Intelligent detection method and system for steel structure weld defects based on cloud platform
Through an intelligent inspection system based on the cloud platform, machine learning and deep learning technologies are used to monitor and evaluate bridge weld defects in real time, solving the problems of inefficiency and inaccuracy of traditional inspection methods, achieving efficient and accurate welding quality control, and ensuring improve the safety and service life of the bridge structure.
Patent Information
- Application Number
- CN202410995356.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2044-07-24
AI Technical Summary
Traditional weld inspection methods are inefficient, inaccurate and costly, and cannot meet the accurate requirements for bridge welding quality, making it difficult to effectively detect and manage weld defects.
The intelligent detection system for steel structure weld defects based on the cloud platform monitors the welding process in real time through data collection, cloud data storage, data preprocessing, defect detection identification and result display modules, combined with cameras or sensors, machine learning and deep learning technology. Calculate the weld defect detection index and provide visual defect assessment and treatment suggestions.
It achieves efficient and accurate detection and management of weld defects, improves welding quality control efficiency, ensures the safety and service life of the bridge structure, and reduces detection costs.
Smart Images

Figure CN118520430B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of intelligent detection technology, and specifically to a cloud platform-based steel structure weld defect intelligent detection method and system. Background Art
[0002] As an important transportation infrastructure, bridge structures undertake the important task of connecting cities and regions. In the construction process of bridges, welding is a key process technology, and the quality of the welding parts directly affects the structural strength and safety of the bridge. However, since the welding process is affected by many factors, such as welding parameters and material quality, welds are prone to various defects, such as pores, inclusions, cracks, etc. These weld defects may reduce the bearing capacity, durability and safety of the bridge, and bring many hidden dangers to the use and maintenance of the bridge.
[0003] Steel structure weld defects are a common but serious problem in bridge structures. Traditional weld inspection methods often rely on manual visual inspection or simple inspection equipment, which has problems such as low efficiency, inaccurate inspection, and high cost, making it difficult to meet the accurate requirements for welding quality. Summary of the invention
[0004] 1. Technical issues to be resolved
[0005] In view of the deficiencies in the prior art, the present invention provides a cloud platform-based intelligent detection method and system for steel structure weld defects, which solves the problems mentioned in the background technology.
[0006] (II) Technical solution
[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions: a steel structure weld defect intelligent detection system based on a cloud platform, including a data acquisition module, a cloud data storage module, a data preprocessing module, a defect detection and identification module, a result display module and a remote access module;
[0008] The data acquisition module uses a camera or other sensor equipment to monitor the welding parts of the bridge in real time, obtains the first data group, the second data group and the third data group, and uploads them to the cloud platform;
[0009] The cloud data storage module is responsible for storing the collected first data group, second data group and third data group on the cloud platform, and provides data management functions, including storage, backup and recovery;
[0010] The data preprocessing module is used to preprocess the collected data, including denoising, image enhancement and geometric correction, and use machine learning and deep learning technologies in the cloud to design and train a detection algorithm model for weld defects to obtain: steel structure weld defect detection index Qlhf;
[0011] The defect detection and identification module is used to compare the steel structure weld defect detection index Qlhf calculated by the trained algorithm model with the preset qualified detection threshold Z and the preset qualified detection threshold X, perform defect detection and identification on the preprocessed data, and obtain an evaluation level scheme;
[0012] The result display module is used to display the detected evaluation level scheme to the user in a visual manner, including the defect location, type and size, as well as treatment suggestions for different defects;
[0013] The remote access module is used to allow users to remotely access the system through the cloud platform, monitor the situation on the welding site in real time, and obtain the detection results so that the staff can take timely measures.
[0014] Preferably, the data acquisition module includes a welding parameter acquisition unit, a weld feature acquisition unit and a material quality acquisition unit;
[0015] The welding parameter acquisition unit is responsible for monitoring characteristic parameters in the welding process, obtaining the welding current value Hjdl, the voltage variation range Dybh, the welding speed variation rate Hjsd and the gas flow value Qtll, and forming a first data group;
[0016] The weld feature acquisition unit is responsible for acquiring the morphological characteristic parameters of the weld, including morphology, size, surface roughness and deformation degree, and acquiring: weld morphological curvature Hfxt, weld average width Hfkd, weld average thickness Hfhd, weld surface roughness Bmcc and weld deformation degree Hfbx, to form a second data set;
[0017] The material quality acquisition unit is responsible for monitoring the quality and process parameters of welding materials, including surface cleanliness, temperature, composition accuracy and thickness, and obtaining: material surface cleanliness Bmqj, material temperature value Clwd, material batching accuracy Pljd and material thickness Clhd, forming a third data group.
[0018] Preferably, the cloud data storage module includes a data storage unit and a data management unit;
[0019] The data storage unit is responsible for storing the collected data on the cloud server, including data storage, index management, and data archiving, to meet the needs of long-term data preservation and rapid retrieval;
[0020] The data management unit is responsible for managing the data stored in the cloud, providing data management functions, including storage management, backup and recovery, including data backup, data recovery, authority management and version control, and providing management and monitoring of data.
