A method for increasing the height of a soldering pad and a method for manufacturing a display panel
By inkjet printing conductive pillars on the substrate and adding an insulation layer and a welding reinforcement layer, the problem of pad height and stability is solved, efficient pad formation and high-quality welding are achieved, and the production efficiency and density of the display panel are improved. .
Patent Information
- Application Number
- CN202410901039.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-05
AI Technical Summary
In the production of high-pixel-density LED display panels, it is difficult to achieve sufficient height and stability of the pads, resulting in short circuits or breakage of conductive pillars during welding. In addition, the traditional pad forming method is long and unstable, affecting industrialization.
Inkjet printing is used to form conductive pillars on the substrate, and new pads are formed through the insulation layer and welding reinforcement layer to improve the height and stability of the pad, ensure welding strength and prevent oxidation.
It achieves the rapid and stable formation of bonding pads higher than the pixel drive circuit or display chip, ensuring high-quality welding, improving the production efficiency and density of display panels, and reducing costs.
Smart Images

Figure CN118431095B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a pad height increasing method and a display panel manufacturing method, belonging to the technical field of display panel manufacturing. Background Art
[0002] There are currently two methods for making active Micro LED displays: the first is to make a TFT substrate first, expose the pads on the top layer, and then transfer a large number of Micro LED display chips to the TFT substrate, and then package them after welding, testing, and repair. This process prolongs the panel preparation time and increases the cost. The second method is more suitable for high-resolution display screens, such as Figure 1 As shown, a pixel driving circuit 81 (usually a thin film transistor, TFT) and a driving pad 82 electrically connected to the pixel driving circuit 81 are made on the driving substrate 8, and a display chip 91 and a chip pad 92 electrically connected to the display chip 91 are made on the light-emitting substrate 9, and then the driving pad 82 and the chip pad 92 are welded and packaged point-to-point. This process can produce a high-density LED display panel. At present, the second solution has been used on small-sized silicon-based processes, while it is currently in the exploration stage on large-sized glass substrates. The main difficulty lies in the difficulty of welding.
[0003] In the field of seamless splicing of high-pixel density LED display panels, the maximum width of the pad is smaller than the width of the display chip. If the dual solder paste pad welding method is used to complete the welding between the driving substrate and the light-emitting substrate, at high pixel density, adjacent pads are prone to short circuits due to the extrusion of solder paste during welding.
[0004] Ideally, if Figure 1 As shown in situation a, when the driving pad 82 is higher than the pixel driving circuit 81 and the chip pad 92 is higher than the display chip 91, the driving substrate 8 and the light-emitting substrate 9 can form a good electrical connection after welding.
[0005] But in fact, in high-precision display panels, since LED devices have a micron-level height, if there is no supporting structure, the micron-level thin and tall metal conductive structure is easy to break and is also easy to oxidize due to exposure to air. Figure 1 As shown in case b, the pixel driving circuit 81 and the display chip 91 have a large height (or thickness). When the driving pad 82 is shorter than the pixel driving circuit 81 and the chip pad 92 is shorter than the display chip 91, after the driving substrate 8 and the light-emitting substrate 9 are welded, the driving pad 82 may not be connected to the chip pad 92. In order to achieve reliable electrical connection, the pad should have a high height. However, the metal column forming the pad is difficult to form independently under the microstructure and is easily oxidized. The traditional method of growing the pad, such as electroplating and sputtering, takes too long to make a pad with a large height, and the pad quality is unstable, which is not conducive to industrialization. Summary of the invention
[0006] In order to overcome the shortcomings of the prior art, the present invention provides a method for increasing the height of a solder pad and a method for manufacturing a display panel, which can efficiently manufacture a solder pad with a large height.
[0007] The technical solution adopted by the present invention to solve the technical problem is:
[0008] In a first aspect, the present application provides a method for increasing the height of a pad, comprising the following steps:
[0009] forming a first insulating layer on the substrate except for the initial pad, so that a first hole leading to the initial pad exists in the first insulating layer;
[0010] Inkjet printing a first conductive material into the first hole to form a conductive column in the first hole;
[0011] forming a second insulating layer on the substrate except for the conductive pillar, so that a second hole leading to the conductive pillar exists in the second insulating layer;
[0012] A welding reinforcement layer is formed in the second hole, and the initial welding pad, the conductive column, and the welding reinforcement layer are sequentially connected to form a new welding pad.
