Laminated ceramic electronic device and method for manufacturing same

By designing ridge parts and side edge parts with specific curvature radii in the protective part of the laminated ceramic electronic device, and forming a base film and a coating film in the external electrode, the problem of poor buffering effect of traditional side parts during impact is solved. Improved the impact resistance reliability and stability of the device.

CN118737700APending Publication Date: 2024-10-01TAIYO YUDEN KK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410374309.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-29
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The sides of conventional laminated ceramic electronic devices have a lower cushioning effect against external impacts, resulting in reduced reliability.

Method used

A laminated ceramic electronic device is designed, the protective part of which includes a ridge part and a side edge part with a specific curvature radius, the first ridge part and the second ridge part are formed by chamfering, and a base is formed in the external electrode Film and coating to cover the end face, sides and recessed parts to ensure that the impact force can be effectively dispersed during impact.

Benefits of technology

It improves the impact resistance reliability of laminated ceramic electronic devices, reduces the incidence of cracks, and enhances the stability and reliability of capacitors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737700A_ABST
    Figure CN118737700A_ABST
Patent Text Reader

Abstract

A laminated ceramic electronic device includes a ceramic element body. The functional portion includes a plurality of internal electrodes stacked in a second direction perpendicular to the first direction. The protective portion includes a covering portion stacked on the functional portion in the second direction, and a side edge portion covering the functional portion in a third direction perpendicular to the first direction and the second direction. The ridge portion includes a first ridge line portion located on the cover portion side and a second ridge line portion located on the side edge portion side, and the recessed portion is interposed between the first ridge line portion and the second ridge line portion. In a cross section including the second direction and the third direction, the radius of curvature R1 of the first ridge line portion is larger than the radius of curvature R2 of the second ridge line portion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a laminated ceramic electronic device and a method for manufacturing the laminated ceramic electronic device. Background Art

[0002] A stacked ceramic electronic device (e.g., a stacked ceramic capacitor) may include a functional portion and a protective portion disposed on the side of the functional portion. The functional portion is formed by alternating a plurality of dielectric layers and a plurality of internal electrodes. A plurality of internal electrodes are exposed on the side of the functional portion. The protective portion disposed on the side of the functional portion is called a side section or a side margin section, and covers the internal electrodes exposed from the side. Conventionally, a structure has been proposed in which the side section is disposed on the side of the functional portion, and the angle between the side section and the imaginary line connecting the end of the internal electrode is less than 90 degrees (e.g., see Japanese Patent Application Publication No. 2012-191159, hereinafter referred to as Patent Document 1). Patent Document 1 points out that, with this structure, a stacked ceramic electronic device with excellent reliability can be provided. Summary of the invention

[0003] According to one aspect of the embodiment, a stacked ceramic electronic device is provided, comprising: a ceramic component body, which includes a protection portion and a functional portion located inside the protection portion, the protection portion including an end face facing a first direction, a plurality of peripheral faces adjacent to the end face and extending along the first direction, and an edge portion having a recess extending along the first direction and connecting the plurality of peripheral faces; and an external electrode, which includes a base film covering the end face and a plating film formed on the base film, wherein the functional portion includes a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, wherein the protection portion includes a covering portion stacked on the functional portion in the second direction and a side edge portion covering the functional portion in a third direction perpendicular to the first direction and the second direction, wherein the edge portion includes a first ridge portion located on one side of the covering portion and a second ridge portion located on one side of the side edge portion, the recess portion is located between the first ridge portion and the second ridge portion, and wherein, in a cross section including the second direction and the third direction, a curvature radius R1 of the first ridge portion is greater than a curvature radius R2 of the second ridge portion.

[0004] According to another aspect of the embodiment, a method for manufacturing a stacked ceramic electronic device is provided, the method comprising: forming a ceramic stacked chip having an end face facing a first direction, a functional portion and a covering portion, the functional portion having a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, the plurality of internal electrodes being exposed on the side of the ceramic stacked chip facing a third direction perpendicular to the first direction and the second direction, the covering portion being stacked on the functional portion along the second direction, forming a first ridge portion adjacent to the end face, which connects the peripheral surface and the side face extending along the first direction; forming a side edge portion, thereby forming a ceramic component body, the side edge portion being stacked on the side face and extending along the first direction, and having a second ridge portion, the second ridge portion being parallel to the first ridge portion and having a recess therebetween; firing the ceramic stacked chip and the side edge portion; and forming an external electrode, which comprises a base film covering the end face and a plating film formed on the base film, wherein the formation of the first ridge portion comprises a chamfering process, wherein in a cross section including the second direction and the third direction, a radius of curvature R1 of the first ridge portion is greater than a radius of curvature R2 of the second ridge portion.

[0005] According to another aspect of the embodiment, a method for manufacturing a stacked ceramic electronic device is provided, the method comprising: forming a ceramic component body having an end face facing a first direction, a functional portion, a covering portion, a side edge portion, a peripheral surface extending along the first direction, and an edge portion connecting the peripheral surface, the functional portion having a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, the plurality of internal electrodes being exposed on the side of the ceramic component body facing a third direction perpendicular to the first direction and the second direction, the covering portion being stacked on the functional portion along the second direction, and the side edge being stacked on the side along the third direction; firing the ceramic component body; forming in the edge portion a first edge line portion having a curvature radius R1 in a cross section including the second direction and the third direction, and a second edge line portion having a curvature radius R2 smaller than the curvature radius R1 in the above cross section, with a recess being between the first edge line portion and the second edge line portion; and forming an external electrode comprising a base film covering the end face and a plating film formed on the base film. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] Figure 1 It is a three-dimensional diagram of a stacked ceramic capacitor;

[0007] Figure 2 is along Figure 1 A cross-sectional view taken along the line A-A';

[0008] Figure 3 is along Figure 1 A cross-sectional view taken along the line BB' in FIG.

[0009] Figure 4 is along Figure 1 The cross-sectional view taken along the line C-C' in FIG.

