A high-performance MOSFET power device epitaxial design structure, manufacturing method and application

By using a high-concentration arsenic-doped first epitaxial layer and a negative-slope step-type doped second epitaxial layer in the power MOSFET device, the problem of increased on-resistance of traditional devices is solved, and the breakdown voltage and energy conversion efficiency are improved. , reducing manufacturing costs and manufacturing complexity.

CN118412381BActive Publication Date: 2024-10-18华羿微电子股份有限公司
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410874826.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-02
Publication Date
2024-10-18
Estimated Expiration
2044-07-02

AI Technical Summary

Technical Problem

While the breakdown voltage of traditional power MOSFET devices increases, the on-resistance increases, resulting in low DC-DC energy conversion efficiency and high manufacturing costs.

Method used

The first epitaxial layer formed by high-concentration arsenic doping and the second epitaxial layer formed by negative slope stepped doping concentration block substrate diffusion, reduce on-resistance, and increase breakdown voltage.

Benefits of technology

While increasing the breakdown voltage, the on-resistance is reduced, the DC-DC energy conversion efficiency is improved, the manufacturing cost of power devices is reduced, and the manufacturing process is simplified and compatible with traditional processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118412381B_ABST
    Figure CN118412381B_ABST
Patent Text Reader

Abstract

The present invention discloses an epitaxial design structure, a manufacturing method and an application of a high-performance MOSFET power device. The epitaxial design structure includes: a first epitaxial layer formed on a substrate with high-concentration doping, and the first epitaxial layer blocks the diffusion of the substrate; a second epitaxial layer formed on the first epitaxial layer with a negative slope step-type doping concentration through ion implantation. Among them, the high-concentration doping is arsenic doping, and the Rdson of the first epitaxial layer accounts for less than 5% of the total Rdson of the MOSFET power device. The present invention adopts an arsenic-formed first epitaxial layer and a second epitaxial layer formed with a precise negative slope step-type doping concentration, so that the power MOSFET reduces the on-resistance while increasing the BV, improves the DC-DC energy conversion efficiency, and reduces the manufacturing cost of the power device. The disclosed method for manufacturing the second epitaxial layer with a negative slope step-type doping concentration is compatible with the power device manufacturing process and can be applied to trench-type and shielded-gate MOSFET power devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor power devices, and in particular to an epitaxial design structure, a manufacturing method and an application of a high-performance MOSFET power device. Background Art

[0002] Power MOSFET devices are commonly used in switching converters. The size of their losses has a direct impact on the performance and efficiency of switching converters. The losses of power MOSFET devices are mainly composed of conduction losses and switching losses. Usually, power MOSFET devices with low on-resistance and low switching losses are selected. Low on-resistance will lead to low conduction losses, but for traditional power MOSFET devices, the on-resistance Ron∝BV 2.5 , using products with high BV (breakdown voltage), Ron (on-resistance) will also increase synchronously.

[0003] The doping profile of the epitaxial layer is a key parameter that determines the performance of power MOSFET devices. Power MOSFET devices usually use a single epitaxial layer, a double epitaxial layer, or even three epitaxial layers, such as trench MOSFET devices and SGT MOSFET devices. N-type MOSFET devices usually use phosphorus as the epitaxial layer doping. In the epitaxial layer design, each epitaxial layer usually uses a constant doping concentration.

[0004] When a power MOSFET device uses a double epitaxial layer, the second epitaxial layer is usually part of the drift epitaxial layer, which is to further increase the breakdown voltage of the MOSFET. The MOSFET with a higher breakdown voltage will also have a higher Rdson (on-resistance). Summary of the invention

[0005] In response to the above-mentioned problems, the present invention aims to provide a high-performance MOSFET power device epitaxial design structure, manufacturing method and application. The MOSFET power device epitaxial design adopts an arsenic-formed first epitaxial layer and a second epitaxial layer formed by a precise negative slope step-type doping concentration, so that the power MOSFET device reduces the on-resistance while increasing the BV, thereby improving the DC-DC energy conversion efficiency and reducing the manufacturing cost of the power device.

