Intelligent monitoring control method for wall thickness of pipe blank of plastic pipe fitting
By intelligently monitoring and adjusting the process parameters in the production process of plastic pipe fittings, the problem of uneven wall thickness of the tube blanks in the existing technology is solved, the mechanical strength and pressure resistance of the pipe fittings are improved, and the frequency of maintenance and replacement is reduced.
Patent Information
- Application Number
- CN202411187179.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing wall thickness monitoring and control technology for plastic pipe fittings fails to effectively control process parameters, such as melt temperature, extrusion speed and cooling rate, resulting in uneven wall thickness of the tube and affecting the mechanical strength and pressure resistance of the product.
An intelligent monitoring and control method is adopted to obtain the actual measured values of process parameters in the heating and melting, extrusion and traction and cooling and shaping stages in real time, and the relevant process parameters are judged and adjusted to ensure the uniformity of the wall thickness of the tube blank. Specific steps include monitoring and adjusting screw speed, thrust, melt temperature, extrusion speed, traction force, traction speed, cooling medium temperature and cooling rate.
It achieves precise monitoring and control of the wall thickness of plastic pipe embryos, avoids uneven wall thickness due to poor process parameters, improves the mechanical strength and pressure resistance of pipe fittings, reduces the frequency of maintenance and replacement, and reduces long-term costs. cost.
Smart Images

Figure CN118721673A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of plastic pipe blank wall thickness monitoring, and particularly relates to an intelligent monitoring and control method for plastic pipe blank wall thickness. Background Art
[0002] Plastic pipe fittings play a vital role in many industries, such as construction, agriculture, chemicals and manufacturing. Monitoring and controlling the wall thickness of plastic pipe fittings is a key step to ensure product quality and performance. Uniform wall thickness can ensure that plastic pipe fittings have good mechanical strength and pressure resistance, avoid leakage or rupture caused by uneven wall thickness, enhance the durability of pipe fittings, reduce the frequency of maintenance and replacement, and reduce long-term costs. Therefore, monitoring and controlling the wall thickness of plastic pipe fittings is of great significance.
[0003] However, the existing monitoring and control technology for the wall thickness of plastic pipe blanks still has some limitations and shortcomings in practical applications.
[0004] For example, the existing Chinese patent with publication number CN103434109A discloses a new Jetta PPS intake pipe extrusion production process, which heats and dehumidifies the PPS material at 100-110℃, adds it to the extruder drying box, and extrudes it into a pipe blank. The wall of the pipe blank is controlled between 0.8-1.0mm, and the outer diameter of the blank pipe is 7.9-8.1mm; the pipe blank is placed in a sizing water tank, and sizing is performed three times under a negative pressure of 0.01-0.03MPa: finally, the pipe product is taken out from the sizing water tank. This invention uses the extrusion method to perform high-temperature multiple vacuum sizing, and produces the PPS intake pipe through the extrusion process, which solves the technical difficulties of producing the PPS intake pipe by the extrusion method.
[0005] The above patent can realize the extrusion molding and tube embryo wall thickness control of plastic pipes of various sizes above 500mm by means of high-temperature multiple vacuum sizing by extrusion method, but it does not involve the regulation of process parameters in the extrusion molding process of plastic pipes, especially process parameters related to tube embryo wall thickness, such as melt temperature, extrusion speed, pulling speed, cooling speed, etc. These process parameters are closely related to the tube embryo wall thickness of plastic pipes. Summary of the invention
[0006] In view of the above problems, the present invention proposes an intelligent monitoring and control method for the wall thickness of a plastic pipe blank. The specific technical scheme is as follows: An intelligent monitoring and control method for the wall thickness of a plastic pipe blank, comprising the following steps: Step 1, monitoring of process parameters affecting the wall thickness of the blank during heating and melting: obtaining the measured values of the process parameters affecting the wall thickness of the plastic pipe blank during the heating and melting stage in the production process of the plastic pipe fittings, and recording them as the measured values of the specified process parameters during the heating and melting stage, wherein the specified process parameters during the heating and melting stage include screw speed, screw thrust, and melt temperature.
[0007] Step 2: Adjustment of process parameters affecting tube embryo wall thickness during heating and melting: According to the measured values of the process parameters specified in the heating and melting stage, determine whether the process parameters specified in the heating and melting stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the heating and melting stage, and provide feedback.
[0008] Step 3. Monitoring of process parameters affecting tube blank wall thickness during extrusion and traction: Obtain the measured values of process parameters affecting tube blank wall thickness during the extrusion and traction stage in the production process of plastic pipe fittings, and record them as the measured values of specified process parameters during the extrusion and traction stage, wherein the specified process parameters during the extrusion and traction stage include extrusion speed, traction force, and traction speed.
[0009] Step 4: Adjustment of process parameters affecting tube embryo wall thickness due to extrusion traction: According to the measured values of the process parameters specified in the extrusion traction stage, determine whether the process parameters specified in the extrusion traction stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the extrusion traction stage, and provide feedback.
