Energy-saving drying method and system for starch
Through a two-stage drying method that combines low-temperature vacuum drying and high-temperature vacuum drying, combined with MVR technology and live steam two-effect evaporation, the existing starch drying technology solves the high energy consumption and product form problems, and achieves energy-efficient starch drying and production. Produce high-quality granular or powdered products.
Patent Information
- Application Number
- CN202410893250.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-04
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2044-07-04
AI Technical Summary
The existing starch drying technology, hot air flow drying and oven drying, has low thermal efficiency, resulting in high energy consumption and the inability to produce granular products, affecting product quality and production efficiency.
Adopting a two-stage drying method that combines low-temperature vacuum drying and high-temperature vacuum drying, combined with mechanical steam recompression (MVR) technology and raw steam two-effect evaporation, low-temperature vacuum drying is used to prevent starch gelatinization, and high-temperature vacuum drying is used to increase drying speed and sterilize , and recover waste heat through an atmospheric pressure dryer to achieve the production of granular or powdery products.
Drying energy consumption is significantly reduced, reaching 18-20% of hot air drying and 12-15% of oven drying, while ensuring product quality and achieving continuous production on the assembly line.
Smart Images

Figure CN118745232A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of starch drying, and in particular to a starch energy-saving drying method and system. Background Art
[0002] Starch is an important basic raw material for food and chemical industry. Most of them are processed and extracted from starch-rich plants, such as corn starch, cassava starch, potato starch, sweet potato starch, water chestnut starch (water chestnut powder), kudzu starch (kudzu powder), etc. In the processing process, the slurry is first dehydrated to obtain wet starch with a moisture content of about 35-40%, and then dried by hot air flow or drying in a drying room (water chestnut powder) to obtain a finished product with a moisture content of 10-14%. The thermal efficiency of hot air flow drying and drying room drying is very low, only 30-50%. my country has a large output of various starches and many manufacturers, and the drying energy consumption accounts for a large proportion! Therefore, it is necessary to develop energy-saving technology for starch drying.
[0003] Due to traditional sales habits, water chestnut powder and kudzu root powder are required to be in granular form. Consumers believe that granular water chestnut powder and kudzu root powder are not counterfeit and are easier to distinguish from other starches. Conventional hot air drying can only produce powdered products. Therefore, current manufacturers can only use drying rooms or tunnel carts with low production efficiency for drying.
[0004] Steam multi-effect evaporation and steam mechanical recompression (MVR) technology have been widely used in the field of food liquid concentration and evaporation, and have achieved good energy-saving effects. However, they are not widely used in the field of solid drying. Literature search shows that they have only been used in sludge drying. Multi-effect evaporation and steam mechanical recompression (MVR) technology have not been used in starch drying. Summary of the invention
[0005] In order to solve the above problems, the present invention provides a starch energy-saving drying method and system.
[0006] The present invention provides a starch energy-saving drying method, which comprises the following steps:
[0007] The wet starch to be dried is subjected to low-temperature vacuum drying to obtain the first wet starch and secondary steam generated by the low-temperature vacuum drying;
[0008] The secondary steam generated by the low-temperature vacuum drying is compressed and superheated, and then used for heating and drying the first wet starch to obtain a second wet starch;
[0009] The second wet starch is subjected to high temperature vacuum drying to obtain dried high temperature starch and secondary steam generated by high temperature vacuum drying;
[0010] Cooling the dried high-temperature starch to obtain dried starch and hot water generated by cooling;
[0011] The secondary steam generated by the high-temperature vacuum drying and the hot water generated by the cooling are refluxed and used as a compensating heat source during the heating and drying of the first wet starch.
[0012] Furthermore, the moisture content of the wet starch to be dried is 35-40% by weight.
[0013] Further, the wet starch to be dried is subjected to low-temperature vacuum drying to 50-55° C., the low-temperature vacuum drying temperature is 50-55° C., and the vacuum degree is -0.088-0.085 MPa.
[0014] Furthermore, the secondary steam generated by the low-temperature vacuum drying is compressed and desuperheated, and then used for heating and drying the first wet starch with a saturated steam temperature of 65 to 70° C. and a vacuum degree of -0.076 to 0.07 MPa.
