A performance testing device and performance testing method for polyurethane material
By designing a polyurethane material performance detection equipment with loading rods and clamping devices combined with variable aperture components, the problem of incomplete and inaccurate detection in the prior art is solved, and a comprehensive evaluation and high-precision detection of the thermal performance of polyurethane pipes is achieved.
Patent Information
- Application Number
- CN202411142822.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-08-20
AI Technical Summary
The existing polyurethane pipe heat resistance testing devices are not comprehensive and inaccurate enough. Mechanical pressurization only detects performance in one direction. Machine vision detection requires the transfer of the light source environment and the temperature drop is affected.
A polyurethane material performance detection equipment is designed, using a loading rod and clamping device combined with a variable aperture assembly, and applying pressure to the suspended pipe from multiple directions through a pressurized sheet to conduct thermal performance testing to avoid the influence of temperature drop.
A comprehensive evaluation of the thermal performance of polyurethane pipes has been achieved, and the detection accuracy and accuracy are improved.
Smart Images

Figure CN118671130B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of material detection, and in particular to a performance detection device and a performance detection method for a polyurethane material. Background Art
[0002] Polyurethane (PU), the full name of polyurethane, is a polymer material with excellent mechanical properties formed by the polycondensation reaction of polyols and polyisocyanates, and has excellent plasticity. Polyurethane materials are generally used to prepare pipes, and the resulting pipes can be used in many fields such as aviation, transportation, medical care, and electronics. However, the heat resistance of polyurethane pipes is poor, and its mechanical properties decrease under high temperature conditions. In actual use, high temperature performance is also an important indicator for evaluating materials. Therefore, during the trial production of polyurethane pipes, heat resistance testing of polyurethane pipes is an important verification step in the development process of polyurethane.
[0003] At present, the heat resistance testing device for polyurethane pipes mainly adopts a closed structure such as an oven. The polyurethane pipe is placed in the oven for heating. After the polyurethane pipe is placed in the oven for a period of time, the performance of the polyurethane pipe after heating can be obtained by mechanically applying stress and observing the state of the polyurethane pipe with machine vision.
[0004] 1. The mechanical stress-applying scheme generally uses a cylinder or a hydraulic cylinder to pressurize the polyurethane pipe, which can only detect the heat resistance performance of the polyurethane pipe in a certain direction, and the heat resistance performance evaluation of the polyurethane pipe is not comprehensive; 2. The machine vision scheme has high requirements for the light source. The polyurethane pipe needs to be taken out of the oven and placed in a specified light source environment. There is a temperature drop during the transfer process, and the detection of the heat resistance performance of the polyurethane pipe is not accurate enough.
[0005] Therefore, it is necessary to propose a new polyurethane testing equipment to solve the defects of the current testing scheme, such as incomplete performance evaluation and inaccurate testing. Summary of the invention
[0006] The purpose of the present invention is to provide a performance testing device and a performance testing method for a polyurethane material, so as to solve the problem of insufficient detection accuracy of the detection scheme in the prior art.
[0007] To achieve this object, the present invention adopts the following technical solutions:
[0008] A performance testing device for polyurethane materials, comprising a baking device with a baking chamber therein; a loading device and a sample device are arranged on one side of the baking device, and a clamping device is arranged on the other side of the baking device;
[0009] The loading device comprises a loading rod which can be inserted into the baking cavity, and the loading rod is sleeved with the polyurethane tube to be tested; the clamping device is used to clamp the end of the polyurethane tube that extends beyond the loading rod; the sample device comprises a variable aperture component which can be inserted into the baking cavity, and the variable aperture component comprises a plurality of pressure sheets arranged around the polyurethane tube, and each of the pressure sheets can move in a direction away from or close to the polyurethane tube;
[0010] When the loading rod is extended into the baking chamber and the heating is completed, the clamping device clamps the polyurethane tube beyond the end of the loading rod, the variable aperture assembly extends into the baking chamber, and the loading rod moves in a direction away from the clamping device to form a suspended polyurethane tube;
[0011] When the loading rod moves in a direction away from the clamping device, the variable aperture assembly moves synchronously with the loading rod, and each of the pressure sheets applies pressure to the suspended polyurethane pipe.
[0012] Optionally, the loading device further comprises a first cylinder, which is arranged at one side of the baking device, and the movable rod of the first cylinder can move in a direction close to or away from the clamping device, and is installed with a loading plate; a plurality of the loading rods are installed on the loading plate at intervals, and the extending direction of the loading rods is parallel to the telescopic direction of the first cylinder;
[0013] The sample device is provided with a variable aperture assembly corresponding to each loading rod, and the variable aperture assembly includes a pressure hole formed by a plurality of pressure sheets, and the axis of the pressure hole coincides with the axis of the loading rod.