[0010] Step 5. Monitoring of process parameters affecting tube blank wall thickness during cooling and forming: Obtain the measured values of process parameters affecting tube blank wall thickness during the cooling and forming stage in the production process of plastic pipe fittings, and record them as the measured values of specified process parameters during the cooling and forming stage, wherein the specified process parameters during the cooling and forming stage include cooling medium temperature, cooling medium flow rate, and cooling speed.
[0011] Step 6. Adjustment of process parameters affecting tube embryo wall thickness during cooling and shaping: According to the measured values of the process parameters specified in the cooling and shaping stage, determine whether the process parameters specified in the cooling and shaping stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the cooling and shaping stage, and provide feedback.
[0012] Compared with the prior art, the method for intelligent monitoring and control of the wall thickness of plastic pipe blanks described in the present invention has the following beneficial effects: 1. The present invention obtains the measured values of screw speed, screw thrust and melt temperature in the heating and melting stage during the production process of plastic pipe fittings, determines whether the process parameters in the heating and melting stage need to be adjusted and obtains the adjustment information, so as to avoid the poor process parameters in the heating and melting stage affecting the wall thickness of the blanks of the finished plastic pipe fittings.
[0013] 2. The present invention obtains the measured values of extrusion speed, traction force and traction speed in the extrusion traction stage during the production process of plastic pipe fittings, determines whether the process parameters in the extrusion traction stage need to be adjusted and obtains the adjustment information, so as to avoid the influence of poor process parameters in the extrusion traction stage on the wall thickness of the tube blank of the finished plastic pipe fittings.
[0014] 3. The present invention obtains the measured values of the cooling medium temperature, cooling medium flow rate and cooling speed in the cooling and molding stage during the production process of plastic pipe fittings, determines whether the process parameters in the cooling and molding stage need to be adjusted and obtains the adjustment information, so as to avoid the poor process parameters in the cooling and molding stage affecting the wall thickness of the tube blank of the finished plastic pipe fittings. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0016] Figure 1 It is a schematic diagram of the method flow of the present invention.
[0017] Figure 2 The present invention is a schematic diagram of monitoring and adjusting process parameters that affect the wall thickness of the tube blank in the production of plastic pipe fittings.
[0018] Figure 3 It is a composition diagram of the present invention. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0020] See also Figure 1-Figure 3 As shown, the present invention provides an intelligent monitoring and control method for the wall thickness of a plastic pipe blank, comprising the following steps: Step 1, monitoring the process parameters affecting the wall thickness of the blank during heating and melting: obtaining the measured values of the process parameters affecting the wall thickness of the plastic pipe blank during the heating and melting stage in the production process of the plastic pipe, and recording them as the measured values of the specified process parameters during the heating and melting stage, wherein the specified process parameters during the heating and melting stage include screw speed, screw thrust, and melt temperature.
[0021] As a preferred solution, the specific analysis process of step 1 is: obtaining the measured values of the screw speed and screw thrust of the extruder during the heating and melting stage of the plastic pipe production process through the sensor, recording them as the measured value of the screw speed in the heating and melting stage and the measured value of the screw thrust in the heating and melting stage, and expressing them as .
[0022] The melt temperature during the heating and melting stage is obtained by an infrared pyrometer and recorded as .
[0023] In another specific embodiment, the melt temperature of the plastic pipe during the heating and melting stage of the production process is obtained by a thermocouple.
[0024] It should be noted that the screw speed and screw thrust of the extruder during the production of plastic pipe fittings affect the conveying rate and plasticizing effect of the plastic pipe fittings raw materials, and thus affect the wall thickness of the plastic pipe fittings. Too high or too low screw speed and screw thrust will lead to changes in the wall thickness of the plastic pipe fittings raw materials.
[0025] It should be noted that the melt temperature in the production process of plastic pipe fittings has a direct impact on the fluidity and viscosity of the melt. Too high a temperature may cause the plastic pipe raw materials to decompose, and too low a temperature will increase the melt extrusion pressure, thereby affecting the consistency of the wall thickness of the plastic pipe blank.
[0026] It should be noted that the specific steps for producing plastic pipe fittings by extrusion are as follows: (1) Raw material preparation: Select suitable plastic resins, such as polyvinyl chloride, polyethylene, polypropylene, etc.; Add stabilizers, lubricants, colorants and other additives as needed.
[0027] (2) Mixing and drying: Mix the raw materials and additives in a high-speed mixer to ensure uniform dispersion; dry the mixed raw materials to remove any moisture that may be present and avoid the generation of bubbles during the extrusion process.
[0028] (3) Extrusion molding: The dried raw materials are fed into the hopper of the extruder, and the raw materials are pushed forward by the rotation of the screw; the raw materials are heated to a molten state in the heating zone, and become a melt with good plasticity; the melt is extruded through a die to form a continuous tubular structure.
