Preparation method of glass cover, glass cover and electronic equipment

An integrated glass cover plate was prepared by tightly stacking and thermally stretching multiple glass rods, which solved the problem of flash light entering the camera and improved the photo quality and waterproof performance.

CN118724440BActive Publication Date: 2026-11-17GUANGDONG OPPO MOBILE TELECOMMUNICATIONS CORP LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310335548.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2026-11-17
Estimated Expiration
2043-03-30

AI Technical Summary

Technical Problem

In existing technologies, when the camera and flash are placed adjacent to each other, the glass cover cannot effectively prevent the flash light from entering the camera along the glass extension direction, affecting the photo quality, and the light-blocking ink reduces the waterproof performance.

Method used

Multiple glass rods with different radial dimensions are tightly stacked and thermally stretched to form a fourth rod with a preset shape. An integrated glass cover plate is then prepared by molding, including a light-transmitting part and a light-blocking part. The light-blocking part prevents light from passing through along the glass extension direction.

Benefits of technology

It effectively blocks light from entering the camera, improving photo quality while maintaining the waterproof and mechanical properties of the glass cover.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118724440B_ABST
    Figure CN118724440B_ABST
Patent Text Reader

Abstract

This application provides a method for manufacturing a glass cover, a glass cover, and an electronic device. The method for manufacturing the glass cover includes: providing a first rod; providing multiple second rods and multiple third rods, and stacking them tightly to obtain a first stack, wherein the third rods are located within the gaps formed by adjacent second rods, and the radial dimensions of the second rods are larger than the radial dimensions of the third rods; thermally stretching the first stack to obtain a fourth rod; tightly surrounding the fourth rods around the outer periphery of the first rods to form a second stack; molding the second stack to obtain a fifth rod; and cutting the fifth rod to obtain a glass cover. This application provides a method for manufacturing a glass cover that can produce an integrated glass cover. When used as a protective cover for a camera, this glass cover can prevent light emitted from a flash from entering the camera along the extension direction of the glass cover, thus avoiding affecting the camera's image capture performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of electronics, specifically to a method for preparing a glass cover, the glass cover, and an electronic device. Background Technology

[0002] Cameras typically include a flash to enhance exposure in low-light environments or adjust the color temperature of outdoor environments, thereby improving image or photo quality. However, in electronic devices such as mobile phones, the camera and flash are usually positioned next to each other, with glass covers protecting the light-emitting / light-receiving surfaces of both. Although light-blocking ink is applied to the areas of the glass cover outside the camera and flash, this ink only blocks light perpendicular to the glass cover; it cannot prevent the light emitted by the flash from passing through the glass cover (along its extension) and entering the camera's viewing window, thus affecting the camera's image quality. Summary of the Invention

[0003] To address the aforementioned issues, this application provides a method for preparing a glass cover plate, which can produce an integrated glass cover plate. When this glass cover plate is used as a protective cover for a camera, it can prevent light emitted from the flash lamp from entering the camera along the extension direction of the glass cover plate, thereby avoiding affecting the camera's image capture performance.

[0004] The first aspect of this application provides a method for preparing a glass cover plate, which includes:

[0005] Provide the first rod;

[0006] Multiple second rods and multiple third rods are provided and stacked tightly to obtain a first stack, wherein the third rod is located within the gap formed by adjacent second rods, and the radial dimension of the second rod is larger than the radial dimension of the third rod.

[0007] The first stack is thermally stretched to obtain the fourth rod.

[0008] The fourth rod is tightly surrounded on the outer periphery of the first rod to form a second stack.

[0009] The second stack is molded to obtain the fifth rod; and

[0010] The fifth rod is cut to obtain a glass cover plate.

[0011] A second aspect of this application provides a glass cover plate, the glass cover plate including a first light-transmitting part, a light-blocking part, and a second light-transmitting part connected sequentially; the light-blocking part is disposed around the outer periphery of the first light-transmitting part, and the second light-transmitting part is disposed around the outer periphery of the light-blocking part; the first light-transmitting part, the light-blocking part, and the second light-transmitting part are an integral structure; the light transmittance of the light-blocking part is less than the light transmittance of the first light-transmitting part and less than the light transmittance of the second light-transmitting part, the light-blocking part is used to prevent light entering the first light-transmitting part from passing through the light-blocking part and entering the second light-transmitting part; the glass cover plate is prepared by the preparation method described in the embodiments of this application, wherein the first light-transmitting part and the light-blocking part are formed by the first rod, and the second light-transmitting part is formed by the fourth rod.

[0012] A third aspect of this application provides an electronic device comprising:

[0013] The glass cover plate described in this application embodiment has a preset surface;

[0014] A flash lamp is disposed on the preset surface side of the glass cover plate, and the light-emitting surface of the flash lamp is projected onto the preset surface within the range of the first light-transmitting part.

[0015] A camera module, wherein the camera module and the flash are disposed on the same side of the glass cover and spaced apart from the glass cover, and the light-incident surface of the camera module, when projected onto the preset surface, falls within the range of the second light-transmitting portion; and

[0016] The processor is electrically connected to both the camera module and the flash, and is used to control the camera module to take pictures and to control the flash to work.

[0017] The fourth rod of this application is formed by thermal stretching of the first stack. By designing the stacking method of the first stack, the cross-section of the fourth rod can have a preset shape. In addition, the first stack uses a second rod with a larger radial dimension and a second rod with a smaller radial dimension to stack. The gap within the first stack can be minimized, thereby minimizing the number of bubbles formed in the resulting fourth rod, resulting in better appearance and mechanical properties. Then, the fourth rod is tightly stacked on the outer periphery of the first rod and molded to obtain the fifth rod. By controlling the light transmittance of the first and fourth rods, a glass cover plate with an integrated light-transmitting part and a light-blocking part can be produced. The light-blocking part can prevent light from passing through the light-blocking part along the extension direction of the glass cover plate (i.e., perpendicular to the thickness direction). Furthermore, by designing the cross-section of the fourth rod to have a preset shape, the fourth rod can be stacked more tightly when stacked on the outer periphery of the first rod, and the gap between the fourth rod and the first rod can be minimized. This minimizes the number of bubbles in the glass cover plate after molding and cutting, resulting in better appearance and mechanical properties. Attached Figure Description

[0018] To more clearly illustrate the technical solutions of the embodiments of this application, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0019] Figure 1 This is a cross-sectional structural diagram of the glass protective cover of the related technology.

