A method for intelligent management of production data for lithium battery diaphragm processing
Through the modular processing of lithium battery separator processing and multi-dimensional data analysis, the problem of incomplete data management in the existing technology is solved, and the fine monitoring of the coating thickness and uniformity of lithium battery separator and dynamic prompts of the overall quality status are realized. , improves the data management effect of lithium battery separator processing.
Patent Information
- Application Number
- CN202410738688.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-06-07
AI Technical Summary
The existing lithium battery separator processing and production data management solution cannot perform local data management prompts from multiple dimensions, resulting in incomplete analysis of the coating status and affecting the overall processing effect.
By modularizing the substrate coated with lithium battery separator, multi-dimensional static testing is performed, thickness and uniformity data are obtained, local and overall data processing is performed, analysis results are integrated, and quality status and alarm prompts are generated.
It improves the diversity and reliability of coating thickness and uniformity data processing, realizes dynamic monitoring and alarm of overall quality status, and improves the overall effect of lithium battery separator processing and production data management.
Smart Images

Figure CN118551934B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of production management, and in particular to an intelligent management method for lithium battery diaphragm processing production data. Background Art
[0002] Lithium battery separator is an important component of lithium battery, which is used to prevent direct contact between positive and negative electrodes while allowing ions to pass; the general steps of lithium battery separator processing are raw material preparation, solution preparation, coating, drying, embossing, cutting and packaging; some problems may be encountered during the production process of lithium battery separator. For example, during the coating process, the separator material needs to be evenly covered on the substrate. If the coating is uneven, it may cause inconsistent separator thickness, affecting the performance and safety of the battery.
[0003] When implementing the existing lithium battery diaphragm processing and production data management solution, it is unable to implement multi-dimensional local data management prompts for the coating status of the lithium battery diaphragm after processing and coating from different aspects, and integrate the analysis results from different aspects to implement overall processing data management prompts, resulting in poor overall effect of lithium battery diaphragm processing and production coating data processing and analysis management. Summary of the invention
[0004] The purpose of the present invention is to provide a method for intelligent management of lithium battery diaphragm processing and production data, which is used to solve the technical problem that the existing scheme cannot implement multi-dimensional local data management prompts on the coating status of the lithium battery diaphragm after processing and coating from different aspects, and integrate the analysis results from different aspects to implement overall processing data management prompts.
[0005] The purpose of the present invention can be achieved through the following technical solutions:
[0006] A method for intelligent management of lithium battery separator processing production data, comprising:
[0007] Modular processing is performed on the substrate coated with the lithium battery separator to obtain a number of divided areas, multi-dimensional static tests are performed on the divided areas in sequence, and the data of the multi-dimensional static tests are processed and combined to obtain a static test data set consisting of thickness measurement data and uniform measurement data;
[0008] Perform local and overall multi-dimensional data processing and analysis on the thickness measurement data in the static test data set to determine the local and overall coating thickness qualification status of the substrate after the lithium battery separator is processed and coated and provide prompts;
[0009] Perform local and overall multi-dimensional data processing and analysis on the uniform measurement data in the static test data set to determine the local and overall coating uniformity qualification status of the substrate after the lithium battery diaphragm is processed and coated and provide prompts;
[0010] The analysis results of multi-dimensional static tests are integrated and calculated to obtain the quality status corresponding to the lithium battery diaphragm processing, and the quality status is adaptively adjusted to dynamically prompt and warn the overall quality status of the lithium battery diaphragm processing.
[0011] Preferably, the size corresponding to the substrate coated with the lithium battery diaphragm is obtained, and the substrate coated with the lithium battery diaphragm is equally divided into a plurality of divided areas according to a preset area division ratio, and the plurality of divided areas are numbered and marked according to a preset numbering sequence, and various static tests are performed on all the divided areas;
[0012] When static testing of coating thickness dimension is performed on all divided areas, non-contact measurement is performed on the coating of several divided areas marked with numbers on the body in sequence, and the measured data is displayed through a pre-constructed thickness measurement coordinate system to obtain the thickness measurement curve of the corresponding divided area;
[0013] All corresponding thickness measurement curves are sorted and combined according to the numbers of the divided areas to obtain thickness measurement data.