[0010] Figure 5 Show Figure 4 A magnified image of

[0011] Fig. 6A A curvature radius of a laminated ceramic capacitor according to an embodiment and a measurement position of the curvature radius are shown;

[0012] Figure 6B The radius of curvature and the method for measuring the radius of curvature are shown;

[0013] Figure 6C Shows the radius of curvature and another method of measuring the radius of curvature;

[0014] Fig. 7A A partially enlarged cross-sectional view showing a first ridgeline portion and a second ridgeline portion of a multilayer ceramic capacitor according to an embodiment;

[0015] Figure 7B A partially enlarged cross-sectional view showing a first ridgeline portion and a second ridgeline portion of a multilayer ceramic capacitor of a comparative example;

[0016] Fig. 8A The figure shows an angle θ1 between a tangent line connecting the first ridgeline portion and the second ridgeline portion and a line extending along the Y-axis direction from the main surface of the ceramic element body, and a height t1 from the mounting surface to the second ridgeline portion in a multilayer ceramic capacitor according to an embodiment;

[0017] Figure 8B The figure shows the angle θ2 between the tangent line connecting the first ridgeline portion and the second ridgeline portion and the line extending along the Y-axis direction from the main surface of the ceramic element body, and the height t2 from the mounting surface to the second ridgeline portion in the multilayer ceramic capacitor of the comparative example;

[0018] Fig. 9 A flow chart showing a method of manufacturing a laminated ceramic capacitor;

[0019] Fig.10 A perspective view showing a method for manufacturing a laminated ceramic capacitor;

[0020] Fig.11 A perspective view showing a method for manufacturing a laminated ceramic capacitor;

[0021] Fig.12 A perspective view showing a method for manufacturing a laminated ceramic capacitor;

[0022] Fig.13 A schematic cross-sectional view showing a method for manufacturing a laminated ceramic capacitor;

[0023] Fig.14 A schematic cross-sectional view showing a method for manufacturing a laminated ceramic capacitor;

[0024] Fig.15A schematic cross-sectional view showing a method for manufacturing a laminated ceramic capacitor;

[0025] Fig.16 A perspective view showing a method for manufacturing a laminated ceramic capacitor;

[0026] Fig.17 A perspective view showing a method of manufacturing a laminated ceramic capacitor; and

[0027] Fig.18 A graph showing the crack occurrence rates in the impact test of Examples and Comparative Examples is shown. DETAILED DESCRIPTION

[0028] However, in the configuration described in Patent Document 1, the side portion becomes thinner toward the edge of the internal electrode in the lamination direction. Therefore, it is conceivable that the buffering effect of the side portion against external impact is reduced.

[0029] Embodiments of the present invention will be described below with reference to the accompanying drawings. In the accompanying drawings, X-axis, Y-axis and Z-axis perpendicular to each other are appropriately shown. X, Y and Z axes are common in all the drawings. The X-axis direction corresponds to the first direction, the Y-axis direction corresponds to the third direction, and the Z-axis direction corresponds to the second direction.

[0030] [Overall Structure of Multilayer Ceramic Capacitor 10]

[0031] Figures 1 to 4 1 is a schematic diagram of a multilayer ceramic capacitor 10 according to a first embodiment of the present invention. Figure 1 1 is a perspective view of the multilayer ceramic capacitor 10 . Figure 2 is along Figure 1 1 is a cross-sectional view of the multilayer ceramic capacitor 10 taken along line AA′ in FIG. Figure 3 is along Figure 1 BB′ line in FIG. 1 is a cross-sectional view of the multilayer ceramic capacitor 10 . Figure 4 is along Figure 1 1 is a cross-sectional view of the multilayer ceramic capacitor 10 taken along the line CC′ in FIG.

[0032] The multilayer ceramic capacitor 10 includes a ceramic element body 11 and two external electrodes 14 a and 14 b. The two external electrodes 14 a and 14 b are formed on the surfaces of the ceramic element body 11, respectively.

[0033] The ceramic element body 11 has a capacitor part 16 and a protection part 17. The protection part 17 constitutes the outer periphery of the ceramic element body 11, which includes two end faces 11a facing the X-axis direction, two side faces 11b facing the Y-axis direction, two main faces 11c facing the Z-axis direction, and an edge 11e connecting the main faces 11c and the side faces 11b. In this embodiment, the side faces 11b and the main faces 11c constitute a plurality of peripheral faces. The end faces 11a, the side faces 11b, and the main faces 11c are, for example, substantially flat faces, but may also be circular.

[0034] Specifically, the protection portion 17 includes a cover portion 18 located outside the capacitor portion 16 in the Z-axis direction, a side edge portion 19 located outside the capacitor portion 16 in the Y-axis direction, and an end edge portion 20 located outside the capacitor portion 16 in the X-axis direction.

[0035] The capacitor section 16 is provided inside the protection section 17 and constitutes a functional section in this embodiment. In the capacitor section 16, a plurality of first internal electrodes 12 and a plurality of second internal electrodes 13 are stacked in the Z-axis direction via ceramic layers 15 (see FIG. 1 ). Figure 2 ). The internal electrodes 12 and 13 are both sheet-shaped, extend along the XY plane, and are alternately arranged along the Z-axis direction.

[0036] The internal electrodes 12, 13 are each made of a good electrical conductor and serve as the internal electrodes of the laminated ceramic capacitor 10. The good electrical conductor forming the internal electrodes 12, 13 is, for example, a metal whose main component is an alloy such as nickel (Ni), copper (Cu), palladium (Pd), platinum (Pt), silver (Ag), gold (Au), or the like.

[0037] like Figure 2 As shown, for example, the first internal electrode 12 is led out to one end surface 11a of the ceramic element body 11 and connected to the external electrode 14a. The second internal electrode 13 is led out to the other end surface 11a and connected to the external electrode 14b.

[0038] The ceramic layer 15 is formed of a dielectric ceramic. In the laminated ceramic capacitor 10, a dielectric ceramic having a high dielectric constant is used to increase the capacitance of each ceramic layer 15 between the internal electrodes 12, 13. Examples of high dielectric constant dielectric ceramics include those having a perovskite structure containing barium (Ba) and titanium (Ti), represented by barium titanate (BaTiO3).

