Biosensor based on inverted T-shaped undoped tunneling field effect transistor and preparation method thereof
By constructing a biodetection cavity and setting up a biodetection cavity in an inverted T-type undoped tunneling field effect transistor, the problems of insufficient sensitivity and conduction current of TFET biosensors are solved, and biotransmission with high sensitivity and high conduction current is realized. sensory effect, simplifying the process and reducing costs.
Patent Information
- Application Number
- CN202410738965.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-10-08
AI Technical Summary
Existing TFET-based biosensors have low sensitivity, insufficient on-current, and complex heavy doping processes, resulting in performance degradation and high cost.
Design an inverted T-type undoped tunneling field effect transistor. By constructing the position of the third gate electrode and the source region, a biological detection cavity is formed, which generates point tunneling and line tunneling, increases the conduction current, and inverts the inverted T-type undoped tunneling field effect transistor. Biological detection cavities are set up on both horizontal sides of the T-shaped channel area to improve sensitivity, and intrinsic doping materials are used to avoid heavy doping processes.
The sensitivity and conduction current of the biosensor are improved, the preparation process is simplified, the cost is reduced, and the biosensing effect of high sensitivity and high conduction current is achieved.
Smart Images

Figure CN118748208A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of semiconductor devices, and in particular relates to a biosensor based on an inverted T-type undoped tunneling field effect transistor and a preparation method thereof. Background Art
[0002] With the advancement of science and technology, medical testing technology and environmental testing have higher and higher requirements for rapid detection and analysis of biosensor technology. Especially in the field of medical testing, due to the increasing demand for instant detection tools, there is an urgent need for a biosensor with high sensitivity and low cost. FET (Field Effect Transistor) biosensors stand out with the advantages of label-free detection that does not destroy the inherent characteristics of biological molecules, miniaturization and good CMOS (Complementary Metal Oxide Semiconductor) process compatibility. Among the many FET-based biosensors, the unique tunneling conduction mechanism of TFET (Tunneling Field Effect Transistor) biosensors gives it a steeper subthreshold swing, lower off-state current and lower power consumption. However, there are also some problems with TFET-based biosensors, such as lower sensitivity and on-current, and random doping fluctuations caused by doping mutations at the junction of the source region and the channel.
[0003] The source region of existing TFET-based biosensors uses a heavy doping process to form a mutation junction at the interface between the source region and the channel. Since ion implantation and thermal annealing processes are required, the thermal budget is increased, and random doping fluctuations cause the performance of TFET-based biosensors to degrade. The on-current of TFET-based biosensors is low, two to three orders of magnitude lower than that of ordinary MOSFETs (Metal Oxide Semiconductor Field Effect Transistors). More importantly, the sensitivity of existing TFET-based biosensors is low, resulting in low biosensing efficiency.
[0004] A Chinese patent application with publication number CN112736142A discloses a biosensor based on a nanosheet stacked field effect transistor and a preparation method thereof, wherein the biosensor comprises a substrate, a source region, a nanosheet stacking region, an isolation region and a drain region; one side of the nanosheet stacking region close to the isolation region is surrounded by a ring-shaped gate metal layer to form a channel region, and the other side is in contact with the source region to form a source contact region; the nanosheet stacking region comprises a plurality of nanosheet conductive channel layers arranged in parallel; cavities are formed between the topmost nanosheet conductive channel layer and the gate metal layer, between every two nanosheet conductive channel layers adjacent to each other, and between the bottommost nanosheet conductive channel layer and the gate metal layer; the space in each cavity close to one end of the isolation region is filled with a gate dielectric, and the space at the other end not filled with the gate dielectric forms a biomolecule-filled cavity; the entrance of the biomolecule-filled cavity is located in the source contact region, and the biosensor stacks three conductive channels and has three cavities, but has low sensitivity.
[0005] Wang et al. (Simulation Study of Dual Metal~Gate Inverted T~Shaped TFETfor Label~Free Biosensing.IEEE SENSORS JOURNAL.2022.22.19.(18266~18272).Wang, Yunqi;Li, Cong;Li, Ouwen;Cheng, Shanlin;Liu, Weifeng;You, Hailong) disclosed a simulation study of a dual metal~Gate Inverted T~Shaped TFET for label~Free biosensing. The biosensor uses an inverted T-shaped channel with the drain region located at both ends of the channel. However, the heavy doping of the source and drain regions will cause the doping to diffuse into the channel, increasing the complexity of the process. In addition, the sensitivity is low.
