Method for producing porous carbon sheet, and porous carbon sheet
The porous carbon sheets are formed by stirring and calcining the copper methyl acetylene solution, which solves the problems of cumbersome and time-consuming steps in the existing technology, and achieves the manufacturing of porous carbon sheets with high conductivity, high air permeability and excellent water retention capacity adjustment.
Patent Information
- Application Number
- CN202410347739.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-28
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-01
AI Technical Summary
The existing porous carbon sheet manufacturing method has many steps and is time-consuming, and the high calcination temperature leads to high equipment and energy consumption.
A linear structure is formed by stirring a copper methyl acetylene solution. After sheet formation, drying and adding phenolic resin, it is calcined at low pressure in the range of 1000°C to 1200°C to grow graphene multi-layer cavity walls and remove copper to form a medium-sized graphene. Porous carbon sheets.
The manufacturing process is simplified, the calcination temperature and energy consumption are reduced, the conductivity and air permeability of the porous carbon sheets are improved, and the water retention capacity adjustment ability is optimized.
Smart Images

Figure CN118723967A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method for manufacturing a porous carbon sheet and a porous carbon sheet. Background Art
[0002] Japanese Laid-Open Patent Publication No. 2014-86305 discloses a method for manufacturing a porous carbon sheet. In the manufacturing method described in the publication, first, methylacetylene gas is sprayed into the ammonia water while stirring the ammonia water containing cuprous chloride, thereby obtaining a precipitate of linear crystals of methylacetylene copper. Next, the precipitate is filtered out with a filter under reduced pressure and heated to obtain a black flocculent solid. Next, an aqueous nitric acid solution is added to the solid to dissolve the copper. The solid is filtered out, washed and dried, and then vacuum heated in a quartz tube at 1100°C for 12 hours. As a result, an organic film is deposited on the inner wall of the end of the quartz tube and copper sublimates and deposits on the inner wall of the end of the quartz tube. Only the carbon component is removed from the sediment and the residual copper is dissolved again with hot nitric acid. It is dried, then placed in an alumina Tammann tube, and heated at 1400°C for 10 hours to obtain a porous carbon material with a graphene layer. Then, a solution obtained by dissolving a porous carbon material, potassium permanganate and sulfuric acid in ultrapure water was refluxed while ultrasonic vibration was applied to the solution. Thereafter, a solid obtained by filtering the solution was heat-treated at 250°C for 3 hours to obtain a porous carbon carrying manganese oxide and having a graphene layer. Then, the porous carbon and PTFE as a binder were dissolved in ethanol and kneaded to obtain a paste ink. The ink was rolled to obtain a flaky porous carbon.
[0003] The manufacturing method disclosed in the above publication requires a relatively large number of manufacturing steps for manufacturing a porous carbon sheet, and takes a relatively long manufacturing time. Summary of the invention
[0004] This Summary is provided to introduce a selection of concepts in a simplified form that are further described below in the Detailed Description. This Summary is not intended to identify key features or essential features of the claimed subject matter, nor is it intended to be used as an aid in determining the scope of the claimed subject matter.
[0005] In a general aspect, a method for manufacturing a porous carbon sheet is provided. The porous carbon sheet is composed of a multilayer cavity wall of graphene, has mesoporosity, and includes a structure in which hollow linear crystals are entangled with each other. The method includes a stirring step for stirring a solution containing copper methylacetylene as a precursor to form a linear structure of the precursor and to entangle the linear structure with each other in the solution, a sheet forming step for forming the precursor into a sheet-like precursor, and a calcining step for calcining the sheet-like precursor in the range of 1000° C. to 1200° C. to grow a multilayer cavity wall of graphene and thermally remove copper to form a porous carbon sheet.
[0006] In another general aspect, the porous carbon sheet is composed of multilayer cavity walls of graphene and includes a structure in which hollow linear crystals with mesoporosity are entangled with each other. The linear diameter of the crystals is in the range of 100nm to 500nm. The diameter of the pores formed by the entangled crystals is in the range of 10nm to 200nm.
[0007] Other features and aspects will be apparent from the following detailed description, drawings, and claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 is a SEM image of a porous carbon sheet according to one embodiment.
[0009] Figure 2 is another SEM image of the porous carbon sheet of this embodiment.
[0010] Figure 3 is an enlarged SEM image of a portion of the porous carbon sheet of this embodiment.
[0011] Figure 4 is an enlarged SEM image of another portion of the porous carbon sheet of this embodiment.
[0012] Figure 5 is a TEM image of the porous carbon sheet of this embodiment.
[0013] Figure 6 is a TEM image of the precursor of this embodiment during the drying step.
[0014] Figure 7 is a flowchart showing a process for manufacturing a porous carbon sheet according to this embodiment.
[0015] Figure 8 This is a SEM image of the porous carbon of the comparative example.