[0006] In order to achieve the above-mentioned object, the technical solution adopted by the present invention is as follows: a high-performance MOSFET power device epitaxial design structure, comprising a substrate, on which a first epitaxial layer and a second epitaxial layer are sequentially arranged from the inside to the outside;

[0007] The first epitaxial layer is formed on the substrate by high-concentration arsenic doping, and the first epitaxial layer blocks the diffusion of the substrate;

[0008] The second epitaxial layer is formed on the first epitaxial layer with a negative slope stepwise doping concentration.

[0009] Preferably, the Rdson of the first epitaxial layer accounts for less than 5% of the total Rdson of the MOSFET power device.

[0010] A method for manufacturing a high-performance MOSFET power device epitaxial design structure comprises the following steps:

[0011] S1. Forming a first epitaxial layer doped with high concentration arsenic, a second epitaxial layer formed by implanting N-type phosphorus ions, and growing a first oxide layer in sequence on a substrate.

[0012] S2, removing the first oxide layer and depositing a hard mask, and then etching a groove on the second epitaxial layer.

[0013] S3, removing the hard mask, growing a sacrificial oxide layer, and after the sacrificial oxide layer is removed, growing a linear oxide layer on the sidewall of the trench and depositing a shielding gate.

[0014] S4, depositing a second oxide layer on the shielding gate and etching to form an IPO.

[0015] S5, growing a third oxide layer on the sidewall of the trench and depositing a control gate, then annealing the control gate, and implanting a P-body implant on the surface of the second epitaxial layer and in the channel region turn-on voltage region of the MOSFET power device to form a P-body region.

[0016] S6. Inject N+ source implant arsenic to form the source of the device, and deposit a layer of BPSG; form a contact hole in the channel area and pass through the source to connect with the P-body area, then inject P-type CT implant, and deposit TI / TIN and metal tungsten as filling contacts to form a contact hole metal layer, and then etch to the BPSG surface.

[0017] S7. Lead the source and P-body region to the front source metal layer through Contact, and then form a back drain metal layer on the back of the MOSFET power device.

[0018] Preferably, N-type phosphorus ion implantation with a gradually decreasing doping concentration is performed in the second epitaxial layer toward the first epitaxial layer to form a second epitaxial layer with a negative slope and stepped doping concentration.

[0019] A method for manufacturing a high-performance MOSFET power device epitaxial design structure as described above is used in manufacturing trench-type and shielded-gate MOSFET power devices.

[0020] The beneficial effects of the present invention are as follows: the present invention adopts a first epitaxial layer formed by high-concentration arsenic doping and a second epitaxial layer formed by precise negative slope step-type doping concentration, so that the power MOSFET device reduces the on-resistance while increasing the BV, improves the DC-DC energy conversion efficiency, and reduces the manufacturing cost of the power device.

[0021] Compared with the structure and manufacturing process of the conventional epitaxial layer with constant doping concentration, the present invention has the following advantages:

[0022] 1. The present invention uses an arsenic-doped buffer layer as the first epitaxial layer on a heavily doped N-type substrate of an N-type MOSFET. Without substantially affecting the overall on-resistance of the power MOSFET device, it can block the influence of changes in the heavily doped concentration of the N-type substrate on the second epitaxial layer, thereby ensuring the stability of the characteristics of the power MOSFET device.

[0023] 2. The present invention adopts a negative slope stepped doping concentration to form the second epitaxial layer. The doping concentration distribution of the second epitaxial layer is precise, which increases BV while reducing Rdson and shortens the R&D cycle.

[0024] 3. The epitaxial design structure manufacturing process of the high-performance power MOSFET device is simple and compatible with the traditional power device manufacturing process.

[0025] 4. Using highly doped arsenic as the first epitaxial layer reduces the width of the transition region between the first and second epitaxial layers, thereby reducing the contribution of the transition region to the on-resistance of the power MOSFET device.