[0006] Talukdar J et al (Talukdar J, Rawat G, Mummaneni K. DielectricallyModulated Single and Double Gate Tunnel FET Based Biosensors for EnhancedSensitivity[J]. IEEE sensorsjournal, 2021(21~23).DOI:10.1109 / JSEN.2021.3122582.)
[0007] A dielectric modulated single-gate and double-gate tunneling FET biosensor for enhancing sensitivity is disclosed. The biosensor adopts a source extension structure and SiGe pocket doping to produce line tunneling and increase the on-current. However, the heavy doping of the source and drain regions brings about the technical problem of random doping fluctuations and has low sensitivity. Summary of the invention
[0008] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a biosensor based on an inverted T-type undoped tunneling field effect transistor and a preparation method thereof. By constructing the positions of the third gate electrode and the source region, a biodetection cavity is formed between the third gate electrode and the source region, and while point tunneling is generated, line tunneling is generated at both ends of the inverted T-type channel region, which can increase the on-current of the biosensor; by arranging four biodetection cavities on the source region on both horizontal sides of the inverted T-type channel region, biological molecules can better modulate the coupling between the source region electrode and the source region, which can increase the sensitivity of the biosensor; the biosensor prepared by the present invention has high sensitivity, high on-current, and does not require a heavy doping process, so the preparation process is simple and the cost is low.
[0009] In order to achieve the above object, the technical solution adopted by the present invention is as follows:
[0010] A biosensor based on an inverted T-type undoped tunneling field effect transistor comprises a channel region 2 of an inverted T-type structure, source regions 1 are arranged on both sides of the horizontal part of the channel region 2, a drain region 3 is arranged on the top of the channel region 2, and first oxide layers 51 are arranged on both sides of the drain region 3 and the channel region 2; a second oxide layer 52 is arranged at the bottom of the channel region 2; the first oxide layer 51 and the top of the drain region 3 are covered with a drain region electrode 8 of an inverted concave structure; a first gate electrode 71 located below the drain region electrode 8 is arranged on the first oxide layer 51, a second gate electrode 72 is arranged at the bottom of the second oxide layer 52, third gate electrodes 73 are arranged on both horizontal sides of the second gate electrode 72, and a second bio-detection cavity 42 is arranged on the top of the third gate electrode 73; a third oxide layer 53 is arranged on both vertical sides of the source region 1, and a first bio-detection cavity 41 is arranged on the side of the third oxide layer 53 located at the top of the source region 1 close to the channel region 2; and the periphery of the third oxide layer 53 and the first bio-detection cavity 41 is covered with a source region electrode 6 of a C-type structure.
[0011] The source region 1, the channel region 2, and the drain region 3 are all intrinsically doped, with a doping concentration of 1×10 15 cm -3 .
[0012] The source electrode 6 is made of metal platinum, the drain electrode 8 is made of metal hafnium, the first gate electrode 71 and the second gate electrode 72 are both made of metal chromium, and the third gate electrode 73 is made of metal aluminum.
[0013] The thickness of the source region 1, the channel region 2, and the drain region 3 are all less than the Debye length; the thickness of the first oxide layer 51 and the second oxide layer 52 are both 0.5-1 nm, and the thickness of the third oxide layer 53 is 5-7 nm; the thickness of the source electrode 6, the drain electrode 8, the first gate electrode 71, the second gate electrode 72, and the third gate electrode 73 are all 15-20 nm; the spacing between the lower horizontal part of the source electrode 6 and the third gate electrode 73 is 2-3 nm, and the spacing between the vertical part of the drain electrode 8 and the vertical part of the first gate electrode 71 is 15-30 nm.
[0014] The thickness of the source region 1 , the channel region 2 , and the drain region 3 are all 10 nm.
[0015] The lengths of the source region 1 and the drain region 3 are both 100-150 nm, the length of the horizontal portion of the channel region 2 is 110-150 nm, and the length of the vertical portion is 50-100 nm; the length of the third oxide layer 53 is 60 nm-120 nm.