[0021] Preferably, the data preprocessing module includes a data cleaning unit and a data calculation unit;
[0022] The data cleaning unit is responsible for cleaning and denoising the collected data, removing interference and noise in the data, including data cleaning, removing outliers and filtering, and preprocessing, image enhancement and geometric correction of the collected image data, including image denoising, sharpening, contrast enhancement and geometric transformation operations, so that the image is clear and weld defects are easy to identify;
[0023] The data calculation unit is responsible for using machine learning and deep learning technology in the cloud to design and train a detection algorithm model for weld defects, and obtain: steel structure weld defect detection index Qlhf, welding stability coefficient Hjwd, weld shape coefficient Hfxt and material quality coefficient Clzl;
[0024] The steel structure weld defect detection index Qlhf is calculated by the following formula:
[0025] ;
[0026] Wherein, Hjwd represents the welding stability coefficient, Hfxt represents the weld shape coefficient, Clzl represents the material quality coefficient, q, w and e represent the proportional coefficients of the welding stability coefficient Hjwd, the weld shape coefficient Hfxt and the material quality coefficient Clzl respectively;
[0027] in, , , ,and , R represents the first correction constant.
[0028] Preferably, the welding stability coefficient Hjwd is calculated by the following formula:
[0029] ;
[0030] Wherein, Hjdl represents the welding current value, Dybh represents the voltage variation range, Hjsd represents the welding speed variation rate, Qtll represents the gas flow value, t, y, u and i represent the proportionality coefficients of the welding current value Hjdl, the voltage variation range Dybh, the welding speed variation rate Hjsd and the gas flow value Qtll respectively;
[0031] in, , , , ,and , O represents the second correction constant.
[0032] Preferably, the weld shape coefficient Hfxt is calculated by the following formula:
[0033] ;
[0034] Wherein, Hfxt represents the curvature of weld shape, Hfkd represents the average width of weld, Hfhd represents the average thickness of weld, Bmcc represents the surface roughness of weld, Hfbx represents the degree of weld deformation, a, s, d, f and g represent the proportional coefficients of weld shape curvature Hfxt, average width of weld Hfkd, average thickness of weld Hfhd, surface roughness of weld Bmcc and degree of weld deformation Hfbx respectively;
[0035] in, , , , , ,and , H represents the third correction constant;
[0036] The material quality coefficient Clzl is calculated by the following formula:
[0037] ;
[0038] Wherein, Bmqj represents the material surface cleanliness, Clwd represents the material temperature value, Pljd represents the material batching accuracy, Clhd represents the material thickness, j, k, c and v represent the proportional coefficients of the material surface cleanliness Bmqj, the material temperature value Clwd, the material batching accuracy Pljd and the material thickness Clhd respectively;
[0039] in, , , , ,and , L represents the fourth correction constant.
[0040] Preferably, the defect detection and identification module includes a defect assessment unit;
[0041] The defect assessment unit is used to perform defect detection on the preprocessed data using the trained algorithm model, compare the calculated steel structure weld defect detection index Qlhf with the preset detection qualified threshold, and determine the defect assessment level scheme:
[0042] When the steel structure weld defect detection index Qlhf ≤ the preset standard threshold Z, it is judged as qualified and no adjustment is required. The welding equipment is maintained at a fixed period, including real-time monitoring of welding parameters to ensure that the current, voltage, welding speed and gas flow are within the specified range;
[0043] When the steel structure weld defect detection index Qlhf is less than the preset standard threshold value Z and the steel structure weld defect detection index Qlhf is less than the preset standard threshold value X, it is judged as a warning, and the problems that cause weld defects are discovered and corrected in time, including checking the weld morphology at a fixed period, discovering the welding speed is too fast or too slow in time, and adjusting the inspection frequency to twice a week;
[0044] When the steel structure weld defect detection index Qlhf ≥ the preset standard threshold X, it is judged as unqualified, the type and cause of the weld defect are analyzed, the welding process parameters, including current, voltage, welding speed and gas flow, are re-evaluated, the parameters that need to be adjusted are determined, the current and voltage are adjusted to be within the qualified range, and the welding speed is adjusted to ensure the welding quality.
[0045] Preferably, the result display module includes a data visualization unit and a defect location unit;
[0046] The data visualization module is responsible for converting the detected weld defect location, type and size information into graphics, charts or other visualization forms, including heat maps, curve charts and bar charts, and presenting the detected weld defect results to the user in a visual manner so that the user can view the analysis and detection results in real time;
[0047] The defect location unit is used to determine the specific location and size of the weld defect according to the result of the detection algorithm, and mark the defect location on the image or map so that the user can accurately identify it, locate the detected weld defect, display the defect location and type on the visual interface, and classify the detected weld defects.
