Quantum dot films and their preparation methods, backlight modules and their preparation methods, display panels
By setting high-brightness, low-brightness, and transition regions with proportional thickness and concentration in the resin layer, and combining them with bubble structures and coating layers to protect the quantum dots, the problem of poor light uniformity of quantum dot films is solved, thus achieving uniform light output of the backlight module and uniform display of the display device.
Patent Information
- Application Number
- CN202410530981.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-28
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-04-28
AI Technical Summary
Quantum dot films have poor light uniformity, resulting in uneven light output from the backlight module.
The resin layer is designed to include high-brightness, low-brightness, and transition regions, with the thickness and quantum dot concentration set proportionally. Combined with a bubble structure and a coating layer to protect the quantum dots, a quantum dot film is formed through photocuring.
The quantum dot film improves the light uniformity, making the backlight module emit light more evenly, thus enhancing the display effect of the display device and saving the cost of the diffuser plate.
Smart Images

Figure CN118550121B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of display technology, and in particular to a quantum dot film and its preparation method, a backlight module and its preparation method, and a display panel. Background Technology
[0002] In recent years, quantum dots have been widely used in liquid crystal display (LCD) products in the form of optical films to meet the high color gamut display requirements of LCD products. Quantum dots are inorganic particles with a particle size of less than 10 nm. When excited by external photons, they absorb photons and re-emit light of a different wavelength. Due to these properties, quantum dots can convert incident light into light of a specific color, thereby enabling display products to have higher color rendering and color reproduction capabilities, producing a rich and colorful visual experience.
[0003] In practical applications, quantum dot films are often placed on the light-emitting surface of the backlight module. However, since the light emitted by the light source is of the Lambau shape, with the highest intensity at the center and weaker intensity around the edges, and the quantum dot film has poor light uniformity, the intensity of other wavelengths of light excited by the quantum dot film will also be uneven, ultimately leading to uneven light output from the backlight module.
[0004] The above content is only used to help understand the technical solution of this application and does not represent an admission that the above content is prior art. Summary of the Invention
[0005] The main purpose of this application is to provide a quantum dot film and its preparation method, a backlight module and its preparation method, and a display panel, which aim to improve the light uniformity of the quantum dot film.
[0006] To achieve the above objectives, this application provides a quantum dot film, the quantum dot film comprising:
[0007] Resin layer;
[0008] Multiple quantum dots, each of which is embedded within the resin layer;
[0009] The resin layer includes at least one high-brightness region, at least one low-brightness region, and a transition region located between the high-brightness region and the low-brightness region;
[0010] The thickness of the high-brightness region is less than the thickness of the low-brightness region, the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region, and the quantum dot concentration in the resin layer is directly proportional to the thickness of the resin layer.
[0011] In one embodiment, the resin layer further includes bubbles encapsulating the quantum dots, wherein the gas within the bubbles includes carbon dioxide.
[0012] In one embodiment, the quantum dot includes: a quantum dot core and a coating layer covering the quantum dot core, wherein the surface of the coating layer is connected with bicarbonate ions.
[0013] In one embodiment, the quantum dot core includes at least one of CdSe, CdS, InP, PbSe, and CdTe;
[0014] And / or, the material of the coating layer includes at least one of ZnS, PbS and CdS;
[0015] And / or, the thickness of the coating layer is 1–3 nm;
[0016] And / or, the particle size of the quantum dot core includes 2-4 nm and 5-7 nm.
[0017] In one embodiment, the thickness of the high-brightness region is 5–8 μm, and the thickness of the low-brightness region is 10–15 μm.
[0018] Furthermore, to achieve the above objectives, this application also proposes a method for preparing quantum dot films, applicable to the preparation of quantum dot films as described above, comprising the following steps:
[0019] Quantum dots are mixed with a first matrix resin to obtain a quantum dot mixture;
[0020] The quantum dot mixture is added to a pre-set mold for photocuring to obtain a quantum dot film.
[0021] In one embodiment, the mass ratio of the quantum dot to the first matrix resin is 1:(50-500);
[0022] And / or, the wavelength of the light source for photocuring is 200-240 nm, and the photocuring time is 5-10 s.
[0023] In addition, to achieve the above objectives, this application also proposes a backlight module, which includes a quantum dot film as described above.
[0024] In one embodiment, the backlight module includes:
[0025] substrate;
[0026] A light source is disposed on one side of the substrate;
[0027] A heat insulation layer is disposed on the side of the substrate near the light source and encloses the light source;
[0028] The quantum dot film is disposed on the light-emitting side of the heat insulation layer, wherein the high-brightness region of the quantum dot film corresponds to the strong light region of the light source, and the low-brightness region of the quantum dot film corresponds to the weak light region of the light source, and the light energy intensity of the strong light region is greater than that of the weak light region.
[0029] In one embodiment, the height difference between the heat insulation layer and the light source is 0.5–2 mm;
[0030] And / or, the material of the insulation layer includes: porous silica.
[0031] Furthermore, to achieve the above objectives, this application also proposes a backlight module fabrication method, applicable to the fabrication of the backlight module as described above, comprising the following steps:
[0032] A light source is placed on the substrate;
[0033] A heat insulation layer coating liquid is provided, and the heat insulation layer coating liquid is applied to the side of the substrate near the light source and cured to obtain a heat insulation layer.
[0034] A quantum dot mixture is provided, and the quantum dot mixture is coated on the light-emitting side of the heat insulation layer;
[0035] A preset mold is set on the light-emitting side of the quantum dot mixture and photocured to obtain a quantum dot film and generate a backlight module.
[0036] In one embodiment, the heat insulation coating liquid comprises a second matrix resin and porous silica, wherein the mass ratio of the porous silica to the second matrix resin is 1:(20-50).
[0037] In addition, to achieve the above objectives, this application also proposes a display panel, which includes: a quantum dot film as described above or a backlight module as described above.