[0016] A method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor comprises the following steps:
[0017] Step 1: depositing silicon nitride on the surface of intrinsic silicon to form a silicon nitride protective layer;
[0018] Step 2: etching the intrinsic silicon with the silicon nitride protective layer to form an inverted T-shaped region; then polishing the surface of the inverted T-shaped region until the silicon nitride protective layer on the surface of the inverted T-shaped region is removed; the inverted T-shaped region includes an inverted T-shaped channel region 2, source regions 1 on both sides of the horizontal part of the inverted T-shaped channel region 2, and a drain region 3 at the top of the inverted T-shaped channel region 2;
[0019] Step 3: silicon dioxide is deposited on both sides of the channel region 2 and the drain region 3 formed in step 2 to form a first oxide layer 51; silicon dioxide is deposited at the bottom of the channel region 2 formed in step 2 to form a second oxide layer 52; silicon dioxide is deposited on both vertical sides of the source region 1 formed in step 2 to form an oxide reserved layer;
[0020] Step 4: depositing metal platinum on the periphery of the oxide reserved layer formed in step 3 to form a source electrode 6; depositing metal hafnium on the top and both sides of the first oxide layer 51 formed in step 3 to form an inverted drain electrode 8; depositing metal chromium on the first oxide layer 51 formed in step 3 and below the drain electrode 8 to form a first gate electrode 71; depositing metal chromium on the bottom of the second oxide layer 52 formed in step 3 to form a second gate electrode 72; depositing metal aluminum on both horizontal sides of the second gate electrode 72 to form a third gate electrode 73;
[0021] Step 5: Partially etch the oxide reserved layer formed in step 3 until the vertical portion 60nm to 120nm away from the source electrode 6, the unetched oxide reserved layer forms the third oxide layer 53, and the etched oxide reserved layer forms the biological detection cavity 4, finally forming an inverted T-type undoped tunneling field effect transistor biosensor.
[0022] The thickness of the inverted T-shaped region in step 1 is 10 nm; the thickness of the first oxide layer 51 and the second oxide layer 52 in step 3 are both 0.5-1 nm, and the thickness of the oxide reserved layer is 5-7 nm; the thickness of the deposited metal platinum, hafnium, aluminum and chromium in step 4 are all 15-20 nm.
[0023] The distance between the lower horizontal portion of the source electrode 6 and the third gate electrode 73 is 2-3 nm, and the distance between the vertical portion of the drain electrode 8 and the vertical portion of the first gate electrode 71 is 15-30 nm.
[0024] The deposition operations of step 1 and step 3 are both carried out by chemical vapor deposition process, the deposition operation of step 4 is carried out by reactive sputtering process, and the etching operations of step 2 and step 5 are carried out by plasma etcher.
[0025] Compared with the prior art, the present invention has the following beneficial effects:
[0026] 1. The present invention constructs the position of the third gate electrode and the source region so that a biological detection cavity is formed between the third gate electrode and the source region. While generating point tunneling, line tunneling is generated at both ends of the inverted T-shaped channel region, thereby increasing the on-current of the biosensor.
[0027] 2. The present invention sets four biological detection cavities on the source region on both sides of the inverted T-shaped channel region horizontally, so that biological molecules can better modulate the coupling between the source region electrode and the source region, thereby increasing the sensitivity of the biosensor.
[0028] 3. The biosensor prepared by the present invention avoids heavy doping of the source region and the drain region by using intrinsic silicon in the source region and the drain region, and does not require ion implantation and thermal annealing. The preparation process is simple and the cost is low.
[0029] In summary, the biosensor prepared by the present invention has high sensitivity and high on-current, does not require heavy doping process, has simple preparation process and low cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is a schematic diagram of the structure of the biosensor provided by the present invention.
[0031] In the figure: source region 1, channel region 2, drain region 3, first biological detection cavity 41, second biological detection cavity 42, first oxide layer 51, second oxide layer 52, third oxide layer 53, source region electrode 6, first gate electrode 71, second gate electrode 72, third gate electrode 73, drain region electrode 8.
[0032] Figure 2 The present invention provides a flow chart for the preparation of the biosensor.
[0033] Figure 3 This is a transfer characteristic curve diagram of the biosensor provided by the present invention.
[0034] Figure 4 This is a sensitivity curve diagram of the biosensor provided by the present invention. DETAILED DESCRIPTION
[0035] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.