[0015] Furthermore, the working condition parameters of the high-temperature vacuum drying include: a drying temperature of 80 to 90° C. and a vacuum degree of -0.054 to 0.031 MPa.
[0016] Furthermore, in terms of weight percentage, the moisture content of the second wet starch is 14-16%.
[0017] Furthermore, in terms of weight percentage, the moisture content of the dried high-temperature starch is 10-14%.
[0018] In a second aspect, the present invention provides a system for implementing the starch energy-saving drying method according to any one of the first aspects, the system comprising a low-temperature vacuum dryer and a low-temperature vacuum dryer heater, a low-temperature steam compressor, a high-temperature vacuum dryer and a high-temperature vacuum dryer heater, and a normal pressure dryer connected in sequence;
[0019] The low-temperature vacuum dryer and high-temperature vacuum dryer can be selected from heat-conductive horizontal disc vacuum dryers, vertical disc vacuum dryers, hollow blade vacuum dryers, etc.
[0020] The atmospheric pressure dryer can be a heat conduction type horizontal disc atmospheric pressure dryer, a vertical disc atmospheric pressure dryer, a hollow blade atmospheric pressure dryer, etc.
[0021] The low-temperature steam compressor can be a Roots steam compressor or a centrifugal steam compressor;
[0022] The vacuum feeder of the low-temperature vacuum dryer is connected to the first conveyor belt, the low-temperature vacuum dryer is connected to the low-temperature steam compressor and the humidifier in sequence, the humidifier is connected to the low-temperature vacuum dryer heater, the low-temperature vacuum dryer heater is connected to the first vapor-liquid separator, and the first vapor-liquid separator is connected to a pump; the low-temperature vacuum dryer is connected to the high-temperature vacuum dryer via the first vacuum discharger;
[0023] The high-temperature vacuum dryer is connected to the humidifier through the second vapor-liquid separator, the second pressure reducing valve, and the non-condensable gas pressure reducing valve; the high-temperature vacuum dryer is connected to the second conveyor belt through the second vacuum feeder, the second conveyor belt is connected to the feed hopper of the atmospheric pressure dryer, the atmospheric pressure dryer is provided with a cooler, and the atmospheric pressure dryer cooler is connected to the humidifier through the third pressure reducing valve.
[0024] Furthermore, the atmospheric pressure dryer is provided with a discharge port.
[0025] The above technical solution provided by the embodiment of the present invention has at least the following advantages compared with the prior art:
[0026] The embodiment of the present invention provides a starch energy-saving drying method and system. The patent scheme adopts steam mechanical recompression (MVR) technology, combined with raw steam two-effect evaporation, to separate wet starch into two-stage drying at low temperature of 50-55°C and high temperature of 80-90°C. Low-temperature vacuum drying can prevent starch gelatinization (temperature lower than gelatinization temperature) when the starch water content is high. The water is mainly controlled to evaporate in the low-temperature section, and the residence time is relatively long; high-temperature vacuum drying can further evaporate the starch combined with water, increase the drying speed, and the high-temperature section has a sterilizing effect. For some starch products with sterilization requirements (such as water chestnut powder), it is a necessary process; the residence time in the high-temperature section is relatively short, and the starch moisture content is low (≤16%), which reduces the characteristic variation of starch and can ensure the quality of the product. After drying, use a normal pressure dryer to cool and recycle the waste heat to obtain a granular product (such as water chestnut powder); adding a powder cabinet to crush and sieve can also obtain a powdered starch product (such as cassava starch), so as to achieve the purpose of continuous production of the assembly line. The overall energy consumption is only 18-20% of hot air drying and 12-15% of drying room. It is a very energy-saving drying method, which makes up for the shortcomings of existing technologies. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.
[0028] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0029] Figure 1 A schematic flow chart of the energy-saving starch drying method provided in an embodiment of the present invention.
[0030] Figure 2 A schematic diagram of a starch energy-saving drying system provided in an embodiment of the present invention.