[0026] 5. The present invention uses a negative slope step-type doping concentration type doped epitaxial layer as the second epitaxial layer of the N-type MOSFET. Compared with traditional power devices, the doping concentration of the channel and drift regions is increased, while the doping concentration at the bottom of the trench is reduced. This design structure reduces the resistance of the channel and drift regions, and due to the low doping concentration at the bottom, the charge balance is more sufficient, and the increase in electric field strength leads to an increase in the breakdown voltage in the same space charge region.

[0027] 6. In the bottom area of ​​the trench, the low doping concentration of the second epitaxial layer is conducive to the expansion of the depletion region, thereby reducing the output capacitance Coss and the output charge Qoss, thereby improving the DC-DC switching efficiency of the power MOSFET device.

[0028] 7. The present invention reduces the on-resistance while increasing the BV. Under the same BV, products with the same on-resistance can be designed with a smaller chip area, thereby reducing the manufacturing cost of the power device.

[0029] 8. The method for manufacturing the second epitaxial layer with a negative slope stepped doping concentration disclosed in the present invention is compatible with the traditional manufacturing process of power devices and can be applied to trench type and shielded gate type MOSFET power devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 FIG. 1 is a diagram of step S1 of the method for making the epitaxial design structure of a power device according to the present invention.

[0031] Figure 2 FIG. 1 is a diagram of step S2 of the method for making the epitaxial design structure of a power device according to the present invention.

[0032] Figure 3 FIG. 1 is a diagram of step S3 of the method for making the epitaxial design structure of a power device according to the present invention.

[0033] Figure 4 FIG. 4 is a diagram of step S4 of the method for making the epitaxial design structure of a power device according to the present invention.

[0034] Figure 5 FIG. 5 is a diagram of step S5 of the method for making the epitaxial design structure of a power device according to the present invention.

[0035] Figure 6 FIG. 1 is a diagram of step S6 of the method for making the epitaxial design structure of a power device according to the present invention.

[0036] Figure 7 FIG. 1 is a diagram of step S7 of the method for making the epitaxial design structure of a power device according to the present invention.

[0037] Figure 8 FIG. 1 is a diagram of step S8 of the method for making the epitaxial design structure of a power device according to the present invention.

[0038] Fig. 9 This is a design diagram of epitaxial doping concentration of an N-type MOSFET power device according to an embodiment of the present invention.

[0039] Fig.10 FIG. 1 is a diagram showing the structure of an N-type MOSFET power device according to an embodiment of the present invention.

[0040] Fig.11 This is an electric field line diagram of an N-type MOSFET power device when it breaks down according to an embodiment of the present invention.

[0041] Fig.12 It is a comparison diagram of the net doping distribution curve and electric field distribution curve of the novel epitaxial structure of the N-type MOSFET power device according to the embodiment of the present invention and the traditional epitaxial structure.

[0042] In the figure: 1-first oxide layer; 2-hard mask; 3-trench; 4-linear oxide layer (lineroxide); 5-shielding gate (poly 1 or source poly); 6-IPO (inter poly oxide); 7-third oxide layer (gate oxide); 8-control gate (gate poly); 9-P-body region (P-type Body implant); 10-N+ sourceimplant arsenic; 11-BPSG (Boro-phospho-silicate Glass); 12-P-type CT implant; 13-CT (Contact); 14-front source metal layer (top metal); 15-back drain metal layer (back metal). DETAILED DESCRIPTION

[0043] In order to enable those skilled in the art to better understand the technical solution of the present invention, the technical solution of the present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0044] The present invention provides a high-performance MOSFET power device epitaxial design structure, referring to the attached Figures 1 to 8 As shown, there is a substrate, on which a first epitaxial layer and a second epitaxial layer are arranged in sequence from the inside to the outside.

[0045] The first epitaxial layer is formed on the substrate with high concentration of arsenic doping. The arsenic doped first epitaxial layer is not a drift layer, and its purpose is to block the diffusion from the heavily doped N-type substrate. The arsenic doping concentration is high enough so that it does not affect the Rdson of the MOSFET power device. The Rdson of the first epitaxial layer accounts for less than 5% of the total Rdson of the power device.