[0020] Figure 2 This is a schematic diagram of the planar structure of a glass cover plate according to an embodiment of this application.

[0021] Figure 3 This application describes a glass cover plate along... Figure 2 A schematic diagram of the cross-sectional structure along the AA direction.

[0022] Figure 4 This is a schematic diagram of the planar structure of a glass cover plate according to another embodiment of this application.

[0023] Figure 5 This application describes a glass cover plate along... Figure 4 Schematic diagram of the cross-sectional structure in the middle BB direction.

[0024] Figure 6 This is a schematic diagram of the manufacturing process of a glass cover plate according to an embodiment of this application.

[0025] Figure 7This is a schematic diagram of the fabrication process of a glass cover plate according to an embodiment of this application.

[0026] Figure 8 This is a schematic diagram of the preparation method of the first rod body according to an embodiment of this application.

[0027] Figure 9 yes Figure 7 Enlarged view of I in the middle.

[0028] Figure 10 This is a schematic diagram of the structure of the fourth rod in one embodiment of this application.

[0029] Figure 11 This is a schematic diagram of the manufacturing process of a glass cover plate according to another embodiment of this application.

[0030] Figure 12 This is a plan view of an electronic device according to an embodiment of this application.

[0031] Figure 13 An electronic device according to an embodiment of this application Figure 12 A schematic diagram of a partial cross-sectional structure along the CC direction.

[0032] Figure 14 This is a circuit block diagram of an electronic device according to an embodiment of this application.

[0033] Figure 15 This is a partial exploded structural diagram of an electronic device according to an embodiment of this application.

[0034] Figure 16 This is a circuit block diagram of an electronic device according to another embodiment of this application.

[0035] Explanation of reference numerals in the attached figures:

[0036] 100'-Glass protective cover, 30'-Light-blocking ink, 100-Glass cover plate, 101-Preset surface, 10-Cover plate body, 11-First light-transmitting part, 13-Light-blocking part, 15-Second light-transmitting part, 10a-First rod, 11a-Core rod, 13a-Ring rod, 20a-Second rod, 30a-Third rod, 40a-Fourth rod, 50a-Fifth rod, 101a-First stack, 102a-Second stack, 400-Electronic device, 410-Flash lamp, 430-Camera module, 440-Processor, 450-Display screen, 460-Middle frame, 470-Housing, 480-Memory. Detailed Implementation

[0037] To enable those skilled in the art to better understand the present application, the technical solutions in the embodiments of the present application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present application, and not all embodiments. Based on the embodiments in the present application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present application.

[0038] The terms "first," "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish different objects, not to describe a specific order. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion. For example, a process, method, system, product, or apparatus that includes a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to these processes, methods, products, or apparatuses.

[0039] The technical solutions in the embodiments of this application will now be described with reference to the accompanying drawings.

[0040] It should be noted that, for ease of explanation, the same reference numerals denote the same components in the embodiments of this application, and for the sake of brevity, detailed descriptions of the same components are omitted in different embodiments.

[0041] Cameras typically include a flash to enhance exposure in low-light conditions or adjust the color temperature in outdoor environments, thereby improving image or photo quality. However, in electronic devices such as mobile phones, the camera and flash are usually positioned next to each other, with a glass protective cover 100' (e.g., on the light-emitting / light-receiving surface of the camera and flash) on either side. Figure 1 As shown, although a light-blocking ink layer 30' is coated on the area of ​​the glass cover 100' outside the flash and camera, the light-blocking ink layer 30' can only block light in the direction perpendicular to the glass cover 100'. It cannot prevent the light emitted by the flash from passing through the glass cover 100' (along the extension direction of the glass cover 100') and entering the camera's viewing window, thus affecting the camera's image quality. Alternatively, a hole could be made in the transparent glass cover 100', and a black ring could be placed in the air to block light and prevent crosstalk between the flash and the camera lens. However, this reduces the waterproof performance of the glass cover 100'.

[0042] Please see Figure 2 and Figure 3This application provides a glass cover plate 100, which includes a first light-transmitting part 11, a light-blocking part 13, and a second light-transmitting part 15 connected in sequence; the light-blocking part 13 is disposed around the outer periphery of the first light-transmitting part 11, and the second light-transmitting part 15 is disposed around the outer periphery of the light-blocking part 13; the first light-transmitting part 11, the light-blocking part 13, and the second light-transmitting part 15 are integral structures; the light transmittance of the light-blocking part 13 is less than the light transmittance of the first light-transmitting part 11 and less than the light transmittance of the second light-transmitting part 15, and the light-blocking part 13 is used to prevent light entering the first light-transmitting part 11 from passing through the light-blocking part 13 and entering the second light-transmitting part 15.

[0043] The light-blocking portion 13 of the glass cover plate 100 of this application has a uniform light transmittance. It is opaque or semi-transparent. It can prevent lines from passing through the light-blocking portion 13 along the arrangement direction of the first light-transmitting portion 11, the light-blocking portion 13 and the second light-transmitting portion 15, and from the first light-transmitting portion 11 to the second light-transmitting portion 15, or from the second light-transmitting portion 15 to the first light-transmitting portion 11.

[0044] Optionally, the number of light-blocking parts 13 can be one or more. When the number of light-blocking parts 13 is more than one, the multiple light-blocking parts 13 are arranged at intervals. "More than one" means two or more.