[0039] In addition to barium titanate, the dielectric ceramics mentioned above can also be, for example, strontium titanate (SrTiO3), calcium titanate (CaTiO3), magnesium titanate (MgTiO3), calcium zirconate (CaZrO3), calcium zirconate titanate (Ca(Zr,Ti)O3), barium zirconate (BaZrO3) or titanium oxide (TiO2), etc.

[0040] The protection portion 17 is also formed of dielectric ceramic. The material forming the protection portion 17 may be any insulating ceramic, but using the same material as the ceramic layer 15 can improve manufacturing efficiency and suppress internal stress in the ceramic element body 11.

[0041] Each of the external electrodes 14a, 14b includes a base film 21 formed to cover the end face 11a and a plated film 22 formed on the base film 21. The base film 21 is composed of, for example, a baked film made of a conductive paste, a sputtered film, etc. The plated film 22 is a film formed by electrolytic plating. Each film of the external electrodes 14a, 14b is mainly composed of, for example, nickel (Ni), copper (Cu), tin (Sn), palladium (Pd), platinum (Pt), silver (Ag), gold (Au), etc. or their alloys.

[0042] The base film 21 of the external electrodes 14a, 14b includes an end face covering portion 25 formed on the end face 11a, a main face covering portion 26c formed on the main face 11c, and a side face covering portion 26b formed on the side face 11b and a recessed portion covering portion 27 formed on the recessed portion 23, which will be described below. In this embodiment, the end face covering portion 25 constitutes a first covering portion. The main face covering portion 26c and the side face covering portion 26b constitute a plurality of second covering portions, and the recessed portion covering portion 27 constitutes a third covering portion.

[0043] In this embodiment, the side cover 26b and the main surface cover 26c of the base film 21 are separated from the recess cover 27 at the ridge 11e, and this interrupted portion is also covered by the plated film 22. Next, the structure near the ridge 11e will be described in detail.

[0044] [Detailed Structure of Multilayer Ceramic Capacitor 10]

[0045] Figure 5 yes Figure 4 The enlarged view of FIG. 1 shows the structure of the ridge 11e and its surroundings. Figure 5 Although the structure of one ridge portion 11 e and its surroundings is shown, the same applies to the other ridge portions 11 e and their surroundings.

[0046] The ridge portion 11e has a recess 23 extending in the X-axis direction. A first ridge portion 24a is formed at the outer edge of the recess 23. The first ridge portion 24a is provided on the cover portion 18 side, forms a boundary with the main surface 11c, and protrudes outward. In addition, a second ridge portion 24b is formed at the outer edge of the recess 23. The second ridge portion 24b is provided on the side edge portion 19 side, forms a boundary with the side surface 11b, and protrudes outward. The first ridge portion 24a and the second ridge portion 24b are provided so as to have a recess 23 therebetween, and both extend in the X-axis direction.

[0047] The straight line Le connecting the first ridgeline portion 24a and the second ridgeline portion 24b is drawn on a cross section taken in the Z-axis direction, specifically, on a cross section including the Z-axis direction and the Y-axis direction. The recessed portion is a portion recessed inward from the straight line Le of the ceramic element body 11. A small step or small bump that does not protrude from the straight line Le may also be formed in the recessed portion 23.

[0048] The first ridge portion 24a has an arc portion having a curvature radius R1 on a cross section including the Z-axis direction and the Y-axis direction. In addition, the second ridge portion 24b has an arc portion having a curvature radius R2 on a cross section including the Z-axis direction and the Y-axis direction. The curvature radius R1 of the first ridge portion 24a is greater than the curvature radius R2 of the second ridge portion 24b.

[0049] The radius of curvature R1 of the first ridge portion 24a can be appropriately set within a range of more than 15μm and less than 25μm. In addition, the radius of curvature R2 of the second ridge portion 24b can be appropriately set within a range of more than 0μm and less than 20μm. Although these two ranges include overlapping ranges, it is preferred to satisfy the condition that the radius of curvature R1 of the first ridge portion 24a is greater than the radius of curvature R2 of the second ridge portion 24b, and both values ​​are set within a range that satisfies this condition. It should be noted that the radius of curvature R2 of the second ridge portion 24b is 0μm, which means that the second ridge portion 24b is right-angled on a cross-section including the Z-axis direction and the Y-axis direction.

[0050] Here, refer to Fig. 6A and Figure 6B , the measurement position and measurement method of the curvature radius R1 and the curvature radius R2 will be described. Fig. 6A , the length of the external electrode 14a in the X-axis direction is set to L[14a]. In this embodiment, the curvature radius R1 and the curvature radius R2 are measured at a position L[14a] / 2 away from the end surface of the external electrode 14a. Therefore, first, the multilayer ceramic capacitor 10 is ground to a position L[14a] / 2 away from the end surface of the external electrode 14a to expose the cross section. Then, an optical microscope is used to photograph the exposed cross section.

[0051] Then, if Figure 6BAs schematically shown in (the first method), the first ridge portion 24a and the second ridge portion 24b captured in the photo can be compared using a virtual circle Vc to measure the radius of curvature R1 and the radius of curvature R2. The radius of curvature R1 and the radius of curvature R2 can be measured in a similar manner. Here, the measurement of the radius of curvature R1 of the first ridge portion 24a will be described. First, three points are set on the contour of the first ridge portion 24a shown in the photo, namely the first point P1, the second point P2 and the third point P3. The method for setting the first point P1 is as follows. A virtual line L1 extending in the Y-axis direction is set along the main surface 11c. The first point P1 is set at a position where the virtual line L1 deviates from the first ridge portion 24a. The second point P2 is set at the end of the first ridge portion 24a opposite to the first point P1. The third point P3 is set at the vertex of the first ridge portion 24a. The vertex of the first ridge portion 24a (the third point P3) is determined as follows. A virtual line L2 is set that passes through the second point P2 and extends along the Z direction. The virtual line L1 and the virtual line L2 are perpendicular to each other. A virtual line L3 is set that passes through the intersection of the virtual lines L1 and L2 and forms an angle θ=45° with the virtual line L1. The intersection of the virtual line L3 and the contour line of the first ridgeline portion 24a is determined as the vertex of the first ridgeline portion 24a, and this point is set as the third point P3.