[0016] Fig. 9 This is an enlarged SEM image of the porous carbon of this comparative example.
[0017] Throughout the drawings and detailed description, like reference numerals refer to like elements. The drawings may not be drawn to scale, and the relative size, proportion, and depiction of elements in the drawings may be exaggerated for clarity, illustration, and convenience. DETAILED DESCRIPTION
[0018] This description provides a comprehensive understanding of the described methods, devices and / or systems. Variations and equivalents of the described methods, devices and / or systems will be apparent to those of ordinary skill in the art. The sequence of operations is exemplary and, except for operations that must occur in a particular order, may be readily apparent to those of ordinary skill in the art. Descriptions of functions and components that are well known to those of ordinary skill in the art may be omitted.
[0019] Exemplary embodiments may have different forms and are not limited to the described examples. However, the described examples are thorough and complete, and convey the full scope of the disclosure to those skilled in the art.
[0020] In the present specification, “at least one of A and B” should be understood to mean “only A, only B, or both A and B”.
[0021] Now refer to Figures 1 to 7 A method for manufacturing a porous carbon sheet and a porous carbon sheet according to one embodiment are described.
[0022] like Figures 1 to 4 As shown, the porous carbon sheet is composed of multi-layer cavity walls of graphene and includes a structure in which hollow linear crystals with mesoporosity are entangled with each other.
[0023] like Figure 5 As shown, the porous carbon sheet has a pore structure separated by multi-layer cavity walls of graphene.
[0024] The diameter of the crystals is in the range of 100nm to 500nm. The diameter of the holes formed by the intertwined crystals is in the range of 10nm to 200nm.
[0025] The porous carbon sheet of the present embodiment can be used as, for example, a gas diffusion layer forming a single cell of a polymer electrolyte fuel cell.
[0026] Next, we will refer to Figure 7 The manufacturing process of the porous carbon sheet of this embodiment is described.
[0027] like Figure 7 The method for manufacturing a porous carbon sheet includes a precursor synthesis step, a stirring step, a sheet forming step, a drying step, an adding step and a calcining step.
[0028] The precursor synthesis step is a step for synthesizing methylacetylene copper as a precursor by a known method.
[0029] The stirring step is a step for stirring a solution containing copper methylacetylene as a precursor to form a linear structure and to entangle the linear structures with each other in the solution. Water is used as a solvent. Adding a small amount of ethanol to the solvent makes the stretching of the precursor easy.
[0030] In the stirring step, the linear structure of the precursor is formed by stirring the solution containing methylacetylene copper. At this time, in the subsequent heating step, due to the difference in specific gravity between copper and carbon, copper becomes spherical or elliptical, and carbon becomes linear covering copper. In addition, the linear structures of the precursor are entangled with each other in the solution.
[0031] The sheet forming step is a step for forming the precursor into a sheet-shaped precursor.
[0032] In the sheet forming step, the linear structure of the precursor entangled with each other is formed into a sheet-like precursor. Examples of the method for forming the linear structure of the precursor into a sheet-like precursor include a method of filtering a solution containing the precursor with filter paper to form a sheet on the filter paper, a method of applying the solution to a planar jig, and a method of spraying the solution onto a planar jig.
[0033] The drying step is a step for heating the sheet-shaped precursor to a temperature in the range of 170° C. to 300° C. under vacuum to dry the precursor. Therefore, although phase separation of copper and carbon occurs, the shape of the precursor is easily maintained.
[0034] Figure 6 The separation of copper and methylacetylene polymers is shown during the drying step in which the precursor is heated to a temperature in the range of 60°C to 200°C. Specifically, Figure 6 It shows how the copper becomes spherical and the methyl groups are released out of the system as methane and ethylene gases.
[0035] The adding step is a step for adding a phenolic resin to the sheet-like precursor. The precursor is preferably dried after the phenolic resin is added.
[0036] The calcination step is a step for calcining the sheet-shaped precursor in the range of 1000° C. to 1200° C. to grow multilayer cavity walls of graphene and thermally remove copper to form a porous carbon sheet.
[0037] The calcining step is preferably carried out at a pressure below atmospheric pressure.
[0038] In the calcining step, copper is sublimated and removed by calcining the precursor in the range of 1000°C to 1200°C. The copper in contact with a portion of the carbon of the precursor melts at a temperature higher than or equal to 1000°C. At this time, an ideal two-dimensional surface of carbon is generated due to the surface tension generated in the carbon, so that the carbon grows into a multi-layer cavity wall of graphene. This forms a porous carbon sheet composed of a multi-layer cavity wall of graphene and including a structure in which hollow linear crystals with mesoporosity are entangled with each other.
[0039] The melting point of copper is 1085° C. However, in the case of particles having a size of 50 nm or less, liquefaction of copper proceeds below 1000° C. due to a decrease in the melting point.