[0036] like Figure 1 As shown, a biosensor based on an inverted T-type undoped tunneling field effect transistor comprises an inverted T-type channel region 2, both sides of the horizontal portion of the channel region 2 are provided with an active region 1, the top of the vertical portion of the channel region 2 is provided with a drain region 3, both sides of the drain region 3, both sides of the vertical portion of the channel region 2 and the top of the horizontal portion of the channel region 2 are provided with an L-shaped first oxide layer 51, and the bottom of the channel region 2 is provided with a second oxide layer 52; the top of the vertical portion of the first oxide layer 51, the top of the drain region 3 and the side of the vertical portion of the first oxide layer 51 are covered with an inverted concave drain electrode 8; the horizontal portion of the first oxide layer 51 The top of the source region 1 and the side of the vertical part of the first oxide layer 51 are provided with an L-shaped first gate electrode 71 located below the drain electrode 8, the bottom of the second oxide layer 52 is provided with a second gate electrode 72, the horizontal sides of the second gate electrode 72 are provided with third gate electrodes 73, and the top of the third gate electrode 73 is provided with a second biological detection cavity 42; the third oxide layer 53 is provided on both vertical sides of the source region 1, and the first biological detection cavity 41 is provided on the side of the third oxide layer 53 located at the top of the source region 1 close to the channel region 2; the periphery of the third oxide layer 53 and the first biological detection cavity 41 is covered with a source electrode 6 with a C-shaped structure;
[0037] The source region 1, the channel region 2, and the drain region 3 are all intrinsically doped, with a doping concentration of 1×10 15 cm -3 ; The lengths of the source region 1 and the drain region 3 are both 100 to 150 nm, the length of the horizontal portion of the channel region 2 is 110 to 150 nm, and the length of the vertical portion is 50 to 100 nm;
[0038] In order to make the induced carriers evenly distributed, the widths of the source region 1, the channel region 2, and the drain region 3 are all smaller than the Debye length, preferably 10 nm; the thickness of the third oxide layer 53 is 5-7 nm, and the length is 60 nm-120 nm; the spacing between the source electrode 6 and the third gate electrode 73 is 2-3 nm, and the spacing between the drain electrode 8 and the first gate electrode 71 is 15-30 nm;
[0039] The source electrode 6 is made of metal platinum, the drain electrode 8 is made of metal hafnium, the first gate electrode 71 and the second gate electrode 72 are both made of metal chromium, and the third gate electrode 73 is made of metal aluminum;
[0040] In order to induce holes in the source region 1, a “P + "Doping, need to meet And induce electrons in the drain region 3 to form "N + "Doping, need to meet Among them, φ m is the work function of the metal, x si is the electron affinity in silicon (x si =4.17eV), E g is the bandgap width of silicon (E g =1.12eV), q represents the charge; the source electrode 6 is made of metal platinum, whose work function φ m is 5.93eV, and the drain electrode 8 is made of metal hafnium, whose work function φ m It is 3.9eV.
[0041] like Figure 2 As shown, a method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor specifically comprises the following steps:
[0042] Step 1: using a chemical vapor deposition process to deposit silicon nitride on a 160-250 nm thick intrinsic silicon surface to form a silicon nitride protective layer;
[0043] Step 2: using a plasma etcher to etch the intrinsic silicon with the silicon nitride protective layer to form an inverted T-shaped region with a thickness of 10 nm; the inverted T-shaped region includes an inverted T-shaped channel region 2, two source regions 1 on both sides of the horizontal part of the inverted T-shaped channel region 2, and a drain region 3 at the top of the inverted T-shaped channel region 2; using a polisher to mechanically polish the surface of the inverted T-shaped region to remove the silicon nitride protective layer on the surface, so that the surface of the inverted T-shaped region is flat, which is convenient for the next step of depositing oxide;
[0044] Step 3: using a chemical vapor deposition process, silicon dioxide is deposited on both sides of the channel region 2 and the drain region 3 formed in step 2 to form an L-shaped first oxide layer 51; silicon dioxide is deposited at the bottom of the channel region 2 formed in step 2 to form a second oxide layer 52, and the thickness of the first oxide layer 51 and the second oxide layer 52 are both 0.5-1 nm; silicon dioxide is deposited on both sides of the source region 1 formed in step 2 to form an oxide reserved layer, and the thickness of the oxide reserved layer is 5-7 nm;
[0045] Step 4: Using a reactive sputtering process, metal hafnium is deposited on the top of the vertical portion of the first oxide layer 51 formed in step 3, the top of the drain region 3, and part of the side of the vertical portion of the first oxide layer 51 to form an inverted drain region electrode 8; metal chromium is deposited on the top of the horizontal portion of the first oxide layer 51 formed in step 3 and part of the side of the vertical portion of the first oxide layer 51 to form a first gate electrode 71, and the distance between the top of the vertical portion of the first gate electrode 71 and the bottom of the vertical portion of the drain region electrode 8 is 15 to 30 nm; and chromium is deposited on the bottom of the second oxide layer 52 formed in step 3. Metal chromium is used to form a second gate electrode 72, and metal aluminum is deposited on both horizontal sides of the second gate electrode 72 to form a third gate electrode 73; metal platinum is deposited on the top of the oxide reserved layer above the source region 1, the side of the oxide reserved layer above the source region 1, the side of the source region 1, the side of the oxide reserved layer below the source region 1, and the bottom of the oxide reserved layer below the source region 1 to form a source region electrode 6, and the distance between the lower horizontal part of the source region electrode 6 and the third gate electrode 73 is 2 to 3 nm; the thickness of the deposited metal platinum, hafnium, aluminum and chromium is 15 to 20 nm;
[0046] Step 5: The oxide reserved layer formed in step 3 is partially etched using a plasma etcher until the vertical portion 60nm to 120nm away from the source electrode 6, the unetched oxide reserved layer forms a third oxide layer 53, and the etched oxide reserved layer forms a biological detection cavity 4, ultimately forming an inverted T-type undoped tunneling field effect transistor biosensor.
