An integrated chip with integrated magnetic core and horizontal Hall element and a preparation method thereof

Through the integrated chip preparation method that integrates the magnetic core and the horizontal Hall element, and the bonding of the magnetic flux concentrator and the Hall ASIC chip, the volume and accuracy problems caused by the large-size ferromagnetic core in the Hall chip are solved, and the Miniaturization and high-precision amplification of magnetic field detection.

CN118393408BActive Publication Date: 2024-10-18NINGBO CRRC TIMES TRANSDUCER TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410855624.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-10-18
Estimated Expiration
2044-06-28

AI Technical Summary

Technical Problem

Existing Hall chips use large-sized ferromagnetic cores when detecting magnetic fields, resulting in larger sizes and poor assembly accuracy, which affects the accuracy of magnetic field detection signals.

Method used

Using an integrated chip preparation method that integrates a magnetic core and a horizontal Hall element, the magnetic flux concentrator and the Hall ASIC chip are aligned and wafer bonded to form an integrated integrated chip, and the magnetic flux condensing film is used to gather the magnetic induction lines , replacing large ferromagnetic cores.

Benefits of technology

It achieves the miniaturization of integrated chips, improves assembly accuracy, is significantly better than the alignment accuracy and thickness control of large magnet cores, and can effectively amplify the intensity of the detected magnetic field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118393408B_ABST
    Figure CN118393408B_ABST
Patent Text Reader

Abstract

An integrated chip with integrated magnetic core and horizontal Hall element and a preparation method thereof, wherein two magnetic flux concentrators are aligned with the Hall ASIC chip respectively by wafer bonding, and then wafer-bonded to the upper and lower surfaces of the Hall ASIC chip respectively to form an integrated integrated chip; a magnetic flux concentrator film is provided in each magnetic flux concentrator, and a horizontal Hall element is provided in the horizontal Hall ASIC chip. The present invention forms an integrated integrated chip by means of magnetic flux concentrators and Hall ASIC chips, wherein the magnetic flux concentrator film can converge magnetic induction lines and amplify the intensity of the detected magnetic field, thereby achieving the same function as a ferromagnetic core. The integrated chip does not require the use of a large ferromagnetic core, and can realize the miniaturization of the Hall current detection chip; the micron-level precision alignment of the real magnetic flux concentrator film and the horizontal Hall element is significantly better than the alignment accuracy of the current magnetic core assembly.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of Hall devices, and in particular to an integrated chip of an integrated magnetic core and a horizontal Hall element and a preparation method thereof. Background Art

[0002] The Hall chip is a magnetic field sensor based on the Hall effect. It converts the changing magnetic field into a change in output voltage, thereby measuring and monitoring the magnetic field. The working principle of the Hall chip is based on the Hall effect. When a semiconductor sheet is placed in a magnetic field, if a current flows through it, an electromotive force will be generated in the direction perpendicular to the current and the magnetic field. This phenomenon is the Hall effect. The Hall chip uses this effect to convert the change in the magnetic field into a voltage signal output.

[0003] Whether it is an open-loop Hall chip or a closed-loop Hall chip, the magnetic field strength detected by a single Hall chip is relatively weak. Currently, it is generally in a package structure or a module structure, by placing ferrite and other ferromagnetic core structures in the upper and lower magnetic field detection areas of the Hall chip, to gather magnetic induction lines and amplify the strength of the detected magnetic field. Generally, the ferromagnetic core is much larger than the Hall chip itself, and the size of the ferromagnetic core ranges from 3mm to 8mm, which limits the application scenarios and fields of the Hall chip and increases the actual use volume; at the same time, the assembly accuracy and consistency of the large ferromagnetic core structure are poor, which can easily affect the accuracy of the magnetic field detection signal.

[0004] Therefore, in view of the shortcomings of the prior art, it is necessary to provide an integrated chip with an integrated magnetic core and a horizontal Hall element and a preparation method thereof to solve the shortcomings of the prior art. Summary of the invention

[0005] One of the purposes of the present invention is to avoid the shortcomings of the prior art and provide a method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element. The integrated chip prepared by the method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element avoids using a large-sized ferromagnetic core in the prior art, can greatly reduce the size of the integrated chip, and has high assembly accuracy.