[0013] The pad heightening method provided by the present application forms a conductive column by inkjet printing in the first hole, which can quickly increase the initial pad at a speed much higher than that of electroplating or sputtering metal, and finally cap the conductive column with a welding reinforcement layer, which not only protects the conductive column, but also ensures the welding strength required when making a display panel, wherein the first insulating layer has a good supporting effect on the conductive column formed by printing, and the second insulating layer also has a good supporting effect on the welding reinforcement layer, so that the new pad formed by sequentially connecting the initial pad, the conductive column, and the welding reinforcement layer is firm and reliable. While improving the stability of the conductive column and the pad, the present invention protects the conductive column and avoids panel display defects caused by oxidation damage to the conductive column.
[0014] Furthermore, the step of forming a first insulating layer on the substrate except for the initial pad comprises:
[0015] Applying a first photoresist on the surface of the substrate, and developing the area except the initial pad to expose the surface;
[0016] Applying a first insulating material on the surface of the substrate and curing the first insulating material;
[0017] dry-etching the first insulating material on the initial pad to expose the first photoresist;
[0018] The first photoresist is washed away to obtain the first insulating layer having the first hole.
[0019] Furthermore, the step of forming a welding reinforcement layer in the second hole comprises:
[0020] Coating a second photoresist on the surface of the substrate, and developing toward the conductive pillars to expose the conductive pillars;
[0021] sputtering a metal material onto the surface of the substrate;
[0022] The second photoresist is removed to obtain the welding strengthening layer higher than the second hole. At this time, the initial pad, the conductive column, and the welding strengthening layer are sequentially connected to form a convex pad.
[0023] Furthermore, the step of forming a welding reinforcement layer in the second hole comprises:
[0024] Coating a second photoresist on the surface of the substrate, and developing toward the conductive pillars to expose the conductive pillars;
[0025] Applying a layer of second conductive material with equal thickness to the surface of the substrate and curing the layer;
[0026] The second photoresist is removed to obtain the welding strengthening layer which is concave downwards. At this time, the initial pad, the conductive column and the welding strengthening layer are sequentially connected to form a concave pad.
[0027] Furthermore, the height of the initial pad is less than 5 μm, and the height of the welding reinforcement layer is less than 5 μm.
[0028] Furthermore, the total thickness of the initial pad and the welding reinforcement layer is greater than one tenth of the height of the conductive column, which is beneficial to ensure the structural stability of the new pad.
[0029] Furthermore, the first conductive material is UV ink dispersed with nano copper-chromium alloy particles.
[0030] In a second aspect, the present application provides three display panel manufacturing methods.
[0031] The first one includes the following steps:
[0032] Take a driving substrate, including a pixel driving circuit and a driving pad, take a light-emitting substrate, including a display chip and a chip pad, and the positions of the driving pad and the chip pad are distributed in a mirror image;
[0033] The driving pad and / or the chip pad is used as an initial pad, at least one of the driving substrate and the light-emitting substrate is formed into a new pad according to the pad heightening method described in the first aspect, and the driving pad is aligned and welded with the chip pad to obtain the display panel.
[0034] The second method includes the following steps:
[0035] Take a driving substrate, including a pixel driving circuit and a driving pad, and take a light-emitting substrate, including a display chip and a chip pad;
[0036] Punching holes on the light-emitting substrate, and connecting the chip pads to the back side of the light-emitting substrate to form back side pads, wherein the driving pads have the same position distribution as the back side pads;
[0037] The driving pad is used as an initial pad, and a new pad is formed on the driving substrate according to the pad heightening method described in the first aspect. The driving pad is aligned and welded with the back pad to obtain the display panel.
[0038] The third method includes the following steps:
[0039] Take a driving substrate, including a pixel driving circuit and a driving pad, take a light-emitting substrate, including a display chip and a chip pad, and the positions of the driving pad and the chip pad are distributed in a mirror image;
[0040] The driving pad and the chip pad are used as initial pads, one of the driving substrate and the light-emitting substrate is formed into a convex pad according to the above-mentioned pad raising method, and the other is formed into a concave pad matching the convex pad according to the above-mentioned pad raising method, and the convex pad is aligned and welded with the concave pad to obtain the display panel.