[0045] Please see Figure 4 and Figure 5 The first light-transmitting part 11, the light-blocking part 13, and the second light-transmitting part 15 constitute the cover plate body 10. The glass cover plate 100 of this application embodiment also includes a light-shielding layer 30. The light-shielding layer 30 is stacked on the surface of the cover plate body 10. The position where the light-shielding layer 30 is stacked with the first light-transmitting part 11 has a first through hole 31. The position where the light-shielding layer 30 is stacked with the second light-transmitting part 15 also has at least one second through hole 33. The second through hole 33 is spaced apart from the first through hole 31 to make the glass cover plate 100 have multiple viewing windows.

[0046] The glass cover 100 of this application can be applied to portable electronic devices such as mobile phones, tablets, laptops, desktop computers, smart bracelets, smartwatches, e-readers, and game consoles, serving as a protective cover for the camera, flash, and other components of the electronic device. The glass cover 100 can be used as a protective cover for the display screen (front cover) of the electronic device, or as part of the back cover of the electronic device.

[0047] Understandably, when the glass cover 100 is applied to an electronic device, the first through-hole 31 corresponds to the position of the flash, and the second through-hole 33 corresponds to the position of the camera. It is also understandable that the flash is located below the first through-hole 31 of the light-shielding layer 30, and the camera is located below the second through-hole 33 of the light-shielding layer 30.

[0048] Glass rods are usually cylindrical. When it is necessary to prepare glass parts with large cross-sections (such as glass covers, especially glass covers with different light transmittance in different parts), multiple glass rods can be stacked and molded together. However, after stacking multiple glass rods, the gaps between the glass rods are large. After molding, it is difficult to completely remove the air inside, resulting in a large number of residual pores inside, which seriously affects the mechanical properties and appearance of the large cross-section glass parts.

[0049] This application provides a method for preparing a glass cover plate 100, which includes:

[0050] Provide the first rod;

[0051] Multiple second rods and multiple third rods are provided and stacked tightly to obtain a first stack, wherein the third rod is located within the gap formed by adjacent second rods, and the radial dimension of the second rod is larger than the radial dimension of the third rod.

[0052] The first stack is thermally stretched to obtain the fourth rod.

[0053] The fourth rod is tightly surrounded on the outer periphery of the first rod to form a second stack.

[0054] The second stack is molded to obtain the fifth rod, and

[0055] The fifth rod is cut to obtain a glass cover plate 100.

[0056] Optionally, the first rod is used to form the first light-transmitting portion 11 and the light-blocking portion 13, and the fourth rod is used to form the second light-transmitting portion 15.

[0057] The fourth rod in this application is formed by thermal stretching of the first stack. By designing the stacking method of the first stack, the cross-section of the fourth rod can have a predetermined shape. In addition, the first stack uses second rods with larger radial dimensions and second rods with smaller radial dimensions to stack, minimizing the gaps within the first stack and thus reducing the number of air bubbles formed within the resulting fourth rod, resulting in better appearance and mechanical properties. Then, the fourth rod is tightly stacked on the outer periphery of the first rod and molded to obtain the fifth rod. By controlling the permeability between the first and fourth rods... The light transmittance is improved, thus enabling the fabrication of a glass cover 100 where the light-transmitting portion and the light-blocking portion 13 are integrated. The light-blocking portion 13 prevents light from passing through the glass cover 100 along its extension direction (i.e., perpendicular to the thickness direction). Furthermore, by designing the cross-section of the fourth rod to have a predetermined shape, the fourth rod can be stacked more tightly around the outer periphery of the first rod, and the gap between the fourth rod and the first rod can be minimized. This results in fewer air bubbles within the glass cover 100 after molding and cutting, leading to better appearance and mechanical properties. Moreover, the glass cover 100 produced in this application has an integrated structure, providing better waterproofing performance.

[0058] Please see Figure 6 and Figure 7 This application provides a method for preparing a glass cover plate 100, which includes:

[0059] S201, providing the first rod 10a;

[0060] Please see also Figure 8 Optionally, providing the first rod 10a includes:

[0061] S2011, providing mandrel 11a and ring rod 13a;

[0062] In this application, the term "rod" refers to an elongated component whose length dimension is greater than its radial dimension (e.g., the dimension perpendicular to the length direction).

[0063] Understandably, the core rod 11a is a solid rod, and the annular rod 13a is a hollow rod.

[0064] Optionally, the light transmittance of the core rod 11a is greater than that of the annular rod 13a. In one specific embodiment, the light transmittance of the core rod 11a is greater than or equal to 85% (understandably, the core rod 11a is transparent), and the light transmittance of the annular rod 13a with a thickness of 1 mm is less than or equal to 3%, for example, a black, high-light-absorbing glass ring or annular rod.

[0065] Optionally, both the core rod 11a and the annular rod 13a are made of glass. The core rod 11a and the annular rod 13a have the same main components, and the annular rod 13a is formed by adding colorant (such as black colorant) to the raw material components of the core rod 11a.

[0066] Optionally, the coefficient of thermal expansion α1 of the mandrel 11a and the coefficient of thermal expansion α2 of the ring rod 13a satisfy 0 ≤ |α1-α2| / α1 ≤ 10%; specifically, |α1-α2| / α1 can be, but is not limited to, 0, 1%, 2%, 4%, 6%, 8%, 10%, etc. The smaller the difference between the coefficient of thermal expansion α1 of the mandrel 11a and the coefficient of thermal expansion α2 of the ring rod 13a, the better. The closer the coefficients of thermal expansion α1 of the mandrel 11a and α2 of the ring rod 13a are, the better the bonding performance between the mandrel 11a and the ring rod 13a will be when the mandrel 11a and the ring rod 13a are thermally stretched to form the first rod body 10a of an integral structure, resulting in better mechanical properties.

[0067] Optionally, the difference between the glass transition temperature Tg1 of the annular rod 13a and the glass transition temperature Tg2 of the core rod 11a satisfies: 0 ≤ |Tg1-Tg2| / Tg1 ≤ 5%, and the light transmittance of the annular rod 13a is less than that of the core rod 11a. Specifically, the difference between the glass transition temperature of the core rod 11a and the glass transition temperature of the annular rod 13a can be, but is not limited to, 0%, 1%, 2%, 3%, 4%, 5%, etc. The closer the glass transition temperatures of the core rod 11a and the annular rod 13a are, the closer their viscosities will be during hot stretching. This allows for better consistency in their hot stretching deformation and better avoids the situation where one reaches a suitable hot stretching temperature while the other has not yet reached a suitable temperature or is too high, resulting in excessively low viscosity.