[0031] Figure 2 In: 1-first conveyor belt, 2-vacuum feeder, 3-low-temperature vacuum dryer, 4-low-temperature steam compressor, 5-low-temperature vacuum dryer heater, 6-first vacuum discharger, 7-first vapor-liquid separator, 8-pump, 9-humidifier, 10-high-temperature vacuum dryer, 11-first pressure reducing valve, 12-high-temperature vacuum dryer heater, 13-second vacuum discharger, 14-second vapor-liquid separator, 15-non-condensable gas pressure reducing valve, 16-second pressure reducing valve, 17-second conveyor belt, 18-feed hopper, 19-normal pressure dryer, 20-cooler, 21-discharge port, 22-third pressure reducing valve. DETAILED DESCRIPTION
[0032] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0033] Unless otherwise specified, various raw materials, reagents, instruments and equipment used in the present invention can be purchased from the market or prepared by existing methods.
[0034] In a first aspect, the present invention provides a starch energy-saving drying method, such as Figure 1 As shown, the starch energy-saving drying method comprises the following steps:
[0035] The wet starch to be dried is subjected to low-temperature vacuum drying to obtain the first wet starch and the secondary steam generated by the preheating drying;
[0036] The secondary steam generated by the low-temperature vacuum drying is compressed and superheated, and then used for heating and drying the first wet starch to obtain a second wet starch;
[0037] The second wet starch is subjected to high temperature vacuum drying to obtain dried high temperature starch and secondary steam generated by high temperature vacuum drying;
[0038] Cooling the dried high-temperature starch to obtain dried starch and hot water generated by cooling;
[0039] The secondary steam generated by the high-temperature vacuum drying and the hot water generated by the cooling are refluxed and used as a compensating heat source during the heating and drying of the first wet starch.
[0040] The embodiment of the present invention provides a starch energy-saving drying method. The patent scheme adopts steam mechanical recompression (MVR) technology, combined with raw steam two-effect evaporation, to separate wet starch into two-stage drying at low temperature of 50-55°C and high temperature of 80-90°C. Low-temperature vacuum drying can prevent starch gelatinization (temperature lower than gelatinization temperature) when the starch water content is high. The water is mainly controlled to evaporate in the low-temperature section, and the residence time is relatively long; high-temperature vacuum drying can further evaporate the starch combined with water, increase the drying speed, and the high-temperature section has a sterilizing effect. For some starch products with sterilization requirements (such as water chestnut powder), it is a necessary process; the residence time in the high-temperature section is relatively short, and the starch moisture content is low (≤16%), which reduces the characteristic variation of starch and can ensure the quality of the product. After drying, use a normal pressure dryer to cool and recycle the waste heat, and a granular product (such as water chestnut powder) can be obtained; adding a powder cabinet to crush and sieve can also obtain a powdered starch product (such as cassava starch), so as to achieve the purpose of continuous production of the assembly line. The overall energy consumption is only 18-20% of hot air drying and 12-15% of drying room. It is a very energy-saving drying method, which makes up for the shortcomings of existing technologies.
[0041] Compared with liquid evaporation and concentration, material drying generally has a lower water content than dry-based materials. Simple steam mechanical recompression (MVR) produces less steam, which is insufficient to compensate for the thermal balance of the system. External raw steam is required during operation. In many cases, the added heat energy is greater than the mechanical compression work! Therefore, the concept of multi-effect evaporation is introduced, and raw steam is used as the heat source of the first-effect dryer to dry the material. The secondary steam generated is then introduced into the second-effect dryer to dry the material. The secondary steam generated by the second-effect dryer is then recompressed (MVR) by the steam compressor and reused in the second-effect dryer. At the same time, the hot water generated by the cooling of the finished product is recovered for preheating the dry material, which can greatly reduce the amount of raw steam.
