or bonding.

[0047] The sealing component 22 is arranged on the body 21 and can open or close the mounting cavity 211 under wireless control. It can provide necessary sealing or opening state in different experimental stages to protect the wafer from environmental pollution, especially after plasma activation, the wafer surface is extremely sensitive and needs good protection.

[0048] Specifically, after the two experimental wafers P are loaded in the mounting chamber 211, the experimental device 2 is placed in the working chamber 11 of the plasma activation device 1. At this time, the sealing component 22 does not seal the mounting chamber 211, so that the working chamber 11 and the mounting chamber 211 of the body 21 are connected. By evacuating the working chamber 11 of the plasma activation device 1, the wafer is placed in a vacuum environment, ensuring that the wafer is in an ideal clean environment. After the surface activation treatment of the experimental wafer P is completed, the two wafers in the experimental device 2 need to be bonded. At this time, the experimental device 2 needs to be taken out of the working chamber 11 of the plasma activation device 1. If the experimental device 2 is taken out directly, the activated wafer will be exposed to the outside air, causing air impurities to contaminate the wafer surface. Therefore, after the wafer activation is completed and before the experimental device 2 is taken out, the sealing component 22 is wirelessly controlled to seal the mounting chamber 211, so that the wafer can be placed in a vacuum environment in the mounting chamber 211, ensuring that the wafer is in a good clean protection environment after the experimental device 2 is taken out from the ion activation device.

[0049] The station switching assembly 23 is disposed in the mounting cavity 211 and has a switchable first station and a switchable second station. The first station is configured to place the experimental wafer P in an ion activation station, and the second station is configured to place the experimental wafer P in a bonding station.

[0050] Specifically, the two experimental wafers P are installed in the workstation switching component 23. Before the initial experiment, the positions of the two experimental wafers P are adjusted through the workstation switching component 23 so that the surfaces of the two wafers to be bonded are horizontally facing upward, and then the two experimental wafers P are subjected to surface activation treatment by the plasma activation equipment 1. After the activation treatment is completed, the mounting cavity 211 is sealed by the sealing component 22. After the experimental device 2 is taken out of the plasma activation equipment 1, the positions of the two wafers can be adjusted by the workstation switching component 23, thereby achieving surface contact bonding of the two wafers.

[0051] The experimental wafer bonding device disclosed in the present invention can greatly improve the reliability and accuracy of the wafer bonding process even in a non-ideal environment by combining the plasma activation device 1 and the experimental device 2. In particular, after plasma activation, the mounting cavity 211 is quickly sealed by the wirelessly controlled sealing component 22, and the activated wafer surface can be sealed and protected before it is exposed to the external environment, which greatly reduces the possibility of re-contamination of the surface and improves the success rate of bonding and the interface quality.

[0052] In order to realize opening or closing of the installation cavity 211 , this embodiment shows a preferred implementation of the sealing assembly 22 . Specifically, the sealing assembly 22 includes a sealing cover 221 , a rotating motor 222 , a battery 223 and a wireless module 224 .

[0053] The rotating motor 222, the battery 223 and the wireless module 224 are all fixedly arranged on the main body 21. The rotating motor 222 is electrically connected to the battery 223 and the wireless module 224 respectively. The sealing cover 221 is horizontally arranged on the top surface of the main body 21. The rotating motor 222 is used to drive the sealing cover 221 to rotate horizontally to close or open the installation cavity 211. The wireless module 224 is used to communicate with the remote control terminal.

[0054] Through the setting of the wireless module 224, a communication signal can be sent to the wireless module 224 through a remote control terminal, such as a remote controller. After receiving the control command, the wireless module 224 controls the rotation of the rotary motor 222, and the rotary motor 222 drives the sealing cover 221 to perform horizontal rotational movement to realize the opening and closing of the installation cavity 211. When wafer installation and surface activation are required, the sealing cover 221 is opened, and when the wafer needs to be bonded, the sealing cover 221 is closed, so that after the experimental device 2 is taken out from the plasma activation device 1, the wafer can maintain the sealed state of the cavity during the bonding process to avoid external contamination.

[0055] By remotely controlling the sealing cover 221 through the wireless module 224, after the experimental device 2 completes the wafer plasma activation treatment in the plasma activation equipment 1, the mounting cavity 211 can be quickly sealed through the sealing cover 221, so as to avoid the surface of the activated wafer being exposed to the external environment when the plasma activation equipment 1 is manually opened for wafer bonding. The mounting cavity 211 can be quickly sealed through the wirelessly controlled sealing component 22, so that the activated wafer surface can be sealed and protected before it is exposed to the external environment, thereby greatly reducing the possibility of re-contamination of the surface and improving the controllability of the bonding process of the experimental wafer P.