[0068] Optionally, when the mandrel 11a is inserted into the annular rod 13a, the outer peripheral sidewall of the mandrel 11a is fitted to the inner peripheral sidewall of the annular rod 13a; in other words, the shape of the outer peripheral sidewall of the mandrel 11a and the shape of the inner peripheral sidewall of the annular rod 13a are the same geometric shape (e.g., the same circle or regular polygon) in the cross-section perpendicular to the length direction. This can better avoid gaps between the mandrel 11a and the annular rod 13a, which would affect the bonding performance of the mandrel 11a and the annular rod 13a when the first rod body 10a with an integral structure is obtained by hot stretching.

[0069] In some embodiments, the core rod 11a is a cylinder, the annular rod 13a is an annular rod, and the diameter of the core rod 11a (i.e., the diameter of the cross section perpendicular to the length direction) is equal to the inner diameter of the annular rod, or the diameter of the core rod 11a is approximately smaller than the inner diameter of the annular rod (e.g., the difference is within 5%).

[0070] In one specific embodiment, the diameter of the core rod 11a is 20 mm, and the outer diameter of the annular rod 13a is 25 mm and the inner diameter is 20.1 mm.

[0071] S2012, insert the core rod 11a into the annular rod 13a; and

[0072] Understandably, the annular rod 13a is sleeved around the outer periphery of the core rod 11a to form a sleeve structure; in other words, the core rod 11a is inserted into the annular rod 13a.

[0073] S2013, the first rod 10a is obtained by hot stretching at a preset temperature T' of Tg1+10℃≤T'≤Tg1+30℃ and a traction speed R' of 0.1m / s≤R'≤1m / s, wherein Tg1 is the glass transition temperature of the annular rod 13a.

[0074] Optionally, the sleeve structure is heated to 10°C to 30°C above the glass transition temperature of the annular rod 13a (e.g., 10°C, 15°C, 20°C, 25°C, or 30°C above the glass transition temperature), and then thermally stretched at a traction speed of 0.1 m / s to 1 m / s to obtain a first rod 10a with a predetermined radial dimension. The first rod 10a includes a connected core rod 11a portion and an annular portion, the annular portion surrounding the core rod 11a portion, and the light transmittance of the annular portion being less than that of the core rod 11a portion. In the embodiments of this application, when referring to the numerical range a to b, unless otherwise specified, the value can be any value between a and b, including the endpoint value a and the endpoint value b.

[0075] Optionally, during stretching, the tension is applied along the direction of gravity. If the temperature is too low during hot stretching, the sleeve structure will not be fully softened or will have a high viscosity, affecting the bonding performance between the mandrel 11a and the annular rod 13a. This can result in residual pores in the first rod 10a, affecting the appearance and mechanical properties of the final glass cover 100. If the temperature is too high, the viscosity of the sleeve structure will be too low, making it difficult to maintain the shape of the stacked outer contour after stretching.

[0076] Optionally, the traction speed R' can be, but is not limited to, 0.1 m / s, 0.2 m / s, 0.3 m / s, 0.4 m / s, 0.5 m / s, 0.6 m / s, 0.7 m / s, 0.8 m / s, 0.9 m / s, 1 m / s, etc. If the traction speed R' is too large, the casing structure is prone to breakage; if the traction speed is too slow, the radial dimensions of the resulting first rod 10a may be uneven due to the weight of the casing structure itself.

[0077] S202, multiple second rods 20a and multiple third rods 30a are provided and stacked tightly to obtain a first stack body 101a, wherein the third rods 30a are located in the gap formed by adjacent second rods 20a, and the radial dimension of the second rods 20a is larger than the radial dimension of the third rods 30a.

[0078] Optionally, providing multiple second rods 20a and multiple third rods 30a includes: forming second rods 20a by hot stretching the aforementioned mandrel 11a; and forming third rods 30a by hot stretching the aforementioned mandrel 11a, wherein the radial dimension of the second rods 20a is larger than the radial dimension of the third rods 30a. A mold with a receiving cavity is provided, and the second rods 20a and third rods 30a are tightly stacked in the receiving cavity, so that the third rods 30a are located within the gaps between the multiple second rods 20a, to obtain a first stack 101a. The first stack 101a is then covered with tin foil to prevent misalignment between the stacked second rods 20a and third rods 30a. By providing smaller third rods 30a within the gaps formed by adjacent second rods 20a, the gaps within the first stack 101a can be minimized, thereby minimizing the number of air bubbles formed within the fourth rod formed by hot stretching the first stack, resulting in better appearance and mechanical properties.

[0079] It should be noted that the structure of the first stack 101a is equivalent to tightly stacking the second rods 20a, with the third rod 30a inserted through the gaps between the tightly stacked second rods 20a, thereby minimizing the gaps within the first stack 101a. Understandably, the extending directions of the second rods 20a, the third rod 30a, and the first stack 101a are parallel to each other.

[0080] Optionally, the core rod 11a, the second rod 20a, and the third rod 30a have the same raw material composition, which can make the fourth rod have a better appearance and more uniform light transmittance, and finally make the light transmittance of the light-transmitting part of the glass cover plate 100 more uniform and the appearance color more uniform.

[0081] Please see also Figure 9 Optionally, the second rod 20a has a first cross-section perpendicular to its length direction, and the third rod 30a has a second cross-section perpendicular to its length direction. The ratio of the equivalent circle diameter d1 of the first cross-section to the equivalent circle diameter d2 of the second cross-section is in the range of d1 / d2≤6.3.

[0082] The term "equivalent circle diameter" refers to the diameter of an irregular geometric figure that is the same as the diameter of a circle with the same area.

