Multi-point glue thickness evaluation method for glass substrate based on data analysis
By analyzing the correlation data and white light interference signal of the adhesive film on the surface of the glass substrate, the interference peaks are separated, and the corrected thickness of the adhesive film is determined. This solves the problem of interference peak overlap in multi-point adhesive thickness measurement and achieves accurate adhesive application on the glass substrate. Glue thickness assessment and accurate analysis of glue distribution flow trends.
Patent Information
- Application Number
- CN202410924051.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-07-11
AI Technical Summary
In the multi-point glue thickness measurement of glass substrate coating, the interference signal is complicated due to the overlapping phenomenon of white light interference peaks, which affects the glue thickness cloud image analysis results and further affects the evaluation of the flow trend of glue distribution.
By analyzing the correlation data of the adhesive film on the surface of the coated glass substrate and the white light interference signal, we construct the interference peak position of the upper surface and the interference peak position of the lower surface, consider the light intensity distribution characteristics, separate the interference peaks, and determine the corrected thickness of the adhesive film. , and then evaluate the glue thickness.
It improves the distinction between interference peaks, eliminates the impact of interference peak overlap on evaluation results, achieves accurate evaluation of multi-point glue thickness on glass substrates, and improves the accuracy of glue distribution and flow trend analysis.
Smart Images

Figure CN118565357B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of data processing, and in particular to a method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis in the technical field of data processing. Background Art
[0002] Gluing is a very important process in the processing of glass substrates. In this process, photoresist or photoresist is coated on the glass substrate to form a transparent adhesive film with uniform thickness. The uniformity of the film thickness is the key to evaluating the quality of the glass substrate. By analyzing the glue thickness data, the glue coating process of the glass substrate can be optimized to reduce product defects and improve production efficiency.
[0003] The multi-point glue thickness measurement method for glass substrate glue coating can obtain enough point cloud data to form a glue thickness cloud map through multi-point sampling, and analyze the distribution and flow trend of the glue coating on the glass substrate based on the glue thickness cloud map, and adjust the subsequent process on this basis. Therefore, in the process of multi-point glue thickness evaluation of glass substrate glue coating, the interference peak of each point needs to be separated and identified, and the glue thickness information of each point is determined based on the peak position information of the identified interference peak. However, the white light interference peaks in the interference signal generated by the transparent glue film formed by the glass substrate glue coating may overlap with each other, and the overlapping of interference peaks will make the interference signal of each point complicated, thereby affecting the glue thickness measurement result of each point, and then affecting the glue distribution flow trend result obtained by the glue thickness cloud map formed by the multi-point data. Summary of the invention
[0004] In order to solve the technical problem that the multi-point glue thickness measurement results affect the glue distribution flow trend analysis results on the glue thickness cloud map, the purpose of the present invention is to provide a multi-point glue thickness evaluation method for glass substrate glue coating based on data analysis, and the technical scheme adopted is as follows:
[0005] In a first aspect, an embodiment of the present invention provides a method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis, the method comprising:
[0006] Obtaining correlation data of the adhesive film on the surface of the adhesive-coated glass substrate and the corresponding white light interference signal;
[0007] Based on the correlation data and the white light interference signal, constructing the peak-to-peak position of the interference peak on the upper surface of the adhesive film and the peak-to-peak position of the interference peak on the lower surface of the adhesive film;
[0008] Determining a corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface;
[0009] The adhesive thickness on the surface of the adhesive-coated glass substrate is evaluated based on the corrected adhesive film thickness.
[0010] In combination with the first aspect above, in some possible implementations, the step of obtaining the associated data of the adhesive film on the surface of the adhesive-coated glass substrate and the corresponding white light interference signal includes:
[0011] Acquire measurement signals of a white light interferometer at a plurality of measurement light points of the adhesive film on the surface of the adhesive-coated glass substrate;
[0012] Preprocessing the measurement signal to obtain a white light interference signal corresponding to the adhesive film on the surface of the adhesive-coated glass substrate;
[0013] The reflectivity of the upper surface, the reflectivity of the reflector and the refractive index of the adhesive film are determined to obtain the associated data of the adhesive film on the surface of the adhesive-coated glass substrate.
[0014] In the above scheme, by obtaining the white light interference signal and the reflectivity of the upper surface, the reflectivity of the reflector and the refractive index of the adhesive film, it is possible to consider the light intensity distribution characteristics between the reflected light generated by the same light beam on different transparent media and the distribution characteristics of the white light interference signal when constructing the peak value positions of the interference peaks of the upper and lower surfaces, thereby improving the distinction between the interference peaks corresponding to the lower and upper surfaces of the adhesive film on the surface of the adhesive-coated glass substrate in the white light interference signal.
[0015] In combination with the first aspect above, in some possible implementations, constructing the interference peak-to-peak position of the upper surface of the adhesive film and the interference peak-to-peak position of the lower surface of the adhesive film based on the correlation data and the white light interference signal includes:
[0016] Based on the light intensity values of the pixels in the white light interference signal, constructing a white light interference signal curve and a reference white light interference signal curve;
[0017] Based on the correlation data, determining the interference peak intensity ratio between the light intensity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the light intensity corresponding to the reflector in the white light interference signal;
[0018] Based on the white light interference signal curve, the reference white light interference signal curve and the interference peak intensity ratio, the interference peak peak position of the upper surface and the interference peak peak position of the lower surface of the adhesive film are constructed.
[0019] In the above scheme, by analyzing the light intensity value of each pixel point in the white light interference signal, the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface of the film can be accurately constructed.
[0020] In combination with the first aspect above, in some possible implementations, determining, based on the association data, an interference peak intensity ratio between the light intensity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the light intensity corresponding to the reflector in the white light interference signal includes:
[0021] Acquire the reflectivity of the upper surface and the reflectivity of the reflector in the associated data;
[0022] The interference peak light intensity ratio is determined based on the reflectivity of the upper surface and the reflectivity of the reflector.
[0023] In the above scheme, by taking the ratio between the reflectivity of the upper surface and the reflectivity of the reflector as the interference peak intensity ratio, the relationship between the light intensities of the interference peak peak points between the upper surface of the film and the reflector in the white light interference signal can be quickly and accurately analyzed.
[0024] In combination with the first aspect above, in some possible implementations, constructing the interference peak-to-peak position of the upper surface and the interference peak-to-peak position of the lower surface of the film based on the white light interference signal curve, the reference white light interference signal curve and the interference peak intensity ratio includes:
[0025] Expanding the data points in the reference white light interference signal curve based on the white light interference signal curve to obtain a first adjusted curve;
[0026] In the first adjusted curve, determining a maximum point;
[0027] Based on the maximum point and the white light interference signal curve, the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface are determined.
[0028] In the above scheme, a white light interference signal curve and a reference white light interference signal curve are constructed by using the light intensity values of the pixel points in the white light interference signal, so that the white light interference signal curve and the reference white light interference signal curve can be combined with the interference peak intensity ratio to construct the interference peak peak position of the upper surface with higher distinction and the interference peak peak position of the lower surface of the film.