[0014] Optionally, the variable aperture assembly includes four pressure sheets arranged around the polyurethane tube, the pressure sheets include a pressure surface and an abutment surface arranged at right angles; between any two adjacent pressure sheets, the pressure surface of one pressure sheet contacts the abutment surface of another pressure sheet, so that the position of each pressure surface relative to the corresponding abutment surface is adjustable;
[0015] The pressure plate also includes an adjustment surface, an adjustment gear is arranged on one side of the adjustment surface, the pressure surface, the abutment surface and the adjustment surface are arranged in a triangle, a tooth groove is formed on the adjustment surface, and the adjustment gear is meshed with the tooth groove.
[0016] Optionally, the thickness of the adjusting gear is greater than the thickness of the pressure sheet, the portion where the adjusting gear overlaps with the pressure sheet is a first tooth portion, and the portion where the adjusting gear exceeds the pressure sheet is a second tooth portion;
[0017] The variable aperture assembly also includes a variable aperture motor and a gear ring. The gear ring is driven by the variable aperture motor and meshes with the second tooth portion of each adjusting gear. The gear ring is formed with external teeth or internal teeth.
[0018] Optionally, the variable aperture assembly further includes a variable aperture motor provided corresponding to each of the adjusting gears, and the adjusting gears are driven to rotate by the variable aperture motor.
[0019] Optionally, a clamping hole is provided on the other side wall of the baking chamber corresponding to the position of each loading rod;
[0020] The clamping device comprises a clamping driving member, an upper clamping member and a lower clamping seat; the lower clamping seat is arranged on the other side of the baking device and is located below the clamping hole;
[0021] The clamping drive member is arranged above the baking device, and the movable end of the clamping drive member is fixedly connected to the upper clamping member, so that the upper clamping member can move in a direction close to the lower clamping seat to make the end of the polyurethane tube beyond the loading rod abut against the lower clamping seat.
[0022] Optionally, a sealing device is further included, and a cavity wall on one side of the baking cavity is provided with an entrance corresponding to the sample device;
[0023] The closing device comprises a closing drive installed above the baking device, a closing plate is installed at a movable end of the closing drive, and the movable end of the closing drive can move in a direction close to the entrance so that the closing plate closes the entrance.
[0024] Optionally, it further comprises a first moving device, the moving end of which is equipped with the baking device, and the first moving device can move in a direction close to or away from the loading device;
[0025] Wherein, the maximum movable distance between the baking device and the loading device is greater than the length of the polyurethane pipe.
[0026] Optionally, a heating unit and a quartz glass plate are provided in the baking chamber, the heating unit is provided below the quartz glass plate, and the quartz glass plate is provided below the inlet.
[0027] A method for detecting the performance of a polyurethane material, applied to the above-mentioned polyurethane material performance detection device, comprises:
[0028] The loading rod with the polyurethane tube is put into the baking chamber, and the polyurethane tube is subjected to a thermal test;
[0029] Fix the end of the polyurethane tube and move the loading rod out of the baking chamber to form a suspended polyurethane tube;
[0030] During the process of the loading rod moving out of the baking chamber, the suspended polyurethane pipe is pressurized from multiple directions;
[0031] Determine whether the removal acceleration of the loading rod exceeds the preset qualified value. If so, mark the polyurethane pipe as an NG sample.
[0032] Compared with the prior art, the present invention has the following beneficial effects:
[0033] The performance testing device and performance testing method of the polyurethane material provided by the present invention, when the polyurethane pipe is subjected to thermal performance testing, the polyurethane pipe is sent into the baking chamber for heating by using a loading rod, after the heating is completed, the end of the polyurethane pipe that exceeds the loading rod is clamped by a clamping device, and as the loading rod moves in a direction away from the clamping device, a suspended polyurethane pipe with both ends supported is formed, and then the suspended polyurethane pipe is pressurized by a variable aperture component extending into the baking chamber to complete the thermal performance test of the polyurethane pipe. During the thermal performance test, a plurality of pressure plates arranged around the polyurethane pipe can be used to apply pressure to the polyurethane pipe from multiple directions, and during the movement of the loading rod in a direction away from the clamping device, any position of the suspended polyurethane pipe can be detected in sequence, so as to achieve a comprehensive evaluation of the thermal performance of the polyurethane pipe. At the same time, during the above-mentioned detection process, the detection of the polyurethane pipe is all located in the baking chamber, avoiding the influence of the temperature drop during the transfer process, thereby improving the accuracy of the detection. Therefore, the performance testing device and performance testing method of the polyurethane material provided by the present scheme have the advantage of high detection accuracy. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0035] The structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with this technology. They are not used to limit the conditions under which the present invention can be implemented, and therefore have no substantive technical significance. Any structural modification, change in proportion or adjustment of size, without affecting the effects and purposes that can be achieved by the present invention, should still fall within the scope of the technical contents disclosed by the present invention.