[0052] Then, a virtual circle Vc whose overlap degree with the first point P1 to the third point P3 is equal to or higher than a predetermined value is set, and the radius of the virtual circle Vc is set as the curvature radius R1. The curvature radius R2 of the second ridgeline portion 24b can also be measured in a similar manner. In this case, the virtual line L1 is set to extend in the Y-axis direction from the first ridgeline portion 24a side, and the second virtual line L2 is set to extend in the Z-axis direction along the side surface 11b.

[0053] The radius of curvature R1 and the radius of curvature R2 may also be measured by other methods. Figure 6C As shown, virtual circles Vc of different radii Rn overlap with the contours of the first ridgeline portion 24a and the contours of the second ridgeline portion 24b. When the degree of overlap between the contours of the first ridgeline portion 24a and the second ridgeline portion 24b and the virtual circle Vc is equal to or higher than a predetermined value, the radius of the virtual circle Vc can be set to the curvature radius R1 and the curvature radius R2 (second method).

[0054] The radius of curvature R1 and the radius of curvature R2 can be measured by the first method or the second method mentioned above. This embodiment includes the case where the radius of curvature R1 and the radius of curvature R2 measured by the first method satisfy the relationship mentioned above, and the case where the radius of curvature R1 and the radius of curvature R2 measured by the second method satisfy the relationship mentioned above. In other words, in this embodiment, the radius of curvature R1 and the radius of curvature R2 measured by the first method satisfy the relationship mentioned above, but the radius of curvature R1 and the radius of curvature R2 measured by the second method do not satisfy the relationship mentioned above. In addition, in this embodiment, the radius of curvature R1 and the radius of curvature R2 measured by the first method do not satisfy the relationship mentioned above, but the radius of curvature R1 and the radius of curvature R2 measured by the second method satisfy the relationship mentioned above. Of course, in this embodiment, the radius of curvature R1 and the radius of curvature R2 measured by the first method satisfy the relationship mentioned above, and the radius of curvature R1 and the radius of curvature R2 measured by the second method also satisfy the relationship mentioned above.

[0055] It should be noted that this measurement position is just an example, and other positions along the X-axis direction may also be used as the measurement position, or multiple positions may be used as the measurement position. If measurement is performed at multiple positions, an average value may be used.

[0056] As described above, the main surface covering portion 26c of the base film 21 is formed on the main surface 11c, and the side covering portion 26b of the base film 21 is formed on the side 11b. The recessed portion covering portion 27 of the base film 21 is formed on the recessed portion 23. The recessed portion covering portion 27 is spaced apart from at least one of the main surface covering portion 26c and the side covering portion 26b at the ridge portion 11e. In this embodiment, the recessed portion covering portion 27 is spaced apart from both the main surface covering portion 26c and the side covering portion 26b.

[0057] In this embodiment, the plating film 22 has a multilayer structure. The plating film 22 includes an intermediate film 28 formed on the base film 21 and a surface film 29 formed on the intermediate film 28. The intermediate film 28 and the surface film 29 continuously cover the end surface covering portion 25, the main surface covering portion 26c, the side covering portion 26b and the recessed portion covering portion 27 of the base film 21. The metal materials constituting the intermediate film 28 and the surface film 29 may be the same or different. The metal material may be selected from, for example, copper, nickel, tin or an alloy thereof.

[0058] Since base film 21 has main surface covering portion 26 c , side surface covering portion 26 b , and recessed portion covering portion 27 that are spaced apart from each other, defects such as cracks caused by temperature changes in ceramic element body 11 can be prevented.

[0059] The electrode material constituting the base film 21 and the ceramic material constituting the ceramic element body 11 have different linear expansion coefficients. Therefore, when the base film 21 is cooled after being baked or after generating heat after mounting, the base film 21 shrinks more than the ceramic element body 11, and tensile stress is generated in the base film 21. On the other hand, compressive stress is generated in the ceramic element body 11 due to the tensile stress.

[0060] For example, tensile stress inward in the Y-axis direction is generated in the main surface covering portion 26c of the base film 21. For example, tensile stress inward in the Z-axis direction is generated in the side covering portion 26b of the base film 21. Therefore, tensile stress in different directions is generated in the base film 21 near the edge portion 11e.

[0061] In this embodiment, the main surface covering portion 26c and the side covering portion 26b are separated from each other. Even when the above-mentioned tensile stress is generated, it is possible to prevent the stress from accumulating in the base film 21. Therefore, it is possible to suppress the occurrence of defects such as cracks in the ceramic element body 11 due to the generation of large compressive stress in the ceramic element body 11.

[0062] Furthermore, in this embodiment, recessed portion covering portion 27 is formed on recessed portion 23. Due to recessed portion covering portion 27, the electrode material of base film 21 remains within recessed portion 23, and the spacing width between base films 21 can be minimized.

[0063] In this embodiment, the recessed portion covering portion 27 is formed by the electrode material remaining in the recessed portion 23. Therefore, the interval width between the main surface covering portion 26c or the side covering portion 26b and the recessed portion covering portion 27 in the base film 21 is adjusted, and the plated film 22 can continuously cover the entire base film 21. This can prevent the generation of gaps between the external electrodes 14a, 14b and the ceramic element body 11, and prevent poor insulation. Therefore, the reliability of the laminated ceramic capacitor 10 can be improved.

[0064] Here, the effect of setting the curvature radius R1 of the first ridge line portion 24 a larger than the curvature radius R2 of the second ridge line portion 24 b will be explained with reference to a comparative example. Fig. 7A It is a partially enlarged cross-sectional view showing the periphery of the first ridgeline portion 24 a and the periphery of the second ridgeline portion 24 b . Fig. 8A 2 is a cross-sectional view of a multilayer ceramic capacitor 10 according to the present embodiment. Figure 7B It is a partially enlarged cross-sectional view showing the periphery of the first ridgeline portion 224 a and the periphery of the second ridgeline portion 224 b . Figure 8B 4 is a cross-sectional view of a multilayer ceramic capacitor 50 according to a comparative example.