[0029] In combination with the first aspect, in some possible implementations, determining a maximum point in the first adjusted curve includes:
[0030] Performing envelope extraction on the first adjusted curve to obtain an interference envelope;
[0031] Based on the interference envelope, the maximum point is determined.
[0032] In the above solution, by advancing the envelope of the first adjusted curve, the maximum value in the envelope can be quickly and accurately obtained, thereby facilitating the analysis of the interference peak-to-peak value in the white light interference signal curve.
[0033] In combination with the first aspect above, in some possible implementations, determining the interference peak-to-peak position of the upper surface and the interference peak-to-peak position of the lower surface based on the maximum point and the white light interference signal curve includes:
[0034] Based on the position of the maximum point in the first modulated curve, determining the position of the interference peak-to-peak value with the minimum value in the white light interference signal curve to obtain the interference peak-to-peak value position of the upper surface;
[0035] Based on the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first modulated curve, adjusting the data points in the first modulated curve to obtain an approximate curve of a white light interference signal;
[0036] Using the data points in the white light interference signal curve to adjust the data points in the white light interference signal approximation curve to obtain a second adjusted curve;
[0037] The position of the interference peak-to-peak value with the smallest value in the second adjusted curve is determined as the interference peak-to-peak value position of the lower surface.
[0038] In the above scheme, the position of the interference peak-to-peak value with the smallest value in the first adjusted curve is taken as the interference peak-to-peak value position of the upper surface, and the second adjusted curve is obtained by combining the interference peak-to-peak value with the smallest value in the first adjusted curve, the interference peak-to-peak value in the first adjusted curve and the data points in the white light interference signal curve, so that the position of the interference peak-to-peak value with the smallest value in the second adjusted curve is taken as the interference peak-to-peak value position of the lower surface; thereby making it easier to distinguish the interference peak-to-peak value position of the upper surface from the interference peak-to-peak value position of the lower surface.
[0039] In combination with the first aspect, in some possible implementations, adjusting the data points in the first modulated curve based on the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first modulated curve to obtain an approximate curve of the white light interference signal includes:
[0040] Determine a difference between the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first adjusted curve;
[0041] The difference value is assigned to the data points in the first adjusted curve to obtain the white light interference signal approximate curve.
[0042] In the above scheme, the data points in the first adjusted curve are adjusted by the difference between the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first adjusted curve, thereby obtaining an approximate curve of the white light interference signal capable of separating the interference peak-to-peak position of the lower surface.
[0043] In combination with the first aspect above, in some possible implementations, the step of using the data points in the white light interference signal curve to adjust the data points in the white light interference signal approximation curve to obtain a second adjusted curve includes:
[0044] The ordinates of the data points in the white light interference signal curve are adjusted by using the ordinates of the data points in the white light interference signal approximation curve to obtain the candidate curve;
[0045] The candidate curve is smoothed to obtain the second adjusted curve.
[0046] In the above solution, by smoothing the candidate curve, the data values in the second adjusted curve can be made more accurate.
[0047] In combination with the first aspect above, in some possible implementations, the evaluating the adhesive thickness on the surface of the adhesive-coated glass substrate based on the corrected thickness of the adhesive film includes:
[0048] Acquire a white light interference signal of any measuring light point on the surface of the glue-coated glass substrate;
[0049] Determine the thickness of the adhesive film at the location of any measuring light point based on the corrected thickness of the adhesive film at multiple pixel points in the white light interference signal of any measuring light point;
[0050] Determining the uniformity and thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the adhesive film thickness at the locations of the plurality of measuring light spots;
[0051] Based on the uniformity and thickness of the adhesive film on the surface of the adhesive-coated glass substrate, the thickness of the adhesive on the surface of the adhesive-coated glass substrate is evaluated.
[0052] In the above scheme, for any measuring light spot, the average value of the corrected film thickness of multiple pixel points in the white light interference signal of the measuring light spot is used as the film thickness of the measuring photoelectric, and then the film uniformity and film thickness of the surface of the coated glass substrate are calculated by further using the film thickness at the locations of the multiple measuring light spots, so as to accurately evaluate the glue thickness on the surface of the coated glass substrate.
[0053] In a second aspect, a device for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis is provided, the device comprising:
[0054] An acquisition module, used to acquire the associated data of the adhesive film on the surface of the adhesive-coated glass substrate and the corresponding white light interference signal;
[0055] A construction module, configured to construct the peak-to-peak value position of the interference peak on the upper surface of the adhesive film and the peak-to-peak value position of the interference peak on the lower surface of the adhesive film based on the correlation data and the white light interference signal;
[0056] A determination module, configured to determine a corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the peak-to-peak value position of the interference peak on the upper surface and the peak-to-peak value position of the interference peak on the lower surface;
[0057] The evaluation module is used to evaluate the adhesive thickness on the surface of the adhesive-coated glass substrate based on the corrected thickness of the adhesive film.
[0058] According to a third aspect, a computer program product is provided, comprising: a computer program code, which, when executed on a computer, enables the computer to execute the method according to the first aspect or any possible implementation of the first aspect.
[0059] In a fourth aspect, a computer-readable storage medium is provided, which stores a computer program code. When the computer program code runs on a computer, the computer executes the method in the above-mentioned first aspect or any possible implementation manner of the first aspect.
[0060] The present invention has the following beneficial effects: by analyzing the associated data of the adhesive film on the surface of the glued glass substrate and the corresponding white light interference signal, the interference peak position of the upper surface of the adhesive film and the interference peak position of the lower surface of the adhesive film are constructed; in this way, the associated data of the adhesive film on the surface of the glued glass substrate and the white light interference signal are considered at the same time, and the discrimination between the corresponding interference peaks of the lower surface and the upper surface of the adhesive film on the surface of the glued glass substrate in the white light interference signal can be improved. Afterwards, the scanning distance of the white light interferometer is determined by the interference peak position of the upper surface and the interference peak position of the lower surface; and the corrected thickness of the adhesive film on the surface of the glued glass substrate is determined by the scanning distance; thus, the adhesive thickness on the surface of the glued glass substrate is evaluated based on the corrected thickness of the adhesive film. In this way, the separation of the corresponding interference peak positions of the lower surface and the upper surface in the white light interference signal is achieved, and the multi-point adhesive thickness evaluation of the glass substrate is completed, and the influence of the mutual overlap phenomenon in the interference signal of each point on the evaluation result during the multi-point adhesive thickness evaluation process is eliminated. BRIEF DESCRIPTION OF THE DRAWINGS
[0061] In order to more clearly illustrate the technical solutions and advantages in the embodiments of the present invention or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0062] Figure 1 It is a schematic diagram of the implementation process of a method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided by an embodiment of the present invention;
[0063] Figure 2 It is a schematic diagram of the position of the measuring light spot of the adhesive film on the surface of the adhesive-coated glass substrate provided by an embodiment of the present invention;
[0064] Figure 3 It is another implementation flow diagram of a method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided by an embodiment of the present invention;
[0065] Figure 4 is a schematic diagram of a white light interference signal curve provided by an embodiment of the present invention;
[0066] Figure 5 is another schematic diagram of a white light interference signal curve provided by an embodiment of the present invention;
[0067] Figure 6 It is another implementation flow diagram of the method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided by an embodiment of the present invention;
[0068] Figure 7 is another schematic diagram of a white light interference signal curve provided by an embodiment of the present invention;
[0069] Figure 8 is a schematic diagram of the interference envelope of a white light interference signal curve provided by an embodiment of the present invention;
[0070] Fig. 9 It is another implementation flow diagram of the method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided by an embodiment of the present invention;
[0071] Fig.10 It is a structural schematic diagram of a computer device provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0072] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the following is a detailed description of the specific implementation method, structure, features and effects of a multi-point glue thickness evaluation method for glass substrate glue coating based on data analysis proposed by the present invention in combination with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "another embodiment" does not necessarily refer to the same embodiment. In addition, specific features, structures or characteristics in one or more embodiments may be combined in any suitable form.
