Vehicle-mounted head-up display optical film with light scattering function and preparation method thereof
By using an optical film with a dynamic scattering layer and a reflective layer in the vehicle head-up display, and using a thermally induced non-external force two-way shape memory polymer material to scatter light when exposed to sunlight, the problem of reduced image recognition and image recognition problems in the vehicle head-up display under direct sunlight is solved. The problem of obstructed vision improves driving safety.
Patent Information
- Application Number
- CN202410645469.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-23
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-05-23
AI Technical Summary
The image recognition of existing vehicle head-up displays decreases under direct sunlight, causing the driver's line of sight to be blocked and increasing safety risks.
A vehicle-mounted head-up display optical film with light scattering function is used, including a dynamic scattering layer and a reflective layer. The dynamic scattering layer is made of a thermotropic, force-free, two-way shape memory polymer material. The scattering part bulges when the sun shines to scatter the light. In other directions, reduce direct sunlight entering the eyes.
It effectively improves driving safety, reduces direct sunlight into the driver's eyes, enhances vision and image recognition under sunlight conditions, and reduces the possibility of the driver being affected by sunlight.
Smart Images

Figure CN118732271A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of automobile head-up display, and in particular to an automobile head-up display optical film with a light scattering function and a preparation method thereof. Background Art
[0002] This section is intended to provide a background or context to the embodiments of the invention recited in the claims. No admission is made that the description herein is prior art by inclusion in this section.
[0003] Compared with traditional head-down displays (HDDs), head-up displays (HUDs) reduce the driver's eye-off-the-road time (EoRT) by projecting virtual images into the driver's forward field of view (FoV). Due to the advantages in information acquisition costs, head-up displays are considered to have the potential to improve driving performance and safety. In addition, head-up displays play an active role in the management of primary and secondary driving matters. Since General Motors first introduced head-up displays in 1988, commercial head-up displays have been used in various mass-produced vehicles. It is predicted that by 2024, almost one-third of cars will be equipped with head-up display systems.
[0004] Under normal light, the head-up display provides great convenience for drivers and reduces safety hazards. However, as the direction of the vehicle changes, the relative position of the car and the sun will also change continuously. When the direction of the vehicle is exactly opposite to the position of the sun, for example, when the sun is lower in the morning and afternoon, driving to the east in the morning and to the west in the afternoon, or when the sun shines directly into the driver's eyes through the front windshield of the car, the sunlight passes through the head-up display area of the windshield and directly enters the driver's eyes, causing the driver's eyes to be unable to open, the line of sight is blocked, and the driving safety is seriously affected. More seriously, if it is necessary to drive on a road in a certain direction for a long time, and this direction happens to be the direction where the sun directly shines on the driver's eyes, the driver will drive for a long time under the glaring sunlight, which will cause huge safety hazards. Although many cars are equipped with sun visors, the driver needs to manually bend it down and adjust it to the appropriate angle during driving to just block the sunlight in front. The whole process requires the driver to exert force on the steering wheel and adjust the angle of the sun visor according to the angle of the sunlight, which is time-consuming and has high safety risks. If the road conditions change when the sun is directly shining into the eyes, and the driver encounters situations that require concentration, such as oncoming vehicles, obstacles, and sharp turns, the driver is taking his hands off the steering wheel and constantly adjusting the sun visor, and cannot respond to the road conditions in time, which is very likely to cause an accident. In addition, the sun visor will also block part of the driver's line of sight, making the driver's field of vision smaller, which is not conducive to timely understanding and judging the road conditions outside the car. On the other hand, the image recognition of the head-up display is significantly reduced under the sunlight, and it may even be completely unclear. The driver cannot judge which direction to go at this time, whether there is a fork in the road or a turn ahead, or what the lane distribution is like. The driver's eyes are temporarily "blind" due to the sunlight and he cannot open them, the navigation fails due to unclear head-up display images, and the brain is temporarily blank due to not knowing the road conditions ahead. Especially inexperienced drivers may become flustered and make operational errors. In the worst case, they may take the wrong road and affect their travel, or suffer serious traffic accidents with disastrous consequences.
[0005] Chinese Patent Application for Invention CN202211174763.9 discloses a windshield, a manufacturing method, a display device and a transportation device. Among them, the windshield includes: a transparent substrate; a transmissive-reflective film located on the transparent substrate, configured to reflect a part of the incident light propagating to the transmissive-reflective film and transmit the other part of the incident light. The transmissive-reflective film includes at least one first layer and at least one second layer arranged alternately. The refractive index n1 of the first layer ranges from 1.8 < n1 ≤ 2.6, and the refractive index n2 of the second layer ranges from 1.2 ≤ n2 ≤ 1.8. The reflection and refraction of the incident light are achieved by the different refractive indices of different layers of the transmissive-reflective film. Chinese Patent Application for Invention CN202010930913.9 discloses an anti-glare method, device and equipment for a windshield. By collecting relevant information of the incident light irradiating on the windshield, including: intensity, incident angle and irradiation area; analyzing the relevant information, differentiating the types of light according to the intensity and / or incident angle of the light, determining the corresponding visual influence area according to the irradiation area and the position of the driver's eyes, and adjusting the light transmittance of the background theme based on the type of light and the visual influence area to achieve an anti-glare effect. Chinese Patent Application for Invention CN202311724126.9 discloses an automatic anti-glare method, device, vehicle and storage medium. By identifying the position of the driver's eyes and the light source information that causes glare to the driver; determining the glare area on the front windshield according to the position of the eyes, and determining the target parameters that can prevent glare when the head-up display system is displayed in the glare area according to the light source information; controlling the head-up display system to perform anti-glare display in the glare area according to the target parameters. The above applications respectively prevent direct sunlight through different refractive indices of the multi-layer structure of the windshield, or adjust the light transmittance of the head-up display background by identifying the type of light and the influence area, or control the head-up display system to perform anti-glare by controlling the target parameters. Summary of the Invention
[0006] The object of the present invention is to propose a brand-new idea for preventing sunlight glare and provide an in-vehicle head-up display optical film with a light scattering function and its preparation method, aiming at the problems in the prior art that the image recognition rate of the head-up display decreases when encountering sunlight and the line of sight of the driver is blocked, causing potential safety hazards, so as to further improve the driving safety.
[0007] In order to achieve the above object, the technical solution adopted by the present invention is as follows.