[0042] This patented solution is aimed at the characteristics of wet starch with high moisture content, easy gelatinization at high temperature, and sterilization and sanitation requirements (such as water chestnut powder). Select a heat conduction vacuum dryer (optional: horizontal disc vacuum dryer, vertical disc vacuum dryer, hollow blade vacuum dryer, etc.). Match the water low-temperature steam compressor (optional: Roots or centrifugal steam compressor) to form a two-effect vacuum + steam mechanical recompression (MVR) vacuum starch drying system. It can meet the needs of most starch drying, and at the same time, it can save a lot of energy. The energy consumption is only 18-20% of hot air drying and 12-15% of drying in a drying room.
[0043] It has good social and economic benefits!
[0044] The heat conduction vacuum dryer can be selected from: horizontal disc vacuum dryer, vertical disc vacuum dryer, hollow blade vacuum dryer and other vacuum dryers; normal pressure heat conduction dryer, horizontal disc type, vertical disc type, hollow blade type and other dryers can also be selected. Disc and hollow blade dryers are both heat conduction dryers, which have the characteristics of small footprint, large unit volume output, high thermal efficiency, less dust, and no need for dust collector; uniform drying, can dry granular (such as water chestnut powder, kudzu root powder) and powder (add powder cabinet to crush and screen) products, and can be produced in a continuous assembly line. It has a good energy-saving effect.
[0045] Vacuum dryer, vacuum feeder and vacuum discharger can use upper and lower pneumatic butterfly valves, cooperate with intermediate storage bin, and electronically control the upper and lower butterfly valves to open and close in turn, and intermittently feed and discharge materials to achieve the purpose of locking vacuum and feeding and discharging materials.
[0046] Commonly used water vapor compressors are Roots steam compressors and centrifugal steam compressors. Roots steam compressors have the characteristics of reliable low-speed operation, large compression ratio, and relatively small flow rate; centrifugal steam compressors have the characteristics of high-speed flow rate, low noise, and low compression ratio. Electric drive can compress low-temperature and low-pressure secondary steam into high-temperature and high-pressure steam for heating steam. When the steam recompression temperature rises by 15°C, the energy efficiency ratio is nearly 10 times! . In evaporation engineering applications, the steam compressor inlet temperature is generally ≥80°C, the compression ratio is ≤2, and the inlet and outlet saturated steam temperature difference is ≤20°C. In a vacuum drying environment, when the drying temperature is selected at 50-55°C, the steam density is very low, the volume flow rate is large, and the pressure difference is small! Therefore, a steam compressor with large flow and low pressure difference should be selected for matching.
[0047] At 50°C, the saturated water vapor pressure is 0.012Mpa (vacuum degree - 0.088Mpa), and the density is 0.083Kg / m 3 , 12m 3 / Kg; compressed to 65°C, the saturated water vapor pressure is 0.025MPa (vacuum degree is -0.076Mpa), and the density is 0.161Kg / m3 , 6.2m 3 / kg. Compression ratio ≈ 2.08, pressure difference ≈ 0.013Mpa.
[0048] Assuming the total efficiency of the Roots steam compressor is 60% (volume coefficient 0.8, mechanical transmission efficiency 0.95, motor efficiency 0.8), the power consumption of the drive motor is: 0.072Kw / Kg steam, which is equivalent to 72Kw / h of power consumption per ton of evaporated water.
[0049] In some specific embodiments, the moisture content of the wet starch to be dried is 35-40% by weight.
[0050] In some specific embodiments, the wet starch to be dried is subjected to low-temperature vacuum drying to 50-55° C., the preheating drying temperature is 50-55° C., and the vacuum degree is -0.088-0.085 MPa.
[0051] In some specific embodiments, the secondary steam generated by the preheating and drying is compressed and desuperheated, and then used for heating and drying the first wet starch with a saturated steam temperature of 65 to 70° C. and a vacuum degree of -0.076 to 0.07 MPa.
[0052] In some specific embodiments, the working condition parameters of the high-temperature vacuum drying include: a drying temperature of 80 to 90° C. and a vacuum degree of -0.054 to 0.031 MPa.
[0053] In some specific embodiments, the moisture content of the second wet starch is 14-16% by weight.
[0054] In some specific embodiments, the moisture content of the dried high-temperature starch is 10-14% by weight.