[0041] The beneficial effects of the present invention are as follows: the present application only requires a very thin initial pad on the substrate, so that the initial pad can be efficiently increased, and a new pad that is higher than the pixel driving circuit or higher than the display chip can be quickly formed to make up for the height difference. The first insulating layer and the second insulating layer can support the new pad to prevent the diffusion of conductive materials, which is beneficial to increase each pad with high precision, so that high-quality welding can be achieved between the driving pad and the chip pad when manufacturing the display panel.
[0042] Other features and advantages of the present application will be described in the following description, and partly become apparent from the description, or understood by practicing the present application. The purpose and other advantages of the present application can be realized and obtained by the structures particularly pointed out in the written description and the drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1 This is a comparison chart of the effect of pad height on welding effect when bonding the driving substrate to the light-emitting substrate.
[0044] Figure 2 It is a schematic diagram of the steps of a method for increasing the height of a pad provided in an embodiment of the present application.
[0045] Figure 3 The figure is a schematic diagram of the steps of forming a first insulating layer on a substrate.
[0046] Figure 4 It is a schematic diagram of the steps of forming a convex pad in the second hole.
[0047] Figure 5 is a schematic diagram of the steps of forming a concave pad in the second hole.
[0048] Figure 6 It is a schematic diagram of the steps of the first display panel manufacturing method provided in an embodiment of the present application.
[0049] Figure 7 It is a schematic diagram of the steps of a second display panel manufacturing method provided in an embodiment of the present application.
[0050] Figure 8 It is a schematic diagram of the steps of a third display panel manufacturing method provided in an embodiment of the present application.
[0051] Figure numerals: 1. substrate; 11. transistor; 12. initial pad; 121. conductive column; 122. welding reinforcement layer; 128. metal layer; 129. second conductive material layer; 18. second hole; 19. first hole; 21. first photoresist; 22. second photoresist; 31. first insulating layer; 32. second insulating layer; 8. driving substrate; 81. pixel driving circuit; 82. driving pad; 9. light-emitting substrate; 91. display chip; 92. chip pad; 93. back pad. DETAILED DESCRIPTION
[0052] The embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0053] The disclosure below provides many different embodiments or examples to implement different structures of the present invention. In order to simplify the disclosure of the present invention, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present invention. In addition, the present invention can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed.
[0054] The present application aims to solve the problem of forming a large height (or thickness) pad, and the main purpose is to improve the processing rate and strength of the large height pad to prevent breakage during welding.
[0055] Reference Figure 1, the driving substrate 8 has a pixel driving circuit 81 and a driving pad 82, and the light-emitting substrate 9 has a display chip 91 and a chip pad 92. The pixel driving circuit 81 can adopt a bottom gate structure. For the convenience of description, in this application, the original driving pad 82 on the driving substrate 8 and the original chip pad 92 on the light-emitting substrate 9 are collectively referred to as initial pads; in the active Micro LED display, the pixel driving circuit 81 is a thin film transistor (TFT), and the display chip 91 is a semiconductor light-emitting diode (essentially a transistor), so the pixel driving circuit 81 and the display chip 91 are collectively referred to as transistors.
[0056] Reference Figure 2 The present invention provides a method for increasing the height of a pad, comprising the following steps:
[0057] S1 : forming a first insulating layer 31 on the substrate 1 except for the initial pad 12 , so that a first hole 19 leading to the initial pad 12 exists in the first insulating layer 31 .
[0058] S2 : inkjet printing a first conductive material into the first hole 19 to form a conductive column 121 in the first hole 19 .
[0059] S3: forming a second insulating layer 32 on the substrate 1 except for the conductive pillar 121 , so that a second hole 18 leading to the conductive pillar 121 exists in the second insulating layer 32 .
[0060] S4: forming a welding reinforcement layer 122 in the second hole 18, and connecting the initial pad 12, the conductive column 121, and the welding reinforcement layer 122 in sequence to form a new pad.
[0061] The overall height of the new pad is not limited by the height of the transistor 11, and the molding speed is fast. The first insulating layer 31 and the second insulating layer 32 structure can provide sufficient support strength to ensure normal welding in the later stage. In addition, the first insulating layer 31 can prevent the diffusion of the first conductive material, and the second insulating layer 32 can prevent the diffusion of the material of the welding reinforcement layer 122. Therefore, the new pad can be molded with high precision, which is conducive to the efficient production of high-density display arrays.