[0038] One or more technical solutions proposed in this application have at least the following technical effects: A quantum dot film is provided, comprising: a resin layer; a plurality of quantum dots, each quantum dot embedded in the resin layer; the quantum dots in the resin layer can absorb blue light energy in light energy, forming hole-electron pair recombination, thereby generating purer green and red light energy and improving the color gamut. Further, the resin layer also includes at least one high-brightness region, at least one low-brightness region, and a transition region located between the high-brightness region and the low-brightness region, wherein the thickness of the high-brightness region is less than the thickness of the low-brightness region, the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region, and the concentration of quantum dots in the resin layer is directly proportional to the thickness of the resin layer. Because the concentration of quantum dots in the resin layer is directly proportional to the thickness of the resin layer—meaning the concentration of quantum dots in the high-brightness region of the quantum dot film is lower than that in the transition region, and vice versa—under the same light source intensity, the light intensity emitted by the high-brightness region of the quantum dot film will be lower than that emitted by the transition region, and vice versa. Furthermore, if the quantum dot film is applied to a practical backlight module, since the light emitted by the backlight module's light source has a Lambau pattern (maximum intensity at the center and weaker intensity around the edges), if the high-brightness region of the quantum dot film is positioned corresponding to the center of the light source, and the low-brightness region is positioned corresponding to the edge of the light source, the luminous efficiency of the high-brightness region will be lower than that of the low-brightness region. This improves the uneven light emission caused by excessive light intensity at the center of the light source (corresponding to the high-brightness region) and weak light intensity at the edge of the light source (corresponding to the low-brightness region), resulting in more uniform light output from the backlight module. By setting the quantum dot film to a structure with varying thickness, the light uniformity of the quantum dot film is greatly improved, and in practical applications, it can make the backlight module emit light uniformly. Attached Figure Description
[0039] Figure 1 This is a schematic diagram of the structure of the quantum dot film involved in the embodiments of this application;
[0040] Figure 2 This is another structural schematic diagram of the quantum dot film involved in the embodiments of this application;
[0041] Figure 3 This is a schematic diagram of the structure of the quantum dots involved in the embodiments of this application;
[0042] Figure 4 This is a schematic diagram of the light intensity distribution of the light source involved in the embodiments of this application;
[0043] Figure 5 This is a schematic diagram of the backlight module involved in the embodiments of this application;
[0044] Figure 6This is another structural schematic diagram of the backlight module involved in the embodiments of this application;
[0045] Figure 7 This is a flowchart of the backlight module fabrication method involved in the embodiments of this application.
[0046] The realization of the purpose, functional features and advantages of this application will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation
[0047] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions in the embodiments of this application will be clearly and completely described below. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall apply. Reagents or instruments whose manufacturers are not specified are all conventional products that can be purchased commercially.
[0048] Furthermore, the meaning of "and / or" throughout the text includes three parallel solutions. Taking "A and / or B" as an example, it includes solution A, solution B, or a solution that simultaneously satisfies A and B. In addition, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. When the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed in this application. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without inventive effort are within the scope of protection of this application.
[0049] The first aspect of this application provides a quantum dot film 100, with reference to... Figure 1 The quantum dot film 100 comprises:
[0050] Resin layer 110;
[0051] Multiple quantum dots 120 are embedded in the resin layer 110;
[0052] The resin layer 110 further includes at least one high-brightness region 130, at least one low-brightness region 140, and a transition region 150 located between the high-brightness region 130 and the low-brightness region 140, wherein the thickness of the high-brightness region 130 is less than the thickness of the low-brightness region 140, the thickness of the transition region 150 gradually increases from the side connecting the high-brightness region 130 to the side connecting the low-brightness region 140, and the concentration of quantum dots 120 in the resin layer 110 is proportional to the thickness of the resin layer 110.
[0053] Optionally, the base resin of the resin layer 110 includes optical adhesives, such as UV-curable adhesives (unsaturated polyester resin system, polyacid acrylate, epoxy acrylate, polyurethane acrylate, polythiol-polyene system, cationic curing base resin, etc.); using optical adhesives as the base resin of the resin layer 110 facilitates the rapid molding of the quantum dot film 100 and simplifies the process flow.
[0054] In one feasible implementation, refer to Figure 2 The resin layer 110 further includes bubbles 160 encapsulating the quantum dots 120, wherein the gas within the bubbles 160 includes carbon dioxide. Since carbon dioxide is stable, by encapsulating the quantum dots 120 with carbon dioxide-containing bubbles 160, a micron-scale multilayered, discontinuous bubble structure 160 is formed in the resin layer 110 of the quantum dot film 100. This protects the quantum dots 120, isolating them from oxygen, moisture, etc., preventing fluorescence quenching and inactivation, and improving the stability of the quantum dot film 100.
[0055] Optionally, the gas within the bubble 160 may also include an inert gas, such as helium (He), neon (Ne), argon (Ar), krypton (Kr), xenon (Xe), nitrogen (N2), etc. By encapsulating the quantum dot 120 with the bubble 160, the quantum dot 120 is protected, isolating it from oxygen, moisture, etc., thereby preventing the quantum dot 120 from fluorescence quenching and inactivation, and improving the stability of the quantum dot film 100.
[0056] In one feasible implementation, refer to Figure 3 The quantum dot 120 includes a quantum dot core 121 and a coating layer 122 covering the quantum dot core 121, wherein the surface of the coating layer 122 is connected with bicarbonate ions. By coating the quantum dot 120 with the coating layer 122, it can provide insulation against temperature, water, and oxygen. Simultaneously, the coating layer 122 can appropriately isolate the quantum dot 120 from the erosion caused by temperature, moisture, and oxygen during processing, protecting the quantum dot 120 and preventing its deactivation during processing. The bicarbonate ions connected to the surface of the coating layer 122 are ligand ions that can rapidly decompose under specific light conditions to produce carbon dioxide. By connecting bicarbonate ligand ions to the surface of the coating layer 122, during the photocuring process of the quantum dot film 100 with the matrix resin, the bicarbonate ions connected to the surface of the coating layer 122 rapidly decompose, thereby generating carbon dioxide inside the matrix resin, thus forming a bubble structure 160.