[0055] In a second aspect, the present invention provides a system for implementing the starch energy-saving drying method according to any one of the first aspects, such as Figure 2 As shown, the system includes a low-temperature vacuum dryer 3, a low-temperature vacuum drying heater 5, a steam compressor 4, a high-temperature vacuum dryer 10, a high-temperature vacuum drying heater 12, and a normal pressure dryer 19 which are connected in sequence;
[0056] The vacuum feeder 2 of the low-temperature vacuum dryer is connected to the first conveyor belt 1, the low-temperature vacuum dryer 3 is connected to the low-temperature steam compressor 4 and the humidifier 9 in sequence, the humidifier 9 is connected to the low-temperature vacuum drying heater 5, the low-temperature vacuum drying heater 5 is connected to the first vapor-liquid separator 7, and the first vapor-liquid separator 7 is connected to a pump 8; the low-temperature vacuum dryer is connected to the high-temperature vacuum dryer 10 via the first vacuum discharger 6;
[0057] The high-temperature vacuum dryer 10 is connected to the humidifier 9 through the second vapor-liquid separator 14, the second pressure reducing valve 16, and the non-condensable gas pressure reducing valve 15; the high-temperature vacuum dryer 10 is connected to the second conveyor belt 17 through the second vacuum feeder 13, the second conveyor belt 17 is connected to the feed hopper 18 of the atmospheric pressure dryer 19, the atmospheric pressure dryer 19 is connected to the cooler 20, and the atmospheric pressure dryer 19 is connected to the humidifier 9 through the third pressure reducing valve 22.
[0058] In some specific embodiments, the atmospheric pressure dryer 19 is provided with a discharge port 21 .
[0059] In some specific embodiments, the system composition is shown in the attached Figure 2 The specific process operation flow is as follows:
[0060] ① Wet starch containing 35-40% moisture is delivered by the first conveyor belt 1 to the vacuum feeder 2 of the low-temperature vacuum dryer 3, and enters the machine for low-temperature vacuum drying. The front section of the low-temperature vacuum dryer 3 is the preheating section, which preheats the material to 50-55°C, the drying temperature is 50-55°C, and the vacuum degree is -0.088-0.085Mpa. The evaporated secondary steam enters the low-temperature steam compressor (Roots or centrifugal) 4, and the compressed steam is sprayed with water through the humidifier 9 to eliminate superheat. The saturated steam temperature is 65-70°C (temperature rise 15°C), and the vacuum degree is -0.076-0.07MPa. Then, it is returned to the low-temperature vacuum drying heater (disc or hollow blade) 5 to heat the starch, and the condensed water is pumped out by the first vapor-liquid separator 7 with a pump 8, and the non-condensable gas is pumped away with a vacuum pump;
[0061] 2. The wet starch is dried to a moisture content of 14-16% by the low-temperature vacuum drying heater 5, and this moisture content has less dust. The drying time is 2-3 hours, and then the material is discharged through the first vacuum discharger 6 and directly falls into the high-temperature vacuum dryer 10 for high-temperature vacuum drying. The drying temperature is 80-90°C, the vacuum degree is -0.054-0.031MPa, and the drying time is about 1 hour. The heated raw steam (102-108°C) enters the high-temperature vacuum dryer heater (disc or hollow blade) 12. The secondary steam is introduced into the humidifier 9 through the first pressure reducing valve 11 to cool down, mixed with the steam of the low-temperature steam compressor 4, and then enters the low-temperature vacuum dryer heater 5 to heat the starch. The condensed water and non-condensable gas pass through the second vapor-liquid separator 14. The condensed water is controlled by the second pressure reducing valve 16 and the non-condensable gas pressure reducing valve 15 respectively, and then enters the humidifier 9 to cool down, and after mixing, enters the low-temperature dryer heater 5 to continue heating.