[0046] The thickness of the first epitaxial layer is determined by the thermal process of the MOSFET manufacturing process. Since the arsenic diffusion coefficient is low, using highly doped arsenic as the first epitaxial layer reduces the width of the transition region with the second epitaxial layer described later, thereby reducing the contribution of this transition region to the device on-resistance.

[0047] The second epitaxial layer is formed on the first epitaxial layer by ion implantation with a negative slope stepwise doping concentration. Note: The negative slope is the slope of the doping concentration gradually decreasing from the outside of the second epitaxial layer toward the first epitaxial layer. The second epitaxial layer formed with a negative slope stepwise doping concentration can form the required doping concentration morphology by precise high-energy ion implantation to achieve a high breakdown voltage and low internal resistance (compared with the traditional epitaxial layer with a constant doping concentration). The concentration distribution of the negative slope stepwise doping concentration is: the doping concentration is high on the surface of the second epitaxial layer, and as it goes deeper from the surface of the second epitaxial layer to the inside of the second epitaxial layer, the doping concentration gradually decreases until it reaches the top of the first epitaxial layer. The second epitaxial layer with a negative slope stepwise doping concentration has a high breakdown voltage, low internal resistance and low output capacitance Coss, while improving the energy conversion efficiency of MOSFET devices in DC-DC, and the low internal resistance can make the chip area design of the same BV product smaller, thereby reducing the manufacturing cost of the wafer.

[0048] The present invention also provides a method for manufacturing a high-performance MOSFET power device epitaxial design structure, comprising the following steps:

[0049] S1, such as Figure 1-2 As shown, a first epitaxial layer doped with high concentration arsenic, a second epitaxial layer formed by N-type phosphorus ion implantation, and a first oxide layer are sequentially formed on the substrate. Among them, the arsenic doping is preferably 4e 18 -8e 18 cm -3 , the doping concentration will not affect the Rdson of the MOSFET power device; a first oxide layer 1 of 250A, the first oxide layer 1 serves as a barrier and protective layer for ion implantation of the second epitaxial layer in step S2 to prevent damage to the second epitaxial layer during ion implantation.

[0050] S2, ion implantation with gradually decreasing doping concentration is performed in the direction from the second epitaxial layer to the first epitaxial layer. The ion implantation is P-type phosphorus ion implantation, energy: 300kev~1Mev; concentration: 1e 12 ~1e 13 cm -3 .

[0051] S3, such as Figure 3 As shown, the first oxide layer 1 is removed, and a hard mask 2 is deposited as a barrier layer for subsequent trench 3 etching.

[0052] Next, the position of the trench 3 is determined by the photoresist and the hard mask 2. After the exposed hard mask 2 is etched away, the photoresist is removed, and the trench 3 is formed by etching on the epitaxial layer using the hard mask 2 as an etching barrier.

[0053] S4, such as Figure 4As shown, the hard mask 2 is removed by wet etching, and then a sacrificial oxide layer is grown by thermal oxidation and then removed to form a clean silicon surface on the side wall of the trench. Thereafter, a linear oxide layer 4 is grown on the side wall of the trench 3 by low-temperature thermal oxidation, and a shielding gate 5 is deposited in turn and etched back by dry etching.

[0054] S5, such as Figure 5 As shown, a second oxide layer is continuously deposited on the shielding gate 5 and is etched back by dry etching to form IPO6.

[0055] S6, such as Figure 6 As shown, a third oxide layer 7 is grown on the side wall of the trench 3, and a control gate 8 is deposited in turn and then subjected to chemical mechanical polishing (CMP). After that, an annealing process is performed on the control gate 8, and a P-body implant is implanted on the surface of the second epitaxial layer and in the channel region of the MOSFET power device to form a P-body region 9, which is preferably boron, with an energy of 80-300kev and a concentration of 1e 12 ~2e 13 cm -3 .