[0036] Figure 1 A schematic diagram of the overall structure of a performance testing device for polyurethane materials provided in an embodiment of the present invention;
[0037] Figure 2 A schematic diagram of a first partial structure of a performance testing device for a polyurethane material provided by an embodiment of the present invention;
[0038] Figure 3 A first top view schematic diagram of the structure of a performance testing device for a polyurethane material provided by an embodiment of the present invention;
[0039] Figure 4 A second top view schematic diagram of the structure of the performance testing device for polyurethane materials provided by an embodiment of the present invention;
[0040] Figure 5 A third top view schematic diagram of the structure of the polyurethane material performance testing device provided by an embodiment of the present invention;
[0041] Figure 6 for Figure 5 Schematic diagram of the cross-section structure along AA;
[0042] Figure 7 A schematic diagram of the first state structure of a performance testing device for polyurethane materials provided by an embodiment of the present invention;
[0043] Figure 8 A schematic diagram of the second state structure of the performance testing device for polyurethane materials provided by an embodiment of the present invention;
[0044] Fig. 9 It is a schematic diagram of the first state structure principle of the variable aperture component in an embodiment of the present invention;
[0045] Fig.10 It is a schematic diagram of the second state structure principle of the variable aperture component in an embodiment of the present invention;
[0046] Fig.11 is a first transmission schematic diagram of the variable aperture assembly in an embodiment of the present invention;
[0047] Fig.12 is a second transmission schematic diagram of the variable aperture assembly in an embodiment of the present invention;
[0048] Illustration: 100, baking device; 101, baking chamber; 102, clamping hole; 103, entrance; 110, heating unit; 120, quartz glass plate; 130, baking shell;
[0049] 200, loading device; 210, loading rod; 220, first cylinder; 230, loading plate;
[0050] 300, clamping device; 310, clamping driving member; 320, upper clamping member; 330, lower clamping seat;
[0051] 400, sample device; 410, variable aperture assembly; 411, pressure plate; 411a, pressure surface; 411b, abutment surface; 411c, adjustment surface; 411d, tooth groove; 412, pressure hole; 413, adjustment gear; 413a, first tooth portion; 413b, second tooth portion; 414, gear ring; 414a, external tooth; 414b, internal tooth; 420, guide rod; 430, third cylinder;
[0052] 500, closing device; 510, closing drive member; 520, closing plate; 600, first moving device; 610, second cylinder; 700, polyurethane pipe. DETAILED DESCRIPTION
[0053] In order to make the purpose, features and advantages of the present invention more obvious and easy to understand, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the embodiments described below are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0054] In the description of the present invention, it should be understood that the terms "upper", "lower", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. It should be noted that when a component is considered to be "connected" to another component, it may be directly connected to the other component or there may be a centrally arranged component at the same time.
[0055] The technical solution of the present invention is further described below with reference to the accompanying drawings and through specific implementation methods.
[0056] Embodiment 1:
[0057] The performance testing equipment for polyurethane materials provided in this embodiment is mainly used in scenarios where thermal performance testing of polyurethane pipes 700 is performed. By optimizing the structure of the performance testing equipment, the testing accuracy can be improved.
[0058] like Figures 1 to 5 As shown, the performance testing equipment of the polyurethane material in this embodiment includes a baking device 100 with a baking chamber 101 therein; a loading device 200 and a sample device 400 are arranged on one side of the baking device 100, and a clamping device 300 is arranged on the other side of the baking device 100.
[0059] like Figure 4 As shown, the loading device 200 includes a loading rod 210 that can extend into the baking chamber 101, and the loading rod 210 is sleeved with a polyurethane pipe 700 to be tested; Figure 2 As shown, the clamping device 300 is used to clamp the end of the polyurethane tube 700 beyond the loading rod 210; Fig. 9 As shown, the sample device 400 includes a variable aperture component 410 that can extend into the baking chamber 101. The variable aperture component 410 includes a plurality of pressure plates 411 arranged around the polyurethane tube 700. Each pressure plate 411 can move in a direction away from or close to the polyurethane tube 700.