[0006] The above-mentioned purpose of the present invention is achieved by the following technical measures:

[0007] Provided is a method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element, wherein two magnetic flux concentrators are aligned with the Hall ASIC chip respectively, and then wafer-bonded to the upper surface and the lower surface of the Hall ASIC chip respectively to form an integrated integrated chip.

[0008] A magnetic flux concentrator film is arranged in each magnetic flux concentrator, a horizontal Hall element is arranged in the horizontal Hall ASIC chip, and the magnetic flux concentrator film is located directly above or directly below the horizontal Hall element.

[0009] The two magnetic flux concentrators are respectively defined as a first magnetic flux concentrator and a second magnetic flux concentrator.

[0010] Preferably, the first magnetic flux concentrator wafer is bonded to the upper surface of the Hall ASIC chip, and the magnetic flux concentrator film of the first magnetic flux concentrator is located directly above the horizontal Hall element;

[0011] Preferably, the second magnetic flux concentrator wafer is bonded to the lower surface of the Hall ASIC chip, and the magnetic flux concentrator film of the second magnetic flux concentrator is located directly below the horizontal Hall element.

[0012] Preferably, each magnetic flux concentrator is also provided with a plurality of first alignment marking points, a first oxide layer and a first wafer substrate, the first alignment marking points and the magnetic flux concentrating film are respectively arranged on the upper surface of the first wafer substrate, and the first oxide layer is arranged on the upper surface of the first wafer substrate, the upper surface of the first alignment marking points and the upper surface of the magnetic flux concentrating film.

[0013] Preferably, the above-mentioned Hall ASIC chip is provided with a plurality of second alignment marking points, a second wafer substrate, a second oxide layer, a structural layer and a debugging circuit; the second alignment marking points, the horizontal Hall element and the debugging circuit are all arranged on the upper surface of the second wafer substrate; the structural layer is arranged on the upper surface of the second wafer substrate, the upper surface of the second alignment marking points and the upper surface of the horizontal Hall element; and the second oxide layer is arranged on the upper surface of the structural layer.

[0014] The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element of the present invention is prepared by the following steps:

[0015] S1, aligning a first alignment mark point of the first magnetic flux concentrator with a second alignment mark point of the Hall ASIC chip, and then bonding the first oxide layer of the first magnetic flux concentrator with the second oxide layer, so that the first magnetic flux concentrator and the Hall ASIC chip form an integrally connected overall structure, and defining the overall structure as a first wafer structure;

[0016] S2, thinning the second wafer substrate in the first wafer structure obtained in S1 to obtain a thinned wafer structure;

[0017] S3, providing a third oxide layer on the surface of the thinned wafer substrate in the thinned wafer structure obtained in S2;

[0018] S4, aligning the first alignment mark point of the second magnetic flux concentrator with the second alignment mark point in the thinned wafer structure, and bonding the third oxide layer to the first oxide layer of the second magnetic flux concentrator, so that the second magnetic flux concentrator and the thinned wafer structure form an integrally connected overall structure, and defining the overall structure as a second wafer structure;

[0019] S5, thinning the first wafer substrate and the second wafer substrate in the second wafer structure obtained in S4 respectively to obtain a third wafer structure;

[0020] S6. Form a through hole on one side of the third wafer structure obtained in S5 by a through silicon via process, and then set a lead in the through hole, and the through hole is connected to the surface of the debugging circuit, and the lead is electrically connected to the debugging circuit to obtain the integrated chip.

[0021] In S2, the second wafer substrate is thinned to a thickness of 230 Å to 280 Å.

[0022] Preferably, the above-mentioned S3 specifically grows silicon on the surface of the thinned second wafer substrate in the thinned wafer structure obtained in S2 at a temperature of 1180°C to 1250°C inside the furnace tube and under oxygen conditions to form a layer of silicon oxide film, wherein the silicon oxide film is the third oxide layer, and the thickness of the third oxide layer is about 2800Å to 3200Å.