[0073] Among them, in the description of the embodiments of the present invention, unless otherwise specified, " / " means or, for example, A / B can mean A or B: "and / or" in the text is only a way to describe the association relationship of associated objects, indicating that there can be three relationships, for example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. In addition, in the description of the embodiments of the present invention, "multiple" refers to two or more than two.
[0074] In the following, the terms "first" and "second" are used for descriptive purposes only and are not to be understood as suggesting or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features.
[0075] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
[0076] The specific scheme of the method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided by the present invention is described in detail below in conjunction with the accompanying drawings.
[0077] See also Figure 1 , which shows a flow chart of a method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided by an embodiment of the present invention, the method comprising:
[0078] 101, obtaining correlation data of the adhesive film on the surface of the adhesive-coated glass substrate and a corresponding white light interference signal.
[0079] Here, the glue-coated glass substrate is a glass substrate after glue coating. The associated data of the glue film on the surface of the glue-coated glass substrate include: the reflectivity of the upper surface, the reflectivity of the reflector, and the refractive index of the glue film. The white light interference signal corresponding to the glue film on the surface of the glue-coated glass substrate includes: the white light interference signal at multiple measurement light points of the glue film on the surface of the glue-coated glass substrate collected by the white light interferometer. In some possible implementations, the measurement signals of the white light interferometer at multiple measurement light points of the glue film on the surface of the glue-coated glass substrate are obtained; wherein the multiple measurement light points of the glue film on the surface of the glue-coated glass substrate can be user-defined measurement points, for example, 16 evenly distributed measurement light points are selected on the glue film on the surface of the glue-coated glass substrate. The white light interference signal corresponding to the glue film on the surface of the glue-coated glass substrate is obtained by preprocessing the measurement signal. In this way, by obtaining the white light interference signal and the reflectivity of the upper surface, the reflectivity of the reflector and the refractive index of the adhesive film, it is possible to consider the intensity distribution characteristics of the reflected light generated by the same light beam on different transparent media and the distribution characteristics of the white light interference signal when constructing the peak values of the interference peaks of the upper and lower surfaces, thereby improving the distinction between the interference peaks corresponding to the lower and upper surfaces of the adhesive film on the surface of the adhesive-coated glass substrate in the white light interference signal.
[0080] In some possible implementations, obtain a glass substrate after the coating is completed, that is, a coated glass substrate, place the coated glass substrate on the stage of a white light interferometer, ensure that the coated glass substrate is parallel to the stage, select multiple measurement light spots on the adhesive film on the surface of the coated glass substrate, the number of measurement light spots can be set by the implementer, and use a white light interferometer to collect white light interference signals at each measurement light spot. For example, a halogen lamp that filters out all wavelengths of light other than 600 to 900 nanometers (nm) through a filter is selected as the light source of the white light interferometer to reduce the effect of the light source on the exposure of the photoresist, and select the wave number with the largest light intensity in the spectrum of the light source as the central wavelength of the light source of the white light interferometer, wherein the light source can be set by the implementer. The scanning direction of the interference objective of the white light interferometer is a vertical direction from top to bottom, and the scanning step size, scanning range, and exposure time of the white light interferometer are set to 30nm, 10 microns (nm), respectively. m), 30 milliseconds (ms), where the scanning direction, scanning step, scanning range, and exposure time can be set by the implementer. When collecting white light interference signals, it is necessary to keep two to three interference bright fringes in the field of view of the white light interferometer. At the same time, the coated glass substrate is replaced with a reflector, and the white light interference signal of the reflector is collected using a white light interferometer, recorded as a reference white light interference signal, and the reflectivity of the upper surface of the adhesive film on the surface of the coated glass substrate, the reflectivity of the reflector, and the refractive index of the adhesive film on the surface of the coated glass substrate are obtained.
[0081] After obtaining the glue-coated glass substrate, place the glue-coated glass substrate on the stage of the white light interferometer, and select 16 evenly distributed measurement light points on the glue film on the surface of the glue-coated glass substrate, such as Figure 2 As shown, 16 evenly distributed measuring light spots are selected on the adhesive film 201 on the surface of the adhesive-coated glass substrate. The number of measuring light spots can be set by the implementer, and a white light interferometer is used to collect white light interference signals at each measuring light spot. The light intensity values of the pixel points in each frame of the white light interference image in the obtained white light interference signal are normalized to obtain the normalized white light interference signal of each measuring light spot on the adhesive-coated glass substrate and the normalized reference white light interference signal. In this way, the white light interference signal and the reference white light interference signal of each measuring light spot on the adhesive-coated glass substrate are obtained, and the reflectivity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate is obtained. , reflectivity of the reflector And the refractive index of the adhesive film on the surface of the coated glass substrate , that is, the associated data of the adhesive film on the surface of the coated glass substrate and the corresponding white light interference signal are obtained.
[0082] 102 . Constructing the peak-to-peak value position of the interference peak on the upper surface of the adhesive film and the peak-to-peak value position of the interference peak on the lower surface of the adhesive film based on the correlation data and the white light interference signal.
[0083] Here, since the associated data includes: the reflectivity of the upper surface, the reflectivity of the reflector, and the refractive index of the adhesive film, the peak position of the interference peak on the upper surface of the adhesive film and the peak position of the interference peak on the lower surface are constructed by analyzing the reflectivity of the upper surface of the adhesive-coated glass substrate, the reflectivity of the reflector, the refractive index of the adhesive film, and the distribution of data in the white light interference signal of the reflector. During the vertical scanning process of the interference objective of the white light interferometer, the reflected light formed by the light source of the white light interferometer on the lower surface and the upper surface of a certain position of the adhesive film on the surface of the adhesive-coated glass substrate will interfere with the light beam of the light source successively, and form interference peaks in the white light interference signal respectively. Among them, the peak position of the interference peak is the zero optical path difference position, and the distance along the vertical direction between the two zero optical path difference positions corresponding to the lower surface and the upper surface of the position in the white light interference signal is the optical thickness of the adhesive film at that position.