[0047] The process conditions of the chemical vapor deposition process in the above steps are as follows: the growth temperature is 800°C, the pressure in the reaction chamber is 760mT, and the reaction source gas SiH 4 , the protective gas is helium; the parameters of the plasma etcher are that the pressure of the etching chamber is 10mT, the power is 20W, and 50sccm of Cl is input into the etching chamber through the gas supply system 2 and 20 sccm of O 2 The process conditions of the reactive sputtering process are as follows: the vacuum pressure of the reaction chamber is 8×10 -6 Torr, the power is 350W, and the Ar pressure is 5mTorr.
[0048] Example 1
[0049] A biosensor based on an inverted T-type undoped tunneling field effect transistor, wherein the lengths of the source region 1 and the drain region 3 are both 100 nm, the length of the horizontal portion of the channel region 2 is 110 nm, and the length of the vertical portion is 50 nm; the thickness of the third oxide layer 53 is 5 nm and the length is 60 nm; the spacing between the source region electrode 6 and the third gate electrode 73 is 2 nm, and the spacing between the drain region electrode 8 and the first gate electrode 71 is 15 nm.
[0050] A method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor comprises the following steps:
[0051] Step 1: Deposit silicon nitride on the surface of 160nm thick intrinsic silicon using a chemical vapor deposition process to form a silicon nitride protective layer;
[0052] Step 2: using a plasma etcher to etch the intrinsic silicon with the silicon nitride protective layer until 10 nm away from the bottom of the intrinsic silicon, to form an inverted T-shaped region, wherein the inverted T-shaped region includes an inverted T-shaped channel region 2, two source regions 1 on both sides of the horizontal part of the inverted T-shaped channel region 2, and a drain region 3 at the top of the inverted T-shaped channel region 2; using a polisher to mechanically polish the surface of the inverted T-shaped region, to remove the silicon nitride protective layer on the surface, to make the surface of the inverted T-shaped region flat, so as to facilitate the deposition of oxide in the next step;
[0053] Step 3: using a chemical vapor deposition process, silicon dioxide is deposited on both sides of the channel region 2 and the drain region 3 formed in step 2 to form an L-shaped first oxide layer 51; silicon dioxide is deposited at the bottom of the channel region 2 formed in step 2 to form a second oxide layer 52, and the thickness of the first oxide layer 51 and the second oxide layer 52 are both 0.5 nm; silicon dioxide is deposited on both vertical sides of the source region 1 formed in step 2 to form an oxide reserved layer, and the thickness of the oxide reserved layer is 5 nm;
[0054] Step 4: Using a reactive sputtering process, metal hafnium is deposited on the top of the vertical portion of the first oxide layer 51 formed in step 3, the top of the drain region 3, and part of the side of the vertical portion of the first oxide layer 51 to form an inverted drain region electrode 8; metal chromium is deposited on the top of the horizontal portion of the first oxide layer 51 formed in step 3 and part of the side of the vertical portion of the first oxide layer 51 to form a first gate electrode 71, and the distance between the top of the vertical portion of the first gate electrode 71 and the bottom of the vertical portion of the drain region electrode 8 is 15nm; and chromium is deposited on the bottom of the second oxide layer 52 formed in step 3. Depositing metal chromium to form a second gate electrode 72, depositing metal aluminum on both horizontal sides of the second gate electrode 72 to form a third gate electrode 73; depositing metal platinum on the top of the oxide reserved layer above the source region 1, the side of the oxide reserved layer above the source region 1, the side of the source region 1, the side of the oxide reserved layer below the source region 1, and the bottom of the oxide reserved layer below the source region 1 to form a source region electrode 6, and the spacing between the lower horizontal part of the source region electrode 6 and the third gate electrode 73 is 2nm; the thickness of the deposited metal platinum, hafnium, aluminum and chromium is 15nm;
[0055] Step 5: The oxide reserved layer formed in step 3 is partially etched using a plasma etcher until it is 60 nm away from the vertical portion of the source electrode 6. The unetched oxide reserved layer forms a third oxide layer 53, and the etched oxide reserved layer forms a biological detection cavity 4, ultimately forming an inverted T-type undoped tunneling field effect transistor biosensor.