[0060] like Figure 6 As shown, the polyurethane tube 700 is first passed through the variable aperture component 410 and sleeved on the loading rod 210 to complete the loading action of the polyurethane tube 700. At this time, the pressure plate 411 is set away from the polyurethane tube 700, which is convenient for the staff to pass the polyurethane tube 700 through the variable aperture component 410 and sleeved on the loading rod 210.
[0061] like Figure 7 and Figure 8 As shown, when the loading rod 210 extends into the baking chamber 101 and completes heating, the clamping device 300 clamps the polyurethane tube 700 beyond the end of the loading rod 210, the variable aperture assembly 410 extends into the baking chamber 101, and the loading rod 210 moves in a direction away from the clamping device 300 to form a suspended polyurethane tube 700.
[0062] like Fig. 9 and Fig.10 As shown, when the loading rod 210 moves in a direction away from the clamping device 300 , the variable aperture assembly 410 moves synchronously with the loading rod 210 , and each pressure sheet 411 applies pressure to the suspended polyurethane tube 700 .
[0063] It should be pointed out that, in the process of the loading rod 210 moving in the direction away from the clamping device 300, the end of the polyurethane tube 700 is clamped, and the loading rod 210 is subjected to the friction force of the polyurethane tube 700. The friction force is balanced with the driving force (the force that moves the loading rod 210 away) exerted on the loading rod 210, which can ensure that the loading rod 210 is slowly separated from the polyurethane tube 700, and the end of the polyurethane tube 700 that exceeds the loading rod 210 is clamped, so that the middle part of the polyurethane tube 700 is suspended. At this time, the variable aperture assembly 410 extending into the baking chamber 101 can move each pressurizing sheet 411 in a direction close to the polyurethane tube 700, and pressurize the polyurethane tube 700 from multiple directions. When the thermal performance of the polyurethane tube 700 is qualified, the suspended polyurethane tube 700 only deforms, indicating that the strength of the polyurethane tube 700 is qualified; when the thermal performance of the polyurethane tube 700 is unqualified, the suspended polyurethane tube 700 breaks, and the polyurethane tube 700 is divided into two parts clamped by the clamping device 300. At this time, the clamping device 300 cannot affect the loading rod 210 through the clamping force and the friction force, which means that the force on the loading rod 210 increases instantaneously, and the acceleration of the loading rod 210 increases. At this time, it is possible to determine whether the polyurethane tube 700 is broken by detecting the acceleration of the loading rod 210, without the need for additional structures such as machine vision to make a judgment. After the break, the pressurizing action of the variable aperture component 410 is stopped, and an error is reported through structures such as lighting and a buzzer.
[0064] The performance testing device for polyurethane materials provided by the present invention performs a thermal performance test on a polyurethane tube 700 by using a loading rod 210 to feed the polyurethane tube 700 into a baking chamber 101 for heating. After the heating is completed, a clamping device 300 is used to clamp the end of the polyurethane tube 700 that extends beyond the loading rod 210. As the loading rod 210 moves in a direction away from the clamping device 300, a suspended polyurethane tube 700 with two ends supported is formed (one end is fixed by the clamping device 300, and the other end is supported by the loading rod 210). Then, the suspended polyurethane tube 700 is pressurized by a variable aperture component 410 extending into the baking chamber 101 to complete the thermal performance test of the polyurethane tube 700. During the thermal performance test, multiple pressure sheets 411 arranged around the polyurethane tube 700 can be used to apply pressure to the polyurethane tube 700 from multiple directions, and during the movement of the loading rod 210 in the direction away from the clamping device 300, any position of the suspended polyurethane tube 700 can be tested in sequence to achieve a comprehensive evaluation of the thermal performance of the polyurethane tube 700. At the same time, during the above-mentioned testing process, the testing of the polyurethane tube 700 is all located in the baking chamber 101, avoiding the influence of the temperature drop during the transfer process, thereby improving the accuracy of the test. Therefore, the performance testing equipment of the polyurethane material provided in this embodiment has the advantage of high testing accuracy.
[0065] Furthermore, if Figures 1 to 4 As shown, the loading device 200 further includes a first cylinder 220, which is disposed on one side of the baking device 100. The movable rod of the first cylinder 220 can move in a direction close to or away from the clamping device 300, and is installed with a loading plate 230; a plurality of loading rods 210 are installed on the loading plate 230 at intervals, and the extension direction of the loading rods 210 is parallel to the extension direction of the first cylinder 220. Fig. 9 and Fig.10 As shown, the sample device 400 is provided with a variable aperture assembly 410 corresponding to each loading rod 210 , and the variable aperture assembly 410 includes a pressurizing hole 412 surrounded by a plurality of pressurizing sheets 411 , and the axis of the pressurizing hole 412 coincides with the axis of the loading rod 210 .