[0023] Preferably, the above-mentioned integrated magnetic core is packaged with an external Hall package lead frame before use, the maximum width of the groove in the external Hall package lead frame is defined as A, the maximum width of the magnetic flux focusing film is defined as B, the maximum width of the horizontal Hall element is defined as C, and 30μm≤C≤B≤A≤100μm exists.

[0024] Preferably, the magnetic flux concentrating film is a FeNi-based magnetic flux concentrating film, a FeZn-based magnetic flux concentrating film, a FeCo-based magnetic flux concentrating film or a FeNiMo-based magnetic flux concentrating film.

[0025] Preferably, the thickness of the first oxide layer and the second oxide layer is between 1000Å and 1 μm.

[0026] Preferably, the material of the first oxide layer and the material of the second oxide layer are silicon dioxide or tetraethyl silicate.

[0027] Preferably, the above-mentioned first wafer substrate is a silicon-based substrate.

[0028] Preferably, the structural layer is at least one of a metal wiring layer, a dielectric layer or a passivation layer.

[0029] Preferably, the first wafer substrate is a silicon-based substrate, a gallium arsenide substrate or an indium antimonide substrate.

[0030] Preferably, the second wafer substrate is a silicon-based substrate, a gallium arsenide substrate or an indium antimonide substrate.

[0031] Another object of the present invention is to provide an integrated chip that avoids the shortcomings of the prior art and avoids using a large-sized ferromagnetic core in the prior art, thereby significantly reducing the size of the integrated chip and having high assembly and alignment accuracy.

[0032] The above-mentioned purpose of the present invention is achieved by the following technical measures:

[0033] Provided is an integrated magnetic core, which is prepared by using the above-mentioned integrated chip preparation method.

[0034] The present invention discloses an integrated chip of an integrated magnetic core and a horizontal Hall element and a preparation method thereof. Two magnetic flux concentrators are aligned with the Hall ASIC chip respectively, and then wafer-bonded to the upper and lower surfaces of the Hall ASIC chip respectively to form an integrated integrated chip. A magnetic flux concentrator film is provided in each magnetic flux concentrator, and a horizontal Hall element is provided in the horizontal Hall ASIC chip, and the magnetic flux concentrator film is located directly above or directly below the horizontal Hall element. The present invention forms an integrated integrated chip through a magnetic flux concentrator and a Hall ASIC chip, wherein the magnetic flux concentrator film can converge magnetic induction lines and amplify the intensity of the detected magnetic field, thereby achieving the same function as a ferromagnetic core. Compared with the prior art, the integrated chip does not need to use a large ferromagnetic core, and can realize the miniaturization of the Hall current detection chip; realizes micron-level precision alignment of the magnetic flux concentrator film and the horizontal Hall element, which is significantly better than the alignment accuracy of the current magnetic core assembly; and can also realize the control of the bonding thickness between the magnetic flux concentrator film layer and the Hall element, and the thickness accuracy is significantly better than the control level of the assembly of a large magnetic core module. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] The present invention is further described with reference to the accompanying drawings, but the contents in the accompanying drawings do not constitute any limitation to the present invention.

[0036] Figure 1 The schematic diagram of the integrated magnetic core obtained by the method for preparing the integrated chip of the integrated magnetic core and the horizontal Hall element of the present invention.

[0037] Figure 2 Schematic diagram of a magnetic flux concentrator.

[0038] Figure 3 Schematic diagram of the Hall ASIC chip.

[0039] Figure 4Schematic diagram of the maximum width of the groove, flux concentrating film and horizontal Hall element in the lead frame for external Hall package.

[0040] Figure 5 It is a schematic diagram of the alignment of the first magnetic flux concentrator and the Hall ASIC chip in S1 of the present invention.

[0041] Figure 6 Schematic diagram of the first wafer structure obtained by S1.

[0042] Figure 7 Schematic diagram of the thinned wafer structure obtained by S2.

[0043] Figure 8 Schematic diagram of the thinned wafer structure with a third oxide layer set in S3.

[0044] Fig. 9 Schematic diagram of the alignment of the second magnetic flux concentrator and the thinned wafer structure in S4.