[0029] (4) Cooling and shaping: The extruded hot pipe immediately enters the cooling water tank or air cooling device to quickly cool and solidify the pipe to maintain its shape.
[0030] Step 2: Adjustment of process parameters affecting tube embryo wall thickness during heating and melting: According to the measured values of the process parameters specified in the heating and melting stage, determine whether the process parameters specified in the heating and melting stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the heating and melting stage, and provide feedback.
[0031] As a preferred solution, the specific analysis process of step 2 includes: extracting the reference values of the process parameters of the heating and melting stage of the plastic pipe stored in the database, screening and obtaining the reference value of the screw speed in the heating and melting stage, the reference value of the screw thrust in the heating and melting stage, and the reference value of the melt temperature in the heating and melting stage, and expressing them as .
[0032] It should be noted that the reference values of the process parameters of the heating and melting stage of plastic pipe fittings stored in the database are obtained based on the historical production experience of plastic pipe fittings and repeated processing tests.
[0033] By analyzing the formula Obtain the compliance coefficient of the specified process parameters in the heating and melting stage ,in It indicates the correction factor of the compliance coefficient of the specified process parameters in the preset heating and melting stage. They respectively represent the preset screw speed deviation threshold value in the heating and melting stage, the preset screw thrust deviation threshold value in the heating and melting stage, and the preset melt temperature deviation threshold value in the heating and melting stage, They respectively represent the weight of the screw speed in the preset heating and melting stage, the weight of the screw thrust in the preset heating and melting stage, and the weight of the melt temperature in the preset heating and melting stage, .
[0034] It should be noted that the correction factor of the compliance coefficient of the specified process parameters in the heating and melting stage plays the role of expanding, reducing or rounding the compliance coefficient of the specified process parameters in the heating and melting stage, thereby facilitating calculation and analysis.
[0035] In a specific embodiment, the deviation threshold of the screw speed in the heating and melting stage is 100 rpm, the deviation threshold of the screw thrust is 50 kN, and the deviation threshold of the melt temperature is 10°C.
[0036] In another specific embodiment, the deviation ranges of the screw speed, screw thrust, and melt temperature in the heating and melting stage are ±5%, ±10%, and ±5°C, respectively.
[0037] It should be noted that the weight of the screw speed in the heating and melting stage, the weight of the screw thrust in the heating and melting stage, and the weight of the melt temperature in the heating and melting stage are set according to the influence of the screw speed, screw thrust, and melt temperature in the heating and melting stage on the wall thickness of the plastic pipe blank. In a specific embodiment, the weight of the screw speed in the heating and melting stage, the weight of the screw thrust in the heating and melting stage, and the weight of the melt temperature in the heating and melting stage are 0.25, 0.25, and 0.5, respectively.
[0038] As a preferred solution, the specific analysis process of step two also includes: A1: comparing the compliance coefficient of the process parameters specified in the heating and melting stage with the preset threshold value of the compliance coefficient of the process parameters specified in the heating and melting stage; if the compliance coefficient of the process parameters specified in the heating and melting stage is less than the preset threshold value of the compliance coefficient of the process parameters specified in the heating and melting stage, the process parameters specified in the heating and melting stage need to be adjusted.
[0039] A2: Obtain the difference between the measured value of the screw speed in the heating and melting stage and its reference value, and record it as the deviation of the screw speed in the heating and melting stage.
[0040] The deviation of the screw speed in the heating and melting stage is compared with the preset deviation threshold of the screw speed in the heating and melting stage. If the deviation of the screw speed in the heating and melting stage is greater than the preset deviation threshold of the screw speed in the heating and melting stage, the screw speed in the heating and melting stage needs to be adjusted.
[0041] According to the measured value and reference value of the screw speed in the heating and melting stage, the adjustment direction and adjustment amount of the screw speed in the heating and melting stage are analyzed to obtain the adjustment information of the screw speed in the heating and melting stage.
[0042] It should be noted that the specific method for analyzing the adjustment direction and amount of the screw speed in the heating and melting stage is as follows: if the measured value of the screw speed in the heating and melting stage is greater than its reference value, the adjustment direction of the screw speed in the heating and melting stage is to decrease; if the measured value of the screw speed in the heating and melting stage is less than its reference value, the adjustment direction of the screw speed in the heating and melting stage is to increase.
[0043] The difference between the measured value of the screw speed in the heating and melting stage and its reference value is used as the adjustment amount of the screw speed in the heating and melting stage.
[0044] A3: Similarly, according to the analysis method of A2, determine whether the screw thrust and melt temperature in the heating and melting stage need to be adjusted, obtain the adjustment information, and provide feedback.
[0045] In a specific embodiment, the adjustment information of the specified process parameters in the heating and melting stage is fed back to the production and processing supervision department of the plastic pipe fittings.