[0066] It should be noted that, in the process of passing the polyurethane tube 700 through the variable aperture assembly 410 and sleeved on the loading rod 210, the first cylinder 220 is in a contracted state, and the pressurized hole 412 is in a state of maximum diameter. At this time, the staff can directly pass the polyurethane tube 700 through the variable aperture assembly 410 and sleeved on the loading rod 210. As other optional embodiments, the first cylinder 220 can be replaced by other power sources such as a linear motor.
[0067] Furthermore, the performance testing device of the polyurethane material further comprises a first moving device 600, a baking device 100 is installed at the moving end of the first moving device 600, and the first moving device 600 can move in a direction close to or away from the loading device 200; wherein, the maximum movable distance between the baking device 100 and the loading device 200 is greater than the length of the polyurethane tube 700. The first moving device 600 comprises a second cylinder 610, and the second cylinder 610 can drive the baking device 100 to move. In the process of passing the polyurethane tube 700 through the variable aperture assembly 410 and sleeved on the loading rod 210, the baking device 100 is driven away from the loading device 200 by the second cylinder 610, leaving enough space for the staff to sleeve the polyurethane tube 700 on the loading rod 210.
[0068] In this embodiment, the performance testing equipment for polyurethane materials also includes a closing device 500, and an entrance port 103 is opened on one side wall of the baking chamber 101 corresponding to the sample device 400; the closing device 500 includes a closing drive member 510 installed above the baking device 100, and a closing plate 520 is installed at the movable end of the closing drive member 510, and the movable end of the closing drive member 510 can move in a direction close to the entrance port 103, so that the closing plate 520 closes the entrance port 103.
[0069] In this embodiment, a clamping hole 102 is opened on the cavity wall on the other side of the baking cavity 101 corresponding to the position of each loading rod 210; the clamping device 300 includes a clamping drive member 310, an upper clamping member 320 and a lower clamping seat 330; the lower clamping seat 330 is arranged on the other side of the baking device 100 and is located below the clamping hole 102; the clamping drive member 310 is arranged above the baking device 100, and the movable end of the clamping drive member 310 is fixedly connected to the upper clamping member 320, so that the upper clamping member 320 can move in a direction close to the lower clamping seat 330, so as to make the end of the polyurethane tube 700 that extends beyond the loading rod 210 abut against the lower clamping seat 330.
[0070] It should be noted that when the loading rod 210 or the variable aperture assembly 410 is extended into the baking chamber 101, the closing plate 520 can be lifted by the closing driving member 510 to expose the entrance 103, so that the loading rod 210 or the variable aperture assembly 410 can be extended into the baking chamber 101; when the polyurethane pipe 700 is heated, the closing plate 520 is lowered by the closing driving member 510 to close the entrance 103. In addition, the wall surface of the variable aperture assembly 410 facing the baking device 100 can be affixed with heat insulation cotton, and after the closing plate 520 is lowered, the heat insulation cotton can be attached to the outer side of the closing plate 520 away from the baking chamber 101 to improve the thermal efficiency.
[0071] After heating is completed, the loading rod 210 is extended to the maximum distance, and the clamping drive 310 drives the upper clamping member 320 away from the lower clamping seat 330, so that the clamping hole 102 is connected to the inside and outside of the baking chamber 101, which facilitates the end of the polyurethane tube 700 to pass through the clamping hole 102 and move to the lower clamping seat 330; then, the clamping drive 310 drives the upper clamping member 320 to approach the lower clamping seat 330, and the upper clamping member 320 and the lower clamping seat 330 complete the clamping of the end of the polyurethane tube 700. During the test, except for the above-mentioned nodes, the upper clamping member 320 and the lower clamping seat 330 are fitted to block the clamping hole 102, thereby improving the thermal efficiency.
[0072] As a supplementary explanation, the above-mentioned clamping drive member 310 and the closing drive member 510 can be selected from structures such as cylinders, liquid cylinders, and lifting motors, and are jointly installed on the baking shell 130 of the baking device 100. A baking box is provided in the baking shell 130, and the baking box is equipped with the above-mentioned baking cavity 101. The baking cavity 101 is provided with a heating unit 110 and a quartz glass plate 120. The heating unit 110 is arranged below the quartz glass plate 120, and the quartz glass plate 120 is arranged below the entrance 103. The heating unit 110 can select an electric heating rod.