[0014] Preferably, when static testing of the coating uniformity dimension is performed on all divided areas, all divided areas are divided equally twice in turn according to a preset test division ratio, and a number of divided sub-areas corresponding to the divided areas are obtained and numbered, and high-resolution scanning is performed on the coating surfaces of all divided sub-areas in different divided areas in turn to obtain the corresponding local surface roughness, and the values of all corresponding local surface roughness are extracted and sorted and combined according to the corresponding numbered marks of different divided sub-areas in the divided areas to obtain a local roughness array;
[0015] And, all local rough arrays are sorted and combined according to the number labels of all divided areas to obtain uniform measurement data.
[0016] Preferably, all thickness measurement curves of the sorted combination in the thickness measurement data are obtained and compared with the standard thickness area in the thickness measurement coordinate system in turn. If the thickness measurement curves are all in the standard thickness area, a thickness normal label is generated and its associated label identifier is set to 1, and the corresponding divided sub-area is marked as the first normal sub-area;
[0017] If the thickness measurement curve is not in the standard thickness area, a thickness anomaly label is generated and its associated flag is set to -1, and the corresponding sub-area is marked as the first abnormal sub-area. According to the thickness anomaly label, the thickness measurement curves that are not in the standard thickness area are counted and marked as abnormal curves. The length L of the abnormal curve is obtained, and the maximum value D of the abnormal curve from the standard thickness area is calculated. The abnormal impact value Y corresponding to the abnormal curve is calculated by the formula Y=L×D.
[0018] Preferably, the thickness label identifiers outputted corresponding to all the divided areas are sorted and combined to obtain a thickness analysis array, and the total number of elements N′ with a value of -1 in the thickness analysis array is traversed and counted, and the first abnormal influence degree Yy corresponding to all abnormal divided areas is calculated by the formula Yy=N′ / N; wherein N is the total number of all elements in the thickness analysis array;
[0019] And, through the formula The second anomaly influence degree Ey corresponding to all abnormal division areas is calculated; where A is the standard abnormal thickness threshold.
[0020] Preferably, when evaluating the qualified state of the overall coating thickness corresponding to the substrate after the lithium battery diaphragm is processed and coated according to the first abnormal influence degree and the second abnormal influence degree, the values of the first abnormal influence degree and the second abnormal influence degree are extracted and combined to obtain an abnormal influence array [y1, y2], and the abnormal influence array is input into a pre-built thickness data recognition model for data analysis to obtain an abnormal influence analysis array; wherein the output abnormal influence analysis array is [1, 1], [-1, 1], [1, -1] or [-1, -1];
[0021] According to the output abnormal impact analysis array, the corresponding normal and abnormal prompts of the overall coating thickness status are generated.
[0022] Preferably, all local rough arrays of sorted combinations in the uniform measurement data are obtained, and the values of all elements in the local rough arrays are obtained in turn and calculated by the formula Calculate and obtain the uniform fit degree Cy corresponding to different sub-divided areas in the corresponding divided area;
[0023] All uniform fit values are sorted and combined to obtain a local roughness analysis array of the corresponding divided area.
[0024] Preferably, the local roughness analysis array is processed, the total number of elements M with a value of 1 in the local roughness analysis array is traversed and counted, and the difference between the total number of elements M and the total number of standard elements M′ is calculated and analyzed to obtain the label identification with a value of 1 and the second normal sub-region, the label identification with a value of -1 and the second abnormal sub-region;
[0025] The rough label identifiers corresponding to the output of all divided areas are sorted and combined to obtain a rough analysis array.
[0026] Preferably, the overall coating uniformity of the substrate after the lithium battery diaphragm is processed and coated is determined according to the rough analysis array, and the formula Calculate and obtain the third abnormal influence degree Sy corresponding to all abnormal division areas; where P is the total number of elements with a value of -1 in the rough analysis array, Q is the total number of elements with a value of 1 in the rough analysis array, and B is the standard abnormal uniformity threshold;
[0027] If the third abnormal influence degree is not greater than zero, a prompt indicating that the overall coating uniformity state is normal is generated;
[0028] Otherwise, an abnormal prompt of the overall coating uniformity status is generated.