[0057] Optionally, bicarbonate ions decompose to produce carbon dioxide when irradiated with light at a wavelength of 200–240 nm.
[0058] Optionally, the quantum dot core 121 comprises a group II-VI compound.
[0059] In one feasible embodiment, the quantum dot core 121 includes at least one of CdSe, CdS, InP, PbSe, and CdTe.
[0060] Preferably, the quantum dot core 121 comprises CdSe.
[0061] In one feasible embodiment, the material of the coating layer 122 includes at least one of ZnS, PbS, and CdS. The coating layer 122 is a metal sulfide, while the matrix resin is an organic material. The significant difference in properties between the two results in low adhesion between the quantum dots 120 and the matrix resin, creating voids. Consequently, the carbon dioxide generated from the decomposition of bicarbonate ligand ions connected to the surface of the coating layer 122 can more easily form bubbles 160. If the coating layer 122 is replaced with an organic material, such as a copolymer resin, the quantum dots 120 may adhere more tightly to the matrix resin, making it difficult to form the bubble 160 structure.
[0062] Preferably, the material of the coating layer 122 includes ZnS.
[0063] In this embodiment, at least one of CdSe, CdS, InP, PbSe, and CdTe can be selected as the quantum dot core 121 in the quantum dot 120. Then, based on considerations of lattice matching, band structure, and physicochemical properties, at least one of ZnS, PbS, and CdS is selected as the coating layer 122 of the quantum dot 120. Since the lattice constants of the quantum core 121 and the coating layer 122 are similar, good lattice matching can be achieved, allowing the coating layer 122 to tightly cover the surface of the quantum dot core 121, thereby improving the stability and performance of the quantum dot 120. Furthermore, the band structure of the coating layer 122 is similar to that of the quantum dot core 121, enabling the coating layer 122 to form a good energy level structure with the quantum dot core 121, thereby optimizing the optical and electronic properties of the quantum dot 120. Furthermore, to ensure that each quantum dot 120 in the resin layer 110 of the quantum dot film 100 can be encapsulated by the bubbles 160, in this embodiment, bicarbonate ligand ions are attached to the surface of the coating layer 122. Since bicarbonate ligand ions have a certain coordination ability in chemistry and can form coordination bonds with metal ions, they can adhere well to the outside of the metal sulfide coating layer 122. If the coating layer 122 is made of other inorganic materials, such as silicon dioxide, since the structure of silicon dioxide is mainly composed of covalent bonds between silicon and oxygen, forming a very stable network structure, this structure makes it difficult for silicon dioxide to form strong chemical bonds with other ions or molecules. Therefore, the binding ability of bicarbonate ligand ions to porous silicon dioxide is relatively weak. Thus, in this embodiment, a metal sulfide is used as the coating layer 122. In addition, if foaming material is added directly during the preparation of the quantum dot film 100, although a bubble structure can be generated, the foaming material may not be able to get close to all the quantum dots 120 during mixing. As a result, after the bubbles are generated, a large number of quantum dots 120 may not be encapsulated by the bubbles, but may be directly embedded in the matrix resin, resulting in poor stability of these unencapsulated quantum dots. In this embodiment, since a metal sulfide is selected as the coating layer 122, bicarbonate ligand ions can be attached to the surface of the coating layer 122 of each quantum dot 120, so that each quantum dot 120 can be encapsulated by the carbon dioxide bubbles 160 generated by the decomposition of bicarbonate, ensuring the stability of the quantum dots 120 in the quantum dot film 100.
[0064] In one feasible embodiment, the thickness of the coating layer 122 is 1–3 nm; for example, 1 nm, 1.5 nm, 2 nm, 2.5 nm, 3 nm, etc. If the thickness of the coating layer 122 is too small, it may be difficult to provide protection for the quantum dots 120 it coats, causing the quantum dots 120 to become inactive due to the influence of temperature, humidity, and oxygen during processing and use; if the thickness of the coating layer 122 is too large, it will cause more light energy loss when the quantum dot film 100 is used; therefore, the thickness of the coating layer 122 is determined to be 1–3 nm.
[0065] In one feasible embodiment, the particle size of the quantum dot core 121 includes 2-4 nm and 5-7 nm. For example, the particle size of the quantum dot core 121 includes 2 nm, 2.5 nm, 3 nm, 3.5 nm, 4 nm, etc., and also includes 5 nm, 5.5 nm, 6 nm, 6.5 nm, 7 nm, etc. Under blue light excitation, quantum dot cores 121 with a particle size of 2-4 nm can generate green light with a narrow half-width, while quantum dot cores 121 with a particle size of 5-7 nm can generate red light with a narrow half-width. The narrower the half-width, the higher the color purity of the light. Therefore, the particle size of the quantum dot core 121 includes 2-4 nm and 5-7 nm so that the quantum dot film 100 can excite green and red light with high purity. Furthermore, the green and red light generated by excitation can be mixed with the blue light emitted by the light source of the backlight module to form white light, which is used as the backlight of the display device.
[0066] In one feasible embodiment, when the quantum dot film 100 is used in actual applications, for example, when it is disposed in a backlight module, the light emitted by the light source of the backlight module exhibits a Lamborghian light pattern; see reference. Figure 4 The solid coils represent the light intensity emitted by the light source in different ranges, according to Figure 4 It is known that the light emitted by the light source has the highest intensity at the center and is weaker around the edges. However, the conventional quantum dot film 100 has poor light homogenization capability, therefore the intensity of other wavelengths of light excited by the quantum dot film 100 will also be uneven, ultimately leading to uneven light output from the backlight module. Therefore, in this embodiment, referring to... Figure 1 In the resin layer 110 of the quantum dot film 100, at least one high-brightness region 130, at least one low-brightness region 140, and a transition region 150 located between the high-brightness region 130 and the low-brightness region 140 are provided. The thickness of the high-brightness region 130 is less than the thickness of the low-brightness region 140. The thickness of the transition region 150 gradually increases from the side connecting the high-brightness region 130 to the side connecting the low-brightness region 140. The concentration of quantum dots 120 in the resin layer 110 is proportional to the thickness of the resin layer 110.