[0073] In this embodiment, if Figures 9 to 12 As shown, the variable aperture component 410 includes four pressure plates 411 arranged around the polyurethane tube 700, and the pressure plates 411 include a pressure surface 411a and an abutment surface 411b arranged at right angles; between any two adjacent pressure plates 411, the pressure surface 411a of one pressure plate 411 contacts the abutment surface 411b of the other pressure plate 411, so that the position of each pressure surface 411a relative to the corresponding abutment surface 411b is adjustable; the pressure plate 411 also includes an adjustment surface 411c, and an adjustment gear 413 is arranged on one side of the adjustment surface 411c. The pressure surface 411a, the abutment surface 411b and the adjustment surface 411c are arranged in a triangle, and a tooth groove 411d is formed on the adjustment surface 411c, and the adjustment gear 413 meshes with the tooth groove 411d. Figures 9 and 10 As shown, when each adjusting gear 413 rotates clockwise, the engagement between the adjusting gear 413 and the tooth groove 411d can drive the pressure plate 411 to move, and the pressure surface 411a of the pressure plate 411 is limited by the adjacent abutting surface 411b, and the abutting surface 411b of the pressure plate 411 is limited by the adjacent pressure surface 411a, so that the pressure plate 411 can move in a directional manner; the size of the rectangular pressure hole 412 can be gradually narrowed to apply pressure to the middle polyurethane pipe 700, which has the advantage of compact structure.
[0074] As another optional embodiment, the variable aperture component 410 includes six pressure plates 411 arranged around the polyurethane tube 700, and the pressure plate 411 includes a pressure surface 411a and abutment surface 411b set at an angle of 60°; the rest of the settings are similar to the above settings and will not be repeated.
[0075] In this embodiment, the thickness of the adjusting gear 413 is greater than the thickness of the pressure plate 411, the portion where the adjusting gear 413 overlaps with the pressure plate 411 is the first tooth portion 413a, and the portion where the adjusting gear 413 extends beyond the pressure plate 411 is the second tooth portion 413b; the variable aperture assembly 410 also includes a variable aperture motor (not shown) and a ring gear 414, the ring gear 414 is driven by the variable aperture motor and meshes with the second tooth portion 413b of each adjusting gear 413, and the ring gear 414 is formed with external teeth 414a or internal teeth 414b.
[0076] For example, Fig.11 As shown, the gear ring 414 is driven to rotate around its axis by a variable diameter motor (the driving method can be gear transmission, worm gear transmission, helical gear transmission, etc., as long as it can drive the gear ring 414 to rotate around its axis). During the rotation of the gear ring 414, it drives each adjustment gear 413 to rotate through the external teeth 414a, thereby driving each pressure plate 411 to move. Fig.12 As shown, during the rotation of the ring gear 414, the inner teeth 414b drive the adjustment gears 413 to rotate, thereby driving the pressure plates 411 to move.
[0077] As another optional implementation, the variable aperture assembly 410 further includes a variable aperture motor provided corresponding to each adjusting gear 413 , and the adjusting gear 413 is driven to rotate by the variable aperture motor, so that each adjusting gear 413 is driven to rotate.
[0078] In this embodiment, the variable aperture assembly 410 is also equipped with a guide rod 420 and a third cylinder 430. The guide rod 420 is installed on the frame to provide a guide for the variable aperture assembly 410. The third cylinder 430 provides power for the variable aperture assembly 410 to move the variable aperture assembly 410. The third cylinder 430 can be replaced by other structures such as a linear motor, which can change the position of the variable aperture assembly 410.
[0079] Embodiment 2:
[0080] The performance testing method of the polyurethane material provided in this embodiment is applied to the performance testing device of the polyurethane material in the first embodiment, and includes:
[0081] S101, sending the loading rod 210 sleeved with the polyurethane tube 700 into the baking chamber 101, and performing a thermal test on the polyurethane tube 700;
[0082] S102, fixing the end of the polyurethane tube 700, and moving the loading rod 210 out of the baking chamber 101, so as to form a suspended polyurethane tube 700;
[0083] S103, while the loading rod 210 is moving out of the baking chamber 101, pressurizing the suspended polyurethane pipe 700 from multiple directions;
[0084] S104, determining whether the removal acceleration of the loading rod 210 exceeds a preset qualified value, and if so, marking the polyurethane tube 700 as an NG sample.