[0046] In this embodiment, the present invention obtains the measured values of screw speed, screw thrust, and melt temperature in the heating and melting stage during the production process of plastic pipe fittings, determines whether the process parameters in the heating and melting stage need to be adjusted and obtains the adjustment information, so as to avoid the poor process parameters in the heating and melting stage affecting the wall thickness of the tube blank of the finished plastic pipe fittings.
[0047] Step 3. Monitoring of process parameters affecting tube blank wall thickness during extrusion and traction: Obtain the measured values of process parameters affecting tube blank wall thickness during the extrusion and traction stage in the production process of plastic pipe fittings, and record them as the measured values of specified process parameters during the extrusion and traction stage, wherein the specified process parameters during the extrusion and traction stage include extrusion speed, traction force, and traction speed.
[0048] As a preferred solution, the specific analysis process of step three is: obtaining the measured values of the extrusion speed, traction force, and traction speed in the extrusion traction stage during the production process of the plastic pipe fittings through sensors, recording them as the measured value of the extrusion speed in the extrusion traction stage, the measured value of the traction force in the extrusion traction stage, and the measured value of the traction speed in the extrusion traction stage, and expressing them as .
[0049] It should be noted that the extrusion speed in the production process of plastic pipe fittings refers to the speed at which the plastic is extruded from the extruder head. A higher extrusion speed may cause the wall thickness of the plastic pipe to become thinner because the plastic does not have enough time to form the ideal thickness in the mold. On the contrary, a lower extrusion speed may cause the wall thickness of the plastic pipe to increase, and it will also increase the cooling time and energy consumption.
[0050] It should be noted that a higher traction force during the production of plastic pipe fittings will cause the wall of the tube embryo of the plastic pipe fittings to become thinner, while a lower traction force may cause the wall of the tube embryo of the plastic pipe fittings to become thicker.
[0051] It should be noted that the pulling speed during the extrusion pulling stage of the plastic pipe production process must match the extrusion speed to ensure that the pipe is not over-stretched or compressed during the extrusion process, thereby maintaining the correct wall thickness.
[0052] Step 4: Adjustment of process parameters affecting tube embryo wall thickness due to extrusion traction: According to the measured values of the process parameters specified in the extrusion traction stage, determine whether the process parameters specified in the extrusion traction stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the extrusion traction stage, and provide feedback.
[0053] As a preferred solution, the specific analysis process of step 4 includes: extracting the reference values of the process parameters of the plastic pipe extrusion traction stage stored in the database, screening to obtain the reference values of the extrusion speed in the extrusion traction stage and the reference values of the traction force in the extrusion traction stage, and expressing them as .
[0054] It should be noted that the reference values of the process parameters of the extrusion and pulling stage of plastic pipe fittings stored in the database are obtained based on the historical production experience of plastic pipe fittings and repeated processing tests.
[0055] Set the reference ratio of the extrusion speed and the traction speed in the extrusion traction stage of the plastic pipe fitting, and obtain the reference value of the traction speed in the extrusion traction stage according to the reference value of the extrusion speed in the extrusion traction stage, which is recorded as .
[0056] By analyzing the formula Obtain the compliance coefficient of the specified process parameters in the extrusion traction stage ,in It represents the correction factor of the compliance coefficient of the specified process parameters in the preset extrusion pulling stage. Indicates the influence factor corresponding to the unit difference between the measured value and the reference value of the extrusion speed in the preset extrusion pulling stage, Indicates the influence factor corresponding to the unit difference between the measured value and the reference value of the pulling speed in the preset extrusion pulling stage, It represents the influence factor corresponding to the unit difference between the measured value and the reference value of the traction force in the preset extrusion traction stage.
[0057] It should be noted that the correction factor of the compliance coefficient of the specified process parameters in the extrusion traction stage plays the role of expanding, reducing or rounding the compliance coefficient of the specified process parameters in the extrusion traction stage, thereby facilitating calculation and analysis.
[0058] As a preferred solution, the specific analysis process of step four also includes: B1: comparing the compliance coefficient of the specified process parameters in the extrusion traction stage with the preset threshold value of the compliance coefficient of the specified process parameters in the extrusion traction stage; if the compliance coefficient of the specified process parameters in the extrusion traction stage is less than the preset threshold value of the compliance coefficient of the specified process parameters in the extrusion traction stage, the specified process parameters in the extrusion traction stage need to be adjusted.
[0059] B2: Obtain the difference between the actual value of the extrusion speed in the extrusion traction stage and its reference value, and record it as the deviation of the extrusion speed in the extrusion traction stage.
[0060] The deviation of the extrusion speed in the extrusion traction stage is compared with a preset deviation threshold of the extrusion speed in the extrusion traction stage. If the deviation of the extrusion speed in the extrusion traction stage is greater than the preset deviation threshold of the extrusion speed in the extrusion traction stage, the extrusion speed in the extrusion traction stage needs to be adjusted.