[0040] Figure 8 and 9 The SEM image of the porous carbon of the comparative example is shown. The porous carbon of the comparative example was formed by dropping the precursor of the present embodiment into a furnace and performing vacuum calcination without forming the precursor into a sheet-like precursor.
[0041] This embodiment has the following advantages.
[0042] (1) The method for producing a porous carbon sheet includes a stirring step, a sheet forming step, and a calcining step.
[0043] In the case of this method, by calcining a flake precursor of methylacetylene copper, the precursor is carbonized while maintaining the linear structure of the precursor. This eliminates the necessity of the steps of forming a sheet by carbonizing the precursor and then pulverizing the precursor in the prior art.
[0044] Furthermore, in the case of the above method, since the calcination temperature is within the range of 1000° C. to 1200° C., the calcination temperature is lowered compared to the conventional manufacturing method of calcining methylacetylene silver at, for example, 2000° C. This allows the size of the calcination furnace and the energy required for calcination to be reduced.
[0045] Furthermore, copper is preferred over silver for growing thick multi-layered cavity walls of graphene to increase conductivity.
[0046] This makes it easy to manufacture porous carbon sheets.
[0047] (2) The method further comprises an adding step for adding a phenolic resin to the sheet-like precursor before the calcining step.
[0048] In the case of this configuration, since the rigidity of the precursor is increased by adding the phenolic resin, the shape of the sheet-shaped precursor is easily maintained, which increases the yield of the porous carbon sheet.
[0049] (3) Because the calcination step is carried out at a pressure lower than normal pressure, the growth of the graphene multilayer cavity wall and the thermal removal of copper can be carried out at a low calcination temperature. This reduces the size of the calcination furnace and the energy required for calcination.
[0050] (4) Since the porous carbon sheet is composed of multilayer cavity walls of graphene and includes a structure in which hollow linear crystals having mesoporosity are entangled with each other, the porous carbon sheet has high conductivity. In addition, according to the above-mentioned structure, the wire diameter of the crystal is in the range of 100nm to 500nm, and the diameter of the pores formed by the entangled crystals is in the range of 10nm to 200nm. Therefore, the porous carbon sheet has high air permeability. Since water can be stored in a large number of mesopores in the crystal and can be discharged therefrom, the porous carbon sheet is excellent in adjusting the water retention amount.
[0051] Therefore, the porous carbon sheet has high electrical conductivity and high air permeability, and is excellent in adjusting the water retention amount.
[0052] Deformation
[0053] The above-mentioned embodiment can be modified as follows: The above-mentioned embodiment and the following modifications can be combined as long as the combined modifications remain technically consistent with each other.
[0054] The calcination step can also be carried out at atmospheric pressure.
[0055] The step of adding the phenolic resin may be omitted.
[0056] Various changes in form and details may be made to the above examples without departing from the spirit and scope of the claims and their equivalents. These examples are for convenience of illustration only and not for the purpose of limitation. The description of the features in each example is considered to be applicable to similar features or aspects in other examples. If the sequence is performed in a different order, and / or if the components in the described system, architecture, device or circuit are combined in a different way, and / or replaced or supplemented by other components or their equivalents, suitable results can be obtained. The scope of the present disclosure is not limited by the specific embodiments, but by the claims and their equivalents. All changes within the scope of the claims and their equivalents are included in the present disclosure.
Claims
1. A method for manufacturing a porous carbon sheet, wherein the porous carbon sheet is composed of a multilayer cavity wall of graphene, has mesoporosity and includes a structure in which hollow linear crystals are entangled with each other, the method comprising: a stirring step for stirring a solution containing copper methylacetylene as a precursor to form a linear structure of the precursor and to entangle the linear structures with each other in the solution; A sheet forming step for forming the precursor into a sheet-shaped precursor; and A calcining step for calcining the sheet-shaped precursor in the range of 1000° C. to 1200° C. to grow multi-layer cavity walls of graphene and thermally remove copper to form the porous carbon sheet.
2. The method for producing a porous carbon sheet according to claim 1, further comprising an adding step for adding a phenolic resin to the sheet-like precursor before the calcining step.
3. The method for producing a porous carbon sheet according to claim 1 or 2, wherein the calcination step is performed at a pressure lower than normal pressure.
4. A porous carbon sheet, which is composed of multi-layer cavity walls of graphene and includes a structure in which hollow linear crystals with mesoporosity are entangled with each other, wherein The crystals have a linear diameter in the range of 100 nm to 500 nm, and The diameter of the pores formed by the mutually entangled crystals ranges from 10 nm to 200 nm.
Citation Information
Patent Citations
Porous electrode base material, method for manufacturing same and precursor sheet
CN104205448A
Catalytic site, positive electrode active material and lithium-sulfur battery comprising the same
KR1020180133063A
Carbon Nanostructure
US20120295108A1
Porous electrode base material, method for manufacturing same, and precursor sheet