[0085] As other optional performance testing methods, which are applied to the performance testing equipment of the polyurethane material in Example 1, they include:
[0086] S201, using the second cylinder 610 to make the distance between the baking device 100 and the loading rod 210 larger than the length of the polyurethane tube 700, and to make the cross-sectional area of the pressure hole 412 larger than the cross-sectional area of the polyurethane tube 700;
[0087] S202, passing the polyurethane tube 700 through the pressure hole 412 and sleeved on the loading rod 210, and then moving the baking device 100 close to the loading rod 210 through the second cylinder 610;
[0088] S203, the sealing driving member 510 lifts the sealing plate 520 to expose the inlet 103, and drives the loading rod 210 to move into the baking chamber 101 through the first cylinder 220 until the loading plate 230 abuts against the variable aperture assembly 410; at this time, most of the polyurethane tube 700 is located in the baking chamber 101;
[0089] S204, the sealing driving member 510 lowers the sealing plate 520 to block the inlet 103, the variable aperture component 410 abuts against the sealing plate 520 through the thermal insulation cotton, and the heating unit 110 is started to heat the polyurethane tube 700 through the quartz glass 120;
[0090] S205, after the heating is completed, the clamping driving member 310 drives the upper clamping member 320 to separate from the lower clamping seat 330 to leak out the clamping hole 102;
[0091] S206, the third cylinder 430 drives the variable aperture assembly 410 to enter the baking chamber 101; the first cylinder 220 continues to drive the loading rod 210 to move into the baking chamber 101 until the end of the polyurethane tube 700 is located on the lower clamping seat 330; the clamping drive member 310 drives the upper clamping member 320 to press the end of the polyurethane tube 700 onto the lower clamping seat 330;
[0092] S207, the third cylinder 430 drives the variable aperture assembly 410 to enter the baking chamber 101, and adjusts the size of the pressurizing hole 412 so that the size of the pressurizing hole 412 is greater than the qualified value; and determines whether the removal acceleration of the loading rod 210 is reduced, and if so, marks the polyurethane pipe 700 as an NG sample;
[0093] It is understandable that after the polyurethane tube 700 is heated, if there is obvious deformation, the deformed part will directly contact the heating plate 412, causing the loading rod 210 to be impacted, which is reflected in the reduction of the removal acceleration. At this time, it means that the heat resistance of the polyurethane tube 700 is poor;
[0094] S208, after the third cylinder 430 reaches the limit position, the loading rod 210 is driven by the first cylinder 220 to move out of the baking chamber 101, and the variable diameter assembly 410 is moved to the suspended polyurethane pipe 700 by the third cylinder 430; and when the variable diameter assembly 410 reaches the inspection position, each pressurizing sheet 411 is moved inward to pressurize the suspended polyurethane pipe 700 from multiple directions;
[0095] S209, determining whether the removal acceleration of the loading rod 210 exceeds a preset qualified value, and if so, marking the polyurethane tube 700 as an NG sample.
[0096] In summary, the performance testing equipment and performance testing method of the polyurethane material in this embodiment can directly realize the heat resistance and thermal performance testing of the polyurethane tube 700 in the baking chamber 101, and has the advantages of compact structure, high precision, and high testing efficiency.
[0097] As described above, the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features thereof may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A performance testing device for polyurethane materials, characterized in that: It comprises a baking device (100) having a baking cavity (101) therein; a loading device (200) and a sample device (400) are arranged on one side of the baking device (100), and a clamping device (300) is arranged on the other side of the baking device (100); The loading device (200) comprises a loading rod (210) capable of extending into the baking cavity (101), the loading rod (210) being sleeved with a polyurethane tube (700) to be tested; the clamping device (300) is used to clamp the end of the polyurethane tube (700) that extends beyond the loading rod (210); the sample device (400) comprises a variable aperture component (410) capable of extending into the baking cavity (101), the variable aperture component (410) comprising a plurality of pressure sheets (411) arranged around the polyurethane tube (700), each of the pressure sheets (411) being capable of moving in a direction away from or close to the polyurethane tube (700); When the loading rod (210) extends into the baking chamber (101) and completes heating, the clamping device (300) clamps the polyurethane tube (700) beyond the end of the loading rod (210), the variable aperture assembly (410) extends into the baking chamber (101), and the loading rod (210) moves in a direction away from the clamping device (300), thereby forming a suspended polyurethane tube (700); When the loading rod (210) moves in a direction away from the clamping device (300), the variable aperture assembly (410) moves synchronously with the loading rod (210), and each of the pressure plates (411) applies pressure to the suspended polyurethane tube (700); The loading device (200) further comprises a first cylinder (220), the first cylinder (220) being arranged at one side of the baking device (100), the movable rod of the first cylinder (220) being able to move in a direction approaching or away from the clamping device (300), and being installed with a loading plate (230); a plurality of the loading rods (210) being installed at intervals on the loading plate (230), the extension direction of the loading rods (210) being parallel to the extension direction of the first cylinder (220); The sample device (400) is provided with a variable aperture assembly (410) corresponding to each loading rod (210), the variable aperture assembly (410) comprising a pressurizing hole (412) formed by a plurality of pressurizing sheets (411), and the axis of the pressurizing hole (412) coincides with the axis of the loading rod (210); The variable aperture component (410) comprises four pressure sheets (411) arranged around the polyurethane tube (700), and the pressure sheets (411) comprise a pressure surface (411a) and an abutment surface (411b) arranged at right angles; between any two adjacent pressure sheets (411), the pressure surface (411a) of one of the pressure sheets (411) contacts the abutment surface (411b) of the other pressure sheet (411), so that the position of each pressure surface (411a) relative to the corresponding abutment surface (411b) is adjustable; The pressure plate (411) further comprises an adjustment surface (411c), an adjustment gear (413) is arranged on one side of the adjustment surface (411c), the pressure surface (411a), the abutment surface (411b) and the adjustment surface (411c) are arranged in a triangular shape, a tooth groove (411d) is formed on the adjustment surface (411c), and the adjustment gear (413) meshes with the tooth groove (411d).