[0008] An in-vehicle head-up display optical film with a light scattering function, the optical film includes a dynamic scattering layer and a reflective layer. The reflective layer is a mixture of a thermoplastic material and a plasticizer, and the reflective layer is wedge-shaped; the dynamic scattering layer includes a dynamic scattering layer matrix and a scattering part. The scattering part is located on the side of the dynamic scattering layer away from the reflective layer. The side of the dynamic scattering layer close to the reflective layer is a plane and is closely attached to the reflective layer; The scattering part is a plurality of light scattering points distributed on the matrix of the dynamic scattering layer. The scattering part is made of a thermotropic, force-free, bidirectional shape memory polymer material. A thermogenic agent capable of converting light energy into heat energy is covered on the surface of the scattering part away from the reflective layer. The scattering part bulges when exposed to direct sunlight and returns to its original shape when there is no direct sunlight.
[0009] The present invention arranges the scattering part of the dynamic scattering layer. When the scattering part is irradiated by the front sunlight, the scattering part bulges, thereby scattering the sunlight to other directions through the scattering effect of light, thereby preventing or reducing the sunlight from directly entering the driver's eyes.
[0010] Preferably, the thermoplastic material is PVB.
[0011] In some embodiments of the present invention, the thermal agent is single-atom gold, carbon black, graphene or carbon nanotube covering the surface of the scattering part.
[0012] In some embodiments of the present invention, a scattering solution is encapsulated in the matrix of the dynamic scattering layer, and the scattering solution is a solution of a thermotropic force-free two-way shape memory polymer. When there is no sunlight, the scattering solution is a transparent system. When exposed to sunlight, the thermotropic force-free two-way shape memory polymer in the scattering solution curls. When exposed to sunlight, the scattering solution can absorb and reflect a portion of the light, thereby further reducing the sunlight penetrating the display film into the driver's field of vision.
[0013] In some embodiments, the light transmittance of the dynamic scattering layer is not less than 70%.
[0014] Specifically, the composition of the scattering solution includes 30%-50% thermotropic force-free two-way shape memory material, 0.2%-0.8% thermogenic agent, 40%-50% plasticizer, 5%-6% dispersant, and 3%-4% defoaming agent. The thermotropic force-free two-way shape memory polymer material is used as a component of the dynamic scattering layer, and a thermogenic agent, i.e., a photothermal material, needs to be added to convert light energy into heat energy. The thermotropic force-free two-way shape memory material deforms under the action of heat energy and forms a stable colloidal solution under the action of the dispersant.
[0015] In order to further enhance the reflection of sunlight, the dynamic scattering layer is uniformly dispersed with light absorbing material particles and light reflecting material particles, so that the dynamic scattering layer itself has a part of light scattering function.
[0016] In some embodiments, the thermogenic agent is selected from at least one of carbon nanoparticles, carbon nanotubes, carbon black, graphene, graphene oxide, graphite, carbon dots, single atomic gold, Ag nanomaterials, Pt nanoparticles, Al nanoparticles, CuS nanosheets, TiO2 nanoparticles, MoO3 quantum dots, Fe3O4, indocyanine green, Prussian blue, thiadiazole derivatives and porphyrin rings.
[0017] In some embodiments, the thickness of the dynamic scattering layer is less than one tenth of the thickness of the light reflecting layer, for example, it may be 0.05 mm.
[0018] In addition, the present invention also provides a method for preparing a vehicle-mounted head-up display optical film with a light scattering function, comprising the following steps: S1: providing the thermotropic force-free bidirectional shape memory polymer material, processing it into a filament with a diameter of 10 μm-20 μm, taking 30%-50% of the processed thermotropic force-free bidirectional shape memory polymer material and adding it to 40%-50% of a plasticizer, and then sequentially adding 5%-6% of a dispersant, 0.2%-0.8% of a thermogenic agent, and 3%-4% of a defoaming agent, and stirring to a homogeneous scattering solution; S2: Encapsulating the scattering solution in a transparent sealing layer, wherein the scattering solution completely fills the sealing layer to form a dynamic scattering layer matrix, wherein the sealing layer uses PVB resin as a main material; S3: providing a thermotropic force-free bidirectional shape memory polymer material, heating it to a flowing or semi-flowing state, stirring it evenly to obtain a stable liquid scattering part, laying the dynamic scattering layer substrate flat, laying a layer of transparent adhesive film on the dynamic scattering layer substrate, applying the liquid scattering part on the surface of the adhesive film according to the distribution of scattering points of the scattering part, and then placing a plurality of carbon nanotubes on the surface of the applied scattering part, placing the dynamic scattering layer substrate at room temperature and standing until the liquid scattering part is cooled and fixed and adhered to the dynamic scattering layer substrate to form a dynamic scattering layer; S4: A wedge-shaped polyvinyl butyral (PVB) film is used as a reflective layer and is flatly attached to a platform, placed in a vacuum environment, and then the dynamic scattering layer prepared in step S3 is pressed onto the reflective layer, and each area of the dynamic scattering layer is pressed so that the reflective layer and the dynamic scattering layer are tightly attached and free of bubbles or impurities, thereby obtaining the vehicle-mounted head-up display optical film.
[0019] Furthermore, the adhesive film is a mixture of a thermoplastic material and a plasticizer, and the thermoplastic material is preferably PVB.
[0020] Furthermore, in order to make the dynamic scattering layer itself have a part of light scattering function, the above step S1 further includes: The light-absorbing material particles and the light-reflecting material particles are ball-milled in a ball mill at a speed of 3000-5000 r / min for 30-60 min, and then the scattering solution is added.
[0021] Furthermore, the diameter of the scattering part of the vehicle-mounted head-up display optical film is 0.05mm-0.1mm, and the total area of the scattering part accounts for one third to two thirds of the area of one side of the scattering dynamic scattering layer.
[0022] Compared with the prior art, the present invention has the following beneficial effects: The present invention adopts the concept of heat-sensitive shape memory, and utilizes the light-sensitive characteristics and shape memory function of photothermal effect shape memory materials. By setting the scattering part of the dynamic scattering layer, when it is irradiated by sunlight in front, the scattering part bulges, thereby scattering the sunlight to other directions through the scattering effect of light, and further by setting the scattering layer matrix as an encapsulated scattering solution, the shape memory material in the scattering solution deforms and curls when irradiated by sunlight, absorbing and reflecting part of the light, thereby further reducing the sunlight penetrating the display film into the driver's line of sight. In addition, reflective particles and light-absorbing particles are pre-added in the scattering solution to further reduce the sunlight penetrating the display film, thereby preventing or reducing the direct sunlight from entering the driver's eyes in many aspects, and further improving driving safety. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of this application. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings: Figure 1 1 is a schematic diagram of the structure of an in-vehicle head-up display optical film with light scattering function according to Example 1 of the present invention; Figure 2 1 is a schematic diagram of the structure of the vehicle head-up display optical film with light scattering function when it is irradiated by sunlight according to Example 1 of the present invention; Figure 3 Schematic diagram of a scattering portion of an in-vehicle head-up display optical film with a light scattering function according to Embodiment 1 of the present invention; Figure 4 This is a graph showing the repeatability and stability test results of the shape memory function of the scattering portion of the vehicle-mounted head-up display optical film with light scattering function according to Example 1 of the present invention.