[0056] Example 2
[0057] A biosensor based on an inverted T-type undoped tunneling field effect transistor, wherein the lengths of the source region 1 and the drain region 3 are both 125 nm, the length of the horizontal portion of the channel region 2 is 130 nm, and the length of the vertical portion is 75 nm; the thickness of the third oxide layer 53 is 6 nm and the length is 90 nm; the spacing between the source region electrode 6 and the third gate electrode 73 is 2.5 nm, and the spacing between the drain region electrode 8 and the first gate electrode 71 is 22.5 nm.
[0058] A method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor comprises the following steps:
[0059] Step 1: Deposit silicon nitride on the surface of 200nm thick intrinsic silicon using a chemical vapor deposition process to form a silicon nitride protective layer;
[0060] Step 2: using a plasma etcher to etch the intrinsic silicon with the silicon nitride protective layer until 10 nm away from the bottom of the intrinsic silicon, to form an inverted T-shaped region, wherein the inverted T-shaped region includes an inverted T-shaped channel region 2, two source regions 1 on both sides of the horizontal part of the inverted T-shaped channel region 2, and a drain region 3 at the top of the inverted T-shaped channel region 2; using a polisher to mechanically polish the surface of the inverted T-shaped region, to remove the silicon nitride protective layer on the surface, to make the surface of the inverted T-shaped region flat, so as to facilitate the deposition of oxide in the next step;
[0061] Step 3: using a chemical vapor deposition process, silicon dioxide is deposited on both sides of the channel region 2 and the drain region 3 formed in step 2 to form an L-shaped first oxide layer 51; silicon dioxide is deposited at the bottom of the channel region 2 formed in step 2 to form a second oxide layer 52, and the thickness of the first oxide layer 51 and the second oxide layer 52 are both 0.75nm; silicon dioxide is deposited on both vertical sides of the source region 1 formed in step 2 to form an oxide reserved layer, and the thickness of the oxide reserved layer is 6nm;
[0062] Step 4: Using a reactive sputtering process, metal hafnium is deposited on the top of the vertical portion of the first oxide layer 51 formed in step 3, the top of the drain region 3, and part of the side of the vertical portion of the first oxide layer 51 to form an inverted drain region electrode 8; metal chromium is deposited on the top of the horizontal portion of the first oxide layer 51 formed in step 3 and part of the side of the vertical portion of the first oxide layer 51 to form a first gate electrode 71, and the distance between the top of the vertical portion of the first gate electrode 71 and the bottom of the vertical portion of the drain region electrode 8 is 22.5nm; and chromium is deposited on the bottom of the second oxide layer 52 formed in step 3. Metal chromium is deposited to form a second gate electrode 72, and metal aluminum is deposited on both horizontal sides of the second gate electrode 72 to form a third gate electrode 73; metal platinum is deposited on the top of the oxide reserved layer above the source region 1, the side of the oxide reserved layer above the source region 1, the side of the source region 1, the side of the oxide reserved layer below the source region 1, and the bottom of the oxide reserved layer below the source region 1 to form a source region electrode 6, and the distance between the lower horizontal part of the source region electrode 6 and the third gate electrode 73 is 2.5nm; the thickness of the deposited metal platinum, hafnium, aluminum and chromium is 17.5nm;
[0063] Step 5: The oxide reserved layer formed in step 3 is partially etched using a plasma etcher until it reaches a vertical portion of 90 nm from the source electrode 6. The unetched oxide reserved layer forms a third oxide layer 53, and the etched oxide reserved layer forms a biological detection cavity 4, ultimately forming an inverted T-type undoped tunneling field effect transistor biosensor.
[0064] Example 3
[0065] A biosensor based on an inverted T-type undoped tunneling field effect transistor, wherein the lengths of the source region 1 and the drain region 3 are both 150 nm, the length of the horizontal portion of the channel region 2 is 150 nm, and the length of the vertical portion is 100 nm; the thickness of the third oxide layer 53 is 7 nm and the length is 120 nm; the spacing between the source region electrode 6 and the third gate electrode 73 is 3 nm, and the spacing between the drain region electrode 8 and the first gate electrode 71 is 30 nm.