[0062] The first conductive material is an ink dispersed with nano-metal particles, which can quickly print out conductive columns to fill the first holes. At the same time, the insulating layer is used to support the conductive columns, and small-sized, high-(thick) slender conductive columns can be efficiently and quickly produced to avoid short circuits and conductive column breakage, while improving the display panel resolution and pixel density, and improving the panel splicing effect. Preferably, the first conductive material is a UV ink dispersed with nano-copper-chromium alloy particles, with a curing temperature below 150°C, and has high strength and is corrosion-free after UV curing.
[0063] The height of the conductive column is between 1um and 50um, the width (bottom diameter) of the conductive column is between 1um and 50um, and the ratio of height to width is between 0.3 and 50.
[0064] Reference Figure 3 , the detailed steps of step S1 include:
[0065] S11: coating a first photoresist 21 (positive photoresist) on the surface of the substrate 1, and developing the area except the initial pad 12 to expose the surface, and the first photoresist 21 is retained on the initial pad.
[0066] S12: coating a first insulating material on the surface of the substrate 1 and curing the first insulating material.
[0067] S13 : dry-etching the first insulating material on the initial pad 12 to expose the first photoresist 21 ; washing away the first photoresist 21 to obtain a first insulating layer 31 having a first hole 19 .
[0068] The formation principle of the first insulating layer 31 is to use a compound containing a highly chemically active component as a precursor, uniformly mix these raw materials in the liquid phase, and perform hydrolysis and condensation chemical reactions to form a stable transparent sol system in the solution. After aging, the sol particles slowly polymerize to form a gel with a three-dimensional network structure. The gel network is filled with a solvent that has lost its fluidity. After drying and sintering and solidification, an insulating material can be prepared. Among them, the first insulating material can be Al 2 O 3 , ZrO 2 , HfO 2 , SiO 2 etc.; the first insulating material is coated by a scraper, so that the first insulating material can completely cover the surface of the substrate 1, and the top surface is flat (such as Figure 3 Similarly, the second insulating layer 32 having the second hole 18 can be formed by a similar method, and the material forming the second insulating layer 32 can be Al 2 O 3 , ZrO 2 , HfO 2 , SiO 2 Etc.; coating can also be completed by blade coating.
[0069] Reference Figure 4 , the detailed steps of step S4 may include:
[0070] S411 : coating the second photoresist 22 on the surface of the substrate 1 , developing toward the conductive pillars 121 to expose the conductive pillars 121 , and retaining the second photoresist 22 on the second insulating layer 32 .
[0071] S412 : sputtering metal material onto the surface of the substrate 1 to form a metal layer 128 .
[0072] S413 : removing the second photoresist 22 to obtain a welding strengthening layer 122 higher than the second hole 18 .
[0073] The new pad thus formed is a convex pad.
[0074] Reference Figure 5 , the detailed steps of step S4 may include:
[0075] S421 : coating the second photoresist 22 on the surface of the substrate 1 , developing toward the conductive pillars 121 to expose the conductive pillars 121 , and retaining the second photoresist 22 on the second insulating layer 32 .
[0076] S422 : coating a layer of second conductive material with equal thickness onto the surface of the substrate 1 and curing the layer to form a second conductive material layer 129 .
[0077] S423: removing the second photoresist 22 to obtain a soldering strengthening layer 122 that is recessed downward.
[0078] The new pad thus formed is a concave pad. Among them, the coating method of step S422 is slit coating, so that the second insulating layer 32 and the second hole 18 have the same thickness of the second conductive material, and the thickness of the second conductive material layer 129 is less than the depth of the second hole 18. The principle of coating and curing the second conductive material in step S422 is the same as the principle of inkjet printing in step S2, that is, nano-metal particles are dispersed in the solvent, and then low-temperature sintering technology is used to form a solid. The second conductive material can be the same as the first conductive material. Preferably, the second conductive material is nickel, which has both easy solderability and conductivity, which is conducive to ensuring that the pads of the drive substrate and the pads of the light-emitting substrate are more closely connected.