[0024] Among them, 1-reflective layer, 2-dynamic scattering layer, 3-scattering part, 4-outer windshield, 5-inner windshield, 6-sealing layer, 7-scattering solution. DETAILED DESCRIPTION
[0025] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with embodiments and drawings. The exemplary embodiments of the present invention and their description are only used to explain the present invention and are not intended to limit the present invention.
[0026] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be an intermediate element at the same time. When an element is referred to as being "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time. When an element is referred to as being "provided with" another element, it may be provided on the surface or inside of the element.
[0027] Unless explicitly stated otherwise, throughout the specification and claims, the term “comprise” or variations such as “include” or “comprising”, etc., will be understood to include the stated elements or components but not to exclude other elements or components.
[0028] The present invention aims to solve the problem that the image recognition of the head-up display in the prior art decreases when encountering sunlight and the driver's vision is blocked, which causes safety hazards. By utilizing the light-sensitive characteristics of the photothermal effect shape memory material and its shape memory function, the present invention provides a vehicle-mounted head-up display optical film with light scattering function and a preparation method thereof, thereby further improving driving safety. The present invention is described below through specific embodiments. Example 1
[0029] This embodiment first provides a vehicle head-up display optical film with a light scattering function, the structure of which is as follows Figure 1 As shown, the optical film includes a dynamic scattering layer 2 and a reflective layer 1, wherein the reflective layer 1 is a wedge-shaped PVB film; the dynamic scattering layer 2 includes a dynamic scattering layer matrix and a scattering portion 3, wherein the scattering portion 3 is a plurality of light scattering points distributed on the dynamic scattering layer matrix, and the scattering portion 3 is made of a thermotropic, force-free, two-way shape memory polymer material, and a heat-inducing agent capable of converting light energy into heat energy is covered on the surface of the scattering portion 3 away from the reflective layer 1, and the scattering portion 3 bulges when exposed to direct sunlight, and returns to its original shape when there is no direct sunlight. The dynamic scattering layer 2 is close to the outer windshield 4, and the reflective layer 1 is close to the inner windshield 5.
[0030] In some embodiments, in order to make the dynamic scattering layer 2 and the reflective layer 1 fit better, the scattering portion 3 is located on the side of the dynamic scattering layer 2 away from the reflective layer 1, and the side of the dynamic scattering layer 2 close to the reflective layer 1 is a plane and fits tightly with the reflective layer 1. The scattering portion 3 is located on the outside close to the windshield, and the reflective layer 1 is located on the inside close to the driver.
[0031] The present invention sets the scattering part 3 of the dynamic scattering layer 2. When the scattering part 3 is exposed to sunlight from the front, it bulges, thereby scattering the sunlight to other directions through the scattering effect of light, preventing or reducing the direct sunlight from entering the driver's eyes. The area and distribution of the shape memory material of the scattering part 3 are very important. If the area is too large, it will affect the driver's vision, and if it is too small, it will not be able to effectively scatter the incident sunlight, and will not achieve a good effect. Figure 3 As shown, the scattering part 3 is a plurality of irregular dots evenly distributed on the base of the dynamic scattering layer. The diameter of the scattering part 3 of the vehicle head-up display optical film of this embodiment is 0.08 mm, and the total area of the scattering part 3 accounts for one half of the area of one side of the scattering dynamic scattering layer 2. The thickness of the scattering part is 0.02 mm, and the thickness of the base of the dynamic scattering layer is 0.03 mm.
[0032] Optionally, the scattering part 3 can be prepared by photothermal effect type shape memory polymer material. The photothermal effect type shape memory polymer material is to introduce photothermal conversion material into the thermotropic force-free two-way shape memory polymer matrix, increase its absorption of light and heat conduction, convert the absorbed light energy into heat energy, and then induce the thermotropic force-free two-way shape memory polymer material to deform, indirectly realizing the photo-induced shape memory property, therefore, it can also be said to belong to the thermotropic shape memory material in essence. The photothermal effect type shape memory polymer material of the scattering part 3 includes a thermogenic agent and a thermotropic force-free two-way shape memory polymer material. When the scattering part 3 is irradiated by sunlight, the thermogenic agent inside it absorbs light and converts the light energy into heat energy, and the thermotropic force-free two-way shape memory polymer material deforms under the action of heat energy, so that the side of the scattering part 3 close to the light shrinks due to heat, and the side away from the light is less deformed or not deformed, so that the material of the scattering part 3 rolls up from all sides to the middle, becoming spherical particles, just scattering the incident sunlight in all directions. Furthermore, the rolled-up scattering portion 3 wraps the thermogenic agent in a smaller space, which is beneficial to the accumulation of heat and the rise of temperature, and further causes the material on the side away from the thermogenic agent, i.e., the surface of the spherical particles, to deform, making the scattering portion 3 more curled and having a better effect on scattering sunlight.