[0084] In some possible implementations, the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface of the film are constructed by analyzing the light intensity value of each pixel in the white light interference signal. That is, the above step 102 can be performed by Figure 3 The steps shown achieve:
[0085] 301 , constructing a white light interference signal curve and a reference white light interference signal curve based on the light intensity values of the pixels in the white light interference signal.
[0086] Here, the first White light interference signal of a measuring light point Pixels in For example, get the pixel point In the signal The corresponding light intensity value in each frame of the white light interference image is used to construct a coordinate system with the light intensity value as the ordinate and the frame number of the white light interference image where the light intensity value is located as the abscissa , connect the coordinate system Each data point in the image is used to form a continuous curve, and the obtained curve is smoothed using a polynomial fitting algorithm to reduce data noise and make the curve smoother. The smoothed curve is recorded as a pixel point White light interference signal curve , to characterize the vertical scanning process of the interference lens of the white light interferometer, the light at the pixel point The intensity of the reflected light at the position changes with the scanning position of the interference lens, which is used to obtain the pixel point later. The zero optical path difference position in the white light interference signal. The white light interference signal curve is as follows Figure 4 As shown in curve 31, Figure 4 The horizontal axis represents the frame number, and the vertical axis represents the light intensity value. The white light interference signal curve can also be as follows Figure 5 As shown, Figure 5 The pixel points in the white light interference signal corresponding to the white light interference signal curve 32 in Figure 4 The pixel points in the white light interference signal corresponding to the curve 31 have different film thicknesses, and the film thickness of the pixel points corresponding to the white light interference signal curve 32 is smaller than the film thickness of the pixel points corresponding to the curve 31 .
[0087] Calculate the reference white light interference signal The average of all light intensity values in each frame of the white light interference image is recorded as the light intensity average of the white light interference image. The coordinate system is constructed with the frame number and light intensity average of the white light interference image as the horizontal and vertical coordinates. , using the white light interference signal curve The same acquisition method is used to obtain the reference white light interference signal Reference white light interference signal curve , where we only need to change the coordinate system Replace with coordinate system That's it.
[0088] 302 , based on the associated data, determine the interference peak intensity ratio between the light intensity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the light intensity corresponding to the reflector in the white light interference signal.
[0089] In some possible implementations, first, the reflectivity of the upper surface and the reflectivity of the reflector in the associated data are obtained; wherein the reflectivity of the reflector is required to maintain two to three interference bright fringes in the field of view of the white light interferometer when collecting white light interference signals. At the same time, the coated glass substrate is replaced with the reflector, and the reflectivity of the reflector is determined.
[0090] Then, based on the reflectivity of the upper surface and the reflectivity of the reflector, the interference peak light intensity ratio is determined. Here, the reflectivity of the upper surface is divided by the reflectivity of the reflector to obtain the interference peak light intensity ratio. The interference peak light intensity ratio is used to characterize the ratio relationship between the light intensities of the peak points of the interference peaks corresponding to the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the reflector in the white light interference signal. In this way, by taking the ratio between the reflectivity of the upper surface and the reflectivity of the reflector as the interference peak light intensity ratio, the relationship between the light intensities of the peak points of the interference peaks between the upper surface of the adhesive film and the reflector in the white light interference signal can be quickly and accurately analyzed.
[0091] 303 , constructing the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface of the film based on the white light interference signal curve, the reference white light interference signal curve and the interference peak intensity ratio.
[0092] Here, the interference peak intensity ratio is used to select the interference peak peak position with the smallest value from the multiple interference peak peaks on the white light interference signal curve and record it as the interference peak peak position of the upper surface. The interference peak peak position of the lower surface of the film is determined by the difference between the interference peak peak of the upper surface and the interference peak peak in the white light interference signal curve, combined with the reference white light interference signal curve.
[0093] In some possible implementations, the peak-to-peak position of the interference peak of the surface and the peak-to-peak position of the interference peak of the lower surface are constructed by using the maximum value in the first adjusted curve and the white light interference signal curve, that is, the above step 303 can be performed by Figure 6 The steps shown achieve:
[0094] 401 , expanding data points in the reference white light interference signal curve based on the white light interference signal curve to obtain a first adjusted curve.
[0095] Here, according to the peak shape and peak value of the interference peak corresponding to the upper surface of the film in the white light interference signal curve, the data points in the reference white light interference signal curve are expanded so that the obtained first adjusted curve has the same peak shape and peak value as the interference peak corresponding to the upper surface of the film in the white light interference signal curve.
[0096] In some possible implementations, since in most cases the reflectivity of the lower surface of the adhesive film on the surface of the adhesive-coated glass substrate is greater than the reflectivity of the upper surface, the light intensity of the interference peak of the lower surface of the adhesive film in the white light interference signal is significantly greater than the light intensity of the interference peak of the upper surface, and when the thickness of the adhesive film is less than half of the coherence length of the light source of the white light interferometer, there will be a large overlap between the interference peak of the lower surface of the adhesive film and the interference peak of the upper surface (e.g. Figure 7 As shown in the curve 41 in FIG. 4 , the film thickness value of the pixel point in the white light interference signal corresponding to the curve 41 is greater than half of the coherence length of the light source of the white light interferometer). At this time, the coherence between the reflected light formed by the light source of the white light interferometer on the upper and lower surfaces of the film is relatively weak, so that the superposition of the light intensity between the reflected light formed on the upper and lower surfaces is approximately the simple addition of the light intensity values. The intensity of the reflected light generated by the same beam of light irradiating different transparent media is related to the reflectivity of the medium, and there is only one interference peak in the white light interference signal of the reflector. Therefore, the interference peaks corresponding to the lower and upper surfaces of the film on the surface of the glass substrate coated with glue in the white light interference signal can be separated according to the interference peaks in the white light interference signal of the reflector.
[0097] In some possible implementations, the reflectivity of the upper surface is calculated , reflectivity of the reflector The ratio between them is recorded as the interference peak intensity ratio , which is used to characterize the ratio between the light intensity of the upper surface of the adhesive film on the surface of the coated glass substrate and the peak point of the interference peak corresponding to the reflector in the white light interference signal. The values of all data points in times to obtain the reference white light interference signal curve The white light interference signal curve in the white light interference signal has the same peak shape and peak value as the corresponding interference peak on the upper surface of the film; the curve with the enlarged value is recorded as the first adjusted curve . Extract the first modulated curve using the envelope extraction method based on Hilbert transform Since there is only one interference peak in the white light interference signal of the reflector, only one interference envelope is obtained. Figure 8 As shown, curve 42 represents the first adjusted curve , the envelope curve 43 represents the first adjusted curve The Gaussian curve fitting method is used to obtain the maximum value point of the interference envelope, and the maximum value point is placed on the first adjusted curve. The corresponding horizontal coordinate in is the first adjusted curve The peak position of the interference peak , which is used to characterize the peak position of the interference peak in the white light interference signal of the reflector.