[0048] Preferably, the remote access module includes a remote monitoring unit and a notification unit;
[0049] The remote monitoring unit is responsible for enabling users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and provide a user interface or application to allow users to remotely access the system through the Internet, view real-time video streams or real-time data, and monitor the progress and situation of the welding process;
[0050] The notification unit is responsible for transmitting the detection results to the user in a timely manner and providing a real-time notification function. It transmits the detected weld defect results to the user in real time and provides real-time notifications via email, SMS and App push, so that the staff can take timely measures to manage and control the welding quality.
[0051] The intelligent detection method of steel structure weld defects based on cloud platform includes the following steps:
[0052] Step 1: The data acquisition module uses a camera or other sensor equipment to monitor the welding parts of the bridge in real time, obtains the first data group, the second data group and the third data group, and uploads them to the cloud platform;
[0053] Step 2: storing the collected first data group, second data group and third data group on the cloud platform, and providing data management functions, including storage, backup and recovery;
[0054] Step 3: Preprocess the collected data, including denoising, image enhancement and geometric correction, and use machine learning and deep learning technologies in the cloud to design and train a detection algorithm model for weld defects to obtain: steel structure weld defect detection index Qlhf;
[0055] Step 4: Compare the steel structure weld defect detection index Qlhf calculated by the trained algorithm model with the preset qualified detection threshold Z and the preset qualified detection threshold X, perform defect detection and identification on the preprocessed data, and obtain an evaluation level scheme;
[0056] Step 5: Display the detected evaluation level scheme to the user in a visual way, including the defect location, type and size, as well as treatment suggestions for different defects;
[0057] Step 6: Allow users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and obtain the test results so that the staff can take timely measures.
[0058] (III) Beneficial effects
[0059] The present invention provides a cloud platform-based steel structure weld defect intelligent detection method and system, which has the following beneficial effects:
[0060] (1) When the system is running, the welding parts of the bridge are monitored in real time by using a camera or other sensor equipment to obtain the first data group, the second data group and the third data group, and the collected image or video data is uploaded to the cloud platform. The collected data is stored in the cloud and data management functions are provided to pre-process the collected data. Machine learning and deep learning technologies are used in the cloud to obtain the weld defect detection algorithm model: steel structure weld defect detection index Qlhf. The steel structure weld defect detection index Qlhf calculated by the trained algorithm model is compared with the preset qualified detection threshold Z and the preset qualified detection threshold X. Defect detection and identification are performed on the pre-processed data to obtain an evaluation level scheme. The detected weld defect results are displayed to the user in a visual manner, allowing the user to remotely access the system through the cloud platform.
[0061] (2) The system can monitor the welding site in real time, obtain data in a timely manner and upload it to the cloud platform to ensure the timeliness and accuracy of the data. The cloud data storage module can effectively manage the collected data, including storage, backup and recovery, to ensure the security and reliability of the data. The data preprocessing module can perform preprocessing operations such as denoising, image enhancement and geometric correction on the collected data to provide high-quality input data for subsequent defect detection algorithms.
[0062] (3) Algorithm model training can design and train detection algorithm models for weld defects through machine learning and deep learning technology to obtain accurate weld defect detection index. The defect detection and recognition module can use the trained algorithm model to detect and identify defects on preprocessed data, evaluate the defects according to the preset standard threshold, and provide a reference for subsequent welding quality management.
[0063] (4) The result display module can display the detected weld defect results to the user in a visual manner and provide treatment suggestions for different defects, so that the user can intuitively understand the welding quality. The remote access module allows the user to monitor the welding site in real time through the cloud platform, obtain the test results, and take timely measures to manage and control the welding quality, thereby improving the work efficiency and quality management level of the staff. BRIEF DESCRIPTION OF THE DRAWINGS
[0064] Figure 1 It is a schematic diagram of the flow chart of the intelligent detection system for steel structure weld defects based on the cloud platform of the present invention;
[0065] Figure 2 This is a schematic diagram of the steps of the intelligent detection method for steel structure weld defects based on a cloud platform of the present invention; DETAILED DESCRIPTION
[0066] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0067] As an important transportation infrastructure, bridge structures undertake the important task of connecting cities and regions. In the construction process of bridges, welding is a key process technology, and the quality of the welding parts directly affects the structural strength and safety of the bridge. However, since the welding process is affected by many factors, such as welding parameters and material quality, welds are prone to various defects, such as pores, inclusions, cracks, etc. These weld defects may reduce the bearing capacity, durability and safety of the bridge, and bring many hidden dangers to the use and maintenance of the bridge.
[0068] Steel structure weld defects are a common but serious problem in bridge structures. Traditional weld inspection methods often rely on manual visual inspection or simple inspection equipment, which has problems such as low efficiency, inaccurate inspection, and high cost, making it difficult to meet the accurate requirements for welding quality.