[0067] Since the concentration of quantum dots 120 in the resin layer 110 is directly proportional to the thickness of the resin layer 110, that is, the concentration of quantum dots 120 in the high-brightness region 130 of the quantum dot film 100 will be lower than that in the transition region 150, and the concentration of quantum dots 120 in the transition region 150 will be lower than that in the low-brightness region 140; therefore, under the same light source intensity, the light intensity emitted by the high-brightness region 130 of the quantum dot film 100 will be lower than that emitted by the transition region 150, and the light intensity emitted by the transition region 150 will be lower than that emitted by the low-brightness region 140. Furthermore, if the quantum dot film 100 is applied to an actual backlight module, since the light emitted by the backlight module's light source has the highest intensity at the center and weaker intensity around the edges, if the high-brightness area 130 of the quantum dot film 100 is set to correspond to the center position of the light source, and the low-brightness area 140 is set to correspond to the edge position of the light source, the luminous efficiency of the high-brightness area 130 will be lower than that of the low-brightness area 140. This improves the uneven light emission phenomenon caused by the excessive light intensity at the center position of the light source (i.e., the position corresponding to the high-brightness area 130) and the weak light intensity at the edge position of the light source (i.e., the position corresponding to the low-brightness area 140), making the backlight module emit light uniformly. By adjusting the thickness of the quantum dot film 100 (i.e., the resin layer 110), the concentration of quantum dots 120 in each region can be controlled, thereby ensuring uniform display brightness in all areas of the display device when the quantum dot film 100 is applied to the display device. This effectively improves uneven brightness, bright edges, and dark corners in the display device, while also saving the cost of expensive diffuser plates in the display device.
[0068] Optionally, when the quantum dot film 100 is applied to the backlight module, the high-brightness area 130 of the quantum dot film 100 can correspond to the strong light area of the light source of the backlight module. That is, the concentration of quantum dots 120 in the quantum dot film 100 in the strong light area is slightly lower, thereby reducing the light energy emitted by the quantum dot film 100 corresponding to the strong light area, so as to weaken the emitted light energy of the strong light area and achieve the effect of reducing the brightness of the strong light area.
[0069] Optionally, when the quantum dot film 100 is applied to the backlight module, the low-brightness area 140 of the quantum dot film 100 can correspond to the weak light area of the light source of the backlight module, that is, the quantum dots 120 in the quantum dot film 100 in the weak light area are more concentrated, thereby increasing the light energy excited by the quantum dot film 100 in the weak light area, so as to enhance the emitted light energy of the weak light area and achieve the effect of improving the brightness of the weak light area.
[0070] In one feasible embodiment, the thickness of the high-brightness region 130 is 5–8 μm; for example, 5 μm, 5.5 μm, 6 μm, 6.5 μm, 7 μm, 7.5 μm, 8 μm, etc. If the thickness of the high-brightness region 130 is too low, the concentration of quantum dots 120 contained in the high-brightness region 130 will be too low, making it difficult to excite sufficient light intensity, and ultimately causing the corresponding area of the display device to be too dark; while if the thickness of the high-brightness region 130 is too high, the concentration of quantum dots 120 contained in the high-brightness region 130 will be too high, resulting in excessively high light intensity, and ultimately causing the corresponding area of the display device to be too bright. Therefore, the thickness of the high-brightness region 130 is determined to be 5–8 μm.
[0071] In one feasible embodiment, the thickness of the low-brightness region 140 is 10–15 μm; for example, 10 μm, 10.5 μm, 11 μm, 11.5 μm, 12 μm, 12.5 μm, 13 μm, 14 μm, 15 μm, etc. If the thickness of the low-brightness region 140 is too low, the concentration of quantum dots 120 contained in the low-brightness region 140 will be too low, making it difficult to excite sufficient light intensity, and ultimately causing the corresponding area of the display device to be too dark; while if the thickness of the low-brightness region 140 is too high, the concentration of quantum dots 120 contained in the low-brightness region 140 will be too high, resulting in excessively high light intensity, and ultimately causing the corresponding area of the display device to be too bright. Therefore, the thickness of the low-brightness region 140 is determined to be 10–15 μm.
[0072] In this embodiment, by embedding quantum dots 120 within the resin layer 110, the resin in the resin layer 110 protects the quantum dots 120, isolating them from oxygen, moisture, etc., thus preventing the quantum dots 120 from fluorescence quenching and inactivation, and improving the stability of the quantum dot film 100. The quantum dots 120 in the resin layer 110 can absorb blue light energy, forming hole-electron pair recombination, thereby generating purer green and red light energy and improving the color gamut. Furthermore, the resin layer 110 also includes at least one high-brightness region 130, at least one low-brightness region 140, and a transition region 150 located between the high-brightness region 130 and the low-brightness region 140. The thickness of the high-brightness region 130 is less than the thickness of the low-brightness region 140, and the thickness of the transition region 150 gradually increases from the side connecting the high-brightness region 130 to the side connecting the low-brightness region 140. The concentration of quantum dots 120 in the resin layer 110 is directly proportional to the thickness of the resin layer 110. Since the concentration of quantum dots 120 in the resin layer 110 is directly proportional to the thickness of the resin layer 110, that is, the concentration of quantum dots 120 in the high-brightness region 130 of the quantum dot film 100 will be lower than that in the transition region 150, and the concentration of quantum dots 120 in the transition region 150 will be lower than that in the low-brightness region 140; therefore, under the same light source intensity, the light intensity emitted by the high-brightness region 130 of the quantum dot film 100 will be lower than that emitted by the transition region 150, and the light intensity emitted by the transition region 150 will be lower than that emitted by the low-brightness region 140. Furthermore, if the quantum dot film 100 is applied to an actual backlight module, since the light emitted by the backlight module's light source has a Lambau pattern (i.e., the intensity is highest at the center and weaker at the edges), if the high-brightness area 130 of the quantum dot film 100 is positioned corresponding to the center of the light source, and the low-brightness area 140 is positioned corresponding to the edge of the light source, the luminous efficiency of the high-brightness area 130 will be lower than that of the low-brightness area 140. This improves the uneven light emission phenomenon caused by excessive light intensity at the center of the light source (i.e., the position corresponding to the high-brightness area 130) and weak light intensity at the edge of the light source (i.e., the position corresponding to the low-brightness area 140), resulting in uniform light output from the backlight module. By setting the quantum dot film 100 to a structure with varying thickness, the light uniformity of the quantum dot film 100 is significantly improved, enabling uniform light output from the backlight module in practical applications.