[0056] In some embodiments, the wireless module 224 may be any one of a Bluetooth module, a WIFI module, a radio frequency (RF) module, a mobile communication module, a Zigbee module, or a LoRa module.

[0057] Preferably, a seal S1 is fixedly provided at the opening of the installation cavity 211. Thus, through the setting of the seal S1, the sealing cover 221 can contact the seal S1 to reliably seal the installation cavity 211, ensuring that the installation cavity 211 is in a vacuum clean environment during the wafer bonding process.

[0058] Since there will be residual ions on the wafer surface after the plasma surface activation treatment, the residual ions on the wafer surface need to be removed before the wafer is bonded.

[0059] If a deionization device is directly provided in the plasma activation device 1 , the structure of the plasma activation device 1 needs to be improved, which undoubtedly increases the structural complexity of the plasma activation device 1 and also increases the manufacturing cost of the device.

[0060] For this purpose, refer to the attached Figure 1 and 7 As shown, in this embodiment, a rubber plug 2210 is fixedly provided on the sealing cover 221. After the wafer surface is activated and the sealing cover 221 has sealed the mounting cavity 211, the experimental device 2 is taken out from the plasma activation equipment 1, and a syringe Q filled with deionized water pierces the rubber plug 2210 and extends into the mounting cavity 211 to clean the experimental wafer P after the surface activation treatment.

[0061] By designing a rubber plug 2210 on the sealing cover 221, after the wafer surface is activated, it can be directly cleaned with deionized water in a sealed environment without moving the wafer out of the experimental device 2. Such a structural setting reduces the handling of the wafer during the processing process and reduces the risk of contamination caused by handling. At the same time, it can ensure that the wafer has a high-quality surface state before bonding, improve the success rate and surface quality of wafer bonding, and thus effectively control the wafer bonding experiment.

[0062] In order to realize the wafer surface activation and the switching of the bonding stations, this embodiment shows a preferred implementation of the station switching component 23. Figure 4-8 As shown, the workstation switching assembly 23 includes a first material loading block 231 , a second material loading block 232 , a first driving unit 233 and a second driving unit 234 .

[0063] The first loading block 231 and the second loading block 232 are arranged in parallel and spaced apart on the inner bottom surface of the installation cavity 211, and the opposite sides of the first loading block 231 and the second loading block 232 are respectively used to install the experimental wafer P. It should be noted that the experimental wafer P is arranged on the opposite sides of the first loading block 231 and the second loading block 232, and the two experimental wafers P are currently in a position that requires bonding. When the first loading block 231 and the second loading block 232 are flipped 90° in opposite directions, the two experimental wafers P are arranged at intervals on the same horizontal plane, and the surfaces of the two experimental wafers P face the opening of the installation cavity 211, and the two experimental wafers P are currently in a position that requires plasma activation.

[0064] In some preferred embodiments, the test wafer P can be bonded to the surface of the carrier block by a small amount of glue.

[0065] The side of the first loading block 231 away from the second loading block 232 is connected to the first driving unit 233, and the side of the second loading block 232 away from the first loading block 231 is connected to the second driving unit 234. The first driving unit 233 is used to drive the first loading block 231 to flip or translate, and the second driving unit 234 is used to drive the second loading block 232 to flip or translate.

[0066] The driving unit is responsible for flipping or translating the corresponding loading block. According to this setting, when the experimental wafer P needs to be switched between different workstations, the driving unit can adjust the position of the wafer by flipping or translating the loading block.

[0067] Specifically, when the driving unit performs the flipping of the loading block, the experimental wafer P can be switched between a vertical state and a horizontal state. That is, when the experimental wafer P is in a vertical state, it indicates that the experimental wafer P needs to be in a bonding operation, and when the experimental wafer P is in a horizontal state, it indicates that the experimental wafer P needs to be in an activation operation.

[0068] When the experimental wafer P is in a vertical state and the driving unit performs the translation of the carrier block, the two experimental wafers P move closer to each other, thereby achieving a bonding operation.

[0069] By controlling the flipping or translation of the carrier block through the built-in drive unit, the wafer can be moved in a closed environment, reducing the risk of contamination or damage during movement. Since the carrier block can be flipped or translated, the device can adapt to different experimental processes and provide flexibility for experimental wafer P surface activation and bonding experiments.