[0083] Furthermore, the ratio of the equivalent circle diameter d1 of the first cross-section to the equivalent circle diameter d2 of the second cross-section is in the range of 3 ≤ d1 / d2 ≤ 6.3; specifically, the ratio of the equivalent circle diameter d1 of the first cross-section to the equivalent circle diameter d2 of the second cross-section can be, but is not limited to, 3, 3.5, 4, 4.5, 5, 5.5, 6, 6.3, etc. If the ratio of the equivalent circle diameter d1 of the first cross-section to the equivalent circle diameter d2 of the second cross-section is too small, the third rod 30a cannot fill the gap formed by the adjacent second rods 20a as much as possible, resulting in a larger gap in the first stack 101a. This makes it easy for the fourth rod formed by hot stretching to have residual pores, affecting the appearance and mechanical properties of the fourth rod. If the ratio of the equivalent circle diameter d1 of the first cross-section to the equivalent circle diameter d2 of the second cross-section is too large, the third rod 30a will expand the tightly stacked second rods 20a, which will also increase the gap in the first stack 101a. This makes it easy for the fourth rod formed by hot stretching to have residual pores, affecting the appearance and mechanical properties of the fourth rod.

[0084] Optionally, along the extension direction perpendicular to the first stack 101a, the cross-sectional shape of the first stack 101a is a similar regular polygon, such as a similar regular hexagon. A similar regular hexagon refers to a shape with a hexagonal shape, but the sides of the hexagon are curved, serrated, or partially irregular. Optionally, the first stack 101a is stacked using a mold with an inverted trapezoidal cross-section, so that the cross-sectional shape of the stacked first stack 101a is a similar regular hexagon. The regular hexagonal structure is more stable, and the gap between the second rod 20a and the third rod 30a is smaller. When the first stack 101a is stretched and deformed, it is easier to maintain its original shape, making the outer contour of the cross-section of the fourth rod obtained after stretching similar to the outer contour of the cross-section of the first stack 101a. "Similar shape" refers to a shape whose outer contour shape is proportionally enlarged or reduced, such as a similar regular hexagon.

[0085] In one specific embodiment, both the second rod 20a and the third rod 30a are cylindrical rods. Any adjacent second rods 20a are tightly stacked and tangent to each other, and each third rod 30a is tangent to each of its adjacent second rods 20a. Specifically, except for the second rods 20a located at the outer periphery, each second rod 20a is tangent to six adjacent third rods 30a, and each third rod 30a is tangent to three adjacent second rods 20a.

[0086] S203, the first stack 101a is thermally stretched to obtain the fourth rod 40a (e.g., Figure 10 (as shown);

[0087] Optionally, the hot stretching of the first stack 101a includes: hot stretching the first stack 101a at a first temperature and a stretching speed, wherein the first temperature is higher than the glass transition temperature of the second rod 20a and higher than the glass transition temperature of the third rod 30a; the stretching speed R is in the range of 0.1m / s ≤ R ≤ 1m / s. Hot stretching of the first stack 101a yields a fourth rod 40a with a predetermined cross-sectional shape. This allows for smaller gaps within the second stack 102a during stacking, resulting in a tighter stack of the fourth rods 40a within the second stack 102a. After molding, this minimizes air bubbles in the cut glass cover 100, leading to better appearance and mechanical properties.

[0088] Alternatively, when stretching, the force is applied along the direction of gravity.

[0089] Optionally, the second rod 20a and the third rod 30a are made of the same material, and the range of the first temperature T1 is: Tg3+10℃≤T1≤Tg3+30℃; Tg3 is the glass transition temperature of the second rod 20a.

[0090] Specifically, the first temperature can be, but is not limited to, Tg3+10℃, Tg3+15℃, Tg3+20℃, Tg3+25℃, Tg3+30℃, etc.

[0091] If the initial temperature is too low during hot stretching, the first stack 101a will not be fully softened or will have a high viscosity, affecting the bonding performance between the second rod 20a and the third rod 30a. This will result in the fourth rod 40a easily retaining pores, affecting the final appearance and mechanical properties of the glass cover 100. If the initial temperature is too high, the viscosity of the first stack 101a will be too low, making it difficult to maintain the shape of the outer contour after stretching.

[0092] In a specific example, if the glass transition temperature of the second rod 20a and the third rod 30a is 700°C, then the first temperature can be between 710°C and 730°C.

[0093] Optionally, the stretching speed R can be, but is not limited to, 0.1 m / s, 0.2 m / s, 0.3 m / s, 0.4 m / s, 0.5 m / s, 0.6 m / s, 0.7 m / s, 0.8 m / s, 0.9 m / s, 1 m / s, etc. If the stretching speed R is too large, the first stack 101a is prone to breakage; if the stretching speed is too slow, the fourth rod 40a may become unbalanced due to the gravity of the first stack 101a itself.

[0094] Optionally, along the extension direction perpendicular to the fourth rod 40a, the cross-sectional shape of the fourth rod 40a is similar to a regular polygon, such as a regular hexagon. In one specific embodiment, the cross-section of the fourth rod 40a along its extension direction is similar to a regular hexagon, with each side of the hexagon being a curve composed of multiple convex semicircles connected sequentially. Thus, when the fourth rods 40a are stacked to form the second stack 102a, the fourth rods 40a can be tightly stacked, with the smallest possible gap between adjacent fourth rods 40a, minimizing the porosity within the resulting glass cover 100 and improving the appearance and mechanical strength of the glass cover 100.

[0095] Understandably, the outer contour of the cross section of the fourth rod 40a along its extension direction is similar in shape to the outer contour of the cross section of the first stack 101a along its extension direction, i.e., they are similar figures.

[0096] In one specific embodiment, the second rod 20a and the third rod 30a are both cylinders, the cross-section of the fourth rod 40a is similar to a regular hexagon, the diameter of the second rod 20a is 3mm, the diameter of the third rod 30a is 0.5mm, and the equivalent circle diameter of the cross-section of the fourth rod 40a is 1mm.

[0097] Understandably, step S201 can be performed before S202, or after S203 and before S204, and this application does not make any specific limitation.