[0029] Preferably, the first abnormal influence degree Yy, the second abnormal influence degree Ey and the third abnormal influence degree Sy corresponding to the multidimensional static test are obtained, and the quality state degree Zz corresponding to the lithium battery diaphragm processing is calculated by the formula Zz=a1×Yy+a2×Ey+0.5×Sy; wherein a1 and a2 are both proportional coefficients, the value ranges of a1 and a2 are both (0, 0.5), and a1+a2=0.5;
[0030] The quality status degree is input into the quality status evaluation table to retrieve the corresponding quality status range, and the corresponding processing quality grade is output and prompted according to the quality status range.
[0031] Compared with the existing solutions, the present invention achieves the following beneficial effects:
[0032] The present invention obtains several divided areas by modularizing the substrate coated with the lithium battery diaphragm processing, so as to realize more refined measurement, data processing and marking of different positions of the substrate. At the same time, static testing, data statistics and processing of the coating thickness dimension are implemented, which can provide reliable measurement data support for the subsequent status analysis of the coating thickness dimension.
[0033] The present invention can effectively improve the diversity and reliability of data processing and analysis in terms of coating thickness by performing data processing in local and overall dimensions on the abnormal impact analysis array and calculating and analyzing the overall coating thickness qualification status from different dimensions.
[0034] The present invention implements local and overall multi-dimensional data processing and analysis on the uniform measurement data in the static test data set, so as to obtain the qualified local and overall coating uniformity status corresponding to the substrate after the lithium battery diaphragm is processed and coated, thereby improving the monitoring and analysis effect of the local and overall coating uniformity after the lithium battery diaphragm is processed and coated.
[0035] The present invention integrates and calculates the analysis results of multi-dimensional static tests to obtain the quality status corresponding to the lithium battery diaphragm processing and analyzes it, so as to obtain the overall quality status of the lithium battery diaphragm processing, realize the integration and analysis of the analysis results of different aspects in the early stage, implement the overall processing data management prompt, and improve the overall effect of the lithium battery diaphragm processing production data management in expanding utilization. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] The present invention will be further described below in conjunction with the accompanying drawings.
[0037] Figure 1 The present invention is a module block diagram of a method for intelligent management of lithium battery diaphragm processing production data.
[0038] Figure 2 This is a flowchart of the thickness analysis array acquisition in the present invention.
[0039] Figure 3 It is a flowchart of processing the local rough analysis array in the present invention. DETAILED DESCRIPTION
[0040] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary operation and maintenance personnel in this field without creative work are within the scope of protection of the present invention.
[0041] like Figure 1 As shown, the present invention is a method for intelligent management of lithium battery separator processing production data, comprising:
[0042] Modular processing is performed on the substrate coated with the lithium battery diaphragm to obtain several divided areas, multi-dimensional static tests are performed on the several divided areas in sequence, and the data of the multi-dimensional static tests are processed and combined to obtain a static test data set consisting of thickness measurement data and uniform measurement data; including:
[0043] Obtain the size corresponding to the substrate coated with the lithium battery diaphragm, the size includes the length and width of the body, and divide the substrate coated with the lithium battery diaphragm equally according to a preset area division ratio to obtain a number of divided areas. The area division ratio can be determined according to the implementation of the subsequent corresponding non-contact measurement scheme, so that all divided areas can be comprehensively measured, and the divided areas are numbered and marked according to a preset numbering sequence, and various static tests are performed on all divided areas; the numbering sequence can be from left to right and from top to bottom;
[0044] When static testing of the coating thickness dimension is performed on all divided areas, a laser scanner or a laser thickness gauge is used to perform non-contact measurement of the coating of several divided areas marked with numbers on the body in sequence, and the measured data is displayed through a pre-constructed thickness measurement coordinate system to obtain a thickness measurement curve of the corresponding divided area; the horizontal axis of the thickness measurement coordinate system is different numbers, and the vertical axis is the thickness value with an arithmetic difference value change, and the specific value of the arithmetic difference value can be determined according to the design parameters of the corresponding lithium battery diaphragm processing coating;
[0045] According to the numbers of the divided areas, all corresponding thickness measurement curves are sorted and combined to obtain thickness measurement data;
[0046] In an embodiment of the present invention, a plurality of divided areas are obtained by modularly processing the substrate coated with the lithium battery diaphragm, so that more refined measurements, data processing and marking can be implemented at different positions of the substrate. At the same time, static testing, data statistics and processing of the coating thickness dimension are implemented, which can provide reliable measurement data support for subsequent status analysis of the coating thickness dimension.