[0045] Fig.10 Schematic diagram of the second wafer structure obtained in S4.

[0046] Fig.11 Schematic diagram of the third wafer structure obtained in S5.

[0047] Fig.12 Schematic diagram of the integrated chip obtained for S6.

[0048] exist Figures 1 to 12 Including:

[0049] Magnetic flux concentrator 100, first alignment mark point 110, magnetic flux concentrator film 120, first oxide layer 130, first wafer substrate 140,

[0050] Hall ASIC chip 200, horizontal Hall element 210, second wafer substrate 220, second oxide layer 230, structural layer 240, debugging circuit 250, second alignment mark point 260,

[0051] The third oxide layer 300 , the through hole 400 , the lead frame 500 for the external Hall package, and the groove 510 . DETAILED DESCRIPTION

[0052] The technical solution of the present invention is further described in conjunction with the following embodiments. Example

[0053] A method for preparing an integrated chip with an integrated magnetic core and a horizontal Hall element, aligning two magnetic flux concentrators 100 with a Hall ASIC chip 200, and then wafer bonding them to the upper surface and the lower surface of the Hall ASIC chip 200 to form an integrated integrated chip, such as Figure 1 A magnetic flux concentrator film 120 is provided in each magnetic flux concentrator 100 , and a horizontal Hall element 210 is provided in the horizontal Hall ASIC chip 200 . The magnetic flux concentrator film 120 is located directly above or directly below the horizontal Hall element 210 .

[0054] The two magnetic flux concentrators 100 are defined as a first magnetic flux concentrator 100 and a second magnetic flux concentrator 100 respectively; the first magnetic flux concentrator 100 is wafer-bonded to the upper surface of the Hall ASIC chip 200, and the magnetic flux concentrator film 120 of the first magnetic flux concentrator 100 is located directly above the horizontal Hall element 210; the second magnetic flux concentrator 100 is wafer-bonded to the lower surface of the Hall ASIC chip 200, and the magnetic flux concentrator film 120 of the second magnetic flux concentrator 100 is located directly below the horizontal Hall element 210, as shown in FIG. Figure 2 .

[0055] Each magnetic flux concentrator 100 is also provided with a plurality of first alignment marking points 110, a first oxide layer 130 and a first wafer substrate 140. The first alignment marking points 110 and the magnetic flux concentrating film 120 are respectively arranged on the upper surface of the first wafer substrate 140, and the first oxide layer 130 is arranged on the upper surface of the first wafer substrate 140, the upper surface of the first alignment marking points 110 and the upper surface of the magnetic flux concentrating film 120.

[0056] The Hall ASIC chip 200 is provided with a plurality of second alignment identification points 260, a second wafer substrate 220, a second oxide layer 230, a structural layer 240 and a debugging circuit 250. The second alignment identification points 260, the horizontal Hall element 210 and the debugging circuit 250 are all arranged on the upper surface of the second wafer substrate 220, the structural layer 240 is arranged on the upper surface of the second wafer substrate 220, the upper surface of the second alignment identification points 260 and the upper surface of the horizontal Hall element 210, and the second oxide layer 230 is arranged on the upper surface of the structural layer 240. Figure 3 .

[0057] It should be noted that the plurality of first alignment mark points 110 are distributed in a cross shape on the upper surface of the first wafer substrate 140, and the plurality of second alignment mark points 260 are distributed in a cross shape on the upper surface of the second wafer substrate 220, and the number and position of the first alignment mark points 110 and the second alignment mark points 260 are one-to-one corresponding, so the magnetic flux concentrator 100 and the Hall ASIC chip 200 can be precisely aligned before wafer bonding. In this field, the technical solution of precisely aligning wafer bonding by alignment mark points is a conventional technical operation, which should be known to those skilled in the art and will not be described one by one here.

[0058] The integrated magnetic core of the present invention is packaged with the external Hall package lead frame 500 before use. The maximum width of the groove 510 in the external Hall package lead frame 500 is defined as A, the maximum width of the magnetic flux concentrating film 120 is defined as B, and the maximum width of the horizontal Hall element 210 is defined as C. There exists 30μm≤C≤B≤A≤100μm. Figure 4 .