[0098] S204, the fourth rod 40a is tightly surrounded on the outer periphery of the first rod 10a to form a second stack 102a;

[0099] Optionally, the fourth rod 40a is stacked tightly, and the first rod 10a is placed in a preset position during stacking to obtain a second stack 102a, that is, the first rod 10a and the fourth rod 40a are arranged together. Optionally, the second stack 102a is a rod with a cross-section similar to a hexagonal structure.

[0100] Optionally, the first rod 10a has a third cross-section perpendicular to its length direction, and the fourth rod 40a has a fourth cross-section perpendicular to its length direction. The equivalent circle diameter of the third cross-section is larger than the equivalent circle diameter of the fourth cross-section. Understandably, the radial dimension of the first rod 10a is larger than the radial dimension of the fourth rod 40a. This allows for a smaller gap between the first rod 10a and the fourth rod 40a during stacking, better reducing the porosity within the resulting glass cover 100 and improving the appearance and mechanical strength of the glass cover 100.

[0101] In a specific example, the first rod 10a is a cylindrical structure (i.e., the third cross-section is a circle), and the fourth rod 40a is a quasi-regular hexagon whose fourth cross-section is composed of semi-circular arcs.

[0102] Optionally, the ratio of the equivalent circle diameter d3 of the third cross-section to the equivalent circle diameter d4 of the fourth cross-section is in the range of 3 ≤ d3 / d4 ≤ 40. Further, the ratio of the equivalent circle diameter d3 of the third cross-section to the equivalent circle diameter d4 of the fourth cross-section is in the range of 6 ≤ d3 / d4 ≤ 17. Specifically, the ratio of the equivalent circle diameter d3 of the third cross-section to the equivalent circle diameter d4 of the fourth cross-section can be, but is not limited to, 3, 5, 8, 10, 15, 20, 25, 30, 35, 40, etc. If the ratio of the equivalent circle diameter d3 of the third cross-section to the equivalent circle diameter d4 of the fourth cross-section is too small, then when the first rod 10a and the fourth rod 40a are stacked, the gap between the outer periphery of the first rod 10a and the fourth rod 40a will be too large, resulting in increased porosity in the fifth rod 50a obtained by molding, affecting the appearance and mechanical properties of the resulting glass cover 100. The larger the ratio of the equivalent circle diameter d3 of the third cross section to the equivalent circle diameter d4 of the fourth cross section, the smaller the gap between the outer periphery of the first rod 10a and the fourth rod 40a. However, when stacking, more fourth rods 40a are required, which increases the complexity of the process and raises the process cost.

[0103] Optionally, the equivalent circle diameter d3 of the third cross section is in the range of 3mm≤d3≤20mm; specifically, the equivalent circle diameter d3 of the third cross section can be, but is not limited to, 3mm, 5mm, 8mm, 10mm, 13mm, 15mm, 18mm, 20mm, etc.

[0104] Optionally, the equivalent circle diameter d4 of the fourth cross-section is in the range of 0.5mm ≤ d4 ≤ 1.2mm. Specifically, the equivalent circle diameter d4 of the fourth cross-section can be, but is not limited to, 0.5mm, 0.6mm, 0.7mm, 0.8mm, 0.9mm, 1.0mm, 1.1mm, 1.2mm, etc.

[0105] S205, the second stack 102a is molded (also known as melt pressing) to obtain the fifth rod 50a, and

[0106] Optionally, the molding of the second stack 102a includes: placing the second stack 102a into a mold, and molding the second stack 102a at a second temperature and under a preset pressure, wherein the second temperature is lower than the glass transition temperature of the fourth rod 40a and lower than the glass transition temperature of the first rod 10a; the preset pressure ranges from 150Kg≤P≤250Kg.

[0107] Understandably, the temperature of compression molding is lower than that of hot stretching.

[0108] Alternatively, compression molding can be performed under vacuum and negative pressure.

[0109] Optionally, the glass transition temperature of the first rod 10a is close to that of the second rod 20a (e.g., differing by within 5%), and the range of the second temperature T2 is: Tg4-30℃≤T2≤Tg4-10℃; where Tg4 is the glass transition temperature of the fourth rod 40a. Specifically, the second temperature T2 can be, but is not limited to, Tg4-30℃, Tg4-25℃, Tg4-20℃, Tg4-15℃, Tg4-10℃, etc. If the second temperature is too low, it affects the adhesion between the fourth rods 40a and between the fourth rod 40a and the first rod 10a. Furthermore, air between the fourth rod 40a and the first rod 10a is difficult to completely eliminate, easily resulting in a significant number of pores remaining in the fifth rod 50a, affecting the mechanical properties and appearance of the manufactured glass cover 100. If the second temperature is too high, the relative positions of the first rods 10a are prone to shifting, making it difficult to maintain the original shape of the first rods 10a (easily deformed) and their relative positions, reducing the design flexibility of the position and size of the light-blocking portion 13 on the manufactured glass cover 100. When the second temperature is within this range, a thinner fifth rod 50a can be formed, ensuring that the fourth rod 40a and the first rod 10a create a seamless, integral structure. It also ensures that the relative position of the first rod 10a within the fourth rod 40a does not change during molding.

[0110] In a specific example, if the glass transition temperature of the fourth rod 40a is 700°C, then the second temperature can be between 670°C and 690°C.

[0111] Optionally, the preset pressure range is: 150Kg≤P≤250Kg. Specifically, the preset pressure can be, but is not limited to, 150Kg, 170Kg, 190Kg, 210Kg, 230Kg, 250Kg, etc. If the preset pressure is too low, the adhesion between the fourth rods 40a and between the fourth rod 40a and the first rod 10a will be poor. If the preset pressure is too high, the first rod 10a will easily deform, and the relative position of the first rod 10a within the fourth rod 40a will also easily shift. This will cause the position of the light-blocking part 13 of the manufactured glass cover 100 to shift, reducing the design flexibility of the position and size of the light-blocking part 13 on the glass cover 100.