[0098] 402: Determine a maximum point in the first adjusted curve.
[0099] In some possible implementations, the interference envelope is obtained by performing envelope extraction on the first modulated curve, for example, the interference envelope of the first modulated curve is extracted by using the envelope extraction method of Hilbert transform. Then, based on the interference envelope, the maximum point is determined. Here, after the interference envelope is extracted, the maximum point of the interference envelope is obtained by using the Gaussian curve fitting method. In this way, by performing envelope advance on the first modulated curve, the maximum value in the envelope can be obtained quickly and accurately, thereby facilitating the analysis of the interference peak-to-peak value in the white light interference signal curve.
[0100] 403 : Determine the peak-to-peak position of the interference peak of the upper surface and the peak-to-peak position of the interference peak of the lower surface based on the maximum point and the white light interference signal curve.
[0101] Here, after obtaining the position of the maximum point in the first modulated curve, the first modulated curve is replaced with the white light interference signal curve in the manner of determining the maximum point, that is, the white light interference signal curve is envelope extracted to obtain all the interference peak-to-peak values in the white light interference signal curve; and the position of the interference peak-to-peak value with the smallest value among these interference peak-to-peak values is used as the interference peak-to-peak value position of the upper surface. Afterwards, according to the difference between the interference peak-to-peak value with the smallest value and the maximum point in the first modulated curve, the data points in the first modulated curve are adjusted to obtain the second modulated curve, the interference peak-to-peak value with the smallest value is determined on the second modulated curve, and the position of the interference peak-to-peak value with the smallest value in the second modulated curve is used as the interference peak-to-peak value position of the lower surface. In this way, the white light interference signal curve and the reference white light interference signal curve are constructed by the light intensity value of the pixel point in the white light interference signal, so that the white light interference signal curve and the reference white light interference signal curve can be combined with the interference peak light intensity ratio to construct the interference peak-to-peak value position of the upper surface with higher discrimination and the interference peak-to-peak value position of the lower surface of the film.
[0102] In some possible implementations, the above step 403 can be performed by Fig. 9 The steps shown achieve:
[0103] 501. Based on the position of the maximum point in the first modulated curve, determine the position of the interference peak-to-peak value with the minimum value in the white light interference signal curve to obtain the interference peak-to-peak value position of the upper surface.
[0104] Here, in accordance with the manner of determining the position of the maximum point in the first adjusted curve, all interference peak-to-peak values are determined in the white light interference signal curve, and the interference peak-to-peak value with the smallest value is selected therefrom, and the position of the interference peak-to-peak value with the smallest value is taken as the interference peak-to-peak value position of the upper surface.
[0105] 502 : Based on the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first modulated curve, adjust the data points in the first modulated curve to obtain an approximate curve of a white light interference signal.
[0106] Here, by determining the difference between the interference peak-to-peak value with the smallest value and the interference peak-to-peak value in the first adjusted curve, the difference value is assigned to the data point in the first adjusted curve to obtain an approximate curve of the white light interference signal. For example, the difference value is obtained by subtracting the interference peak-to-peak value in the first adjusted curve (i.e., the maximum value in the first adjusted curve) from the interference peak-to-peak value with the smallest value; in this way, the difference value can represent the difference between the peak position of the interference peak corresponding to the upper surface of the film and the reflector in the white light interference signal. The horizontal coordinate of each data point in the first adjusted curve is added with the difference value to obtain an approximate curve of the white light interference signal. In this way, the approximate curve of the white light interference signal is consistent with the white light interference signal curve. The interference peak corresponding to the upper surface of the film in the white light interference signal has the same peak shape, peak value and position, which is used for subsequent analysis from the white light interference signal curve The interference peak corresponding to the lower surface of the film in the white light interference signal is separated. In this way, the data points in the first adjusted curve are adjusted by the difference between the interference peak-to-peak value with the smallest value and the interference peak-to-peak value in the first adjusted curve, thereby obtaining an approximate curve of the white light interference signal that can separate the interference peak-to-peak position of the lower surface.
[0107] 503 , using the data points in the white light interference signal curve to adjust the data points in the white light interference signal approximation curve to obtain a second adjusted curve.
[0108] Here, first, the ordinates of the data points in the white light interference signal curve are used to adjust the ordinates of the data points in the white light interference signal approximate curve to obtain the candidate curve; for example, the ordinates of the data points in the white light interference signal curve are respectively subtracted from the ordinates of the data points in the white light interference signal approximate curve to obtain the candidate curve. Then, the candidate curve is smoothed to obtain the second adjusted curve. For example, the candidate curve is smoothed by noise reduction filtering or other smoothing processing to obtain the second adjusted curve. In this way, by smoothing the candidate curve, the data values in the second adjusted curve can be made more accurate.
[0109] 504 , determine the position of the interference peak-to-peak value with the smallest value in the second adjusted curve as the interference peak-to-peak value position of the lower surface.
[0110] Here, multiple interference peak-to-peak values in the second modulated curve are obtained by performing envelope extraction on the second modulated curve, and the interference peak-to-peak value with the smallest value is selected from the second modulated curve, and the position of the interference peak-to-peak value with the smallest value in the second modulated curve is determined as the interference peak-to-peak value position of the lower surface. In this way, the position of the interference peak-to-peak value with the smallest value in the first modulated curve is used as the interference peak-to-peak value position of the upper surface, and the second modulated curve is obtained by combining the interference peak-to-peak value with the smallest value in the first modulated curve, the interference peak-to-peak value in the first modulated curve, and the data points in the white light interference signal curve, so that the position of the interference peak-to-peak value with the smallest value in the second modulated curve is used as the interference peak-to-peak value position of the lower surface; thereby making it easier to distinguish the interference peak-to-peak value position of the upper surface from the interference peak-to-peak value position of the lower surface.
[0111] In some possible implementations, the peak position of the interference peak in the first modulated curve is calculated using (i.e., the maximum point in the first adjusted curve) Replaced with white light interference signal curve , and the white light interference signal curve is obtained The peak positions of all interference peaks are shown in Figure 2. Since the first white light interference signal received by the white light interferometer when collecting the white light interference signal of the coated glass substrate is the white light interference signal on the upper surface of the adhesive film, the upper surface of the adhesive film is on the white light interference signal curve. If the abscissa of the peak-to-peak value of the interference in the film is smaller than the abscissa of the peak-to-peak value of the interference on the lower surface of the film, then the white light interference signal curve The interference peak position with the smallest value is recorded as the interference peak position on the upper surface of the film. .Will The value of is recorded as the difference in the peak position of the interference peak , used to characterize the difference between the peak position of the interference peak corresponding to the upper surface of the adhesive film on the surface of the coated glass substrate and the reflector in the white light interference signal, and the first adjusted curve The horizontal coordinates of all data points in the , to obtain the white light interference signal curve The white light interference signal curve in which the interference peak corresponding to the upper surface of the film in the white light interference signal has the same peak shape, peak value and position is used for subsequent analysis from the white light interference signal curve The interference peak corresponding to the white light interference signal of the lower surface of the film is separated from the white light interference signal, and the obtained curve is recorded as the approximate curve of the white light interference signal of the upper surface of the film. .