[0066] A method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor comprises the following steps:
[0067] Step 1: Deposit silicon nitride on the surface of 250nm thick intrinsic silicon using a chemical vapor deposition process to form a silicon nitride protective layer;
[0068] Step 2: using a plasma etcher to etch the intrinsic silicon with the silicon nitride protective layer until 10 nm away from the bottom of the doped region, to form an inverted T-shaped region, wherein the inverted T-shaped region includes an inverted T-shaped channel region 2, two source regions 1 on both sides of the horizontal part of the inverted T-shaped channel region 2, and a drain region 3 at the top of the inverted T-shaped channel region 2; using a polisher to mechanically polish the surface of the inverted T-shaped region, to remove the silicon nitride protective layer on the surface, to make the surface of the inverted T-shaped region flat, so as to facilitate the deposition of oxide in the next step;
[0069] Step 3: using a chemical vapor deposition process, silicon dioxide is deposited on both sides of the channel region 2 and the drain region 3 formed in step 2 to form an L-shaped first oxide layer 51; silicon dioxide is deposited at the bottom of the channel region 2 formed in step 2 to form a second oxide layer 52, and the thickness of the first oxide layer 51 and the second oxide layer 52 are both 1nm; silicon dioxide is deposited on both sides of the source region 1 formed in step 2 to form an oxide reserved layer, and the thickness of the oxide reserved layer is 7nm;
[0070] Step 4: Using a reactive sputtering process, metal hafnium is deposited on the top of the vertical portion of the first oxide layer 51 formed in step 3, the top of the drain region 3, and part of the side of the vertical portion of the first oxide layer 51 to form an inverted drain region electrode 8; metal chromium is deposited on the top of the horizontal portion of the first oxide layer 51 formed in step 3 and part of the side of the vertical portion of the first oxide layer 51 to form a first gate electrode 71, and the distance between the top of the vertical portion of the first gate electrode 71 and the bottom of the vertical portion of the drain region electrode 8 is 30nm; and chromium is deposited on the bottom of the second oxide layer 52 formed in step 3. Depositing metal chromium to form a second gate electrode 72, depositing metal aluminum on both horizontal sides of the second gate electrode 72 to form a third gate electrode 73; depositing metal platinum on the top of the oxide reserved layer above the source region 1, the side of the oxide reserved layer above the source region 1, the side of the source region 1, the side of the oxide reserved layer below the source region 1, and the bottom of the oxide reserved layer below the source region 1 to form a source region electrode 6, and the spacing between the lower horizontal part of the source region electrode 6 and the third gate electrode 73 is 3nm; the thickness of the deposited metal platinum, hafnium, aluminum and chromium is 20nm;
[0071] Step 5: The oxide reserved layer formed in step 3 is partially etched using a plasma etcher until the vertical portion 120 nm away from the source electrode 6, the unetched oxide reserved layer forms a third oxide layer 53, and the etched oxide reserved layer forms a biological detection cavity 4, ultimately forming an inverted T-type undoped tunneling field effect transistor biosensor.
[0072] like Figure 3 As shown, through computer-aided design software, the biosensor of the present invention causes a significant change in the drain current of the biosensor after the biomolecules with different dielectric constants K completely fill the biodetection cavity, so that the biosensor can detect electrically neutral biomolecules.
[0073] like Figure 4 As shown, according to Figure 3 The sensitivity of the biosensor of the present invention is calculated by using the drain current in the electrode. Compared with the conventional undoped TFET biosensor, the sensitivity of the biosensor of the present invention is significantly higher than that of the conventional undoped TFET biosensor at different dielectric constants K. When the dielectric constant K is 12, the sensitivity of the biosensor of the present invention reaches 9.2×10 8 , an increase of 9.7×10 3 times, enabling more accurate resolution of biomolecules.
Claims
1. A biosensor based on an inverted T-type undoped tunneling field-effect transistor. Features: The invention comprises a channel region (2) of an inverted T-shaped structure, source regions (1) are arranged on both sides of the horizontal part of the channel region (2), a drain region (3) is arranged on the top of the channel region (2), and first oxide layers (51) are arranged on both sides of the drain region (3) and the channel region (2); a second oxide layer (52) is arranged on the bottom of the channel region (2); the first oxide layer (51) and the top of the drain region (3) are covered with a drain region electrode (8) of an inverted concave structure; a first gate electrode (71) located below the drain region electrode (8) is arranged on the first oxide layer (51), and the second oxide layer (52) is arranged on the drain region electrode (8) A second gate electrode (72) is arranged at the bottom of the source region (52), third gate electrodes (73) are arranged on both horizontal sides of the second gate electrode (72), and a second biological detection cavity (42) is arranged on the top of the third gate electrode (73); a third oxide layer (53) is arranged on both vertical sides of the source region (1); a first biological detection cavity (41) is arranged on the side of the third oxide layer (53) located at the top of the source region (1) close to the channel region (2); and a source region electrode (6) with a C-shaped structure is covered on the periphery of the third oxide layer (53) and the first biological detection cavity (41).