[0033] The thermotropic force-free bidirectional shape memory polymer material of this embodiment can be selected from heat-shrinkable shape memory polymer materials with a thermal response temperature of 0°C-70°C, such as liquid crystal elastomers, cross-linked crystalline polymers and their composite materials. Generally, bidirectional shape memory polymers under force-free conditions can be divided into four categories according to the preparation method: (1) thermoplastic polymers, (2) chemically cross-linked semi-crystalline polymers, (3) liquid crystal polymers, and (4) layered polymer composites. Cross-linked crystalline polymers refer to two interpenetrating network polymers that are interlaced with each other; one of the network polymers is a shape memory polymer of a crystalline cross-linked polymer, and the other network polymer is a cross-linked elastic material. The crystalline cross-linked polymer is one or more of the shape memory polymers of polyurethane, polyethylene, polynorbornene, trans-polyisoprene or styrene-butadiene copolymer; the cross-linked elastic material is one or more of polyurethane elastomer resin, SBS resin, propylene-butylene copolymer, hard rubber or silicone rubber. Among them, polyurethane can also be selected as a shape memory polyurethane material polymerized from three monomer raw materials: polytetramethylene glycol (PTMG), 4,4-diphenylmethane diisocyanate (MDI) and a chain extender. The glass transition temperature Tg is adjusted by adjusting the raw material ratio to obtain shape memory polyurethanes with different response temperatures. For example, display films with different response temperatures can be set according to the city and season of use of the car, such as response temperatures at 25°C, 35°C, 45°C, 55°C, etc. Thermotropic force-free bidirectional shape memory materials can also select polymer materials with bidirectional reversible shape memory effect with a single crystal thermosetting system (CN201510016304.1 Polymer with bidirectional reversible shape memory effect and preparation method thereof). This material uses a high-temperature amorphous phase as a stress phase to achieve reversible shape memory; that is, the low-temperature crystalline phase in the cross-linked system changes with temperature to achieve reversible deformation of the shape, and has a bidirectional memory function of repeatedly memorizing the shapes of two states. The material contains at least one amorphous phase and one crystalline phase, wherein the glass transition temperature of the amorphous phase is higher than the melting temperature of the crystalline phase, and the difference between the two is at least 20°C. This polymer bidirectional reversible shape function can achieve the regulation of the two-phase ratio, crosslinking density, melting temperature of the crystalline phase and glass transition temperature of the amorphous phase under the premise of ensuring that the glass transition temperature of the amorphous phase is higher than the melting temperature of the crystalline phase, so as to meet the needs of different application scenarios. Specifically, a certain amount of polyethylene glycol diacrylate and cyclohexyl methacrylate (where the mass ratio of PEGDA to CMA is 3:1) can be used, benzoyl peroxide (the amount added is 3% of the total mass of the system) can be added, dissolved at 70°C, stirred evenly, poured into a sealed glass tank, and cured at 100°C for 2 to 3 hours. The shape memory function is specifically achieved in the following way: the polymer is heated to 156°C, stretched with a force of 1N, cooled to 56°C under this tension, and the tension is removed. This process is a programmed deformation process.Then continue to cool down to 0℃ and heat up to 56℃. This polymer can repeat the cold extension and heat contraction dual shape memory phenomenon at 0℃~56℃. Thermotropic force-free bidirectional shape memory materials can also use semi-crystalline polymers. Bidirectional shape memory elastomers constructed based on the self-nucleation effect can achieve the differentiation of polymer crystal morphology through the self-nucleation heat treatment procedure, induce the formation of thickened lamellae and original lamellae with different melting points, and make the chemically cross-linked semi-crystalline polymer show excellent bidirectional shape memory behavior under no external force conditions. The principle is as follows: The bidirectional shape memory elastomer is prepared from a semi-crystalline polymer through a chemical cross-linking reaction. During the shape fixing process, the elastomer undergoes a self-nucleation heat treatment process: first, the elastomer is heated to complete melting, then cooled to below the crystallization temperature to form a crystalline phase, and then heated to the self-nucleation temperature. Most of the lamellae in the crystalline phase of the elastomer melt, and the unmelted lamellae are annealed at this temperature. The thickness of the lamellae increases, the crystallization is more perfect, and the melting point is increased, so that an anisotropic structure is formed inside the network. The elastomer is then cooled to below the crystallization temperature. Due to the presence of self-seed crystals, the molten molecular chains can quickly crystallize to form original lamellae. Finally, the bidirectional shape memory elastomer is cyclically heated and cooled without external force to achieve bidirectional reversible deformation. The thickened lamellae are never melted during the subsequent heating process, thus maintaining the differentiation of the internal crystal structure of the bidirectional shape memory elastomer. The coexistence of the two types of lamellae (thickened lamellae and original lamellae) ensures the bidirectional shape memory effect of the bidirectional shape memory elastomer. The specific preparation method is as follows: poly(ε-caprolactone) diacrylate, pentaerythritol tetrakis(3-mercaptopropionate) and triethylamine are dissolved in dimethylformamide, and the first three together constitute a prepolymer; in the mixed solution, the concentration of poly(ε-caprolactone) diacrylate is 0.5 g / ml, and the molar ratio of the double bond in poly(ε-caprolactone) diacrylate to the mercapto group in pentaerythritol tetrakis(3-mercaptopropionate) is 1:1; triethylamine accounts for 10wt% of the total mass of the prepolymer; the mixed solution is transferred to a mold, reacted at 80°C for 8h to complete cross-linking, and after demolding, vacuum dried at 40°C for 24h to obtain a semi-crystalline cross-linked polymer, i.e., an elastomer, whose crystallization temperature is 20°C. Self-nucleation heat treatment procedure: heat the elastomer to 70°C and keep it isothermal for 3 minutes to make it completely melt; apply a constant strain of 10%-97% relative to its original length to the elastomer, and cool it to 10°C at the same time; keep it isothermal for 20 minutes to make the elastomer form a crystalline phase; keep the constant strain, heat it to the self-nucleation temperature (anywhere between 40-45°C), and isothermal anneal for 5 minutes to melt some of the lamellae in the crystalline phase, and thicken the unmelted lamellae to form thickened lamellae; then cool it to 10°C again and keep it isothermal for 20 minutes to make the molten crystallizable segments partially crystallize to form original lamellae, and finally obtain a two-way shape memory elastomer. Characterization of two-way memory behavior: The two-way shape memory elastomer is placed at T. high and T lowThe reversible thermal contraction and cold elongation deformation are achieved by performing a cyclic temperature change program between T and T. (1) The elastomer with a permanent shape A undergoes a self-nucleation thermal program while being pre-stretched and deformed into shape B; (2) The bidirectional shape memory elastomer fixed in shape B is placed at T high (3) placing the bidirectional shape memory elastomer with shape C in a T low In the environment of T, cold elongation is achieved and the shape is transformed into D. (4) high and T low The bidirectional shape memory elastomer can switch reversibly between shape C and shape D by cycling the temperature program between the two-way shape memory elastomer. The temperature range of the self-nucleation temperature is controlled at 40-45℃, T hig The temperature range of h was controlled at 39℃-49℃, T low The temperature range is controlled at 10°C, so that it can respond between 10°C and 49°C. This embodiment can also use polycaprolactone diacrylate prepolymer (PCLDA) with a gradient molecular weight and free radical copolymerization and crosslinking with n-butyl acrylate (BA) to prepare a series of force-free two-way shape memory materials with a wide melting transition. This material achieves the force-free two-way shape memory behavior of the material through stress-induced crystallization and self-nucleation behavior. The thermotropic force-free two-way shape memory material of this embodiment is preferably the above-mentioned polymer material with a single crystal thermosetting system and a two-way reversible shape memory effect. This material phenomenon has a wider range of applications.