[0112] S206, the fifth rod 50a is cut (i.e., cold-worked) to obtain the glass cover plate 100.

[0113] Optionally, the fifth rod 50a is cut along a direction perpendicular to its extension to form a glass sheet of the required thickness (e.g., a sheet 0.4 mm to 0.7 mm thick). The glass sheet is then CNC machined into the desired shape and polished to a mirror finish to obtain the glass cover plate 100.

[0114] In one specific embodiment, the core rod 11a is used to form the first light-transmitting portion 11 of the glass cover 100, and the annular rod 13a is used to form the light-blocking portion 13 of the glass cover 100; in other words, the first rod 10a is used to form the first light-transmitting portion 11 and the light-blocking portion 13 of the glass cover 100. The fourth rod 40a is used to form the second light-transmitting portion 15 of the glass cover 100.

[0115] Please see Figure 11 This application provides a method for preparing a glass cover plate 100, which includes:

[0116] S301, providing the first rod 10a;

[0117] S302, multiple second rods 20a and multiple third rods 30a are provided and stacked tightly to obtain a first stack body 101a, wherein the third rods 30a are located in the gap formed by adjacent second rods 20a, and the radial dimension of the second rods 20a is larger than the radial dimension of the third rods 30a.

[0118] S303, the first stack 101a is thermally stretched to obtain the fourth rod 40a;

[0119] S304, the fourth rod 40a is tightly surrounded on the outer periphery of the first rod 10a to form a second stack 102a;

[0120] S305, the second stack 102a is molded to obtain the fifth rod 50a;

[0121] S306, the fifth rod 50a is cut to obtain a glass sheet, and the glass sheet is CNC machined and polished;

[0122] For detailed descriptions of S301 to S306, please refer to the descriptions of the corresponding parts of the above embodiments, which will not be repeated here.

[0123] S307, chemical strengthening of CNC-machined and polished glass sheets; and

[0124] Optionally, the S306 glass sheet is placed in molten potassium nitrate for ion exchange to obtain the cover plate body 10, and stress is formed on the surface of the glass sheet to improve the mechanical strength of the cover plate body 10.

[0125] Optionally, the first rod 10a is used to form the first light-transmitting portion 11 and the light-blocking portion 13 of the cover body 10. The fourth rod 40a is used to form the second light-transmitting portion 15 of the cover body 10.

[0126] S308, a light-shielding layer 30 is formed on the surface of the cover plate body 10.

[0127] Optionally, ink is printed on the surface of the chemically strengthened glass sheet (i.e., the surface of the cover plate body 10) and cured to form a light-shielding layer 30.

[0128] Optionally, the light-shielding layer 30 at least partially covers the second light-transmitting portion 15. Understandably, the position where the light-shielding layer 30 overlaps with the first light-transmitting portion 11 has a first through-hole 31, and the position where the light-shielding layer 30 overlaps with the second light-transmitting portion 15 also has at least one second through-hole 33, the second through-hole 33 being spaced apart from the first through-hole 31, for providing the glass cover 100 with multiple viewing windows.

[0129] Please see Figures 12 to 14This application also provides an electronic device 400, which includes a glass cover plate 100, a flash lamp 410, a camera module 430, and a processor 440 as described in this application embodiment. The glass cover plate 100 has a preset surface 101. The flash lamp 410 is disposed on the preset surface 101 side of the glass cover plate 100, and the light-emitting surface of the flash lamp 410 is projected onto the preset surface 101 within the range of the first light-transmitting portion 11. The camera module 430 is disposed on the same side of the glass cover plate 100 as the flash lamp 410 and is spaced apart from the glass cover plate 100. The light-incident surface of the camera module 430 is projected onto the preset surface 101 within the range of the second light-transmitting portion 15. The processor 440 is electrically connected to the camera module 430 and the flash lamp 410 respectively, and is used to control the camera module 430 to take pictures and to control the flash lamp 410 to work.

[0130] The electronic device 400 in this application embodiment can be, but is not limited to, a mobile phone, tablet computer, laptop computer, desktop computer, smart bracelet, smartwatch, e-reader, game console, or other portable electronic device 400.

[0131] For a detailed description of the glass cover 100, please refer to the description of the corresponding part of the above embodiment, which will not be repeated here.

[0132] Optionally, processor 440 includes one or more general-purpose processors, wherein the general-purpose processor 440 can be any type of device capable of processing electronic instructions, including a central processing unit (CPU), microprocessor, microcontroller, main processor, controller, and ASIC, etc. Processor 440 is used to execute various types of digital storage instructions, such as software or firmware programs stored in memory 480, which enables the computing device to provide a wide range of services.

[0133] Please see Figure 15 and Figure 16 Optionally, the electronic device 400 of this application further includes a display screen 450, a mid-frame 460, a housing 470, and a memory 480. The display screen 450, mid-frame 460, and housing 470 are stacked sequentially. The camera module 430, processor 440, memory 480, flash 410, and other components are disposed within the space enclosed by the mid-frame 460 and housing 470. The display screen 450 and the memory 480 are electrically connected to the processor 440. The display screen 450 is used to display under the control of the processor 440. The memory 480 is used to store the program code required for the processor 440 to run, the program code required to control the display screen 450, camera module 430, and flash 410, and the display content of the display screen 450.

[0134] The display screen 450 can be, but is not limited to, one or more of the following: liquid crystal display screen, light-emitting diode display screen (LED display screen), micro light-emitting diode display screen (Micro LED display screen), mini light-emitting diode display screen (Mini LED display screen), organic light-emitting diode display screen (OLED display screen).

[0135] Optionally, the camera module 430 can take pictures through the viewing window on the second light-transmitting portion 15 of the glass cover plate 100. The camera module 430 can be a front-facing camera module 430 or a rear-facing camera module 430; when the camera module 430 is a front-facing camera module 430, the glass cover plate 100 serves as a protective cover or part of a protective cover for the display screen 450, and is used to protect the front-facing camera module 430 and the flash 410, and to provide a viewing window for the camera module 430 and the flash 410; when the camera module 430 is a front-facing camera module 430, the glass cover plate 100 serves as part of the housing 470 or is supported on the housing 470, and is used to protect the rear-facing camera module 430 and the flash 410, and to provide a viewing window for the camera module 430 and the flash 410.