[0073] A second aspect of this application provides a method for preparing a quantum dot film, the method comprising the following steps:
[0074] Step S10: Mix quantum dots with the first matrix resin to obtain a quantum dot mixture;
[0075] In one feasible embodiment, a first matrix resin and quantum dots are mixed to obtain a quantum dot mixture.
[0076] Optionally, the mass ratio between the first matrix resin and the quantum dots is 1:(50-500); for example, the mass ratio between the first matrix resin and the quantum dots is 1:50, 1:100, 1:200, 1:300, 1:400, 1:500, etc. Since light energy is reflected and refracted at the interface between the bubbles and the first matrix resin after incident on the quantum dot film, and the refracted light energy reaches the next interface and repeats the reflection and refraction, given a fixed substrate, the more layers of the bubble structure, the higher the photoluminescence efficiency of the quantum dot film. Increasing the quantum dot content in the quantum dot mixture can effectively increase the number of stacked layers of the bubble structure in the prepared quantum dot film, thereby improving the photoluminescence efficiency of the quantum dot film. However, if the quantum dot content is too high, it may be difficult for the quantum dots to be completely encapsulated in the first matrix resin, i.e., the quantum dots are exposed in the resin layer, causing quantum dot deactivation.
[0077] Optionally, the first matrix resin includes an optical adhesive, such as a UV-curable adhesive; using an optical adhesive as the first matrix resin facilitates the rapid prototyping of quantum dot films and simplifies the process flow.
[0078] In one feasible embodiment, the quantum dot comprises: a quantum dot core and a coating layer covering the quantum dot core, wherein the surface of the coating layer is connected to bicarbonate ions. By coating the quantum dot, it can provide insulation against temperature, water, and oxygen. Simultaneously, the coating layer can appropriately isolate the quantum dot from the erosion caused by temperature, moisture, and oxygen during processing, protecting the quantum dot and preventing its deactivation during processing. The bicarbonate ions connected to the surface of the coating layer are ligand ions that can rapidly decompose under specific light conditions to produce carbon dioxide. By connecting bicarbonate ligand ions to the surface of the coating layer, during the photocuring process of the quantum dot film with the first matrix resin, the bicarbonate ions connected to the surface of the coating layer rapidly decompose, thereby generating carbon dioxide inside the first matrix resin, thus forming a bubble structure.
[0079] Optionally, the quantum dot core comprises a group II-VI compound.
[0080] In one feasible embodiment, the quantum dot core includes at least one of CdSe, CdS, InP, PbSe, and CdTe.
[0081] Preferably, the quantum dot core comprises CdSe.
[0082] In one feasible embodiment, the coating layer material includes at least one of ZnS, PbS, and CdS. The coating layer material is a metal sulfide, while the first matrix resin is an organic material. The significant difference in properties between the two results in low adhesion between the quantum dots and the first matrix resin, creating voids. Consequently, the carbon dioxide generated from the decomposition of bicarbonate ligand ions connected to the coating layer surface can more easily form bubbles. If the coating layer is replaced with an organic material, such as a copolymer resin, the quantum dots may adhere more tightly to the first matrix resin, making bubble formation difficult.
[0083] Preferably, the material of the coating layer includes ZnS.
[0084] Optionally, the resin layer may further include multiple embedded quantum dots that are not encapsulated by the air bubbles, meaning that some quantum dots are directly embedded in the first matrix resin. Since the quantum dot cores are encapsulated by the coating layer, if the coating layer is thick enough to provide insulation against temperature, water, and oxygen, the quantum dots in the resin layer that are not encapsulated by the air bubbles can also have good stability.
[0085] In one feasible embodiment, the thickness of the coating layer is 1–3 nm; for example, 1 nm, 1.5 nm, 2 nm, 2.5 nm, 3 nm, etc. If the thickness of the coating layer is too small, it may be difficult to provide protection for the quantum dots it coats, causing the quantum dots to become inactive due to the influence of temperature, humidity, and oxygen during processing and use; if the thickness of the coating layer is too large, it will cause more light energy loss when the quantum dot film is used; therefore, the thickness of the coating layer is determined to be 1–3 nm.
[0086] In one feasible embodiment, the particle size of the quantum dot core includes 2-4 nm and 5-7 nm. For example, the particle size of the quantum dot core includes 2 nm, 2.5 nm, 3 nm, 3.5 nm, 4 nm, etc., and also includes 5 nm, 5.5 nm, 6 nm, 6.5 nm, 7 nm, etc. Under blue light excitation, quantum dot cores with a particle size of 2-4 nm can generate green light with a narrow half-width, while quantum dot cores with a particle size of 5-7 nm can generate red light with a narrow half-width. The narrower the half-width, the higher the color purity of the light. Therefore, the particle size of the quantum dot core includes 2-4 nm and 5-7 nm so that the quantum dot film can excite green and red light with high purity. Furthermore, the green and red light generated by excitation can be mixed with the blue light emitted by the light source of the backlight module to form white light, which is used as the backlight of the display device.
[0087] Step S20: The quantum dot mixture is added to a preset mold for photocuring to obtain a quantum dot film.