[0034] According to the principle of photothermal effect type shape memory, the thermogenic agent should be selected from a material with photothermal effect, and the thermogenic agent is covered on the surface of the scattering portion 3. The thermogenic agent can be selected from any organic photothermal material or inorganic photothermal material, specifically, it can be selected from carbon nanoparticles, carbon nanotubes, carbon black, graphene, graphene oxide, graphite, carbon dots, single atomic gold, Ag nanomaterials, Pt nanoparticles, Al nanoparticles, CuS nanosheets, TiO2 nanoparticles, MoO3 quantum dots, Fe3O4, indocyanine green, Prussian blue, thiadiazole derivatives and porphyrin rings. Among them, single atomic gold refers to a nanomaterial composed of a single gold atom, which has unique photothermal effect characteristics due to its special structure and electronic properties. This is mainly due to its surface plasmon resonance (SPR). When light is irradiated to the surface of single atomic gold, its surface plasma oscillation is excited, thereby absorbing light energy and converting it into heat energy, so that the surface temperature of single atomic gold increases. Since the size of single atomic gold is very small and its surface area is very large relative to its volume, the photothermal effect is very strong. The photothermal conversion efficiency of different thermogenic agents is different. Taking the nano-photothermal materials of Jiangsu Xianfeng Nanomaterials Technology Co., Ltd. as an example, Table 1 is a comparison of the performance parameters of Xianfeng's multiple product series.
[0035] Table 1 Parameters of photothermal conversion materials of Jiangsu Xianfeng Nanomaterial Technology Co., Ltd. Product Number Product Name Temperature rise (measured data) XFK01 Titanium carbide (Ti3C2Tx) MXene multilayer nanosheets 52℃ XFK41-1 Titanium Carbide (Ti3C2Tx) MXene Nanosheets 52℃ XF019-1 Single-layer graphene dispersion 60℃ XFM01 Multi-walled carbon nanotubes 52℃ XFS22 Ultra-high purity single-walled carbon nanotubes with large specific surface area 56℃ XFD01 Double-walled carbon nanotubes 52℃ XFP03 Ordered mesoporous carbon CMK-3 41℃ XFP12 Mesoporous Carbon Spheres 38℃ XF207 Black phosphorus nanosheet dispersion 40℃ XF283 Purple Phosphorus Crystal Powder 42℃ The thermogenic agent used in the scattering part 3 of this embodiment is the XFS22 product of Jiangsu Xianfeng Nanomaterial Technology Co., Ltd., that is, ultra-high purity single-walled carbon nanotubes with large specific surface area. In order to improve the photothermal conversion efficiency of the thermogenic agent, the incident sunlight is converted into thermal energy as quickly as possible to drive the thermotropic force-free two-way shape memory material to deform, thereby reducing the time the driver is affected by the sunlight. In this embodiment, the thermogenic agent is covered on the surface of the scattering part 3 close to the front of the car, so that the thermogenic agent is densely distributed on the illuminated side, so that the heat generated by the thermogenic agent after absorbing light is locked on the surface of the illuminated side of the scattering part 3, so that the surface of the illuminated side of the scattering part 3 is quickly heated to the thermal response temperature without heating the scattering part 3 as a whole, so as to improve the photothermal conversion efficiency, generate and accumulate more heat faster, and improve the response speed of the display film to light. The larger the specific surface area of the thermogenic agent, the higher the photothermal conversion efficiency. The more thermogenic agent, the greater the heat generated. The particle size of the thermogenic agent in this embodiment is 1nm-50nm. In practical applications, the amount of thermogenic agent added can be controlled according to specific circumstances. The more thermogenic agent added, the higher the photothermal conversion efficiency and speed. However, it may also bring about the problem of transmittance, which needs to be reasonably designed according to actual conditions. However, in general, the transmittance of the dynamic scattering layer should not be less than 70%. The thermogenic agent of the scattering part 3 of this embodiment selects carbon nanotubes.
[0036] The shape memory repeatability and stability test of the scattering part 3 prepared in this embodiment are as follows: Figure 4 As shown. Specifically, by designing the experiment, a temperature monitoring device, such as a thermometer, a temperature sensor, etc., and a stress gauge are set at the scattering part 3, and the same scattering part 3 sample is placed in sunlight for different durations of continuous irradiation, and the temperature changes at different durations are recorded. The stress changes of the optical film sample at different temperatures are observed to evaluate the stability of the shape memory effect. As can be seen from the figure, after multiple irradiations, the scattering part 3 can be repeatedly curled and stretched between 0°C and 56°C to achieve light scattering with good performance stability. The temperature changes of the scattering part 3 under different irradiation durations are shown in Table 2. Since the sun is higher at noon, the sunlight generally does not directly hit the driver's eyes, so this embodiment uses sunlight at nine o'clock in the morning or four o'clock in the afternoon for the experiment.
[0037] Table 2 Temperature changes of the scattering part under different irradiation time Irradiation time / s 10 50 100 200 300 400 500 600 Scattering part temperature rise / ℃ 2 4 7 10 16 26 39 55 In order to further enhance the light scattering effect, in some embodiments, the entire dynamic scattering layer 2 can be provided with uniformly dispersed light-absorbing particles and light-reflecting particles to absorb and reflect part of the light. That is to say, the scattering part 3 and the main body of the dynamic scattering layer substrate can be provided with uniformly dispersed light-absorbing particles and light-reflecting particles. When the scattering part 3 is irradiated by sunlight, the side irradiated by sunlight, due to the limited irradiation depth of light, the light irradiates on the surface of the scattering part 3, and the surface pyrogen quickly absorbs light energy and converts it into heat energy, and transmits it to the thermotropic type no external force two-way shape memory polymer of the scattering part 3, so that the material close to the pyrogen side shrinks first, while the deformation of the unirradiated side is small or remains unchanged, and the shrinkage tension of the shrinking side pulls the material of the holding side to roll up, so that the entire scattering part 3 curls up to form a spherical structure. At this time, the curled scattering part 3 will scatter the sunlight in all directions, and the light-absorbing particles and light-reflecting particles in the scattering part 3 will also absorb and reflect part of the sunlight, which reduces the sunlight entering the driver's eyes in two aspects and reduces the impact of sunlight on the driver.
[0038] In order to further enhance the light scattering effect, in some embodiments, a scattering solution 7 is encapsulated in the dynamic scattering layer matrix, and the scattering solution 7 is a solution of a thermotropic force-free bidirectional shape memory polymer material. The thermotropic force-free bidirectional shape memory polymer material is cut into filaments with a diameter of 10μm-20μm and uniformly dispersed in its plasticizer.