[0079] Preferably, the height of the initial pad is less than 5 μm, and the height of the welding reinforcement layer is less than 5 μm. When manufacturing the light-emitting substrate and the driving substrate, it is only required to form a very thin initial pad. When finally forming the welding reinforcement layer, it is also only necessary to form a very thin welding reinforcement layer. The height of the new pad is mainly provided by a section of the conductive column 121 in the middle, and a new pad higher than the transistor 11 can be formed at high speed. In addition, under the support, surrounding and protection of the bottom initial pad 12, the top welding reinforcement layer 122, the first insulating layer 31 and the second insulating layer 32, the conductive column 121 generated at high speed also has good structural strength, which can ensure the subsequent welding is firm. Furthermore, the total thickness of the initial pad and the welding reinforcement layer is greater than one tenth of the height of the conductive column, which is conducive to ensuring the structural stability of the new pad.
[0080] Reference Figure 6 The present application embodiment provides a first display panel manufacturing method, comprising the following steps:
[0081] Take a driving substrate 8 including a pixel driving circuit 81 and a driving pad 82 , take a light-emitting substrate 9 including a display chip 91 and a chip pad 92 , and the positions of the driving pad 82 and the chip pad 92 are distributed in a mirror image.
[0082] A new pad is formed on at least one of the driving substrate and the light-emitting substrate according to the above-mentioned pad heightening method, and the driving pad 82 and the chip pad 92 are aligned and welded to obtain a display panel.
[0083] like Figure 6 In the embodiment shown, both the driving substrate 8 and the light-emitting substrate 9 have pad heightening. In fact, as long as the total height of the driving pad 82 and the chip pad 92 is greater than the total height of the pixel driving circuit 81 and the display chip 91, only one of the driving substrate 8 and the light-emitting substrate 9 may be heightened. Preferably, in order to simplify the process design and facilitate engineering implementation, since the thickness of the LED (display chip 91) is actually much greater than the thickness of the TFT (pixel driving circuit 81), only the light-emitting substrate 9 can be heightened to a new pad, and only the initial pad is retained at the driving substrate end, so as to prevent displacement during welding.
[0084] Reference Figure 7 The present application embodiment provides a second display panel manufacturing method, comprising the following steps:
[0085] Take a driving substrate 8 including a pixel driving circuit 81 and a driving pad 82 , and take a light-emitting substrate 9 including a display chip 91 and a chip pad 92 .
[0086] Holes are punched on the light-emitting substrate 9, and the chip pads are wired to the back side of the light-emitting substrate to form back side pads 93. The driving pads 82 and the back side pads 93 have the same position distribution.
[0087] A new pad is formed on the driving substrate 8 according to the above-mentioned pad heightening method, and the driving pad 82 and the back pad 93 are aligned and welded to obtain a display panel.
[0088] Reference Figure 8 The present application embodiment provides a third display panel manufacturing method, comprising the following steps:
[0089] Take a driving substrate 8 including a pixel driving circuit 81 and a driving pad 82 , take a light-emitting substrate 9 including a display chip 91 and a chip pad 92 , and the positions of the driving pad 82 and the chip pad 92 are distributed in a mirror image.
[0090] One of the driving substrate 8 and the light-emitting substrate 9 is formed into a convex pad according to the above-mentioned pad raising method, and the other is formed into a concave pad matching the convex pad according to the above-mentioned pad raising method. The convex pad and the concave pad are aligned and welded to obtain a display panel.
[0091] like Figure 8 In the embodiment shown, the driving substrate 8 forms a concave pad, and the light-emitting substrate 9 forms a convex pad. The concave and convex matching can further improve the welding strength, and it is easier to align the pads when bonding the driving substrate 8 and the light-emitting substrate 9, and the contact between the pads is tighter. Preferably, in the concave pad, the concave depth is greater than one-third of the maximum thickness of the welding reinforcement layer 122, which is conducive to concave and convex alignment and ensures welding quality and bonding strength.
[0092] The present invention adopts inkjet printing to prepare conductive columns and insulating layers to ensure the stability of the conductive column structure, which can be used to manufacture high-density sandwich LED display panels, improve the production efficiency of display panels, reduce the production cost of LED display screens, save process time, improve production efficiency, and facilitate the efficient and high-quality production of high-pixel resolution Micro LED display screens.
[0093] In the description of this specification, the description with reference to the terms "one embodiment", "certain embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0094] The above is a preferred embodiment of the present invention. It should be pointed out that a person skilled in the art can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications are also considered to be within the scope of protection of the present invention.