[0070] In this embodiment, the first driving unit 233 and the second driving unit 234 have the same structure. The first driving unit 233 is taken as an example for description, wherein the first driving unit 233 includes a rotating rod 2331 , a pushing rod 2332 and a connecting seat 2333 .

[0071] The connection seat 2333 is fixedly disposed on a side of the first loading block 231 away from the mounting surface of the experimental wafer P, providing a connection point for the rotating rod 2331 and the pushing rod 2332 .

[0072] One end of the push rod 2332 is located in the installation cavity 211, and the other end is movable through the outside of the body 21. The push rod 2332 is perpendicular to the length direction of the first loading block 231. One end of the push rod 2332 located in the installation cavity 211 is rotatably connected to the connecting seat 2333. The push rod is used to drive the loading block to perform a translation movement in the installation cavity 211. When the two loading blocks are relatively translated, two experimental wafers P can be bonded.

[0073] One end of the rotating rod 2331 is located in the installation cavity 211, and the other end is movable through the outside of the main body 21. The rotating rod 2331 is perpendicular to the pushing rod 2332. The end of the rotating rod 2331 located in the installation cavity 211 is detachably connected to the connecting seat 2333, and the rotating rod 2331 can drive the connecting seat 2333 and the first loading block 231 to flip relative to the end of the pushing rod 2332.

[0074] In the specific implementation process, when the experimental wafer P is located on the top surface of the loading block, the experimental wafer P needs to be activated or has completed the activation. If a bonding operation is required, the rotating rod 2331 is first used to drive the connecting seat 2333 to drive the loading block to flip 90°, so that the experimental wafer P is in a vertical state. When both loading blocks are flipped 90° and the two experimental wafers P are in a vertical parallel state, the rotating rod 2331 is disconnected from the connecting seat 2333, and the connecting seat 2333 is pushed by the pushing rod 2332 to drive the loading block to move horizontally, so that the two loading blocks are brought closer to each other, and then the two experimental wafers P are bonded.

[0075] By setting the driving unit above, the flexibility and controllability of the experimental wafer P in the experimental device 2 are improved.

[0076] In order to achieve accurate alignment of the two experimental wafers P after bonding, the solution adopted in this embodiment is: a first positioning portion 2311 is fixedly provided on one side of the first loading block 231 away from the first driving unit 233, and a second positioning portion 2321 corresponding to the position of the first positioning portion 2311 is fixedly provided on one side of the second loading block 232 away from the second driving unit 234. The first positioning portion 2311 and the second positioning portion 2321 are respectively used to position the experimental wafer P. By adopting the above solution, the first positioning portion 2311 and the second positioning portion 2321 can ensure accurate alignment of the two experimental wafers P during the bonding process.

[0077] In some preferred embodiments, the first positioning portion 2311 and the second positioning portion 2321 are both L-shaped structures, which can adapt to experimental wafers P of different sizes.

[0078] A positioning protrusion D1 and a positioning groove D2 connected to each other are provided between the first material loading block 231 and the second material loading block 232, which are in contact with the inner bottom surface of the mounting cavity 211. With the above technical solution, when the two material loading blocks are close to each other, the positioning protrusion D1 and the positioning groove D2 can be used in coordination to align the two material loading blocks when connected to each other, thereby ensuring that the two experimental wafers P are aligned when bonded. In this embodiment, the positioning protrusion D1 can be provided on the bottom surface of the first material loading block 231 or the bottom surface of the second material loading block 232.

[0079] As some optional embodiments, a movable channel 212 is provided on the main body 21 for the rotating rod 2331 and the pushing rod 2332 to pass through, allowing the rotating rod 2331 and the pushing rod 2332 to pass through the movable channel 212 through the main body 21 and enter the installation cavity 211, and the rotating rod 2331 and the pushing rod 2332 can move in the movable channel 212.

[0080] Since there is a gap between the rotating rod 2331 and the pushing rod 2332 and the active channel 212, external air will enter the installation cavity 211 through the above gap, thereby polluting the surface of the experimental wafer P. To this end, in this embodiment, a dynamic seal S2 is provided between the rotating rod 2331 and the pushing rod 2332 and the active channel 212. Thus, the dynamic seal S21 can realize the movement of the rotating rod 2331 and the pushing rod 2332 in the active channel 212 on the one hand, and can realize the sealing between the rotating rod 2331 and the pushing rod 2332 and the active channel 212 on the other hand, so as to prevent external gas from entering the installation cavity 211 through the active channel 212, thereby ensuring that the interior of the installation cavity 211 is in a clean environment and improving the surface quality of the experimental wafer P after bonding.