[0047] When static testing of the coating uniformity dimension is performed on all divided areas, all divided areas are divided equally twice in turn according to a preset test division ratio. The test division ratio can be set according to the scanning area of the scanning electron microscope, so that the scanning electron microscope can perform a more comprehensive scanning measurement on the divided sub-areas, obtain a number of divided sub-areas corresponding to the divided areas and mark them with numbers, and perform high-resolution scanning on the coating surfaces of all divided sub-areas in different divided areas in turn through the scanning electron microscope to obtain the corresponding local surface roughness, and extract the corresponding values of all local surface roughness according to the corresponding number marks of different divided sub-areas in the divided areas and sort and combine them to obtain a local roughness array;
[0048] The local surface roughness in the embodiment of the present invention may be Ra (average roughness), Rz (10-point height) or Rq (root mean square roughness);
[0049] And, all local rough arrays are sorted and combined according to the number marks of all divided areas to obtain uniform measurement data;
[0050] In an embodiment of the present invention, by performing a second equal division on all divided areas, performing a high-resolution scan on the coated surfaces of all divided sub-areas to obtain the corresponding local surface roughness and processing and combining them to obtain the local roughness array of the corresponding area, reliable measurement data support can be provided for the subsequent state analysis of the coating uniformity dimension.
[0051] Perform local and overall multi-dimensional data processing and analysis on the thickness measurement data in the static test data set to determine the local and overall coating thickness qualification status of the substrate after lithium battery diaphragm processing and coating and provide prompts; including:
[0052] like Figure 2 As shown, all thickness measurement curves of the sorted combination in the thickness measurement data are obtained and compared and verified with the standard thickness area in the thickness measurement coordinate system in turn. The standard thickness area is an area surrounded by the minimum standard thickness value and the maximum standard thickness value. The minimum standard thickness value and the maximum standard thickness value are determined according to the design requirement parameters corresponding to the coating thickness of the lithium battery diaphragm processing;
[0053] If the thickness measurement curves are all within the standard thickness area, a normal thickness label is generated and its associated label identifier is set to 1, and the corresponding divided sub-area is marked as the first normal sub-area;
[0054] If the thickness measurement curve is not in the standard thickness area, a thickness anomaly label is generated and its associated flag is set to -1, and the corresponding sub-area is marked as the first abnormal sub-area. According to the thickness anomaly label, the thickness measurement curves that are not in the standard thickness area are counted and marked as abnormal curves. The length L of the abnormal curve is obtained, and the maximum value D of the abnormal curve from the standard thickness area is calculated. The abnormal impact value Y corresponding to the abnormal curve is calculated by the formula Y=L×D.
[0055] The thickness label identifiers corresponding to all the divided areas are sorted and combined to obtain a thickness analysis array, and the total number of elements N′ with a value of -1 is traversed through the thickness analysis array, and the first abnormal influence Yy corresponding to all abnormal divided areas is calculated by the formula Yy=N′ / N; where N is the total number of all elements in the thickness analysis array;
[0056] And, through the formula Calculate and obtain the second abnormal influence degree Ey corresponding to all abnormal divided areas; where A is the standard abnormal thickness threshold, and the standard abnormal thickness threshold is determined according to the design requirement parameters corresponding to the coating thickness of the lithium battery diaphragm processing;
[0057] When evaluating the qualified state of the overall coating thickness corresponding to the substrate after the lithium battery separator is processed and coated according to the first abnormal influence degree and the second abnormal influence degree, the values of the first abnormal influence degree and the second abnormal influence degree are extracted and combined to obtain an abnormal influence array [y1, y2], and the abnormal influence array is input into a pre-built thickness data recognition model for data analysis to obtain an abnormal influence analysis array;
[0058] Among them, the expression of thickness data recognition model is: Wherein, U1 is the standard first abnormal impact data range, U2 is the standard second abnormal impact data range, and both U1 and U2 are determined according to the design requirement parameters corresponding to the coating thickness of the lithium battery diaphragm processing;
[0059] The output abnormal impact analysis array is [1, 1], [-1, 1], [1, -1] or [-1, -1];
[0060] Generate corresponding normal and abnormal prompts for the overall coating thickness status according to the output abnormal impact analysis array; wherein, generate a normal prompt for the overall coating thickness status according to the abnormal impact analysis array of [1, 1], generate a slight abnormal prompt for the overall coating thickness status according to the abnormal impact analysis array of [-1, 1] or [1, -1], and generate a severe abnormal prompt for the overall coating thickness status according to the abnormal impact analysis array of [-1, -1];
[0061] Obtain historical thickness measurement and analysis data of lithium battery diaphragm processing and coating, and establish a corresponding parameter matching model based on the historical thickness measurement and analysis data. The parameter matching model is established based on the isolation forest algorithm. The establishment steps are the existing conventional technical solutions, and the specific steps are not repeated here;
[0062] In the embodiment of the present invention, by performing local and overall dimensional data processing on the abnormal impact analysis array and calculating and analyzing the overall coating thickness qualification status from different dimensions, the diversity and reliability of data processing and analysis in terms of coating thickness can be effectively improved.