[0069] Example 1
[0070] The present invention provides a steel structure weld defect intelligent detection system based on a cloud platform, please refer to Figure 1 , including data acquisition module, cloud data storage module, data preprocessing module, defect detection and identification module, result display module and remote access module;
[0071] The data acquisition module uses a camera or other sensor equipment to monitor the welding parts of the bridge in real time, obtains the first data group, the second data group and the third data group, and uploads them to the cloud platform;
[0072] The cloud data storage module is responsible for storing the collected first data group, second data group and third data group on the cloud platform, and provides data management functions, including storage, backup and recovery;
[0073] The data preprocessing module is used to preprocess the collected data, including denoising, image enhancement and geometric correction, and use machine learning and deep learning technologies in the cloud to design and train a detection algorithm model for weld defects to obtain: steel structure weld defect detection index Qlhf;
[0074] The defect detection and identification module is used to compare the steel structure weld defect detection index Qlhf calculated by the trained algorithm model with the preset qualified detection threshold Z and the preset qualified detection threshold X, perform defect detection and identification on the preprocessed data, and obtain an evaluation level scheme;
[0075] The result display module is used to display the detected evaluation level scheme to the user in a visual manner, including the defect location, type and size, as well as treatment suggestions for different defects;
[0076] The remote access module is used to allow users to remotely access the system through the cloud platform, monitor the situation on the welding site in real time, and obtain the detection results so that the staff can take timely measures.
[0077] In this embodiment, a camera or other sensor device is used to monitor the welding parts of the bridge in real time, and a first data group, a second data group and a third data group are obtained. The collected image or video data is uploaded to a cloud platform, the collected data is stored in the cloud, and a data management function is provided to pre-process the collected data. Machine learning and deep learning technologies are used in the cloud to obtain a weld defect detection algorithm model: a steel structure weld defect detection index Qlhf, a steel structure weld defect detection index Qlhf calculated using the trained algorithm model, and compared with a preset qualified detection threshold Z and a preset qualified detection threshold X, defect detection and identification are performed on the pre-processed data, an evaluation grade scheme is obtained, and the detected weld defect results are displayed to the user in a visual manner, allowing the user to remotely access the system through the cloud platform.
[0078] Example 2
[0079] This embodiment is explained in Example 1, please refer to Figure 1 ,Specifically: the data acquisition module includes a welding parameter acquisition unit, a weld feature acquisition unit and a material quality acquisition unit;
[0080] The welding parameter acquisition unit is responsible for monitoring characteristic parameters in the welding process, obtaining the welding current value Hjdl, the voltage variation range Dybh, the welding speed variation rate Hjsd and the gas flow value Qtll, and forming a first data group;
[0081] The weld feature acquisition unit is responsible for acquiring the morphological characteristic parameters of the weld, including morphology, size, surface roughness and deformation degree, and acquiring: weld morphological curvature Hfxt, weld average width Hfkd, weld average thickness Hfhd, weld surface roughness Bmcc and weld deformation degree Hfbx, to form a second data set;
[0082] The material quality acquisition unit is responsible for monitoring the quality and process parameters of welding materials, including surface cleanliness, temperature, composition accuracy and thickness, and obtaining: material surface cleanliness Bmqj, material temperature value Clwd, material batching accuracy Pljd and material thickness Clhd, forming a third data group.
[0083] The cloud data storage module includes a data storage unit and a data management unit;
[0084] The data storage unit is responsible for storing the collected data on the cloud server, including data storage, index management, and data archiving, to meet the needs of long-term data preservation and rapid retrieval;
[0085] The data management unit is responsible for managing the data stored in the cloud, providing data management functions, including storage management, backup and recovery, including data backup, data recovery, authority management and version control, and providing management and monitoring of data.
[0086] In this embodiment, the welding parameter acquisition unit is responsible for real-time monitoring of characteristic parameters in the welding process, including welding current value, voltage variation range, welding speed variation rate and gas flow value, etc. These parameters directly affect the formation and quality of the weld. By collecting these parameters, a first data group can be formed to provide basic data for subsequent data analysis. The weld feature acquisition unit focuses on collecting the morphological characteristic parameters of the weld, including the shape, size, surface roughness and deformation degree of the weld. These characteristic parameters are crucial for judging the quality and defects of the weld. By collecting these parameters, a second data group can be formed to provide an important reference for subsequent defect detection. The material quality acquisition unit is responsible for monitoring the quality and process parameters of the welding material. By collecting these parameters, a third data group can be formed to provide important information for subsequent data analysis, and the cloud data storage module is responsible for storing the collected data on the cloud server and providing data management functions. The data storage unit is responsible for long-term storage and rapid retrieval of data.
[0087] Example 3
[0088] This embodiment is explained in Example 1, please refer to Figure 1 ,Specifically: the data preprocessing module includes a data cleaning unit and a data calculation unit;
[0089] The data cleaning unit is responsible for cleaning and denoising the collected data, removing interference and noise in the data, including data cleaning, removing outliers and filtering, and preprocessing, image enhancement and geometric correction of the collected image data, including image denoising, sharpening, contrast enhancement and geometric transformation operations, so that the image is clear and weld defects are easy to identify;
[0090] The data calculation unit is responsible for using machine learning and deep learning technology in the cloud to design and train a detection algorithm model for weld defects, and obtain: steel structure weld defect detection index Qlhf, welding stability coefficient Hjwd, weld shape coefficient Hfxt and material quality coefficient Clzl;
[0091] The steel structure weld defect detection index Qlhf is calculated by the following formula:
[0092] ;
[0093] Wherein, Hjwd represents the welding stability coefficient, Hfxt represents the weld shape coefficient, Clzl represents the material quality coefficient, q, w and e represent the proportional coefficients of the welding stability coefficient Hjwd, the weld shape coefficient Hfxt and the material quality coefficient Clzl respectively;
[0094] in, , , ,and , R represents the first correction constant.