[0062] 3 Starch is dried at high temperature to a moisture content of 10-14% (according to the product implementation standard requirements), discharged from the second vacuum feeder 13, and sent to the feed hopper 18 of the atmospheric pressure dryer 19 by the second conveyor belt 17, and enters the machine for atmospheric pressure cooling. Cooling uses ≤25℃ flowing water to pass through the cooler (disc or hollow blade) 20 to cool the starch, and adjust the cooling water flow to control the outlet hot water temperature at about 65℃. The cooled hot water is decompressed by the third pressure reducing valve 22 and enters the humidifier 9 for mixing and then enters the low-temperature dryer heater 5 for supplementary heating heat. The starch can be discharged from the discharge port 21 when it is cooled to below 30℃. For starch that requires powder (such as cassava starch, corn starch), it can be crushed and sieved with a powder cabinet, and then packaged into finished products; for starch that requires granular (such as water chestnut powder, kudzu root powder), it can be directly packed into bags into finished products.
[0063] By adjusting the input and output amount, the amount of heating steam and the drying time, the moisture content of the finished product after drying can be controlled.
[0064] 4 When the system is running, low-pressure raw steam (pressure <0.1Mpa, lower than the pressure vessel boiler standard) at 102-108℃ is added to the high-temperature vacuum dryer heater; and hot water generated by cooling the finished starch is recovered as a compensation heat source. Controlling the amount of both added can ensure the thermal balance of the entire system and achieve the purpose of continuous production.
[0065] The compensating heat source of the low-temperature vacuum dryer mainly comes from the secondary steam evaporated by the high-temperature vacuum dryer and the hot water recovered from the cooling of the finished starch. The high-temperature vacuum dryer also shares part of the drying amount of the starch moisture, which is equivalent to the second-effect evaporation drying, reducing the power consumption of the steam compressor; the cooling hot water is recycled, reducing the amount of raw steam, and further saving energy.
[0066] It should be noted that in the starch energy-saving drying method provided in the embodiment of the present invention, the raw materials involved, unless otherwise specified or limited, can all be commercially available products; at the same time, the process steps and parameters involved can all be carried out according to the existing starch production method preparation process or using existing equipment in a conventional operating manner.
[0067] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are intended only to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods in the following examples that do not specify specific conditions are usually measured according to national standards. If there is no corresponding national standard, then the conditions recommended by the manufacturer are followed.
[0068] Example 1
[0069] This example provides a starch energy-saving drying method and system, taking water chestnut powder drying as an example, including the following processes:
[0070] ① Wet starch with a moisture content of 38% is sent by a conveyor belt to the vacuum feeder of the low-temperature disc vacuum dryer and enters the machine for low-temperature vacuum drying. The front section of the low-temperature disc dryer is the preheating section, which preheats the material to 50°C, the drying temperature is 50°C, and the vacuum degree is -0.088Mpa. The evaporated secondary steam enters the low-temperature Roots steam compressor. After compression, the steam is sprayed with water through the humidifier to eliminate superheat. The saturated steam temperature is 65°C (temperature rise of 15°C), and the vacuum degree is -0.076MPa. Then, it is returned to the low-temperature vacuum drying heater (disc) to heat the starch, and the condensed water is pumped out through the vapor-liquid separator with a pump, and the non-condensable gas is pumped away with a vacuum pump;
[0071] 2. The wet starch is dried in a low-temperature disc vacuum dryer to a moisture content of 14%, and this moisture content produces less dust. The drying time is 2.5 hours, and then the material is discharged through the vacuum discharger and directly falls into the high-temperature disc vacuum dryer for high-temperature vacuum drying. The drying temperature is 85°C, the vacuum degree is -0.042MPa, and the drying time is about 1 hour. The heated raw steam (105°C) enters the high-temperature vacuum dryer heater (disc). The secondary steam is introduced into the humidifier through the pressure reducing valve to cool it down, mixed with the steam from the low-temperature steam compressor, and then enters the low-temperature vacuum dryer heater to heat the starch. Condensed water and non-condensable gas are controlled by the condensed water pressure reducing valve and the non-condensable gas pressure reducing valve of the vapor-liquid separator, respectively, and then enter the humidifier for cooling, and after mixing, enter the low-temperature dryer heater for continued heating.