[0063] Perform local and overall multi-dimensional data processing and analysis on the uniform measurement data in the static test data set to determine the local and overall coating uniformity qualification status of the substrate after lithium battery diaphragm processing and coating and provide prompts; including:
[0064] Get all the local rough arrays of sorted combinations in the uniform measurement data, and get the values of all elements in the local rough arrays in turn and use the formula Calculate and obtain the uniform fit degree Cy corresponding to different sub-divided areas in the corresponding divided area;
[0065] All uniform fit values are sorted and combined to obtain a local roughness analysis array of the corresponding divided area;
[0066] like Figure 3 As shown, the local roughness analysis array is processed, the total number of elements M with a value of 1 in the local roughness analysis array is traversed and counted, and the difference between the total number of elements M and the total number of standard elements M′ is calculated and analyzed; M′ is determined according to the design requirement parameters corresponding to the uniformity of lithium battery diaphragm processing and coating;
[0067] If the difference is not greater than zero, a rough normal label is generated and its associated label flag is set to 1, and the corresponding divided sub-region is marked as a second normal sub-region;
[0068] If the difference is greater than zero, a rough abnormal label is generated and its associated label identifier is set to -1, and the corresponding divided sub-region is marked as a second abnormal sub-region;
[0069] Sort and combine the rough label identifiers corresponding to the output of all divided areas to obtain a rough analysis array;
[0070] According to the rough analysis array, the overall coating uniformity of the substrate after the lithium battery diaphragm is processed and coated is determined. The formula Calculate and obtain the third abnormal influence degree Sy corresponding to all abnormal division areas; where P is the total number of elements with a value of -1 in the rough analysis array, Q is the total number of elements with a value of 1 in the rough analysis array, and B is the standard abnormal uniformity threshold, which is determined according to the design requirement parameters corresponding to the uniformity of lithium battery diaphragm processing and coating;
[0071] If the third abnormal influence degree is not greater than zero, a prompt indicating that the overall coating uniformity state is normal is generated;
[0072] Otherwise, an abnormal prompt of the overall coating uniformity status is generated;
[0073] In an embodiment of the present invention, by performing local and overall multi-dimensional data processing and analysis on the uniform measurement data in the static test data set, the local and overall coating uniformity qualified status corresponding to the substrate after lithium battery diaphragm processing and coating can be obtained, thereby improving the monitoring and analysis effect of the local and overall coating uniformity after lithium battery diaphragm processing and coating.
[0074] The analysis results of multi-dimensional static tests are integrated and calculated to obtain the quality status corresponding to the lithium battery diaphragm processing, and the quality status is adaptively adjusted to dynamically prompt and warn the overall quality status of the lithium battery diaphragm processing; including:
[0075] The first abnormal influence degree Yy, the second abnormal influence degree Ey and the third abnormal influence degree Sy corresponding to the multi-dimensional static test are obtained, and the quality state degree Zz corresponding to the lithium battery diaphragm processing is calculated by the formula Zz=a1×Yy+a2×Ey+0.5×Sy; where a1 and a2 are both proportional coefficients, the value ranges of a1 and a2 are both (0, 0.5), and a1+a2=0.5;
[0076] Input the quality status into the quality status evaluation table to retrieve the corresponding quality status range, and output the corresponding processing quality level and prompt according to the quality status range;
[0077] Among them, the quality status evaluation table contains several different quality status ranges and their associated processing quality grades, and the quality status range is pre-associated with a corresponding processing quality grade; the quality status range is determined according to the design requirement parameters of the lithium battery diaphragm processing and coating;
[0078] The processing quality grades include qualified processing quality grade, slightly unqualified processing quality grade and severely unqualified processing quality grade.