[0095] The welding stability coefficient Hjwd is calculated by the following formula:
[0096] ;
[0097] Wherein, Hjdl represents the welding current value, Dybh represents the voltage variation range, Hjsd represents the welding speed variation rate, Qtll represents the gas flow value, t, y, u and i represent the proportionality coefficients of the welding current value Hjdl, the voltage variation range Dybh, the welding speed variation rate Hjsd and the gas flow value Qtll respectively;
[0098] in, , , , ,and , O represents the second correction constant.
[0099] The weld shape coefficient Hfxt is calculated by the following formula:
[0100] ;
[0101] Wherein, Hfxt represents the curvature of weld shape, Hfkd represents the average width of weld, Hfhd represents the average thickness of weld, Bmcc represents the surface roughness of weld, Hfbx represents the degree of weld deformation, a, s, d, f and g represent the proportional coefficients of weld shape curvature Hfxt, average width of weld Hfkd, average thickness of weld Hfhd, surface roughness of weld Bmcc and degree of weld deformation Hfbx respectively;
[0102] in, , , , , ,and , H represents the third correction constant;
[0103] The material quality coefficient Clzl is calculated by the following formula:
[0104] ;
[0105] Wherein, Bmqj represents the material surface cleanliness, Clwd represents the material temperature value, Pljd represents the material batching accuracy, Clhd represents the material thickness, j, k, c and v represent the proportional coefficients of the material surface cleanliness Bmqj, the material temperature value Clwd, the material batching accuracy Pljd and the material thickness Clhd respectively;
[0106] in, , , , ,and , L represents the fourth correction constant.
[0107] The defect detection and identification module includes a defect assessment unit;
[0108] The defect assessment unit is used to perform defect detection on the preprocessed data using the trained algorithm model, compare the calculated steel structure weld defect detection index Qlhf with the preset detection qualified threshold, and determine the defect assessment level scheme:
[0109] When the steel structure weld defect detection index Qlhf ≤ the preset standard threshold Z, it is judged as qualified and no adjustment is required. The welding equipment is maintained at a fixed period, including real-time monitoring of welding parameters to ensure that the current, voltage, welding speed and gas flow are within the specified range;
[0110] When the steel structure weld defect detection index Qlhf is less than the preset standard threshold value Z and the steel structure weld defect detection index Qlhf is less than the preset standard threshold value X, it is judged as a warning, and the problems that cause weld defects are discovered and corrected in a timely manner, including checking the weld morphology at a fixed period, discovering the welding speed is too fast or too slow in time, and adjusting the inspection frequency to twice a week. According to the characteristics of the weld morphology, curvature and thickness, the parameters of the welding equipment are appropriately adjusted, and the light source or lighting equipment is used to illuminate the welding area to improve the image quality and visibility of the weld;
[0111] When the steel structure weld defect detection index Qlhf ≥ the preset standard threshold value X, it is judged as unqualified, the type and cause of the weld defect are analyzed, the welding process parameters, including current, voltage, welding speed and gas flow, are re-evaluated, the parameters that need to be adjusted are determined, the current and voltage are adjusted to be within the qualified range, the welding speed is adjusted to ensure the welding quality, the cleaning and preparation of the welding materials are strengthened, the quality of the welded joint is guaranteed, and there are no impurities during the welding process.
[0112] Example 4
[0113] This embodiment is explained in Example 1, please refer to Figure 1 ,Specifically: the result display module includes a data visualization unit and a defect ,location unit;
[0114] The data visualization module is responsible for converting the detected weld defect location, type and size information into graphics, charts or other visualization forms, including heat maps, curve charts and bar charts, and presenting the detected weld defect results to the user in a visual manner so that the user can view the analysis and detection results in real time;
[0115] The defect location unit is used to determine the specific location and size of the weld defect according to the result of the detection algorithm, and mark the defect location on the image or map so that the user can accurately identify it, locate the detected weld defect, display the defect location and type on the visual interface, and classify the detected weld defects.
[0116] The remote access module includes a remote monitoring unit and a notification unit;
[0117] The remote monitoring unit is responsible for enabling users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and provide a user interface or application to allow users to remotely access the system through the Internet, view real-time video streams or real-time data, and monitor the progress and situation of the welding process;
[0118] The notification unit is responsible for transmitting the detection results to the user in a timely manner and providing a real-time notification function. It transmits the detected weld defect results to the user in real time and provides real-time notifications via email, SMS and App push, so that the staff can take timely measures to manage and control the welding quality.