[0059] It should be noted that the integrated magnetic core of the present invention can be directly used in current detection scenarios after conventional packaging process. The conventional packaging process is to package it with the lead frame 500 for external Hall package. When the lead frame 500 for external Hall package is packaged, the magnetic flux concentrator 100 in the integrated chip is located in the groove 510 area. The maximum width of the magnetic flux concentrator film 120 of the present invention needs to be less than or equal to the maximum width of the groove 510, and greater than or equal to the maximum width of the horizontal Hall element 210. The function of the groove 510 opened in the lead frame 500 for external Hall package is to avoid eddy current effect.

[0060] Compared with the prior art, the flux concentrating film 120 of the present invention can converge magnetic induction lines and amplify the detected magnetic field strength, thereby achieving the same function as a ferromagnetic core, while its size is much smaller than that of a ferromagnetic core. Therefore, the present invention can greatly reduce the size of the integrated magnetic core and achieve miniaturization.

[0061] The present invention achieves micron-level precision alignment of the magnetic flux focusing film 120 and the horizontal Hall element 210 through the second alignment marking point 260 and the first alignment marking point 110. Compared with the prior art assembly alignment of large magnetic core modules, the present invention has greatly improved accuracy.

[0062] It should also be noted that the preparation methods of the magnetic flux concentrator 100 and the Hall ASIC chip 200 of the present invention are common knowledge in the technical field, and the preparation methods of the magnetic flux concentrator 100 and the Hall ASIC chip 200 are not the focus of the present invention, and will not be described in detail here. Moreover, the arrangement of the debugging circuit 250 in the Hall ASIC chip 200 in the second wafer substrate 220 is related to the specific design layout of the Hall ASIC chip 200. The present invention only requires the magnetic flux concentrator 100 and the Hall ASIC chip 200 to be aligned and positioned so that the magnetic flux concentrating film 120 is located on the upper surface and the lower surface of the horizontal Hall element 210. The arrangement of the debugging circuit 250 is not the focus of the present invention, and will not be described in detail here.

[0063] The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element of the present invention is specifically prepared by the following steps:

[0064] S1, aligning the first alignment mark point 110 of the first magnetic flux concentrator 100 with the second alignment mark point 260 of the Hall ASIC chip 200, as shown in FIG. Figure 5 Then, the first oxide layer 130 of the first magnetic flux concentrator 100 is bonded to the second oxide layer 230, so that the first magnetic flux concentrator 100 and the Hall ASIC chip 200 form an integrally connected overall structure, such as Figure 6 and defining the overall structure as a first wafer structure;

[0065] S2, thinning the second wafer substrate 220 in the first wafer structure obtained in S1 to a thickness of 230 Å to 280 Å to obtain a thinned wafer structure, such as Figure 7 ;

[0066] S3, setting a third oxide layer 300 on the surface of the thinned wafer substrate in the thinned wafer structure obtained in S2; specifically, when the temperature inside the furnace tube is 1180° C. to 1250° C. and under oxygen conditions, silicon is grown on the surface of the thinned second wafer substrate 220 in the thinned wafer structure obtained in S2 to form a layer of silicon oxide film, which is the third oxide layer 300, such as Figure 8 , and the thickness of the third oxide layer 300 is about 2800Å to 3200Å;

[0067] S4, aligning the first alignment mark point 110 of the second magnetic flux concentrator 100 with the second alignment mark point 260 in the thinned wafer structure, such as Fig. 9 The third oxide layer 300 is bonded to the first oxide layer 130 of the second magnetic flux concentrator 100, so that the second magnetic flux concentrator 100 and the thinned wafer structure form an integrally connected overall structure, such as Fig.10 and defining the overall structure as a second wafer structure;

[0068] S5, thinning the first wafer substrate 140 and the second wafer substrate 220 in the second wafer structure obtained in S4 respectively to obtain a third wafer structure, such as Fig.11 ;

[0069] S6, forming a through hole 400 through a through silicon via 400 process on one side of the third wafer structure obtained in S5, and then setting a lead in the through hole 400, and the through hole 400 is connected to the surface of the debugging circuit 250, and the lead is electrically connected to the debugging circuit 250 to obtain an integrated chip, such as Fig.12 .