[0061] According to the measured value and reference value of the extrusion speed in the extrusion traction stage, the adjustment direction and adjustment amount of the extrusion speed in the extrusion traction stage are analyzed to obtain the adjustment information of the extrusion speed in the extrusion traction stage.
[0062] It should be noted that the specific method for analyzing the adjustment direction and adjustment amount of the extrusion speed in the extrusion traction stage is as follows: if the measured value of the extrusion speed in the extrusion traction stage is greater than its reference value, then the adjustment direction of the extrusion speed in the extrusion traction stage is to decrease; if the measured value of the extrusion speed in the extrusion traction stage is less than its reference value, then the adjustment direction of the extrusion speed in the extrusion traction stage is to increase.
[0063] The difference between the measured value of the extrusion speed in the extrusion traction stage and its reference value is used as the adjustment amount of the extrusion speed in the extrusion traction stage.
[0064] B3: Similarly, according to the analysis method of B2, determine whether the traction force and traction speed in the extrusion traction stage need to be adjusted, obtain the adjustment information, and provide feedback.
[0065] In this embodiment, the present invention obtains the measured values of extrusion speed, traction force, and traction speed in the extrusion traction stage during the production process of plastic pipe fittings, determines whether the process parameters in the extrusion traction stage need to be adjusted and obtains the adjustment information, so as to avoid the poor process parameters in the extrusion traction stage affecting the wall thickness of the tube blank of the finished plastic pipe fittings.
[0066] Step 5. Monitoring of process parameters affecting tube blank wall thickness during cooling and forming: Obtain the measured values of process parameters affecting tube blank wall thickness during the cooling and forming stage in the production process of plastic pipe fittings, and record them as the measured values of specified process parameters during the cooling and forming stage, wherein the specified process parameters during the cooling and forming stage include cooling medium temperature, cooling medium flow rate, and cooling speed.
[0067] It should be noted that the actual measured values of the cooling medium temperature, cooling medium flow rate and cooling speed during the cooling and shaping stage in the production process of plastic pipe fittings are obtained through sensors.
[0068] It should be noted that the cooling medium includes but is not limited to: cooling water or air.
[0069] It should be noted that the cooling rate in the cooling and shaping stage refers to the speed at which the plastic pipe blank is cooled to a solidified state after being extruded from the mold. In a specific embodiment, the cooling rate in the cooling and shaping stage is expressed as the temperature drop of the plastic pipe blank per unit time.
[0070] It should be noted that the temperature and flow rate of the cooling medium during the cooling and shaping stage of the plastic pipe production process will affect the uniformity of the wall thickness of the plastic pipe blank and the dimensional stability of the pipe.
[0071] It should be noted that the cooling speed during the cooling and shaping stage of the plastic pipe production process will affect the crystallinity and shrinkage of the plastic pipe blank, thereby affecting the wall thickness of the plastic pipe blank. Cooling too quickly may cause a large temperature difference between the inside and outside of the plastic pipe wall, resulting in uneven wall thickness, while cooling too slowly will increase the production cycle.
[0072] Step 6. Adjustment of process parameters affecting tube embryo wall thickness during cooling and shaping: According to the measured values of the process parameters specified in the cooling and shaping stage, determine whether the process parameters specified in the cooling and shaping stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the cooling and shaping stage, and provide feedback.
[0073] As a preferred solution, the specific analysis process of step six includes: extracting reference values of process parameters of the plastic pipe cooling and shaping stage stored in the database, and screening to obtain reference values of cooling medium temperature, cooling medium flow rate, and cooling speed in the cooling and shaping stage.
[0074] It should be noted that the reference values of the process parameters of the cooling and shaping stage of plastic pipe fittings stored in the database are obtained based on the historical production experience of plastic pipe fittings and repeated processing tests.
[0075] The measured values of the cooling medium temperature and the cooling medium flow rate in the cooling and shaping stage are compared with their corresponding reference values to obtain the difference between the cooling medium temperature and the cooling medium flow rate in the cooling and shaping stage.
[0076] It should be noted that the difference between the cooling medium temperature and the cooling medium flow rate in the cooling and shaping stage represents the absolute value of the difference between the actual measured values of the cooling medium temperature and the cooling medium flow rate and their corresponding reference values.
[0077] Substitute the difference between the cooling medium temperature and the cooling medium flow rate in the cooling finalization stage into the relationship function between the preset cooling medium temperature and flow rate difference and the cooling medium compliance coefficient to obtain the cooling medium compliance coefficient in the cooling finalization stage, which is recorded as .
[0078] It should be noted that the smaller the difference between the temperature and flow rate of the cooling medium, the greater the compliance coefficient of the cooling medium.
[0079] The measured value of the cooling rate in the cooling and shaping stage and the reference value of the cooling rate in the cooling and shaping stage are respectively recorded as and .