[0056] S7, such as Figure 7 As shown, an N-type N+ source implant arsenic 10 is implanted to form the source of the device; a layer of BPSG11 is deposited as an isolation layer between the surface of the second epitaxial layer and the metal (front source metal layer 14); a contact hole is formed in the channel area using a CT mask photoresist and passes through the N+ source implant arsenic 10 area to connect with the P-body area 9, and a P-type CT implant 12 is formed by high-concentration ion implantation to form a good ohmic contact, and then TI / TIN and CT (Contact) 13 are deposited as filling contacts to form a contact hole metal layer, which is then etched back to the surface of BPSG11 by dry etching.

[0057] S8, such as Figure 8 As shown, the source and P-body region 9 are led out to the front source metal layer 14 through contacts using photoresist of a metal mask, and then a back drain metal layer 15 is formed on the back of the device through thinning and back gold processes.

[0058] The source and the P-body region 9 are led out to the front source metal layer 14 through contacts, and then a back drain metal layer 15 is formed on the back of the MOSFET power device through thinning and back gold processes.

[0059] In addition to performing N-type phosphorus ion implantation to form the second epitaxial layer in step S2, the present application can also preferably perform step-type phosphorus ion implantation in step S2, and then form the second epitaxial layer through an N-type phosphorus ion implantation process with multiple thermal annealing, or perform phosphorus element step concentration implantation before step S6 body implant, and then perform bodyimplant and other processes to form this negative slope step epitaxial layer. And this application mainly provides the concept principle of this new epitaxial layer and several manufacturing methods, and the other manufacturing methods will not be repeated one by one.

[0060] The method for manufacturing the epitaxial design structure of the high-performance MOSFET power device disclosed in the present invention can be applied to manufacturing trench-type and shielded-gate MOSFET power devices. Example

[0061] like Fig. 9 As shown in the figure, it is an example of the present invention using an arsenic-doped buffer layer to form a first epitaxial layer and a negative slope step-type doping concentration to form a second epitaxial layer. The arsenic-doped buffer layer is used as the first epitaxial layer on the heavily doped N-type substrate of the N-type MOSFET. The purpose of this layer is to block the diffusion from the heavily doped N-type substrate, and the Rdson of the first epitaxial layer accounts for less than 5% of the total Rdson of the power device (according to the following implementation results, for a BV 38V device, the total RSP is 5.28mΩ·mm 2 , the RSP of the arsenic-doped epitaxial layer is 0.21 mΩ· mm 2 , accounting for about 4%). As the diffusion capacity of arsenic itself is low, it will not affect the concentration and thickness of the second epitaxial layer. At the same time, this buffer layer can help the second epitaxial layer block the diffusion from the heavily doped N-type substrate, ensuring the stability of the device. And using highly doped arsenic as the first epitaxial layer reduces the width of the transition zone between the first epitaxial layer and the second epitaxial layer, thereby reducing the contribution of this transition zone to the on-resistance of the device.

[0062] The second epitaxial layer is doped as Fig. 9 The negative slope step shown in the figure increases the doping concentration of the channel and drift region and reduces the doping concentration at the bottom of the trench compared to the traditional power device. This design structure reduces the resistance of the channel and drift region, and due to the low doping concentration at the bottom of the second epitaxial layer, the charge balance is more sufficient, the electric field strength of the space charge region is improved, and the breakdown voltage is increased. The low doping concentration at the bottom of the trench 3 is conducive to the extension of the depletion layer, reducing the output capacitance of the MOSFET and improving the DC-DC energy conversion efficiency of the device.

[0063] like Figures 10-11As shown in FIG. 1 , the N-type MOSFET device structure used in the simulation verification of the present invention and the electric field distribution diagram of the device at critical breakdown, wherein the integral area under the electric field curve represents the breakdown voltage of the device.

[0064] like Fig.12 As shown, it is the simulation comparison result of the new epitaxial structure designed by the present invention and the traditional epitaxial structure on the doping concentration and electric field distribution, wherein:

[0065] Dark solid line: negative slope stepwise doping concentration shaping doping curve of the second epitaxial layer;

[0066] Light solid line: doping curve of constant concentration epitaxial layer;

[0067] Dark dashed line: electric field distribution curve of the second epitaxial layer shaped by negative slope stepwise doping concentration;

[0068] Light dashed line: electric field distribution curve of constant concentration epitaxial layer.