[0112] The white light interference signal curve The vertical coordinates of the data points are respectively subtracted from the white light interference signal approximate curve The vertical coordinate of the corresponding data point in the image is used to smooth the candidate curve obtained, and the processed curve is recorded as the second adjusted curve . Use and Location The same method is used to obtain the second adjusted curve. The peak positions of all interference peaks are The interference peak position with the smallest value is recorded as the interference peak position of the lower surface of the film. .
[0113] 103 , determining a corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the peak-to-peak value position of the interference peak on the upper surface and the peak-to-peak value position of the interference peak on the lower surface.
[0114] Here, based on the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface, the scanning distance of the white light interferometer of the adhesive film on the surface of the adhesive-coated glass substrate is determined. The scanning distance is the scanning distance of the white light interferometer corresponding to the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface. Then, the corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate is determined according to the scanning distance.
[0115] In some possible implementations, the white light interference signal curve is calculated The peak position of the interference peak on the upper surface , the peak position of the interference peak on the lower surface The corresponding scanning distance of the white light interferometer is combined with the refractive index S of the surface adhesive film on the coated glass substrate to obtain the surface adhesive film on the coated glass substrate at the pixel point. Corrected film thickness at , as shown in formula (1):
[0116] (1);
[0117] 104 , based on the corrected thickness of the adhesive film, evaluating the adhesive thickness on the surface of the adhesive-coated glass substrate.
[0118] Here, for any measuring light spot on the surface of the glue-coated glass substrate, the glue film correction thicknesses of multiple pixel points in the white light interference signal of the measured photoelectric are combined as the glue film thickness of the measured photoelectric, thereby obtaining the glue film thickness of multiple measuring light spots, and then the glue film thickness of multiple measuring light spots can be used to quickly and accurately evaluate the glue thickness on the surface of the glue-coated glass substrate.
[0119] In the embodiment of the present invention, by analyzing the correlation data of the adhesive film on the surface of the glued glass substrate and the corresponding white light interference signal, the peak-value position of the interference peak on the upper surface of the adhesive film and the peak-value position of the interference peak on the lower surface of the adhesive film are constructed; in this way, the correlation data of the adhesive film on the surface of the glued glass substrate and the white light interference signal are considered at the same time, which can improve the distinction between the corresponding interference peaks of the lower surface and the upper surface of the adhesive film on the surface of the glued glass substrate in the white light interference signal. Afterwards, the scanning distance of the white light interferometer is determined by the peak-value position of the interference peak on the upper surface and the peak-value position of the interference peak on the lower surface; and the corrected thickness of the adhesive film on the surface of the glued glass substrate is determined by the scanning distance; thus, the adhesive thickness on the surface of the glued glass substrate is evaluated based on the corrected thickness of the adhesive film. In this way, the separation of the peak-value positions of the interference peaks corresponding to the lower surface and the upper surface in the white light interference signal is achieved, and the adhesive thickness information of each point is determined based on the peak position information of the identified interference peak, and the evaluation result of the adhesive thickness at multiple points after the glass substrate is glued is obtained.
[0120] In some possible implementations, the above step 104 may be implemented by the following process:
[0121] First, a white light interference signal of any measuring light point on the surface of the glue-coated glass substrate is obtained.
[0122] Here, the surface of the glue-coated glass substrate includes a plurality of measuring light spots. For example, 16 measuring light spots are set on the surface of the glue-coated glass substrate. For each measuring light spot, a white light interference signal of the white light interferometer at the measuring light spot is obtained.
[0123] Secondly, based on the corrected thickness of the adhesive film at a plurality of pixel points in the white light interference signal of any of the measuring light points, the thickness of the adhesive film at the position where any of the measuring light points is located is determined.
[0124] Here, the average value of the corrected thickness of the adhesive film at multiple pixel points in the white light interference signal of any measuring light point is taken as the thickness of the adhesive film at the position where the measuring light point is located.
[0125] Thirdly, based on the thickness of the adhesive film at the locations of the plurality of measuring light spots, the uniformity and thickness of the adhesive film on the surface of the adhesive-coated glass substrate are determined.
[0126] Here, after obtaining the film thickness at each measuring light spot, the standard deviation and mean of the multiple measuring light spots are further calculated. The standard deviation represents the uniformity of the film on the surface of the coated glass substrate, and the mean represents the film thickness on the surface of the coated glass substrate.
[0127] Finally, based on the uniformity and thickness of the adhesive film on the surface of the adhesive-coated glass substrate, the thickness of the adhesive on the surface of the adhesive-coated glass substrate is evaluated.
[0128] Here, the more uniform the distribution of the glue film thickness on the surface of the glue-coated glass substrate is, the smaller the standard deviation is, and the closer the mean is to the expected glue coating thickness value of the glue-coated glass substrate, the better the glue coating quality of the substrate glue-coated sample is.
[0129] In some possible implementations, the first Take the measurement light point as an example, and take the white light interference signal The average value of the film correction thickness of all pixels in the The film thickness at each measuring point is calculated in the same way as above. The standard deviation of the film thickness at all measuring points is calculated. and mean ; Set the standard deviation , mean As the uniformity and thickness of the adhesive film of the substrate coating sample, the more uniform the distribution of the adhesive film thickness on the surface of the coated glass substrate, the lower the standard deviation. The smaller the value of The closer the estimated glue thickness value of the glue-coated glass substrate is, the better the glue coating quality of the substrate glue-coated sample is, thus completing the multi-point glue thickness evaluation of the glue coating quality of the glue-coated glass substrate. In this way, for any measuring light point, the average of the glue film correction thickness of multiple pixel points in the white light interference signal of the measuring light point is used as the glue film thickness of the measured photoelectric, and then the glue film thickness at the locations of multiple measuring light points is further used to calculate the glue film uniformity and glue film thickness on the surface of the glue-coated glass substrate, so as to accurately evaluate the glue thickness on the surface of the glue-coated glass substrate.
[0130] The embodiment of the present invention provides a device for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis, the device comprising:
[0131] An acquisition module is used to acquire the associated data of the adhesive film on the surface of the adhesive-coated glass substrate and the corresponding white light interference signal; a construction module is used to construct the interference peak-to-peak value position of the upper surface of the adhesive film and the interference peak-to-peak value position of the lower surface of the adhesive film based on the associated data and the white light interference signal; a determination module is used to determine the corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the interference peak-to-peak value position of the upper surface and the interference peak-to-peak value position of the lower surface; and an evaluation module is used to evaluate the adhesive thickness on the surface of the adhesive-coated glass substrate based on the corrected thickness of the adhesive film.