[0039] When there is no sunlight, the scattering solution 7 is a transparent system. When exposed to sunlight, the thermotropic force-free two-way shape memory polymer in the scattering solution 7 curls up to become light-absorbing particles or light-reflecting particles uniformly dispersed in the solution 7, so that the scattering solution 7 becomes a stable colloidal solution. When there is no sunlight, the thermotropic force-free two-way shape memory material fully stretches in the solution under the action of the plasticizer. The scattering solution 7 is a transparent system. When exposed to sunlight, the thermogenic agent in the solution absorbs light intensity, converts light into heat energy, and transfers heat to the thermotropic force-free two-way shape memory material, so that the thermotropic force-free two-way shape memory material curls up to become light-absorbing particles or light-reflecting particles, which are uniformly dispersed in the colloidal solution under the action of the dispersant. The shape memory material in the scattering solution 7 can be phase-separated when exposed to sunlight, and the formed light-absorbing particles or light-reflecting particles can be used to absorb and reflect part of the light, thereby further reducing the sunlight penetrating the display film into the driver's line of sight.
[0040] It should be understood that the above-mentioned thermotropic force-free bidirectional shape memory material is a material that has been prepared and shaped in advance in this embodiment, and can be directly applied to the scattering part 3 or the scattering solution 7 of this embodiment.
[0041] The selection of photothermal effect shape memory polymer material in the scattering solution 7 of the dynamic scattering layer 2 is the same as the selection of photothermal effect shape memory polymer material in the scattering part 3. The composition of the scattering solution 7 includes 39.4% thermotropic force-free two-way shape memory material, 0.6% thermogenic agent, 50% plasticizer, 6% dispersant, and 4% defoaming agent. The thermogenic agent of this embodiment selects single atomic gold. The selection of the thermogenic agent here is consistent with the selection of the thermogenic agent of the scattering part 3. Graphite, carbon nanoparticles, carbon nanotubes, etc. can also be selected. The thermotropic force-free two-way shape memory polymer material can select any polymer material that is sensitive to heat, shrinks when heated, and is soluble. As a component of the dynamic scattering layer 2, the thermotropic force-free two-way shape memory polymer material needs to be added with a thermogenic agent, that is, a photothermal material, to convert light energy into heat energy. The thermotropic force-free two-way shape memory material deforms under the action of heat energy and forms a stable colloidal solution under the action of the dispersant.
[0042] In order to further enhance the reflection of sunlight, the dynamic scattering layer 2 is uniformly dispersed with light absorbing material particles and light reflecting material particles, so that the dynamic scattering layer 2 itself has a part of light scattering function.
[0043] Accordingly, this embodiment also provides a method for preparing a vehicle head-up display optical film with a light scattering function, comprising the following steps: Dynamic scattering layer 2 preparation First, prepare the dynamic scattering layer substrate: S1: Provide the above-mentioned thermotropic force-free bidirectional shape memory polymer material, process it into a filament with a diameter of 10μm-20μm, add 39.4% of the above-mentioned treated thermotropic force-free bidirectional shape memory polymer material into 50% of plasticizer, then add 6% of dispersant, 0.6% of carbon nanoparticle heat agent, and 4% of defoamer in sequence, and stir at the dissolution temperature until it is completely dissolved into a transparent and stable scattering solution 7; the dispersant can be selected from metal soap dispersants, such as metal salts of higher fatty acids, called metal soaps, such as barium stearate (BaSt), zinc stearate (ZnSt), calcium stearate (CaSt) and other stearic acid soaps such as cadmium stearate (CdSt), magnesium stearate (MgSt), copper stearate (CuSt), etc. The defoamer can be selected from alcohols, fatty acids and fatty acid esters, amides, phosphates, silicones, polyethers, polyether-modified polysiloxane defoamers, etc.;
[0044] S2: Encapsulate the scattering solution 7 in a transparent sealing layer 6, and the scattering solution 7 completely fills the transparent sealing layer 6 to form a dynamic scattering layer matrix; in order to prevent bubbles from affecting the line of sight, it is necessary to ensure that the scattering solution 7 completely fills the sealing layer 6, so that the appearance of the entire dynamic scattering layer matrix is a uniform and transparent structure. The sealing layer 6 here can be a transparent hard material or a transparent soft material. For the soft sealing layer 6, in the next step when it is bonded with the reflective layer 1, attention should be paid to the flatness and the liquid in the sealing layer 6 should be evenly bonded to the reflective layer 1 and not deformed when the entire display film stands up after bonding. The sealing layer uses PVB resin as the main material;
[0045] Then the dynamic scattering layer 2 is prepared; S3: providing the above-mentioned thermotropic force-free bidirectional shape memory polymer material, heating the thermotropic force-free bidirectional shape memory polymer material to a flowing or semi-flowing state, stirring it evenly, obtaining a stable liquid scattering part, laying the dynamic scattering layer substrate prepared in step S2 flat, laying a layer of transparent adhesive film on the dynamic scattering layer substrate, the adhesive film is a mixture of a thermoplastic material and a plasticizer, the thermoplastic material is PVB, applying the liquid scattering part on the surface of the adhesive film according to the distribution of scattering points of the scattering part 3, and then applying the liquid scattering part on the surface of the scattering part 3 after the point coating. Place a plurality of carbon nanotubes, and place the dynamic scattering layer substrate at room temperature until the liquid scattering part 3 cools down and is bonded to the dynamic scattering layer substrate to form a dynamic scattering layer 2; carbon nanotubes are selected as the thermogenic agent here, and in order to improve the light-to-heat conversion efficiency, the carbon nanotubes are arranged on the surface of the scattering part 3. For the thermogenic agent in granular or powder form, the thermogenic agent can be directly covered on the surface of the scattering part 3 by scattering. This step should be performed before the liquid scattering part is solidified, so that the thermogenic agent and the liquid scattering part are solidified together to prevent the thermogenic agent from falling. The thermogenic agent addition ratio of the scattering part 3 is 0.4%.
[0046] B. Preparation of optical display film S4: a polyvinyl butyral (PVB) film is used as the reflective layer 1, and is flatly attached to a platform and placed in a vacuum environment. Then, the dynamic scattering layer 2 prepared in step S3 is pressed onto the reflective layer 1, and each area of the dynamic scattering layer 2 is pressed so that the reflective layer 1 and the dynamic scattering layer 2 are tightly attached and free of bubbles or impurities. Vacuum heating is turned on to fully bond the reflective layer 1 and the dynamic scattering layer 2. A certain pressure can be applied when necessary. When applying pressure, it is ensured that the structure of the dynamic scattering layer 2 is not damaged, so as to obtain the vehicle-mounted head-up display optical film.