[0080] As a preferred solution, the specific analysis process of step 6 also includes: by analyzing the formula Get the compliance coefficient of the specified process parameters in the cooling and shaping stage ,in It represents the correction factor of the compliance coefficient of the specified process parameters in the preset cooling and shaping stage. represents a natural constant, Indicates the threshold value of the preset cooling medium compliance coefficient. Indicates the deviation threshold of the preset cooling rate.
[0081] The compliance coefficient of the specified process parameters in the cooling and finalizing stage is compared with the preset threshold of the compliance coefficient of the specified process parameters in the cooling and finalizing stage. If the compliance coefficient of the specified process parameters in the cooling and finalizing stage is less than the preset threshold of the compliance coefficient of the specified process parameters in the cooling and finalizing stage, the specified process parameters in the cooling and finalizing stage need to be adjusted.
[0082] It should be noted that the correction factor of the compliance coefficient of the specified process parameters in the cooling and finalizing stage plays the role of expanding, reducing or rounding the compliance coefficient of the specified process parameters in the cooling and finalizing stage, thereby facilitating calculation and analysis.
[0083] In a specific embodiment, the threshold value of the cooling medium compliance coefficient is 0.8.
[0084] In a specific embodiment, the deviation threshold of the cooling rate is 0.5°C / min.
[0085] As a preferred solution, the specific analysis process of step six also includes: S1: comparing the cooling medium compliance coefficient of the cooling finalization stage with the preset cooling medium compliance coefficient threshold. If the cooling medium compliance coefficient of the cooling finalization stage is less than the preset cooling medium compliance coefficient threshold, the cooling medium of the cooling finalization stage needs to be adjusted.
[0086] According to the measured values of the temperature and flow rate of the cooling medium in the cooling and finalizing stage and their corresponding reference values, it is determined whether the temperature and flow rate of the cooling medium in the cooling and finalizing stage need to be adjusted. If adjustment is required, the adjustment information of the temperature and flow rate of the cooling medium in the cooling and finalizing stage is analyzed and feedback is provided.
[0087] S2: judging whether the cooling speed in the cooling and shaping stage needs to be adjusted according to the measured value and reference value of the cooling speed in the cooling and shaping stage; if adjustment is required, analyzing the adjustment information of the cooling speed in the cooling and shaping stage and providing feedback.
[0088] It should be noted that the method for determining whether the cooling medium temperature, cooling medium flow rate, and cooling speed need to be adjusted during the cooling and shaping stage and analyzing the adjustment information is based on the same principle as the method for determining whether the screw speed needs to be adjusted during the heating and melting stage and analyzing the adjustment information.
[0089] In this embodiment, the present invention obtains the measured values of the cooling medium temperature, cooling medium flow rate, and cooling speed in the cooling and molding stage during the production process of plastic pipe fittings, determines whether the process parameters in the cooling and molding stage need to be adjusted and obtains the adjustment information, so as to avoid the poor process parameters in the cooling and molding stage affecting the wall thickness of the tube blank of the finished plastic pipe fitting.
[0090] The above contents are merely examples and explanations of the concept of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the concept of the invention or exceed the scope defined by the present invention, they shall all fall within the protection scope of the present invention.
Claims
1. A method for intelligent monitoring and control of the wall thickness of a plastic pipe blank, characterized in that: The steps include: Step 1: Monitoring the process parameters affecting the wall thickness of the tube blank during heating and melting: obtaining the measured values of the process parameters affecting the wall thickness of the tube blank during the heating and melting stage in the production process of plastic pipe fittings, and recording them as the measured values of the specified process parameters during the heating and melting stage, wherein the specified process parameters during the heating and melting stage include screw speed, screw thrust, and melt temperature; Step 2: Adjustment of process parameters affecting tube embryo wall thickness during heating and melting: According to the measured values of the specified process parameters during the heating and melting stage, determine whether the specified process parameters during the heating and melting stage need to be adjusted, further obtain adjustment information of the specified process parameters during the heating and melting stage, and provide feedback; Step 3: Monitoring of process parameters affecting tube wall thickness during extrusion traction: obtaining the measured values of process parameters affecting tube wall thickness during the extrusion traction stage in the production process of plastic pipe fittings, and recording them as the measured values of the specified process parameters during the extrusion traction stage, wherein the specified process parameters during the extrusion traction stage include extrusion speed, traction force, and traction speed; Step 4: Adjustment of process parameters affecting tube embryo wall thickness during extrusion traction: According to the measured values of the specified process parameters during the extrusion traction stage, determine whether the specified process parameters during the extrusion traction stage need to be adjusted, further obtain the adjustment information of the specified process parameters during the extrusion traction stage, and provide feedback; Step 5. Monitoring of process parameters affecting the wall thickness of the tube blank during cooling and finalizing: obtaining the measured values of process parameters affecting the wall thickness of the tube blank during the cooling and finalizing stage in the production process of plastic pipe fittings, and recording them as the measured values of the specified process parameters during the cooling and finalizing stage, wherein the specified process parameters during the cooling and finalizing stage include the cooling medium temperature, the cooling medium flow rate, and the cooling speed; Step 6. Adjustment of process parameters affecting tube embryo wall thickness during cooling and shaping: According to the measured values of the process parameters specified in the cooling and shaping stage, determine whether the process parameters specified in the cooling and shaping stage need to be adjusted, further obtain the adjustment information of the process parameters specified in the cooling and shaping stage, and provide feedback.