[0079] In the embodiment of the present invention, the overall quality status of the lithium battery diaphragm processing can be obtained by integrating and calculating the analysis results of the multi-dimensional static test to obtain the quality status corresponding to the lithium battery diaphragm processing and analyzing it, thereby realizing the integration and analysis of the analysis results of different aspects in the early stage to implement the overall processing data management prompt, thereby improving the overall effect of the lithium battery diaphragm processing production data management in expanding utilization.
[0080] In the several embodiments provided by the present invention, it should be understood that the disclosed method can be implemented in other ways. For example, the above-described embodiments of the invention are only illustrative, for example, the division of modules is only a logical function division, and there may be other division methods in actual implementation.
[0081] The modules described as separate components may or may not be physically separated, and the components shown as modules may or may not be physical modules, and may be located in one place or distributed on multiple network modules. Some or all of the modules may be selected according to actual needs to achieve the purpose of the solution of this embodiment.
[0082] In addition, each functional module in each embodiment of the present invention may be integrated into one processing module, or each module may exist physically separately, or two or more modules may be integrated into one module. The above-mentioned integrated module may be implemented in the form of hardware or in the form of hardware plus software functional modules.
[0083] It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and that the present invention can be implemented in other specific forms without departing from the basic features of the present invention.
[0084] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, ordinary operation and maintenance personnel in the field should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention.
Claims
1. A method for intelligent management of lithium battery diaphragm processing production data, characterized in that: include: Modular processing is performed on the substrate coated with the lithium battery separator to obtain a number of divided areas, multi-dimensional static tests are performed on the divided areas in sequence, and the data of the multi-dimensional static tests are processed and combined to obtain a static test data set consisting of thickness measurement data and uniform measurement data; Among them, the size corresponding to the substrate coated with the lithium battery diaphragm is obtained, and the substrate coated with the lithium battery diaphragm is equally divided into a plurality of divided areas according to a preset area division ratio, and the plurality of divided areas are numbered and marked according to a preset numbering sequence, and a multi-dimensional static test is performed on all the divided areas; When static testing of coating thickness dimension is performed on all divided areas, non-contact measurement is performed on the coating of several divided areas marked with numbers on the body in sequence, and the measured data is displayed through a pre-constructed thickness measurement coordinate system to obtain the thickness measurement curve of the corresponding divided area; According to the numbers of the divided areas, all corresponding thickness measurement curves are sorted and combined to obtain thickness measurement data; When static testing of the coating uniformity dimension is performed on all divided areas, all divided areas are divided equally twice in turn according to the preset test division ratio, and a number of divided sub-areas corresponding to the divided areas are obtained and numbered, and high-resolution scanning is performed on the coating surfaces of all divided sub-areas in different divided areas in turn to obtain the corresponding local surface roughness, and the values of all corresponding local surface roughness are extracted and sorted and combined according to the corresponding number marks of different divided sub-areas in the divided areas to obtain a local roughness array; And, all local rough arrays are sorted and combined according to the number marks of all divided areas to obtain uniform measurement data; Perform local and overall multi-dimensional data processing and analysis on the thickness measurement data in the static test data set to determine the local and overall coating thickness qualification status of the substrate after the lithium battery separator is processed and coated and provide prompts; Perform local and overall multi-dimensional data processing and analysis on the uniform measurement data in the static test data set to determine the local and overall coating uniformity qualification status of the substrate after the lithium battery diaphragm is processed and coated and provide prompts; Among them, all local rough arrays of sorted combinations in uniform measurement data are obtained, and the values of all elements in the local rough arrays are obtained in turn and calculated by formula Calculate and obtain the uniform fit degree Cy corresponding to different sub-divided areas in the corresponding divided area; All uniform fit values are sorted and combined