[0132] In the above-mentioned device, the acquisition module is also used to obtain the measurement signals of the white light interferometer at multiple measurement light points of the adhesive film on the surface of the glue-coated glass substrate; pre-process the measurement signals to obtain the white light interference signals corresponding to the adhesive film on the surface of the glue-coated glass substrate; determine the reflectivity of the upper surface, the reflectivity of the reflector and the refractive index of the adhesive film to obtain the associated data of the adhesive film on the surface of the glue-coated glass substrate.
[0133] In the above device, the construction module is also used to construct a white light interference signal curve and a reference white light interference signal curve based on the light intensity values of the pixel points in the white light interference signal; based on the associated data, determine the interference peak intensity ratio between the light intensity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the light intensity corresponding to the reflector in the white light interference signal; based on the white light interference signal curve, the reference white light interference signal curve and the interference peak intensity ratio, construct the interference peak peak position of the upper surface and the interference peak peak position of the lower surface of the adhesive film. In the above device, the construction module is also used to obtain the reflectivity of the upper surface and the reflectivity of the reflector in the associated data; based on the reflectivity of the upper surface and the reflectivity of the reflector, determine the interference peak intensity ratio.
[0134] In the above device, the construction module is also used to expand the data points in the reference white light interference signal curve based on the white light interference signal curve to obtain a first adjusted curve; determine the maximum point in the first adjusted curve; determine the interference peak-to-peak position of the upper surface and the interference peak-to-peak position of the lower surface based on the maximum point and the white light interference signal curve. In the above device, the construction module is also used to perform envelope extraction on the first adjusted curve to obtain an interference envelope; determine the maximum point based on the interference envelope.
[0135] In the above-mentioned device, the construction module is also used to determine the position of the interference peak-to-peak value with the smallest value in the white light interference signal curve based on the position of the maximum point in the first modulated curve, so as to obtain the interference peak-to-peak value position of the upper surface; based on the interference peak-to-peak value with the smallest value and the interference peak-to-peak value in the first modulated curve, adjust the data points in the first modulated curve to obtain a white light interference signal approximate curve; use the data points in the white light interference signal curve to adjust the data points in the white light interference signal approximate curve to obtain a second modulated curve; and determine the position of the interference peak-to-peak value with the smallest value in the second modulated curve as the interference peak-to-peak value position of the lower surface.
[0136] In the above device, the construction module is also used to determine the difference between the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first adjusted curve; assign the difference value to the data point in the first adjusted curve to obtain the white light interference signal approximate curve.
[0137] In the above device, the construction module is also used to adjust the vertical coordinates of the data points in the white light interference signal approximation curve using the vertical coordinates of the data points in the white light interference signal curve to obtain the candidate curve; and smooth the candidate curve to obtain the second adjusted curve.
[0138] In the above device, the evaluation module is also used to obtain a white light interference signal of any measuring light point on the surface of the glue-coated glass substrate; determine the glue film thickness at the location of any measuring light point based on the glue film correction thickness of multiple pixel points in the white light interference signal of any measuring light point; determine the glue film uniformity and glue film thickness on the surface of the glue-coated glass substrate based on the glue film thickness at the locations of multiple measuring light points; and evaluate the glue thickness on the surface of the glue-coated glass substrate based on the glue film uniformity and glue film thickness on the surface of the glue-coated glass substrate.
[0139] Optionally, the transmission medium can be a wired link (such as but not limited to coaxial cable, optical fiber and digital subscriber line (DSL)) or a wireless link (such as but not limited to wireless Fidelity (WIFI), Bluetooth and mobile device network).
[0140] It should be noted that: the device provided in the above embodiment is only illustrated by the division of the above functional modules. In actual applications, the above functions can be assigned to different functional modules as needed, that is, the internal structure of the computer device is divided into different functional modules to complete all or part of the functions described above. In addition, the shopping guide device provided in the above embodiment and the image extension method embodiment belong to the same concept. The specific implementation process is detailed in the method embodiment and will not be repeated here.
[0141] Fig.10 is a schematic diagram of the structure of a computer device provided by an embodiment of the present invention. Fig.10 As shown, the computer device 900 includes: a memory 901, a processor 902, and a computer program 903 stored in the memory 901 and running on the processor 902, wherein when the processor 902 executes the computer program 903, the computer device can execute any of the glass substrate glue coating multi-point thickness evaluation methods based on data analysis introduced above.
[0142] In addition, an embodiment of the present invention also protects a device, which may include a memory and a processor, wherein the memory stores an executable program code, and the processor is used to call and execute the executable program code to execute the glass substrate multi-point glue thickness evaluation method based on data analysis provided by an embodiment of the present invention.
[0143] This embodiment can divide the functional modules of the device according to the above method example. For example, it can correspond to each functional module, or two or more functions can be integrated into one processing module. The above integrated module can be implemented in the form of hardware. It should be noted that the division of modules in this embodiment is schematic and is only a logical function division. There may be other division methods in actual implementation. In the case of dividing each module corresponding to each function, the device may also include a signal uploading module, a determination module, an adjustment module, etc. It should be noted that all relevant contents of each step involved in the above method embodiment can be referred to the functional description of the corresponding functional module, which will not be repeated here.
[0144] It should be understood that the device provided in this embodiment is used to perform the above-mentioned glass substrate glue coating multi-point glue thickness evaluation method based on data analysis, so the same effect as the above-mentioned implementation method can be achieved. In the case of an integrated unit, the device may include a processing module and a storage module. Among them, when the device is applied to a device, the processing module can be used to control and manage the actions of the device. The storage module can be used to support the device to execute mutual program codes, etc. Among them, the processing module can be a processor or a controller, which can implement or execute various exemplary logic boxes, modules and circuits described in conjunction with the disclosure of the present invention. The processor can also be a combination that implements a computing function, such as a combination of one or more microprocessors, a combination of digital signal processing (DSP) and a microprocessor, etc., and the storage module can be a memory.
[0145] In addition, the device provided in the embodiment of the present invention may be a chip, a component or a module, and the chip may include a connected processor and a memory; wherein the memory is used to store instructions, and when the processor calls and executes the instructions, the chip may execute the method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided in the above embodiment. This embodiment also provides a computer-readable storage medium, in which a computer program code is stored, and when the computer program code is run on a computer, the computer executes the above-mentioned related method steps to implement the method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis provided in the above embodiment.
[0146] This embodiment also provides a computer program product. When the computer program product is run on a computer, the computer executes the above-mentioned related steps to implement the glass substrate glue coating multi-point glue thickness evaluation method based on data analysis provided in the above embodiment. Among them, the device, computer-readable storage medium, computer program product or chip provided in this embodiment are all used to execute the corresponding method provided above. Therefore, the beneficial effects that can be achieved can refer to the beneficial effects in the corresponding method provided above, and will not be repeated here. Through the description of the above implementation mode, the technicians in the relevant field can understand that for the convenience and simplicity of description, only the division of the above-mentioned functional modules is used as an example. In practical applications, the above-mentioned function allocation can be completed by different functional modules as needed, that is, the internal structure of the device is divided into different functional modules to complete all or part of the functions described above. In the embodiments provided by the present invention, it should be understood that the disclosed device and method can be implemented in other ways. For example, the device embodiment described above is only schematic. For example, the division of modules or units is only a logical function division. There may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another device, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed may be an indirect coupling or communication connection through some interface, device or unit, which may be electrical, mechanical or other forms.