Claims
1. A method for increasing the height of a pad. It is characterized in that The following steps are involved: forming a first insulating layer on the substrate except for the initial pad, so that a first hole leading to the initial pad exists in the first insulating layer; Inkjet printing a first conductive material into the first hole to form a conductive column in the first hole; The height of the conductive column is between 1um and 50um, the width of the conductive column is between 1um and 50um, and the ratio of height to width is between 0.3 and 50; forming a second insulating layer on the substrate except for the conductive pillar, so that a second hole leading to the conductive pillar exists in the second insulating layer; forming a welding reinforcement layer in the second hole, wherein the initial welding pad, the conductive column and the welding reinforcement layer are sequentially connected to form a new welding pad; The step of forming a first insulating layer on the substrate except for the initial pad comprises: Applying a first photoresist on the surface of the substrate, and developing the area except the initial pad to expose the surface; Applying a first insulating material on the surface of the substrate and curing the first insulating material; dry-etching the first insulating material on the initial pad to expose the first photoresist; The first photoresist is washed away to obtain the first insulating layer having the first hole.
2. The pad height increasing method according to claim 1, It is characterized in that The step of forming a welding reinforcement layer in the second hole comprises: Coating a second photoresist on the surface of the substrate, and developing toward the conductive pillars to expose the conductive pillars; sputtering a metal material onto the surface of the substrate; The second photoresist is removed to obtain the welding strengthening layer higher than the second hole.
3. The pad height increasing method according to claim 1, It is characterized in that The step of forming a welding reinforcement layer in the second hole comprises: Coating a second photoresist on the surface of the substrate, and developing toward the conductive pillars to expose the conductive pillars; Applying a layer of second conductive material with equal thickness to the surface of the substrate and curing the layer; The second photoresist is removed to obtain the welding strengthening layer which is recessed downward.
4. The pad height increasing method according to claim 1, It is characterized in that The height of the initial pad is less than 5 μm, and the height of the welding reinforcement layer is less than 5 μm.
5. The pad height increasing method according to claim 4, It is characterized in that The total thickness of the initial pad and the soldering reinforcement layer is greater than one tenth of the height of the conductive column.
6. The pad height increasing method according to claim 1, It is characterized in that The first conductive material is UV ink dispersed with nano copper-chromium alloy particles.
7. A method for manufacturing a display panel, It is characterized in that The following steps are involved: Take a driving substrate, including a pixel driving circuit and a driving pad, take a light-emitting substrate, including a display chip and a chip pad, and the positions of the driving pad and the chip pad are distributed in a mirror image; The driving pad and / or the chip pad is used as an initial pad, at least one of the driving substrate and the light-emitting substrate is formed into a new pad according to the pad heightening method described in any one of claims 1 to 6, and the driving pad is aligned and welded with the chip pad to obtain the display panel.
8. A method for manufacturing a display panel, It is characterized in that The following steps are involved: Take a driving substrate, including a pixel driving circuit and a driving pad, and take a light-emitting substrate, including a display chip and a chip pad; Punching holes on the light-emitting substrate, and connecting the chip pads to the back side of the light-emitting substrate to form back side pads, wherein the driving pads have the same position distribution as the back side pads; The driving pad is used as an initial pad, a new pad is formed on the driving substrate according to the pad heightening method according to any one of claims 1 to 6, and the driving pad is aligned and welded with the back pad to obtain the display panel.
9. A method for manufacturing a display panel, It is characterized in that The following steps are involved: Take a driving substrate, including a pixel driving circuit and a driving pad, take a light-emitting substrate, including a display chip and a chip pad, and the positions of the driving pad and the chip pad are distributed in a mirror image; The driving pad and the chip pad are used as initial pads, one of the driving substrate and the light-emitting substrate is formed into a convex pad according to the pad raising method described in claim 2, and the other is formed into a concave pad matching the convex pad according to the pad raising method described in claim 3, and the convex pad is aligned and welded with the concave pad to obtain the display panel.
Citation Information
Patent Citations
Light-emitting module, preparation method and display device
CN116845061A
Multiple group lug-to-lug packing structure
CN2508397Y
An anchor system for solder bump, a method for forming the same, and chip package having the same
KR1020060094248A
Fabricating process of an electrically conductive structure on a circuit board
US20060223299A1
Copper pillar full metal via electrical circuit structure
US20120168948A1