[0119] In this embodiment, the data visualization unit is responsible for converting the detected weld defect location, type and size information into graphics, charts or other visualization forms. The distribution and characteristics of weld defects can be intuitively displayed. Through visualization, users can quickly understand the welding quality status, find problems in time and take measures to solve them. The defect location unit is responsible for determining the specific location and size of the weld defect based on the results of the detection algorithm, and marking the defect location on the image or map. In this way, users can accurately identify the location and type of weld defects and classify and locate the detected weld defects.
[0120] Example 5
[0121] For intelligent detection method of steel structure weld defects based on cloud platform, please refer to Figure 2 , specifically: including the following steps:
[0122] Step 1: The data acquisition module uses a camera or other sensor equipment to monitor the welding parts of the bridge in real time, obtains the first data group, the second data group and the third data group, and uploads them to the cloud platform;
[0123] Step 2: storing the collected first data group, second data group and third data group on the cloud platform, and providing data management functions, including storage, backup and recovery;
[0124] Step 3: Preprocess the collected data, including denoising, image enhancement and geometric correction, and use machine learning and deep learning technologies in the cloud to design and train a detection algorithm model for weld defects to obtain: steel structure weld defect detection index Qlhf;
[0125] Step 4: Compare the steel structure weld defect detection index Qlhf calculated by the trained algorithm model with the preset qualified detection threshold Z and the preset qualified detection threshold X, perform defect detection and identification on the preprocessed data, and obtain an evaluation level scheme;
[0126] Step 5: Display the detected evaluation level scheme to the user in a visual way, including the defect location, type and size, as well as treatment suggestions for different defects;
[0127] Step 6: Allow users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and obtain the test results so that the staff can take timely measures.
[0128] In this embodiment, by displaying the defect location and type on the visual interface, the user can understand the test results more intuitively, so as to take targeted measures to repair or adjust the welding process and improve the welding quality. The remote access module is another important component of the system, which is designed to allow users to remotely access the system through the cloud platform, monitor the situation of the welding site in real time, and obtain the test results in time. The remote monitoring unit is responsible for enabling users to remotely access the system through the cloud platform and monitor the situation of the welding site in real time. Users can remotely access the system through the Internet, view real-time video streams or real-time data, and monitor the progress and situation of the welding process. Users do not need to be on site to understand the welding situation in time, improve the efficiency and timeliness of monitoring, and the notification unit is responsible for transmitting the test results to the user in time and providing real-time notification function. When a weld defect is detected, the system will promptly send the test results to the user by email, SMS and App push, so that the staff can take timely measures to manage and control the welding quality. Users can learn about welding quality problems at the first time and take corresponding measures in time to ensure welding quality and engineering safety.
[0129] Specific example:
[0130] Assume that the welding process of a bridge structure is being monitored. After normalization, the following data is obtained:
[0131] First data set:
[0132] Welding current value Hjdl=150, voltage variation range Dybh=5, welding speed variation rate Hjsd=0.1, gas flow value Qtll=20;
[0133] Second data set:
[0134] The weld curvature Hfxt=0.8, the average weld width Hfkd=6, the average weld thickness Hfhd=4, the surface roughness Bmcc=0.05, and the weld deformation degree Hfbx=0.3;
[0135] The third data set:
[0136] Material surface cleanliness Bmqj=0.9, material temperature value Clwd=200, material batching accuracy Pljd=0.95, material thickness Clhd=10;
[0137] Corresponding proportional coefficients: q=0.25, w=0.24, e=0.32, t=0.2, y=0.20, u=0.20, i=0.15, a=0.18, s=0.18, d=0.15, f=0.16, g=0.08, j=0.18, k=0.18, c=0.18, v=0.31;
[0138] The first correction constant: R = 0.76, the second correction constant: O = 0.48, the third correction constant: H = 0.15, the fourth correction constant: L = 0.57;
[0139] Slcs=(150×0.25)+(5×0.20)+(0.1×0.20)+(20×0.15)+0.48=42;
[0140] Hfxt=(0.8×0.18)+(6×0.18)+(4×0.15)+(0.05×0.16)+(0.3×0.08)+0.15=2;
[0141] Clzl=(0.9×0.18)+(200×0.18)+(0.95×0.18)+(10×0.31)+0.57=40;
[0142] Qlhf=[(0.25×42)+(0.24×2)] / (0.25+0.24)+(0.32×40)+0.76=36;
[0143] Set the preset standard threshold Z to 30, the preset standard threshold X to 50, and the preset standard threshold Z < When the steel structure weld defect detection index Qlhf < the preset standard threshold X, it is judged as a warning, and the problems that cause weld defects are discovered and corrected in time, including checking the weld morphology at a fixed period, discovering in time that the welding speed is too fast or too slow, and adjusting the inspection frequency to twice a week.