[0081] The present invention also discloses an experimental wafer bonding method, comprising the following steps:

[0082] Step 1: vertically fix two experimental wafers P on the first loading block 231 and the opposite side of the second loading block 232 respectively, and drive the first loading block 231 to flip by the first driving unit 233 so that the experimental wafer P on the first loading block 231 is in a horizontal state, and drive the second loading block 232 to flip by the second driving unit 234 so that the experimental wafer P on the second loading block 232 is in a horizontal state;

[0083] Step 2: Place the experimental device 2 in the plasma activation device 1, and make the mounting cavity 211 on the body 21 open;

[0084] Step 3: Setting a vacuum environment through the plasma activation device 1 and performing surface activation treatment on the experimental wafer P in the mounting cavity 211;

[0085] Step 4: After the plasma activation treatment of the wafer surface is completed, the wirelessly controlled rotary motor 222 rotates to make the sealing cover 221 seal the installation cavity 211;

[0086] Step 5: Take the experimental device 2 out of the plasma activation device 1, and clean the experimental wafer P in the mounting cavity 211 by piercing the rubber stopper 2210 on the sealing cover 221 with a syringe Q filled with deionized water;

[0087] Step 6: After cleaning is completed, the first driving unit 233 drives the first loading block 231 to flip, and the second driving unit 234 drives the second loading block 232 to flip, to ensure that the experimental wafers P on the first loading block 231 and the second loading block 232 are arranged vertically opposite to each other;

[0088] Step 7: The first driving unit 233 drives the first loading block 231 to translate, and the second driving unit 234 drives the second loading block 232 to translate, so that the experimental wafers P on the first loading block 231 and the second loading block 232 are in contact and bonded.

[0089] The present invention solves the problem of improving the reliability and accuracy of wafer bonding experiments in the absence of ideal clean room facilities by performing plasma activation and cleaning of the wafer in the sealed mounting chamber 211 and using a precisely controlled flipping and translational mechanical device to align the wafer. This method reduces the risk of contamination from the external environment, ensures the cleanliness and activation of the wafer surface, and thus achieves high-quality wafer bonding even under non-ideal cleaning conditions.

[0090] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. An experimental wafer bonding device, characterized in that: It comprises a plasma activation device (1) and an experimental device (2); The experimental device (2) comprises a body (21), a sealing component (22) and a station switching component (23); a mounting cavity (211) is provided on the surface of the body (21) for mounting an experimental wafer (P); the station switching component (23) is arranged in the mounting cavity (211) and has a switchable first station and a switchable second station; the first station is configured to place the experimental wafer (P) in an ion activation station, and the second station is configured to place the experimental wafer (P) in a bonding station; the sealing component (22) is arranged on the body (21) and can open or close the mounting cavity (211) under wireless control; The plasma activation device (1) has a working chamber (11) for accommodating the experimental device (2), and can perform surface activation treatment on an experimental wafer (P) in an open mounting chamber (211) under a vacuum environment; The sealing assembly (22) comprises a sealing cover (221), a rotating motor (222), a battery (223) and a wireless module (224); the rotating motor (222), the battery (223) and the wireless module (224) are all fixedly arranged on the body (21); the rotating motor (222) is electrically connected to the battery (223) and the wireless module (224) respectively; the sealing cover (221) is horizontally arranged on the top surface of the body (21); the rotating motor (222) is used to drive the sealing cover (221) to rotate horizontally to close or open the installation cavity (211); and the wireless module (224) is used to communicate with a remote control terminal.

2. The experimental wafer bonding device according to claim 1, characterized in that: A sealing member (S1) is fixedly arranged at the opening of the installation cavity (211).

3. The experimental wafer bonding device according to claim 1, characterized in that: The sealing cover (221) is fixedly provided with a rubber plug (2210) for allowing a syringe (Q) filled with deionized water to pierce the rubber plug (2210) to clean the experimental wafer (P) after the surface activation treatment when the sealing cover (221) closes the installation cavity (211).