[0065] Similar to the laminated ceramic capacitor 10 of the embodiment, the laminated ceramic capacitor 50 of the comparative example includes an edge portion 51e. In addition, the laminated ceramic capacitor 50 also includes a covering portion 58 and a side edge portion 59 surrounding the capacitor portion 56. The edge portion 51e has a recess 53 extending in the X-axis direction. The first edge portion 224a is formed on the outer edge of the recess 53, which is arranged on the side of the covering portion 58, forms a boundary with the main surface 51c, and protrudes outward. In addition, the second edge portion 224b is formed on the outer edge of the recess 53, which is arranged on the side of the side edge portion 59, forms a boundary with the side surface 51b, and protrudes outward. The first edge portion 224a and the second edge portion 224b are arranged to have a recess 53 between them, and both extend in the X-axis direction.

[0066] The first ridge portion 224a has an arc portion on a cross section including the Z-axis direction and the Y-axis direction. In addition, the second ridge portion 224b has an arc portion on a cross section including the Z-axis direction and the Y-axis direction. Here, the curvature radius of the first ridge portion 224a and the curvature radius of the second ridge portion 224b are substantially the same. This is different from the multilayer ceramic capacitor 10 of the embodiment.

[0067] Reference Fig. 7A , which schematically depicts the propagation of force when an impact force is applied to the edge portion 11e of the multilayer ceramic capacitor 10 of the embodiment. The radius of curvature R1 of the first edge portion 24a is different from the radius of curvature R2 of the second edge portion 24b. Therefore, the input direction of the impact force is different between the first edge portion 24a and the second edge portion 24b. Therefore, the impact force propagating inside the ceramic component body 11 is expected to be offset inside the ceramic component body 11. Therefore, the impact force toward the capacitor portion 16 is mitigated.

[0068] On the other hand, refer to Figure 7B , which schematically shows the propagation of force when an impact force is applied to the edge portion 51e of the comparative example multilayer ceramic capacitor 50. The curvature radius R of the first edge portion 224a and the curvature radius R of the second edge portion 224b are substantially the same. Therefore, the input direction of the impact force is substantially the same between the first edge portion 224a and the second edge portion 224b. For this reason, it can be considered that the effect of offsetting the impact force propagating inside the ceramic element body 51 in the ceramic element body 51 as in the multilayer ceramic capacitor 10 of the embodiment is low.

[0069] Reference Fig. 8A , which shows the angle θ1 between the tangent line connecting the first ridgeline portion 24a and the second ridgeline portion 24b and the line extending from the main surface 11c of the ceramic element body 11 along the Y-axis direction. Also shown is the height t1 from the main surface 11c, which is the mounting surface of the multilayer ceramic capacitor 10, to the second ridgeline portion 24b. Figure 8BAs a comparative example, it shows the angle θ2 between the tangent line connecting the first ridgeline portion 224a and the second ridgeline portion 224b and the line extending along the Y-axis direction from the main surface 51c of the ceramic element body 51. The height t2 from the main surface 51c, which is the mounting surface of the multilayer ceramic capacitor 50, to the second ridgeline portion 224b is also shown.

[0070] The angle θ1 is smaller than the angle θ2, and the height t1 is lower than the height t2. Therefore, the multilayer ceramic capacitor 10 of the embodiment is less likely to fall down during mounting than the multilayer ceramic capacitor 50 of the comparative example.

[0071] It should be noted that in the multilayer ceramic capacitor 10 of the embodiment, the radius of curvature R1 of the first ridge portion 24a is larger than the radius of curvature R2 of the second ridge portion 24b. If the radius of curvature R2 of the second ridge portion 24b is made larger than the radius of curvature R1 of the first ridge portion 24a, the area where the thickness of the side edge portion 19 is thinner increases. This is because as the radius of curvature increases, the chamfered area becomes wider and the arc drawn approaches the inside of the ceramic element body 11. In the embodiment, in order to avoid this, the radius of curvature R1 is set larger than the radius of curvature R2.

[0072] [Method of Manufacturing Multilayer Ceramic Capacitor 10]

[0073] Fig. 9 1 is a flowchart of a method for manufacturing the multilayer ceramic capacitor 10 . Figures 10 to 17 1 is a diagram schematically illustrating a manufacturing process of a laminated ceramic capacitor 10. Fig. 9 , and make appropriate reference Figures 10 to 17 A method for manufacturing the multilayer ceramic capacitor 10 will be described.

[0074] (Step S01: Manufacturing Ceramic Laminated Chip C) In step S01, the ceramic sheets 101, 102 for forming the capacitor portion 16 and the ceramic sheet 103 for forming the cover portion 18 are stacked and cut to form an unfired ceramic laminated chip (laminated chip) C.

[0075] Fig.10 The ceramic sheets 101, 102 and 103 shown are constructed as unfired dielectric green sheets, which include a ceramic material made of dielectric ceramic, an organic binder and other additives. An unfired first internal electrode 112 corresponding to the first internal electrode 12 is formed on the ceramic sheet 101. An unfired second internal electrode 113 corresponding to the second internal electrode 13 is formed on the ceramic sheet 102. The ceramic sheet 103 has no internal electrodes formed thereon.

[0076] Each of the internal electrodes 112 and 113 has a plurality of strip-shaped electrode patterns that cross the cut lines Lx parallel to the X-axis direction and extend along the cut lines Ly parallel to the Y-axis direction. These internal electrodes 112 and 113 are formed by applying conductive paste on the ceramic sheets 101 and 102 by printing or the like.