2. According to claim 1, a method for intelligent monitoring and controlling the wall thickness of a plastic pipe blank is characterized by: The specific analysis process of step 1 is as follows: The measured values of the screw speed and screw thrust of the extruder during the heating and melting stage of the plastic pipe production process are obtained by sensors, which are recorded as the measured value of the screw speed in the heating and melting stage and the measured value of the screw thrust in the heating and melting stage, and are expressed as ; The melt temperature during the heating and melting stage is obtained by an infrared pyrometer and recorded as .
3. The method for intelligent monitoring and controlling the wall thickness of a plastic pipe blank according to claim 2 is characterized in that: The specific analysis process of step 2 includes: The reference values of the process parameters of the heating and melting stage of plastic pipe fittings stored in the database are extracted, and the reference values of the screw speed, the screw thrust and the melt temperature in the heating and melting stage are obtained by screening and expressed as ; By analyzing the formula Obtain the compliance coefficient of the specified process parameters in the heating and melting stage ,in It indicates the correction factor of the compliance coefficient of the specified process parameters in the preset heating and melting stage. They respectively represent the preset screw speed deviation threshold value in the heating and melting stage, the preset screw thrust deviation threshold value in the heating and melting stage, and the preset melt temperature deviation threshold value in the heating and melting stage, They respectively represent the weight of the screw speed in the preset heating and melting stage, the weight of the screw thrust in the preset heating and melting stage, and the weight of the melt temperature in the preset heating and melting stage, .
4. The method for intelligent monitoring and controlling the wall thickness of a plastic pipe blank according to claim 3 is characterized in that: The specific analysis process of step 2 also includes: A1: Compare the compliance coefficient of the specified process parameters in the heating and melting stage with the preset threshold of the compliance coefficient of the specified process parameters in the heating and melting stage. If the compliance coefficient of the specified process parameters in the heating and melting stage is less than the preset threshold of the compliance coefficient of the specified process parameters in the heating and melting stage, the specified process parameters in the heating and melting stage need to be adjusted; A2: Obtain the difference between the measured value of the screw speed in the heating and melting stage and its reference value, and record it as the deviation of the screw speed in the heating and melting stage; The deviation of the screw speed in the heating and melting stage is compared with a preset deviation threshold of the screw speed in the heating and melting stage. If the deviation of the screw speed in the heating and melting stage is greater than the preset deviation threshold of the screw speed in the heating and melting stage, the screw speed in the heating and melting stage needs to be adjusted; According to the measured value and reference value of the screw speed in the heating and melting stage, the adjustment direction and adjustment amount of the screw speed in the heating and melting stage are analyzed to obtain the adjustment information of the screw speed in the heating and melting stage; A3: Similarly, according to the analysis method of A2, determine whether the screw thrust and melt temperature in the heating and melting stage need to be adjusted, obtain the adjustment information, and provide feedback.
5. The method for intelligent monitoring and controlling the wall thickness of a plastic pipe blank according to claim 1, characterized in that: The specific analysis process of step three is as follows: The measured values of extrusion speed, traction force and traction speed in the extrusion traction stage during the production process of plastic pipe fittings are obtained by sensors, which are recorded as the measured value of extrusion speed in the extrusion traction stage, the measured value of traction force in the extrusion traction stage, and the measured value of traction speed in the extrusion traction stage, and expressed as .
6. The method for intelligent monitoring and controlling the wall thickness of a plastic pipe blank according to claim 5, characterized in that: The specific analysis process of step 4 includes: The reference values of the process parameters of the plastic pipe extrusion traction stage stored in the database are extracted, and the reference values of the extrusion speed and the traction force in the extrusion traction stage are obtained by screening and expressed as ; Set the reference ratio of the extrusion speed and the traction speed in the extrusion traction stage of the plastic pipe fitting, and obtain the reference value of the traction speed in the extrusion traction stage according to the reference value of the extrusion speed in the extrusion traction stage, which is recorded as ; By analyzing the formula Obtain the compliance coefficient of the specified process parameters in the extrusion traction stage ,in It represents the correction factor of the compliance coefficient of the specified process parameters in the preset extrusion pulling stage. Indicates the influence factor corresponding to the unit difference between the measured value and the reference value of the extrusion speed in the preset extrusion pulling stage, Indicates the influence factor corresponding to the unit difference between the measured value and the reference value of the pulling speed in the preset extrusion pulling stage, It represents the influence factor corresponding to the unit difference between the measured value and the reference value of the traction force in the preset extrusion traction stage.