[0069] The simulated electric field curve shows that the negative slope step epitaxial doping has a higher breakdown voltage than the constant epitaxial doping, and because the negative slope step doping concentration shapes the second epitaxial layer with a higher doping concentration than the constant doping epitaxial layer, the negative slope step epitaxial doping device has a lower Rdson.

[0070] The simulation results show that the BV of the negative slope step doped epitaxial layer is 38.2V and the Rsp is 5.27mOhm-mm2; while the BV of the constant doped epitaxial layer is 36.5V and the Rsp is 5.85mOhm-mm2. From the simulation results, the negative slope step epitaxial doping has a BV 1.7V higher than the constant epitaxial doping, and the Rsp is reduced by 9.9%, that is, the Rdson is reduced by 9.9%. Therefore, the negative slope step epitaxial layer doping distribution can provide high BV and low Rdson. Low Rdson means that a smaller chip size can be designed for the same Rdson device, which means reducing the manufacturing cost of power devices.

[0071] The above shows and describes the basic principle, main features and advantages of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention claimed.

Claims

1. A high-performance MOSFET power device epitaxial design structure, comprising a substrate, It is characterized in that A first epitaxial layer and a second epitaxial layer are sequentially arranged on the substrate from bottom to top; The first epitaxial layer is formed on the substrate by high-concentration arsenic doping, and the first epitaxial layer blocks the diffusion of the substrate; The second epitaxial layer is formed on the first epitaxial layer with a negative slope doping concentration; the negative slope is a slope in which the doping concentration gradually decreases from the outside of the second epitaxial layer toward the first epitaxial layer; The Rdson of the first epitaxial layer accounts for less than 5% of the total Rdson of the MOSFET power device.

2. A method for manufacturing a high performance MOSFET power device epitaxial design structure according to claim 1, It is characterized in that The following steps are involved: S1, sequentially forming a first epitaxial layer doped with high concentration arsenic, a second epitaxial layer formed by N-type phosphorus ion implantation, and a first oxide layer on a substrate; S2, removing the first oxide layer and depositing a hard mask, and then etching a groove on the second epitaxial layer; S3, removing the hard mask, growing a sacrificial oxide layer, and after the sacrificial oxide layer is removed, growing a linear oxide layer on the sidewall of the trench and depositing a shielding gate; S4, depositing a second oxide layer on the shielding gate and etching to form an IPO; S5, growing a third oxide layer on the sidewall of the trench and depositing a control gate, then annealing the control gate, and implanting a P-body implant on the surface of the second epitaxial layer and in the channel region of the MOSFET power device as a turn-on voltage region to form a P-body region; S6, implanting N+ source implant arsenic to form the source of the device, and depositing a layer of BPSG; forming a contact hole in the channel area and passing through the source to connect to the P-body area, then implanting a P-type CT implant, and depositing TI / TIN and metal tungsten as filling contacts to form a contact hole metal layer, and then etching to the BPSG surface; S7. Lead the source and P-body region to the front source metal layer through Contact, and then form a back drain metal layer on the back of the MOSFET power device.

3. A method for manufacturing a high performance MOSFET power device epitaxial design structure according to claim 2, Features: N-type phosphorus ion implantation with a gradually decreasing doping concentration is performed in the second epitaxial layer toward the first epitaxial layer to form a second epitaxial layer with a negative slope stepwise doping concentration.

4. An application of the method for manufacturing the epitaxial design structure of a high-performance MOSFET power device as claimed in claims 2 to 3 in manufacturing trench-type and shielded-gate MOSFET power devices.

Citation Information

Patent Citations

  • Semiconductor device with power transistor cells and lateral transistors and method of manufacturing

    CN105226020A

  • Up-diffusion suppression in a power mosfet

    US20220020851A1