Wide-temperature-range steam energy storage fused salt heat storage medium material

By adjusting the proportion of components in the mixed molten salt of potassium nitrate, calcium nitrate, and sodium nitrate, the problems of high melting point and narrow temperature range of existing salts were solved, and a low-cost, low-melting point, and wide-temperature steam energy storage system was developed. Molten salt heat storage medium material achieves efficient heat conduction performance and cost reduction.

CN118745332AInactive Publication Date: 2024-10-08河北井矿新能源科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410744984.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-11
Publication Date
2024-10-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing binary salts and ternary salts have high melting points and narrow operating temperature ranges, resulting in high cost and high consumption. It has not been possible to develop an ideal mixed molten salt formula with low melting point and wide temperature range.

Method used

Use a mixed molten salt composed of potassium nitrate, calcium nitrate, and sodium nitrate, 50-60wt% potassium nitrate, 10-15wt% calcium nitrate, 30-40wt% sodium nitrate. By adjusting the component ratio and treatment process, the melting point is lowered and increased decomposition temperature to form a low melting point, low-cost, wide temperature range steam energy storage molten salt heat storage medium material.

Benefits of technology

A low-cost mixed molten salt with a melting point of about 90°C and a decomposition temperature of over 660°C has been achieved. It has a wide operating temperature range, low corrosiveness and high thermal conductivity, significantly reducing the cost of the thermal storage system.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

The invention belongs to the technical field of physical heat transfer and energy storage in high and new technologies, and particularly relates to a mixed molten salt heat transfer and storage medium material which is low in melting point, high in decomposition temperature, low in cost and low in corrosivity. The material is composed of potassium nitrate, calcium nitrate and sodium nitrate, and the mixed molten salt medium material comprises 50-60 wt% of potassium nitrate, 10-15 wt% of calcium nitrate and 30-40 wt% of sodium nitrate. The mixed molten salt has the beneficial effects that the melting point of the mixed molten salt is about 90 DEG C, the decomposition temperature reaches 660 DEG C or above, and the medium material is wide in liquid temperature range and large in heat storage density. The material does not contain precious metal salt, so that the cost of a heat storage system is greatly reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of physical heat transfer and energy storage in high-tech, and specifically relates to a mixed molten salt heat transfer and heat storage medium material with low melting point, high decomposition temperature, low cost and low corrosion. Background Art

[0003] In the production process of some steam energy storage and heat treatment industries, the temperature of the heat transfer medium material needs to be above 600℃, but the heat transfer medium materials currently used are either too expensive or consume a lot of energy, and the production cost remains high. Molten salt is a high-temperature heat transfer medium material that is favored by domestic and foreign experts due to its advantages of high operating temperature, high thermal stability, high specific heat capacity, high convection heat transfer coefficient, low viscosity, low saturated vapor pressure, and low price. At present, binary salts and ternary salts have the defects of high melting point and narrow operating temperature range. Some mixed molten salts with low melting point and wide operating temperature range have been prepared at home and abroad, but an ideal mixed molten salt formula has not been developed. Summary of the invention

[0004] Based on this, it is necessary to provide a mixed molten salt with a low melting point, low cost and high decomposition temperature to address the problems of high melting point and narrow operating temperature range of existing molten salts. Its melting point is about 90°C, and its decomposition temperature reaches above 660°C. It does not contain precious metal salts and has a low cost.

[0005] To achieve the above purpose, the present invention discloses a wide temperature range steam energy storage molten salt thermal storage medium material, which is composed of potassium nitrate, calcium nitrate and sodium nitrate. The mixed molten salt medium material contains 50-60wt% potassium nitrate, 10-15wt% calcium nitrate and 30-40wt% sodium nitrate.

[0006] The beneficial effects of the present invention are:

[0007] (1) The present invention discloses a mixed molten salt heat transfer and heat storage medium material with a low melting point and a wide temperature range. The melting point of the mixed molten salt is 90°C, and the decomposition temperature reaches above 660°C. The medium material has a wide liquid temperature range and a large heat storage density.

[0008] (2) The mixed molten salt heat transfer and heat storage medium material with a low melting point and a wide temperature range described in the present invention does not contain precious metal salts, which greatly reduces the cost of the heat storage system. Specific embodiments

[0009] The embodiments of the technical solution of the present invention are described in detail below. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and are therefore only used as examples, and cannot be used to limit the scope of protection of the present invention. It should be noted that, unless otherwise specified, the technical terms or scientific terms used in this application should be the usual meanings understood by those skilled in the art to which the present invention belongs.

[0010] The present invention discloses a wide temperature range steam energy storage molten salt heat storage medium material, which is composed of potassium nitrate, calcium nitrate and sodium nitrate. The mixed molten salt medium material contains: 50-60wt% potassium nitrate, 10-15wt% calcium nitrate and 30-40wt% sodium nitrate. The melting point of this mixed molten salt is about 90°C, and its decomposition temperature is above 660°C, even reaching 680°C. The present invention utilizes the characteristics of nitrate molten salt, such as low electrical conductivity, low viscosity, good thermal conductivity, weak corrosiveness, low vapor pressure and wide operating temperature range. For mixed molten salts of different components, comprehensive consideration can be made from different performance aspects such as specific heat, molten salt, initial crystallization temperature and thermal stability to select the most suitable molten salt product.