[0070] The material of the first oxide layer 130 and the material of the second oxide layer 230 of the present invention are silicon dioxide or tetraethyl silicate; the first wafer substrate 140 is a silicon-based substrate; the first wafer substrate 140 is a silicon-based substrate, a gallium arsenide substrate or an indium antimonide substrate; the second wafer substrate 220 is a silicon-based substrate, a gallium arsenide substrate or an indium antimonide substrate. The magnetic flux concentrating film 120 is a FeNi-based magnetic flux concentrating film 120, a FeZn-based magnetic flux concentrating film 120, a FeCo-based magnetic flux concentrating film 120 or a FeNiMo-based magnetic flux concentrating film 120.

[0071] The structural layer 240 is at least one of a metal wiring layer, a dielectric layer or a passivation layer; when the structural layer 240 of the present invention is a metal wiring layer, the through hole 400 will be avoided according to the metal wiring position, and will not cause the metal wiring line to be cut off. The through silicon via 400 process of the present invention is a conventional semiconductor process, which should be known to those skilled in the art and will not be described in detail here.

[0072] The debugging circuit 250 of the present invention refers to a signal circuit that realizes the signal amplification, filtering, chopping, clock, storage, etc. of the horizontal Hall element 210. The shape and size of the horizontal Hall element 210 of the present invention include all possible Hall disk shapes that can implement the Hall effect, including but not limited to square, cross, diagonal, polygonal, etc. The magnetic flux concentrating film 120 can be a single-layer film or a multi-layer film, or a composite film layer structure formed by alternating magnetic and non-magnetic layers.

[0073] It should be noted that the preparation method of the present invention can adjust the thickness of the insulating layer between the magnetic flux focusing film 120 and the Hall element through the bonding between the oxide layers. Multiple experiments have proved that its thickness accuracy and consistency of multiple batches are significantly better than the assembly control level of the magnetic core module.

[0074] The integrated chip of the present invention ensures that the intensity of the induced magnetic field of the Hall element is increased, and in cooperation with the lead frame for the Hall package having the groove 510, it can also prevent the strong magnetic field from forming an eddy current effect in the metal frame. In addition, the integrated chip of the present invention integrates a magnetic flux concentrator 100, which can realize the magnetic field concentration and detection of the three-axis magnetic field, and the structure itself can realize the vertical magnetic field detection. For the horizontal magnetic field, the magnetic core magnetic concentration effect can make the parallel magnetic field converge and transform into a vertical magnetic field, thereby realizing the detection of the three-dimensional magnetic field.

[0075] The integrated chip preparation method of the integrated magnetic core and the horizontal Hall element forms an integrated integrated chip through the magnetic flux concentrator 100 and the Hall ASIC chip 200, wherein the magnetic flux concentrator film 120 can converge the magnetic induction lines and amplify the intensity of the detected magnetic field to achieve the same function as the ferromagnetic core. Compared with the prior art, the integrated chip does not need to use a large ferromagnetic core, and can achieve the miniaturization of the Hall current detection chip; the micron-level precision alignment of the real magnetic flux concentrator film 120 and the horizontal Hall element 210 is significantly better than the alignment accuracy of the current magnetic core assembly; it can also achieve the control of the bonding thickness between the magnetic flux concentrator film layer and the Hall element, and the thickness accuracy is significantly better than the control level of the assembly of the large magnetic core module. In addition, the present invention can achieve the thickness adjustment of the insulating layer between the magnetic flux concentrator film 120 and the Hall element. Example

[0076] A method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element, the other features of which are the same as those of Example 1, except that the thickness of the first oxide layer 130 and the second oxide layer 230 is 5000Å, the magnetic flux concentrating film 120 is a FeNi-based magnetic flux concentrating film 120; the material of the first oxide layer 130 and the material of the second oxide layer 230 are both silicon dioxide, the structural layer 240 is a passivation layer, and the first wafer substrate 140 and the second wafer substrate 220 are both silicon-based substrates.