2. The performance testing equipment for polyurethane materials according to claim 1, characterized in that: The thickness of the adjusting gear (413) is greater than the thickness of the pressure plate (411); the portion where the adjusting gear (413) overlaps with the pressure plate (411) is a first tooth portion (413a); and the portion where the adjusting gear (413) exceeds the pressure plate (411) is a second tooth portion (413b); The variable aperture assembly (410) further comprises a variable aperture motor and a gear ring (414); the gear ring (414) is driven by the variable aperture motor and meshes with the second tooth portion (413b) of each adjusting gear (413); and the gear ring (414) is formed with external teeth (414a) or internal teeth (414b).
3. The performance testing equipment for polyurethane materials according to claim 1, characterized in that: The variable aperture assembly (410) further comprises a variable aperture motor arranged corresponding to each of the adjustment gears (413), and the adjustment gears (413) are driven to rotate by the variable aperture motor.
4. The performance testing device for polyurethane materials according to claim 1, characterized in that: A clamping hole (102) is provided on the other side wall of the baking cavity (101) at a position corresponding to each loading rod (210); The clamping device (300) comprises a clamping drive member (310), an upper clamping member (320) and a lower clamping seat (330); the lower clamping seat (330) is arranged on the other side of the baking device (100) and is located below the clamping hole (102); The clamping drive member (310) is disposed above the baking device (100), and the movable end of the clamping drive member (310) is fixedly connected to the upper clamping member (320), so that the upper clamping member (320) can move in a direction approaching the lower clamping seat (330) to make the end of the polyurethane tube (700) that extends beyond the loading rod (210) abut against the lower clamping seat (330).
5. The performance testing equipment for polyurethane materials according to claim 1, characterized in that: It also includes a sealing device (500), and a cavity wall on one side of the baking cavity (101) is provided with an entrance (103) corresponding to the sample device (400); The closing device (500) comprises a closing drive member (510) installed above the baking device (100), a closing plate (520) being installed at a movable end of the closing drive member (510), and the movable end of the closing drive member (510) can move in a direction approaching the entrance opening (103), so that the closing plate (520) closes the entrance opening (103).
6. The performance testing device for polyurethane material according to claim 5, characterized in that: It also comprises a first moving device (600), the moving end of the first moving device (600) being mounted with the baking device (100), and the first moving device (600) being capable of moving in a direction approaching or moving away from the loading device (200); Wherein, the maximum movable distance between the baking device (100) and the loading device (200) is greater than the length of the polyurethane pipe (700).
7. The performance testing device for polyurethane materials according to claim 6, characterized in that: A heating unit (110) and a quartz glass plate (120) are arranged in the baking cavity (101); the heating unit (110) is arranged below the quartz glass plate (120); and the quartz glass plate (120) is arranged below the entrance (103).
8. A method for detecting the performance of a polyurethane material, characterized in that: The performance testing device for the polyurethane material as described in any one of claims 1 to 7 comprises: The loading rod with the polyurethane tube is put into the baking chamber, and the polyurethane tube is subjected to a thermal test; Fix the end of the polyurethane tube and move the loading rod out of the baking chamber to form a suspended polyurethane tube; During the process of the loading rod moving out of the baking chamber, the suspended polyurethane pipe is pressurized from multiple directions; Determine whether the removal acceleration of the loading rod exceeds the preset qualified value. If so, mark the polyurethane pipe as an NG sample.