[0072] 3 Starch is dried at high temperature to a moisture content of 10%, discharged from the vacuum feeder, and sent to the feed hopper of the atmospheric pressure dryer by a conveyor belt, and enters the machine for atmospheric pressure cooling. The cooling uses running water of ≤25℃ to pass through the cooler (disc or hollow blade) to cool the starch, and the cooling water flow is adjusted to control the outlet hot water temperature at around 65℃. The cooled hot water is decompressed by the pressure reducing valve and then enters the humidifier for mixing and then enters the low-temperature dryer heater for supplementary heating. Water chestnut powder can be discharged from the discharge port when it cools to below 30℃, maintained in granular form, and directly packaged in bags. The moisture content of the finished product meets local or enterprise standards of ≤13%; the color is the same as the product dried by hot air in the drying room.
[0073] Based on the drying system with a production capacity of 1000 kg / h of finished water chestnut powder (the moisture content is 10%), the energy consumption indicators are as follows:
[0074] ① Wet water chestnut powder: water content 38%, feed temperature 10℃ (winter), feed rate 1452Kg / h;
[0075] ②Water evaporation: 452Kg / h;
[0076] ③ Heating steam (105℃, 0.12MPa) gas consumption: about 100Kg / h, equivalent to 80kw / h of electricity (electric boiler);
[0077] ④ Roots steam compressor power consumption: 30Kw / h, flow rate 82.4m 3 / min, pressure difference 13Kpa;
[0078] ⑤ Low temperature disc dryer heating area: 250㎡;
[0079] ⑥ High temperature disc dryer heating area: 38㎡;
[0080] ⑦Cooling area of atmospheric pressure dryer: 38㎡;
[0081] ⑧ Auxiliary machines: disc vacuum dryer shaft stirring, feeder, transport belt, vacuum pump, etc. about 40Kw / h;
[0082] Total power consumption: 150Kw / h.
[0083] Compare this to:
[0084] ① Hot air flow drying: thermal efficiency is 50%, steam consumption is 904Kg / h, and auxiliary equipment such as fans is about 70Kw / h;
[0085] ② Drying in drying room: The thermal efficiency is 30%, the steam consumption is 1507Kg / h, and the auxiliary equipment such as fans is about 60Kw.
[0086] It can be seen that this technical solution saves a lot of steam, and the comprehensive energy consumption is only about 12% of arch room drying and 18% of hot air flow drying, with a very significant energy-saving effect.
[0087] Example 2
[0088] This example provides a starch energy-saving drying method and system, taking cassava starch drying as an example, including the following processes:
[0089] The difference from Example 1 is that the dried material is cassava starch, and the drying process is different in that the product is dried to a moisture content of 12%, and after cooling, it is crushed and sieved in a powder cabinet to obtain a powdered product, and then packaged into a finished product. The quality of the finished product meets the national standard of moisture ≤14%; the color is the same as that of the hot air dried product.
[0090] Various embodiments of the present invention may be presented in the form of a range; it should be understood that the description in the form of a range is only for convenience and brevity, and should not be understood as a rigid limitation on the scope of the present invention; therefore, the range description should be considered to have specifically disclosed all possible sub-ranges and single numerical values within the range. For example, the range description from 1 to 6 should be considered to have specifically disclosed sub-ranges, such as from 1 to 3, from 1 to 4, from 1 to 5, from 2 to 4, from 2 to 6, from 3 to 6, etc., as well as single numbers within the range, such as 1, 2, 3, 4, 5 and 6, which apply regardless of the range. In addition, whenever a numerical range is indicated herein, it is meant to include any cited number (fractional or integer) within the indicated range.
[0091] In the present invention, in the absence of contrary instructions, the directional words used, such as "upper" and "lower", are specifically the directions of the drawings in the accompanying drawings. In addition, in the description of the specification of the present invention, the terms "including", "comprising", etc. refer to "including but not limited to". In this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. In this article, "and / or" describes the association relationship of associated objects, indicating that three relationships may exist, for example, A and / or B, which can represent: A exists alone, A and B exist at the same time, and B exists alone. Wherein A, B can be singular or plural. In this article, "at least one" refers to one or more, and "plural" refers to two or more. "At least one", "at least one of the following" or similar expressions refer to any combination of these items, including any combination of singular or plural items. For example, "at least one of a, b, or c", or "at least one of a, b, and c", can both mean: a, b, c, ab (i.e., a and b), ac, bc, or abc, where a, b, c can be single or plural, respectively.