2. A biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 1, Features: The source region (1), the channel region (2) and the drain region (3) are all intrinsically doped, with a doping concentration of 1×10 15 cm -3 .
3. A biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 1, Features: The source electrode (6) is made of metal platinum, the drain electrode (8) is made of metal hafnium, the first gate electrode (71) and the second gate electrode (72) are both made of metal chromium, and the third gate electrode (73) is made of metal aluminum.
4. A biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 1, Features: The thickness of the source region (1), the channel region (2) and the drain region (3) are all less than the Debye length; the thickness of the first oxide layer (51) and the second oxide layer (52) are both 0.5-1 nm, and the thickness of the third oxide layer (53) is 5-7 nm; the thickness of the source region electrode (6), the drain region electrode (8), the first gate electrode (71), the second gate electrode (72) and the third gate electrode (73) are all 15-20 nm; the spacing between the lower horizontal part of the source region electrode (6) and the third gate electrode (73) is 2-3 nm, and the spacing between the vertical part of the drain region electrode (8) and the vertical part of the first gate electrode (71) is 15-30 nm.
5. A biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 4, Features: The thickness of the source region (1), the channel region (2) and the drain region (3) are all 10 nm.
6. A biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 1 or 4, Features: The lengths of the source region (1) and the drain region (3) are both 100-150 nm, the length of the horizontal portion of the channel region (2) is 110-150 nm, and the length of the vertical portion is 50-100 nm; the length of the third oxide layer (53) is 60 nm-120 nm.
7. A method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor according to any one of claims 1 to 6, It is characterized in that The steps include: Step 1: depositing silicon nitride on the surface of intrinsic silicon to form a silicon nitride protective layer; Step 2: etching the intrinsic silicon with the silicon nitride protective layer to form an inverted T-shaped region; then polishing the surface of the inverted T-shaped region until the silicon nitride protective layer on the surface of the inverted T-shaped region is removed; the inverted T-shaped region includes an inverted T-shaped channel region (2), source regions (1) on both sides of the horizontal part of the inverted T-shaped channel region (2), and a drain region (3) at the top of the inverted T-shaped channel region (2); Step 3: silicon dioxide is deposited on both sides of the channel region (2) and the drain region (3) formed in step 2 to form a first oxide layer (51); silicon dioxide is deposited at the bottom of the channel region (2) formed in step 2 to form a second oxide layer (52); silicon dioxide is deposited on both vertical sides of the source region (1) formed in step 2 to form an oxide reserved layer; Step 4: depositing metal platinum on the periphery of the oxide reserved layer formed in step 3 to form a source electrode (6); depositing metal hafnium on the top and both sides of the first oxide layer (51) formed in step 3 to form a concave drain electrode (8); depositing metal chromium on the first oxide layer (51) formed in step 3 and below the drain electrode (8) to form a first gate electrode (71); depositing metal chromium on the bottom of the second oxide layer (52) formed in step 3 to form a second gate electrode (72), and depositing metal aluminum on both horizontal sides of the second gate electrode (72) to form a third gate electrode (73); Step 5: Partially etch the oxide reserved layer formed in step 3 until the vertical portion is 60nm to 120nm away from the source electrode (6), the unetched oxide reserved layer forms a third oxide layer (53), and the etched oxide reserved layer forms a biological detection cavity (4), and finally forms an inverted T-type undoped tunneling field effect transistor biosensor.
8. A method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 7, Features: The thickness of the inverted T-shaped region in step 1 is 10 nm; the thickness of the first oxide layer (51) and the second oxide layer (52) in step 3 are both 0.5-1 nm, and the thickness of the oxide reserved layer is 5-7 nm; the thickness of the deposited metal platinum, hafnium, aluminum and chromium in step 4 are all 15-20 nm.
9. The method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 8, Features: The spacing between the lower horizontal part of the source electrode (6) and the third gate electrode (73) is 2-3 nm, and the spacing between the vertical part of the drain electrode (8) and the vertical part of the first gate electrode (71) is 15-30 nm.
10. The method for preparing a biosensor based on an inverted T-type undoped tunneling field effect transistor according to claim 7, Features: The deposition operations of step 1 and step 3 are both carried out by chemical vapor deposition process, the deposition operation of step 4 is carried out by reactive sputtering process, and the etching operations of step 2 and step 5 are carried out by plasma etcher.
Citation Information
Patent Citations