[0047] The preparation method of the wedge-shaped polyvinyl butyral (PVB) film can adopt the existing disclosed technology, and the specific process is as follows: adopt a hot pressing molding process, including the following steps: S1, sandwich the PVB raw material between two protective films and then put it into a preheated mold; or, first place the first protective film of the two protective films in the preheated mold, then place the PVB raw material on the first protective film, and finally place the second protective film of the two protective films on the PVB raw material; wherein, the material of the two protective films can be a material with a certain hardness relative to the softened PVB film, and the material can be a non-stick coating coated or sprayed on a high-temperature resistant substrate. Preferably, the material can be a glass fiber substrate and a Teflon coating. The thickness of the two protective films can be 0.1 to 1 mm, respectively, and the thickness of the two protective films can preferably be 0.1 to 0.25 mm, respectively. S2, close the mold; S3, pressurize and heat the mold until the required temperature is reached. The pressure range of this step can be 10 to 100 MPa, and the pressure range can preferably be 20 to 30 MPa. The time for heating to the required temperature is 20 to 180 seconds, and the required time is preferably 60 to 120 seconds. S4 takes out the formed PVB film together with the two protective films; S5 cools the formed PVB film; S6 peels off the two protective films to obtain the PVB film for HUD. Among them, the cross-sectional shape of the obtained PVB film for HUD in one direction can be wedge-shaped. That is, the obtained PVB film can be wedge-shaped in cross-sectional shape in one direction like the PVB film obtained by the extrusion molding process. Preferably, the cross-sectional shape of the obtained PVB film for HUD in one direction is wedge-shaped.
[0048] It is worth noting that the “providing” in this embodiment may be any method of obtaining the target material, such as preparation, procurement, customization, etc.
[0049] In step S3, the photothermal effect type shape memory polymer material of the scattering part 3 is formed into a flat shape under ordinary light, and after being bonded with the reflective layer 1 to form a head-up display film, it is installed on the car. In actual use, when sunlight shines on the display film in front of the car, Figure 2As shown, one side of the scattering part 3 of the dynamic scattering layer 2 is irradiated by sunlight. Due to the limited irradiation depth of light, the photothermal effect type shape memory polymer material on the side of the dynamic scattering layer 2 facing the sunlight absorbs sunlight through the carbon nanoparticle heat agent under the action of sunlight and converts it into heat energy. The heat energy is transferred to the thermotropic type force-free two-way shape memory polymer material, causing the thermotropic type force-free two-way shape memory polymer material to shrink and deform, while the deformation of the unirradiated side is smaller or remains unchanged, so that the entire scattering part 3 curls up to form a spherical structure. At this time, the curled scattering part 3 will scatter sunlight in all directions, and the light-absorbing particles and light-reflecting particles in the scattering part 3 will also absorb and reflect part of the sunlight, reducing the sunlight entering the driver's eyes in both aspects and reducing the impact of sunlight on the driver. When the sunlight disappears, the photothermal effect type shape memory polymer material of the scattering part 3 is not irradiated by sunlight, and the heat energy is reduced and restored to its original state, and the scattering part 3 returns to its initial flat state.
[0050] Furthermore, in order to make the dynamic scattering layer 2 itself have a part of light scattering function, the above step S1 further includes: The light-absorbing material particles and the light-reflecting material particles are ball-milled in a ball mill at a speed of 3000-5000 r / min for 30-60 min, and the scattering solution 7 is added.
[0051] When the head-up display optical display film of this embodiment is used, the prepared head-up display optical display film is set between the outer windshield 4 and the inner windshield 5 of the front windshield of the car, and it is ensured that it is pressed flat and there are no bubbles or impurities between the layers to ensure a good field of vision for the driver. Example 2
[0052] In this embodiment, based on the embodiment 1, the amount of the heat-generating agent added to the scattering part 3 is adjusted, and the proportion of the heat-generating agent added to the scattering part 3 is 0.8%. Example 3
[0053] In this embodiment, on the basis of the embodiment 1, the amount of the heat-generating agent added to the scattering part 3 is adjusted, and the addition ratio of the heat-generating agent to the scattering part 3 is 0.2%. Example 4
[0054] In this embodiment, on the basis of the embodiment 1, the amount of the heat-generating agent added to the scattering part 3 is adjusted, and the proportion of the heat-generating agent added to the scattering part 3 is 0.6%.
[0055] The present invention sets different experiments, adjusts the amount of heat-generating agent added to the scattering part 3 and the irradiation time, and sets a blank experiment. The blank experiment uses an ordinary PVB display film without a dynamic scattering part 3 as a blank sample. The display films obtained by the formulas of Example 1, Example 2, Example 3 and Example 4 and the ordinary PVB display film are respectively installed in the front windshield of the car, and irradiated with sunlight from a fixed distance, and the light signal is received at the position of the driver's eyes. The same optical film sample is repeatedly irradiated with sunlight and stopped irradiation, and the transmittance of the optical film sample under different parameters is observed. The comparative experimental results are as follows: Table 3 Effect of scattering solution formula on total transmittance of display film Shape memory polymer materials / % Plasticizer / % Pyrogenic agent / % Dispersant / % Defoaming agent / % Amount of heat-generating agent added to the scattering part / mm Total light transmittance / & Example 1 39.4 50 0.6 6 4 0.4 80 Example 2 39.4 50 0.6 6 4 0.8 60 Example 3 39.4 50 0.6 6 4 0.2 90 Example 4 39.4 50 0.6 6 4 0.6 75 From the comparative data in Table 3, it can be seen that the more the shape memory material is added, the better. If too much is added, the polymer will easily form blocks after shrinking under light, and cannot be well dispersed in the solution, and the light scattering effect will be greatly reduced. If the amount added is too little, it will not be able to form enough particles, and the light scattering effect will not be ideal. The more the amount of heat-generating agent added to the scattering part 3, the better. Too much heat-generating agent will affect the light transmittance of the entire film. Therefore, the best embodiment should be embodiment 4. Example 5
[0056] In this embodiment, based on the first embodiment, the diameter of the scattering part 3 of the vehicle head-up display optical film is 1 mm, and the total area of the scattering part 3 accounts for half of the area of one side of the dynamic scattering layer 2 . Example 6
[0057] In this embodiment, based on the fourth embodiment, the diameter of the scattering part 3 of the vehicle head-up display optical film is 0.5 mm, and the total area of the scattering part 3 accounts for two-thirds of the area of one side of the dynamic scattering layer 2 .