[0077] The preparation method of the integrated chip is prepared by the following steps:

[0078] S1, aligning the first alignment mark point 110 of the first magnetic flux concentrator 100 with the second alignment mark point 260 of the Hall ASIC chip 200, and then bonding the first oxide layer 130 of the first magnetic flux concentrator 100 with the second oxide layer 230, so that the first magnetic flux concentrator 100 and the Hall ASIC chip 200 form an integrally connected overall structure, and the overall structure is defined as a first wafer structure;

[0079] S2, thinning the second wafer substrate 220 in the first wafer structure obtained in S1 to a thickness of 250 Å to obtain a thinned wafer structure;

[0080] S3, growing silicon on the surface of the thinned second wafer substrate 220 in the thinned wafer structure obtained in S2 at a temperature of 1200° C. in the furnace tube under oxygen conditions to form a layer of silicon oxide film, the silicon oxide film being the third oxide layer 300, and the thickness of the third oxide layer 300 being about 3000 Å;

[0081] S4, aligning the first alignment mark point 110 of the second magnetic flux concentrator 100 with the second alignment mark point 260 in the thinned wafer structure, and bonding the third oxide layer 300 with the first oxide layer 130 of the second magnetic flux concentrator 100, so that the second magnetic flux concentrator 100 and the thinned wafer structure form an integrally connected overall structure, and defining the overall structure as a second wafer structure;

[0082] S5, thinning the first wafer substrate 140 and the second wafer substrate 220 in the second wafer structure obtained in S4 respectively to obtain a third wafer structure;

[0083] S6. Form a through hole 400 on one side of the third wafer structure obtained in S5 by a through silicon via 400 process, and then set a lead in the through hole 400, and the through hole 400 is connected to the surface of the debugging circuit 250, and the lead is electrically connected to the debugging circuit 250 to obtain an integrated chip.

[0084] It has been verified through experiments that the integrated chip and the external Hall package lead frame 500 obtained by the preparation method of this embodiment can be directly used in current detection scenarios after undergoing conventional packaging processes, and can also be used for three-axis magnetic field detection. Example

[0085] An integrated chip is prepared by using the integrated magnetic core and horizontal Hall element integrated chip preparation method of embodiment 1 or 2.

[0086] The integrated magnetic core is composed of a magnetic flux concentrator 100 and a Hall ASIC chip 200, wherein the magnetic flux concentrator film 120 can converge magnetic induction lines and amplify the strength of the detected magnetic field, achieving the same function as the ferromagnetic core. Compared with the prior art, the integrated chip does not need to use a large ferromagnetic core, and can achieve the miniaturization of the Hall current detection chip; it can achieve micron-level precision alignment of the magnetic flux concentrator film 120 and the horizontal Hall element 210, which is significantly better than the alignment accuracy of the current magnetic core assembly; it can also achieve the control of the bonding thickness between the magnetic flux concentrator film layer and the Hall element, and the thickness accuracy is significantly better than the control level of the assembly of the large magnetic core module.

[0087] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the present invention.