[0088] In one feasible embodiment, the quantum dot film mixture is combined with a preset mold, for example, the quantum dot mixture is added into the mold; the quantum dot film mixture can also be coated on the surface of a preset substrate, and a mold is set on the surface of the quantum dot film mixture. The thickness of the quantum dot film is controlled by the structure of the mold and the extrusion; then photocuring is performed to obtain the quantum dot film.
[0089] In one feasible embodiment, the wavelength of the light source for photocuring is 200–240 nm; for example, 200 nm, 210 nm, 220 nm, 230 nm, 240 nm, etc.; the bicarbonate ligand ions connected to the surface of the coating layer can rapidly decompose to produce carbon dioxide under irradiation with light of wavelength 200–240 nm, thereby forming a bubble structure encapsulating quantum dots in the resin layer of the quantum dot film. At the same time, the first matrix resin of the resin layer can be a UV-curable adhesive; therefore, the wavelength of the light source for photocuring can be 200–240 nm, or a light source containing a wavelength of 200–240 nm, so as to achieve the simultaneous development of bubble structure and curing.
[0090] In one feasible embodiment, the photocuring time is 5 to 10 seconds, for example, 5 seconds, 6 seconds, 7 seconds, 8 seconds, 9 seconds, 10 seconds, etc.; the bicarbonate ligand ions connected to the surface of the coating layer can decompose rapidly to generate carbon dioxide, and the first matrix resin of the resin layer can also be cured rapidly. Therefore, the photocuring time can be 5 to 10 seconds to save preparation time and improve the preparation efficiency of quantum dot film.
[0091] Optionally, the photocuring temperature can be 20-35℃.
[0092] Optionally, the resin layer includes at least one high-brightness region, at least one low-brightness region, and a transition region between the high-brightness region and the low-brightness region. The thickness of the high-brightness region is less than the thickness of the low-brightness region, and the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region. The quantum dot concentration in the resin layer is directly proportional to the thickness of the resin layer. The high-brightness region of the quantum dot film can appropriately reduce the light intensity corresponding to the center position of the light source, while the low-brightness region of the quantum dot film can appropriately increase the light intensity corresponding to the surrounding positions of the light source, thus making the backlight module emit light uniformly.
[0093] Optionally, the thickness of the high-brightness region is 5–8 μm, and the thickness of the low-brightness region is 10–15 μm.
[0094] Optionally, the resin layer may further include multiple embedded quantum dots that are not encapsulated by the air bubbles, meaning that some quantum dots are directly embedded in the first matrix resin. Since the quantum dot cores are encapsulated by the coating layer, if the coating layer is thick enough to provide insulation against temperature, water, and oxygen, the quantum dots in the resin layer that are not encapsulated by the air bubbles can also have good stability.
[0095] In this embodiment, a quantum dot mixture is obtained by mixing quantum dots with a first matrix resin. The quantum dot mixture is then added to a pre-set mold for photocuring. Photocuring causes the bicarbonate ions attached to the surface of the quantum dot coating to decompose, generating carbon dioxide, which in turn generates carbon dioxide within the first matrix resin, thus forming a bubble structure. Simultaneously, the first matrix resin can be an optical adhesive, allowing for simultaneous bubble formation and curing to produce a quantum dot film. Compared to conventional quantum dot film preparation processes, the mold-curing method greatly simplifies the process, reduces costs, and improves preparation efficiency.
[0096] A third aspect of this application provides a backlight module, which includes a quantum dot film. The quantum dot film includes a resin layer and a plurality of quantum dots embedded in the resin layer. The resin layer includes at least one high-brightness region, at least one low-brightness region, and a transition region between the high-brightness region and the low-brightness region. The thickness of the high-brightness region is less than the thickness of the low-brightness region, and the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region. The concentration of quantum dots in the resin layer is proportional to the thickness of the resin layer.
[0097] Optionally, the resin layer further includes bubbles encapsulating the quantum dots, wherein the gas within the bubbles includes carbon dioxide.
[0098] Optionally, the quantum dot includes: a quantum dot core and a coating layer covering the quantum dot core, wherein the surface of the coating layer is connected with bicarbonate ions.
[0099] Optionally, the quantum dot core includes at least one of CdSe, CdS, InP, PbSe, and CdTe.
[0100] Optionally, the coating material includes at least one of ZnS, PbS, and CdS.
[0101] Optionally, the thickness of the coating layer is 1 to 3 nm.
[0102] Optionally, the particle size of the quantum dot core includes 2-4 nm and 5-7 nm.
[0103] In one feasible implementation, refer to Figure 5 The backlight module includes:
[0104] substrate 200;
[0105] Optionally, the substrate 200 can be a PCB (Printed Circuit Board).
[0106] A light source 300 is disposed on one side of the substrate 200;
[0107] Optionally, the light source 300 is electrically connected to the substrate 200. The light source 300 can be an LED (light-emitting diode), mini LED, etc., and this embodiment does not limit it.
[0108] A heat insulation layer 400 is disposed on the side of the substrate 200 near the light source 300 and wraps around the light source 300;
[0109] In one feasible embodiment, the heat insulation layer 400 can isolate the heat generated when the light source 300 emits light, avoid affecting the quantum dots in the quantum dot film 100, and improve the stability of the quantum dot film 100; at the same time, it can protect the light source 300.
[0110] A quantum dot film 100 is disposed on the light-emitting side of the heat insulation layer 400, wherein the high-brightness area of the quantum dot film 100 corresponds to the strong light area of the light source 300, and the low-brightness area of the quantum dot film 100 corresponds to the weak light area of the light source 300, and the light energy intensity of the strong light area is greater than that of the weak light area.