[0077] like Fig.10 As shown, ceramic sheets 101 and 102 are alternately stacked in the Z-axis direction. The capacitor portion 16 and the edge portion 20 correspond to the stacked body of ceramic sheets 101 and 102. Ceramic sheet 103 is stacked on the top and bottom surfaces of the stacked structure of ceramic sheets 101 and 102 in the Z-axis direction. The stacked structure of ceramic sheet 103 corresponds to the cover portion 18. It should be noted that the number of stacked ceramic sheets 101, 102, 103, etc. can be adjusted appropriately.

[0078] Subsequently, the stacked structure of the ceramic sheets 101, 102 and 103 is pressed from the Z-axis direction and cut along the cutting lines Lx and Ly. As a result, a structure such as Fig. 9 The stacked chip C is shown.

[0079] The laminated chip C has an unfired capacitor portion 116 (in which unfired internal electrodes 112 and 113 are formed), an unfired cover portion 118, and an unfired edge portion 120. The laminated chip C has a side surface Cb (which is a cutting surface corresponding to the cutting line Lx) and an end surface Ca (which is a cutting surface corresponding to the cutting line Ly). The ends of the unfired internal electrodes 112 and 113 are exposed from the side surface Cb.

[0080] (Step S02: Forming the first ridge portion 124a) In step S02, the first ridge portion 124a is formed at the side portion connecting the side surface Cb and the main surface Cc of the stacked chip C. The first ridge portion 124a is a portion corresponding to the first ridge portion 24a obtained after firing, and it is processed into an arc so that the first ridge portion 24a obtained after firing has a curvature radius R1. In the embodiment, sandblasting is performed using a nozzle 40 to perform chamfering to form the first ridge portion 124a. It should be noted that other known conventional construction methods can also be used as long as the first ridge portion 24a with the desired arc shape can be obtained.

[0081] (Step S03: Forming the Side Edge 119) In step S03, the side edge 119 is formed on the side surface Cb of the stacked chip C. The forming method will be described below by way of example.

[0082] First, if Fig.13 As shown, a laminated sheet S, which is a laminated structure of ceramic sheets, is placed on a flat elastic member E, and the laminated chip C, one side Cb of which is fixed by a tape T, faces the laminated sheet S with the other side Cb thereof.

[0083] In this embodiment, the laminated sheet S has a laminated structure of a first ceramic sheet 104, a second ceramic sheet 105, and a third ceramic sheet 106 for forming the side edge portion. Like the ceramic sheets 101, 102, 103, each of the ceramic sheets 104, 105, 106 includes a ceramic material, an organic binder, and other additives.

[0084] The heat shrinkage rate of the second ceramic sheet 105 is higher than that of the first ceramic sheet 104. In addition, the heat shrinkage rate of the third ceramic sheet 106 is higher than that of the second ceramic sheet 105. The heat shrinkage rate may be adjusted by adjusting the amount of the organic binder and the additive.

[0085] Next, if Fig.14 As shown, the laminate sheet S is attached to the side Cb of the laminated chip C by punching the laminate sheet S on the side Cb. Specifically, the laminated chip C is subjected to a strong pressure from the laminate sheet S in the Y-axis direction. As a result, the laminated chip C and the laminate sheet S are partially and deeply sunk into the elastic component E. At this time, a shear force acts on the laminate sheet S along the outer edge of the side Cb, and when the shear force exceeds the shear strength of the laminate sheet S, the laminate sheet S is punched out.

[0086] Then, if Fig.15 As shown, a portion of the laminated sheet S that sinks together with the laminated chip C is cut off. Therefore, a first side edge portion 119a laminated on the side Cb and a second side edge portion 119b laminated on the first side edge portion 119a are formed. In addition, in this embodiment, a third side edge portion 119c is laminated on the second side edge portion 119b. Therefore, an unfired side edge portion 119 including the first side edge portion 119a, the second side edge portion 119b and the third side edge portion 119c is formed on the side Cb of the laminated chip C.

[0087] Similarly, a side edge portion 119 is formed on the other side surface Cb. Fig.16 The unfired ceramic component body 111 is shown. At this stage, no recess 23 is formed in the ridge 111e between the main surface 111c and the side surface 111b.

[0088] (Step S04: Firing) In step S04, the ceramic element body 111 obtained in step S03 is fired to obtain a ceramic element body 111 as shown in FIG. Fig.17 and Figures 1 to 3 The ceramic element body 11 of the laminated ceramic capacitor 10 is shown. The firing temperature in step S04 can be determined according to the sintering temperature of the ceramic element body 111. In addition, the firing can be performed in a reducing atmosphere or a low oxygen partial pressure atmosphere, for example.

[0089] By firing, each side edge portion 119a, 119b and 119c undergoes thermal contraction at a different rate. Specifically, the second side edge portion 119b contracts more than the first side edge portion 119a. The third side edge portion 119c contracts more than the second side edge portion 119b.

[0090] Therefore, if Fig.17 As shown, a gentle step or slope is formed on the edge 11e of the ceramic element body 11. The outer edges of the side edges 119a, 119b, and 119c shrink inward in the Z-axis direction to form a concave portion 23. The outer edge of the third side edge 119c forms a second ridgeline 24b.

[0091] By setting the thermal shrinkage rate of the third side edge portion 119c, the radius of curvature R2 of the second ridgeline portion 24b formed after firing can be adjusted to a desired value. In addition, in order to achieve the desired radius of curvature R2, the second ridgeline portion 24b can also be chamfered after firing. The chamfering process can use a sandblasting method or a known traditional method. When processing the second ridgeline portion 24b, the first ridgeline portion 24a may be affected by the processing. Therefore, when the first ridgeline portion 24a is chamfered in step S02, the process can be performed taking into account the impact of the process on the second ridgeline portion 24b. In addition, the second ridgeline portion 24b can also be chamfered before firing.

[0092] It should be noted that Fig.17 , portions corresponding to the side edge portions 119a, 119b, and 119c in the side edge portion 19 are indicated by dotted lines, but the boundaries become almost invisible after firing.