[0144] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. Intelligent detection system for steel structure weld defects based on cloud platform, characterized by: It includes data acquisition module, cloud data storage module, data preprocessing module, defect detection and identification module, result display module and remote access module; The data acquisition module uses a camera or other sensor equipment to monitor the welding parts of the bridge in real time, obtains the first data group, the second data group and the third data group, and uploads them to the cloud platform; The cloud data storage module is responsible for storing the collected first data group, second data group and third data group on the cloud platform, and provides data management functions, including storage, backup and recovery; The data preprocessing module is used to preprocess the collected data, including denoising, image enhancement and geometric correction, and use machine learning and deep learning technologies in the cloud to design and train a detection algorithm model for weld defects to obtain: steel structure weld defect detection index Qlhf; The defect detection and identification module is used to compare the steel structure weld defect detection index Qlhf calculated by the trained algorithm model with the preset qualified detection threshold Z and the preset qualified detection threshold X, perform defect detection and identification on the preprocessed data, and obtain an evaluation level scheme; The result display module is used to display the detected evaluation level scheme to the user in a visual manner, including the defect location, type and size, as well as treatment suggestions for different defects; The remote access module is used to allow users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and obtain the test results so that the staff can take timely measures; The data preprocessing module includes a data cleaning unit and a data calculation unit; The data cleaning unit is responsible for cleaning and denoising the collected data, removing interference and noise in the data, including data cleaning, removing outliers and filtering, and preprocessing, image enhancement and geometric correction of the collected image data, including image denoising, sharpening, contrast enhancement and geometric transformation operations, so that the image is clear and weld defects are easy to identify; The data calculation unit is responsible for using machine learning and deep learning technology in the cloud to design and train a detection algorithm model for weld defects, and obtain: steel structure weld defect detection index Qlhf, welding stability coefficient Hjwd, weld shape coefficient Hfxt and material quality coefficient Clzl; The steel structure weld defect detection index Qlhf is calculated by the following formula: Wherein, Hjwd represents the welding stability coefficient, Hfxt represents the weld shape coefficient, Clzl represents the material quality coefficient, q, w and e represent the proportional coefficients of the welding stability coefficient Hjwd, the weld shape coefficient Hfxt and the material quality coefficient Clzl respectively; Wherein, 0.12≤q≤0.28, 0.23≤w≤0.35, 0.22≤e≤0.37, and q+w+e≤1.0, R represents the first correction constant; The welding stability coefficient Hjwd is calculated by the following formula: Slcs=[(Hjdl*t)+(Dybh*y)+(Hjsd*u)+(Qtll*i)]+O; Wherein, Hjdl represents the welding current value, Dybh represents the voltage variation range, Hjsd represents the welding speed variation rate, Qtll represents the gas flow value, t, y, u and i represent the proportionality coefficients of the welding current value Hjdl, the voltage variation range Dybh, the welding speed variation rate Hjsd and the gas flow value Qtll respectively; Wherein, 0.13≤t≤0.23, 0.17≤y≤0.23, 0.18≤u≤0.24, 0.11≤i≤0.30, and t+y+u+i≤1.0, O represents the second correction constant; The weld shape coefficient Hfxt is calculated by the following formula: Hfxt=[(Hfxt*a)+(Hfkd*s)+(Hfhd*d)+(Bmcc*f)+(Hfbx*g)]+H; Wherein, Hfxt represents the curvature of weld shape, Hfkd represents the average width of weld, Hfhd represents the average thickness of weld, Bmcc represents the surface roughness of weld, Hfbx represents the degree of weld deformation, a, s, d, f and g represent the proportional coefficients of weld shape curvature Hfxt, average width of weld Hfkd, average thickness of weld Hfhd, surface roughness of weld Bmcc and degree of weld deformation Hfbx respectively; Wherein, 0.12≤a≤0.25, 0.17≤s≤0.20, 0.13≤d≤0.25, 0.15≤f≤0.20, 0.05≤g≤0.10, and a+s+d+f+g≤1.0, H represents the third correction constant; The material quality coefficient Clzl is calculated by the following formula: Clzl=[(Bmqj*j)+(Clwd*k)+(Pljd*c)+(Clhd*v)]+L; Wherein, Bmqj represents the material surface cleanliness, Clwd represents the material temperature value, Pljd represents the material batching accuracy, Clhd represents the material thickness, j, k, c and v represent the proportional coefficients of the material surface cleanliness Bmqj, the material temperature value Clwd, the material batching accuracy Pljd and the material thickness Clhd respectively; Among them, 0.12≤j≤0.25, 0.15≤k≤0.20, 0.17≤c≤0.20, 0.13≤v≤0.35, and j+k+c+v≤1.0, and L represents the fourth correction constant.