[0136] Optionally, memory 480 may include volatile memory, such as random access memory (RAM); memory 480 may also include non-volatile memory (NVM), such as read-only memory (ROM), flash memory (FM), hard disk drive (HDD), or solid-state drive (SSD). Memory 480 may also include combinations of the above types of memory.

[0137] It is understood that the electronic device 400 described in this embodiment is merely one form of the electronic device 400 used on the glass cover 100, and should not be construed as a limitation on the electronic device 400 provided in this application, nor should it be construed as a limitation on the glass cover 100 provided in various embodiments of this application.

[0138] In this application, the terms "embodiment" and "implementation" mean that a specific feature, structure, or characteristic described in connection with an embodiment can be included in at least one embodiment of this application. The appearance of these phrases in various locations throughout the specification does not necessarily refer to the same embodiment, nor are they independent or alternative embodiments mutually exclusive with other embodiments. Those skilled in the art will understand, explicitly and implicitly, that the embodiments described in this application can be combined with other embodiments. Furthermore, it should be understood that the features, structures, or characteristics described in the various embodiments of this application can be arbitrarily combined to form another embodiment that does not depart from the spirit and scope of the technical solution of this application, provided there is no contradiction between them.

[0139] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application and are not intended to limit it. Although this application has been described in detail with reference to the above preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions to the technical solutions of this application should not depart from the spirit and scope of the technical solutions of this application.

Claims

1. A method for preparing a glass cover plate, characterized in that, include: Provide the first rod; Multiple second rods and multiple third rods are provided and stacked tightly to obtain a first stack, wherein the third rod is located within the gap formed by adjacent second rods, and the radial dimension of the second rod is larger than the radial dimension of the third rod. The first stack is thermally stretched to obtain the fourth rod. The fourth rod is tightly surrounded on the outer periphery of the first rod to form a second stack. The second stack is molded to obtain the fifth rod; and The fifth rod is cut to obtain a glass cover plate.

2. The method for preparing the glass cover plate according to claim 1, characterized in that, The second rod has a first cross-section perpendicular to its length direction, and the third rod has a second cross-section perpendicular to its length direction. The ratio of the equivalent circle diameter d1 of the first cross-section to the equivalent circle diameter d2 of the second cross-section is in the range of d1 / d2≤6.

3.

3. The method for preparing the glass cover plate according to claim 1, characterized in that, The first rod has a third cross-section perpendicular to its length direction, and the fourth rod has a fourth cross-section perpendicular to its length direction. The equivalent circle diameter of the third cross-section is larger than the equivalent circle diameter of the fourth cross-section.

4. The method for preparing the glass cover plate according to claim 3, characterized in that, The range of the ratio of the equivalent circle diameter d3 of the third cross section to the equivalent circle diameter d4 of the fourth cross section is: 3≤d3 / d4≤40.

5. The method for preparing the glass cover plate according to claim 1, characterized in that, The hot stretching of the first stack includes: The first stack is thermally stretched at a stretching speed at a first temperature, wherein the first temperature is higher than the glass transition temperature of the second rod and higher than the glass transition temperature of the third rod; the stretching speed R is in the range of 0.1 m / s ≤ R ≤ 1 m / s.

6. The method for preparing the glass cover plate according to claim 1, characterized in that, The molding of the second stack includes: The second stack is molded under a preset pressure at a second temperature, wherein the second temperature is lower than the glass transition temperature of the fourth rod and lower than the glass transition temperature of the first rod; the preset pressure ranges from 150Kg≤P≤250Kg.

7. The method for preparing a glass cover plate according to claim 1, characterized in that, The provision of the first rod includes: Mandrels and ring rods are provided; The mandrel is inserted into the annular rod; and The first rod is obtained by hot stretching at a preset temperature T' of Tg1+10℃≤T'≤Tg1+30℃ and a traction speed R' of 0.1m / s≤R'≤1m / s, where Tg1 is the glass transition temperature of the annular rod.

8. The method for preparing the glass cover plate according to claim 7, characterized in that, The difference between the glass transition temperature Tg1 of the annular rod and the glass transition temperature Tg2 of the core rod satisfies: 0≤|Tg1-Tg2| / Tg1≤5%, and the light transmittance of the annular rod is less than that of the core rod.

9. A glass cover plate, characterized in that, The glass cover plate includes a first light-transmitting portion, a light-blocking portion, and a second light-transmitting portion connected in sequence; the light-blocking portion is arranged around the outer periphery of the first light-transmitting portion, and the second light-transmitting portion is arranged around the outer periphery of the light-blocking portion; the first light-transmitting portion, the light-blocking portion, and the second light-transmitting portion are an integral structure; the light transmittance of the light-blocking portion is less than the light transmittance of the first light-transmitting portion and less than the light transmittance of the second light-transmitting portion, and the light-blocking portion is used to prevent light entering the first light-transmitting portion from passing through the light-blocking portion and entering the second light-transmitting portion; the glass cover plate is prepared by the preparation method according to any one of claims 1-8, wherein the first light-transmitting portion and the light-blocking portion are formed by the first rod, and the second light-transmitting portion is formed by the fourth rod.

10. An electronic device, characterized in that, include: The glass cover plate according to claim 9, wherein the glass cover plate has a predetermined surface; A flash lamp is disposed on the preset surface side of the glass cover plate, and the light-emitting surface of the flash lamp is projected onto the preset surface within the range of the first light-transmitting part. A camera module, wherein the camera module and the flash are disposed on the same side of the glass cover and spaced apart from the glass cover, and the light-incident surface of the camera module is projected onto the preset surface within the range of the second light-transmitting part; as well as The processor is electrically connected to both the camera module and the flash, and is used to control the camera module to take pictures and to control the flash to work.

Citation Information

Patent Citations

  • Glass with high mechanical strength and manufacturing method