[0093] (Step S05: Forming a base film) In step S05, a conductive base film 21 is formed, which includes an end face covering portion 26a formed on the end face 11a, a side face covering portion 26b formed on the side face 11b, a main face covering portion 26c formed on the main face 11c, and a recess covering portion 27 formed on the recess 23 and spaced apart from the side face covering portion 26b and the main face covering portion 26c.

[0094] Specifically, first, the unfired electrode material is applied to the end face 11a, and also applied to the side face 11b, the main face 11c and a part of the edge portion 11e connected to the end face 11a. The coating method is, for example, an immersion method. In the immersion method, the end face 11a side of the ceramic element body 11 is immersed in an immersion tank containing an electrode material such as a conductive paste. Thus, the unfired electrode material can be applied to the side face 11b, the main face 11c and the recess 23 almost simultaneously with the end face 11a.

[0095] The unfired electrode material is applied thinly so that the recessed portion covering portion 27, the side covering portion 26b and the main surface covering portion 26c after baking are separated from each other. However, it is not necessary to separate these parts when applying. The application thickness of the electrode material can be adjusted by adjusting the immersion time, the pulling speed, the viscosity of the electrode material, etc.

[0096] It should be noted that the method of forming the base film is not limited to the dipping method, and may be, for example, a printing method, a sputtering method, or a combination of these methods.

[0097] Next, the unfired electrode material is baked. Baking can be performed, for example, in a reducing atmosphere or in a low oxygen partial pressure atmosphere. During baking, the electrode material formed on each surface shrinks due to heat. The shrinkage rate of the electrode material is greater than the shrinkage rate of the ceramic element body 11. Therefore, the electrode material applied on each surface generates tensile stress in a direction away from the edge portion 11e. Thus, the recessed portion covering portion 27, the side surface covering portion 26b, and the main surface covering portion 26c are formed separately from each other.

[0098] (Step S06: Forming a plated film) In step S06, the plated film 22 is formed so as to continuously cover the end surface covering portion 26a, the side surface covering portion 26b, the main surface covering portion 26c, and the recessed portion covering portion 27. Specifically, the multilayer ceramic capacitor 10 on which the base film 21 is formed is immersed in a plating solution corresponding to the intermediate film 28 and the surface film 29, respectively, for electrolytic plating. As a result, the plated film 22 having a plurality of layers (including the intermediate film 28 and the surface film 29) is formed.

[0099] Through the above steps, the Figures 1 to 3 The laminated ceramic capacitor 10 shown in FIG. 1 is a laminated ceramic capacitor. In this embodiment, the side edge portion 119 is added to the laminated chip C so that the ends of the internal electrodes 112 and 113 are aligned within a range of 0.5 μm in the Y-axis direction. As a result, the proportion of the volume occupied by the capacitor portion 16 in the ceramic element body 11 can be increased, and the capacitance can be increased without increasing the size of the laminated ceramic capacitor 10.

[0100] [Other embodiments]

[0101] Although the embodiments of the present invention have been described above, the present invention is not limited to the above-described embodiments, and it goes without saying that various changes can be made without departing from the gist of the present invention.

[0102] The number of ceramic sheets forming each side edge 19 is not limited to three. For example, by using more than 2 and less than 4 ceramic sheets to form the side edge 19, the recess 23 can be formed into a desired shape and the side edge 19 can be prevented from peeling off after attachment.

[0103] For example, in the above-described embodiment, it has been explained that the unfired side edge portion 119 is formed by attaching the laminated sheet S in which different ceramic sheets are laminated, but a plurality of ceramic sheets may be attached one by one.

[0104] Furthermore, the method of attaching the ceramic sheet is not limited to sheet punching, and a ceramic sheet cut in advance into a predetermined size may be attached to the side surface Cb.

[0105] Alternatively, the side edge portion 19 may be formed by applying ceramic materials having different heat shrinkage rates in layers on the side surfaces Cb of the laminated core C. This may also form a laminated structure having a plurality of side edge portions having different heat shrinkage rates.

[0106] In addition, the recessed portion can also be formed by forming the cover 18 with a plurality of ceramic sheets having different heat shrinkage rates. In this case, a plurality of ceramic sheets each having a side edge formed around the internal electrode are stacked, and a plurality of ceramic sheets having gradually increasing heat shrinkage rates are stacked above and below in the Z-axis direction. Thus, a ridge including the recessed portion is formed at the outer edge of the ceramic sheet used to form the cover.

[0107] Furthermore, the recessed portion is not limited to being formed by the thermal shrinkage of the ceramic material, and the recessed portion may be formed by grinding the edge line of the ceramic element body formed in a rectangular parallelepiped shape.

[0108] Furthermore, the stacked ceramic capacitor may be of a so-called tall type in which the dimension in the Z-axis direction is larger than the dimension in the Y-axis direction.

[0109] [Example]

[0110] Next, the results of the impact test of the example will be described together with the comparative example. The example corresponds to the laminated ceramic capacitor 10 of the embodiment, and its dimensions are as follows. Figure 7B or Figure 8B The illustrated multilayer ceramic capacitor 50 has the following dimensions.

[0111] The conditions of the impact test are as follows.

[0112] Equipment (test equipment): i220 manufactured by IMY

[0113] Test method: Place the product to be tested (laminated ceramic capacitor) into a specified plastic box and vibrate.

[0114] Test target product size: 0603 (length × width × height = 0.6mm × 0.3mm × 0.3mm)

[0115] Number of test objects: 7000 pieces (assuming shape is 0603)

[0116] Vibration frequency: 10Hz

[0117] Cycle times: 600 times

[0118] Evaluation method: Visual evaluation using a stereo microscope (n = 100 pieces)

[0119] The test results are as follows Fig.18 As shown. The crack occurrence rate in the embodiment is about 3%. On the other hand, the crack occurrence rate in the comparative example is about 15%. As described above, the embodiment has higher impact resistance reliability than the comparative example.