[0058] The display films obtained by the formulations of Example 4, Example 5 and Example 6 were installed in the front windshield of the car, and the sunlight was irradiated from a fixed distance, and the light signal was received at the position of the driver's eyes. The comparative experimental results are as follows: Table 4 Effect of scattering diameter and area on total light transmittance of display film Scattering diameter / mm Scattering area ratio Total light transmittance Example 4 0.8 One-half 80% Example 5 1 One-half 88% Example 6 0.5 Two-thirds 78% It can be seen from the comparative data in Table 4 that the setting of the scattering part 3, such as the diameter and total area ratio of the scattering part 3, has a great influence on the transmittance of the display film. The scattering part 3 has a large point diameter and is sparsely distributed, and the lower the scattering effect, the higher the total transmittance. The scattering part 3 has a small diameter and is densely distributed, and the total transmittance of the display film is low, and the anti-glare effect is better. Therefore, the best design of the scattering part 3 should be Example 6, the diameter of the scattering part 3 is 0.5 mm, and the total area of the scattering part 3 accounts for two-thirds of the area of one side of the dynamic scattering layer 2.
[0059] In the description of the present invention, it is necessary to understand that the terms "up", "down", "front", "back", "left", "right", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.
[0060] Finally, it should be pointed out that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit them. Although the present invention has been described in detail with reference to the above embodiments, a person skilled in the art should understand that the technical solutions described in the above embodiments can still be modified, or some of the technical features can be replaced by equivalents, and these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A vehicle head-up display optical film with light scattering function, characterized in that: The optical film comprises a dynamic scattering layer and a reflective layer, wherein the reflective layer is a mixture of a thermoplastic material and a plasticizer, and the reflective layer is wedge-shaped; the dynamic scattering layer comprises a dynamic scattering layer substrate and a scattering portion, wherein the scattering portion is located on a side of the dynamic scattering layer away from the reflective layer, and a side of the dynamic scattering layer close to the reflective layer is a plane and is closely attached to the reflective layer; The scattering part is a plurality of light scattering points distributed on the matrix of the dynamic scattering layer. The scattering part is made of a thermotropic, force-free, bidirectional shape memory polymer material. A thermogenic agent capable of converting light energy into heat energy is covered on the surface of the scattering part away from the reflective layer. The scattering part bulges when exposed to direct sunlight and returns to its original shape when there is no direct sunlight.
2. The vehicle-mounted head-up display optical film with light scattering function according to claim 1, characterized in that: The thermoplastic resin is PVB.
3. The vehicle-mounted head-up display optical film with light scattering function according to claim 1, characterized in that: The dynamic scattering layer matrix encapsulates a scattering solution, which is a solution of a thermotropic force-free two-way shape memory polymer. The scattering solution is a transparent system when there is no sunlight. When exposed to sunlight, the thermotropic force-free two-way shape memory polymer in the scattering solution curls.
4. The vehicle-mounted head-up display optical film with light scattering function according to claim 1, characterized in that: The light transmittance of the dynamic scattering layer is not less than 70%.
5. The vehicle-mounted head-up display optical film with light scattering function according to claim 3, characterized in that: The scattering solution comprises 30%-50% of a thermotropic force-free bidirectional shape memory material, 0.2%-0.8% of a thermogenic agent, 40%-50% of a plasticizer, 5%-6% of a dispersant, and 3%-4% of a defoaming agent.
6. The vehicle-mounted head-up display optical film with light scattering function according to claim 1, characterized in that: The pyrogen is selected from at least one of carbon nanoparticles, carbon nanotubes, carbon black, graphene, graphene oxide, graphite, carbon dots, single atomic gold, Ag nanomaterials, Pt nanoparticles, Al nanoparticles, CuS nanosheets, TiO2 nanoparticles, MoO3 quantum dots, Fe3O4, indocyanine green, Prussian blue, thiadiazole derivatives and porphyrin rings.
7. The method for preparing the vehicle-mounted head-up display optical film with light scattering function according to claim 1, characterized in that: The following steps are involved: S1: providing the thermotropic force-free bidirectional shape memory polymer material, processing it into a filament with a diameter of 10 μm-20 μm, taking 30%-50% of the processed thermotropic force-free bidirectional shape memory polymer material and adding it to 40%-50% of a plasticizer, and then sequentially adding 5%-6% of a dispersant, 0.2%-0.8% of a thermogenic agent, and 3%-4% of a defoaming agent, and stirring to a homogeneous scattering solution; S2: encapsulating the scattering solution in a transparent sealing layer, wherein the scattering solution completely fills the sealing layer to form a dynamic scattering layer matrix; S3: providing the thermotropic force-free bidirectional shape memory polymer material, heating it to a flowing or semi-flowing state, stirring it evenly to obtain a stable liquid scattering part, laying the dynamic scattering layer substrate flat, laying a layer of transparent adhesive film on the dynamic scattering layer substrate, applying the liquid scattering part on the surface of the adhesive film according to the distribution of scattering points of the scattering part, and then covering the surface of the applied scattering part with a layer of thermogenic agent, placing the dynamic scattering layer substrate at room temperature and standing until the liquid scattering part is cooled and fixed and adhered to the dynamic scattering layer substrate to form a dynamic scattering layer; S4: A wedge-shaped polyvinyl butyral (PVB) film is used as a reflective layer and is flatly attached to a platform and placed in a vacuum environment. The dynamic scattering layer prepared in step S3 is then laminated onto the adhesive film. Each area of the dynamic scattering layer is pressed so that the reflective layer is tightly attached to the dynamic scattering layer without bubbles or impurities, thereby obtaining the vehicle-mounted head-up display optical film.
8. The preparation method according to claim 7, characterized in that: The adhesive film in step S3 is a mixture of a thermoplastic material and a plasticizer.
9. The preparation method according to claim 8, characterized in that: The thermoplastic material is PVB.
10. The preparation method according to claim 9, characterized in that: The diameter of the scattering part of the vehicle-mounted head-up display optical film is 0.05mm-0.1mm, and the total area of the scattering part accounts for one third to two thirds of the area of one side of the scattering dynamic scattering layer.
Citation Information
Patent Citations
Active material based bodies for varying surface texture and frictional force levels
CN101368663A
Antiglare sticking layer and manufacturing process
CN107573860A
Thermochromic polyvinyl butyral (PVB) or ethylene-vinyl acetate (EVA) film
CN109880553A
Vehicle-mounted head-up display film and vehicle-mounted head-up display system
CN117348121A
Optical film, optical film manufacturing method, polarizing plate, and liquid crystal display device
JP2009157323A