[0011] The main mechanism of this technology to reduce the melting point of mixed molten salts is that the melting point of a single-component molten salt is too high, and mixing several molten salts to form a eutectic mixed molten salt can significantly reduce the melting point of the eutectic molten salt mixture. The eutectic mixed molten salt can ensure stable and uniform thermal properties of phases and components within a wide operating temperature range. The more components in the mixed molten salt, the lower the melting point of the mixture, but its decomposition temperature will also be reduced accordingly. The composition and proportion of the eutectic mixed molten salt are different, and its thermal properties are also different. Therefore, in the preparation of mixed molten salts, the needs of all parties should be weighed, and the types and proportions of components of the mixed molten salt should be carefully selected.

[0012] The preferred specific implementation of this series of mixed molten salts is:

[0013] First, the physical properties of binary mixed nitrates (NaNO3, KNO3) are modified and optimized by changing the component ratio and adding calcium nitrate and sodium nitrite. The present invention prepares mixed molten salts according to mass ratio, and preliminarily prepares 8 kinds of mixed molten salts with different component ratios. The specific operation method is as follows: three elemental salts are weighed by a high-precision balance, and they are fully mixed and ground and placed in a crucible for uniform mixing to form a solid mixed molten salt; the solid mixed molten salt is placed in a drying oven for constant temperature drying treatment, the drying oven temperature is set to 100°C, and the constant temperature drying time is 50h, so that the water contained in the mixture overflows; the dried solid mixed molten salt is transferred to a muffle furnace, and a heating program is set. After the muffle furnace is heated to a set temperature of 300°C at a heating rate of 5°C / min, the constant temperature heating is maintained for more than 12h, so that the mixed molten salt is completely melted to obtain a molten salt; after the mixed molten salt is cooled, it is taken out. Since the molten salt will form a hard solid crystalline salt after being melted and cooled, the present invention uses an ultra-fine grinder to crush the mixture, and the sample fineness can reach 20-200 meshes. While ensuring the fineness, the mixture is fully mixed, thereby ensuring the accuracy of the experiment; finally, the crushed molten salt is placed in a drying oven for constant temperature drying treatment for use in the experiment. After a large number of experimental analyses, four formulas of molten salt are finally selected. The following table shows the melting point, initial crystallization point and decomposition temperature of the four molten salt ratios.

[0014]

[0015] Example 1

[0016] This mixed molten salt is composed of 10wt% calcium nitrate, 60wt% potassium nitrate, and 30wt% sodium nitrate. Its melting point is 89.7°C as tested by DSC (differential scanning calorimetry), and its decomposition temperature is 673.4°C as tested by TG (thermogravimetric analysis).

[0017] Compared with Solar Salt, the melting point of this formula is reduced by nearly 130℃, and compared with Hitec salt, the melting point of this formula is reduced by nearly 60℃, while the decomposition temperature is as high as 673.4℃, which has a wider operating temperature range.

[0018] Example 2

[0019] This mixed molten salt is composed of 12.5wt% calcium nitrate, 55wt% potassium nitrate, and 32.5wt% sodium nitrate. The melting point is 90.3℃ according to DSC (differential scanning calorimetry) and the decomposition temperature is 669.5℃ according to TG (thermogravimetric analysis). Compared with Solar Salt, the melting point of this formula is reduced by nearly 130℃, and compared with Hitec salt, the melting point of this formula is reduced by nearly 55℃, while the decomposition temperature is as high as 669.5℃, which has a wider operating temperature range.

[0020] Example 3

[0021] This mixed molten salt is composed of 15wt% calcium nitrate, 50wt% potassium nitrate, and 35wt% sodium nitrate. Its melting point is 91.2°C as tested by DSC (differential scanning calorimetry), and its decomposition temperature is 681.3°C as tested by TG (thermogravimetric analysis).

[0022] Compared with Solar Salt, the melting point of this formula is reduced by nearly 130℃, and compared with Hitec salt, the melting point of this formula is reduced by nearly 55℃, while the decomposition temperature is as high as 681.3℃, which has a wider operating temperature range.

[0023] Example 4

[0024] This mixed molten salt is composed of 10wt% calcium nitrate, 50wt% potassium nitrate, and 40wt% sodium nitrate. Its melting point is 91.8°C as tested by DSC (differential scanning calorimetry), and its decomposition temperature is 677.8°C as tested by TG (thermogravimetric analysis).

[0025] Compared with Solar Salt, the melting point of this formula is reduced by nearly 130℃, and compared with Hitec salt, the melting point of this formula is reduced by nearly 55℃, while the decomposition temperature is as high as 677.8℃, which has a wider operating temperature range.

[0026] In addition, further experimental results show that the specific heat of this ternary mixed nitrate in the liquid temperature range is about 1.5-1.6 J / (g﹒K), and the density value is in the range of 1.75-1.95 g / cm3, so it has a high heat capacity. From room temperature to 300°C, its thermal conductivity is about 0.50-0.54 W / (m*K), and its thermal diffusion coefficient is about 0.17-0.19 mm / s, with good thermal conductivity. Its viscosity at 200°C is about 2.5-4.5 cp, at 300°C is about 2-3 cp, and at 400°C is about 1.8-2.2 cp.

[0027] The above description is only used to illustrate the technical solution of the present invention rather than to limit it. Other modifications or equivalent substitutions made to the technical solution of the present invention by ordinary technicians in this field should be included in the scope of the claims of the present invention as long as they do not depart from the spirit and scope of the technical solution of the present invention.

Claims

1. A wide temperature range steam energy storage molten salt thermal storage medium material, Features: The mixed molten salt medium material is composed of potassium nitrate, calcium nitrate and sodium nitrate, and contains: 50-60wt% potassium nitrate, 10-15wt% calcium nitrate and 30-40wt% sodium nitrate.