Claims

1. A method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element, characterized in that: Aligning the two magnetic flux concentrators with the Hall ASIC chip respectively, and then wafer bonding them to the upper and lower surfaces of the Hall ASIC chip respectively to form an integrated chip; A magnetic flux concentrator film is provided in each magnetic flux concentrator, a horizontal Hall element is provided in the horizontal Hall ASIC chip, and the magnetic flux concentrator film is located directly above or directly below the horizontal Hall element; The two magnetic flux concentrators are respectively defined as a first magnetic flux concentrator and a second magnetic flux concentrator; Each magnetic flux concentrator is also provided with a plurality of first alignment marking points, a first oxide layer and a first wafer substrate. The Hall ASIC chip is provided with a plurality of second alignment marking points, a second wafer substrate, a second oxide layer, a structural layer and a debugging circuit. The thickness of the first oxide layer and the second oxide layer is between 1000Å and 1μm; the integrated magnetic core is packaged with an external Hall package lead frame before use, the maximum width of the groove in the external Hall package lead frame is defined as A, the maximum width of the magnetic flux concentrating film is defined as B, the maximum width of the horizontal Hall element is defined as C, and 30μm≤C≤B≤A≤100μm exists; Prepared by the following steps: S1, aligning a first alignment mark point of the first magnetic flux concentrator with a second alignment mark point of the Hall ASIC chip, and then bonding the first oxide layer of the first magnetic flux concentrator with the second oxide layer, so that the first magnetic flux concentrator and the Hall ASIC chip form an integrally connected overall structure, and defining the overall structure as a first wafer structure; S2, thinning the second wafer substrate in the first wafer structure obtained in S1 to obtain a thinned wafer structure; S3, providing a third oxide layer on the surface of the thinned wafer substrate in the thinned wafer structure obtained in S2; S4, aligning the first alignment mark point of the second magnetic flux concentrator with the second alignment mark point in the thinned wafer structure, and bonding the third oxide layer to the first oxide layer of the second magnetic flux concentrator, so that the second magnetic flux concentrator and the thinned wafer structure form an integrally connected overall structure, and defining the overall structure as a second wafer structure; S5, thinning the first wafer substrate and the second wafer substrate in the second wafer structure obtained in S4 respectively to obtain a third wafer structure; S6. Form a through hole on one side of the third wafer structure obtained in S5 by a through silicon via process, and then set a lead in the through hole, and the through hole is connected to the surface of the debugging circuit, and the lead is electrically connected to the debugging circuit to obtain the integrated chip.

2. The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element according to claim 1, characterized in that: The first magnetic flux concentrator wafer is bonded to the upper surface of the Hall ASIC chip, and the magnetic flux concentrator film of the first magnetic flux concentrator is located directly above the horizontal Hall element; The second magnetic flux concentrator wafer is bonded to the lower surface of the Hall ASIC chip, and the magnetic flux concentrator film of the second magnetic flux concentrator is located directly below the horizontal Hall element.

3. The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element according to claim 2, characterized in that: The first alignment marking point and the magnetic flux focusing film are respectively arranged on the upper surface of the first wafer substrate, and the first oxide layer is arranged on the upper surface of the first wafer substrate, the upper surface of the first alignment marking point and the upper surface of the magnetic flux focusing film.

4. The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element according to claim 3, characterized in that: The second alignment marking point, the horizontal Hall element and the debugging circuit are all arranged on the second wafer substrate, the structural layer is arranged on the upper surface of the second wafer substrate, the upper surface of the second alignment marking point and the upper surface of the horizontal Hall element, and the second oxide layer is arranged on the upper surface of the structural layer.

5. The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element according to claim 4, characterized in that: In S2, the second wafer substrate is thinned to a thickness of 230 Å to 280 Å.

6. The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element according to claim 5, characterized in that: Specifically, S3 is as follows: when the temperature inside the furnace tube is 1180°C to 1250°C and under oxygen conditions, silicon is grown on the surface of the thinned second wafer substrate in the thinned wafer structure obtained in S2 to form a layer of silicon oxide film, wherein the silicon oxide film is the third oxide layer, and the thickness of the third oxide layer is 2800Å to 3200Å.

7. The method for preparing an integrated chip of an integrated magnetic core and a horizontal Hall element according to any one of claims 1 to 6, characterized in that: The magnetic flux concentrating film is a FeNi-based magnetic flux concentrating film, a FeZn-based magnetic flux concentrating film, a FeCo-based magnetic flux concentrating film or a FeNiMo-based magnetic flux concentrating film; The material of the first oxide layer and the material of the second oxide layer are silicon dioxide or tetraethyl silicate; The first wafer substrate is a silicon-based substrate; The structural layer is at least one of a metal wiring layer, a dielectric layer or a passivation layer; The first wafer substrate is a silicon-based substrate, a gallium arsenide substrate or an indium antimonide substrate; The second wafer substrate is a silicon-based substrate, a gallium arsenide substrate or an indium antimonide substrate.

8. An integrated magnetic core, characterized in that: The integrated chip is prepared by the integrated chip preparation method according to any one of claims 1 to 7.

Citation Information

Patent Citations

  • Current sensor and preparation method thereof

    CN115166334A