[0111] In one feasible embodiment, since the light emitted by the light source 300 has the highest intensity at its center and is weaker around the edges, the area covered by the light emitted by each light source 300 can be divided into a strong light area, a weak light area, and an intermediate area. The strong light area is close to the center of the light source 300, the weak light area is far from the center, and the intermediate area is located between the strong light area and the weak light area. The light intensity of the strong light area is greater than that of the intermediate area, and the light intensity of the intermediate area is greater than that of the weak light area. Therefore, when setting the quantum dot film 100, the high-brightness area of the quantum dot film 100 can be aligned with the strong light area of the light source 300, the low-brightness area of the quantum dot film 100 can be aligned with the weak light area of the light source 300, and the transition area of the quantum dot film 100 can be aligned with the intermediate area. Furthermore, since the thickness of the high-brightness region of the quantum dot film 100 is relatively small, while the light energy intensity of the strong light region of the light source 300 is relatively large, the luminous efficiency of the high-brightness region will be lower than that of the low-brightness region. This improves the uneven light emission phenomenon caused by the excessive light intensity in the strong light region of the light source 300 (i.e., the position corresponding to the high-brightness region) and the weak light intensity in the weak light region of the light source 300 (i.e., the position corresponding to the low-brightness region), thus achieving a uniform light effect.
[0112] For example, refer to Figure 6 The light emitted by the light source 300 includes a first solid angle range 310 corresponding to the strong light area, a second solid angle range 320 and a third solid angle range 330 corresponding to the intermediate area, and a fourth solid angle range 340 and a fifth solid angle range 350 corresponding to the weak light area. The maximum value of the fifth solid angle range 350 is less than the minimum value of the third solid angle range 330, and the maximum value of the third solid angle range 330 is less than the minimum value of the first solid angle range 310. The maximum value of the first solid angle range 310 is less than the minimum value of the second solid angle range 320, and the maximum value of the second solid angle range 320 is less than the minimum value of the fourth solid angle range 340.
[0113] In one feasible embodiment, the height difference between the heat insulation layer 400 and the light source 300 is 0.5–2 mm; for example, 0.5 mm, 0.6 mm, 0.8 mm, 1 mm, 1.2 mm, 1.4 mm, 1.6 mm, 1.8 mm, 2 mm, etc. If the height difference between the heat insulation layer 400 and the light source 300 is too small, it indicates that the heat insulation layer 400 is too thin, resulting in poor heat insulation. If the height difference between the heat insulation layer 400 and the light source 300 is too large, it indicates that the heat insulation layer 400 is too thick, leading to light energy loss. Therefore, the height difference between the heat insulation layer 400 and the light source 300 is determined to be 0.5–2 mm.
[0114] In one feasible embodiment, the material of the heat insulation layer 400 includes porous silica. Porous silica has a melting point above 1600°C and has good heat insulation properties.
[0115] In this embodiment, by providing a heat insulation layer 400 between the light source 300 and the quantum dot film 100 in the backlight module, the heat generated when the light source 300 emits light can be isolated, preventing any impact on the quantum dots in the quantum dot film 100 and improving the stability of the quantum dot film 100; at the same time, it can protect the light source 300. Furthermore, the quantum dot film 100 in the backlight module includes a thin strong light region, a moderately thick transition region, and a thick weak light region, which are respectively provided corresponding to the strong light region, intermediate region, and weak light region of the light source 300, so that the quantum dot film 100 has good light uniformity, thereby making the light output of the backlight module uniform.
[0116] A fourth aspect of this application provides a method for manufacturing a backlight module, referring to... Figure 7 The backlight module manufacturing method includes the following steps:
[0117] Step A10: Set a light source on the substrate;
[0118] In one feasible embodiment, a light source is placed on a pre-prepared substrate and electrically connected to the substrate.
[0119] Step A20: Provide a heat insulation layer coating liquid, apply the heat insulation layer coating liquid to the side of the substrate near the light source, and cure it to obtain a heat insulation layer;
[0120] In one feasible embodiment, a heat insulation coating liquid is provided, and then the heat insulation coating liquid is applied to the side of the substrate near the light source and cured to form a heat insulation layer.
[0121] Optionally, the heat insulation coating liquid includes a second matrix resin and porous silica, wherein the second matrix resin can be an optical adhesive, such as a UV-curable adhesive.
[0122] For example, a second matrix resin is mixed with porous silica to obtain a heat insulation layer coating liquid, wherein the second matrix is an optical adhesive; the heat insulation layer coating liquid is applied to the side of the substrate near the light source and photocured under light with a wavelength of 10-400 nm for 10-15 s to form a heat insulation layer.
[0123] Optionally, the mass ratio of the porous silica to the second matrix resin is 1:(20-50); for example, 1:20, 1:25, 1:30, 1:35, 1:40, 1:45, 1:50, etc. Increasing the content of porous silica in the insulating layer coating liquid can effectively improve the heat insulation effect of the obtained insulating layer; however, if the content of porous silica is too high, it may make the insulating layer structure too dense, which may reduce its heat insulation effect. Therefore, the mass ratio of porous silica to the second matrix resin is determined to be 1:(20-50).
[0124] Step A30: Provide a quantum dot mixture and coat the quantum dot mixture on the light-emitting side of the heat insulation layer;
[0125] In one feasible embodiment, quantum dots are mixed with a first matrix resin to obtain a quantum dot mixture, wherein the mass ratio between the quantum dots and the first matrix resin is 1:(50-500); and then the quantum dot mixture is uniformly coated on the light-emitting side of the heat insulation layer.
[0126] Step A40: A preset mold is set on the light-emitting side of the quantum dot mixture and photocured to obtain a quantum dot film and generate a backlight module.
[0127] In one feasible embodiment, a preset mold is set on the light-emitting side of the quantum dot mixture to fix the shape of the quantum dot film, so that the quantum dot film includes at least one high-brightness region, at least one low-brightness region, and a transition region located between the high-brightness region and the low-brightness region. The thickness of the high-brightness region is less than the thickness of the low-brightness region, and the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region. The quantum dot concentration in the resin layer is proportional to the thickness of the resin layer. Then, the film is photocured at a wavelength of 200-240 nm for 5-10 s to obtain the quantum dot film and generate a backlight module.
[0128] A fifth aspect of this application provides a display panel, the display panel including the quantum dot film as described above, or the backlight module as described above.