[0147] It should be noted that the sequence of the above-mentioned embodiments of the present invention is only for description and does not represent the advantages and disadvantages of the embodiments. The process depicted in the accompanying drawings does not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multi-tasking and parallel processing are also possible or may be advantageous. The various embodiments in this specification are described in a progressive manner, and the same and similar parts between the various embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. The above content is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can easily think of changes or replacements within the technical scope disclosed by the present invention, which should be covered within the protection scope of the present invention. Therefore, the protection scope of the present invention shall be based on the protection scope of the claims.
Claims
1. A method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis, characterized in that: The method comprises: Obtaining correlation data of the adhesive film on the surface of the adhesive-coated glass substrate and the corresponding white light interference signal; Based on the correlation data and the white light interference signal, constructing the peak-to-peak position of the interference peak on the upper surface of the adhesive film and the peak-to-peak position of the interference peak on the lower surface of the adhesive film; Determining a corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface; Based on the corrected thickness of the adhesive film, evaluating the adhesive thickness on the surface of the adhesive-coated glass substrate; The step of constructing the peak-to-peak interference position of the upper surface of the adhesive film and the peak-to-peak interference position of the lower surface of the adhesive film based on the correlation data and the white light interference signal comprises: Based on the light intensity values of the pixels in the white light interference signal, constructing a white light interference signal curve and a reference white light interference signal curve; Based on the correlation data, determining the interference peak intensity ratio between the light intensity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the light intensity corresponding to the reflector in the white light interference signal; Based on the white light interference signal curve, the reference white light interference signal curve and the interference peak intensity ratio, constructing the interference peak peak position of the upper surface and the interference peak peak position of the lower surface of the film; The step of determining the corrected thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface comprises: Calculate the white light interference signal curve The peak position of the interference peak on the upper surface , the peak position of the interference peak on the lower surface The corresponding scanning distance of the white light interferometer is combined with the refractive index S of the surface adhesive film on the coated glass substrate to obtain the surface adhesive film on the coated glass substrate at the pixel point. Corrected film thickness at , as shown in the formula: .
2. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 1, characterized in that: The step of obtaining the associated data of the adhesive film on the surface of the adhesive-coated glass substrate and the corresponding white light interference signal comprises: Acquire measurement signals of a white light interferometer at a plurality of measurement light points of the adhesive film on the surface of the adhesive-coated glass substrate; Preprocessing the measurement signal to obtain a white light interference signal corresponding to the adhesive film on the surface of the adhesive-coated glass substrate; The reflectivity of the upper surface, the reflectivity of the reflector and the refractive index of the adhesive film are determined to obtain the associated data of the adhesive film on the surface of the adhesive-coated glass substrate.
3. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 1, characterized in that: The step of determining the interference peak intensity ratio between the light intensity of the upper surface of the adhesive film on the surface of the adhesive-coated glass substrate and the light intensity corresponding to the reflector in the white light interference signal based on the associated data includes: Acquire the reflectivity of the upper surface and the reflectivity of the reflector in the associated data; The interference peak light intensity ratio is determined based on the reflectivity of the upper surface and the reflectivity of the reflector.
4. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 1, characterized in that: The method of constructing the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface of the adhesive film based on the white light interference signal curve, the reference white light interference signal curve and the interference peak intensity ratio comprises: Expanding the data points in the reference white light interference signal curve based on the white light interference signal curve to obtain a first adjusted curve; In the first adjusted curve, determining a maximum point; Based on the maximum point and the white light interference signal curve, the peak-to-peak position of the interference peak on the upper surface and the peak-to-peak position of the interference peak on the lower surface are determined.
5. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 4, characterized in that: Determining a maximum point in the first adjusted curve includes: Performing envelope extraction on the first adjusted curve to obtain an interference envelope; Based on the interference envelope, the maximum point is determined.
6. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 4, characterized in that: The determining, based on the maximum point and the white light interference signal curve, the interference peak-to-peak position of the upper surface and the interference peak-to-peak position of the lower surface comprises: Based on the position of the maximum point in the first modulated curve, determining the position of the interference peak-to-peak value with the minimum value in the white light interference signal curve to obtain the interference peak-to-peak value position of the upper surface; Based on the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first modulated curve, adjusting the data points in the first modulated curve to obtain an approximate curve of a white light interference signal; Using the data points in the white light interference signal curve to adjust the data points in the white light interference signal approximation curve to obtain a second adjusted curve; The position of the interference peak-to-peak value with the smallest value in the second adjusted curve is determined as the interference peak-to-peak value position of the lower surface.
7. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 6, characterized in that: The step of adjusting the data points in the first modulated curve based on the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first modulated curve to obtain an approximate curve of the white light interference signal includes: Determine a difference between the interference peak-to-peak value with the minimum value and the interference peak-to-peak value in the first adjusted curve; The difference value is assigned to the data points in the first adjusted curve to obtain the white light interference signal approximate curve.
8. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 6, characterized in that: The step of adjusting the data points in the white light interference signal approximation curve by using the data points in the white light interference signal curve to obtain a second adjusted curve comprises: Using the ordinates of the data points in the white light interference signal curve to adjust the ordinates of the data points in the white light interference signal approximation curve to obtain a candidate curve; The candidate curve is smoothed to obtain the second adjusted curve.
9. The method for evaluating the thickness of multi-point glue coating on a glass substrate based on data analysis according to claim 1, characterized in that: The step of evaluating the adhesive thickness on the surface of the adhesive-coated glass substrate based on the corrected adhesive film thickness includes: Acquire a white light interference signal of any measuring light point on the surface of the glue-coated glass substrate; Determine the thickness of the adhesive film at the location of any measuring light point based on the corrected thickness of the adhesive film at multiple pixel points in the white light interference signal of any measuring light point; Determining the uniformity and thickness of the adhesive film on the surface of the adhesive-coated glass substrate based on the adhesive film thickness at the locations of the plurality of measuring light spots; Based on the uniformity and thickness of the adhesive film on the surface of the adhesive-coated glass substrate, the thickness of the adhesive on the surface of the adhesive-coated glass substrate is evaluated.
Citation Information
Patent Citations
Method and apparatus for performing film thickness measurements using white light scanning interferometry
CN102620665A
Ultrathin film device three-dimensional morphology detection method based on structure illumination obvious microsystem
CN111829457A
Method for measuring thickness and refractive index of thin film
CN113834430A
Novel white light interference detection method for displaying thin film morphology in jet printing manufacturing
CN118243010A
Thickness measurement instrument and thickness measurement method of light-transmissive object
JP2014048216A