7. The method for intelligently monitoring and controlling the wall thickness of a plastic pipe blank according to claim 6, characterized in that: The specific analysis process of step 4 also includes: B1: Compare the compliance coefficient of the specified process parameters in the extrusion traction stage with the preset threshold of the compliance coefficient of the specified process parameters in the extrusion traction stage. If the compliance coefficient of the specified process parameters in the extrusion traction stage is less than the preset threshold of the compliance coefficient of the specified process parameters in the extrusion traction stage, the specified process parameters in the extrusion traction stage need to be adjusted; B2: Obtain the difference between the measured value of the extrusion speed in the extrusion traction stage and its reference value, and record it as the deviation of the extrusion speed in the extrusion traction stage; Comparing the deviation of the extrusion speed in the extrusion traction stage with a preset deviation threshold of the extrusion speed in the extrusion traction stage, if the deviation of the extrusion speed in the extrusion traction stage is greater than the preset deviation threshold of the extrusion speed in the extrusion traction stage, the extrusion speed in the extrusion traction stage needs to be adjusted; According to the measured value and reference value of the extrusion speed in the extrusion traction stage, the adjustment direction and adjustment amount of the extrusion speed in the extrusion traction stage are analyzed to obtain the adjustment information of the extrusion speed in the extrusion traction stage; B3: Similarly, according to the analysis method of B2, determine whether the traction force and traction speed in the extrusion traction stage need to be adjusted, obtain the adjustment information, and provide feedback.
8. The method for intelligently monitoring and controlling the wall thickness of a plastic pipe blank according to claim 4, characterized in that: The specific analysis process of step six includes: Extract reference values of process parameters of the cooling and shaping stage of plastic pipe fittings stored in the database, and screen and obtain reference values of cooling medium temperature, cooling medium flow rate, and cooling speed in the cooling and shaping stage; The measured values of the cooling medium temperature and the cooling medium flow rate in the cooling and shaping stage are compared with the corresponding reference values to obtain the difference of the cooling medium temperature and the cooling medium flow rate in the cooling and shaping stage; Substitute the difference between the cooling medium temperature and the cooling medium flow rate in the cooling finalization stage into the relationship function between the preset cooling medium temperature and flow rate difference and the cooling medium compliance coefficient to obtain the cooling medium compliance coefficient in the cooling finalization stage, which is recorded as ; The measured value of the cooling rate in the cooling and shaping stage and the reference value of the cooling rate in the cooling and shaping stage are respectively recorded as and .
9. The method for intelligently monitoring and controlling the wall thickness of a plastic pipe blank according to claim 8, characterized in that: The specific analysis process of step six also includes: By analyzing the formula Get the compliance coefficient of the specified process parameters in the cooling and shaping stage ,in It represents the correction factor of the compliance coefficient of the specified process parameters in the preset cooling and shaping stage. represents a natural constant, Indicates the threshold value of the preset cooling medium compliance coefficient. Indicates the deviation threshold of the preset cooling rate; The compliance coefficient of the specified process parameters in the cooling and finalizing stage is compared with the preset threshold of the compliance coefficient of the specified process parameters in the cooling and finalizing stage. If the compliance coefficient of the specified process parameters in the cooling and finalizing stage is less than the preset threshold of the compliance coefficient of the specified process parameters in the cooling and finalizing stage, the specified process parameters in the cooling and finalizing stage need to be adjusted.
10. The method for intelligently monitoring and controlling the wall thickness of a plastic pipe blank according to claim 9, characterized in that: The specific analysis process of step six also includes: S1: Compare the cooling medium compliance coefficient in the cooling finalization stage with the preset cooling medium compliance coefficient threshold. If the cooling medium compliance coefficient in the cooling finalization stage is less than the preset cooling medium compliance coefficient threshold, the cooling medium in the cooling finalization stage needs to be adjusted. According to the measured values of the temperature and flow rate of the cooling medium in the cooling and shaping stage and their corresponding reference values, it is judged whether the temperature and flow rate of the cooling medium in the cooling and shaping stage need to be adjusted. If adjustment is required, the adjustment information of the temperature and flow rate of the cooling medium in the cooling and shaping stage is analyzed and feedback is provided; S2: judging whether the cooling speed in the cooling and shaping stage needs to be adjusted according to the measured value and reference value of the cooling speed in the cooling and shaping stage; if adjustment is required, analyzing the adjustment information of the cooling speed in the cooling and shaping stage and providing feedback.
Citation Information
Cited By
Plastic sheet manufacturing system and manufacturing method thereof
CN119017611A
Barrier type multi-layer composite pipeline and preparation process thereof
CN119408207A
Operation monitoring method and system based on PE pipeline processing extruder
CN119610613A
An operation monitoring method and system based on a PE pipe processing extruder
CN119610613B
Shear force control method and system for plastic particle production equipment
CN121535867A