2. The cloud platform-based intelligent steel structure weld defect detection system according to claim 1 is characterized in that: The data acquisition module includes a welding parameter acquisition unit, a weld feature acquisition unit and a material quality acquisition unit; The welding parameter acquisition unit is responsible for monitoring characteristic parameters in the welding process, obtaining the welding current value Hjdl, the voltage variation range Dybh, the welding speed variation rate Hjsd and the gas flow value Qtll, and forming a first data group; The weld feature acquisition unit is responsible for acquiring the morphological characteristic parameters of the weld, including morphology, size, surface roughness and deformation degree, and acquiring: weld morphological curvature Hfxt, weld average width Hfkd, weld average thickness Hfhd, weld surface roughness Bmcc and weld deformation degree Hfbx, to form a second data set; The material quality acquisition unit is responsible for monitoring the quality and process parameters of welding materials, including surface cleanliness, temperature, composition accuracy and thickness, and obtaining: material surface cleanliness Bmqj, material temperature value Clwd, material batching accuracy Pljd and material thickness Clhd, forming a third data group.
3. The cloud platform-based intelligent steel structure weld defect detection system according to claim 1 is characterized in that: The cloud data storage module includes a data storage unit and a data management unit; The data storage unit is responsible for storing the collected data on the cloud server, including data storage, index management, and data archiving, to meet the needs of long-term data preservation and rapid retrieval; The data management unit is responsible for managing the data stored in the cloud, providing data management functions, including storage management, backup and recovery, including data backup, data recovery, authority management and version control, and providing management and monitoring of data.
4. The cloud platform-based intelligent steel structure weld defect detection system according to claim 1 is characterized in that: The defect detection and identification module includes a defect assessment unit; The defect assessment unit is used to perform defect detection on the preprocessed data using the trained algorithm model, compare the calculated steel structure weld defect detection index Qlhf with the preset detection qualified threshold, and determine the defect assessment level scheme: When the steel structure weld defect detection index Qlhf ≤ the preset standard threshold Z, it is judged as qualified and no adjustment is required. The welding equipment is maintained at a fixed period, including real-time monitoring of welding parameters to ensure that the current, voltage, welding speed and gas flow are within the specified range; When the steel structure weld defect detection index Qlhf is less than the preset standard threshold value Z and the steel structure weld defect detection index Qlhf is less than the preset standard threshold value X, it is judged as a warning, and the problems that cause weld defects are discovered and corrected in time, including checking the weld morphology at a fixed period, discovering the welding speed is too fast or too slow in time, and adjusting the inspection frequency to twice a week; When the steel structure weld defect detection index Qlhf ≥ the preset standard threshold X, it is judged as unqualified, the type and cause of the weld defect are analyzed, the welding process parameters, including current, voltage, welding speed and gas flow, are re-evaluated, the parameters that need to be adjusted are determined, the current and voltage are adjusted to be within the qualified range, and the welding speed is adjusted to ensure the welding quality.
5. The cloud platform-based intelligent steel structure weld defect detection system according to claim 1 is characterized in that: The result display module includes a data visualization unit and a defect location unit; The data visualization module is responsible for converting the detected weld defect location, type and size information into graphics, charts or other visualization forms, including heat maps, curve charts and bar charts, and presenting the detected weld defect results to the user in a visual manner so that the user can view the analysis and detection results in real time; The defect location unit is used to determine the specific location and size of the weld defect according to the result of the detection algorithm, and mark the defect location on the image or map so that the user can accurately identify it, locate the detected weld defect, display the defect location and type on the visual interface, and classify the detected weld defects.
6. The cloud platform-based intelligent steel structure weld defect detection system according to claim 1, characterized in that: The remote access module includes a remote monitoring unit and a notification unit; The remote monitoring unit is responsible for enabling users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and provide a user interface or application to allow users to remotely access the system through the Internet, view real-time video streams or real-time data, and monitor the progress and situation of the welding process; The notification unit is responsible for transmitting the detection results to the user in a timely manner and providing a real-time notification function. It transmits the detected weld defect results to the user in real time and provides real-time notifications via email, SMS and App push, so that the staff can take timely measures to manage and control the welding quality.
7. A cloud-based intelligent detection method for steel structure weld defects, comprising a cloud-based intelligent detection system for steel structure weld defects as described in any one of claims 1 to 6, characterized in that: The following steps are involved: Step 1: The data acquisition module uses a camera or other sensor equipment to monitor the welding parts of the bridge in real time, obtains the first data group, the second data group and the third data group, and uploads them to the cloud platform; Step 2: storing the collected first data group, second data group and third data group on the cloud platform, and providing data management functions, including storage, backup and recovery; Step 3: Preprocess the collected data, including denoising, image enhancement and geometric correction, and use machine learning and deep learning technologies in the cloud to design and train a detection algorithm model for weld defects to obtain: steel structure weld defect detection index Qlhf; Step 4: Compare the steel structure weld defect detection index Qlhf calculated by the trained algorithm model with the preset qualified detection threshold Z and the preset qualified detection threshold X, perform defect detection and identification on the preprocessed data, and obtain an evaluation level scheme; Step 5: Display the detected evaluation level scheme to the user in a visual way, including the defect location, type and size, as well as treatment suggestions for different defects; Step 6: Allow users to remotely access the system through the cloud platform, monitor the situation at the welding site in real time, and obtain the test results so that the staff can take timely measures.