[0120] The impact is applied to each test object under test by vibration. In the comparative example, the directions of the impact force input from the first ridgeline portion 124a and the second ridgeline portion 124b are substantially the same. Therefore, it can be considered that the impact force is not dispersed, but may be propagated in the direction where the capacitor portion 56 exists (see Figure 8B ). Therefore, it is considered that the crack occurrence rate is high. On the other hand, in the embodiment, the directions of the impact force input from the first ridgeline portion 24a and the second ridgeline portion 24b are different. Therefore, it can be considered that the impact force is offset and the impact force propagating in the direction where the capacitor portion 16 exists is weakened (see Fig. 8A ). Therefore, it is considered that the crack occurrence rate is low.

[0121] In this way, it can be confirmed that the example has higher impact resistance reliability than the comparative example.

[0122] Although the above embodiment describes the laminated ceramic capacitor 10 as an example of a laminated ceramic electronic device, the present invention is applicable to all laminated ceramic electronic devices in which ceramic layers and internal electrodes are laminated. Examples of such laminated ceramic electronic devices include chip varistors, chip thermistors, laminated inductors, etc.

Claims

1. A laminated ceramic electronic device comprising: A ceramic element body, comprising a protection portion and a functional portion located inside the protection portion, wherein the protection portion comprises an end surface facing a first direction, a plurality of peripheral surfaces adjacent to the end surface and extending along the first direction, and an edge portion having a recess extending along the first direction and connecting the plurality of peripheral surfaces; and an external electrode including a base film covering the end surface and a plated film formed on the base film, wherein the functional portion includes a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, The protection portion includes a covering portion stacked on the functional portion along the second direction and a side edge portion covering the functional portion in a third direction perpendicular to the first direction and the second direction. The ridge portion includes a first ridge portion located on one side of the covering portion and a second ridge portion located on one side of the side edge portion, the concave portion is located between the first ridge portion and the second ridge portion, and In the cross section including the second direction and the third direction, the curvature radius R1 of the first ridge portion is greater than the curvature radius R2 of the second ridge portion.

2. The multilayer ceramic electronic device according to claim 1, in, The size of the stacked ceramic electronic device in the second direction is greater than the size of the stacked ceramic electronic device in the third direction.

3. The multilayer ceramic electronic device according to claim 1 or 2, in, The first ridge portion has a curvature radius R1 of not less than 15 μm and not more than 25 μm.

4. The multilayer ceramic electronic device according to any one of claims 1 to 3, in, The curvature radius R2 of the second ridgeline portion is greater than or equal to 0 μm and less than or equal to 20 μm.

5. The multilayer ceramic electronic device according to any one of claims 1 to 4, in, The base film includes a first covering portion formed on the end surface, a plurality of second covering portions formed on the plurality of peripheral surfaces, and a third covering portion formed on the recessed portion, the third covering portion being spaced apart from at least one of the plurality of second covering portions, and Wherein, the coating film continuously covers the first covering portion, the plurality of second covering portions and the third covering portion.

6. The multilayer ceramic electronic device according to any one of claims 1 to 5, in, Edges of the plurality of internal electrodes in a third direction perpendicular to the first direction and the second direction are aligned within a range of 0.5 μm.

7. A method for manufacturing a laminated ceramic electronic device, the method comprising the following steps: forming a ceramic laminated chip, the ceramic laminated chip having an end surface facing a first direction, a functional portion, and a covering portion, the functional portion having a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, the plurality of internal electrodes being exposed on a side surface of the ceramic laminated chip facing a third direction perpendicular to the first direction and the second direction, the covering portion being stacked on the functional portion along the second direction; forming a first ridge portion adjacent to the end surface and connecting the peripheral surface extending along the first direction and the side surface; forming a side edge portion, thereby forming a ceramic element body, the side edge portion being stacked on the side surface and extending in the first direction and used to form a second ridge portion, the second ridge portion being formed to have a concave portion therebetween; firing the ceramic laminate chip and the side edge portion; and forming an external electrode, the external electrode comprising a base film covering the end surface and a plated film formed on the base film, The step of forming the first ridge portion includes chamfering so that, in a cross section including the second direction and the third direction, a curvature radius R1 of the first ridge portion is greater than a curvature radius R2 of the second ridge portion.

8. The method according to claim 7, in, In the step of forming the external electrode, a base film is formed, the base film including a first covering portion formed on an end surface of the ceramic element body, a plurality of second covering portions formed on the plurality of peripheral surfaces adjacent to the end surface and extending in the first direction, and a third covering portion formed on the recess and spaced apart from at least one of the plurality of second covering portions, and The method includes forming a plating film that continuously covers the first covering portion, the plurality of second covering portions, and the third covering portion.

9. The method according to claim 7 or 8, in, In the step of forming the side edge portion, a first side edge portion stacked on the side surface and a second side edge portion stacked on the first side edge portion and having a higher thermal shrinkage rate than the first side edge portion are formed.

10. The method according to claim 9, in, The first side edge is formed by attaching a first ceramic sheet to the side surface, and The second side edge portion is formed by attaching a second ceramic sheet having a higher thermal shrinkage rate than the first ceramic sheet to the first ceramic sheet.

11. A method for manufacturing a laminated ceramic electronic device, the method comprising the following steps: forming a ceramic component body, the ceramic component body having an end face facing a first direction, a functional portion, a covering portion, a side edge portion, a plurality of peripheral surfaces extending in the first direction, and an edge portion connecting the plurality of peripheral surfaces, the functional portion having a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, the plurality of internal electrodes being exposed on a side surface of the ceramic component body facing a third direction perpendicular to the first direction and the second direction, the covering portion being stacked on the functional portion along the second direction, and the side edge being stacked on the side surface along the third direction; Firing the ceramic element body; In the ridge portion, a first ridge portion having a curvature radius R1 in a cross section including the second direction and the third direction and a second ridge portion having a curvature radius R2 smaller than the curvature radius R1 in the cross section are formed, and a concave portion is interposed between the first ridge portion and the second ridge portion; and An external electrode is formed, the external electrode including a base film covering the end surface and a plated film formed on the base film.

12. The method according to claim 11, wherein: The size of the stacked ceramic electronic device in the second direction is greater than the size of the stacked ceramic electronic device in the third direction.