to obtain a local roughness analysis array of the corresponding divided area; The local rough analysis array is processed, the total number of elements M with a value of 1 in the local rough analysis array is traversed and counted, and the difference between the total number of elements M and the total number of standard elements M′ is calculated and analyzed to obtain the label identification with a value of 1 and the second normal sub-region, the label identification with a value of -1 and the second abnormal sub-region; Sort and combine the rough label identifiers corresponding to the output of all divided areas to obtain a rough analysis array; According to the rough analysis array, the overall coating uniformity of the substrate after the lithium battery diaphragm processing and coating is determined, and the formula Calculate and obtain the third abnormal influence degree Sy corresponding to all abnormal division areas; where P is the total number of elements with a value of -1 in the rough analysis array, Q is the total number of elements with a value of 1 in the rough analysis array, and B is the standard abnormal uniformity threshold; If the third abnormal influence degree is not greater than zero, a prompt indicating that the overall coating uniformity state is normal is generated; Otherwise, an abnormal prompt of the overall coating uniformity status is generated; The analysis results of multi-dimensional static tests are integrated and calculated to obtain the quality status corresponding to the lithium battery diaphragm processing, and dynamic prompts and alarms are adaptively given to the overall quality status of the lithium battery diaphragm processing based on the quality status.
2. The method for intelligent management of lithium battery diaphragm processing production data according to claim 1, characterized in that: Obtain all thickness measurement curves of the sorted combination in the thickness measurement data and compare and verify them with the standard thickness area in the thickness measurement coordinate system in turn. If the thickness measurement curves are all in the standard thickness area, generate a thickness normal label and set its associated label identifier to 1, and mark the corresponding divided sub-area as the first normal sub-area; If the thickness measurement curve is not in the standard thickness area, a thickness anomaly label is generated and its associated flag is set to -1, and the corresponding sub-area is marked as the first abnormal sub-area. According to the thickness anomaly label, the thickness measurement curves that are not in the standard thickness area are counted and marked as abnormal curves. The length L of the abnormal curve is obtained, and the maximum value D of the abnormal curve from the standard thickness area is calculated. The abnormal impact value Y corresponding to the abnormal curve is calculated by the formula Y=L×D.
3. The method for intelligent management of lithium battery diaphragm processing production data according to claim 2, characterized in that: The thickness label identifiers corresponding to all the divided areas are sorted and combined to obtain a thickness analysis array, and the total number of elements N′ with a value of -1 is traversed through the thickness analysis array, and the first abnormal influence Yy corresponding to all abnormal divided areas is calculated by the formula Yy=N′ / N; where N is the total number of all elements in the thickness analysis array; And, through the formula The second anomaly influence degree Ey corresponding to all abnormal division areas is calculated; where A is the standard abnormal thickness threshold.
4. The method for intelligent management of lithium battery diaphragm processing production data according to claim 3, characterized in that: When evaluating the qualified state of the overall coating thickness corresponding to the substrate after the lithium battery diaphragm is processed and coated according to the first abnormal influence degree and the second abnormal influence degree, the values of the first abnormal influence degree and the second abnormal influence degree are extracted and combined to obtain an abnormal influence array [y1, y2], and the abnormal influence array is input into a pre-built thickness data recognition model for data analysis to obtain an abnormal influence analysis array; wherein the output abnormal influence analysis array is [1, 1], [-1, 1], [1, -1] or [-1, -1]; According to the output abnormal impact analysis array, the corresponding normal and abnormal prompts of the overall coating thickness status are generated.
5. A method for intelligent management of lithium battery separator production data according to claim 1 or 3, characterized in that: The first abnormal influence degree Yy, the second abnormal influence degree Ey and the third abnormal influence degree Sy corresponding to the multi-dimensional static test are obtained, and the quality state degree Zz corresponding to the lithium battery diaphragm processing is calculated by the formula Zz=a1×Yy+a2×Ey+0.5×Sy; where a1 and a2 are both proportional coefficients, the value ranges of a1 and a2 are both (0, 0.5), and a1+a2=0.5; The quality status degree is input into the quality status evaluation table to retrieve the corresponding quality status range, and the corresponding processing quality grade is output and prompted according to the quality status range.