[0129] In one feasible embodiment, the quantum dot film includes: a resin layer; a plurality of quantum dots, each quantum dot being embedded in the resin layer; the resin layer includes at least one high-brightness region, at least one low-brightness region, and a transition region located between the high-brightness region and the low-brightness region; wherein the thickness of the high-brightness region is less than the thickness of the low-brightness region, the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region, and the quantum dot concentration in the resin layer is proportional to the thickness of the resin layer.
[0130] In one feasible embodiment, the resin layer further includes bubbles encapsulating the quantum dots, wherein the gas within the bubbles includes carbon dioxide.
[0131] In one feasible embodiment, the quantum dot includes: a quantum dot core and a coating layer covering the quantum dot core, wherein the surface of the coating layer is connected with bicarbonate ions.
[0132] In one feasible embodiment, the quantum dot core comprises at least one of CdSe, CdS, InP, PbSe, and CdTe; and / or, the coating layer comprises at least one of ZnS, PbS, and CdS; and / or, the coating layer has a thickness of 1–3 nm; and / or, the quantum dot core has a particle size of 2–4 nm and 5–7 nm.
[0133] In one feasible embodiment, the thickness of the high-brightness region is 5-8 μm, and the thickness of the low-brightness region is 10-15 μm.
[0134] In one feasible embodiment, the backlight module includes: a substrate; a light source disposed on one side of the substrate; a heat insulation layer disposed on the side of the substrate close to the light source and enclosing the light source; and a quantum dot film disposed on the light-emitting side of the heat insulation layer, wherein the high-brightness area of the quantum dot film corresponds to the strong light area of the light source, the low-brightness area of the quantum dot film corresponds to the weak light area of the light source, and the light energy intensity of the strong light area is greater than the light energy intensity of the weak light area.
[0135] In one feasible embodiment, the height difference between the heat insulation layer and the light source is 0.5 to 2 mm; and / or, the material of the heat insulation layer includes porous silicon dioxide.
[0136] The above are merely preferred embodiments of this application and do not limit the patent scope of this application. Various modifications and variations can be made to this application by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the patent protection scope of this application.
Claims
1. A quantum dot film, characterized in that, The quantum dot film comprises: Resin layer; Multiple quantum dots are embedded in the resin layer; wherein each quantum dot includes a quantum dot core and a coating layer covering the quantum dot core, wherein the surface of the coating layer is connected to bicarbonate ions; the resin layer also includes bubbles encapsulating the quantum dots, wherein the gas inside the bubbles includes carbon dioxide; the bicarbonate ions decompose during photocuring to produce the carbon dioxide and generate the bubbles; The resin layer includes at least one high-brightness region, at least one low-brightness region, and a transition region located between the high-brightness region and the low-brightness region; The thickness of the high-brightness region is less than the thickness of the low-brightness region, the thickness of the transition region gradually increases from the side connecting the high-brightness region to the side connecting the low-brightness region, and the quantum dot concentration in the resin layer is directly proportional to the thickness of the resin layer; the thickness of the high-brightness region is 5~8μm, and the thickness of the low-brightness region is 10~15μm. The quantum dot film is prepared by photocuring.
2. The quantum dot film of claim 1, wherein, The quantum dot core includes at least one of CdSe, CdS, InP, PbSe, and CdTe; And / or, the material of the coating layer includes at least one of ZnS, PbS and CdS; And / or, the thickness of the coating layer is 1~3 nm; And / or, the particle size of the quantum dot core includes 2~4nm and 5~7nm.
3. A method for preparing a quantum dot film, characterized by, The quantum dot film preparation method is applied to the preparation of quantum dot films as described in any one of claims 1 to 2, and includes the following steps: Quantum dots are mixed with a first matrix resin to obtain a quantum dot mixture; The quantum dot mixture is added to a pre-set mold for photocuring to obtain a quantum dot film.
4. The quantum dot film production method of claim 3, wherein, The mass ratio of the quantum dots to the first matrix resin is 1:(50~500); And / or, the wavelength of the light source for photocuring is 200~240nm, and the photocuring time is 5~10s.
5. A backlight module, characterized in that, The backlight module includes a quantum dot film as described in any one of claims 1 to 2.
6. The backlight module of claim 5, wherein, The backlight module includes: substrate; A light source is disposed on one side of the substrate; A heat insulation layer is disposed on the side of the substrate near the light source and encloses the light source; The quantum dot film is disposed on the light-emitting side of the heat insulation layer, wherein the high-brightness region of the quantum dot film corresponds to the strong light region of the light source, and the low-brightness region of the quantum dot film corresponds to the weak light region of the light source, and the light energy intensity of the strong light region is greater than that of the weak light region.
7. The backlight module of claim 6, wherein, The height difference between the heat insulation layer and the light source is 0.5~2mm; And / or, the material of the insulation layer includes: porous silica.
8. A method for manufacturing a backlight module, characterized in that, The backlight module manufacturing method is applied to the manufacturing of a backlight module as described in any one of claims 5 to 7, and includes the following steps: A light source is placed on the substrate; A heat insulation layer coating liquid is provided, and the heat insulation layer coating liquid is applied to the side of the substrate near the light source and cured to obtain a heat insulation layer. A quantum dot mixture is provided, and the quantum dot mixture is coated on the light-emitting side of the heat insulation layer; A preset mold is set on the light-emitting side of the quantum dot mixture and photocured to obtain a quantum dot film and generate a backlight module.
9. The backlight module manufacturing method as described in claim 8, characterized in that, The heat insulation coating liquid comprises: a second matrix resin and porous silica, wherein the mass ratio of the porous silica to the second matrix resin is 1:(20~50).
10. A display panel, characterized in that, The display panel includes: a quantum dot film as described in any one of claims 1 to 2, or a backlight module as described in any one of claims 5 to 7.
Citation Information
Patent Citations
Compound and preparation method thereof, and light conversion device and display device comprising same
CN113980400A
Quantum dot film, manufacturing method thereof, and display panel
US20230155076A1