[0092] The foregoing is merely a specific embodiment of the present invention, which enables those skilled in the art to understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features claimed herein.
Claims
1. A starch energy-saving drying method, characterized in that: The starch energy-saving drying method comprises the following steps: The wet starch to be dried is subjected to low-temperature vacuum drying to obtain the first wet starch and secondary steam generated by the low-temperature vacuum drying; The secondary steam generated by the low-temperature vacuum drying is compressed and superheated, and then used for heating and drying the first wet starch to obtain a second wet starch; The second wet starch is subjected to high temperature vacuum drying to obtain dried high temperature starch and secondary steam generated by high temperature vacuum drying; Cooling the dried high-temperature starch to obtain dried starch and hot water generated by cooling; The secondary steam generated by the high-temperature vacuum drying and the hot water generated by the cooling are refluxed and used as a compensating heat source during the heating and drying of the first wet starch.
2. The energy-saving starch drying method according to claim 1, characterized in that: In terms of weight percentage, the moisture content of the wet starch to be dried is 35-40%.
3. The energy-saving starch drying method according to claim 1, characterized in that: The wet starch to be dried is subjected to low-temperature vacuum drying to 50-55° C., the low-temperature vacuum drying temperature is 50-55° C., and the vacuum degree is -0.088-0.085 MPa.
4. The energy-saving starch drying method according to claim 1, characterized in that: The secondary steam generated by the low-temperature vacuum drying is compressed and desuperheated, and then used for heating and drying the first wet starch at a saturated steam temperature of 65 to 70° C. and a vacuum degree of -0.076 to 0.07 MPa.
5. The energy-saving starch drying method according to claim 1, characterized in that: The working condition parameters of the high-temperature vacuum drying include: a drying temperature of 80 to 90° C. and a vacuum degree of -0.054 to 0.031 MPa.
6. The energy-saving starch drying method according to claim 1, characterized in that: Measured in percentage by weight, the moisture content of the second wet starch is 14-16%.
7. The energy-saving starch drying method according to claim 1, characterized in that: Calculated in weight percentage, the moisture content of the dried high-temperature starch is 10-14%.
8. A system for implementing the starch energy-saving drying method according to any one of claims 1 to 7, characterized in that: The system comprises a low-temperature vacuum dryer and a low-temperature vacuum dryer heater, a water vapor compressor, a high-temperature vacuum dryer, a high-temperature vacuum dryer heater and a normal-pressure dryer which are connected in sequence; The vacuum feeder of the low-temperature vacuum dryer is connected to the first conveyor belt, the low-temperature vacuum dryer is connected to the low-temperature steam compressor and the humidifier in sequence, the humidifier is connected to the low-temperature vacuum dryer heater, the low-temperature vacuum dryer heater is connected to the first vapor-liquid separator, and the first vapor-liquid separator is connected to a pump; the low-temperature vacuum dryer is connected to the high-temperature vacuum dryer via the first vacuum discharger; The high-temperature vacuum dryer is connected to the humidifier through the second vapor-liquid separator, the second pressure reducing valve, and the non-condensable gas pressure reducing valve; the high-temperature vacuum dryer is connected to the second conveyor belt through the second vacuum feeder, the second conveyor belt is connected to the feed hopper of the atmospheric pressure dryer, the atmospheric pressure dryer is provided with a cooler, and the atmospheric pressure dryer cooler is connected to the humidifier through the third pressure reducing valve.
9. The system according to claim 8, characterized in that The atmospheric pressure dryer is provided with a discharge port.
Citation Information
Patent Citations
Method and system for drying solid material
CN102080922A
Method and device for material drying in steam recompression mode
CN103217008A
Energy-saving vacuum drying technique and system
CN105157358A
Vacuum tube bundle drying system with waste heat for multiple-effect evaporation and pneumatic drying
CN105466157A
Method for reusing dry exhaust gas and combining with heat pump to realize energy saving
CN106554424A