4. The experimental wafer bonding device according to claim 3, characterized in that: The workstation switching assembly (23) comprises a first loading block (231), a second loading block (232), a first driving unit (233) and a second driving unit (234); the first loading block (231) and the second loading block (232) are arranged in parallel and spaced apart on the inner bottom surface of the mounting cavity (211); opposite sides of the first loading block (231) and the second loading block (232) are respectively used for mounting the experimental wafer (P); a side of the first loading block (231) away from the second loading block (232) is connected to the first driving unit (233); a side of the second loading block (232) away from the first loading block (231) is connected to the second driving unit (234); the first driving unit (233) is used to drive the first loading block (231) to flip or translate; the second driving unit (234) is used to drive the second loading block (232) to flip or translate.

5. The experimental wafer bonding device according to claim 4, characterized in that: The first driving unit (233) and the second driving unit (234) have the same structure, wherein the first driving unit (233) comprises a rotating rod (2331), a pushing rod (2332) and a connecting seat (2333), wherein the connecting seat (2333) is fixedly arranged on a side of the first loading block (231) away from the mounting surface of the experimental wafer (P), one end of the pushing rod (2332) is located in the mounting cavity (211), and the other end is movable through the outside of the body (21), the pushing rod (2332) is perpendicular to the length direction of the first loading block (231), and the pushing rod (2332) is perpendicular to the length direction of the first loading block (231). One end of the rotating rod (2332) located in the installation cavity (211) is rotatably connected to the connecting seat (2333), one end of the rotating rod (2331) is located in the installation cavity (211), and the other end is movable through the outside of the main body (21), the rotating rod (2331) is perpendicular to the pushing rod (2332), one end of the rotating rod (2331) located in the installation cavity (211) is detachably connected to the connecting seat (2333), and the rotating rod (2331) can drive the connecting seat (2333) and the first loading block (231) to flip relative to the end of the pushing rod (2332).

6. The experimental wafer bonding device according to claim 5, characterized in that: A first positioning portion (2311) is fixedly provided on one side of the first loading block (231) away from the first driving unit (233), and a second positioning portion (2321) corresponding to the position of the first positioning portion (2311) is fixedly provided on one side of the second loading block (232) away from the second driving unit (234). The first positioning portion (2311) and the second positioning portion (2321) are respectively used to position the experimental wafer (P).

7. The experimental wafer bonding device according to claim 5 or 6, characterized in that: Interconnected positioning protrusions (D1) and positioning grooves (D2) are provided between the surfaces of the first material loading block (231) and the second material loading block (232) that are in contact with the inner bottom surface of the installation cavity (211).

8. The experimental wafer bonding device according to claim 5, characterized in that: The main body (21) is provided with a movable channel (212) for the rotating rod (2331) and the pushing rod (2332) to pass through, and dynamic sealing components are provided between the rotating rod (2331) and the pushing rod (2332) and the movable channel (212).

9. An experimental wafer bonding method, using the experimental wafer bonding device according to any one of claims 4 to 8, characterized in that: The steps include: S1. Two experimental wafers (P) are respectively fixed vertically on opposite sides of a first material carrier block (231) and a second material carrier block (232); a first driving unit (233) is used to drive the first material carrier block (231) to flip so that the experimental wafers (P) on the first material carrier block (231) are in a horizontal state; a second driving unit (234) is used to drive the second material carrier block (232) to flip so that the experimental wafers (P) on the second material carrier block (232) are in a horizontal state; S2, placing the experimental device (2) in the plasma activation device (1), and making the mounting cavity (211) on the body (21) open; S3, setting a vacuum environment through a plasma activation device (1), and performing surface activation treatment on the experimental wafer (P) in the mounting cavity (211); S4, when the plasma activation treatment on the wafer surface is completed, the wirelessly controlled rotating motor (222) rotates so that the sealing cover (221) closes the installation cavity (211); S5, taking the experimental device (2) out of the plasma activation device (1), and piercing the rubber stopper (2210) on the sealing cover (221) with a syringe (Q) filled with deionized water to clean the experimental wafer (P) in the mounting cavity (211); S6. After the cleaning is completed, the first driving unit (233) drives the first material loading block (231) to flip, and the second driving unit (234) drives the second material loading block (232) to flip, so as to ensure that the experimental wafers (P) on the first material loading block (231) and the second material loading block (232) are arranged vertically opposite to each other; S7. The first driving unit (233) is then used to drive the first material carrier block (231) to translate, and the second driving unit (234) is used to drive the second material carrier block (232) to translate, so that the experimental wafers (P) on the first material carrier block (231) and the second material carrier block (232) are contacted and bonded.